Method for diagnosing film for degradation
A multi-faceted analysis approach using non-destructive and destructive techniques effectively addresses the limitations of existing methods, providing a precise and efficient diagnosis of resin film deterioration, ensuring the preservation of historical records.
Patent Information
- Application Number
- JP2024125697
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2019-11-06
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-13
- Estimated Expiration
- 2040-11-04
AI Technical Summary
Existing methods for diagnosing resin film deterioration, particularly cellulose triacetate (TAC) film, face challenges in accurately detecting acetic acid gas generation and other signs of deterioration such as oxidation reactions, plasticizer elution, and cracks, often leading to inaccurate assessments of film condition.
A comprehensive method involving non-destructive and destructive analysis techniques, including visual observation, olfactory tests, Fourier Transform Infrared Spectroscopy (FT-IR), pH measurement, High-Performance Liquid Chromatography (HPLC), Karl Fischer moisture meter, thermogravimetric differential thermal analysis (TG-DTA), pyrolysis gas chromatography mass spectrometry (Py-GC/MS), and tensile testing, to assess film condition.
The method provides a more efficient and reliable assessment of resin film deterioration, enabling precise detection of various signs of degradation and allowing for timely preventive measures to preserve historical records.
Smart Images

Figure 2024160276000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for diagnosing deterioration of film, and more particularly to a method for diagnosing deterioration of resin-based archival film. [Background technology]
[0002] Traditionally, resin-based archival film (hereinafter simply referred to as "resin film") has been used to record and preserve various historical materials and documents in the form of "cinematograph film," "microfilm," "photographic film," "magnetic recording film," etc. Among resins, film using triacetate cellulose (TAC) as the base material (hereinafter referred to as "TAC film") has high flame resistance compared to the nitrocellulose film used in the past, and has been called a safety film and touted as being capable of being preserved for more than 100 years.
[0003] However, in recent years, it has become clear that under normal storage conditions, a phenomenon called vinegar syndrome occurs, and even when TAC film is used, it starts to deteriorate after about 30 years. When TAC film is stored in a high-temperature, high-humidity environment, the temperature and humidity cause hydrolysis of TAC. Acetic acid gas generated by the hydrolysis of TAC acts as a catalyst and promotes the hydrolysis reaction of TAC. Vinegar syndrome refers to this rapid deterioration of film caused by the hydrolysis of TAC.
[0004] When TAC film deteriorates due to factors other than the above-mentioned phenomenon called vinegar syndrome, such as oxidation reactions, elution of plasticizers, and cracks in the image-quality layer, the information recorded on the TAC film may be lost. Therefore, various methods have been used to diagnose the deterioration of resin films, including TAC.
[0005] For example, Non-Patent Document 1 describes a method using a piece of paper impregnated with bromocresol green sodium salt. That is, in the method described in Non-Patent Document 1, the piece of paper is placed in a film storage can together with a TAC film, and the presence or absence of acetic acid gas inside the storage can is detected from the color change of the piece of paper after a certain period of time has passed.
[0006] Patent Document 1 also describes a method using a glass detector tube filled with inorganic particles coated with sodium metasilicate and cresol red. That is, the method described in Patent Document 1 determines the concentration of acetic acid gas from the amount of color change of the particles inside the glass detector tube when gas present around a film storage can is passed through the glass detector tube.
[0007] In addition, Non-Patent Document 2 describes that the water content in the TAC film increases and the pH of the surface of the TAC film decreases as the deterioration of the TAC film progresses. That is, the method described in Non-Patent Document 2 checks the water content in the TAC film or checks the presence or absence of acetic acid attached to the TAC film by pH measurement.
[0008] In addition, Non-Patent Document 3 describes that when a TAC film plasticized with diethyl phthalate is subjected to accelerated aging, the decrease in the plasticizer content in the TAC film can be confirmed by thermogravimetric differential thermal analysis (hereinafter referred to as "TG-DTA") and Fourier transform infrared spectroscopy (hereinafter referred to as "FT-IR") analysis. That is, the method described in Non-Patent Document 3 confirms the thermal stability of the TAC film by TG-DTA analysis, or confirms the presence or absence of acid anhydride and signs of hydrolysis reaction by FT-IR analysis.
[0009] In addition, Non-Patent Document 4 describes that when a TAC film that has deteriorated over time is analyzed in a room temperature environment, a phthalate ester-based plasticizer is dissolved on the surface of the TAC film and then hydrolyzed to be detected as white crystals. That is, the method described in Non-Patent Document 4 confirms the presence or absence of white crystals dissolved on the surface of the TAC film.
[0010] In addition, Non-Patent Document 5 describes that the plasticizer contained in the TAC film can be analyzed by pyrolysis gas chromatography / mass spectrometry (hereinafter referred to as "Py-GC / MS") analysis or solvent extraction method, and the deterioration state of the film can be estimated based on the residual components of the plasticizer. That is, the method described in Non-Patent Document 5 confirms the type of plasticizer in the TAC film by Py-GC / MS analysis. [Prior art documents] [Patent documents]
[0011] [Patent Document 1] Japanese Patent Application JP2009-257838A [Non-patent literature]
[0012] [Non-Patent Document 1] E. Fran▲c▼ais, “The Safe and Accurate Way to Check Film for Vinegar Syndrome”, Image Permanence Institute, Rochester, NY (2001). [Non-Patent Document 2] NS Allen, M. Edge, JH Appleyard, TS Jewitt, CV Horie, D. Francis, “Acid-catalysed degradation of historic cellulose triacetate, cinematographic film: Influence of various film parameters”, Eur. Polym. J., 24(8), 707-712, (1988). [Non-Patent Document 3] E. Richardson, MT Giachet, M. Schilling, T. Learner, “Assessing the physical stability of archival cellulose acetate films by monitoring plasticizer loss”, Polym. Degrad. Stabil., 107, 231-236 (2014). [Non-Patent Document 4] Keiko Takahashi, Dai Hayakawa, Tomohiro Okamoto, Shoji Fujiwara, and Jin Yajima, "Analysis of white solids precipitated from deteriorated movie films - Chemical verification of the vinegar syndrome (1)," Bulletin of the Faculty of Engineering, Tokyo Polytechnic University, 36(1), 27-33 (2013). [Non-Patent Document 5] MT Giachet, M. Schilling, K. McCormick, J. Mazurek, E. Richardson, H. Khanjian, T. Learner, “Assessment of the composition and condition of animation cels made from cellulose acetate”, Polym. Degrad. Stabil., 107, 223-230 (2014). Summary of the Invention [Problem to be solved by the invention]
[0013] However, although the methods described in Non-Patent Document 1 and Patent Document 1 can detect acetic acid gas easily and at low cost, it is difficult to accurately determine whether acetic acid gas has been generated from the TAC film because acetic acid gas may be mixed into the film storage can from the external environment. In addition, the methods described in Non-Patent Document 1 and Patent Document 1 have difficulty in accurately detecting signs of the start of film deterioration other than vinegar syndrome, such as oxidation reactions, elution of plasticizers, and cracks in the image quality layer. Furthermore, the AD Strips in Non-Patent Document 1 and the detector tube in Patent Document 1 can only determine the acetic acid gas concentration approximately based on the color change.
[0014] In addition, the methods described in Non-Patent Document 2 and Non-Patent Document 3 forcibly accelerate the deterioration of TAC films under high temperature and high humidity, but the reactions that occur during this process are not necessarily the same as the reactions that occur during aging at room temperature in an actual storage site. Therefore, the methods described in Non-Patent Document 2 and Non-Patent Document 3 may evaluate a state that is different from the deterioration state in the actual storage site.
[0015] Furthermore, the methods described in Non-Patent Document 4 and Non-Patent Document 5 above have a problem in that they do not provide clear indicators for determining and diagnosing the deterioration state.
[0016] In view of the above, an object of the present invention is to provide a new film deterioration diagnosis method that can grasp the deterioration state of a resin film more efficiently and reliably than conventional methods. [Means for solving the problem]
[0017] As a result of intensive research, the present inventors have achieved the above object by employing the following film deterioration diagnosis method.
[0018] The film deterioration diagnostic method according to the present invention is a method for diagnosing deterioration of a resin film, and is characterized by using the following analysis method A and / or analysis method B, which are non-destructive analysis methods. Analysis method A: Visual observation and olfactory testing are used to check for abnormalities in the resin film. Analysis method B: Fourier transform infrared spectroscopy is used to confirm the presence of acid anhydrides and signs of hydrolysis in the resin film.
[0019] In addition, in the film deterioration diagnosis method according to the present invention, after using the analysis method A and / or the analysis method B, it is preferable to use the analysis method C and / or the analysis method D shown below, which are non-destructive analysis methods. Analysis method C: Check for the presence or absence of acetic acid attached to the resin film by pH measurement Analysis method D: Confirm the concentration of acetic acid gas released from the film by high performance liquid chromatography (hereinafter referred to as "HPLC") analysis.
[0020] Furthermore, it is more preferable that the film deterioration diagnosis method according to the present invention uses, after using the non-destructive analysis method, one or a combination of two or more of the following analysis methods E to H, which are destructive analysis methods. Analysis method E: Check the moisture content in the resin film using a Karl Fischer (hereinafter referred to as "KF") moisture meter. Analysis method F: Confirm the thermal stability of the resin film by thermogravimetric differential thermal analysis Analysis method G: Identify the type of plasticizer in the resin film by pyrolysis gas chromatography mass spectrometry Analysis method H: Check the mechanical strength of the resin film by tensile testing
[0021] Furthermore, in the film deterioration diagnosis method according to the present invention, it is preferable that the resin film is a cellulose triacetate film. Effect of the Invention
[0022] According to the present invention, the deterioration state of a resin film can be grasped more efficiently and reliably than in the past. [Brief description of the drawings]
[0023] [Figure 1] FIG. 13 is a diagram showing an FT-IR spectrum obtained by analysis method B according to the present embodiment. [Diagram 2] FIG. 13 is a diagram showing peak intensity ratios in the FT-IR spectrum obtained by analysis method B according to the present embodiment. [Diagram 3] FIG. 13 is a diagram showing the pH measurement results obtained by analysis method C according to the present embodiment. [Figure 4] FIG. 13 is a diagram showing the acetic acid gas concentration in a film storage canister determined by HPLC measurement using analysis method D according to the present embodiment. [Diagram 5] FIG. 13 is a diagram showing the results of moisture content measurement by analysis method E according to the present embodiment. [Figure 6] FIG. 13 is a diagram showing the results of TG curve measurement using analysis method F according to the present embodiment. [Figure 7] FIG. 13 is a diagram showing the thermal decomposition peak temperatures in analysis method F according to the present embodiment. [Figure 8] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (undegraded film A) using analysis method G according to the present embodiment. [Figure 9] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (undegraded film B) using analysis method G according to the present embodiment. [Figure 10] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (undegraded C film) using analysis method G according to the present embodiment. [Figure 11] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (film A without odor) using analysis method G according to the present embodiment. [Figure 12] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (odorless B film) using analysis method G according to the present embodiment. [Figure 13] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (odorless C film) using analysis method G according to the present embodiment. [Figure 14] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (film A having an odor) using analysis method G according to the present embodiment. [Figure 15] FIG. 13 is a diagram showing the results of Py-GC / MS measurement (film B having an odor) using analysis method G according to the present embodiment. [Figure 16] FIG. 13 is a diagram showing stress values at the time of film breakage obtained from a tensile test by analysis method H according to the present embodiment. [Figure 17] 1 is a chart showing an outline of a film deterioration diagnosis method according to an embodiment of the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] Hereinafter, an embodiment of the film deterioration diagnosis method according to the present invention will be described.
[0025] The film deterioration diagnostic method according to the present invention is a method for diagnosing deterioration of a resin film, and is characterized by using the following analysis method A and / or analysis method B, which are non-destructive analysis methods. Analysis method A: Visual observation and olfactory testing are used to check for abnormalities in the film. Analysis method B: Fourier transform infrared spectroscopy (FT-IR) analysis is used to check the film for the presence of acid anhydrides and signs of hydrolysis reactions.
[0026] The film deterioration diagnosis method according to the present invention uses at least one of the non-destructive analysis methods, the analysis method A and the analysis method B. If the deterioration of the film can be sufficiently confirmed by the analysis method A or the analysis method B, there is no need to carry out the analysis methods C to G described below. Therefore, in the film deterioration diagnosis method according to the present invention, the analysis method A and / or the analysis method B are essential analysis methods. The analysis method A and the analysis method B will be described below.
[0027] (A) Analysis method A Since the analysis method A checks for the presence or absence of abnormality in the resin film by visual observation and olfactory testing, it is possible to easily check the deterioration state of the resin film. Here, the visual observation checks for the presence or absence of elution of plasticizers and the occurrence of mold on the film surface. When the resin film deteriorates significantly, the elution of plasticizers and the occurrence of mold occur, which can be easily confirmed by visual inspection. In addition, the olfactory test checks for the presence or absence of abnormality by collecting air from inside the container in which the resin film is stored and using a person's sense of smell. For example, when a TAC film deteriorates, the TAC releases acetic acid gas due to the hydrolysis reaction of TAC. This generation of acetic acid causes an acetic acid odor to occur inside the film storage container. In this way, when an abnormal odor that can be smelled by a person occurs inside the film storage container, it becomes possible to confirm that the resin film has deteriorated significantly.
[0028] (B) Analysis method B Since the analysis method B checks the presence or absence of acid anhydride and signs of hydrolysis in the resin film by FT-IR analysis, it is possible to grasp the deterioration state of the resin film even if no abnormality is found in the olfactory test of the above analysis method A. For example, even if the TAC film does not smell of acetic acid, hydrolysis may progress and the plasticizer may precipitate or decompose. The film deterioration diagnosis method using the analysis method B will be described in detail below with reference to the embodiment.
[0029] In the analysis method B according to the present embodiment, an FT-IR Nicolet iS50 manufactured by Thermo Fisher Scientific Co., Ltd. was used as the apparatus. The measurement conditions were a resolution of 4 cm -1 , the number of accumulations is 32, and the measurement wave number range is 500 cm -1 From 4000cm -1 The automatic atmospheric correction was turned on, and a diamond crystal was used. The base side of the TAC film was measured by total reflectance (ATR). The spectrum obtained was corrected by ATR with an incidence angle of 45°, 1 reflection, and a refractive index of 1.5.
[0030] As the TAC films used in the measurement by the analysis method B according to the present embodiment, undegraded films and degraded films were used. Here, the undegraded films were prepared by visual and olfactory inspection using the above analysis method A, and those for which no signs of degradation were found (undegraded A to C (developed after 2010)). The degraded films were prepared by visual and olfactory inspection using the above analysis method A, and those for which no signs of degradation were found (odorless A to C (developed in April 1958)) and those for which signs of degradation were found by visual and olfactory inspection using the above analysis method A, and those for which signs of degradation were found by visual and olfactory inspection using the above analysis method A, and those for which signs of degradation were found by visual and olfactory inspection using the above analysis method A, respectively (odorful A, B (developed in December 1958)).
[0031] Figure 1 shows the FT-IR spectra for the three films, undegraded A, odorless A, and odorous A. Table 1 below shows the assignments of the main peaks in the FT-IR spectra obtained from Figure 1.
[0032] [Table 1]
[0033] As shown in FIG. 1 and Table 1, in the odorless A film and odorous A film, a peak due to acid anhydride C=O was observed at a wavenumber of 1790 cm -1 From 1850cm -1 The peaks derived from acid anhydride C=O were observed because acetic anhydride was formed by dehydration condensation of acetic acid molecules, and phthalic acid esters contained as plasticizers were dissolved on the film surface to form phthalic anhydride. As no peaks derived from acid anhydride C=O were observed for undegraded film A, it is believed that no generation of acetic acid gas or dissolution of plasticizers occurred. Thus, for TAC films, the presence or absence of peaks derived from acid anhydrides can be used as one criterion for the degradation of the film.
[0034] In addition, Figure 2 shows the peak intensity ratios of the FT-IR spectra for the eight films, undegraded A to C, odorless A to C, and odorous A and B. This peak intensity ratio is the value obtained by dividing the peak intensity derived from OH groups by the peak intensity derived from CH groups for each TAC film, specifically, the peak intensity at a wave number of 3480 cm -1 The peak intensity at wavenumber 1370 cm -1 The peak intensity ratio is calculated by dividing the peak intensity ratio by the peak intensity at 1000 nm. The error bars in the figure indicate the standard error of the peak intensity ratio. FIG. 2 shows that the peak intensity ratio increases in the order of undegraded film, odorless film, and odorous film. This result is believed to be due to the fact that as the hydrolysis reaction of TAC progresses, the peak intensity derived from OH groups increases and the peak intensity of bonds derived from acetyl groups in TAC (e.g., CH3 groups, C=O groups, and CO-O groups) decreases. Therefore, although the results shown in this embodiment are based on CH3 groups, the peak intensity derived from CO-O groups and C=O groups can also be used in the film deterioration diagnosis method according to the present invention. In this way, the deterioration progress of the resin film can be determined from the peak intensity ratio as well.
[0035] The above-described analytical method A and analytical method B are effective when the deterioration of the resin film has progressed significantly. When the deterioration of the resin film can be confirmed using at least one of the non-destructive analytical methods A and B, there is no need for further deterioration diagnosis.
[0036] In addition, in the film deterioration diagnosis method according to the present invention, it is preferable to use the above-mentioned analytical method A and / or the above-mentioned analytical method B, and then use the following analytical method C and / or analytical method D, which are non-destructive analytical methods. Analysis method C: Check for the presence of acetic acid on the film by pH measurement Analysis method D: Confirm the concentration of acetic acid gas released from the film by HPLC analysis
[0037] In the film deterioration diagnosis method according to the present invention, the deterioration state of the resin film can be grasped more reliably by using the nondestructive analysis method of the analysis method A and / or the analysis method B, and then using at least one of the nondestructive analysis methods C and D. Hereinafter, these analysis methods C and D will be described.
[0038] (C) Analysis method C Analysis method C confirms the presence or absence of acetic acid attached to the film by pH measurement, and is therefore effective when the deterioration state of the resin film cannot be sufficiently confirmed using the above analysis method A and / or the above analysis method B. Hereinafter, a film deterioration diagnosis method using analysis method C will be described in detail with reference to an embodiment.
[0039] In the analysis method C according to the present embodiment, a portable pH meter D-71 manufactured by Horiba Ltd. was used as the device. The ultrapure water was collected from a tap water direct-connected ultrapure water production device Direct-Q UV5 manufactured by Merck Ltd. Then, 100 mL of ultrapure water was placed in a glass beaker, and a part of the TAC film (width 3.5 cm x length 10 cm) was immersed in the ultrapure water for 10 seconds, and the pH of the immersed solution was measured. As the TAC films used for measurement in the analysis method C according to the present embodiment, eight films, namely undegraded A to C, odorless A to C, and odorous A and B, shown in the analysis method B according to the above embodiment, were used.
[0040] Figure 3 shows the pH measurement results for eight films, A to C, odorless A to C, and odorous A and B. The error bars in the figure indicate the standard error of the pH measurement results. Figure 3 shows a tendency for the pH to decrease in the order of undegraded A to C, odorless A to C, and odorous A and B. This is thought to be because acetic acid molecules attached to the TAC film dissolved in the ultrapure water. Here, the pH of odorless B and C films is lower than that of odorless A, suggesting the possibility that there are more acetic acid molecules attached to the film. Incidentally, the pH of ultrapure water is theoretically 7.0, but since it immediately absorbs carbon dioxide in the air, the pH becomes slightly more acidic (6.9 to 6.0) as time passes after it is taken from the ultrapure water production device. As the amount of acetic acid attached to the surface of TAC film tends to increase as it deteriorates, so when the pH of the water in which the film is immersed becomes 6.0 or less, it can be considered that deterioration is progressing. In this way, it is possible to grasp the deterioration state of a resin film by the presence or absence of acetic acid attached to it.
[0041] (D) Analysis method D Analysis method D uses HPLC analysis to confirm the concentration of acetic acid gas released from the film, and is therefore effective when the deterioration state of the resin film cannot be sufficiently confirmed using the above analysis method A and / or the above analysis method B. Hereinafter, a film deterioration diagnosis method using analysis method D will be described in detail with reference to an embodiment.
[0042] In the analysis method D according to the present embodiment, an HPLC system Prominence LC-20A manufactured by Shimadzu Corporation and a UV-vis detector SPD-20A were used as the apparatus. In addition, a Shim-pack SCR-102H manufactured by Shimadzu GLC Corporation was used as the column. The analysis conditions were as follows: mobile phase: 5.0 mM perchloric acid aqueous solution (pH 2.3), flow rate: 1.5 mL / min, UV detection wavelength: 210 nm, cell temperature: 40° C., and sample solution injection amount: 20 μL. Then, a hole was made in the center of the lid of a film storage can (diameter 27.8 cm, height 4.5 cm) made of zinc-plated steel plate, and the can was sealed with a silicone rubber stopper and caulking agent, and a TAC film roll was placed in the film storage can and the lid was closed. After leaving it at room temperature for one week, a hole was made in the silicone stopper with a syringe needle, and 60 mL of gas in the can was collected using a glass syringe (capacity 100 mL) manufactured by Tsubasa Kogyo Co., Ltd., and dissolved in 1 mL of ultrapure water to prepare a sample solution for HPLC measurement.
[0043] Since the area value of the peak observed at a retention time of about 7.1 min in the chromatogram is proportional to the acetic acid concentration, the acetic acid gas concentration in the film storage can was calculated from the calibration curve. The calibration curve was created using acetic acid (special grade, purity 99.7%) manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. The eight TAC films used for measurement in analysis method D according to the present embodiment were those shown in analysis method B according to the above embodiment, namely undegraded A to C, odorless A to C, and odorous A and B.
[0044] FIG. 4 shows the acetic acid gas concentration inside the film storage can, determined by HPLC measurements of eight films: undegraded A to C, odorless A to C, and odorous A and B. FIG. 4 confirms that no acetic acid gas is released into the film storage can from undegraded A to C and odorless A films. On the other hand, it was shown that odorless B film released approximately 14 ppm of acetic acid gas, odorless C film released approximately 28 ppm, and odorous A and B films released approximately 1300 to 1500 ppm of acetic acid gas. In this way, it is possible to quantitatively evaluate the acetic acid gas concentration of resin films during long-term storage in a storage can by HPLC measurement, and to grasp the state of deterioration.
[0045] Furthermore, in the film degradation diagnosis method according to the present invention, it is preferable to use the above-mentioned non-destructive analysis method, and then use one or a combination of two or more of the following analysis methods E to H, which are destructive analysis methods. Analysis method E: Check the moisture content in the film using a KF moisture meter Analysis method F: Confirming the thermal stability of the film by thermogravimetric-differential thermal (TG-DTA) analysis Analysis method G: Identifying the plasticizer species in the film by pyrolysis gas chromatography mass spectrometry Analysis method H: Check the mechanical strength of the film by tensile testing
[0046] In the film deterioration diagnosis method according to the present invention, the deterioration state of the resin film can be grasped more reliably by using at least one of the destructive analysis methods (Analysis Methods E to H) after using the non-destructive analysis methods (Analysis Methods A to D). Hereinafter, these Analysis Methods E to H will be described.
[0047] (E) Analysis method E Analysis method E is effective when the deterioration state of the resin film cannot be sufficiently confirmed by the above non-destructive analysis methods (Analysis methods A to D) because the moisture content in the film is confirmed by a KF moisture meter. The film deterioration diagnosis method using analysis method E will be described in detail below with reference to the embodiment.
[0048] In the analysis method E according to the present embodiment, a KF moisture meter AQ-2100 and a moisture vaporizer EV-5A manufactured by Hiranuma Sangyo Co., Ltd. were used as the devices. The measurement was carried out by placing the TAC film sample in a heating furnace maintained at 120°C, and quantifying the amount of moisture generated in 20 minutes by the KF method. As the TAC films used for the measurement in the analysis method E according to the present embodiment, eight films, namely undegraded A to C, odorless A to C, and odorous A and B, shown in the analysis method B according to the above embodiment, were used.
[0049] Figure 5 shows the results of measuring the moisture content of eight films: undegraded A to C, odorless A to C, and odorous A and B. The error bars in the figure indicate the standard error of the KF moisture measurement results. Figure 5 shows that the moisture content in the film tends to increase as the degradation of the TAC film progresses. It is thought that leaving the TAC film in the air for a long period of time causes moisture to adhere to the base of the TAC film or to be absorbed into the image-quality layer of the film. This is thought to be why the moisture content of undegraded A to C films is low. In addition, since the hydrolysis of TAC progresses at an accelerated rate once it begins, it is thought that odorous A and B films tend to absorb more moisture than odorless A to C films.
[0050] It is known that as resin films deteriorate, their moisture content tends to increase. Therefore, when the moisture content exceeds a certain value, it suggests that the relative humidity of the film storage environment is high, making it more likely that hydrolysis will occur in the future. According to the results shown in Figure 5, a moisture content of 5.5 wt% in the film can be used as one of the standards for film deterioration indicators.
[0051] (F) Analysis method F Analysis method F is effective when the deterioration state of the resin film cannot be sufficiently confirmed by the above non-destructive analysis methods (Analysis methods A to D) because the thermal stability of the film is confirmed by TG-DTA analysis. The film deterioration diagnosis method using analysis method F will be described in detail below with reference to the embodiment.
[0052] In the analysis method F according to the present embodiment, a differential thermobalance Thermo plus EVO2 manufactured by Rigaku Corporation was used as the apparatus. The measurement conditions were as follows: under N2 gas atmosphere, flow rate 100mL / min, heating rate 20℃ / min, measurement temperature range 25 to 450℃, reference α-alumina powder manufactured by Rigaku Corporation, sample pan Al, data acquisition interval 1.0s. After placing the TAC film and the reference in the sample chamber, N2 gas was allowed to flow for about 15 minutes, and the measurement was started after confirming that the mass had reached a steady state. As the TAC films used for the measurement in the analysis method F according to the present embodiment, eight films, namely undegraded A to C, odorless A to C, and odorous A and B, shown in the analysis method B according to the above embodiment, were used.
[0053] Figure 6 shows the TG curve measurement results for three films: undegraded A, odorless A, and odorous A. Figure 6 shows that as the degradation of the TAC film progresses, mass loss tends to begin to occur at lower temperatures. Here, the TG curve was differentiated with respect to time, and the temperature at which the slope of the tangent to the TG curve was the largest was taken as the thermal decomposition peak temperature, and these were compared for each film.
[0054] Figure 7 shows the peak thermal decomposition temperatures of TAC films obtained from the TG curves for eight films: undegraded A-C, odorless A-C, and odorous A and B. Figure 7 shows a tendency for the peak thermal decomposition temperature to decrease as the degradation of the TAC film progresses. It can also be seen that the peak thermal decomposition temperatures of odorless A-C films are approximately 5°C lower than those of undegraded A-C films. This is thought to be due to main chain scission of the TAC occurring as it deteriorates over time, resulting in a decrease in the degree of polymerization.
[0055] From the above, in the case of TAC film, when the thermal decomposition peak temperature falls below a certain value, the degree of polymerization decreases due to the cleavage of the main chain in the resin structure, suggesting the progression of oxidation reactions and plasticizer elution. In this way, by focusing on the thermal decomposition peak temperature, it is possible to quantitatively determine the deterioration state of a resin film. The thermal decomposition peak temperature does not require drawing a baseline, etc., and can be easily calculated using software, so it can be said to be an index with little reading error.
[0056] (G) Analysis method G Analysis method G is effective when the deterioration state of the resin film cannot be sufficiently confirmed by the above non-destructive analysis methods (analysis methods A to D) because the type of plasticizer in the film is confirmed by Py-GC / MS analysis. The film deterioration diagnosis method using analysis method G will be described in detail below with reference to the embodiment.
[0057] In the analysis method G according to the present embodiment, a GC-MS system 7890B / 5977B manufactured by Agilent Technologies, Inc. and a multi-shot pyrolyzer EGA / PY-3030D manufactured by Frontier Labs, Inc. were used as the apparatus. In addition, a UA + -5, or ZB-MultiResidue-1 or ZB-×LB-HT Inferno manufactured by Phenomenex were used. The TAC film was analyzed using these devices and columns. The GC conditions were as follows: inlet temperature 300°C, carrier gas He, column flow rate 1.2mL / min (constant flow mode), split ratio 50:1, furnace temperature 550°C, ITF temperature 300°C, oven temperature 40°C (2min)-20°C / min-300°C (5min). The MS conditions were as follows: ionization method electron ionization (70eV), ion source temperature 250°C, quadrupole temperature 150°C, interface temperature 250°C, scan range m / z 29-400 (sampling 3), gain 1. As the TAC films used for measurement in the analysis method G of this embodiment, eight films were used: undegraded A to C, odorless A to C, and odorous A and B, as shown in the analysis method B of the above embodiment.
[0058] Figure 8 shows the results of Py-GC / MS measurement for each film, undegraded A, Figure 9 shows the results of undegraded B, and Figure 10 shows the results of Py-GC / MS measurement for each film, unscented A, unscented B, unscented C, and unscented C. Figure 11 shows the results of Py-GC / MS measurement for each film, unscented A, unscented B, unscented C, unscented A, and unscented B. Figures 8 to 15 show triphenyl phosphate was detected in all films. Ethyl phthalyl ethyl glycolate was detected in the unscented A to C films, but was not detected in the unscented A to C films and the odorous A and B films. Phthalic anhydride was detected in the odorous A and B films. This is thought to be the result of the decomposition of ethyl phthalyl ethyl glycolate that was originally contained in the films as they deteriorated. These results suggest that the presence or absence of ethyl phthalyl ethyl glycolate may be involved in the progression of deterioration.
[0059] From the above, the result of the analysis method G according to the present embodiment shows that ethyl phthalyl ethyl glycolate is contained as a plasticizer in the TAC film, and it is suggested that this content may be related to the deterioration of the film. In this way, Py-GC / MS is positioned as a method for qualitatively analyzing whether the plasticizer in the resin film has volatilized or decomposed, and judging whether deterioration is progressing, and is effective in evaluating the presence or absence of precipitates derived from the plasticizer and whether the plasticizer necessary for deterioration countermeasures is contained.
[0060] (H) Analysis Method H Analysis method H is effective when the deterioration state of the resin film cannot be sufficiently confirmed by the above non-destructive analysis methods (Analysis methods A to D) because the mechanical strength of the film is confirmed by a tensile test. Hereinafter, the film deterioration diagnosis method using analysis method H will be described in detail based on the embodiment.
[0061] In the analysis method H according to the present embodiment, a bench-top precision universal testing machine Autograph AGS-X manufactured by Shimadzu Corporation and an SD type lever type sample cutter SDL-100 manufactured by Dumbbell Corporation were used as the equipment. The measurement conditions were a load cell of 1 kN, a test speed of 10 mm / min, and a gripper distance of 20 mm. The film sample was a TAC film cut into a JIS K6251 dumbbell shape No. 7, and the stress (breaking force) at the moment of breakage was measured. As the TAC film used for measurement in the analysis method H according to the present embodiment, eight films, namely undegraded A to C, odorless A to C, and odorous A and B, shown in the analysis method B according to the above embodiment, were used.
[0062] FIG. 16 shows the stress values at the time of film breakage obtained from tensile tests on eight films, undegraded A to C, odorless A to C, and odorous A and B. The error bars in the figure show the standard error of the stress values at the time of film breakage. FIG. 16 shows a tendency for the breaking strength to be smaller as hydrolysis progresses in the TAC film. Furthermore, compared to undegraded A to C and odorless A films, odorless B and C films had smaller breaking strengths. Possible causes of this include a decrease in the plasticizer content and a decrease in molecular weight due to cleavage of the TAC main chain, suggesting that such degradation other than hydrolysis occurs in the aged TAC film.
[0063] It is generally known that the mechanical strength of a polymer decreases as it deteriorates. Therefore, according to the results shown in FIG. 16, the breaking strength is 120 N / mm 2 The following can be used as one of the standards for the deterioration index of TAC film. In this way, by conducting a tensile test in addition to the chemical analysis method, it is possible to evaluate the deterioration state of the resin film from the viewpoint of physical strength.
[0064] In the film deterioration diagnosis method according to the present invention, the resin film is preferably a TAC film. TAC film has high flame resistance and can be stored for a long time, so it can be suitably used as a film for archiving. In addition, the deterioration state of the TAC film can be efficiently and reliably grasped by the film deterioration diagnosis method according to the present invention, so that the safety and reliability of the TAC film as a film for archiving can be significantly improved compared to other resin films.
[0065] The above describes an embodiment of the film deterioration diagnosis method of the present invention. The film deterioration diagnosis method of the present invention can improve the accuracy of determining the deterioration of a resin film compared to the conventional method by combining multiple types of analysis results and making a complementary judgment.
[0066] FIG. 17 is a chart showing an outline of the film deterioration diagnosis method according to the present embodiment. In the film deterioration diagnosis method according to the present invention, information obtained for each analysis item is fixed, and the deterioration state is judged based on whether the analysis result exceeds (or falls below) a certain threshold. Therefore, the film deterioration diagnosis method according to the present invention can perform deterioration diagnosis comprehensively and with high accuracy by performing a plurality of analysis methods in stages. Also, although the analysis procedure shown in FIG. 17 is in the order of the above-mentioned analysis methods A to H, the film deterioration diagnosis method according to the present invention does not necessarily have to perform the same procedure, and it is not necessarily required to perform all the analysis methods. Therefore, the film deterioration diagnosis method according to the present invention can perform deterioration diagnosis efficiently. [Industrial Applicability]
[0067] According to the present invention, the deterioration state of the resin film can be grasped more efficiently and reliably than in the past. Therefore, measures against deterioration of the resin film can be taken quickly, and valuable historical materials, documents, etc. recorded on the film can be prevented from being lost.
Claims
1. A method for diagnosing deterioration of a cellulose triacetate film, comprising the steps of: Analysis method B: The cellulose triacetate film is examined by Fourier transform infrared spectroscopy to confirm the presence or absence of acid anhydride and any signs of hydrolysis reaction.
2. The method for diagnosing deterioration of a cellulose triacetate film according to claim 1, further comprising, after using the non-destructive analytical method, using one or a combination of two or more of the following analytical methods E to H, which are destructive analytical methods. Analysis Method E: The moisture content in the cellulose triacetate film is determined using a Karl Fischer moisture meter. Analysis Method F: The thermal stability of the cellulose triacetate film is confirmed by thermogravimetric differential thermal analysis. Analysis Method G: The type of plasticizer in the cellulose triacetate film is identified by pyrolysis gas chromatography mass spectrometry. Analytical Method H: The mechanical strength of the cellulose triacetate film is confirmed by a tensile test.
Citation Information
Patent Citations
Analysis of uncured epoxy resin composition
JP1985117151A
Resin laminate inspecting method, and manufacturing method including the inspecting method
JP2002311019A
Dielectric deterioration diagnosing method of electric device
JP2005308424A
Rheological properties measuring device and process for forming micro pattern in color filter using the same
KR1020160115060A
Methods of measuring the extent of cure of a binder in fibrous products
US20050287675A1
Cited By