Power storage device and manufacturing method of the power storage device
By laminating and heat-treating the separator sheet in the winding process, the method addresses springback issues in secondary battery manufacturing, enhancing assembly stability and reducing terminal stress.
Patent Information
- Application Number
- JP2023076056
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-02
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2043-05-02
AI Technical Summary
Existing methods for manufacturing secondary batteries with wound electrode bodies fail to adequately suppress springback, leading to increased stress on electrode current collector terminals during assembly.
A manufacturing method involving laminating positive and negative electrode sheets with a separator sheet, followed by winding and heat-treating the separator sheet at the winding end region to thermally denature and harden it, thereby suppressing springback in the wound electrode body.
The method effectively reduces springback in the wound electrode body, ensuring stable assembly and reducing stress on electrode terminals.
Smart Images

Figure 2024160753000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an electricity storage device and a method for manufacturing the electricity storage device. [Background technology]
[0002] For example, the following Patent Document 1 discloses a method for manufacturing a secondary battery equipped with a wound electrode body, which includes a step of fabricating a wound electrode body by placing a separator sheet on which a heat-resistant layer is formed between positive and negative electrode sheets and winding them. It is described that the method for manufacturing a secondary battery suppresses loosening of the wound electrode body (hereinafter, also referred to as "springback"). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2014-137985 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, according to the study by the present inventor, it was found that there is still room for improvement in the manufacturing method of the secondary battery as described above from the viewpoint of suppressing the springback of the wound electrode body. In addition, it was found that a wound electrode body in which the springback occurs as described above is likely to be subjected to a load at the joint between the wound electrode body and the sealing plate (for example, an electrode current collector terminal between the wound electrode body and the sealing plate) when inserted into a battery case. In other words, there is a demand for further development of a technology that can obtain an electricity storage device including a wound electrode body in which springback is suitably suppressed.
[0005] The present disclosure has been made in consideration of the above circumstances, and its main objective is to provide a technique that can obtain an electricity storage device including a wound electrode body in which springback is suitably suppressed. [Means for solving the problem]
[0006] In order to achieve this object, the present disclosure provides a method for manufacturing an electricity storage device in which a positive electrode sheet and a negative electrode sheet are stacked and wound with a separator sheet interposed therebetween. The method for manufacturing such an electricity storage device preferably includes a preparation step of preparing the positive electrode sheet, the negative electrode sheet, and the separator sheet. The method for manufacturing such an electricity storage device preferably includes a winding step of winding the positive electrode sheet and the negative electrode sheet with the separator sheet interposed therebetween to prepare a wound body. The method for manufacturing such an electricity storage device preferably includes a winding step of heat-treating the separator sheet present in the winding end region of the wound body and winding it around the wound body. Although details will be described later, according to the method for manufacturing an electricity storage device having such a configuration, it is possible to obtain an electricity storage device including a wound electrode body in which springback is suitably suppressed.
[0007] From another aspect, the present disclosure provides an electricity storage device obtained by any one of the manufacturing methods for an electricity storage device disclosed herein. The electricity storage device is an electricity storage device including a wound electrode body in which a positive electrode sheet and a negative electrode sheet are stacked with a separator sheet interposed therebetween and wound, in which, when the porosity of the separator sheet present in the end winding region of the wound electrode body is P and the porosity of the separator sheet present in a region other than the end winding region of the wound electrode body is Q, the ratio of P to Q (P / Q) is smaller than 1. Since the electricity storage device is an electricity storage device obtained by any one of the manufacturing methods for an electricity storage device disclosed herein, it can be said that the electricity storage device includes a wound electrode body in which springback is suitably suppressed. [Brief description of the drawings]
[0008] [Figure 1] 2 is a flowchart showing each step of a battery manufacturing method according to one embodiment. [Diagram 2]1 is a schematic diagram showing a configuration of a wound electrode manufacturing apparatus according to one embodiment. FIG. [Diagram 3] 1A to 1C are schematic diagrams for explaining the production of a roll according to an embodiment. [Figure 4] 5A to 5C are schematic diagrams for explaining adjustment of the position of a separator sheet according to one embodiment. [Diagram 5] 5A to 5C are schematic diagrams for explaining adjustment of the position of a separator sheet according to one embodiment. [Figure 6] 5A to 5C are schematic diagrams for explaining cutting of a separator sheet according to one embodiment. [Figure 7] 5A and 5B are schematic diagrams for explaining a heat treatment of a separator sheet present in a winding end region of a winding body according to an embodiment. [Figure 8] FIG. 2 is a schematic diagram for explaining application of a tape to a roll according to one embodiment. [Figure 9] FIG. 2 is a schematic diagram showing a configuration of a winding body according to an embodiment. [Figure 10] FIG. 2 is a schematic diagram illustrating a state of a wound body before pressing according to an embodiment. [Figure 11] FIG. 2 is a schematic diagram showing an aspect of a rolled body after pressing according to an embodiment. [Figure 12] FIG. 1 is a front view showing a schematic internal structure of a battery according to an embodiment. [Figure 13] FIG. 2 is a perspective view showing a schematic diagram of a wound electrode body according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Hereinafter, some embodiments of the technology disclosed herein will be described with reference to the drawings. In the following drawings, the same reference numerals are used to describe members and parts that perform the same function. In addition, the dimensional relationships (length, width, thickness, etc.) in each drawing do not reflect the actual dimensional relationships. In addition, matters other than those specifically mentioned in this specification and necessary for implementing the technology disclosed herein (for example, the general configuration and manufacturing process of an electricity storage device that does not characterize this disclosure) can be understood as design matters of a person skilled in the art based on the conventional technology in the field. The technology disclosed herein can be implemented based on the contents disclosed in this specification and the technical common sense in the field. In addition, the following description is not intended to limit the present disclosure to the following forms. In addition, the manufacturing method of the battery disclosed herein may further include other steps at any stage, and if the steps are not described as essential, they can be appropriately deleted. In addition, the order of the steps can be changed as long as the effect of the technology disclosed herein is exerted.
[0010] In this specification, the expression "A to B" indicating a range means "A or more and B or less". It also includes the meanings of "greater than A" and "less than B". In this specification, the term "electricity storage device" refers to a device that can perform charging and discharging. The electricity storage device includes batteries such as primary batteries and secondary batteries (for example, non-aqueous electrolyte secondary batteries such as lithium ion secondary batteries, nickel-metal hydride batteries), and capacitors (physical batteries) such as electric double layer capacitors. The electrolyte may be any of a liquid electrolyte (electrolytic solution), a gel electrolyte, and a solid electrolyte. Hereinafter, a lithium ion secondary battery (hereinafter simply referred to as "battery 100"), which is one embodiment of the electricity storage device disclosed herein, will be described as an example.
[0011] <Battery manufacturing method> First, the manufacturing method of the battery according to the present embodiment will be described with reference to the wound electrode body manufacturing apparatus 200. Before describing the manufacturing method of the battery according to the present embodiment, the wound electrode body manufacturing apparatus 200 will be described. Here, FIG. 1 is a flowchart showing each step of the manufacturing method of the battery according to one embodiment. FIG. 2 is a schematic diagram showing the configuration of the wound electrode body manufacturing apparatus according to one embodiment. FIG. 3 is a schematic diagram for explaining the production of the wound body according to one embodiment. FIG. 4 and FIG. 5 are schematic diagrams for explaining the adjustment of the position of the separator sheet according to one embodiment. FIG. 6 is a schematic diagram for explaining the cutting of the separator sheet according to one embodiment. FIG. 7 is a schematic diagram for explaining the heat treatment of the separator sheet present in the winding end region of the wound body according to one embodiment. FIG. 8 is a schematic diagram for explaining the application of tape to the wound body according to one embodiment. FIG. 9 is a schematic diagram showing the configuration of the wound body according to one embodiment. Note that in FIG. 7 and FIG. 8, only the first winding core 204 is shown for ease of explanation. Hereinafter, each component of the wound electrode body manufacturing apparatus 200 according to the present embodiment will be described.
[0012] The first winding core 204 shown in FIG. 2 is a member that winds up the positive electrode sheet 50 and the negative electrode sheet 60 via the separator sheet 70. The first winding core 204 has a function of holding each sheet that is wound around the side circumferential surface. As shown in FIG. 2, in this embodiment, in addition to the first winding core 204, a second winding core 206 and a third winding core 208 are provided. Here, the third winding core 208 is a member that operates when adjusting the position of the separator sheet 70 described later. The first winding core 204, the second winding core 206, and the third winding core 208 are present in the index 202. Note that the first winding core 204, the second winding core 206, and the third winding core 208 are two semicircular members here, and have a structure divided into two, but the shape of these winding cores may be cylindrical, and when winding into a flat shape, a flat winding core may be used.
[0013] Adjustment roller 210 shown in Fig. 5 is a roller that adjusts the position of separator sheet 70 to an appropriate position when cutting separator sheet 70, which will be described later. Cutter 212 shown in Fig. 6 is a cutter that cuts separator sheet 70 to a desired length. Chuck 214 shown in Fig. 6 is a member for holding separator sheet 70. Chuck 214 is, for example, an electrostatic chuck.
[0014] 7 is a member for heat-treating the surface of the separator sheet 70A present in the winding end region of the roll 20A. Examples of the heat applicator 216 include a dryer, an infrared heater (IR heater), and an electromagnetic induction heater (IH heater). Commercially available products can be used without any particular restrictions.
[0015] 8 is a member that applies a stop tape to the winding end of the separator sheet 70 of the winding body 20A. As such a tape, any stop tape used for this type of winding body can be used without any particular restriction.
[0016] Each component of the wound electrode manufacturing apparatus 200 preferably has a required actuator as appropriate. The control device is configured to control each component of the wound electrode manufacturing apparatus 200 so that required operations are performed at predetermined timings according to a preset program. The control device can be embodied by a computer such as a microcontroller, for example.
[0017] Next, the manufacturing method of the battery according to this embodiment will be described with reference to the wound electrode body manufacturing apparatus 200. As shown in FIG. 1, first, the manufacturing method of the battery according to this embodiment is a manufacturing method of a battery 100 including a wound electrode body 20 in which a positive electrode sheet 50 and a negative electrode sheet 60 are stacked and wound with a separator sheet 70 interposed therebetween. The manufacturing method of the battery includes a preparation step (step S1) of preparing a positive electrode sheet 50, a negative electrode sheet 60, and a separator sheet 70. The manufacturing method of the battery includes a winding step (step S2) of winding the positive electrode sheet 50 and the negative electrode sheet 60 with the separator sheet 70 interposed therebetween to prepare a wound body 20A. The manufacturing method of the battery includes a winding step (step S3) of heat-treating the separator sheet 70 present in the winding end region of the wound body 20A and winding it around the wound body 20A. In this embodiment, after the winding step, a pressing step (step S4) is further included in which the rolled body 20A is pressed to form a flat shape.
[0018] As described above, in the manufacturing method of the wound electrode body, in the winding step (step S3), the separator sheet 70A present in the winding end region of the wound body 20A is heat-treated and wound around the wound body 20A. This heat treatment can thermally modify and harden the separator sheet 70A present in the winding end region of the wound body 20A. By winding the hardened separator sheet 70A around the wound body 20A, the wound body 20A can be fastened. This fastening allows a load to be continuously applied to the wound body 20A (wound electrode body 20), so springback of the wound electrode body 20 can be suitably suppressed. Each step will be described below.
[0019] The "winding end region" may be, for example, a region within 5 revolutions, 4 revolutions, 3 revolutions, 2 revolutions, or 1 revolution from the outermost circumference (corresponding to the region P1-P2 in FIG. 9) of the turns (turns) of the sheet constituting the winding body. Alternatively, the "winding end region" may be only the outermost circumference of the turns (turns) of the sheet constituting the winding body, or may be a region within 1 / 2 revolution of the outermost circumference. For example, in this embodiment, the winding end region is only the outermost circumference (i.e., the region P1-P2 in FIG. 9), and the separator sheet 70 present only in the outermost circumference is stretched in the winding process described later. In addition, from the viewpoint of making it easier to perform heat treatment in the winding process described later, it is preferable that the winding end region of the winding body 20A does not include the positive electrode sheet 50 and the negative electrode sheet 60, and is composed of only two separator sheets 70, as in this embodiment. However, the technology disclosed here is not limited to the above description. The "winding end region" of a wound electrode body, which will be described later, can be defined in the same manner. That is, the "wound body" in the above description can be read as the "wound electrode body".
[0020] (Preparation process: Step S1) In this step, there are prepared a positive electrode sheet 50, a negative electrode sheet 60, and a separator sheet 70. In this embodiment, two separator sheets 70 are prepared. Each member will be described below.
[0021] A known positive electrode current collector foil used in lithium ion secondary batteries may be used as the positive electrode current collector foil 52 constituting the positive electrode sheet 50, and examples of such a foil include aluminum foil, aluminum alloy foil, etc. The thickness of the positive electrode current collector foil 52 is not particularly limited and is, for example, 3 μm to 35 μm, and preferably 5 μm to 20 μm.
[0022] The positive electrode active material layer 54 contains a positive electrode active material. As the positive electrode active material, a known positive electrode active material used in a lithium ion secondary battery may be used. Specifically, for example, as the positive electrode active material, a lithium composite oxide, a lithium transition metal phosphate compound, or the like may be used. The crystal structure of the positive electrode active material is not particularly limited, and may be a layered structure, a spinel structure, an olivine structure, or the like. Examples of the lithium composite oxide include a lithium nickel composite oxide, a lithium cobalt composite oxide, a lithium manganese composite oxide, a lithium nickel manganese composite oxide, a lithium nickel cobalt manganese composite oxide, a lithium nickel cobalt aluminum composite oxide, and a lithium iron nickel manganese composite oxide. These positive electrode active materials may be used alone or in combination of two or more. The positive electrode active material is preferably a lithium nickel cobalt manganese composite oxide.
[0023] The average particle diameter (median diameter: D50) of the positive electrode active material is not particularly limited, but is, for example, 0.05 μm to 25 μm, preferably 1 μm to 20 μm, and more preferably 3 μm to 15 μm. The average particle diameter (D50) of the positive electrode active material can be determined, for example, by a laser diffraction scattering method.
[0024] The content of the positive electrode active material in the positive electrode active material layer 54 (i.e., the content of the positive electrode active material relative to the total mass of the positive electrode active material layer 54) is not particularly limited, but is, for example, 80 mass % or more, preferably 85 mass % or more, and more preferably 90 mass % or more.
[0025] The positive electrode active material layer 54 may contain a component (i.e., an optional component) other than the positive electrode active material. Examples of the optional component include a conductive material, a binder, and the like. As the conductive material, for example, a carbon material such as carbon black (e.g., acetylene black), carbon nanotubes (CNT), graphite, and the like may be suitably used. As the binder, for example, polyvinylidene fluoride (PVDF) and the like may be used. When CNT is used as the conductive material, the positive electrode active material layer 54 may further contain a dispersant for CNT.
[0026] The content of the conductive material in the positive electrode active material layer 54 is not particularly limited, but is preferably 0.1% by mass to 15% by mass, and more preferably 0.5% by mass to 13% by mass. The content of the binder in the positive electrode active material layer 54 is not particularly limited, but is preferably 1% by mass to 15% by mass, and more preferably 1.5% by mass to 10% by mass. The thickness of the positive electrode active material layer 54 is not particularly limited, but is, for example, 10 μm to 300 μm, and preferably 20 μm to 200 μm. The positive electrode sheet 50 may contain an insulating layer (not shown) at the boundary between the positive electrode active material layer non-forming portion 52a and the positive electrode active material layer 54. The insulating layer contains, for example, ceramic particles.
[0027] A known negative electrode current collector foil used in lithium ion secondary batteries may be used as the negative electrode current collector foil 62 constituting the negative electrode sheet 60, and an example of such a foil is copper foil. The thickness of the negative electrode current collector foil 62 is not particularly limited and is, for example, 3 μm to 35 μm, and preferably 5 μm to 20 μm.
[0028] The negative electrode active material layer 64 contains a negative electrode active material. As the negative electrode active material, for example, a carbon material such as graphite, hard carbon, soft carbon, etc. The graphite may be natural graphite or artificial graphite, or may be amorphous carbon-coated graphite in which graphite is coated with an amorphous carbon material.
[0029] The average particle diameter (median diameter: D50) of the negative electrode active material is not particularly limited, but is, for example, 0.1 μm to 50 μm, preferably 1 μm to 25 μm, and more preferably 5 μm to 20 μm. The average particle diameter (D50) of the negative electrode active material can be determined, for example, by a laser diffraction scattering method.
[0030] The negative electrode active material layer 64 may contain components other than the active material, such as a binder and a thickener. As the binder, for example, styrene butadiene rubber (SBR), polyvinylidene fluoride (PVDF), etc. may be used. As the thickener, for example, carboxymethyl cellulose (CMC), etc. may be used. The content of the negative electrode active material in the negative electrode active material layer 64 is preferably 90 mass% or more, more preferably 95 mass% to 99 mass%. The content of the binder in the negative electrode active material layer 64 is preferably 0.1 mass% to 8 mass%, more preferably 0.5 mass% to 3 mass%. The content of the thickener in the negative electrode active material layer 64 is preferably 0.3 mass% to 3 mass%, more preferably 0.5 mass% to 2 mass%. The thickness of the negative electrode active material layer 64 is not particularly limited, but is, for example, 10 μm to 300 μm, and preferably 20 μm to 200 μm.
[0031] Examples of the separator sheet 70 include porous sheets (films) made of resins such as polyethylene (PE), polypropylene (PP), polyester, cellulose, and polyamide. Among these, from the viewpoint of suitably carrying out the above-mentioned heat treatment (for example, thermal modification and hardening), separator sheets made of polyolefin resins such as PE and PP can be preferably used. Moreover, such a porous sheet may have a single-layer structure or a laminated structure of two or more layers (for example, a three-layer structure in which PP layers are laminated on both sides of a PE layer). A heat-resistant layer (HRL) may be provided on the surface of the separator sheet 70.
[0032] The thickness of the separator sheet 70 is not particularly limited, but is, for example, 5 μm to 50 μm, and preferably 10 μm to 30 μm. In this embodiment, the wound electrode body 20 includes two separator sheets 70. The porosity of the separator sheet 70 is generally 20 to 60%, and may be, for example, 30 to 50%. Here, as the "porosity", for example, a value calculated from the amount of pores measured using mercury intrusion porosimetry can be adopted (porosities measured in a similar manner can also be adopted for the porosities A, B, P, and Q described later). The porosity can be measured, for example, using a commercially available mercury intrusion porosimeter. The porosity can be measured according to the method described in the catalog. The air permeability of the separator sheet 70 is, for example, 30sec / 100cc to 500sec / 100cc, and may be 30sec / 100cc to 300sec / 100cc or 50sec / 100cc to 200sec / 100cc. In this embodiment, the two separators have the same configuration, but in other embodiments, they may have different configurations. In other embodiments, the separator sheet 70 may be one sheet. As in this embodiment, it is preferable to prepare a separator sheet 70 that is longer than the positive electrode sheet 50 and the negative electrode sheet 60 so that the separator sheet 70 is present in the winding end region of the winding body 20A.
[0033] (Winding process: step S2) In this step, the positive electrode sheet 50 and the negative electrode sheet 60 are wound with the separator sheet 70 interposed therebetween to prepare the wound body 20A. In this embodiment, as shown in FIG. 9, the wound body 20A is prepared so that only the separator sheet 70 is present in the winding end region. Specifically, first, as shown in FIG. 3, the positive electrode sheet 50, the negative electrode sheet 60, and the separator sheet 70 are wound around the first winding core 204. At this time, the third winding core is moved to the back so as not to interfere with the position adjustment of the separator sheet 70. Next, as shown in FIG. 3 and FIG. 4, the index 202 is rotated 120° in the direction of the arrow S. Next, as shown in FIG. 5, the third winding core 208 is rotated by an angle so that the separator sheet 70 can be sandwiched. In addition, the position of the separator sheet 70 is adjusted by the adjustment roller 210 so that the third winding core 208 can sandwich the separator sheet 70. Then, the third winding core 208 is advanced onto the surface of the index 202. Next, as shown in Fig. 6, the separator sheet 70 is cut to a desired length by a cutter 212. At this time, it is preferable that the separator sheet 70 on both sides of the cutter 212 is held down by a chuck 214.
[0034] Here, the number of windings (number of turns) of the wound body 20A (or the wound electrode body 20 described later) is not particularly limited, but may be, for example, 10 or more, 20 or more, 30 or more, or 40 or more. The upper limit of the number of windings is, for example, 60 or less, and may be 50 or less.
[0035] (Winding process: step S3) In this step, the separator sheet 70A present in the winding end region of the winding body 20A (i.e., the region P1 to P2 in FIG. 9) is wound around the winding body 20A in a heat-treated state. Specifically, first, as shown in FIG. 7, the surface of the separator sheet 70 present in the winding end region of the winding body 20A is heat-treated (heated) by the heat application device 216. The temperature of the heat treatment is preferably changed appropriately depending on the type of resin constituting the separator sheet 70, but can be about 50°C to 150°C (for example, 60°C to 130°C). The time of the heat treatment is preferably changed appropriately depending on the type of resin constituting the separator sheet 70, but can be about 0.3 seconds to 1 hour (for example, 0.5 seconds to 30 minutes). After the heat treatment, the separator sheet 70 may be cooled to room temperature (for example, 20°C±5°C). Although not particularly limited, the heat treatment is preferably performed until the porosity B of the surface of the separator sheet 70A present in the winding end region of the winding body 20A after the heat treatment becomes smaller than A, where A is the porosity of the surface of the separator sheet 70A present in the winding end region of the winding body 20A before the heat treatment. From the viewpoint of more effectively obtaining the above-mentioned effect of suppressing springback, the heat treatment is preferably performed until the porosity B becomes 0.8A or less, more preferably until the porosity B becomes 0.5A or less, and even more preferably until the porosity B becomes 0.2A or less or 0.1A or less (for example, it may be 0). The above B can be within a range of 0 to 0.1A, for example.
[0036] In the present embodiment, only one side of the separator sheet 70A is heat-treated, but in other embodiments, both sides of the separator sheet 70A may be heat-treated. In the present embodiment, the surfaces of both of the two separator sheets 70 are heat-treated, but in other embodiments, only the surface of one separator sheet 70 may be heat-treated. By this heat treatment, the separator sheet 70A present in the winding end region of the wound body 20A can be thermally denatured and hardened. Then, the hardened separator sheet 70A after the heat treatment is wound around the wound body 20A and the wound body 20A is fastened, so that a load can be continuously applied to the wound body 20A (wound electrode body 20), and the springback of the wound electrode body 20 can be suitably suppressed.
[0037] Next, as shown in FIG. 8, a take-up tape is applied to the take-up end of the wound body 20A produced as described above by a tape applying member.
[0038] (Press process: step S4) In this embodiment, the method further includes a pressing step of pressing the wound body 20A to form it into a flat shape after the winding step. Here, FIG. 10 is a schematic diagram showing a state of the wound body according to one embodiment before pressing. Also, FIG. 11 is a schematic diagram showing a state of the wound body according to one embodiment after pressing. The pressing step can be performed by pressing the wound body 20A produced as described above in the direction of the outline arrow by a press machine 300. Although not particularly limited, the pressing pressure can be, for example, 20N to 200kN (preferably, 50N to 120kN). The pressing can be a heated press or a non-heated press. By performing the pressing step, the springback of the produced wound electrode body 20 can be more suitably suppressed. In the above manner, the wound electrode body 20 can be produced.
[0039] As shown in Fig. 13, the wound electrode body 20 has a configuration in which a laminate in which a long positive electrode sheet 50 and a long negative electrode sheet 60 are laminated with two long separator sheets 70 interposed therebetween is wound in the longitudinal direction. The positive electrode sheet 50 has a configuration in which a positive electrode active material layer 54 is formed along the longitudinal direction on one or both sides (both sides here) of a long positive electrode current collector foil 52. The negative electrode sheet 60 has a configuration in which a negative electrode active material layer 64 is formed along the longitudinal direction on one or both sides (both sides here) of a long negative electrode current collector foil 62. The positive electrode active material layer-free portion 52a (i.e., a portion where the positive electrode active material layer 54 is not formed and the positive electrode current collector foil 52 is exposed) and the negative electrode active material layer-free portion 62a (i.e., a portion where the negative electrode active material layer 64 is not formed and the negative electrode current collector foil 62 is exposed) are formed so as to protrude outward from both ends in the winding axis direction (i.e., the width direction perpendicular to the longitudinal direction) of the wound electrode body 20. Also, in the center in the winding axis direction, there is a core portion 20a where the positive electrode active material layer 54 and the negative electrode active material layer 64 face each other. WL in FIG. 13 indicates the winding axis.
[0040] Next, the positive electrode current collector terminal 42a and the negative electrode current collector terminal 44a are attached to the positive electrode current collector foil laminated portion 52A and the negative electrode current collector foil laminated portion 62A in the wound electrode body 20 produced as described above by resistance welding, ultrasonic welding, or the like. It is assumed here that the positive electrode terminal 42, the negative electrode terminal 44, the positive electrode current collector terminal 42a, and the negative electrode current collector terminal 44a are attached to the lid body 34 of the battery case 30. In this way, the electrode body 20 is connected to the lid body 34 of the battery case 30. Then, the electrode body 20 is inserted into the case body 32 through the opening of the case body 32. Thereafter, the case body 32 and the lid body 34 are sealed by laser welding or the like.
[0041] Here, the battery case 30 is made of, for example, a metal (for example, aluminum, stainless steel, nickel-plated steel, etc.). The battery case 30 is preferably made of aluminum because it has good electrical conductivity, thermal conductivity, strength, and is lightweight. The case body 32 has a flattened rectangular parallelepiped shape, and one of its faces (the upper face in the figure) is an opening. The lid body 34 has a substantially rectangular shape that fits the shape of the opening. The lid body 34 is provided with a positive electrode terminal 42 and a negative electrode terminal 44 for external connection, and a thin-walled safety valve 36 that is set to release the internal pressure when the internal pressure of the battery case 30 rises to a predetermined level or higher. In addition, the lid body is provided with a liquid injection hole (not shown) for injecting the non-aqueous electrolyte 80. The positive electrode terminal 42 is electrically connected to the positive electrode collector terminal 42a. The negative electrode terminal 44 is electrically connected to the negative electrode collector terminal 44a. The positive electrode terminal 42 and the positive electrode collector terminal 42a are made of, for example, aluminum, an aluminum alloy, or the like. The negative electrode terminal 44 and the negative electrode current collector terminal 44a are made of, for example, copper or a copper alloy.
[0042] Next, the non-aqueous electrolyte 80 is prepared according to a known method. The non-aqueous electrolyte 80 typically contains a non-aqueous solvent and a supporting salt (electrolyte salt). As the non-aqueous solvent, various organic solvents such as carbonates, ethers, esters, nitriles, sulfones, and lactones that are used in the electrolyte of a general lithium ion secondary battery can be used without any particular limitation. Among them, carbonates and esters are preferable, and specific examples thereof include ethylene carbonate (EC), propylene carbonate (PC), diethyl carbonate (DEC), dimethyl carbonate (DMC), ethyl methyl carbonate (EMC), methyl acetate, and methyl propionate. Such non-aqueous solvents can be used alone or in appropriate combination of two or more.
[0043] As the supporting salt, for example, a lithium salt such as LiPF6, LiBF4, lithium bis(fluorosulfonyl)imide (LiFSI) (preferably LiPF6) can be suitably used. The concentration of the supporting salt is preferably 0.7 mol / L to 1.3 mol / L.
[0044] In addition, the non-aqueous electrolyte 80 may contain various additives other than the above-mentioned components, such as film-forming agents such as vinylene carbonate (VC) and oxalate complexes; gas generating agents such as biphenyl (BP) and cyclohexylbenzene (CHB); thickeners, etc., so long as the effects of the present disclosure are not significantly impaired.
[0045] Then, the non-aqueous electrolyte 80 is poured into the battery case 30 through the pouring hole in the lid 34 of the battery case 30, and the pouring hole is sealed. In this manner, the battery 100 can be obtained.
[0046] Next, a battery 100 obtained by the battery manufacturing method as described above will be described. Here, FIG. 12 is a front view showing a schematic internal structure of a battery according to one embodiment. FIG. 13 is a perspective view showing a schematic wound electrode body according to one embodiment. The hatched portion of the separator sheet 70A present in the winding end region of the wound electrode body 20 in FIG. 13 indicates a state in which the separator sheet 70A is thermally denatured and hardened by heat treatment. First, the battery 100 according to this embodiment is a battery including a wound electrode body 20 in which a positive electrode sheet 50 and a negative electrode sheet 60 are stacked with a separator sheet 70 interposed therebetween and wound. In addition, when the porosity of the separator sheet 70A present in the end winding region of the wound electrode body 20 is P and the porosity of the separator sheet 70 present in the other region of the wound electrode body 20 (in other words, the region of the separator sheet 70 present in the wound electrode body 20 other than the separator sheet 70A) is Q, the ratio of P to Q (P / Q) is smaller than 1. That is, the porosity of the separator sheet 70A heat-treated by the winding step (step S4) as described above is smaller than the porosity of the separator sheet 70 not heat-treated. Since the battery 100 is a battery obtained by any of the battery manufacturing methods disclosed herein, it can be said to be a battery equipped with a wound electrode body in which springback is suitably suppressed.
[0047] From the viewpoint of suitably suppressing springback of the wound electrode body 20, the ratio (P / Q) is preferably 0.8 or less, more preferably 0.5 or less, and even more preferably 0.2 or less or 0.1 or less (for example, it may be 0. In this case, P is 0). The ratio (P / Q) can be set within the range of 0 to 0.1, for example.
[0048] Moreover, the wound electrode body 20 preferably includes, as the separator sheet 70, a separator sheet made of a polyolefin resin.
[0049] The battery 100 can be used for various purposes. Specific applications include portable power sources for personal computers, portable electronic devices, portable terminals, etc.; power sources for driving vehicles such as electric vehicles (BEVs), hybrid vehicles (HEVs), and plug-in hybrid vehicles (PHEVs); and storage batteries for small power storage devices, among which a power source for driving vehicles is preferable. The battery 100 can also be used in the form of a battery pack, typically consisting of a plurality of batteries connected in series and / or parallel.
[0050] Although one embodiment of the present disclosure has been described above, the above embodiment is merely an example. The present disclosure can be implemented in various other forms. The present disclosure can be implemented based on the contents disclosed in this specification and the technical common sense in the field. The technology described in the claims includes various modifications and changes to the above-exemplified embodiments. For example, it is possible to replace a part of the above-mentioned embodiment with another modified form, and it is also possible to add another modified form to the above-mentioned embodiment. In addition, if the technical feature is not described as essential, it is also possible to delete it as appropriate.
[0051] For example, in the above embodiment, the shape of the wound electrode body 20 is flat, but is not limited to this. In other embodiments, the shape of the wound electrode body may be cylindrical or the like.
[0052] For example, in the above embodiment, the method for manufacturing the wound electrode body includes the pressing step (step S4), but is not limited to this. For example, when the wound electrode body is cylindrical, the pressing step can be omitted.
[0053] Although the embodiment of the present disclosure has been described above, the above embodiment is merely an example. The present disclosure can be implemented in various other forms. The present disclosure can be implemented based on the contents disclosed in this specification and the technical common sense in the relevant field. The technology described in the claims includes various modifications and changes of the above-exemplified embodiment. [Explanation of symbols]
[0054] 20 Wound electrode body 30 Battery case 32 Case body 34 Lid 36 Safety valve 42 Positive terminal 42a Positive collector terminal 44 Negative terminal 44a Negative current collector terminal 50 Positive electrode sheet (positive electrode) 52 Positive electrode current collector foil 52a Portion where positive electrode active material layer is not formed 52A Positive current collector foil laminate 54 Cathode active material layer 60 Negative electrode sheet (positive electrode) 62 Negative electrode current collector foil 62a Part where negative electrode active material layer is not formed 62A Negative electrode current collector foil laminate 64 Negative electrode active material layer 70 Separator sheet (separator) 80 Non-aqueous electrolytes 100 batteries 200 Wound electrode body manufacturing equipment 202 Index 204 First core 206 Second winding core 208 3rd core 210 Adjustment roller 212 Cutter 214 Chuck 216 Heat Applicator 218 Tape-attached parts 300 Press Machine
Claims
1. A method for producing an electricity storage device including a wound electrode body in which a positive electrode sheet and a negative electrode sheet are stacked with a separator sheet interposed therebetween and wound, the method comprising the steps of: a preparation step of preparing the positive electrode sheet, the negative electrode sheet, and the separator sheet; a winding step of winding the positive electrode sheet and the negative electrode sheet with the separator sheet interposed therebetween to prepare a wound body; and a winding step of heat-treating the separator sheet present in the winding end region of the winding body and winding the separator sheet around the winding body; A method for producing an electricity storage device comprising the steps of:
2. The method for producing an electricity storage device according to claim 1 , wherein in the preparing step, a separator sheet made of a polyolefin resin is prepared as the separator sheet.
3. The method for producing an electricity storage device according to claim 1 , further comprising, after the winding step, a pressing step of pressing the wound body to form it into a flat shape.
4. A power storage device including a wound electrode body in which a positive electrode sheet and a negative electrode sheet are stacked with a separator sheet interposed therebetween and wound, An electricity storage device, wherein, when the porosity of the separator sheet present in the end region of the wound electrode body is P and the porosity of the separator sheet present in the region other than the end region of the wound electrode body is Q, the ratio of P to Q (P / Q) is smaller than 1.
5. The electricity storage device according to claim 4 , wherein the separator sheet comprises a separator sheet made of a polyolefin resin.
6. The power storage device according to claim 4 , wherein the ratio (P / Q) is 0.1 or less.
Citation Information
Patent Citations
Enclosed cell
JP1989041176A
Method for manufacturing secondary battery
JP2016058381A
Secondary battery
JP2014137985A