Magnetoresistive element and semiconductor device

By inserting a metal oxide layer and amorphous layer with different crystal symmetries between the BiSb SOT electrode and MTJ element, the issues of interface roughness and diffusion are addressed, enhancing the spin Hall angle and reducing switching current in SOT-MRAM.

JP2024162252APending Publication Date: 2024-11-21SAMSUNG ELECTRONICS CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023077596
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-10
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

The challenges of obtaining a flat BiSb thin film using sputter deposition for SOT-MRAM, leading to rough BiSb/ferromagnetic layer interfaces, spin diffusion loss, and interdiffusion issues, which degrade the spin Hall angle and increase switching current requirements.

Method used

Incorporating a metal oxide layer and a low-resistance amorphous layer between the BiSb SOT electrode and the MTJ element, with different crystal symmetries and acting as a diffusion barrier, to improve surface flatness and reduce spin loss.

Benefits of technology

Enhances the spin Hall angle and reduces switching current, improving the magnetic properties and efficiency of SOT-MRAM by confining the switching current and suppressing mutual diffusion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162252000001_ABST
    Figure 2024162252000001_ABST
Patent Text Reader

Abstract

To provide a magnetoresistive element and a semiconductor device that can improve magnetic characteristics.SOLUTION: A magnetoresistive element 1 comprises an SOT electrode layer 20, a metal oxide layer 30, a first nonmagnetic layer A10, a first magnetic layer B10, a second nonmagnetic layer A20, and a second magnetic layer B20, and the first magnetic layer B10, second nonmagnetic layer A20, and second magnetic layer B20 constitute a magnetic tunnel junction element, wherein the SOT electrode layer 20 includes BiSb as a material, the metal oxide layer 30 includes metal oxide as a material, and the first nonmagnetic layer A10 at least partially includes amorphous. Crystals included in the SOT electrode layer and crystals in the first magnetic layer differ in symmetry of rotation of the crystals on the lamination direction of those layers as an axis of rotation.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a magnetoresistive element and a semiconductor device. [Background technology]

[0002] In order to reduce the switching current of spin orbit torque (SOT)-magnetoresistive random access memory (MRAM), it is necessary to increase the spin Hall angle, which is the efficiency of conversion from electric current to spin current in the SOT electrode.

[0003] Patent Document 1 proposes a technology for significantly increasing the spin Hall angle and reducing the switching current by using an SOT electrode made of bismuth antimony (hereinafter referred to as BiSb), a topological insulator, with a (012) crystal orientation.

[0004] Patent Document 2 proposes a buffer layer configuration for promoting the (012) crystal orientation that provides a large spin Hall angle in a BiSb SOT electrode.

[0005] By using a BiSb SOT electrode with crystal orientation in the (012) plane direction grown by molecular beam epitaxy (MBE), a spin Hall angle of 52 can be obtained, which is much larger than the value obtained when SOT electrodes made of heavy metals such as tungsten (W) and tantalum (Ta) are used.

[0006] Furthermore, the spin Hall conductivity, which is an indicator of power saving, has been found to be approximately two orders of magnitude higher than in the previous cases of W and Ta. [Prior art documents] [Patent documents]

[0007] [Patent Document 1] JP 2019-054484 A [Patent Document 2] JP 2021-128814 A [Patent Document 3] Patent Publication No. 2021-057357 [Non-patent literature]

[0008] [Non-Patent Document 1] L. Zhu et al., Phys. Rev. Lett. 126 (2021) 107204 Summary of the Invention [Problem to be solved by the invention]

[0009] However, it is known that it is difficult to obtain a flat thin film of BiSb using a sputtering deposition method, which is more suitable for manufacturing SOT-MRAM. When a ferromagnetic layer constituting a magnetic tunnel junction (MTJ) element is laminated on such a BiSb thin film with reduced flatness, the interface between the BiSb and the ferromagnetic layer becomes rough. As a result, spin diffusion loss occurs at the interface between the BiSb and the ferromagnetic layer, resulting in a large decrease in the spin Hall angle.

[0010] Furthermore, since the BiSb material has a tendency to diffuse, even immediately after sputtering deposition, Sb in BiSb diffuses into the ferromagnetic layer containing CoPt or the like, and conversely, Pt diffuses into the BiSb layer, creating a problem of interdiffusion.

[0011] On the other hand, SOT-MRAM generally has a laminated structure of an SOT electrode and a ferromagnetic layer, so the switching current flowing through the SOT electrode is diverted to the ferromagnetic layer, reducing the effective switching current flowing through the SOT electrode. This causes a problem of shunt current, which increases the threshold current required for switching. All of these problems deteriorate the magnetic properties of the magnetoresistance element.

[0012] The present disclosure is intended to solve at least one of these problems, and has an object to provide a magnetoresistive element and a semiconductor device capable of improving magnetic characteristics. [Means for solving the problem]

[0013] In one embodiment, the magnetoresistance element comprises an SOT electrode layer, a metal oxide layer provided on the SOT electrode layer, a first non-magnetic layer provided on the metal oxide layer, a first magnetic layer provided on the first non-magnetic layer, a second non-magnetic layer provided on the first magnetic layer, and a second magnetic layer provided on the second non-magnetic layer, wherein the first magnetic layer, the second non-magnetic layer, and the second magnetic layer constitute a magnetic tunnel junction element, the SOT electrode layer contains BiSb as a material, the metal oxide layer contains a metal oxide as a material, the first non-magnetic layer is at least partially amorphous, and the crystals contained in the SOT electrode layer and the crystals contained in the first magnetic layer have different rotational symmetries of crystals with the stacking direction of these layers as the rotation axis.

[0014] The above magnetoresistance element may further include a third magnetic layer provided between the metal oxide layer and the first nonmagnetic layer, the third magnetic layer being magnetically coupled to the first magnetic layer.

[0015] The above magnetoresistance element may further include a third nonmagnetic layer provided between the metal oxide layer and the third magnetic layer, and the third nonmagnetic layer may have a crystal structure that reduces crystal lattice mismatch between the metal oxide layer and the third magnetic layer.

[0016] The above-mentioned magnetoresistance element may further include a third non-magnetic layer provided between the metal oxide layer and the third magnetic layer, and the third magnetic layer formed on the third non-magnetic layer may be suppressed from growing in an island shape and have improved flatness.

[0017] In the above magnetoresistance element, the metal oxide layer may include a first metal oxide layer and a second metal oxide layer, and the first metal oxide layer may include, as a material thereof, a metal oxide different from that of the second metal oxide layer.

[0018] In the above magnetoresistance element, the metal oxide layer may include the metal oxide having a spin diffusion length longer than the distance between the SOT electrode layer and the first magnetic layer.

[0019] In the above magnetoresistance element, the first magnetic layer may include the crystals with four-fold rotational symmetry, and the SOT layer may include the crystals with three-fold rotational symmetry.

[0020] In the above magnetoresistance element, the metal oxide layer is made of Cr 2 O 3 may include:

[0021] In the magnetoresistance element, the metal oxide layer may have a thickness of 0.5 to 2.5 nm.

[0022] In the magnetoresistance element, the first nonmagnetic layer may at least partially contain an amorphous metal.

[0023] In the above magnetoresistance element, the first nonmagnetic layer may contain at least one of a simple transition metal, an alloy of transition metals, a compound of a transition metal and a metalloid, a transition metal nitride, a transition metal oxide, and a BCN-based material.

[0024] In the above magnetoresistance element, the first nonmagnetic layer may have a thickness of 0.8 to 1.0 nm.

[0025] In the magnetoresistance element, the third magnetic layer may contain at least one of Co and a Co--Pt alloy as a material.

[0026] In the magnetoresistance element, the third magnetic layer may include the crystals having three-fold rotational symmetry with the stacking direction as the rotation axis.

[0027] In the magnetoresistance element, the third nonmagnetic layer may contain a metal as a material.

[0028] In the above magnetoresistance element, the third nonmagnetic layer is made of TiCr 2 may include:

[0029] In the above magnetoresistance element, the third nonmagnetic layer may have a thickness greater than 0 nm and equal to or less than 1.0 nm.

[0030] In the magnetoresistive element, the third nonmagnetic layer may include the crystals having three-fold rotational symmetry with the stacking direction as the rotation axis.

[0031] In the above magnetoresistance element, the first metal oxide layer is made of Cr 2 O 3 The second metal oxide layer may include, as a material, at least one of aluminum oxide, tantalum oxide, magnesium oxide, ruthenium oxide, hafnium oxide, and chromium oxide.

[0032] The above magnetoresistance element may further include an underlayer, and the SOT electrode layer may be provided on the underlayer.

[0033] A semiconductor device according to one embodiment includes the above-described magnetoresistive element. Effect of the Invention

[0034] According to the inspection device of the present disclosure, it is possible to provide a magnetoresistive element and a semiconductor device capable of improving switching characteristics. [Brief description of the drawings]

[0035] [Figure 1] 1 is a cross-sectional view illustrating a magnetoresistance element according to a first embodiment. [Diagram 2] 1 is a cross-sectional view illustrating a magnetoresistance element according to a first embodiment. [Diagram 3] 10 is a cross-sectional view illustrating a magnetoresistance element according to a modified example of the first embodiment. [Figure 4] FIG. 11 is a cross-sectional view illustrating a magnetoresistance element according to a second embodiment. [Diagram 5] 13 is a cross-sectional view illustrating a magnetoresistance element according to a modified example of the second embodiment. FIG. [Figure 6] FIG. 11 is a cross-sectional view illustrating a magnetoresistance element according to a third embodiment. [Figure 7] 13 is a cross-sectional view illustrating a magnetoresistance element according to a modified example of the third embodiment. FIG. [Figure 8] FIG. 11 is a cross-sectional view illustrating a magnetoresistance element according to embodiment 4. [Figure 9] 13 is a cross-sectional view illustrating a magnetoresistance element according to a modified example of the fourth embodiment. FIG. [Figure 10] FIG. 13 is a circuit diagram illustrating a semiconductor device according to a fifth embodiment. [Figure 11] FIG. 13 is a circuit diagram illustrating a semiconductor device according to a fifth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0036] For clarity of explanation, the following description and drawings have been omitted and simplified as appropriate. In addition, in each drawing, the same elements are given the same reference numerals, and duplicate explanations are omitted as necessary.

[0037] (Overview of the embodiment) First, an outline of the embodiment will be described. Spin Transfer Torque MRAM (hereinafter referred to as STT-MRAM), which is currently being widely researched and developed, performs write and read operations on an MTJ element using a two-terminal structure. Therefore, when STT-MRAM is highly integrated, there are problems in that a sufficient read margin cannot be obtained and that thermal disturbance resistance cannot be obtained for a sufficiently long period of time.

[0038] SOT-MRAM, which utilizes the spin Hall effect (SHE), is attracting attention as a method that not only solves these problems but also enables high-speed, low-power writing. SOT-MRAM has a three-terminal structure in which writing is performed by generating a spin current from an electric current. By using a BiSb topological insulator as the material for the SOT electrodes of such SOT-MRAM, highly efficient SOT switching can be achieved.

[0039] However, when BiSb is used for the SOT electrode, problems arise such as surface flatness, interdiffusion of the constituent elements, and shunt current to the ferromagnetic material, which reduce the performance of SOT-MRAM and make it difficult to put it to practical use.

[0040] In this disclosure, in the element structure of SOT-MRAM, a metal oxide capable of propagating spin current is inserted between the BiSb SOT electrode layer and the recording layer of the MTJ element on top of it. Furthermore, a low-resistance amorphous layer is inserted to separate the crystal structures of the BiSb SOT electrode layer / metal oxide film and the MTJ element containing CoFeB / MgO, which have different crystal systems. This increases the write efficiency of SOT-MRAM and improves the read efficiency of the MTJ element, making it possible to provide a SOT-MRAM with good characteristics.

[0041] (Embodiment 1) A magnetoresistance element according to the first embodiment will be described. FIGS. 1 and 2 are cross-sectional views illustrating the magnetoresistance element according to the first embodiment. As shown in FIG. 1, the magnetoresistance element 1 includes an underlayer 10, an SOT electrode layer 20, a metal oxide layer 30, a first non-magnetic layer A10, a first magnetic layer B10, a second non-magnetic layer A20, and a second magnetic layer B20. As shown in FIG. 2, the magnetoresistance element 1 may omit the underlayer 10. In the following figures, the underlayer 10 is omitted. For convenience of explanation, the figures show the materials or names contained in each layer, but these materials and names are merely examples and do not limit the materials of each layer to these materials.

[0042] For ease of explanation, the metal oxide layer 30 is referred to as a metal oxide layer (metal oxide) 30, the first nonmagnetic layer A10 is referred to as a first nonmagnetic layer (amorphous) A10, and the first magnetic layer B10 is referred to as a first magnetic layer (recording layer) B10.

[0043] The SOT electrode layer 20, the metal oxide layer (metal oxide) 30, the first non-magnetic layer (amorphous) A10, the first magnetic layer (recording layer) B10, the second non-magnetic layer A20 and the second magnetic layer B20 may be formed by a thin film formation method such as sputtering, reactive sputtering, MBE, electron beam deposition, or other thin film formation methods. All layers may be formed by a predetermined thin film formation method, or some layers may be formed by a thin film formation method different from the other layers.

[0044] The first magnetic layer (recording layer) B10, the second non-magnetic layer A20, and the second magnetic layer B20 constitute an MTJ element. The MTJ element including the first magnetic layer (recording layer) B10, the second non-magnetic layer A20, and the second magnetic layer B20 may be patterned. The patterning may be performed on the first non-magnetic layer (amorphous) A10, the first magnetic layer (recording layer) B10, the second non-magnetic layer A20, and the second magnetic layer B20.

[0045] <Underlayer> The underlying layer 10 includes a layer that serves as a base when forming the SOT electrode layer 20. Also, the underlying layer 10 may be an insulating buffer layer. The underlying layer 10 includes, for example, an insulator such as silicon oxide (SiO 2 ). Note that the underlying layer 10 is not limited to those containing an insulator such as silicon oxide as long as it is a material that serves as a base when forming the SOT electrode layer 20, and may include other materials such as sapphire.

[0046] <SOT electrode layer> The SOT electrode layer 20 is provided on the underlying layer 10. The SOT electrode layer 20 is a layer for applying spin-orbit torque to the first magnetic layer (recording layer) B10, which is the recording layer of the MTJ element. Specifically, by passing a current through the SOT electrode layer 20, spin-orbit torque can be applied to the first magnetic layer (recording layer) B10 of the MTJ element. The SOT electrode layer 20 contains BiSb as a material. The SOT electrode layer 20 may have a trigonal crystal structure. The stable structure of BiSb is trigonal, and in a structure where its (001) plane is oriented on the underlying layer 10, a relatively large spin Hall angle can be obtained. In this case, the SOT electrode layer 20 has a crystal structure with three-fold rotational symmetry about the film plane normal direction as the rotation axis. However, a structure in which the (012) plane of BiSb is oriented on the underlying layer 10 also exhibits a very large spin Hall angle. In this case, since the SOT electrode layer 20 has a face-centered lattice that is shifted into a rectangle in the plane, it has a structure that is neither three-fold nor four-fold rotationally symmetric about the film plane normal direction as the rotation axis. Hereinafter, the rotation axis of rotational symmetry will be described as the stacking direction of each layer.

[0047] <Metal oxide layer (metal oxide)> The metal oxide layer (metal oxide) 30 is provided on the SOT electrode layer 20. The metal oxide layer (metal oxide) 30 contains a metal oxide as a material. The metal oxide layer (metal oxide) 30 contains, for example, a metal oxide whose spin diffusion length is longer than the element size. Specifically, the metal oxide layer (metal oxide) 30 contains a metal oxide whose spin diffusion length is longer than the distance between the SOT electrode layer 20 and the first magnetic layer (recording layer) B10. For example, the metal oxide layer (metal oxide) 30 contains, for example, Cr 2 O 3 The metal oxide layer (metal oxide) 30 may contain Cr. 2 O 3 However, the metal oxide layer (metal oxide) 30 is not limited to Cr. 2 O 3 When the metal oxide layer (metal oxide) 30 contains Cr, the magnetic properties of the magnetoresistance element 1 can be significantly improved. The thickness of the metal oxide layer (metal oxide) 30 is preferably 0.5 to 2.5 nm, and more preferably 1.0 to 1.1 nm. 2 O 3 When the thickness of the metal oxide layer (metal oxide) 30 containing the metal oxide is 0.5 to 2.5 nm, the magnetic characteristics of the magnetoresistance element 1 can be significantly improved. When the thickness is 1.0 to 1.1 nm, the magnetic characteristics can be further significantly improved.

[0048] <First non-magnetic layer (amorphous)> The first non-magnetic layer (amorphous) A10 is provided on the metal oxide layer (metal oxide) 30. The first non-magnetic layer (amorphous) A10 includes a non-magnetic material. The first non-magnetic layer (amorphous) A10 includes a material for dividing the rotational symmetry of the crystals of the first magnetic layer B10 and the SOT electrode layer 20 with the film vertical direction (stacking direction) as the rotation axis. Specifically, the first magnetic layer B10 and the SOT electrode layer 20 have different rotational symmetries of the crystals with the stacking direction of each layer as the rotation axis, and the lattice constants in the parallel direction in the film are significantly different. For example, the first magnetic layer B10 includes a crystal structure with four-fold rotational symmetry with the film surface vertical direction (stacking direction) as the rotation axis, and the SOT electrode layer 20 includes a crystal structure with three-fold rotational symmetry with the stacking direction of each layer as the rotation axis. In this case, since the first non-magnetic layer (amorphous) A10 is amorphous, the SOT electrode layer 20 and the first magnetic layer B10 have a rotational symmetry of crystals with the lamination direction of each layer as the rotation axis broken, so the metal oxide layer (metal oxide) 30 in contact with the lower surface of the first non-magnetic layer (amorphous) A10 may be either crystalline or amorphous. The crystals contained in the SOT electrode layer 20 and the crystals contained in the first magnetic layer (recording layer) B10 have different rotational symmetries of crystals with the lamination direction of these layers as the rotation axis.

[0049] The first nonmagnetic layer (amorphous) A10 includes at least a portion of an amorphous material. For example, the first nonmagnetic layer (amorphous) A10 includes a low-resistance amorphous material as a material. Specifically, the first nonmagnetic layer (amorphous) A10 may include a metal layer at least a portion of which is amorphous. The first nonmagnetic layer (amorphous) A10 may include a low-resistance material of which half or more is amorphous. Preferably, the first nonmagnetic layer (amorphous) A10 may include at least a half of an amorphous metal.

[0050] The first non-magnetic layer (amorphous) A10 may include, for example, Ta as a material. The first non-magnetic layer (amorphous) A10 is not limited to a material including Ta, as long as it includes a low-resistance material at least partially configured as amorphous. For example, the first non-magnetic layer (amorphous) A10 may include, as a material, at least one of a simple transition metal, an alloy of transition metals, a compound of a transition metal and a metalloid, a transition metal nitride, a transition metal oxide, and a BCN-based material. Specifically, the first non-magnetic layer (amorphous) A10 may include a simple transition metal such as Ta, W, and hafnium (Hf), an alloy of transition metals such as Ta-Cu, or a compound of a transition metal such as Ta, W, Hf, molybdenum (Mo), or niobium (Nb) and a metalloid such as boron (B), carbon (C), silicon (Si), or germanium (Ge). In addition, the first nonmagnetic layer (amorphous) A10 may include an amorphous thin film made of transition metal nitrides or oxides, such as zirconium nitride (ZrN) and titanium nitride (TiN), which have relatively low resistivity, as well as BCN-based materials, such as diamond-like carbon (DLC), boron nitride (BN), and carbon nitride (CN).

[0051] The first non-magnetic layer (amorphous) A10 preferably has a thickness of 0.8 to 1.0 nm, the details of which will be described later.

[0052] <First magnetic layer (recording layer)> The first magnetic layer (recording layer) B10 is provided on the first non-magnetic layer (amorphous) A10. The first magnetic layer (recording layer) B10 includes a magnetic material. The first magnetic layer (recording layer) B10 may include a ferromagnetic material. The first magnetic layer (recording layer) B10 functions as a recording layer of the MTJ element. Therefore, the first magnetic layer (recording layer) B10 of the MTJ element is applied with a spin orbit torque by a current flowing through the SOT electrode layer 20. The first magnetic layer (recording layer) B10 may include, for example, CoFeB as a material. Therefore, the first magnetic layer (recording layer) B10 may include a crystal structure with four-fold rotational symmetry. Note that the material of the first magnetic layer (recording layer) B10 is not limited to one including CoFeB as long as it functions as a recording layer of the MTJ element and includes a crystal structure with four-fold rotational symmetry.

[0053] <Second non-magnetic layer> The second non-magnetic layer A20 is provided on the first magnetic layer (recording layer) B10. The second non-magnetic layer A20 includes a non-magnetic material. The second non-magnetic layer A20 functions as a tunnel barrier layer of the MTJ element. The second non-magnetic layer A20 may include, for example, magnesium oxide (MgO) as a material. Therefore, the second non-magnetic layer A20 may include a crystal structure with four-fold rotational symmetry.

[0054] <Second magnetic layer> The second magnetic layer B20 is provided on the second non-magnetic layer A20. The second magnetic layer B20 includes a magnetic material. The second magnetic layer M20 may include a ferromagnetic material. The second magnetic layer B20 functions as a reference layer of the MTJ element. The second magnetic layer B20 may include, for example, CoFeB as a material. Therefore, the second magnetic layer B20 may include a cubic crystal system. Note that the second magnetic layer B20 is not limited to including CoFeB as a material as long as it functions as a reference layer of the MTJ element and includes a crystal structure with four-fold rotational symmetry.

[0055] <Laminated structure> The magnetoresistance element 1 of this embodiment may include, for example, an SOT-MRAM element. In the magnetoresistance element 1, a metal oxide layer (metal oxide) 30 and a first nonmagnetic layer (amorphous) A10 are disposed between an SOT electrode layer 20 and a first magnetic layer (recording layer) B10. The metal oxide layer (metal oxide) 30 includes, for example, a metal oxide layer having a long spin diffusion length. The first nonmagnetic layer (amorphous) A10 includes an amorphous low-resistance material. As a result, as shown below, the problems of the SOT-MRAM having the SOT electrode layer 20 including BiSb described above can be solved.

[0056] Specifically, the structure of the magnetoresistance element 1 of this embodiment has a laminated structure including, from the bottom, an insulating buffer layer / SOT electrode layer 20 / metal oxide layer (metal oxide) 30 / first nonmagnetic layer (amorphous) A10 / first magnetic layer (recording layer) B10 / second nonmagnetic layer A20 / second magnetic layer B20 on an underlayer 10 including an interlayer insulating film such as silicon oxide. The magnetoresistance element 1 having such a structure is formed by laminating layers, for example, in a sputtering film forming apparatus, and patterning the MTJ element. The patterning may be performed on the MTJ element and the first nonmagnetic layer (amorphous) A10.

[0057] BiSb contained in the SOT electrode layer 20 and Cr contained in the metal oxide layer (metal oxide) 30 2 O 3 It is known that a stacked body constituting an MTJ element has three-fold rotational symmetry as a priority. On the other hand, when the stacked body constituting the MTJ element has four-fold rotational symmetry, good MTJ element characteristics can be obtained. That is, the layer in contact with the upper surface of the first non-magnetic layer (amorphous) A10 and the layer in contact with the lower surface of the first non-magnetic layer (amorphous) A10 have different crystal structures. If an MTJ element with four-fold rotational symmetry is formed directly on a layer with three-fold rotational symmetry, the first magnetic layer (recording layer) B10 at the bottom will be affected by the layer with three-fold rotational symmetry and will be deteriorated.

[0058] In contrast, the magnetoresistance element 1 of this embodiment is made of Cr 2 O 3A first non-magnetic layer (amorphous) A10 is inserted between a metal oxide layer (metal oxide) 30 including three-fold rotational symmetry such as CoFeB and a first magnetic layer (recording layer) B10 including four-fold rotational symmetry such as CoFeB. Thus, the metal oxide layer (metal oxide) 30 with three-fold rotational symmetry and the first magnetic layer (recording layer) B10 with four-fold rotational symmetry are separated from each other above and below. This allows the metal oxide layer (metal oxide) 30 and the first magnetic layer (recording layer) B10 to fully exhibit their respective characteristics.

[0059] The element structure of the magnetoresistance element 1 having the SOT electrode layer 20 containing BiSb is 2 O 3 The effect of using a laminate of a metal oxide layer (metal oxide) 30 containing Ta and a first nonmagnetic layer (amorphous) A10 containing Ta will be experimentally clarified below. For example, a magnetoresistance element 1 having the following laminate structure is produced. Here, the numbers in parentheses indicate the thickness of each layer.

[0060] [Sample I] Sapphire substrate / BiSb (10 nm) / CrOx (1.0 nm) / Ta (0.8 nm) / CoFeB (0.9 nm) / MgO (2.0 nm) / Ta (2.0 nm) layered structure

[0061] When such a sample was annealed at 250° C. for 60 minutes, a perpendicular magnetic anisotropy of about 1.7 kOe was obtained as the anisotropy field Hk.

[0062] Furthermore, when the spin Hall angle of the magnetoresistance element 1 was measured using the second harmonic Hall measurement method, the magnetoresistance element 1 of this embodiment was able to obtain a value of 2.8, which is approximately one order of magnitude larger than when heavy metals such as W or Ta are used for the SOT electrode layer.

[0063] Subsequent experiments investigating the thickness dependence of CrOx (using a different method of forming BiSb) showed that increasing the thickness of CrOx from 1.0 nm to 2.5 nm reduced the spin Hall angle from 2.5 to 1.2. In other words, the optimal thickness of the metal oxide film, CrOx, is about 1 nm. For example, the thickness of CrOx is preferably 1 nm. Thus, when the metal oxide layer (metal oxide) 30 is Cr 2 O 3 When the magnetoresistance element 1 contains Cr, the magnetic properties of the magnetoresistance element 1 can be significantly improved. 2 O 3 When the thickness of the metal oxide layer (metal oxide) 30 containing the metal oxide is 1.0 to 1.1 nm, the magnetic properties can be improved more significantly.

[0064] The spin diffusion length of non-magnetic CrOx is thought to be several nm or longer. However, at present, it is thought that spin decay occurs with an increase in film thickness of 1 nm or more.

[0065] When the thickness of Ta, which is an amorphous metal, is increased to 0.8 nm or more, a significant decrease in the spin Hall angle is observed. In the case of Ta, which has a large atomic weight and a large spin-orbit interaction, it is considered that the spin diffusion length is further shortened even though it is a non-magnetic metal. Therefore, the thickness of the first non-magnetic layer (amorphous) A10 is preferably 1 nm or less. The thickness of the first non-magnetic layer A10 is preferably 0.8 to 1.0 nm.

[0066] The metal oxide layer (metal oxide) 30, as an antiferromagnetic oxide film, has a very long spin diffusion length of about several tens to several hundreds of nm. Therefore, the spin current generated in the SOT electrode layer 20 containing BiSb can be transmitted to the first magnetic layer (recording layer) B10 with almost no attenuation. As a result, the magnetoresistance element 1 can provide a large SOT to the first magnetic layer (recording layer) B10, thereby improving the magnetic characteristics.

[0067] Furthermore, the metal oxide layer (metal oxide) 30 has the effect of mitigating surface roughness of the SOT electrode layer 20 containing BiSb, which is difficult to flatten by sputtering deposition, and of flattening the first magnetic layer (recording layer) B10 on the SOT electrode layer 20. That is, by inserting a laminate of the metal oxide layer (metal oxide) 30 / first non-magnetic layer (amorphous) A10 between the SOT electrode layer 20 and the first magnetic layer (recording layer) B10, it is possible to reduce spin diffusion loss caused by the interface between the SOT electrode layer 20 / first magnetic layer (recording layer) B10 and obtain a large spin Hall angle.

[0068] Furthermore, the metal oxide layer (metal oxide) 30 acts as an element diffusion barrier between the SOT electrode layer 20 and the first magnetic layer (recording layer) B10, and can suppress the interdiffusion described above. This diffusion barrier is stable even during high-temperature annealing, so it can suppress not only interdiffusion during film formation, but also interdiffusion during high-temperature annealing for improving magnetic properties. Due to the flattening effect of the first magnetic layer (recording layer) B10 and the suppression effect of interdiffusion, the magnetoresistance element 1 of this embodiment can obtain the magnetic properties such as the good perpendicular magnetic anisotropy described above.

[0069] Also, Cr 2 O 3 Since BiSb is an insulator with a band gap of about 3.2 eV, it is possible to suppress the shunting of the switching current from the SOT electrode layer 20 containing BiSb to the first magnetic layer (recording layer) B10. As a result, the magnetoresistance element 1 of this embodiment can confine the switching current within the SOT electrode layer 20 containing BiSb, and can perform more efficient SOT switching.

[0070] Another effect of inserting the metal oxide layer (metal oxide) 30 / first non-magnetic layer (amorphous) A10 stack is that the first non-magnetic layer (amorphous) A10 improves the wettability of the metal film formed on the metal oxide layer (metal oxide) 30, enabling flat film formation. Furthermore, the amorphous metal of Ta absorbs B of the adjacent CoFeB and promotes the crystallization of CoFeB, thereby improving the magnetic properties of the MTJ element including CoFeB / MgO / CoFeB.

[0071] In order to perform switching with low current consumption in SOT-MRAM, it is necessary to select a material for the SOT electrode layer 20 that can obtain a large spin Hall angle. The SOT electrode layer 20 containing BiSb can obtain a much larger spin Hall angle than SOT electrode layers containing heavy metals, but has problems that hinder practical use, such as surface roughness due to sputtering deposition and interdiffusion.

[0072] In contrast, the magnetoresistance element 1 of this embodiment has a metal oxide layer (metal oxide) 30, which has a sufficiently long spin diffusion length and also functions as a diffusion barrier, inserted between the SOT electrode layer 20 containing BiSb and the first magnetic layer (recording layer) B10. Furthermore, the magnetoresistance element 1 of this embodiment separates the crystal structures of the upper and lower layers with the first nonmagnetic layer (amorphous) A10. This makes it possible to eliminate factors that cause deterioration of the SOT switching characteristics, thereby improving the magnetic characteristics including the switching characteristics.

[0073] (Variation 1) 1 and 2, the magnetoresistance element 1 has a BiSb bottom structure in which the SOT electrode layer 20 containing BiSb is located on the lower side. However, the magnetoresistance element 1 may have a BiSb top structure in which the entire structure is inverted upside down and the SOT electrode layer 20 is located on the upper side.

[0074] Fig. 3 is a cross-sectional view illustrating a magnetoresistance element 1a according to a modified example of the first embodiment. As shown in Fig. 3, the magnetoresistance element 1a may include, from the bottom, a second magnetic layer B20, a second non-magnetic layer A20, a first magnetic layer (recording layer) B10, a first non-magnetic layer (amorphous) A10, a metal oxide layer (metal oxide) 30, and an SOT electrode layer 20. The magnetoresistance element 1a may be formed from the bottom in this order. With such a structure, the same effect as the magnetoresistance element 1 described above can be obtained.

[0075] (Embodiment 2) Next, a magnetoresistance element according to the second embodiment will be described. FIG. 4 is a cross-sectional view illustrating a magnetoresistance element 2 according to the second embodiment. As shown in FIG. 4, the magnetoresistance element 2 of this embodiment further includes a third magnetic layer B30 in addition to the configuration of the magnetoresistance element 1 of the first embodiment. The third magnetic layer B30 is called a third magnetic layer (magnetic layer) B30. The third magnetic layer (magnetic layer) B30 is provided between a metal oxide layer (metal oxide) 30 and a first non-magnetic layer (amorphous) A10. In other words, for example, the metal oxide layer (metal oxide) 30 / third magnetic layer (magnetic layer) B30 / first non-magnetic layer (amorphous) A10 are inserted between the SOT electrode layer 20 containing BiSb and the first magnetic layer (recording layer) B10 containing CoFeB.

[0076] <Third magnetic layer> The third magnetic layer (magnetic layer) B30 is provided on the metal oxide layer (metal oxide) 30. Therefore, the first non-magnetic layer (amorphous) A10 is provided on the third magnetic layer (magnetic layer) B30. Therefore, the third magnetic layer (magnetic layer) B30 is disposed between the metal oxide layer (metal oxide) 30 and the first non-magnetic layer (amorphous) A10.

[0077] The third magnetic layer (magnetic layer) B30 includes a magnetic material. The third magnetic layer (magnetic layer) B30 may include a ferromagnetic material. The third magnetic layer (magnetic layer) B30 is magnetically coupled to the first magnetic layer (recording layer) B10. As a result, the first magnetic layer (recording layer) B10 and the third magnetic layer (magnetic layer) B30 function as a recording layer of the MTJ element as a whole. The third magnetic layer (magnetic layer) B30 may include, for example, Co as a material. Therefore, the third magnetic layer (magnetic layer) B30 may include three-fold rotational symmetry of a hexagonal system. Note that the third magnetic layer (magnetic layer) B30 may include, as a material, Co-Pt alloy, etc., as long as it is a magnetic layer including three-fold rotational symmetry.

[0078] <Laminated structure> The structure of the magnetoresistance element 2 of this embodiment is a laminated structure including, from the bottom, an insulating buffer layer / SOT electrode layer 20 / metal oxide layer (metal oxide) 30 / third magnetic layer (magnetic layer) B30 / first non-magnetic layer (amorphous) A10 / first magnetic layer (recording layer) B10 / second non-magnetic layer A20 / second magnetic layer B20 on an underlayer 10 including an interlayer insulating film such as silicon oxide. The magnetoresistance element 2 having such a structure is laminated in a sputtering film forming apparatus and formed by patterning the MTJ element portion. The patterning may be performed on the MTJ element portion, the first non-magnetic layer (amorphous) A10, and the third magnetic layer (magnetic layer) B30.

[0079] In the structure of the magnetoresistance element 2, the layers above and below the first non-magnetic layer (amorphous) A10 also have different crystal systems. For example, a third magnetic layer (magnetic layer) B30 having three-fold rotational symmetry is disposed on the lower surface of the first non-magnetic layer (amorphous) A10. The layers above and below the first non-magnetic layer (amorphous) A10 can each have an optimal crystal structure suited to their function. This allows the magnetoresistance element 2 to have improved magnetic properties.

[0080] The magnetoresistance element 2 of this embodiment has the following features that are different from the magnetoresistance element 1 described above. That is, the third magnetic layer (magnetic layer) B30 on the metal oxide layer (metal oxide) 30 is magnetically coupled to the first magnetic layer (recording layer) B10. As a result, the first magnetic layer (recording layer) B10 and the third magnetic layer (magnetic layer) B30 function as a recording layer of the MTJ element as a whole. The magnetically coupled two recording layers can increase the overall volume, thereby improving thermal disturbance resistance.

[0081] In addition, since the interface magnetic anisotropy of the interface between the metal oxide layer (metal oxide) 30 / the third magnetic layer (magnetic layer) B30 can be utilized, the perpendicular magnetic anisotropy of the MTJ element can be improved, and the thermal disturbance resistance can be further improved. Furthermore, the third magnetic layer (magnetic layer) B30, which also has three-fold rotational symmetry, is directly bonded to the layers having three-fold rotational symmetry, such as the SOT electrode layer 20 and the metal oxide layer (metal oxide) 30. This makes it possible to suppress spin loss at the interface. In this way, the magnetoresistance element 2 of this embodiment can further improve the magnetic characteristics.

[0082] (Modification) FIG. 5 is a cross-sectional view illustrating a magnetoresistance element 2a according to a modification of the second embodiment. As shown in FIG. 5, the magnetoresistance element 2a according to the modification may have a BiSb top structure. Specifically, the magnetoresistance element 2a may include, from the bottom, a second magnetic layer B20, a second non-magnetic layer A20, a first magnetic layer (recording layer) B10, a first non-magnetic layer (amorphous) A10, a third magnetic layer (magnetic layer) B30, a metal oxide layer (metal oxide) 30, and an SOT electrode layer 20. The magnetoresistance element 2a may be deposited from the bottom in this order. With such a structure, the same effect as that of the magnetoresistance element 2 of the second embodiment can be obtained.

[0083] (Embodiment 3) Next, a magnetoresistance element according to the third embodiment will be described. FIG. 6 is a cross-sectional view illustrating a magnetoresistance element 3 according to the third embodiment. As shown in FIG. 6, the magnetoresistance element 3 of this embodiment further includes a third nonmagnetic layer A30 in addition to the configuration of the magnetoresistance element 2 of the second embodiment. The third nonmagnetic layer A30 is called a third nonmagnetic layer (crystalline metal) A30. The third nonmagnetic layer (crystalline metal) A30 is provided between a metal oxide layer (metal oxide) 30 and a third magnetic layer (magnetic layer) B30. In other words, the metal oxide layer (metal oxide) 30 / third nonmagnetic layer (crystalline metal) A30 / third magnetic layer (magnetic layer) B30 / first nonmagnetic layer (amorphous) A10 are inserted between the SOT electrode layer 20 containing BiSb and the first magnetic layer (recording layer) B10 containing CoFeB.

[0084] <Third nonmagnetic layer> The third non-magnetic layer (crystalline metal) A30 is provided on the metal oxide layer (metal oxide) 30. Therefore, the third magnetic layer (magnetic layer) B30 is provided on the third non-magnetic layer (crystalline metal) A30. Therefore, the third non-magnetic layer (crystalline metal) A30 is disposed between the metal oxide layer (metal oxide) 30 and the third magnetic layer (magnetic layer) B30.

[0085] The third non-magnetic layer (crystalline metal) A30 may include a non-magnetic material. The third non-magnetic layer (crystalline metal) A30 may include a metal as a material. Specifically, the third non-magnetic layer (crystalline metal) A30 may include a crystalline metal layer. The third non-magnetic layer (crystalline metal) A30 has a crystal structure that alleviates the mismatch of the crystal lattices between the metal oxide layer (metal oxide) 30 and the third magnetic layer (magnetic layer) B30, and functions as a buffer layer that alleviates the mismatch of the crystal lattices. Therefore, the third non-magnetic layer (crystalline metal) A30 can reduce the spin loss in the spin injection from the SOT electrode layer 20 to the third magnetic layer (magnetic layer) B30.

[0086] The trigonal BiSb crystal system having three-fold rotational symmetry has a lattice constant of 4.31 to 4.55 Å. The metal oxide layer (metal oxide) 30 formed on the SOT electrode layer 20 containing BiSb is, for example, Cr 2 O3 is a hexagonal crystal with three-fold rotational symmetry and a lattice constant of 4.96 Å. 2 O 3 Crystals grow on BiSb with a lattice mismatch of about 10%.

[0087] Here, the lattice constant of Co in the hexagonal system with three-fold rotational symmetry is about 2.51 Å, so Cr 2 O 3 If the lattice of the third non-magnetic layer (crystalline metal) A30 is not relaxed, it is believed that the crystals will grow with a double period with a lattice mismatch of about 10%. In order to relax this lattice mismatch, the third non-magnetic layer (crystalline metal) A30 is preferably made of a material that has three-fold rotational symmetry and a lattice constant intermediate between the lattice constant of BiSb and twice the lattice constant of Co. Therefore, the third non-magnetic layer (crystalline metal) A30 is preferably made of such a material as TiCr. 2 It may contain TiCr 2 is an intermetallic compound having a hexagonal three-fold rotational symmetry and a lattice constant of about 4.84 Å. The third nonmagnetic layer (crystalline metal) A30 is made of a material having a three-fold rotational symmetry crystal structure and a lattice constant intermediate between the lattice constant of BiSb and twice the lattice constant of Co, such as TiCr 2 Not limited to those including.

[0088] Here, it is considered that the insertion of the third non-magnetic layer (crystalline metal) A30 may cause the bond between the third magnetic layer (magnetic layer) B30 and the metal oxide layer (metal oxide) 30 to be lost. For this reason, there is concern that the magnetic anisotropy utilizing the interface magnetic anisotropy between the third magnetic layer (magnetic layer) B30 and the metal oxide layer (metal oxide) 30 may be reduced. In this case, a Pt layer is inserted under the third magnetic layer (magnetic layer) B30. Alternatively, a Co 3 In this way, if the third magnetic layer (magnetic layer) B30 is made of a Co-Pt alloy having three-fold rotational symmetry and bulk perpendicular magnetic anisotropy, the perpendicular magnetic anisotropy can be increased.

[0089] The main effect of the third non-magnetic layer (crystalline metal) A30 in this embodiment is to function as a buffer layer that reduces lattice mismatch. However, the third non-magnetic layer (crystalline metal) A30 also has the effect of improving the wettability of the third magnetic layer (magnetic layer) B30 formed on the metal oxide layer (metal oxide) 30.

[0090] For example, it is known that Co contained in the third magnetic layer (magnetic layer) B30 generally has a large surface energy and a low wettability when formed on an oxide film. In this case, if at least one metal with good wettability, such as Cr or Ti, is formed as a thin film of 1 nm or less, and then Co is formed, the Co film can be formed flat. Therefore, in order to realize such film formation, it is preferable that the thickness of the third non-magnetic layer (crystalline metal) is greater than 0 nm and less than 1.0 nm. In this way, the magnetoresistance element 3 further includes a third non-magnetic layer (crystalline metal) A30 provided between the metal oxide layer (metal oxide) 30 and the third magnetic layer (magnetic layer) B30. The surface energy of the third magnetic layer (magnetic layer) B30 formed on the third non-magnetic layer (crystalline metal) is smaller than the surface energy of the third magnetic layer (magnetic layer) B30 when formed on the metal oxide layer (metal oxide) 30. Therefore, the third magnetic layer (magnetic layer) B30 formed on the third non-magnetic layer (crystalline metal) is prevented from growing in an island shape, and the flatness is improved.

[0091] In this case, the thin film of Cr and Ti is Cr 2 O 3 Since the crystal system and lattice constant are different from those of the metal oxide layer (metal oxide) 30 containing Co, it may not show a clear orientation. However, even if the crystallinity of the third magnetic layer (magnetic layer) B30 containing Co is reduced due to this, the magnetization can be reversed by the spin current injected from the SOT electrode layer 20 containing BiSb.

[0092] <Laminated structure> The structure of the magnetoresistance element 3 of this embodiment is a laminated structure including, from the bottom, an insulating buffer layer / SOT electrode layer 20 / metal oxide layer (metal oxide) 30 / third non-magnetic layer (crystalline metal) A30 / third magnetic layer (magnetic layer) B30 / first non-magnetic layer (amorphous) A10 / first magnetic layer (recording layer) B10 / second non-magnetic layer A20 / second magnetic layer B20 on an underlayer 10 including an interlayer insulating film such as silicon oxide. The magnetoresistance element 3 having such a structure is laminated in a sputtering film forming apparatus and formed by patterning the MTJ element portion. Patterning may be performed on the MTJ element portion, the first non-magnetic layer (amorphous) A10, the third magnetic layer (magnetic layer) B30, and the third non-magnetic layer (crystalline metal) A30.

[0093] In the structure of the magnetoresistance element 3, the layers above and below the first non-magnetic layer (amorphous) A10 also have different crystal systems. The layers above and below the first non-magnetic layer (amorphous) A10 can each have an optimal crystal structure suited to their respective functions. This allows the magnetoresistance element 3 to have improved magnetic properties.

[0094] The magnetoresistance element 3 of this embodiment has the following features that are different from the above-mentioned magnetoresistance element 2. That is, the third nonmagnetic layer (crystalline metal) A30 is a buffer layer for alleviating the difference in crystal structure and lattice mismatch between the metal oxide layer (metal oxide) 30 and the third magnetic layer (magnetic layer) B30, and therefore can reduce spin loss during spin injection from the SOT electrode layer 20 to the third magnetic layer (magnetic layer) B30. As a result, the magnetic characteristics of the magnetoresistance element 3 can be improved by the configuration of this embodiment as well.

[0095] (Modification) FIG. 7 is a cross-sectional view illustrating a magnetoresistance element 3a according to a modification of the third embodiment. As shown in FIG. 7, the magnetoresistance element 3a according to the modification has a BiSb top structure. Specifically, the magnetoresistance element 3a may include, from the bottom, a second magnetic layer B20, a second non-magnetic layer A20, a first magnetic layer (recording layer) B10, a first non-magnetic layer (amorphous) A10, a third magnetic layer (magnetic layer) B30, a third non-magnetic layer (crystalline metal) A30, a metal oxide layer (metal oxide) 30, and an SOT electrode layer 20. The magnetoresistance element 3a may be deposited from the bottom in this order. With such a structure, the same effect as that of the magnetoresistance element 3 of the third embodiment can be obtained.

[0096] (Embodiment 4) Next, a magnetoresistance element according to the fourth embodiment will be described. FIG. 8 is a cross-sectional view illustrating a magnetoresistance element 4 according to the fourth embodiment. As shown in FIG. 8, the magnetoresistance element 4 of this embodiment includes a first metal oxide layer (metal oxide) 40 and a second metal oxide layer (metal oxide) 50 instead of the metal oxide layer (metal oxide) 30 in the magnetoresistance element 2 of the second embodiment. That is, the metal oxide layer (metal oxide) 30 includes the first metal oxide layer (metal oxide) 40 and the second metal oxide layer (metal oxide) 50. The first metal oxide layer (metal oxide) 40 is provided between the SOT electrode layer 20 and the second metal oxide layer (metal oxide) 50. The second metal oxide layer (metal oxide) 50 is provided between the first metal oxide layer (metal oxide) 40 and the third magnetic layer (magnetic layer) B30.

[0097] <First metal oxide layer (metal oxide)> The first metal oxide layer (metal oxide) 40 is provided on the SOT electrode layer 20. The first metal oxide layer (metal oxide) 40 may have the same function as the metal oxide layer (metal oxide) 30. The first metal oxide layer (metal oxide) 40 may have the same material and crystal structure as the metal oxide layer 30 (metal oxide). That is, the first metal oxide layer (metal oxide) 40 may contain a metal oxide as a material. The first metal oxide layer (metal oxide) 40 may contain a metal oxide with three-fold rotational symmetry. For example, the first metal oxide layer (metal oxide) 40 may contain, as a material, Cr. 2 O 3 The first metal oxide layer (metal oxide) 40 may include a metal oxide different from that of the second metal oxide layer (metal oxide) 50, and is not limited to a material including the same material and crystal structure as the metal oxide layer 30 (metal oxide).

[0098] <Second metal oxide layer (metal oxide)> The second metal oxide layer (metal oxide) 50 is provided on the first metal oxide layer (metal oxide) 40. Therefore, the third magnetic layer (magnetic layer) B30 is provided on the second metal oxide layer (metal oxide) 50.

[0099] The second metal oxide layer (metal oxide) 50 preferably contains a material that induces high interface magnetic anisotropy at the interface with the third magnetic layer (magnetic layer) B30. Such a material may be, for example, an amorphous oxide or may be selected from many oxides such as polycrystalline oxides. The method for forming the second metal oxide layer (metal oxide) 50 may be selected from a wide range of techniques such as natural oxidation, plasma oxidation, and direct sputtering of oxide.

[0100] The second metal oxide layer (metal oxide) 50 may contain at least one of aluminum oxide, tantalum oxide, magnesium oxide, ruthenium oxide, hafnium oxide, and chromium oxide as a material. By containing such a material, it is possible to have the effect of inducing high interface magnetic anisotropy.

[0101] Furthermore, the second metal oxide layer (metal oxide) 50 can perform more effective spin injection by matching the crystal system and lattice constant between the third magnetic layer (magnetic layer) B30 having three-fold rotational symmetry and the first metal oxide layer (metal oxide) 40 having three-fold rotational symmetry. However, as in the above case, even if the second metal oxide layer (metal oxide) 50 contains an amorphous phase or has a different crystal system from the third magnetic layer (magnetic layer) B30 and the first metal oxide layer (metal oxide) 40, the magnetization of the second metal oxide layer (metal oxide) 50 can be reversed as a magnetic layer by the spin current injected from the SOT electrode layer 20.

[0102] <Laminated structure> The structure of the magnetoresistance element 4 of this embodiment is a laminated structure including, from the bottom, an insulating buffer layer / SOT electrode layer 20 / first metal oxide layer (metal oxide) 40 / second metal oxide layer (metal oxide) 50 / third magnetic layer (magnetic layer) B30 / first non-magnetic layer (amorphous) A10 / first magnetic layer (recording layer) B10 / second non-magnetic layer A20 / second magnetic layer B20 on an underlayer 10 including an interlayer insulating film such as silicon oxide. The magnetoresistance element 4 having such a structure is laminated in a sputtering film forming apparatus and formed by patterning the MTJ element. Patterning may be performed on the MTJ element, the first non-magnetic layer (amorphous) A10, and the third magnetic layer (magnetic layer) B30.

[0103] In the structure of the magnetoresistance element 4, the layers above and below the first non-magnetic layer (amorphous) A10 also have different crystal systems. The layers above and below the first non-magnetic layer (amorphous) A10 can each have an optimal crystal structure suited to their respective functions. This allows the magnetoresistance element 4 to have improved magnetic properties.

[0104] In the magnetoresistance element 4 of this embodiment, the first metal oxide layer (metal oxide) 40 and the second metal oxide layer (metal oxide) 50 have different functions. For example, the first metal oxide layer (metal oxide) 40 contains a material that increases the efficiency of spin injection from the SOT electrode layer 20, including BiSb. Furthermore, the first metal oxide layer (metal oxide) 40 is made of a material that does not easily oxidize BiSb during film formation. On the other hand, the second metal oxide layer (metal oxide) 50 is made of a material that induces high interface magnetic anisotropy at the interface with the third magnetic layer (magnetic layer) B30. As a result, the magnetoresistance element 4 of this embodiment can improve its magnetic characteristics.

[0105] (Modification) FIG. 9 is a cross-sectional view illustrating a magnetoresistance element 4a according to a modification of the fourth embodiment. As shown in FIG. 8, the magnetoresistance element 4a according to the modification may have a BiSb top structure. Specifically, the magnetoresistance element 4a may include, from the bottom, a second magnetic layer B20, a second non-magnetic layer A20, a first magnetic layer (recording layer) B10, a first non-magnetic layer (amorphous) A10, a third magnetic layer (magnetic layer) B30, a second metal oxide layer (metal oxide) 50, a first metal oxide layer (metal oxide) 40, and an SOT electrode layer 20. The magnetoresistance element 4a may be deposited from the bottom in this order. With such a structure, the same effect as that of the magnetoresistance element 4 of the fourth embodiment described above can be obtained.

[0106] (Embodiment 5) Next, a fifth embodiment will be described. This embodiment is a semiconductor device including any one of the magnetoresistance elements 1 to 4. Figs. 10 and 11 are circuit diagrams illustrating a semiconductor device 5 according to the fifth embodiment. As shown in Figs. 10 and 11, the semiconductor device 5 of this embodiment may include a magnetic memory MM or may include a memory cell MC.

[0107] As shown in FIG. 10, the magnetic memory MM includes a memory cell array 100 in which memory cells MC are arranged in an array, two word lines WL1 and WL2 arranged corresponding to the memory cells MC arranged in the same column direction, three bit lines BL1, BL2, and BL3 arranged corresponding to the memory cells MC arranged in the same row direction, a word line selection circuit 110, bit line selection circuits 12a and 12b, write circuits 13a and 13b, and read circuits 14a and 14b.

[0108] 11, each memory cell MC includes any one of the above-mentioned magnetoresistance elements 1 to 4 and 1a to 4a, and transistors TR1 and TR2. Here, an example in which the magnetoresistance element 1 is used will be described.

[0109] In the memory cell MC, the second magnetic layer B20 of the magnetoresistance element 1 is connected to one of the source and drain of the transistor TR1. The other of the source and drain of the transistor TR1 is connected to the bit line BL1, and the gate is connected to the word line WL1. One end of the SOT electrode layer 20 is connected to one of the source and drain of the transistor TR2, and the other end is connected to the bit line BL3. The other of the source and drain of the transistor TR2 is connected to the bit line BL2, and the gate is connected to the word line WL2.

[0110] (Write operation) Next, writing to a memory cell MC will be described. First, the word line selection circuit 110 applies a high level potential to the word line WL2 to which the gate of the transistor TR2 of the memory cell MC to be written is connected so that the transistor TR2 of the memory cell MC to be written is turned on. At this time, the transistors TR2 of the other memory cells MC in the column to which the memory cell MC belongs are also turned on. However, a low level potential is applied to the word line WL1 connected to the gate of the transistor TR1 in the memory cell MC and the word lines WL1 and WL2 corresponding to the other columns.

[0111] Next, the bit lines BL2 and BL3 connected to the memory cell MC to be written are selected by the bit line selection circuits 12a and 12b. Then, the write circuits 13a and 13b pass a write current from one of the bit line selection circuits 12a and 12b to the other of the selected bit lines BL2 and BL3. This write current allows the magnetization direction of the first magnetic layer (recording layer) B10 of the magnetoresistance element 1 to be reversed, and writing is performed. If a write current is passed from the other of the bit line selection circuits 12a and 12b to one, the magnetization direction of the first magnetic layer (recording layer) B10 of the magnetoresistance element 1 becomes reversible in the opposite direction to that described above, and writing is performed.

[0112] (Read operation) Next, the read operation from the memory cell MC will be described. First, a high-level potential is applied to the word line WL1 connected to the memory cell MC to be read, and the transistor TR1 in the memory cell MC is turned on. At this time, the transistors TR1 in the other memory cells MC in the column to which the memory cell MC belongs are also turned on. However, a low-level potential is applied to the word line WL2 connected to the gate of the transistor TR2 in the memory cell MC and the word lines WL1 and WL2 corresponding to the other columns.

[0113] Then, the bit lines BL1 and BL3 connected to the memory cell MC to be read are selected by the bit line selection circuits 12a and 12b. Then, the read circuits 14a and 14b pass a read current from one of the bit line selection circuits 12a and 12b to the other of the selected bit lines BL1 and BL3. At this time, for example, by detecting the voltage between the selected bit lines BL1 and BL3 by the read circuits 14a and 14b, it can be detected whether the magnetization directions between the first magnetic layer (recording layer) B10 and the second magnetic layer (reference layer) B20 of the magnetoresistance element 1 are parallel (same direction) or antiparallel (opposite directions). That is, reading can be performed.

[0114] The semiconductor device 5 of this embodiment includes the above-mentioned magnetoresistance element 1, and therefore can improve the magnetic characteristics and the write and read operations.

[0115] The present disclosure is not limited to the above-described embodiments, and can be modified as appropriate without departing from the spirit and scope of the present disclosure. For example, combinations of the configurations of the first to fifth embodiments are also within the scope of the technical concept of the present invention. [Explanation of symbols]

[0116] 1, 1a, 2, 2a, 3, 3a, 4, 4a Magnetoresistance element 5. Semiconductor Devices 10 Base layer 12a, 12b Bit line selection circuit 13a, 13b Write circuit 14a, 14b Readout circuit 20 SOT electrode layer 30 Metal oxide layer 40 First metal oxide layer 50 Second metal oxide layer 100 Memory Cell Array 110 Word line selection circuit A10 1st nonmagnetic layer A20 Second non-magnetic layer A30 Third non-magnetic layer B10 1st magnetic layer B20 2nd magnetic layer B30 3rd magnetic layer BL1, BL2, BL3 bit lines MC memory cell MM Magnetic Memory WL1, WL2 word lines

Claims

1. A SOT electrode layer; a metal oxide layer provided on the SOT electrode layer; a first nonmagnetic layer provided on the metal oxide layer; a first magnetic layer provided on the first nonmagnetic layer; a second non-magnetic layer provided on the first magnetic layer; a second magnetic layer provided on the second nonmagnetic layer; Equipped with The first magnetic layer, the second nonmagnetic layer, and the second magnetic layer are forming a magnetic tunnel junction element; The SOT electrode layer is The material includes BiSb, The metal oxide layer is The material includes a metal oxide, The first nonmagnetic layer is At least a portion of the amorphous phase is included, The crystals included in the SOT electrode layer and the crystals included in the first magnetic layer are The rotational symmetry of the crystals around the stacking direction of these layers is different. Magnetoresistance element.

2. A layer formed between the metal oxide layer and the first nonmagnetic layer Third magnetic layer Further equipped with The third magnetic layer is magnetically coupled to the first magnetic layer; The method according to claim 1 Magnetoresistance element.

3. A layer is provided between the metal oxide layer and the third magnetic layer. Further comprising a third non-magnetic layer; The third nonmagnetic layer is having a crystal structure that reduces mismatch between the crystal lattices of the metal oxide layer and the third magnetic layer; The method according to claim 2 Magnetoresistance element.

4. A layer is provided between the metal oxide layer and the third magnetic layer. Further comprising a third non-magnetic layer; The third magnetic layer formed on the third nonmagnetic layer is Island growth is suppressed, The flatness is improved, The method according to claim 2 Magnetoresistance element.

5. The metal oxide layer is a first metal oxide layer and a second metal oxide layer; The first metal oxide layer is The material includes a metal oxide different from that of the second metal oxide layer. The method according to claim 2 Magnetoresistance element.

6. The metal oxide layer is The spin diffusion length is longer than the distance between the SOT electrode layer and the first magnetic layer. The metal oxide is included. The method according to claim 1 Magnetoresistance element.

7. the first magnetic layer includes the crystals having four-fold rotational symmetry; The SOT electrode layer includes the crystal having three-fold rotational symmetry. The method according to claim 1 Magnetoresistance element.

8. The metal oxide layer is made of Cr. 2 O 3 Including, The method according to claim 1 Magnetoresistance element.

9. The thickness of the metal oxide layer is 0.5 to 2.5 nm. The method according to claim 8 . Magnetoresistance element.

10. the first nonmagnetic layer at least partially contains an amorphous metal; The method according to claim 1 Magnetoresistance element.

11. the first nonmagnetic layer includes, as a material, at least one of a simple transition metal, an alloy of transition metals, a compound of a transition metal and a metalloid, a transition metal nitride, a transition metal oxide, and a B-C-N based material; The method according to claim 1 Magnetoresistance element.

12. The first nonmagnetic layer has a thickness of 0.8 to 1.0 nm. The method according to claim 10 Magnetoresistance element.

13. The third magnetic layer contains at least one of Co and a Co-Pt alloy as a material. The method according to claim 2 Magnetoresistance element.

14. the third magnetic layer includes the crystals having three-fold rotational symmetry with the lamination direction as the rotation axis; The method according to claim 2 Magnetoresistance element.

15. the third nonmagnetic layer contains a metal as a material; The method according to claim 3 Magnetoresistance element.

16. The third nonmagnetic layer is made of TiCr. 2 Including, The method according to claim 3 Magnetoresistance element.

17. The thickness of the third nonmagnetic layer is greater than 0 nm and is equal to or less than 1.0 nm.

16. The method of claim 15 Magnetoresistance element.

18. the third nonmagnetic layer includes the crystals having three-fold rotational symmetry with the lamination direction as the rotation axis; The method according to claim 3 Magnetoresistance element.

19. The first metal oxide layer is made of Cr. 2 O 3 Including, The second metal oxide layer contains at least one of aluminum oxide, tantalum oxide, magnesium oxide, ruthenium oxide, hafnium oxide, and chromium oxide as a material. The method according to claim 5 Magnetoresistance element.

20. Further comprising a base layer; The SOT electrode layer is provided on the underlayer. The method according to claim 1 Magnetoresistance element.

21. A magnetic resistance element according to any one of claims 1 to 20 is provided. Semiconductor device.

Citation Information

Patent Citations

  • Piezoelectric device

    JP2019054484A

  • Magnetoresistive memory

    JP2021057357A

  • Sot (spin orbit torque) MTJ (magnetic tunnel junction) device, mamr (microwave-assisted magnetic recording) write head, MRAM (magnetoresistive random access memory) device