Method of producing semi-carbonized piece and wood piece
By producing torrefied biomass fuel with controlled moisture and surface pyrolysis, the method addresses co-combustion stability issues with non-biomass fuels, enhancing handling and mixing properties.
Patent Information
- Application Number
- JP2023077481
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-09
- Publication Date
- 2024-11-21
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional biomass fuel torrefaction methods do not consider the co-combustion stability issues when mixed with non-biomass fuels like coal, as non-biomass fuels have higher specific gravity, leading to potential combustion disruptions.
A method to produce torrefied biomass fuel by heating wood pieces with a moisture content of 37% to 56% to 20% to 30% and pyrolyzing the surface, resulting in torrefied chips with improved hydrophobicity and reduced specific gravity, facilitating stable co-combustion with non-biomass fuels.
The method enables stable and easy handling of torrefied biomass fuel during co-combustion with non-biomass fuels, reducing the risk of combustion disruptions and improving mixing and stirring properties.
Smart Images

Figure 2024162178000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for producing torrefied pieces and wood pieces. [Background technology]
[0002] Conventionally, methods for producing biomass fuel by semi-carbonizing biomass have been proposed. For example, Patent Document 1 discloses an apparatus mainly consisting of a semi-carbonization device (semi-carbonization furnace) that pyrolyzes wood pellets in an oxygen-free or low-oxygen atmosphere at 200°C to 300°C. Patent Document 3 discloses that the semi-carbonization of this invention refers to a state in which biomass is heated and pressurized to a completely dehydrated and decomposed state, or a state before being carbonized and pyrolyzed, in which moisture that does not contribute to combustion is dehydrated, and cellulose and hemicellulose are modified and decomposed, but lignin is not modified. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 7108354 [Patent Document 2] JP 2019-45078 A [Patent Document 3] JP 2018-83876 A [Patent Document 4] JP 2021-127443 A Summary of the Invention [Problem to be solved by the invention]
[0004] Incidentally, an example of the use of biomass fuel is mixed combustion, in which biomass fuel is mixed with coal or other non-biomass fuel and burned. However, the above-mentioned conventional technology does not take into consideration the case of mixing biomass fuel with non-biomass fuel. In general, non-biomass fuels such as coal have a higher specific gravity than biomass fuels such as semi-carbonized chips. For this reason, when biomass fuel is mixed with non-biomass fuels such as coal, it is expected that the non-biomass fuel will be blown up by hot air in the combustion furnace, making it difficult to continue stable mixed combustion.
[0005] An object of the present invention is to provide a torrefied biomass fuel that is easy to handle when mixed with non-biomass fuels. [Means for solving the problem]
[0006] The disclosed embodiment can be exemplified by a method for producing torrefied pieces, which includes heating wood pieces having a moisture content of more than 37% to control the moisture content to 20% to 30% and pyrolyzing at least a portion of the surface. The disclosed embodiment can also be exemplified by wood pieces having a moisture content of 20% to 30% and at least a portion of the surface being pyrolyzed. Effect of the Invention
[0007] According to the present production method, it is possible to provide semi-carbonized biomass fuel that is easy to handle when mixed with non-biomass fuel. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is a diagram illustrating a configuration of a manufacturing facility according to an embodiment. [Diagram 2] FIG. 2 is an example of moisture content data. [Diagram 3] FIG. 3 is a diagram illustrating the change in weight over time when green wood chips and semi-carbonized chips are immersed in water. [Figure 4]FIG. 4 is a graph comparing the hydrophobicity measurement results of dry start and wet start for torrefied chips. [Diagram 5] FIG. 5 is a diagram illustrating the configuration of a control table illustrating the relationship between the type of green wood (tree) that becomes green wood chips, the heating temperature, and the heating time. [Figure 6] FIG. 6 is a diagram illustrating a manufacturing process performed by the control device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Hereinafter, the torrefied chips, the torrefied chip manufacturing apparatus, and the torrefied chip manufacturing method according to one embodiment of the present invention will be described with reference to the drawings. In one aspect, the torrefied chip manufacturing apparatus and the torrefied chip manufacturing method of this embodiment aim to manufacture torrefied chips that are easy to handle when mixed with non-biomass fuel. In addition, for example, a substance with a low specific gravity has a characteristic that it is difficult to mix with a substance with a high specific gravity even when stirred. Therefore, the torrefied chips of this embodiment also have an aspect of facilitating handling of the fuel stirring and mixing.
[0010] <Configuration and operation of manufacturing equipment> 1 is a diagram illustrating the configuration of a semi-carbonized chip manufacturing apparatus 1. The manufacturing apparatus 1 has a carbonization furnace 10, a control device 11, and a storage device 12. The semi-carbonized chips can be called semi-carbonized pieces.
[0011] The carbonization furnace 10 is fed with green wood chips C1, which are heated in the space within the furnace to produce semi-carbonized chips C2. Both the green wood chips C1 and the semi-carbonized chips C2 are produced by crushing or cutting wood, and can be considered as an example of wood pieces. The semi-carbonized chips C2 can be considered as an example of semi-carbonized chips. The green wood chips C1 can be considered as an example of wood pieces that have not been dried after felling. The semi-carbonized chips C2 can be considered as an example of wood pieces where at least a part of the surface has been thermally decomposed. That is, in this embodiment, the semi-carbonized chips are also included in the wood pieces.
[0012] There is no limitation on the heating method of the carbonization furnace 10. The carbonization furnace 10 heats the green wood chips C1 by heat transfer or radiation from a heat transfer surface in an inert atmosphere in which the green wood chips C1 are exposed to an inert gas with low oxygen content, such as nitrogen, carbon dioxide, or water vapor. The carbonization furnace 10 may also be a furnace that blows hot air such as a heated inert gas or water vapor onto the green wood chips C1 in the furnace. Furthermore, there is no limitation on the heating mechanism for performing such heating. For example, the heating mechanism may have an electric heater. The heating mechanism may also have a combustion furnace that burns fuel such as heavy oil, kerosene, city gas, propane gas, methane gas, natural gas, and dry distillation gas generated from biomass.
[0013] The control device 11 controls the heating in the carbonization furnace 10 or the temperature inside the carbonization furnace 10. The control device 11 measures the temperature inside the furnace from, for example, a temperature sensor inside the carbonization furnace 10. The temperature sensor is, for example, a thermocouple. The temperature sensor may also be a suction-type thermometer that measures by sucking in a portion of the high-temperature gas inside the furnace. The temperature sensor may also be made of a material such as ceramics whose shape or dimensions change depending on the temperature, or a material whose color changes depending on the temperature. Furthermore, the temperature sensor may be a thermograph that measures the surface temperature of the green wood chips C1 and the semi-carbonized chips C2 being processed in the carbonization furnace 10 through heat-resistant glass. In short, it is sufficient for the control device 11 to be able to measure the temperature inside the carbonization furnace 10, the green wood chips C1 being processed in the carbonization furnace 10, or the semi-carbonized chips C2 into which the green wood chips C1 have been semi-carbonized.
[0014] The control device 11 controls the temperature detected by the temperature sensor to the target value for a predetermined period of time. There is no limitation on the method of controlling the temperature. For example, if the carbonization furnace 10 has an electric heater, the control device 11 may perform feedback control by increasing or decreasing the power supplied to the electric heater so that the detected temperature approaches the target value. In addition, when the carbonization furnace 10 burns fuel, In the case where a combustion furnace is provided, the control device 11 may perform feedback control by adjusting the amount of fuel supplied to the combustion furnace so that the detected temperature approaches the target value.
[0015] The storage device 12 stores control parameters when the control device 11 controls the carbonization furnace 10. The storage device 12 may be configured separately from the control device 11 and may be configured to be capable of inputting and outputting data from the control device 11 via wired or wireless communication, for example. The storage device 12 may be configured integrally with the control device 11, or may be called a main storage device built into the control device 11. The control device 11 with the built-in storage device 12 may be called a microcontroller or microcomputer. However, the control device 11 may have a built-in main storage device, and the storage device 12 may be an external storage device other than the main storage device built into the control device 11.
[0016] The control parameters stored in the storage device 12 are, for example, a furnace temperature of 300 degrees, 350 degrees, 400 degrees, etc. Also, the control parameters are, for example, a heating time of 5 minutes, 10 minutes, 15 minutes, etc. In this embodiment, the control device 11 performs semi-carbonization processing by heating for a relatively short period of time, so the control parameters can also be said to be parameters of rapid heating conditions.
[0017] There is no limitation on the mechanism for feeding raw wood chips C1 as raw material into the carbonization furnace 10 and the mechanism for discharging semi-carbonized chips C2 produced in the carbonization furnace 10. The carbonization furnace 10 may be operated in a batch manner. That is, a predetermined amount of raw wood chips C1 as raw material may be fed into the carbonization furnace 10, the raw wood chips C1 may be heated under rapid heating conditions stored in the storage device 12, and the semi-carbonized chips C2 produced may be discharged after the heating is stopped. The raw wood chips C1 may be fed into the carbonization furnace 10, for example, from an opening and closing opening by a conveyor or the like. The carbonization furnace 10 may have a scraper or actuator that moves in a parallel manner in a predetermined direction in the carbonization furnace 10 and can scrape off the semi-carbonized chips C2. The semi-carbonized chips C2 produced may be scraped out from a discharge opening by a scraper or the like.
[0018] However, the carbonization furnace 10 may be operated continuously and may produce semi-carbonized chips C2 continuously or intermittently at a predetermined production speed. In the continuous operation, a predetermined amount of green wood chips C1 is fed into the carbonization furnace 10 at a predetermined time interval, for example, from an inlet that can be opened and closed by a conveyor or the like. The carbonization furnace 10 has a cylindrical container that is rotatably held, for example, tilted at a predetermined angle with respect to the horizontal plane. The cylindrical container is held such that the inlet is relatively high and the outlet is relatively low. The cylindrical container rotates while heating the green wood chips C1 as the raw material in the container, gradually moving the green wood chips C1 to the outlet, and after heating at the target heating temperature for a predetermined time, the semi-carbonized chips C2 may be discharged from the outlet. The semi-carbonized chips C2 may be scraped out from the outlet by an actuator or the like provided near the outlet. However, the carbonization furnace 10 may be a cylindrical container having an inlet on the vertical upper side and an outlet on the vertical lower side. The inlet and the outlet may be provided with, for example, butterfly valves. The butterfly valve at the inlet opens at predetermined time intervals to feed the green wood chips C1 into the carbonization furnace 10. The butterfly valve at the outlet opens at predetermined time intervals to discharge the semi-carbonized chips C2 from the outlet.
[0019] When the manufacturing apparatus 1 starts operating, the control device 11 reads out control parameters from the storage device 12 and controls the carbonization furnace 10. That is, the control device 11 controls the carbonization furnace 10 to burn at a target temperature, and also feeds raw wood chips C1, which are raw materials, into the carbonization furnace 10. After a predetermined processing time has elapsed, the control device 11 discharges the semi-carbonized chips C2 manufactured in the carbonization furnace 10 from the carbonization furnace 10.
[0020] <Moisture content of green wood chips C1> The green wood chips C1 are characterized by their moisture content. It is known that the moisture content can be almost completely determined by the type of living wood. For example, Figure 2 shows the moisture content data published in Nagano Prefectural Forestry General Center Mini Technical Information No. 50, May 2014 (https: / / www.pref.nagano.lg.jp / ringyosogo / joho / minigijutsu / documents / 50chipmc.pdf, accessed April 15, 2023).
[0021] The moisture content is calculated in two ways: dry moisture content and wet moisture content. The dry moisture content is defined as (weight before drying - weight after drying) / weight after drying. The wet moisture content is defined as (weight before drying - weight after drying) / weight before drying. Hereinafter, in this embodiment, the wet moisture content is used as the moisture content.
[0022] In the example of Figure 2, when looking at the wet basis moisture content, the lowest wet basis moisture content of the trunks or branches of standing trees is the tops or branches of oak, at 37.7%. Also, the highest wet basis moisture content is the trunks of cedar, at 56.0%. Therefore, generally speaking, the wet basis moisture content of green wood chips C1 can be considered to be in the range of 37% to 56%.
[0023] <Features of Semi-Carbonized Chip C2> The inventors heated the first group of green wood chips, which were a mixture of various wood materials, at a heating temperature of 350 degrees Celsius for 11 minutes to obtain semi-carbonized chips C21 with an average moisture content of 25.2% based on wet weight. The inventors also heated the second group of green wood chips similarly at 330 degrees Celsius for 11 minutes to obtain semi-carbonized chips C22 with an average moisture content of 18.6% based on wet weight (hereinafter, Celsius will be omitted). From this result, the inventors have obtained the prospect of obtaining semi-carbonized chips C2 with a moisture content of about 20% to 30% based on wet weight by heating the green wood chips C1 at a heating temperature of about 300 to 400 degrees for 5 to 15 minutes (or 20 minutes). The semi-carbonized chips C21 and C22 are examples of subdivisions of the semi-carbonized chips C2.
[0024] <Hydrophobicity of semi-carbonized chips C21 and C22> FIG. 3 is a diagram illustrating the change in weight over time when green wood chips C1, semi-carbonized chips C21, and semi-carbonized chips C22 are soaked in water. If the weight change of a material after soaking in water is large, the material is said to have high water absorption and low hydrophobicity. Therefore, FIG. 3 is a diagram illustrating the results of measuring the hydrophobicity of semi-carbonized chips C21 and C22 in comparison with green wood chips C1. Note that green wood chips C1 are an example of raw wood pieces before semi-carbonization.
[0025] In Fig. 3, the horizontal axis is the time elapsed after soaking in water, and the vertical axis shows the weight change in percentage for green wood chips C1, semi-carbonized chips C21, and semi-carbonized chips C22. The measurements in Fig. 3 were taken after green wood chips C1, semi-carbonized chips C21, and semi-carbonized chips C22 were each dried in a drying device until there was no change in weight, and then each was soaked in water. This type of weight change is called the dry start weight change.
[0026] As shown in Fig. 3, for example, between 40 and 80 hours after immersion, the rate of weight increase of the semi-carbonized chips C21 (the rate of increase relative to the weight at the time of its dry start) is about 25% less than that of the green wood chips C1. Also, the rate of weight increase of the semi-carbonized chips C22 (the rate of increase relative to the weight at the time of its dry start) is about 50% less than that of the green wood chips C1. In other words, the results in Fig. 3 illustrate that the semi-carbonized chips have lower water absorption when immersed in water, that is, are more hydrophobic, compared to the green wood chips C1.
[0027] That is, the semi-carbonized chips C21 have higher hydrophobicity than the green wood chips C1. For example, in Fig. 3, after 40 hours, the weight increase rate of the green wood chips C1 is 300%, and the weight increase rate of the semi-carbonized chips C21 is about 275%. This is maintained for 40 to 80 hours after immersion. Therefore, it can be seen that the water absorption rate of the semi-carbonized chips C21 is approximately 275 / 300 = 91% compared to the green wood chips C1 for 40 to 80 hours after immersion. Conversely, it can be seen that the hydrophobicity of the semi-carbonized chips C21 is improved to 300 / 275 = 1.09 times compared to the green wood chips C1.
[0028] Moreover, after 40 hours, the weight increase rate of the semi-carbonized chips C22 is about 250%. Therefore, it can be seen that the water absorption rate of the semi-carbonized chips C22 is approximately 250 / 300=83% compared to the green wood chips C1 between 40 and 80 hours after immersion. Conversely, it can be seen that the hydrophobicity of the semi-carbonized chips C22 is improved by 300 / 250=1.2 times compared to the green wood chips C1.
[0029] Fig. 4 is a diagram comparing the measurement results of hydrophobicity of semi-carbonized chips C22, which were obtained by heating a group of green wood chips at 330 degrees for 11 minutes and had a moisture content of 18.617%, after a dry start and a wet start. As in Fig. 3, the horizontal axis of Fig. 4 shows the time elapsed after immersion in water, and the vertical axis shows the change in weight of the semi-carbonized chips C22 in %, as an example. As explained in Fig. 3, the process of immersing the semi-carbonized chips C22 produced by the production apparatus 1 in water without drying the semi-carbonized chips C22 until there is no change in weight can be called a wet start.
[0030] However, in the case of a wet start, the semi-carbonized chips C22 have an average moisture content of 18.617%, so the rate of change in weight after immersion is smaller than that of a dry start. Therefore, in FIG. 4, the semi-carbonized chips C22 (moisture content 0%) in the dry start are used as the reference, so the measurement result of the weight change in the wet start is corrected by increasing the increase rate of 29.66%. The moisture content (wet standard) of the chips semi-carbonized at 330 degrees was an average of 18.617%. This contains 0.22875g of water per 1g of dry chips. The graph (D22) of the wet start is a curve showing the change in weight from the start of immersion (elapsed time 0) when 1g of wet chips containing 0.22875g of water is taken as 1g. The weight of the dry chips obtained by drying 1g of these wet chips is 1-0.22875=0.77125g. When comparing the wet start graph (D22) and the dry start graph (C22) in terms of the weight increase rate (%) after immersion, it is necessary to match the weight standards for both at the start of immersion (elapsed time 0). For example, if the dry tip weight is 1g, the wet tip weight must be 1 / (1-0.22875) = 1.2966 times, and the wet tip weight increase rate (%) graph (D22) will increase the base by 29.66% (E22).
[0031] In FIG. 4, C22 is a graph illustrating the weight change of the semi-carbonized chips C22, which are the same as those in FIG. 3. D22 is a graph illustrating the weight change of the semi-carbonized chips C22 in the case of a wet start. E22 is a graph in which the weight change of the semi-carbonized chips C22 in the case of a wet start is corrected by an increase rate of 29.66%. As shown in FIG. 4, the weight change in the dry start (C22) and the corrected weight change in the wet start (E22) are almost the same. Therefore, it can be seen that the weight change rate after immersion is properly measured for the semi-carbonized chips C22, regardless of whether it is a dry start or a wet start. It can also be assumed that the same results as those in FIG. 4 will be obtained for the semi-carbonized chips C21 and the green wood chips C1.
[0032] <Manufacturing method steps> 5 is a diagram illustrating the configuration of a control table showing the relationship between the type of green wood (tree) to be used as the green wood chips C1, the heating temperature, and the heating time. The moisture content of the chips C1 can be determined almost by the type of green wood. Therefore, by conducting experiments with different heating temperatures and heating times for each type of green wood, it is possible to determine the heating temperature and heating time for setting the wet standard moisture content of the semi-carbonized chips C2 to an appropriate value, for example, about 20% to 30%, and obtain the control table of FIG. 5. FIG. 5 is a diagram illustrating the configuration of a control table stored in the storage device 12 based on the experimental results. In other words, the heating temperature and heating time can be set according to the type of green wood (tree) or the moisture content of the wood pieces.
[0033] In the example of FIG. 5, the relationship between the appropriate heating temperature and the appropriate heating time is illustrated for each type of green wood. In FIG. 5, a plurality of heating temperatures and heating times are illustrated for each type of green wood. However, the optimum heating temperature and heating time may be further selected from the plurality of sets of these heating temperatures and heating times. In the example of FIG. 5, one row of the table corresponds to the heating control for semi-carbonizing the green wood chips C1. In the example of FIG. 5, a single constant heating temperature and a heating time at that heating temperature are set in the heating control for semi-carbonizing the green wood chips C1. However, the manufacturing method by the manufacturing apparatus 1 is not limited to such a procedure. For example, the manufacturing apparatus 1 may semi-carbonize the green wood chips C1 by a plurality of sets (TMPk, TMk) of a heating temperature TMPk and a heating time TMk, k=1, 2, 3.
[0034] For example, the control device 11 may record the amount of power consumption or fuel consumption in the manufacturing device 1 for each combination of heating temperature and heating time, and determine the combination of heating temperature and heating time that empirically minimizes the amount of power consumption or fuel consumption as the optimal one. For example, the control device 11 may receive and record the data of the change in weight after immersion, which is the same data as in FIG. 3, for the semi-carbonized chips C2 manufactured by a plurality of combinations of heating temperature and heating time. Then, the control device 11 may determine the heating temperature and heating time for the semi-carbonized chips C2 with relatively little weight change (or the semi-carbonized chips C2 with the smallest weight change) as the optimal one. For example, the control device 11 may select, from among a plurality of combinations of heating temperature and heating time when the moisture content is controlled to 20% to 30%, a combination that improves the hydrophobicity of the semi-carbonized chips C2 after semi-carbonization by at least 1.09 times or 1.2 times compared to the green wood chips C1 before semi-carbonization. Furthermore, the control device 11 may select, for example, from among a plurality of sets of heating temperatures and heating times when the moisture content is controlled to 20% to 30%, a set that causes less change in weight of the semi-carbonized chips C2 after immersion (a set in which hydrophobicity is relatively improved). Furthermore, the control device 11 may determine, as an optimal set, a set of heating temperatures and heating times that empirically minimizes the amount of power consumption or fuel consumption, from among a plurality of sets in which the hydrophobicity of the semi-carbonized chips C2 after carbonization is relatively improved. Such an optimal set of heating temperatures and heating times may include a plurality of heating temperatures and heating times.
[0035] Furthermore, the manufacturing apparatus 1 may obtain the moisture content of the raw wood chips C1 as the raw material through input from an operator before the heat treatment. When the moisture content of the raw wood chips C1 as the raw material is obtained, a control table for adjusting the moisture content of the semi-carbonized chips C2 to an appropriate value may be created using the relationship between the moisture content range of the raw wood chips C1, the heating temperature, and the heating time instead of the table of Fig. 5. Here, the moisture content range of the raw wood chips C1 is a range divided in several percent increments, for example, 5% or 10% increments.
[0036] Furthermore, instead of classifying raw materials based on the type of green wood, moisture content of the green wood, etc., a control table may be created that assumes an average moisture content and uses the relationship between heating temperature and heating time to set the moisture content of the semi-carbonized chips C2 to an appropriate value.
[0037] In order to obtain the average moisture content, the control device 11 may constantly receive and monitor, for example, the input of the type of green wood of the green wood chips C1 fed into the manufacturing device 1 or the moisture content of the green wood chips C1. The control device 11 may then use the actual average moisture content currently obtained as the moisture content of the green wood chips C1 currently being processed. The control device 11 may sequentially record the types of raw wood of the raw wood chips C1 input by the operator via the input device of the control device 11. The control device 11 may also sequentially record the moisture contents of the raw material samples input by the operator via the input device of the control device 11.
[0038] As described above, when the average moisture content of the green wood chips C1 is constantly monitored, the control device 11 may refer to a control table that specifies the relationship between the moisture content range, the heating temperature, and the heating time. However, the control device 11 may continue to use the average moisture content of the green wood chips C1 obtained by such monitoring for a predetermined period, such as one month or one year. The control device 11 may also update the average moisture content of the green wood chips C1 obtained by such monitoring daily or hourly.
[0039] The control device 11 may specify the relationship between the type of green wood chips C1 (or the moisture content of the green wood chips C1), the heating temperature, the heating time, and the target moisture content of the semi-carbonized chips C2 in an empirical formula by regression analysis. The control device 11 uses one of the type of green wood chips C1 (or the moisture content), the heating temperature, the heating time, and the target moisture content of the semi-carbonized chips C2 as an objective variable in the empirical formula by regression analysis instead of a control table. The control device 11 may obtain an empirical formula with the remaining parameters as independent variables and store it in memory. The control device 11 may then obtain the heating time by inputting values for the independent variables (such as the heating temperature other than the heating time) with the heating time as the objective variable, for example. The control device 11 may also obtain the heating temperature by storing an empirical formula with the heating temperature as the objective variable instead of the heating time and with variables other than the heating temperature as independent variables in memory.
[0040] FIG. 6 is a diagram illustrating a manufacturing process performed by the control device 11. This process is performed, for example, by a Central Processing Unit (CPU) or a processor in the control device 11. It is executed by a computer program that is executablely deployed in the memory of the computer.
[0041] In this process, first, the control device 11 acquires a target temperature and a heating time from the type of raw wood chips C1 to be processed (S1). The type of raw wood chips to be processed is input by an operator's operation from a user interface on an input device connected to the control device 11. The input device is, for example, a keyboard, a touch panel, or a combination of a display and a pointing device.
[0042] Then, the control device 11 heats the carbonization furnace 10 to a target temperature (S2). The target temperature is the temperature of the space inside the furnace, the surface temperature of the raw materials, the temperature of the gas that heats the raw materials, etc. The process of S2 can be considered as initial heating for bringing the carbonization furnace 10 into a target operating state.
[0043] Next, the control device 11 feeds the green wood chips C1 through the feed port of the carbonization furnace 10 (S3). Next, the control device 11 controls the heating so that the carbonization furnace 10 is maintained at the target temperature (S4). Then, the control device 11 determines whether or not a predetermined heating time has elapsed (S5). If the predetermined heating time has not elapsed, the control device 11 returns the process to S4. In the processes of S4 and S5, the green wood chips C1 are heated, for example, at 300 to 400 degrees Celsius for 5 to 15 minutes. On the other hand, if the predetermined heating time has elapsed, the control device 11 discharges the semi-carbonized chips from the carbonization furnace 10 (S6).
[0044] Next, the control device 11 judges whether or not to end the process (S7). If the process is not to be ended, the control device 11 returns the process to S3 and inputs the next green wood chip C1. If the next green wood chip C1 is not to be processed, for example, the control device 11 ends the process according to the operation of the operator. The processes from S1 to S6 can be said to be one batch process. However, in continuous or intermittent processing, the processes from S3 to S6 may be performed for a predetermined time. This will be repeated every time.
[0045] <Effects of the embodiment> In this embodiment, the manufacturing apparatus 1 and the manufacturing method using the manufacturing apparatus 1 heat green wood chips C1 with a moisture content of over 37%, control the moisture content to 20% to 30%, and thermally decompose at least a part of the surface to produce semi-carbonized chips C2. Therefore, semi-carbonized chips C2 with a moisture content of 20% to 30% can be stably and mass-produced from the green wood chips C1.
[0046] The step of pyrolyzing at least a part of the surface includes, for example, heating the green wood chips C1 at 300 to 400 degrees Celsius for 5 to 15 minutes. Therefore, the manufacturing apparatus 1 and the manufacturing method using the manufacturing apparatus 1 can manufacture the semi-carbonized chips C2 in a relatively short period of time, within 15 minutes. Furthermore, the manufacturing apparatus 1 and the manufacturing method using the manufacturing apparatus 1 can select an appropriate heating temperature and heating time depending on the type of green wood of the green wood chips C1 and the moisture content of the raw material, thereby reducing the amount of electricity or fuel consumed in the carbonization furnace 10. Furthermore, the manufacturing apparatus 1 and the manufacturing method using the manufacturing apparatus 1 can improve the hydrophobicity of the semi-carbonized chips C2 manufactured by selecting an appropriate heating temperature and heating time depending on the type of green wood of the green wood chips C1 and the moisture content of the raw material.
[0047] The raw wood chips C1 are pieces of wood that have not been dried after felling. Therefore, the manufacturing device 1 and the manufacturing method using the manufacturing device 1 can produce a large amount of semi-carbonized chips C2 using raw wood that has not been pretreated.
[0048] The semi-carbonized chips C2 in this embodiment have a moisture content of 20% to 30%, and at least a part of the surface is pyrolyzed. The semi-carbonized chips C2 have a relatively high moisture content and a heavy mass compared to normal semi-carbonized chips. As a result, even when the semi-carbonized chips C2 are mixed with other fuels such as coal in a combustion furnace, the possibility of being blown up by the hot air generated in the combustion furnace is reduced, and the semi-carbonized chips C2 are effective in implementing stable mixed combustion. That is, the semi-carbonized chip manufacturing apparatus and manufacturing method of this embodiment make it possible to manufacture semi-carbonized chips that are easy to handle when mixed with non-biomass fuel. In addition, for example, a substance with a low specific gravity has a characteristic that it is difficult to mix with a substance with a high specific gravity even when stirred. Therefore, the semi-carbonized chips of this embodiment can facilitate handling of the fuel when stirring and mixing.
[0049] The semi-carbonized chips C21 (green wood chips heated at 350°C for 11 minutes) in this embodiment have improved hydrophobicity by at least 1.09 times between 40 and 80 hours after immersion compared to the raw green wood chips C1. Also, the semi-carbonized chips C22 (green wood chips heated at 330°C for 11 minutes) have improved hydrophobicity by at least 1.2 times between 40 and 80 hours after immersion compared to the raw green wood chips C1. Therefore, the semi-carbonized chips C21 and C22 in this embodiment are likely to maintain their properties such as moisture content even in an outdoor environment where they are exposed to rain. [Explanation of symbols]
[0050] 1 Manufacturing equipment 10 Carbonization furnace 11 Control device 12 Storage device
Claims
1. Heating wood pieces with a moisture content of more than 37%, The moisture content is controlled to 20% to 30%; A method for producing torrefied pieces, comprising a step of pyrolyzing at least a portion of a surface thereof.
2. 2. The method of claim 1, wherein the pyrolysis step comprises heating the wood pieces at 300 to 400 degrees Celsius for 5 to 15 minutes.
3. The method for producing semi-carbonized pieces according to claim 1, wherein the wood pieces are wood pieces that have not been subjected to a drying treatment after felling.
4. 2. The method for producing semi-carbonized pieces according to claim 1, wherein in the pyrolysis step, a heating temperature and a heating time are set according to the type of tree that constitutes the wood pieces or the moisture content of the wood pieces.
5. The method for producing semi-carbonized pieces as described in claim 4, wherein the heating temperature and heating time are selected from among multiple combinations of heating temperatures and heating times when the moisture content is controlled to 20% to 30%, and a combination that consumes relatively less electricity or fuel in the pyrolysis process is selected.
6. The method for manufacturing semi-carbonized pieces as described in claim 4, wherein the heating temperature and heating time are selected from among multiple combinations of heating temperatures and heating times when the moisture content is controlled to 20% to 30%, and a combination is selected in which the hydrophobicity of the semi-carbonized pieces after treatment by the pyrolysis process is improved by 1.09 times compared to the wood pieces before treatment by the pyrolysis process.
7. A piece of wood having a moisture content of 20% to 30% and at least a portion of the surface of which has been pyrolyzed.
8. 8. The wood piece of claim 7, wherein said surface has at least a portion thereof improved in hydrophobicity by a factor of at least 1.09 by pyrolysis compared to the raw wood piece prior to pyrolysis.
9. 8. The wood piece of claim 7, wherein the hydrophobicity of at least a portion of the surface of the piece is improved by at least a factor of 1.2 by pyrolysis compared to the hydrophobicity of the raw wood piece before pyrolysis.
Citation Information
Patent Citations
Production method of woody composite resin material and woody composite resin material
JP2018083876A
Method of semi-carbonizing biomass and device therefor
JP2019045078A
Method for producing biomass fuel
JP2021127443A
Biomass fuel torrefied pellet manufacturing equipment and biomass power generation system
JP7108354B1