Manufacturing method for parison for balloon catheter, manufacturing method for balloon catheter, and manufacturing device for parison for balloon catheter
The method stabilizes parison formation by using close-proximity heating and controlled cooling in the manufacturing process, addressing heating inconsistencies and ensuring consistent balloon shape in balloon catheters.
Patent Information
- Application Number
- JP2023078675
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-11
- Publication Date
- 2024-11-21
AI Technical Summary
Existing methods for manufacturing a parison for a balloon catheter face instability in heating due to distance between the heating surface and the tube, leading to inconsistent balloon shape formation.
A method involving a pair of thermoplastic tubes fixed in a fixing region with a heat source close to the surface, heated through radiant and convective heat transfer, and stretched to form a large diameter portion, using a thermal mold with minimal distance for efficient heating and cooling to stabilize the shape.
The method ensures stable and efficient heating and shaping of the parison, allowing for consistent balloon formation with controlled temperature differences, resulting in a balloon catheter with a stable shape.
Smart Images

Figure 2024162783000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a parison, which is an intermediate product in the manufacture of a balloon of a balloon catheter, a method for manufacturing a balloon catheter, and an apparatus for manufacturing a parison for a balloon catheter. [Background technology]
[0002] Balloon catheters are widely used to treat lesions (stenosis) that occur in biological lumens. A balloon catheter usually has a long shaft and a balloon that is provided at the tip of the shaft and can expand in the radial direction. The balloon is contracted and reaches a target location inside the body via a narrow biological lumen, and then expanded to expand the lesion.
[0003] The main components of a balloon catheter are the balloon and the shaft, as mentioned above. A balloon is formed by processing a tube formed by extrusion molding or the like into an intermediate product called a parison, and then biaxially stretching the parison in the radial and axial directions to finally form the balloon. The formed balloon is attached to the shaft and assembled. The manufacturing method for processing the tube, via the parison, into a balloon is disclosed in Patent Document 1. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. 2014 / 141382 Summary of the Invention [Problem to be solved by the invention]
[0005] The processing from a tube to a parison is performed by stretching a part of the tube in the longitudinal direction on both sides of the part to be processed into a balloon, while maintaining the original diameter of the part in the longitudinal direction. The part of the parison stretched in the longitudinal direction of the tube is oriented and has high strength. Therefore, when the parison is biaxially stretched, the part of the tube stretched in the longitudinal direction does not expand, and only the part of the tube that maintains its original diameter expands to form a balloon.
[0006] When producing a parison, both longitudinal sides of the tube to be processed into a balloon are heated and stretched in the longitudinal direction. The tube is heated by arranging the portion to be heated so that it is surrounded by the heating surface of a heating means having a space inside. However, since the heating surface of the heating means and the tube are separated from each other, the heating of the tube may become unstable. In addition, in order to keep the space between the heating surface of the heating means and the tube at an appropriate temperature, the temperature of the heating surface needs to be increased, so that the unheated parts of the tube are heated, and the shape of the parison formed becomes unstable, which may affect the shape of the balloon formed from the parison.
[0007] The present invention has been made to solve the above-mentioned problems, and has an object to provide a method and an apparatus for manufacturing a parison for a balloon catheter, which can stably form the shape of the parison by lowering the heating temperature of the tube, and a method and an apparatus for manufacturing a parison for a balloon catheter. [Means for solving the problem]
[0008] To achieve the above object, (1) a method for producing a parison for a balloon catheter includes a fixing step of fixing a thermoplastic tube extending along a longitudinal direction at a pair of fixing regions spaced apart in the longitudinal direction, a heating step of heating a pair of heating regions spaced apart in the longitudinal direction of the tube between the pair of fixing regions by bringing a heat source close to a surface of the tube or by bringing a heat source into contact with at least a part of the surface of the tube, and a stretching step of pulling the tube in a direction in which the pair of fixing regions are separated from each other, thereby stretching the pair of heating regions of the tube heated in the heating step, and forming a thick-diameter portion between the pair of heating regions stretched in the stretching step, the outer diameter of which is larger than that of the stretched portion.
[0009] (12) A manufacturing apparatus for a parison for a balloon catheter that achieves the above-mentioned object includes a fixing mechanism that fixes a thermoplastic tube extending along a longitudinal direction at a pair of fixing regions spaced apart in the longitudinal direction, a heating mechanism that heats a surface of the tube by bringing a heat source close to the surface of the tube or by bringing the heat source into contact with at least a part of the surface of the tube in a pair of heating regions that are spaced apart in the longitudinal direction and between the pair of fixing regions of the tube, and a pulling mechanism that moves the fixing mechanism in a direction that increases the distance between the pair of fixing regions of the tube. Effect of the Invention
[0010] In the method for manufacturing a parison for a balloon catheter configured as described above, the heat source is brought into close proximity to or into contact with the surface of the tube in the heating step, so that the tube can be stably heated by a combination of radiant heat and convective heat transfer, or by thermal conduction. Therefore, even if the heating temperature of the heat source is kept low, the tube can be efficiently heated and the shape of the parison can be stably formed.
[0011] (2) In the method for manufacturing a parison for a balloon catheter according to (1) above, in the heating step, the tube may be heated in a hot mold having a space surrounded by a wall surface with a square cross-sectional shape cut in a plane perpendicular to the major axis direction. Thereby, the surface of the hot mold and the surface of the tube can be surely brought close to each other, and heating can be performed efficiently.
[0012] (3) In the method for manufacturing a parison for a balloon catheter according to (2) above, the minimum distance Y between the wall surface and the tube can be set to 0 < Y ≤ 1.5 mm. Thereby, the tube can be efficiently heated by the radiant heat from the surface of the hot mold.
[0013] (4) In the method for manufacturing a parison for a balloon catheter according to (2) or (3) above, in the cross-sectional shape of the wall surface of the hot mold cut in a plane perpendicular to the major axis direction, the wall surface includes a long wall extending in one direction and a short wall extending in a direction different from the long wall and having a length shorter than the long wall, and a plurality of the tubes may be arranged and heated along the direction in which the long wall extends within the space. Thereby, a plurality of tubes can be heated at once, and the production of the parison can be made more efficient.
[0014] (5) In the method for manufacturing a parison for a balloon catheter according to (1) above, in the heating step, the heat source may be brought into contact with the entire circumference of the surface of the tube. Thereby, the tube can be efficiently heated by heat conduction.
[0015] (6) In the method for manufacturing a parison for a balloon catheter according to any one of (1) to (5) above, after the heating step, in the stretching step, a step of separating the heat source brought close to or in contact with the surface of the tube from the surface of the tube may be included. Thereby, the stretching step can be performed without interference from the heat source.
[0016] (7) In the method for producing a parison for a balloon catheter according to any one of (1) to (6) above, in the heating step, the heat source may maintain the surface of the heated region at a temperature higher than the glass transition temperature of the tube, thereby making it possible to reliably stretch the heated region of the tube in the stretching step and increase its strength.
[0017] (8) In the method for producing a parison for a balloon catheter according to any one of (1) to (7) above, a cooling step may be provided between the heating steps, in which at least a part of the region between the pair of heated regions is cooled, thereby making it possible to clearly create a temperature difference between the region between the pair of heated regions in the tube and the heated regions.
[0018] (9) In the method for producing a parison for a balloon catheter according to (8) above, the surface of the region between the pair of heating regions may be maintained at a temperature lower than the glass transition temperature of the tube in the cooling step, thereby suppressing a temperature rise in the portion that will become the large-diameter portion of the tube and enabling the shoulder of the produced parison to be clearly shaped.
[0019] (10) In the method for producing a parison for a balloon catheter according to either (8) or (9) above, the difference between the surface temperature of the tube in the heating step and the surface temperature of the tube in the cooling step can be set to 50° C. or more and 140° C. or less. This allows a sufficient temperature difference to be created between the heating area and the cooling area of the tube, thereby stably forming the shape of the large-diameter portion of the tube.
[0020] (11) A method for producing a balloon catheter includes biaxially stretching the parison for a balloon catheter produced by any one of the production methods (1) to (10) above to form a balloon, and then installing a shaft in the formed balloon. Since the shape of the parison for a balloon catheter is stably formed by any one of the production methods (1) to (10) above, a balloon catheter having a balloon with a stable shape can be produced.
[0021] In the balloon catheter parison manufacturing apparatus configured as described above, the heat source is in close proximity to or in contact with the portion of the tube to be stretched, so the tube can be stably heated by a combination of radiant heat and convective heat transfer, or by thermal conduction. Therefore, even if the heating temperature of the heat source is kept low, the tube can be efficiently heated and the shape of the parison can be stably formed. [Brief description of the drawings]
[0022] [Figure 1] FIG. 2 is an overall front view of the balloon catheter. [Diagram 2] FIG. 2 is an overall front view of the parison. [Diagram 3] FIG. 2 is an enlarged cross-sectional view of the central portion of the parison. [Figure 4] FIG. 2 is a front view of the parison manufacturing apparatus, showing a state in which a tube is fixed to a fixing mechanism portion. [Diagram 5] FIG. 2 is a front view of the parison manufacturing apparatus, showing a state in which the heating mechanism is closed. [Figure 6] FIG. 13 is a cross-sectional view of a thermal mold in an open state with tubes in place. [Figure 7] FIG. 13 is a cross-sectional view of a thermal mold with tubes in a closed state. [Figure 8] FIG. 2 is a front view of the parison manufacturing apparatus, illustrating a state in which a tube is being stretched by a tension mechanism. [Figure 9] 1A is an enlarged cross-sectional view of the vicinity of the center of the parison before biaxial stretching processing, and FIG. 1B is an enlarged cross-sectional view of the vicinity of the center of the parison after biaxial stretching processing. [Figure 10] FIG. 2 is an enlarged cross-sectional view of the vicinity of the balloon with a shaft installed in the manufactured balloon. [Figure 11] FIG. 1 is a cross-sectional view of a thermal mold in which multiple tubes are arranged. [Figure 12] FIG. 13 is a cross-sectional view of a modified thermal mold in which a tube is disposed in an open state. [Figure 13] FIG. 13 is a cross-sectional view of a modified thermal mold in which a tube is disposed in a closed state. [Figure 14] FIG. 13 is a cross-sectional view of a modified thermal mold in which multiple tubes are arranged in a closed state. [Figure 15] FIG. 13 is a cross-sectional view of a thermal mold according to a second modified example in which a tube is arranged in a closed state. [Figure 16] FIG. 2 is a front view of a parison manufacturing apparatus having a cooling mechanism, illustrating a state in which a tube is fixed to the fixing mechanism. [Figure 17] FIG. 13 is a cross-sectional view of a cooling mold with tubes in a closed state. [Figure 18] FIG. 2 is a front view of a parison manufacturing apparatus having a cooling mechanism, illustrating a state in which a tube is being stretched by a tension mechanism. [Figure 19] FIG. 13 is a cross-sectional view of a cooling mold in a closed state according to a modified example in which a tube is arranged. [Figure 20] FIG. 11 is a cross-sectional view of a cooling mold according to a second modified example in which a tube is arranged, in a closed state. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. Note that the dimensional ratios in the drawings may be exaggerated for convenience of explanation and may differ from the actual ratios. In addition, in this specification, the side of the balloon catheter 10 that is inserted into a body lumen is referred to as the "distal end" or "distal side", and the side that is operated by the operator is referred to as the "base end" or "base side".
[0024] In the method for producing a parison for a balloon catheter according to the embodiment of the present invention, a part of a tube 30 made of a thermoplastic material is heated and stretched to produce a parison 20 in which the unheated part of the tube 30 is formed into a large diameter part 21 and the heated part of the tube 30 is formed into a small diameter part 22. A balloon 12 is formed from this parison 20, and the balloon catheter 10 is produced by placing the balloon 12 on the shaft 11.
[0025] 1, the manufactured balloon catheter 10 has a balloon 12 at the tip end of a long shaft 11, and a hub 13 is provided at the base end of the shaft 11. The balloon 12 can be expanded radially by an expansion fluid injected from the hub 13.
[0026] As shown in FIG. 2, the parison 20 extends along the long axis direction, has a large diameter portion 21 in the center in the long axis direction, and has thin diameter portions 22 on both sides of the large diameter portion 21 in the long axis direction, the thin diameter portions 22 having a smaller diameter than the large diameter portion 21.
[0027] 3, the parison 20 is a hollow tube. The large diameter portion 21 of the parison 20 has a same diameter portion 21a having the same diameter along the long axis direction, and an inclined shoulder portion 21b connecting the same diameter portion 21a and the small diameter portion 22 at both ends of the same diameter portion 21a in the long axis direction.
[0028] The parison 20 is made of a thermoplastic material. In this embodiment, the material forming the parison 20 is polyamide. The material forming the parison 20 is not limited to this, and for example, polyolefins such as polyethylene, polypropylene, polybutene, ethylene-propylene copolymer, ethylene-vinyl acetate copolymer, ionomer, or a mixture of two or more of these, and thermoplastic resins such as soft polyvinyl chloride resin, polyamide elastomer, polyester, polyester elastomer, polyurethane, and fluororesin can be used.
[0029] A manufacturing device 50 and a manufacturing method for the parison 20 will be described. As shown in Fig. 4, the manufacturing device 50 for the parison 20 has a fixing mechanism 51 for fixing the tube 30, a heating mechanism 52 for heating the tube 30, a pulling mechanism 53 for moving the fixing mechanism 51 to pull the tube 30 along the longitudinal direction, and a moving mechanism 54 for opening and closing the heating mechanism 52.
[0030] The fixing mechanism 51 fixes the tube 30 extending along the longitudinal direction at a pair of fixing regions 31, 31 spaced apart in the longitudinal direction. The fixing mechanism 51 has a through space through which both ends of the tube 30 can be inserted, and has fixing means for radially pressing and holding the inserted tube 30.
[0031] The heating mechanism 52 can heat a pair of heating regions 32, 32 that are spaced apart in the longitudinal direction between a pair of fixing regions 31 of the tube 30. The heating mechanism 52 is composed of a pair of thermal molds 70, 70 that are heat sources disposed on both radial sides of the tube 30. The thermal molds 70, 70 can be opened and closed by moving them close to and away from each other along the radial direction of the tube 30 by the moving mechanism 54. In FIG. 4, the thermal molds 70, 70 are in an open state in which they are spaced apart from each other to expose the heating region 32 of the tube 30.
[0032] Pulling mechanism 53 has an arm 81 connected to fixing mechanism 51, and a main body 80 that extends and retracts arm 81. By causing main body 80 to extend and retract arm 81, fixing mechanism 51 can be moved along the longitudinal direction of tube 30, and tube 30 fixed to fixing mechanism 51 can be pulled along the longitudinal direction.
[0033] The movement mechanism 54 has an arm 91 connected to the thermal mold 70, and a main body 90 that extends and retracts the arm 91. The main body 90 extends and retracts the arm 91, thereby moving the thermal molds 70, 70 facing each other so as to open and close.
[0034] To manufacture the parison 20, first, the fixing regions 31, 31 of the tube 30 are fixed to the fixing mechanism parts 51, 51 of the manufacturing apparatus 50, respectively, as shown in Fig. 4 (fixing step). Next, as shown in Fig. 5, the moving mechanism part 54 brings the mutually facing thermal molds 70, 70 of the heating mechanism part 52 into a closed state by bringing them close to each other, and the pair of heating regions 32, 32 of the tube 30 are covered and heated by the thermal molds 70, 70 (heating step).
[0035] As shown in Fig. 6, the pair of thermal molds 70, 70 have concave wall surfaces 72, 72 on the surfaces facing each other. The thermal mold 70 also has a heating section 71 inside. A heater can be used as the heating section 71. However, the heating section 71 may be provided on the outer surface of the thermal mold 70, or may be a heating means other than a heater. The heating section 71 heats the thermal mold 70, and the temperature of the wall surfaces 72 can be increased.
[0036] As shown in FIG. 7, the pair of thermal molds 70, 70 are in close proximity to each other in a closed state, thereby accommodating the tube 30 therein. The thermal molds 70, 70 in the closed state have a space 73 surrounded by wall surfaces 72 having a rectangular cross section cut along a plane perpendicular to the long axis direction. The wall surfaces 72 have a long wall 72a extending horizontally in the cross section cut along a plane perpendicular to the long axis direction, and a short wall 72b extending vertically, which is a different direction from the long wall 72a, and having a shorter length than the long wall 72a. The tube 30 disposed in the space 73 formed by the pair of thermal molds 70, 70 is in close proximity to the long wall 72a of the wall surfaces 72. The minimum distance Y between the wall surfaces 72 and the tube 30 is the distance between the long wall 72a and the tube 30, and is 0. <Y≦1.5mmである。
[0037] The temperature of the wall surface 72 is increased by the heating unit 71, and this generates radiant heat from the wall surface 72 and convective heat transfer within the space 73 heated by the wall surface 72, thereby heating the tube 30. The heating of the tube 30 is maintained for a certain period of time. In the heating process, the heat mold 70, which is a heat source, maintains the surfaces of the heating regions 32, 32 at a temperature higher than the glass transition temperature of the tube 30. In this embodiment, the heat mold 70 is heated to a temperature of 80° C. or higher and 160° C. or lower in the heating process. The heating process is performed for 1 second or higher and 30 seconds or shorter.
[0038] Since the wall surface 72 of the thermal mold 70 is close to the tube 30, the tube 30 can be stably heated by a combination of radiant heat and convective heat transfer. Therefore, even if the heating temperature of the thermal mold 70 is kept low, the tube 30 can be efficiently heated. In the heating process, by lowering the heating temperature of the thermal mold 70, so-called accidental heating of areas other than the heating area 32 of the tube 30 can be prevented, so that the temperature rise of the area can be suppressed. This allows the length of the parison 20 to be manufactured to be stably formed. Furthermore, the shape of the shoulder portion 21b of the parison 20 can be clearly formed, making it easier to identify the shape during inspection. Since the shape of the shoulder portion 21b of the parison 20 is clear, it can be determined that the large diameter portion 21 of the parison 20 has not been stretched. From the above, the parison 20 can be stably manufactured.
[0039] After the tube 30 is heated in the heating step, as shown in Fig. 8, the pulling mechanism 53 pulls the tube 30 in a direction in which the pair of fixed regions 31, 31 are separated from each other, and the pair of heated regions 32, 32 heated in the heating step of the tube 30 are stretched (stretching step). During the stretching step, a step is performed in which the moving mechanism 54 opens the thermal mold 70 to separate the thermal mold 70 from the surface of the tube 30. The thermal mold 70 may be opened after the heating step and before the stretching step, or may be opened simultaneously with the start of the stretching step, or may be opened during the stretching step.
[0040] The stretching process stretches the heated region 32 of the tube 30 in the longitudinal direction, and the stretched portion is oriented and strengthened. The stretching process forms a thick-diameter portion 21 having an outer diameter larger than that of the thin-diameter portion 22 between a pair of heated regions 32, 32 that have been stretched to form the thin-diameter portion 22 in the tube 30.
[0041] The balloon 12 is formed by biaxially stretching the large diameter portion 21 of the parison 20 shown in FIG. 9(a) and expanding it as shown in FIG. 9(b). The biaxial stretching of the large diameter portion 21 is performed by blow molding so as to expand the large diameter portion 21 in two axial directions, the longitudinal direction and the radial direction. During the biaxial stretching, only the portion of the large diameter portion 21 of the tube 30 that is not stretched expands, forming the intermediate portion 12c and the distal end portion 12a and the proximal end portion 12b extending before and after it. After the parison 20 is biaxially stretched, both ends in the longitudinal direction are cut so that a predetermined length remains as the distal end portion 12a and the proximal end portion 12b, and the balloon 12 can be obtained. Details of the biaxial stretching process can be appropriately adopted by known methods. The intermediate portion 12c of the balloon 12 has the function of pushing and widening a narrowed portion or the like when it is expanded. The distal end portion 12a and the proximal end portion 12b are liquid-tightly joined to the shaft 11, as described later.
[0042] Once the balloon 12 is formed, a shaft 11 having a hub 13 is placed on the formed balloon 12. Specifically, as shown in Fig. 10, an inner tube shaft 11a is fixed to a tip end 12a of the balloon 12 by a known method such as fusion, an outer tube shaft 11b disposed outside the inner tube shaft 11a is fixed to a base end 12b of the balloon 12 by a similar method, and the shaft 11 is placed on the balloon 12, thereby manufacturing a balloon catheter 10.
[0043] The method for manufacturing a parison for a balloon catheter according to this embodiment can also process a plurality of tubes 30 at once to manufacture a plurality of parisons 20. As shown in Fig. 11, a plurality of tubes 30 can be arranged along the long wall 72a of the wall surface 72 in the space 73 of the thermal molds 70, 70 of the heating mechanism unit 52. The plurality of tubes 30 arranged in the space 73 are heated by the thermal molds 70, 70 at once.
[0044] When one or more tubes 30 are arranged in the space 73 of the thermal mold 70, 70, the ratio of the cross-sectional area of the space 73 cut by a plane perpendicular to the long axis direction of the tube 30 to the total cross-sectional area of the tube 30 cut by a plane perpendicular to the long axis direction of the tube 30 is 2 times or more and less than 10 times, preferably 4 times or more and less than 8 times.
[0045] Next, a thermal mold 110 according to a modified example will be described. As shown in Fig. 12, the thermal mold 110 has a heating section 111, and the surfaces facing each other are planar wall surfaces 112. The thermal mold 110 is made of an elastic material.
[0046] 13, when the thermal mold 110 is closed, the wall surface 112 is deformed by the tube 30. Therefore, in the heating process, the thermal mold 110, which is a heat source, can be brought into contact with the entire circumference of the surface of the tube 30. By heating the thermal mold 110 in contact with the surface of the tube 30, heat is transferred from the thermal mold 110 to the tube 30 by thermal conduction, and the tube 30 can be heated efficiently even if the heating temperature of the thermal mold 110 is kept low.
[0047] After the heating step is performed with the hot mold 110 closed, the hot mold 110 is opened and separated from the surface of the tube 30, and then the stretching step is performed.
[0048] As shown in Fig. 14, a plurality of tubes 30 can be heated at once by the thermal mold 110. Also, as shown in Fig. 15, the thermal mold 110 may have a recess 113 on a wall surface 112, and the thermal mold 110 may be in contact with a part of the surface of the tube 30 in the circumferential direction.
[0049] The method for manufacturing the parison 20 for a balloon catheter may include a step of cooling the portion that will become the balloon 12. As shown in Fig. 16, the manufacturing apparatus 50 for the parison 20 may include a cooling mechanism 55 that cools the region between the pair of heating regions 32, 32 of the tube 30. The cooling mechanism 55 can be opened and closed by a moving mechanism 54.
[0050] The cooling mechanism 55 is composed of a pair of cooling dies 100, 100 which are cooling means respectively arranged on both radial sides of the tube 30. The cooling dies 100, 100 can be opened and closed by moving them close to and away from each other along the radial direction of the tube 30 by the moving mechanism 54. In Fig. 16, the cooling dies 100, 100 are in a closed state.
[0051] 17, a pair of cooling dies 100, 100 have concave wall surfaces 102, 102 facing each other, and when the facing cooling dies 100, 100 approach each other, a space 103 surrounded by the wall surfaces 102, 102 is formed. The cross section of the space 103 taken along a plane perpendicular to the long axis direction has a rectangular shape.
[0052] The cooling mold 100 has a cooling part 101 therein, which can lower the temperature of the wall surface 102 and cool the tube 30 in the space 103. The cooling part 101 can be a heat transfer tube that flows cooling water. However, the cooling part 101 is not limited to a heat transfer tube as long as it is a means that can cool the cooling mold 100.
[0053] When the pair of cooling dies 100, 100 are closed, the wall surface 102 has, in a cross section cut along a plane perpendicular to the long axis direction, a long wall 102a extending horizontally and a short wall 102b extending vertically, which is a different direction from the long wall 102a, and having a shorter length than the long wall 102a. The tube 30 disposed in the space 103 formed by the pair of cooling dies 100, 100 is adjacent to the long wall 102a of the wall surface 102.
[0054] By cooling the wall surface 102 by the cooling section 101, radiation cooling to the wall surface 102 and convection heat transfer within the space 103 cooled by the wall surface 102 occur, and the tube 30 can be cooled.
[0055] The manufacturing process of the parison 20 using the manufacturing apparatus 50 having the cooling mechanism 55 includes a cooling process for cooling the region between the pair of heating regions 32, 32 during the heating process. The cooling mold 100 is changed from an open state to a closed state by the moving mechanism 54 after the fixing process. The timing for closing the cooling mold 100 may be simultaneous with the timing for closing the heating mold 70 of the heating mechanism 52, or there may be a slight time difference.
[0056] The cooling step is continued while the heating step is being performed. In the cooling step, the surface of the region between the pair of heating regions 32, 32 of the tube 30 is maintained below the glass transition temperature of the tube 30. In the cooling step, the time from the start of cooling of the tube 30 to the state where the temperature is maintained below the glass transition temperature of the tube 30 is 5 seconds or more and 45 seconds or less. In addition, the difference between the surface temperature of the tube 30 in the heating step and the surface temperature of the tube 30 in the cooling step is 50°C or more and 140°C or less. In the cooling step, the region that will become the large diameter portion 21 of the tube 30 is cooled while the region that will be stretched in the stretching step is heated, and the temperature difference between the two regions can be clearly created. This suppresses the temperature rise of the portion that will become the large diameter portion 21 of the tube 30, and the shape of the shoulder portion 21b of the parison 20 to be manufactured can be clearly formed, and the parison 20 can be stably manufactured.
[0057] When the heating step is completed, the cooling step is also stopped. Next, as shown in Fig. 18, the hot molds 70, 70 and the cooling molds 100, 100 are opened, and the stretching step is performed. However, when the cooling step is performed with the cooling mold 100 whose wall surface 102 is close to the surface of the tube 30, the stretching step may be performed after the cooling step with the cooling molds 100, 100 kept closed.
[0058] 19, the cooling molds 120, 120 may be formed of an elastically deformable material and may be in contact with the surface of the tube 30. The cooling mold 120 having a cooling portion 121 has a wall surface 122 on the surface facing the opposing cooling mold 120, and is elastically deformed by the surface of the tube 30, so that when the cooling molds 120, 120 are closed, the wall surface 122 of the cooling mold 120 is in contact with the surface of the tube 30, so that heat is transferred between the cooling mold 120 and the tube 30 by thermal conduction, and the tube 30 can be cooled efficiently.
[0059] 20, the cooling dies 120, 120 may have a recess 123 on a wall surface 122. In this case, the cooling dies 120, 120 can contact a part of the surface of the tube 30 in the circumferential direction.
[0060] As described above, the method for manufacturing a parison 20 for a balloon catheter according to this embodiment (1) includes a fixing step of fixing a thermoplastic tube 30 extending along the longitudinal direction at a pair of fixing regions 31, 31 spaced apart in the longitudinal direction, a heating step of heating a pair of heating regions 32, 32 spaced apart in the longitudinal direction between the pair of fixing regions 31, 31 of the tube 30 by bringing a heat source close to the surface of the tube 30 or by bringing the heat source into contact with at least a portion of the surface of the tube 30, and a stretching step of pulling the tube 30 in the direction in which the pair of fixing regions 31, 31 are separated, and stretching the pair of heating regions 32, 32 heated in the heating step of the tube 30, thereby forming a thick-diameter portion 21 having an outer diameter larger than the portion stretched between the pair of heating regions 32, 32 stretched in the stretching step. In the manufacturing method of the parison 20 for a balloon catheter configured as described above, the heat source is brought into close proximity to or into contact with the surface of the tube 30 in the heating step, so that the tube 30 can be stably heated by a combination of radiant heat and convective heat transfer, or by thermal conduction. Therefore, even if the heating temperature of the heat source is kept low, the tube 30 can be efficiently heated, and the shape of the parison 20 can be stably formed.
[0061] (2) In the method for manufacturing the parison 20 for the balloon catheter as described in (1) above, in the heating step, the tube 30 may be heated in a hot mold 70 having a space surrounded by a wall surface 72 with a rectangular cross-sectional shape cut in a plane perpendicular to the major axis direction. Thereby, the surface of the hot mold 70 and the surface of the tube 30 can be surely brought close to each other, and heating can be performed efficiently.
[0062] (3) In the method for manufacturing the parison 20 for the balloon catheter as described in (2) above, the minimum distance Y between the wall surface 72 and the tube 30 can be set to 0 < Y ≤ 1.5 mm. Thereby, the tube 30 can be efficiently heated by the radiant heat from the surface of the hot mold 70.
[0063] (4) In the method for manufacturing the parison 20 for the balloon catheter as described in (2) or (3) above, the wall surface 72 of the hot mold 70 includes, in a cross-sectional shape cut in a plane perpendicular to the major axis direction, a long wall 72a extending in one direction and a short wall 72b extending in a direction different from that of the long wall 72a and having a length shorter than that of the long wall 72a. A plurality of tubes 30 may be arranged and heated along the direction in which the long wall 72a extends in the space. Thereby, a plurality of tubes 30 can be heated at once to make the production of the parison 20 more efficient.
[0064] (5) In the method for manufacturing the parison 20 for the balloon catheter as described in (1) above, in the heating step, the heat source may be brought into contact with the entire circumference of the surface of the tube 30. Thereby, the tube 30 can be efficiently heated by heat conduction.
[0065] (6) In the method for manufacturing the parison 20 for the balloon catheter according to any one of (1) to (5) above, after the heating step, in the stretching step, a step of separating the heat source brought close to or in contact with the surface of the tube 30 from the surface of the tube 30 may be included. Thereby, the stretching step can be performed without interference from the heat source.
[0066] (7) In any one of the above (1) to (6) methods for producing the parison 20 for a balloon catheter, in the heating step, the heat source may maintain the surface of the heated region at a temperature higher than the glass transition temperature of the tube 30. This allows the heated region of the tube 30 to be reliably stretched in the stretching step, thereby increasing its strength.
[0067] (8) In any one of the above (1) to (7) methods for producing a parison 20 for a balloon catheter, a cooling step may be provided between the heating steps to cool at least a part of the region between the pair of heated regions 32, 32. This allows a clear temperature difference to be created between the region between the pair of heated regions 32, 32 in the tube 30 and the heated regions.
[0068] (9) In the above (8) method for producing a parison 20 for a balloon catheter, the surface of the region between the pair of heating regions 32, 32 may be maintained at a temperature lower than the glass transition temperature of the tube 30 in the cooling step. This makes it possible to suppress a rise in temperature in the portion that will become the large diameter portion 21 of the tube 30, and to clearly form the shape of the shoulder of the produced parison 20.
[0069] (10) In the method for producing the parison 20 for a balloon catheter according to either (8) or (9) above, the difference between the surface temperature of the tube 30 in the heating step and the surface temperature of the tube 30 in the cooling step can be set to 50° C. or more and 140° C. or less. This allows a sufficient temperature difference to be created between the heating area and the cooling area of the tube 30, and the shape of the large diameter portion 21 of the tube 30 can be stably formed.
[0070] (11) In the method for producing a balloon catheter 10 according to this embodiment, a balloon catheter parison 20 produced by any one of the production methods (1) to (10) above is biaxially stretched to form a balloon 12, and a shaft 11 is placed on the formed balloon 12. Because the shape of the balloon catheter parison 20 is stably formed by any one of the production methods (1) to (10) above, a balloon catheter 10 having a balloon 12 with a stable shape can be produced.
[0071] The manufacturing apparatus 50 for a balloon catheter parison 20 according to the present embodiment (12) includes a fixing mechanism 51 for fixing a thermoplastic tube 30 extending along the longitudinal axis at a pair of fixing regions 31, 31 spaced apart in the longitudinal direction, a heating mechanism 52 for heating a pair of heating regions 32, 32 spaced apart in the longitudinal direction between the pair of fixing regions 31, 31 of the tube 30 by bringing a heat source close to the surface of the tube 30 or by bringing the heat source into contact with at least a part of the surface of the tube 30, and a pulling mechanism 53 for moving the fixing mechanism 51 in a direction in which the distance between the pair of fixing regions 31, 31 of the tube 30 increases. The manufacturing apparatus 50 for a balloon catheter parison 20 thus configured is capable of stably heating the tube 30 by a combination of radiant heat and convective heat transfer or by thermal conduction, since the heat source is close to or in contact with the portion of the tube 30 to be stretched. Therefore, even if the heating temperature of the heat source is kept low, the tube 30 can be efficiently heated, and the shape of the parison 20 can be stably formed.
[0072] The present invention is not limited to the above-described embodiment, and various modifications can be made by those skilled in the art within the technical concept of the present invention. [Explanation of symbols]
[0073] 10 Balloon Catheter 11 Shaft 12. Balloon 13. Hub 20 Parison 21 Large diameter part 21a Same diameter part 21b Shoulder 22 Thin section 30 Tubes 31 Fixed area 32 Heating area 50 Manufacturing equipment 51 Fixing mechanism section 52 Heating mechanism section 53 Pulling mechanism 54 Moving mechanism section 55 Cooling mechanism section 60 Fixed part 70 Heat type 71 Heating section 72 Wall 72a long wall 72b short wall 73 Space
Claims
1. 1. A method for producing a parison for a balloon catheter, comprising: A fixing step of fixing a thermoplastic tube extending along a longitudinal direction at a pair of fixing regions spaced apart in the longitudinal direction; a heating step of heating a pair of heating regions spaced apart in the longitudinal direction between the pair of fixing regions of the tube by bringing a heat source close to the surface of the tube or by bringing the heat source into contact with at least a portion of the surface of the tube; a stretching step of pulling the tube in a direction in which the pair of fixed regions are separated from each other to stretch the pair of heated regions of the tube heated in the heating step; Equipped with a thickened portion having an outer diameter larger than that of the stretched portion is formed between the pair of heated regions stretched by the stretching step.
2. 2. The method for producing a parison for a balloon catheter according to claim 1, wherein in the heating step, the tube is heated in a thermal mold having a space surrounded by walls having a rectangular cross-sectional shape cut along a plane perpendicular to the longitudinal axis.
3. 3. The method for producing a parison for a balloon catheter according to claim 2, wherein a minimum distance Y between the wall surface and the tube is 0<Y≦1.5 mm.
4. 3. The method for manufacturing a parison for a balloon catheter according to claim 2, wherein the wall surface of the thermal mold has, in a cross-sectional shape cut along a plane perpendicular to the longitudinal direction, a long wall extending in one direction and a short wall extending in a different direction from the long wall with a length shorter than that of the long wall, and a plurality of the tubes are arranged in the space along the direction in which the long walls extend and are heated.
5. 2. The method for producing a parison for a balloon catheter according to claim 1, wherein in the heating step, the heat source is brought into contact with the entire circumference of the surface of the tube.
6. 2. The method for producing a parison for a balloon catheter according to claim 1, further comprising the step of separating the heat source that was in close proximity to or in contact with the surface of the tube during the stretching step from the surface of the tube after the heating step.
7. 2. The method for manufacturing a parison for a balloon catheter according to claim 1, wherein in the heating step, the heat source maintains the surface of the heating region at a temperature higher than the glass transition temperature of the tube.
8. The method for producing a parison for a balloon catheter according to claim 1 , further comprising a cooling step of cooling at least a part of the region between the pair of heating regions during the heating step.
9. 9. The method for producing a parison for a balloon catheter according to claim 8, wherein in the cooling step, a surface of the region between the pair of heated regions is maintained at a temperature lower than the glass transition temperature of the tube.
10. 9. The method for producing a parison for a balloon catheter according to claim 8, wherein a difference between a surface temperature of the tube in the heating step and a surface temperature of the tube in the cooling step is 50° C. or more and 140° C. or less.
11. A method for producing a balloon catheter, comprising biaxially stretching the parison for a balloon catheter produced by the method according to any one of claims 1 to 10 to form a balloon, and installing a shaft in the formed balloon.
12. An apparatus for manufacturing a parison for a balloon catheter, comprising: a fixing mechanism that fixes a thermoplastic tube extending along a longitudinal direction at a pair of fixing regions that are spaced apart in the longitudinal direction; a heating mechanism for heating the tube by bringing a heat source close to the surface of the tube or by bringing the heat source into contact with at least a portion of the surface of the tube in a pair of heating regions that are spaced apart in the longitudinal direction between the pair of fixing regions of the tube; a tension mechanism that moves the fixing mechanism in a direction that increases the distance between the pair of fixing regions of the tube; An apparatus for manufacturing a parison for a balloon catheter, comprising:
Citation Information
Patent Citations
Balloon and production method for same
WO2014141382A1