Manufacturing method of structure, structure, and housing
The method improves electrical conduction accuracy by transitioning from uneven to smooth surfaces in contact structures, addressing instability and foreign matter interference.
Patent Information
- Application Number
- JP2023172593
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-09-27
- Filing Date
- 2023-10-04
- Publication Date
- 2024-11-08
AI Technical Summary
Existing contact structures between electronic devices have a small contact area due to uneven surfaces, leading to instability in electrical conduction and potential disruption by foreign matter.
A method involving a first and second plate-like part with an elastic member having a bent portion, where a smooth and uneven surface are used to enhance contact accuracy by transitioning from uneven to smooth surfaces for stable conduction.
Ensures high-precision electrical conduction by removing foreign matter and maintaining contact area, thereby stabilizing electrical continuity.
Smart Images

Figure 2024159419000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a structure, a structure, and a housing. [Background technology]
[0002] In electronic devices such as personal computers and office machines, it is necessary to lower the electrical resistance value to ensure stable conduction between the contacts. However, if foreign matter gets into the contacts, it can cause problems with conduction. To address this issue, Patent Document 1 discloses a configuration in which an uneven structure is provided on the contact surface. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2012-195277 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in the embodiment of Patent Document 1, since the contact has an uneven structure, the contact area between the movable contact part and the electrode pad is small, and there is a risk that stable conduction cannot be achieved. Therefore, an object of the present invention is to improve the accuracy of conduction. [Means for solving the problem]
[0005] The means for solving the above problem is a method for manufacturing a structure comprising a first plate-shaped portion having electrical conductivity and a second plate-shaped portion having electrical conductivity, wherein the first plate-shaped portion has an elastic member extending from the first plate-shaped portion, the elastic member has a bent portion protruding toward the second plate-shaped portion, and the surface of the bent portion facing the second plate-shaped portion is provided with a smooth portion and an uneven portion having a rougher surface than the smooth portion, and the uneven portion is moved while being abutted against the second plate-shaped portion, and then the smooth portion is abutted against the second plate-shaped portion. Effect of the Invention
[0006] According to the present invention, continuity can be established with a higher degree of accuracy. [Brief description of the drawings]
[0007] [Figure 1] FIG. 2 is a perspective view of a housing constituting the structure of the present invention. [Diagram 2] 2A is a perspective view of the structure shown in FIG. 1, and FIG. 2B is a cross-sectional view taken along line AA in FIG. [Diagram 3] This is an enlarged view of the area surrounded by circle C in FIG. 2(b). [Figure 4] 6A and 6B are diagrams illustrating sliding between a first plate-shaped portion and a second plate-shaped portion. [Diagram 5] 6A and 6B are diagrams illustrating sliding between a first plate-shaped portion and a second plate-shaped portion. [Figure 6] 1A to 1C are diagrams illustrating a method for forming a concave-convex portion. [Figure 7] 13 is a top view of a main part of a movable contact 7 in a second embodiment. FIG. [Figure 8] 2A is a perspective view of the structure shown in FIG. 1, and FIG. 2B is a cross-sectional view taken along line DD in FIG. [Figure 9] 8(b) is an enlarged view of the area surrounded by circle E in FIG. 8(b). [Figure 10] 13A and 13B are diagrams showing modified examples of the elastic member. [Figure 11] 5 is an explanatory diagram illustrating a method of electrically connecting the first plate-shaped portion and the second plate-shaped portion. FIG. [Figure 12] 5 is an explanatory diagram illustrating a method of electrically connecting the first plate-shaped portion and the second plate-shaped portion. FIG. [Figure 13] 13A to 13C are diagrams illustrating modified examples of a method for electrically connecting the first plate-shaped portion and the second plate-shaped portion. [Figure 14] 1A to 1C are diagrams illustrating a method for manufacturing a molding surface. [Figure 15] 13 is a diagram illustrating a structure according to a fourth embodiment. FIG. [Figure 16] 15(b) is an enlarged view of the area surrounded by a circle G in FIG. [Figure 17]13 is a diagram illustrating a structure according to a fifth embodiment. FIG. [Figure 18] FIG. 17(b) is an enlarged view of the area surrounded by circle J in FIG. [Figure 19] 13A to 13C are diagrams showing modified examples of the structure in the sixth embodiment. [Figure 20] FIG. 3 is an enlarged view of a modified example of the area surrounded by a circle C in FIG. [Figure 21] 1 is a perspective view of an image forming apparatus to which the structure of an embodiment can be applied; [Figure 22] FIG. 2 is a schematic diagram of an image forming unit installed in the image forming apparatus. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] Hereinafter, the embodiment for carrying out the present invention will be described with reference to the drawings. However, the embodiment described below is one embodiment of the invention, and the present invention is not limited to this. Then, common configurations will be described with mutual reference to multiple drawings, and the description of configurations with common symbols will be omitted as appropriate. Items with the same name but different can be distinguished by adding "No. 0", such as the first item and the second item.
[0009] FIG. 1 is a perspective view showing an embodiment in which the structure according to the present invention is applied to a housing 1 made of a metal plate. The housing 1 is composed of a part consisting of a container 2 formed from a metal plate and a lid 3 covering the opening of the container 2. The container 2 is provided with an attachment surface 4 formed by bending the edge of the metal plate. The lid 3 is placed on the attachment surface 4 of the container 2 and fixed at a fastening portion 5 with screws, welding, or the like, to form the housing 1 into a box shape. The housing 1 can be used for housings of home appliances and personal computers, control boxes for copiers, processing machines, and the like, and electrical components and control-related devices can be attached or stored in the container 2. In order to prevent static electricity and electromagnetic interference generated in the housing 1, the container 2 and the lid 3 are each formed of a conductive material such as metal. In addition, when either the container 2 or the lid 3 is grounded, the other is also grounded, so that a structure is configured in which conduction is ensured between them.
[0010] In the housing 1 of this embodiment, a structural portion 6 provided on at least a part of a plurality of fastening portions 5 provided on an attachment surface 4 is configured to establish electrical continuity between the container 2 and the lid 3. The conductive materials constituting the container 2 and the lid 3 may be the same material or different materials.
[0011] The metal plate material used for the container 2 and the lid 3 of the housing 1 is preferably a conductive material such as iron or copper with a low electrical resistance. The thickness of the plate material is preferably 0.4 to 1.2 mm. The present invention can be implemented with any material and plate thickness that is a conductive material that can be plastically deformed. In some cases, the surface of the conductive material may be coated with a coating such as zinc plating in order to maintain rust resistance.
[0012] The surfaces of the metal plates forming the container 2 and the lid 3 are preferably covered with a coating having a lower conductivity than the conductive material constituting the metal plates. As the coating, an insulating coating made of an insulating material with high lubricity is preferably used to prevent scratches and fingerprints from remaining and to maintain a good appearance. However, from the viewpoint of conductivity, it is preferable that no coating is provided on the contact portions.
[0013] First Embodiment The configuration of the structure 6 in the first embodiment of Fig. 1 will be described with reference to Fig. 2 and Fig. 3. Fig. 2(a) is an enlarged view of the structure 6 in Fig. 1, and Fig. 2(b) is a cross-sectional view taken along line A-A in Fig. 2(a). Fig. 3 is an enlarged view of the area surrounded by a circle C in Fig. 2(b).
[0014] The structural portion 6 is a structure of a contact point between the plate-shaped portion 101 and the plate-shaped portion 102, where the plate-shaped portion 101 is provided, for example, on the lid 3, and the plate-shaped portion 102 is provided, for example, on the mounting surface 4 of the container 2. Then, by placing the lid 3 on the mounting surface 4, the plate-shaped portion 101 and the plate-shaped portion 102 overlap each other.
[0015] The plate-shaped part 101 has a movable contact 7 that is surrounded by the fixed contact 8 and extends from the connection part 9 of the plate-shaped part 101. The movable contact 7 and the fixed contact 8 are not provided with a protective insulating coating, and the movable contact 7 and the fixed contact 8 come into contact with each other to obtain electrical continuity. Here, the width direction of the movable contact 7 is the X direction, the direction in which the movable contact 7 extends is the Y direction, and the plate thickness direction is the Z direction. The movable contact 7 is configured to be deformable when a force is applied, and the thickness of the movable contact 7 is preferably equal to or less than the thickness of the plate-shaped part 101. The width of the movable contact 7 in the X direction is preferably equal to or less than the width of the connection part 9, and is preferably three times or more the thickness of the plate-shaped part 101. Here, the width of the connection part 9 is the width at the first bend in the direction from the connection part 9 toward the tip part 13 of the movable contact 7. The width of the movable contact 7 in the X direction is preferably configured to gradually narrow toward the tip part 13, and is preferably constant from a certain point. The tip portion 13 is an open end so as not to hinder the deformation of the movable contact 7.
[0016] The bent portion 11 of the movable contact 7 is preferably bent at an obtuse angle. This makes the bent portion 11 more easily deformable when pressure is applied thereto, and the angle becomes larger when pressure is applied. The bent portion 11 may be bent at an acute angle, and when it is bent at an acute angle, it is preferable that the smooth portion 14 is provided on the tip portion 13 side of the uneven portion 15. The smooth portion 14 and the uneven portion 15 may be arranged in the opposite direction. That is, the smooth portion 14 may be provided on the tip portion 13 side, and the uneven portion 15 may be provided on the bent portion 11 side (connection portion 9 side). Even in this case, the uneven portion 15 and the fixed contact 8 come into contact with each other and then the smooth portion 14 and the fixed contact 8 come into contact with each other, thereby achieving highly accurate electrical continuity. Another bent portion 12 is bent so as to protrude toward the plate-shaped portion 102 side, and the plate-shaped portion 101 and the plate-shaped portion 102 are configured to be electrically connected at the bent portion 12. It is preferable that the bent portion 12 has a curvature, and the surface of the bent portion 12 that is in electrical contact with the plate-like portion 102 has a curvature radius of 0.3 mm or more and 1.0 mm or less.
[0017] As shown in FIG. 3, on the plate-shaped portion 102 side of the bent portion 12, the smooth portion 14 and the uneven portion 15 are provided adjacent to each other with a boundary 16 interposed therebetween. The smooth portion 14 and the uneven portion 15 are in a relative relationship to each other, and by comparing the arithmetic mean roughness Ra of the two portions, the portion with the larger arithmetic mean roughness Ra may be the uneven portion 15, and the portion with the smaller arithmetic mean roughness Ra may be the smooth portion 14. The arithmetic mean roughness Ra of the smooth portion 14 is, for example, 0.3 μm or more and 0.9 μm or less, and the arithmetic mean roughness Ra of the uneven portion 15 is, for example, 10 μm or more and 20 μm or less. However, since the smooth portion 14 and the uneven portion 15 are in a relative relationship to each other as described above, they are not limited to the above ranges.
[0018] The uneven portion 15 is preferably in the form of a plurality of grooves extending in the X direction as shown in Fig. 3, but may be in a surface state in which the unevenness is not aligned, for example, as obtained by blasting treatment in which particulate abrasive is projected to roughen the surface. It is sufficient that the uneven portion 15 is configured so that foreign matter can be removed at least. The smooth portion 14 is a flat surface that has not been subjected to any special surface treatment to roughen the surface, and refers to a surface state equivalent to that obtained by rolling, cutting, or the like.
[0019] Next, a method of electrical connection between plate-like portion 101 and plate-like portion 102 in this embodiment will be described with reference to Fig. 4. When movable contact 7 descends toward plate-like portion 102, movable contact 7 (folded portion 12) comes into contact with plate-like portion 102. At this time, since fixed contact 8 is designed to have high rigidity, pushing folded portion 11 downward in the Z direction causes movable contact 7 to deform. The locations that deform are connection portion 9 and folded portion 11, and the deformation occurs in a direction that increases the bending angle. Note that the deformation that occurs here is designed to be within the range of elastic deformation, so when movable contact 7 is released from fixed contact 8, it recovers to its original shape.
[0020] FIG. 4(a) shows a state where the bent portion 12 and the plate-like portion 102 are not in contact with each other, and in this state, the plate-like portion 101 and the plate-like portion 102 are not yet electrically connected. By lowering the movable contact 7 toward the fixed contact 8 from the state shown in FIG. 4(a), the movable contact 7 (uneven portion 15) comes into contact with the fixed contact 8 as shown in FIG. 4(b). Although it is possible to obtain electrical conduction by the uneven portion 15 coming into contact with the fixed contact 8, it is difficult to obtain electrical conduction with high accuracy because the contact area is small. As the movable contact 7 continues to come into contact with the fixed contact 8, it gradually undergoes elastic deformation, but since the position of the lid 3 on which the movable contact 7 is provided is fixed with respect to the mounting surface 4, the lid 3 does not move, and the angle of the connection portion 9 with low rigidity and the bent portion 11 changes, so that the bent portion 12 moves in the Y direction.
[0021] Since a rotation moment around the X-axis occurs in the bent portion 12 as the bent portion deforms, the curved surface on which the uneven portion 15 and the smooth portion 14 are provided rotates around the X-axis in accordance with the movement in the Y-direction. The position of the boundary 16 also changes with the rotation, and the surface of the movable contact 7 that contacts the fixed contact 8 switches from the uneven portion 15 to the smooth portion 14 as shown in Fig. 4(c). The abutment of the smooth portion 14 and the fixed contact 8 allows for highly accurate electrical continuity between the plate-like portion 101 and the plate-like portion 102.
[0022] In the state of FIG. 4(b), the uneven portion 15 and the plate-shaped portion 102 come into contact with each other and slide, so that even if foreign matter such as dust is mixed in the plate-shaped portion 102, it can be collected by the uneven portion 15. If the smooth portion 14 comes into contact with the fixed contact 8 in a state where foreign matter is mixed in, there is a risk that good conduction cannot be achieved. Therefore, by returning to the state of FIG. 4(c) after removing the foreign matter, there is no foreign matter between the smooth portion 14 and the fixed contact 8, and good conduction can be achieved between the plate-shaped portion 101 and the plate-shaped portion 102. Even when the bent portion 12 is formed only by the uneven portion 15 without the smooth portion 14, it is possible to remove the foreign matter, but there is a risk that the contact area with the fixed contact 8 is small due to the formation of a groove, and the conduction stability cannot be achieved. Here, the foreign matter may be a substance that has been scraped off from plate-shaped portion 101 or plate-shaped portion 102 due to wear, or a material that is different from that of plate-shaped portion 101 and plate-shaped portion 102 (foreign matter from outside structure 1).
[0023] The plate-shaped portion 101 and the plate-shaped portion 102 may overlap to form the state shown in Fig. 4(b), or the plate-shaped portion 101 and the plate-shaped portion 102 may overlap to form the state shown in Fig. 4(a). When the state shown in Fig. 4(a) is formed, the plate-shaped portions can be overlapped and then pressure can be applied to the bent portion 11 to form the state shown in Fig. 4(b).
[0024] The uneven portion 15 shown in Fig. 4 has been described as having a constant arithmetic mean roughness Ra from the tip portion 13 side to the smooth portion 14 side, but is not limited to this. Fig. 5(a) is a diagram showing a state in which the bent portion 12 and the plate-shaped portion 102 are not in contact with each other. Fig. 5(b) is a diagram showing a state in which the uneven portion 15 and the plate-shaped portion 102 are in contact with each other. Fig. 5(c) is a diagram showing a state in which the smooth portion 14 and the plate-shaped portion 102 are in contact with each other.
[0025] For example, as shown in FIG. 5, the arithmetic mean roughness Ra of the uneven portion 15 may be smaller from the tip portion 13 side to the smooth portion 14 side. In other words, the frictional force against the fixed contact 8 may be smaller from the tip portion 13 side to the smooth portion 14 side. By configuring in this way, foreign matter is removed by the uneven portion 15 (first uneven portion) having a large arithmetic mean roughness Ra, and wear powder generated during the removal can be removed by the uneven portion 15 (second uneven portion) having a small arithmetic mean roughness Ra. In this case, the arithmetic mean roughness Ra of the uneven portion 15 on the tip portion 13 side is preferably 15 μm or more and 25 μm or less, and the arithmetic mean roughness Ra of the uneven portion 15 on the smooth portion 14 side is preferably 0.5 μm or more and 1.5 μm or less. It is preferable that the arithmetic mean roughness Ra of the uneven portion 15 on the tip portion 13 side is 10 times or more than the arithmetic mean roughness Ra of the uneven portion 15 on the smooth portion 14 side.
[0026] Next, a manufacturing method of the movable contact 7 according to this embodiment will be described with reference to Fig. 6. Fig. 6(a) is a diagram showing the state of the mold before molding, Fig. 6(b) is a diagram showing the state of the mold during molding, and Fig. 6(c) is a diagram showing the main part of the movable contact 7 which is a molded product.
[0027] The punch 21 is lowered onto the metal plate 20, which has been punched in advance to the outer shape of the movable contact 7, and the bent portion 12 is formed by clamping it with the die 22. At this time, it is also possible to press the metal plate 20 at a location away from the bent portion 12 with a die so that the metal plate 20 does not undergo molding distortion. The angle of the groove shape provided on the die 22 is equal to the angle of the bent portion 12 provided at the tip of the movable contact 7. The angle of the inclined surface of the punch 21 is preferably the same angle as the angle of the groove shape of the die 22 or an angle 1° to 2° smaller than that of the groove shape of the die 22. In the case of manufacturing by such a die molding, if an uneven shape is provided on the groove shape surface of the die 22 as shown in FIG. 6, the uneven shape is transferred to the metal plate 20 when the metal plate 20 is clamped between the punch 21 and the die 22. The uneven portion 15 may be formed by such a die transfer method, or may be formed by direct processing such as laser irradiation or blasting.
[0028] <Second embodiment> The movable contact 7 according to this embodiment will be described with reference to Fig. 7. Fig. 7(a) and Fig. 7(b) are top views of the main part of the movable contact 7. The movable contact 7 of this embodiment differs from the first embodiment in that the concave-convex portion 15 is not provided linearly in the X direction.
[0029] As shown in Fig. 7(a) and Fig. 7(b), the center of the uneven portion 15 in this embodiment is provided on the tip portion 13 side or the bent portion 11 side (connection portion 9 side) with respect to both ends of the movable contact 7 in the X direction. This configuration makes it easy to grasp the position where the smooth portion 14 and the fixed contact 8 abut. If the uneven portion 15 is provided linearly as in the first embodiment, it is difficult to grasp the position where the smooth portion 14 and the fixed contact 8 abut even when viewed from the side of the movable contact 7. Therefore, by not providing the uneven portion 15 linearly in the X direction as in this embodiment, it is easier to grasp the abutment position.
[0030] Here, the concave-convex portion 15 is described as being V-shaped and curved in the Y direction, but the shape is not limited to this. For example, the concave-convex portion 15 may be curved in a wavy manner. For example, in the case of a V-shape as shown in FIG. 7, the angle θ is preferably 100° or more and less than 180°.
[0031] <Third embodiment> The configuration of the structure 6 in the third embodiment of Fig. 1 will be described with reference to Fig. 8 and Fig. 9. Fig. 8(a) is an enlarged view of the structure 6 in Fig. 1, and Fig. 8(b) is a cross-sectional view taken along line D-D in Fig. 8(a). Fig. 9 is an enlarged view of the area surrounded by a circle E in Fig. 8(b).
[0032] The structural portion 6 is a contact structure between the plate-shaped portion 101 and the plate-shaped portion 102, where the plate-shaped portion 101 is provided, for example, on the attachment surface 4 of the lid 3, and the plate-shaped portion 102 is provided, for example, on the container 2. When the lid 3 is placed on the attachment surface 4, the plate-shaped portion 101 and the plate-shaped portion 102 overlap each other.
[0033] The plate-shaped portion 101 has a movable contact (elastic member) 7 that is surrounded by the fixed contact 8 and extends from a connection portion 9 of the plate-shaped portion 101. Here, the width direction of the movable contact 7 is defined as the X direction, the extension direction of the movable contact 7 is defined as the Y direction, and the plate thickness direction is defined as the Z direction. The movable contact 7 is configured to be deformable when a force is applied, and the thickness of the movable contact 7 is preferably equal to or less than the thickness of the plate-shaped portion 101.
[0034] The width of the movable contact 7 in the X direction is preferably equal to or smaller than the width of the connection portion 9, and is preferably three times or more the thickness of the plate-like portion 101. Here, the width of the connection portion 9 refers to the width at the first bending point in the direction from the connection portion 9 toward the tip portion 13 of the movable contact 7. The width of the movable contact 7 in the X direction is preferably configured to gradually narrow toward the tip portion 13, and is preferably constant from a certain point. The tip portion 13 is an open end so as not to hinder deformation of the movable contact 7.
[0035] The angle between the connection part 9 and the movable contact 7 is preferably 45° or less. Here, the angle between the connection part 9 and the movable contact 7 is the angle in the direction in which the movable contact 7 warps up relative to the plate-shaped part 101. In FIG. 8, the angle between the connection part 9 and the movable contact 7 is 0°. The higher the angle, the greater the amount of movement in the Y direction associated with the deformation of the movable contact 7 as the plate-shaped part 101 moves in the Z direction when the movable contact 7 of the plate-shaped part 101 abuts against the plate-shaped part 102. The length of the movable contact 7 extending from the connection part 9 to the tip part 13 in the Y direction is preferably 20 times or more the plate thickness and as long as possible. By making it longer, the amount of movement in the Y direction increases when the movable contact 7 abuts against the plate-shaped part 102.
[0036] It is preferable that the tip 13 has a curvature towards the plate-like portion 102, and the dimension of the curvature is preferably equal to or less than the plate thickness. Figure 10 shows examples of tip shapes in which the tip 13 is further provided with a curvature. Figures 10(a) and (b) show tip 13 of the movable contact 7 being provided with a shape that is bent towards the plate-like portion 102. Figure 10(c) shows tip 13 being provided with a convex shape towards the plate-like portion 102. By providing the tip shape of Figure 10, the dimension of the curvature can be made equal to or greater than the plate thickness. Tip 13 is a surface where the conductive material is exposed.
[0037] 9, the plate-shaped portion 102 has a covering portion 30 on the plate-shaped portion 101 side, which is covered with a material having a lower coefficient of friction than the plate-shaped portion 102. The covering portion 30 includes a molding surface 31 and a molding surface 32. The molding surface 32 is a thinner surface made of a material having a lower coefficient of friction than the molding surface 31.
[0038] The width of the molding surfaces 31, 32 is greater than the width of the movable contact 7, and the length is greater than the length over which the movable contact 7 moves when in contact with the plate-like portion 102. The thickness of the coating in the coating portion 30 decreases in the Y direction (the extension direction of the movable contact 7) from the connection portion 9 of the movable contact 7. The thickness of the coating portion 30 is, for example, from 2 μm to 3 μm, and the surface of the coating portion 30 where the coating is thinnest is 50 nm or less. However, the above-mentioned thickness of the coating is a value that depends on the appearance quality required for the plate-like portion 102 and the conductivity (resistance value) required for the structural portion 6, and is therefore not limited to the above range.
[0039] Next, a method of electrical connection between plate-shaped portion 101 and plate-shaped portion 102 in this embodiment will be described with reference to Fig. 11. Movable contact 7 descends toward plate-shaped portion 102 and moves in the Y direction until tip portion 13 comes into contact with plate-shaped portion 102. At this time, since fixed contact 8 is designed to have high rigidity, pushing tip portion 13 downward in the Z direction causes movable contact 7 to deform. The location that deforms is connection portion 9, which deforms in a direction that increases the bending angle. Note that the deformation that occurs here is designed to be within the range of elastic deformation, so when movable contact 7 is released from fixed contact 8, it recovers to its original shape.
[0040] FIG. 11(a) shows a state where the tip 13 and the plate-shaped portion 102 are not in contact with each other, and in this state, the plate-shaped portion 101 and the plate-shaped portion 102 are not yet electrically connected. By lowering the movable contact 7 toward the plate-shaped portion 102 from the state shown in FIG. 11(a), the tip 13 of the movable contact 7 comes into contact with the molding surface 31 as shown in FIG. 11(b). As the movable contact 7 continues to come into contact with the plate-shaped portion 102, it gradually undergoes elastic deformation, and the tip 13 moves in the Y direction along with the change in the bending angle of the movable contact 7. As the tip 13 moves in the Y direction on the molding surface 31, the thickness of the coating that it comes into contact with becomes thinner, and it comes into contact with the molding surface 32. In FIG. 11(c), when the movable contact 7 gradually deforms as it continues to come into contact with the covering portion 30, the contact load toward the plate-shaped portion 102 side increases, and the tip 13 approaches the plate-shaped portion 102 by crushing the thin coating of the molding surface 32, so that highly reliable electrical connection can be obtained.
[0041] In the state of FIG. 11(b), the coating of the coating 30 reduces the friction coefficient of the coating 30 to 0.05 or less, allowing the coating 30 to abut and slide with the tip 13 while reducing the frictional force. When the tip 13 abuts against the surface of the plate 102, the friction coefficient of the plate 102 is 0.5 or more, and the frictional force between the tip 13 and the plate 102 increases. If the surface roughness of the tip 13 and the plate 102 increases due to friction, the contact area between the tip 13 and the fixed contact 8 decreases, and there is a risk that good electrical continuity cannot be achieved. Therefore, by keeping the coating 30 in the state of FIG. 11(c), the increase in the frictional force during the contact between the tip 13 and the plate 102 can be suppressed, and the contact area does not decrease, allowing good electrical continuity to be achieved.
[0042] 12 shows another configuration of the contact state between the tip 13 of the movable contact 7 and the molding surface 32 of the fixed contact 8. When the movement of the movable contact 7 is completed, the coating on the molding surface 32 is almost zero, i.e., there is no coating. This allows the tip 13 to have a more reliable electrical connection with the plate-like portion 102. However, if the sliding distance of the tip 13 on the plate-like portion 102 increases, the contact area decreases due to wear, and there is a risk that the electrical connection will not be stable.
[0043] 12, the position of the movable contact 7 sliding on the molding surface 32 is determined by the shape and tool near the structural portion 6. The configuration in which the tip portion 13 rests on the plate-like portion 102 when the contact is complete, i.e., the sliding is completed on the molding surface 32 that is not coated, can ensure stability of conduction. In this case, the movable contact 7 slides on the molding surface 31, and only the position where the sliding is completed may be the molding surface 32, or the coating may become thinner from the molding surface 31 toward the molding surface 32.
[0044] Next, a method for manufacturing the molding surface 32 according to this embodiment will be described with reference to Fig. 13. Fig. 13(a) is a diagram showing the state of the mold before molding, and Fig. 13(b) is a diagram showing the state of the mold after molding.
[0045] The metal plate 24 which forms the forming surface 32 is placed on the die 23, and the punch 25 and the cam driver 26 are lowered together onto the metal plate 24. The surface of the metal plate 24 on the punch 25 side has a coating.
[0046] 13(b), the metal sheet 24 is sandwiched between the punch 25 and the die 23, and only the cam driver 26 is further lowered. The inclined surface of the cam driver 26 is pushed against the inclined surface of the punch 25 that contacts it, causing the punch 25 to move horizontally. The coating on the surface of the metal sheet 24 is peeled off by friction with the contacting surface of the punch 25, forming a forming surface 32.
[0047] When adjusting the thickness of the coating on the forming surface 32, the surface of the punch 25 that contacts the metal sheet 24 is tilted with respect to the horizontal surface along which the punch 25 moves. By increasing the contact pressure with the metal sheet 24 when the punch 25 moves, the amount of coating that is peeled off (the thickness of the coating to be peeled off) can be increased. By changing the amount of peeling, the thickness of the coating on the forming surface 32 can be controlled. The forming surface 32 may be formed using such a mold forming method, or the forming surface 32 may be provided by direct processing using laser irradiation.
[0048] <Fourth embodiment> The configuration of the structure 6 in the fourth embodiment will be described with reference to Fig. 14 and Fig. 15. Fig. 14(a) is an enlarged view of the structure 6 in this embodiment, and Fig. 14(b) is a cross-sectional view taken along line F-F in Fig. 14(a). Fig. 15 is an enlarged view of the area surrounded by a circle G in Fig. 14(b).
[0049] The structural portion 6 of this embodiment differs from that of the first embodiment in that the covering portions 30 and the plate-like portions 102 exposed from the covering portions 30 are arranged alternately in the extending direction of the movable contact 7.
[0050] In this embodiment, the ratio of the area of the plate-shaped portion 102 exposed from the coating to the direction (Y direction) in which the tip 13 of the movable contact 7 abuts and slides increases from 0% to 80% in the coating 30. That is, as shown in Fig. 14(b) and Fig. 15, the thickness of the coating is also gradually reduced in the direction in which the tip 13 abuts and slides in this embodiment.
[0051] When the surface of the plate-shaped portion 102 is rough, the plate-shaped portion 102 is partially exposed from the convex portion of the rough surface of the plate-shaped portion 102 toward the covering portion 30 as the thickness of the coating gradually decreases. The exposed ratio of the plate-shaped portion 102, which increases toward the Y direction of the covering portion 30, is preferably set to 30% or more and 80% or less. If it is 30% or more and 80% or less, the frictional force between the plate-shaped portion 102 and the movable contact 7 can be reduced compared to the frictional force when the plate-shaped portion 102 is 100% exposed. If the arithmetic mean roughness Ra of the surface of the plate-shaped portion 102 is, for example, 5 μm and the thickness of the coating is 2 μm or more and 3 μm or less, the exposed ratio of the conductive material can be increased to 30% or more and 80% by forming the molding surface 32 so that the thickness of the coating is 50 nm or less.
[0052] In this embodiment, the exposed ratio of the surface of the plate-shaped portion 102 where the tip portion 13 abuts against the plate-shaped portion 102 may be 100%. However, it is preferable to reduce the contact and sliding between the tip portion 13 and the surface where the plate-shaped portion 102 is 100% exposed in the Y direction in order to reduce wear between the tip portion 13 and the plate-shaped portion 102 due to friction. By adopting such a configuration, the surface where the tip portion 13 directly abuts against the plate-shaped portion 102 can be secured, so that conduction can be achieved with higher accuracy.
[0053] <Fifth embodiment> The configuration of the structure 6 in the fifth embodiment will be described with reference to Fig. 16 and Fig. 17. Fig. 16(a) is an enlarged view of the structure 6 according to this embodiment, Fig. 16(b) is a cross-sectional view taken along line H-H in Fig. 16(a), and Fig. 17 is a top view of Fig. 16(a). Fig. 18 is an enlarged view of the area surrounded by a circle J in Fig. 16(b).
[0054] The fixed contact 8 of this embodiment differs from the first and second embodiments in that the exposed plate-like portions 102 of the coating 30 are alternately arranged in a line in the direction in which the tip 13 of the movable contact 7 abuts and slides. The tip 13 can abut against a conductive material at the surface where the coating is thin, which is arranged in parallel and in a line.
[0055] 17, the plate-like portion 102 of the covering portion 30 is exposed linearly from the connection portion 9 side of the movable contact 7 toward the abutting side. The thickness of the covering portion 30 becomes thinner in the direction in which the tip of the movable contact 7 abuts and slides. The width and interval of the linear plate-like portion 102 of the covering portion 30 and the covering portion 30 in the X direction do not need to be constant.
[0056] It is preferable that the width of the movable contact 7 on the connection portion 9 side is formed so that the total width of the covering portion 30 is four or more times the total width of the exposed plate-like portion 102. By arranging the width at this ratio, it is possible to avoid contact between the tip portion 13 of the movable contact 7 and the plate-like portion 102 from the moment when the tip portion 13 starts to abut against the covering portion 30, and sliding can be performed with low friction.
[0057] 16(b) and 18, when the tip 13 of the movable contact 7 abuts against and slides against the covering 30, the contact pressure of the tip 13 presses the coverings 30 arranged in a line, and the tip 13 comes into contact with the exposed surface of the plate-like portion 102. Alternatively, as shown in Fig. 19, a configuration in which the width of the exposed conductive material increases in the Y direction may be used. In this case, it is preferable to mold the covering 30 on the tip 13 side of the movable contact 7 so that the total width of the exposed plate-like portion 102 is four times or less than the total width of the covering 30.
[0058] When the plate-shaped portion 102 is not exposed, the surface of the covering portion 30 that contacts the tip portion 13 may be such that the rate at which the plate-shaped portion 102 is exposed is 80% or less. By configuring in this manner, it becomes easier to grasp the conductivity between the plate-shaped portion 102 and the movable contact 7.
[0059] If the tip portion 13 abuts against a surface with a thin coating of the coating portion 30 (molded surface 32) or a surface with a large exposed ratio of the plate-like portion 102, as in the first and second embodiments, it is difficult to grasp the degree of conductivity (resistance value) obtained from the contact state of the movable contact 7. For this reason, as in the present embodiment, the amount of contact between the coating portion 30 and the surface on which the exposed plate-like portions 102 are linearly arranged relative to the width of the movable contact 7 can be confirmed from the outside, making it easier to grasp the degree of conductivity obtained.
[0060] Sixth embodiment Next, a structural portion 6 of the sixth embodiment will be described with reference to Fig. 20. Fig. 20 is an enlarged view of a modified example of the area surrounded by a circle C in Fig. 2(b).
[0061] The structural portion 6 of this embodiment is characterized by having a smooth portion 14 and an uneven portion 15 as in the first embodiment, and having a molding surface 31 and a molding surface 32 as in the third embodiment.
[0062] In this embodiment, the uneven portion 15 collects a small amount of lubricant applied to the molding surface 32, and good electrical conduction can be achieved by contacting the collected portion with the smooth portion 14. The uneven portion 15 does not necessarily have to collect the lubricant, and it is sufficient for it to simply remove dust from the molding surfaces 31 and 32.
[0063] In this way, by combining the various embodiments, the structure 6 can be made to be more easily conductive.
[0064] <Example> The present invention will be described in detail below with reference to examples, although the present invention is not limited to these examples.
[0065] Example 1 is an example of embodiment 1, Examples 2 and 3 are examples of embodiment 2, and Examples 4 and 5 are examples of embodiment 3. As comparative examples, Comparative Example 1 without the molding surface 32 and Comparative Example 2 without the covering portion 30 formed on the plate-shaped portion 102 were prepared.
[0066] The shape of the movable contact 7 is the same in Comparative Examples 1 and 2 and Examples 1 to 5. The thickness of the plate-like portion 101 is 0.6 mm, and the length of the movable contact 7 provided on the plate-like portion 101 from the connection portion 9 to the tip portion 13 is 18 mm. The width of the movable contact 7 is 6.6 mm at the connection portion 9 and narrows to 2 mm at a position 7.8 mm toward the tip portion 13. The angle between the connection portion 9 and the movable contact 7 before contact is 10 degrees with respect to the surface of the plate-like portion 101, and the specifications are such that a contact load of up to 1.5 kgf is applied when the movable contact 7 and the plate-like portion 102 contact each other.
[0067] The manufacturing conditions for the examples and comparative examples other than those mentioned above are as follows.
[0068] [Structure] Sliding distance of movable contact 7: 3 mm Material of moving contact 7: SECC (electrolytic zinc-plated steel sheet / friction coefficient 0.5) Material of fixed contact 8: SECC (electrolytic galvanized steel sheet / friction coefficient 0.5) Material of coating 30: Silicon-based organic coating (friction coefficient 0.05) Thickness of the coating 30: about 3 μm
[0069] In the example and comparative example, a comparative evaluation was performed on the frictional force and resistance generated between the movable contact 7, the plate-like portion 102, and the covering portion 30. The evaluation of the resistance was performed under the condition that the resistance value in the absence of electrical continuity was 200 Ω.
[0070] The exposed ratio of the plate-shaped portion 102 on the covering portion 30 was measured at each position on the covering portion 30 by energy dispersive X-ray spectroscopy.
[0071] The conditions and evaluation results of the example are shown in Table 1. The exposed width of the base material is the sum of the widths of the exposed plate-like portion 102. The maximum resistance value is shown.
[0072] [Table 1]
[0073] As shown in Table 1, the results showed that Examples 1 to 5 had lower frictional forces and resistance values than Comparative Examples 1 and 2.
[0074] In Comparative Example 1, the presence of covering portion 30 reduced the frictional force when movable contact 7 and plate-like portion 102 (or covering portion 30) came into contact with each other, but the resistance value increased due to covering portion 30. In Comparative Example 2, the resistance value decreased, but the frictional force during contact and sliding was high, reducing slidability, which resulted in rough surfaces of tip portion 13 and molding surface 32 and sometimes made the resistance value unstable.
[0075] In Example 1, since the covering portion 30 exists until the movable contact 7 completely abuts against the fixed contact 8, the frictional force at the time of abutment is reduced, and since the tip portion 13 contacts the plate-shaped portion 102 at the molding surface 32, the resistance value is lower than that of Comparative Example 2.
[0076] In Examples 2 and 3, the frictional force was low for the same reason as in Example 1, and the resistance value was lower than in Example 1 because the tip portion 13 came into contact with the plate-like portion 102 exposed from the molding surface 32 when the contact was completed. When the exposed ratio of the plate-like portion 102 was up to 80%, the frictional force was less than half that of Comparative Example 2, and the resistance value did not increase.
[0077] In Examples 4 to 5, tip portion 13 slides on coating portion 30 and contacts plate-shaped portion 102, resulting in frictional force and resistance values equivalent to those of Examples 2 to 3. From the above, it was confirmed that Examples 1 to 5 improve the slidability by reducing the frictional force between movable contact 7 and fixed contact 8 (plate-shaped portion 102 and coating portion 30), and stable conduction can be achieved.
[0078] FIG. 21 is an explanatory diagram of an image forming apparatus 600 as an example of an apparatus to which the housing 1 using the structural portion 6 according to the first and second embodiments can be applied.
[0079] The image forming apparatus 600 is, for example, an electrophotographic laser beam printer. The image forming apparatus 600 includes a housing 1, an exterior cover 601, an image forming section 610, and an image reading section 620.
[0080] The image reading unit 620 is a device that reads an image of a set document. The image forming unit 610 forms an image on a sheet based on image data. The sheet is a recording medium including ordinary paper, special paper such as coated paper, envelopes, paper such as index paper, plastic film for overhead projectors, and cloth.
[0081] FIG. 22 is a schematic diagram of the image forming unit 610 shown in FIG. 21. The image forming unit 610 is controlled by a control device provided inside the housing 1. As shown in FIG. 22, the image forming unit 610 includes an electrophotographic image forming unit PU and a fixing device 608. When an instruction to start an image forming operation is given, a photosensitive drum 602, which is a photosensitive member, rotates, and the surface of the photosensitive drum 602 is uniformly charged by a charging device 603. Then, an exposure device 604 modulates and outputs a laser beam based on image data transmitted from an image reading unit 620 or an external computer, and scans the surface of the photosensitive drum 602 to form an electrostatic latent image. This electrostatic latent image is developed by toner supplied from a developing device 605 to become a toner image.
[0082] In parallel with such an image forming operation, a feeding operation is performed to feed a sheet loaded on a cassette or manual feed tray (not shown) toward the image forming unit 610. The fed sheet is transported in accordance with the progress of the image forming operation by the image forming unit PU. Then, the toner image carried on the photosensitive drum 602 is transferred to the sheet by the transfer roller 606. The toner remaining on the photosensitive drum 602 after the toner image transfer is collected by the cleaning device 607. The sheet to which the toner image has been transferred is delivered to the fixing device 608, where it is sandwiched between a pair of rollers and heated and pressed. The sheet on which the toner has been melted and fixed to the sheet and the image has been fixed is discharged outside the machine by a pair of discharge rollers. In the case of double-sided printing, the sheet is conveyed in an inverted state by the inverting conveying unit 609, and is discharged outside the machine after an image has been formed on the back side by the image forming unit 610. The image forming unit 610 is an example of an image forming means capable of forming an image on a sheet as a recording medium, and may use an intermediate transfer type configuration including an intermediate transfer body instead of the above-mentioned direct transfer type, or may use other mechanisms such as an inkjet type.
[0083] The above-described embodiments can be modified as appropriate without departing from the technical concept. For example, in the previous embodiment, the container constituting the housing has a first plate-shaped portion and the lid has a second plate-shaped portion, but each may have an opposite plate-shaped portion. Also, in the previous embodiment, an example of a housing that provides electrical conduction between the container and the lid was described. However, the present invention can be applied to any structure that provides electrical conduction between members that have overlapping plate-shaped portions.
[0084] In addition, the above-described multiple embodiments may be combined with each other. In addition, some of the features of at least one of the embodiments may be deleted or replaced. Furthermore, new features may be added to at least one of the embodiments.
[0085] The disclosure of this specification includes not only what is explicitly described in this specification, but also all matters that can be understood from this specification and the drawings attached to this specification.
[0086] Furthermore, the disclosure of this specification includes the complement of each concept described in this specification. In other words, if this specification contains a statement that "A is greater than B," for example, even if the statement that "A is not greater than B" is omitted, this specification can be said to disclose that "A is not greater than B." This is because when a statement that "A is greater than B" is made, it is assumed that the case in which "A is not greater than B" is taken into consideration.
[0087] The disclosure of the present invention is given below.
[0088] (Method 1) A method for manufacturing a structure comprising a first plate-shaped portion having electrical conductivity and a second plate-shaped portion having electrical conductivity, wherein the first plate-shaped portion has an elastic member extending from the first plate-shaped portion, the elastic member has a bent portion protruding toward the second plate-shaped portion, and a surface of the bent portion facing the second plate-shaped portion is provided with a smooth portion and an uneven portion having a rougher surface than the smooth portion, and the uneven portion is moved while being abutted against the second plate-shaped portion, and then the smooth portion is abutted against the second plate-shaped portion.
[0089] (Method 2) A method for producing a structure according to method 1, characterized in that the uneven portion is provided closer to the tip of the elastic member than the smooth portion.
[0090] (Method 3) A method for manufacturing the structure described in Method 1 or 2, characterized in that the first plate-shaped portion and the second plate-shaped portion are abutted against each other, the uneven portion is moved while abutting against the second plate-shaped portion, and then the smooth portion is abutted against the second plate-shaped portion.
[0091] (Method 4) The method for manufacturing a structure described in any one of Methods 1 to 3, characterized in that the elastic member has another folded portion between the connection portion with the first plate-shaped portion and the folded portion, and the angle of the another folded portion on the side of the second plate-shaped portion is an obtuse angle.
[0092] (Method 5) 5. A method for producing a structure according to any one of methods 1 to 4, wherein the bent portion has a curvature.
[0093] (Method 6) Method 6. The method for producing a structure according to Method 5, wherein the radius of curvature of the surface of the bent portion on the side of the second plate-shaped portion is 0.3 mm or more and 1.0 mm or less.
[0094] (Method 7) 7. The method for producing a structure according to any one of Methods 1 to 6, wherein the uneven portion includes a first uneven portion and a second uneven portion having different arithmetic mean roughnesses Ra.
[0095] (Method 8) The method for producing a structure described in Method 7, characterized in that the first uneven portion has a larger arithmetic mean roughness Ra than the second uneven portion, and the first uneven portion is located closer to the tip of the elastic member than the second uneven portion.
[0096] (Method 9) 9. The method for producing a structure according to Method 7 or 8, wherein the arithmetic mean roughness Ra of the first uneven portion is 15 μm or more and 25 μm or less, and the arithmetic mean roughness Ra of the second uneven portion is 0.5 μm or more and 1.5 μm or less.
[0097] (Method 10) A method for producing the structure described in Method 8 or 9, characterized in that the first uneven portion is moved while being in contact with the second plate-shaped portion, and then the second uneven portion is moved while being in contact with the second plate-shaped portion, and the smooth portion is brought into contact with the second plate-shaped portion.
[0098] (Method 11) 11. The method for producing a structure according to any one of Methods 1 to 10, wherein the arithmetic mean roughness Ra of the concave and convex portions is 10 μm or more and 20 μm or less.
[0099] (Method 12) 12. The method for producing a structure according to any one of Methods 1 to 11, wherein the smooth portion has an arithmetic mean roughness Ra of 0.3 μm or more and 0.9 μm or less.
[0100] (Configuration 1) A structure comprising a first plate-shaped portion having electrical conductivity and a second plate-shaped portion having electrical conductivity, wherein the first plate-shaped portion has an elastic member extending from the first plate-shaped portion, the elastic member has a bent portion protruding toward the second plate-shaped portion, and a surface of the bent portion facing the second plate-shaped portion is provided with a smooth portion and an uneven portion having an arithmetic mean roughness greater than that of the smooth portion.
[0101] (Configuration 2) 2. The structure according to configuration 1, wherein the uneven portion is provided closer to the tip of the elastic member than the smooth portion.
[0102] (Configuration 3) 3. The structure according to configuration 1 or 2, wherein the first plate-shaped portion and the second plate-shaped portion abut against each other, and the smooth portion and the second plate-shaped portion abut against each other.
[0103] (Configuration 4) 4. The structure according to any one of configurations 1 to 3, wherein the concave-convex portion includes a first concave-convex portion and a second concave-convex portion having different arithmetic mean roughnesses Ra.
[0104] (Configuration 5) The structure described in configuration 4, characterized in that the first uneven portion has an arithmetic mean roughness Ra greater than that of the second uneven portion, and the first uneven portion is provided closer to the tip of the elastic member than the second uneven portion.
[0105] (Configuration 6) The structure described in configuration 4 or 5, wherein the arithmetic mean roughness Ra of the first uneven portion is 15 μm or more and 25 μm or less, and the arithmetic mean roughness Ra of the second uneven portion is 0.5 μm or more and 1.5 μm or less.
[0106] (Configuration 7) 7. The structure according to any one of configurations 1 to 6, wherein the uneven portion is coated with powder of the same material as that of the first plate-shaped portion or the second plate-shaped portion.
[0107] (Case 1) A housing comprising a container having one of the first plate-shaped portion and the second plate-shaped portion, and a lid having the other of the first plate-shaped portion and the second plate-shaped portion and covering an opening of the container, comprising a structure as described in any one of structures 1 to 7.
[0108] (Case 2) The housing described in Housing 1 is characterized in that the housing is made of sheet metal.
[0109] (Equipment 1) An electrical box comprising a control unit disposed inside the housing described in Housing 1 or 2, the control unit controlling electronic equipment outside the housing.
[0110] (device 1) An image forming unit that forms an image on a sheet, 13. An image forming apparatus, comprising: a control device provided inside the housing described in Housing 1 or 2, for controlling the image forming unit. [Explanation of symbols]
[0111] 6 Structure 7 Elastic member 12 Bending section 14 Smooth section 15 Uneven part 101 First plate-shaped part 102 Second plate-shaped portion
Claims
1. A method for manufacturing a structure including a first plate-shaped portion having electrical conductivity and a second plate-shaped portion having electrical conductivity, comprising: the first plate-shaped portion has an elastic member extending from the first plate-shaped portion, The elastic member has a bent portion protruding toward the second plate-shaped portion, The surface of the bent portion on the side of the second plate-shaped portion is provided with a smooth portion and an uneven portion having a roughness larger than that of the smooth portion, A method for manufacturing a structure, comprising moving the uneven portion while keeping it in contact with the second plate-like portion, and then bringing the smooth portion into contact with the second plate-like portion.
2. The method for manufacturing a structure according to claim 1, wherein the uneven portion is provided closer to the tip of the elastic member than the smooth portion.
3. The method for manufacturing a structure described in claim 1, characterized in that the first plate-shaped portion and the second plate-shaped portion are abutted against each other, the uneven portion is moved while abutting against the second plate-shaped portion, and then the smooth portion is abutted against the second plate-shaped portion.
4. The method for manufacturing a structure described in claim 1, characterized in that the elastic member has another bent portion between the connection portion with the first plate-shaped portion and the bent portion, and the angle of the another bent portion on the side of the second plate-shaped portion is an obtuse angle.
5. The method for manufacturing a structure according to claim 1 , wherein the bent portion has a curvature.
6. 6. The method for manufacturing a structure according to claim 5, wherein a radius of curvature of the surface of the bent portion on the side of the second plate-shaped portion is 0.3 mm or more and 1.0 mm or less.
7. 2. The method for manufacturing a structure according to claim 1, wherein the uneven portion includes a first uneven portion and a second uneven portion having different arithmetic mean roughnesses Ra.
8. The first uneven portion has an arithmetic mean roughness Ra greater than that of the second uneven portion, The method for manufacturing a structure according to claim 7 , wherein the first uneven portion is provided closer to the tip of the elastic member than the second uneven portion.
9. 8. The method for manufacturing a structure according to claim 7, wherein the arithmetic mean roughness Ra of the first uneven portion is 15 μm or more and 25 μm or less, and the arithmetic mean roughness Ra of the second uneven portion is 0.5 μm or more and 1.5 μm or less.
10. The method for manufacturing a structure described in claim 8, characterized in that the first uneven portion is moved while being in contact with the second plate-like portion, and then the second uneven portion is moved while being in contact with the second plate-like portion, and the smooth portion is brought into contact with the second plate-like portion.
11. 2. The method for manufacturing a structure according to claim 1, wherein the arithmetic mean roughness Ra of the concave and convex portions is 10 μm or more and 20 μm or less.
12. 2. The method for manufacturing a structure according to claim 1, wherein the smooth portion has an arithmetic mean roughness Ra of 0.3 μm or more and 0.9 μm or less.
13. A method for manufacturing a structure including a first plate-shaped portion having electrical conductivity and a second plate-shaped portion having electrical conductivity, comprising the steps of: a surface of the second plate-shaped portion on the side of the first plate-shaped portion has a covering portion that is covered with a material having a lower friction coefficient than the second plate-shaped portion; the first plate-shaped portion has an elastic member extending from the first plate-shaped portion, the covering portion has a first molding surface and a second molding surface having a thickness of the material smaller than that of the first molding surface, A method for manufacturing a structure, comprising the steps of: the elastic member abutting against the first molding surface, moving against the first molding surface, and then abutting against the second molding surface.
14. The method for manufacturing a structure according to claim 13 , wherein the first molding surface is provided in an extending direction relative to the elastic member of the second molding surface.
15. The method for manufacturing a structure according to claim 13, wherein the second plate-shaped portion is exposed at the second molding surface more than at the first molding surface.
16. The method for manufacturing a structure according to claim 13, characterized in that an exposed ratio of the second plate-shaped portion on the second molding surface is 30% or more and 80% or less.
17. A structure including a first plate-shaped portion having electrical conductivity and a second plate-shaped portion having electrical conductivity, the first plate-shaped portion has an elastic member extending from the first plate-shaped portion, The elastic member has a bent portion protruding toward the second plate-shaped portion, A structure characterized in that the surface of the bent portion facing the second plate-shaped portion is provided with a smooth portion and an uneven portion having a roughness greater than that of the smooth portion.
18. 18. The structure according to claim 17, wherein the uneven portion is provided closer to the tip of the elastic member than the smooth portion.
19. The structure according to claim 17 , wherein the first plate-shaped portion and the second plate-shaped portion are in contact with each other, and the smooth portion and the second plate-shaped portion are in contact with each other.
20. 18. The structure according to claim 17, wherein the uneven portion includes a first uneven portion and a second uneven portion having different arithmetic mean roughnesses Ra.
21. The first uneven portion has an arithmetic mean roughness Ra greater than that of the second uneven portion, 21. The structure according to claim 20, wherein the first uneven portion is provided closer to the tip of the elastic member than the second uneven portion.
22. The structure according to claim 20, wherein the arithmetic mean roughness Ra of the first uneven portion is 15 μm or more and 25 μm or less, and the arithmetic mean roughness Ra of the second uneven portion is 0.5 μm or more and 1.5 μm or less.
23. 18. The structure according to claim 17, wherein the uneven portion is adhered with the same material as the first plate-shaped portion or the second plate-shaped portion.
24. A structure including a first plate-shaped portion having electrical conductivity and a second plate-shaped portion having electrical conductivity, a surface of the second plate-shaped portion on the side of the first plate-shaped portion has a covering portion that is covered with a material having a lower friction coefficient than the second plate-shaped portion; the first plate-shaped portion has an elastic member extending from the first plate-shaped portion, A structure characterized in that the covering portion has a first molding surface and a second molding surface having a thickness of the material smaller than that of the first molding surface.
25. 25. The structure of claim 24, wherein the first molding surface is provided in a direction in which the elastic member extends relative to the second molding surface.
26. The structure according to claim 24 , wherein the second plate-shaped portion is exposed at the second molding surface more than at the first molding surface.
27. The structure according to claim 24, characterized in that an exposed ratio of the second plate-shaped portion on the second molding surface is 30% or more and 80% or less.
28. A housing comprising a container having one of the first plate-shaped portion and the second plate-shaped portion, and a lid having the other of the first plate-shaped portion and the second plate-shaped portion and covering an opening of the container, comprising a structure as described in any one of claims 13 to 27.
29. The housing of claim 28 , wherein the housing is made of sheet metal.
30. 29. An electrical equipment box comprising: a control unit provided inside the housing according to claim 28 for controlling electronic equipment outside the housing.
31. An image forming unit that forms an image on a sheet, 29. An image forming apparatus, comprising: a control device provided inside the housing according to claim 28, which controls the image forming unit.
Citation Information
Patent Citations
Contact and method of manufacturing the same
JP2012195277A