Liquid discharge head and manufacturing method of the same

By integrating a thin film of silicon carbide or silicon oxide with carbon, nitride, or oxynitride on the ejection port protection member, the liquid ejection head addresses adhesion and dissolution resistance issues, ensuring robustness and longevity against ink interaction.

JP2024162904APending Publication Date: 2024-11-21CANON KK
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023078883
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Existing liquid ejection heads face issues with adhesion failure and insufficient dissolution resistance due to stress differences and ink interaction, particularly when using corrosion-resistant metals like stainless steel for ejection port protection.

Method used

The ejection head incorporates a thin film containing silicon carbide, silicon oxide, silicon nitride, or silicon oxynitride on the discharge port protection member to enhance adhesion and resistance to ink, using materials like stainless steel for the protection member and epoxy resin for the discharge port forming member, with specific adhesion improving layers to maintain integrity.

Benefits of technology

The solution provides enhanced adhesion and durability against ink, preventing peeling and maintaining the functionality of the ejection port protection member, even under prolonged ink exposure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162904000001_ABST
    Figure 2024162904000001_ABST
Patent Text Reader

Abstract

To improve adhesion between an adhesive applied to a discharge port surface of a liquid discharge head and a metallic material to enhance adhesion strength of a discharge port protection member.SOLUTION: A liquid discharge head includes: a substrate provided with a passage of a discharged liquid; a discharge port forming member provided with a discharge port from which the liquid that has passed through the passage is discharged; a discharge port protection member joined to the discharge port forming member through an adhesive; and a thin film formed on a surface, which is located at the side joined to the discharge port forming member, of the discharge port protection member and including silicon carbide or one of silicon oxide, silicon nitride, and silicon oxynitride which contains carbon.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a liquid ejection head that ejects liquid, and a manufacturing method thereof. [Background technology]

[0002] In a recording method using a liquid ejection head, such as a recording head for an inkjet printer, thermal energy or vibration energy is applied to a liquid such as ink, causing the ink to be ejected from an ejection port in the form of minute droplets, thereby forming an image on a recording medium.

[0003] A liquid ejection head has a photosensitive resin layer that forms ejection ports and flow paths, and a substrate. The photosensitive resin layer that forms the ejection ports and flow paths is provided on the substrate. A supply port that supplies liquid to the flow paths is formed in the substrate. The surface of the substrate on the side where the flow paths and ejection ports are provided has energy generating elements. Liquid is supplied from the supply port to the flow paths, energy is imparted by the energy generating elements, and the liquid is ejected from the liquid ejection port and lands on a recording medium such as paper.

[0004] In recent years, there has been an increasing demand for recording devices such as inkjet printers to print out recorded materials with higher resolution than before at higher speeds for commercial and industrial printing applications, etc. However, when printing out at higher speeds, there is a possibility that paper that has been bent due to a paper jam or the like may come into contact with the surface of the ejection ports of the liquid ejection head, which is made of a photosensitive resin layer, and the surface of the ejection ports may be damaged.

[0005] Furthermore, in fields where demand is growing for recording devices such as inkjet printers, particularly in the field of industrial printing, robust liquid ejection heads are required, and there is a demand for stronger base materials to prevent damage to the ejection orifices in the event of a paper jam.

[0006] Furthermore, in order to achieve high image quality, recording devices such as inkjet printers have a wider range of freedom in the selection of ejection liquids, which has led to a demand for improved resistance to dissolution of components that come into contact with ink.

[0007] In view of this, Patent Document 1 proposes that a metal material be adhesively bonded and laminated onto a substrate on which ejection ports (nozzles) are formed, thereby protecting the ejection port surface from paper. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] Patent No. 3108771 Summary of the Invention [Problem to be solved by the invention]

[0009] However, in a liquid ejection head having ejection ports made of a photosensitive resin layer, when a metal material is adhesively bonded to the ejection port surface as in Patent Document 1, the metal and the photosensitive resin layer are bonded to each other as dissimilar materials. Therefore, stress differences are likely to occur due to cure shrinkage and linear expansion differences, and prolonged contact with ink can cause peeling between the adhesive and the metal material, which has low adhesion.

[0010] In addition, the general metal material of Patent Document 1 alone does not have sufficient resistance to dissolution by ink, and there is a demand for a head made of a corrosion-resistant metal with high resistance to dissolution. However, it has become clear that the high-quality inks developed in recent years do not have sufficient resistance to dissolution by ink, even when corrosion-resistant metal members such as stainless steel with high resistance to dissolution are used.

[0011] More specifically, in order to simply improve the robustness of the head, stainless steel, a corrosion-resistant metal, is used for the ejection port protection member, and the ejection port protection member is adhesively bonded to the nozzle plate. It has been found that the stainless steel at the bonding interface dissolves due to the ink, peeling off the adhesive used for bonding and reducing the adhesive strength of the ejection port protection member.

[0012] Therefore, the object of the present invention is to provide a liquid ejection head and a method for manufacturing the same that can increase the adhesion between the adhesive applied to the ejection port surface of the liquid ejection head and the metal material without impairing the inherent dissolution resistance of the corrosion-resistant metal, and strengthen the adhesive strength of the ejection port protection member. [Means for solving the problem]

[0013] In order to achieve the above object, the liquid ejection head of the present invention comprises: A substrate in which a flow path for the liquid to be discharged is formed; a discharge port forming member having a discharge port formed therein through which the liquid that has passed through the flow path is discharged; a discharge port protection member bonded to the discharge port forming member via an adhesive; a thin film formed on a surface of the ejection port protection member that is to be bonded to the ejection port formation member, the thin film including silicon carbide, or any one of silicon oxide containing carbon, silicon nitride, and silicon oxynitride; The present invention is characterized by having the following. In order to achieve the above object, a method for producing a liquid ejection head according to the present invention includes the steps of: A substrate in which a flow path for the liquid to be discharged is formed; a discharge port forming member having a discharge port formed therein through which the liquid that has passed through the flow path is discharged; a discharge port protection member that is bonded to the discharge port forming member via an adhesive in order to protect the discharge port; A method for manufacturing a liquid ejection head comprising the steps of: The method is characterized by including a step of forming a thin film containing silicon carbide or any one of silicon oxide, silicon nitride, and silicon oxynitride containing carbon on the surface of the ejection port protection member that is to be joined to the ejection port formation member. Effect of the Invention

[0014] According to the present invention, it is possible to provide a liquid ejection head in which the adhesion between the surface of the liquid ejection head, including the ejection port surface, and the metal material is high, and the adhesive strength of the ejection port protection member is enhanced. [Brief description of the drawings]

[0015] [Figure 1] 3 is a structural diagram of a liquid ejection head in the first and second embodiments. [Diagram 2] 3A to 3C are explanatory diagrams of a manufacturing method of the liquid ejection head in the first embodiment. [Diagram 3] 4A to 4C are structural diagrams of liquid ejection heads in Comparative Example 1 and Example 3. [Figure 4] 5A to 5C are explanatory diagrams of a manufacturing method of a liquid ejection head in Comparative Example 1 and Example 3. [Diagram 5] 5A and 5B are structural diagrams of liquid ejection heads in Comparative Example 2 and Example 4. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, with reference to the drawings, the mode for carrying out the present invention will be described in detail by way of example. The dimensions, materials, shapes, and relative positions of the components described in the embodiments should be appropriately changed depending on the configuration of the device to which the invention is applied and various conditions. Furthermore, not all of the combinations of features described in the embodiments are necessarily essential to the solution of the present invention. The components described in the embodiments are merely examples, and are not intended to limit the scope of the present invention to only those.

[0017] Example 1 The ink jet recording substrate and the liquid ejection head to which the present invention is applied will be described below. Fig. 1 shows a liquid ejection head formed by adhesively bonding a substrate 4 to a head bonding member 20. Fig. 1(a) is a plan view, and Fig. 1(b) is a cross-sectional view taken along line DD in Fig. 1(a). Note that Fig. 1(b) shows the liquid ejection port facing upward.

[0018] In the liquid ejection head of this embodiment, energy generated by an energy generating element (heater) 3 causes liquid to flow from the head joining member 20 into the substrate, pass through the supply port 5 and flow path in the substrate, and be ejected from the ejection port 1, where the liquid lands on the recording medium to perform printing.

[0019] In order to supply the liquid by causing the liquid to flow into the substrate, it is necessary to form a flow path that communicates with the substrate 4 and through which the liquid flows.

[0020] The manufacturing method for the communicating holes varies depending on the required shape. Methods for forming a single large groove common to multiple ejection port rows (nozzle rows) include wet anisotropic etching, laser methods, and sandblasting.

[0021] Furthermore, in order to form a large number of small holes with high precision for the nozzle rows, a dry etching method using Deep-RIE is available.

[0022] Regarding the method of forming the nozzle / discharge port from which the liquid is discharged, the nozzle part is called an orifice plate, and there is a method of forming it on the substrate by spin coating, or a method of forming it from a separate material and then bonding it to the substrate; details will be given later.

[0023] In this embodiment, a method was selected in which a photosensitive epoxy resin was used for the ejection port forming member. The resin was also bonded using a dry film. After bonding, exposure, development, and hardening baking were performed to complete the product.

[0024] As described above, recording devices such as inkjet printers to which the liquid ejection head of the present invention is applied are intended to be used particularly in the field of industrial printing, and therefore require a robust head and a reinforced base material to prevent damage to the ejection port 1 in the event of a paper jam.

[0025] Therefore, by joining the ejection port protection member 11 directly above the ejection port forming member 2, even if paper or the like comes into contact with the surface of the head, direct contact with the ejection port forming member 2 is prevented, thereby protecting the ejection port 1.

[0026] In this embodiment, epoxy resin is selected as the material for the ejection port forming member 2, and stainless steel material is selected as the material for the ejection port protection member 11. This is aimed at improving the resistance to dissolution by ink, which is the ejection liquid.

[0027] Moreover, since the ejection port protection member 11 is intended to protect the ejection port forming member 2, it is sufficient for it to be made of a material with higher mechanical strength than epoxy resin, and the candidates for this are a silicon substrate or a metal member. Among these, when considering resistance to dissolution by ink, it is more desirable for the ejection port protection member 11 to be made of corrosion-resistant metals such as stainless steel, aluminum alloys, titanium alloys, and nickel alloys.

[0028] The ejection port forming member 2 and the ejection port protection member 11 are bonded with an adhesive 13 in order to bond the ejection port protection member 11 to the ejection port without touching or changing the ejection port 1 once it has been completed. Normally, the choice of adhesive depends on the bonding material, but this adhesive can be bonded to the head bonding member 20, which is a ceramic material, the substrate 4, which is a silicon material, and the ejection port forming member 2, which is made of resin such as epoxy resin. In consideration of ink resistance, it is preferable to use an adhesive that uses an epoxy resin as the base material, a curing catalyst, and an acid anhydride.

[0029] The epoxy resin used in the adhesive may be an alicyclic epoxy resin, an aromatic epoxy resin, an aliphatic epoxy resin, or the like.

[0030] Examples of alicyclic epoxy resins include the following: polyglycidyl ethers of polyhydric alcohols having at least one alicyclic ring, or compounds containing a cyclohexene oxide structure or a cyclopentene oxide structure obtained by epoxidizing a compound containing a cyclohexene or cyclopentene ring with an oxidizing agent, or compounds containing a vinylcyclohexane oxide structure obtained by epoxidizing a compound having a vinylcyclohexane structure with an oxidizing agent. For example, hydrogenated bisphenol A diglycidyl ether, 3,4-epoxycyclohexylmethyl-3,4-epoxycyclohexyl carboxylate, 3,4-epoxy-1-methylcyclohexyl-3,4-epoxy-1-methylcyclohexane carboxylate, 6-methyl-3,4-epoxycyclohexylmethyl-6-methyl-3,4-epoxycyclohexane carboxylate, 3,4-epoxy-3-methylcyclohexylmethyl-3,4-epoxy-3-methylcyclohexane carboxylate, 3,4-epoxy-5-methylcyclohexylmethyl-3,4-epoxy-5-methylcyclohexane carboxylate, 2-(3,4-epoxycyclohexyl-5,5- spiro-3,4-epoxy)cyclohexane-metadioxane, bis(3,4-epoxycyclohexylmethyl)adipate, vinylcyclohexene dioxide, 4-vinylepoxycyclohexane, bis(3,4-epoxy-6-methylcyclohexylmethyl)adipate, 3,4-epoxy-6-methylcyclohexylcarboxylate, methylene bis(3,4-epoxycyclohexane), dicyclopentadiene diepoxide, ethylene glycol di(3,4-epoxycyclohexylmethyl)ether, ethylene bis(3,4-epoxycyclohexanecarboxylate), dioctyl epoxyhexahydrophthalate, di-2-ethylhexyl epoxyhexahydrophthalate, and the like.

[0031] Specific examples of aromatic epoxy resins include the following: polyglycidyl ethers of polyhydric phenols having at least one aromatic ring or their alkylene oxide adducts, or those containing a naphthalene ring, such as glycidyl ethers of bisphenol A, bisphenol F, or compounds obtained by further adding alkylene oxide to these, epoxy novolac resins, bisphenol A novolac diglycidyl ether, bisphenol F novolac diglycidyl ether, etc.

[0032] Specific examples of aliphatic epoxy resins include the following: polyglycidyl ethers of aliphatic polyhydric alcohols or their alkylene oxide adducts, polyglycidyl esters of aliphatic long-chain polybasic acids, epoxy-containing compounds obtained by oxidizing aliphatic long-chain unsaturated hydrocarbons with an oxidizing agent, homopolymers of glycidyl acrylate or glycidyl methacrylate, and copolymers of glycidyl acrylate or glycidyl methacrylate. Representative compounds include glycidyl ethers of polyhydric alcohols such as 1,4-butanediol diglycidyl ether, 1,6-hexanediol diglycidyl ether, triglycidyl ether of glycerin, triglycidyl ether of trimethylolpropane, tetraglycidyl ether of sorbitol, hexaglycidyl ether of dipentaerythritol, diglycidyl ether of polyethylene glycol, and diglycidyl ether of polypropylene glycol; polyglycidyl ethers of polyether polyols obtained by adding one or more alkylene oxides to aliphatic polyhydric alcohols such as propylene glycol and glycerin; and diglycidyl esters of aliphatic long-chain dibasic acids.

[0033] Further examples include monoglycidyl ethers of aliphatic higher alcohols, phenol, cresol, butylphenol, and monoglycidyl ethers of polyether alcohols obtained by adding alkylene oxides to these, glycidyl esters of higher fatty acids, epoxidized soybean oil, epoxy octyl stearate, epoxy butyl stearate, and epoxidized linseed oil.

[0034] The adhesive that can be selected in the present invention is not limited to the one selected in this embodiment, since it is necessary to satisfy the above-mentioned factors. Also, in this embodiment, the same adhesive as the back adhesive 21 of the substrate is used for the adhesive 13.

[0035] An adhesion improving layer 12 is formed on the adhesive bonding surface of the discharge port protection member 11 that is bonded to the discharge port forming member 2 in order to improve adhesion. Since the adhesion improving layer 12 has an important adhesive property with the adhesive 13, it is preferable that the adhesion improving layer contains silicon oxide, and contains oxygen (O) at a ratio of 5% or more to silicon (Si).

[0036] Furthermore, in consideration of the ink resistance of the adhesion improving layer itself, it is preferable that the ratio of oxygen to silicon is 50% or less. That is, it is preferable to form the adhesion improving layer 12 as a thin film containing silicon oxide, in which the ratio of oxygen (O) to silicon (Si) in the silicon oxide is 5% or more and 50% or less. In this embodiment, the adhesion improving layer 12 is formed so that the ratio of O to Si is 25%.

[0037] Regarding the film thickness, it is sufficient that it is about 30 nm or more so that it can be optically recognized as a film, and it is also important not to cause deformation of the stainless steel member that is the base material, so it is preferable to make the film thickness about 100 nm or less by taking a balance into consideration. In other words, the thickness of the adhesion improving layer 12 is preferably 30 nm or more and 100 nm or less.

[0038] Furthermore, taking into consideration the characteristics of the adhesion improving layer 12, it is advantageous to increase the compressive stress as the film stress of the film within a range that does not cause warping of the stainless steel member of the discharge port protection member 11, which serves as the base material, and it is desirable to set the compressive stress to be 300 MPa or more and 700 MPa or less.

[0039] Fig. 2 is a diagram showing the structure and manufacturing method of a substrate 4 and a liquid ejection head corresponding to the first embodiment of the present invention. Corresponding parts are given the same reference numerals as in Fig. 1. The manufacturing method of the substrate 4 and the liquid ejection head will be described in detail below.

[0040] As shown in FIG. 2(a), a silicon substrate 4 having a thickness of 500 μm was prepared, on the front side of which an energy generating element 3 and a driving circuit (not shown) made up of semiconductor elements and wiring were built in.

[0041] Next, as shown in FIG. 2(b), the substrate 4 was etched from the front surface side to form a 50×50 μm recessed hole to serve as the supply port 5. In this embodiment, the etching gas was SF 6 and C. 4 F 8 The Deep-RIE method is used, which alternates between etching and film formation.

[0042] Next, as shown in FIG. 2( c ), a dry film containing a photosensitive epoxy resin that will become the ejection port forming member 2 is attached onto the substrate 4 .

[0043] Furthermore, as shown in Fig. 2(d), the photosensitive dry film was divided into parts, exposed to light, and developed to form the flow path for the liquid and the discharge port 1. At this point, the process up to the discharge port 1 is temporarily completed.

[0044] Next, as shown in Fig. 2(e), a 30 μm thick stainless steel member with a shape created as a separate part is prepared as the discharge port protection member 11. The shape is created by processing the stainless steel member using photoetching technology, forming a resist, and carrying out wet etching. Note that in this embodiment, a 30 μm thick member is used, but this is not limiting, and a thickness of 10 μm to 50 μm is preferable.

[0045] Next, as shown in FIG. 2(f), a SiOC film was formed on the rear surface of the discharge port protection member 11 to a thickness of 50 nm so that the ratio of O to Si was 25%, forming a thin adhesion improving layer 12. In this embodiment, the film forming gas was SiH 4 and C.H. 4 The film was formed by the plasma CVD method among the vacuum film forming methods.

[0046] Next, as shown in FIG. 2( g ), the discharge port protection member 11 with the adhesion improving layer 12 formed as a separate part is bonded to the discharge port forming member 2 by using an adhesive 13 .

[0047] Finally, as shown in FIG. 2(h), the substrate 4 was bonded to the head bonding member 20 using a substrate back adhesive 21 to form a liquid ejection head.

[0048] Here, the features of the first embodiment of the present invention will be described. In this embodiment, as described above, the SiOC film as the adhesion improving layer 12 is formed so that the Si:O ratio is 100:25. The film forming gas is SiH 4 and C.H. 4 The film was formed by plasma CVD using the above material.

[0049] Even when the liquid ejection head of this embodiment was subjected to an ink durability test and an ink immersion test, no peeling occurred between the adhesive 13 and the ejection port protection member 11, and no damage occurred. As a result, the liquid ejection head was not destroyed as a product.

[0050] For comparison, a stainless steel member serving as the ejection port protection member 11 was bonded to the ejection port forming member 2 using the adhesive 13 without forming a SiOC film as an adhesion improving layer on the rear surface thereof, and the same ink durability test and ink immersion test were carried out.

[0051] As a result, the ink penetrated into the interface between the adhesive and the stainless steel member, reducing the adhesive strength. As a result, it was found that using the stainless steel member as the ejection port protection member 11 without forming a SiOC film does not adequately protect the ejection port.

[0052] For comparison, a discharge port protection member 11 was formed using a silicon substrate, which is originally low in resistance to ink, and a SiOC film serving as an adhesion improving layer was formed on the rear surface. This was then adhesively bonded to the discharge port forming member 2 using an adhesive 13, and the same ink durability test and ink immersion test were performed.

[0053] As a result, only the area where the SiOC film was formed did not dissolve, and the adhesive strength of the silicon substrate did not decrease.

[0054] However, the portions of the silicon substrate on which the SiOC film was not formed were dissolved, and a decrease in performance as the ejection port protection member 11 was observed.

[0055] Comparative Example 1 3 and 4 are diagrams showing the structure and manufacturing method of a substrate 4 and a liquid ejection head corresponding to Comparative Example 1 of the present invention. Corresponding parts are given the same reference numerals. The manufacturing method of the substrate 4 and the liquid ejection head will be described in detail below. In Comparative Example 1, two substrates 4 are arranged side by side in one liquid ejection head as shown in FIG. 3(b).

[0056] As shown in FIG. 4(a), the front side is provided with an energy generating element 3 and a semiconductor element and wiring. A silicon substrate 4 having a thickness of 500 μm and incorporating a driving circuit (not shown) was prepared.

[0057] Next, as shown in FIG. 4(b), the substrate 3 was etched from the front surface side to form a 50×50 μm recessed hole to serve as the supply port 5. As in Example 1, SF was used as the etching gas. 6 and C. 4 F 8 The Deep-RIE method is used, which alternates between etching and film formation.

[0058] Next, as shown in FIG. 4(c), a dry film containing a photosensitive epoxy resin that will become the ejection port forming member 2 is attached onto the substrate 4.

[0059] Next, as shown in FIG. 4(d), the photosensitive dry film was divided into parts, exposed to light, and developed to form flow paths through which liquid flows and discharge ports 1, in the same manner as in Example 1.

[0060] Next, as shown in Fig. 4(e), the two horizontally arranged substrates 4 are adhesively bonded to one head bonding member 20 using a substrate back adhesive 21. This completes the process of bonding the two substrates 4, each having a discharge port 1 formed thereon, to one liquid discharge head.

[0061] Next, as shown in Fig. 4(f), a 30 μm thick stainless steel member with a shape fabricated as a separate part is prepared as the discharge port protection member 11. The shape is formed by photoetching technology, and the stainless steel member is processed by forming a resist and wet etching. For comparison with Example 1, a similar 30 μm thick member is used.

[0062] 4(g), a SiOC film is formed on the rear surface of the discharge port protection member 11 to a thickness of 100 nm so that the ratio of O to Si is 4%, i.e., Si:O is 100:4, to form the adhesion improving layer 12. In Comparative Example 1, SiOC was used as the film formation target, and the film formation was performed by bias RF sputtering, which is a type of vacuum film formation.

[0063] Next, as shown in FIG. 4(h), a discharge port protection member 11 with an adhesion improving layer 12 formed as a separate part was bonded to the discharge port forming member 2 with an adhesive 13 to form a liquid discharge head.

[0064] An ink durability test and an ink immersion test were conducted on the liquid ejection head of Comparative Example 1. As a result of prolonged ink immersion, the ink penetrated into the interface between the adhesion improving layer and the stainless steel, causing peeling. In Comparative Example 1, a SiOC film was formed as the adhesion improving layer with a Si:O ratio of 100:4. It is believed that the ink penetrated into the interface because the adhesive strength at the interface decreased as the proportion of oxygen that contributes to adhesion in the film decreased.

[0065] Comparative Example 2 5 is a diagram showing the structure of a substrate 4 and a liquid ejection head corresponding to Comparative Example 2 of the present invention. In Comparative Example 2, two substrates 4 are arranged side by side in one ejection head. In Comparative Example 2, the substrate 4, ejection port forming member 2, and ejection port protection member 11 are the same as those in Example 1 and Comparative Example 1, so a description of the manufacturing method of the substrate 4 and the liquid ejection head will be omitted.

[0066] In Comparative Example 2, a SiOC film was formed to a thickness of 30 nm so that the ratio of Si:O was 100:55, and the adhesion improving layer 12 was formed. 4 and C.H. 4 The film was formed by plasma CVD using the above material.

[0067] As a result of carrying out an ink durability test and an ink immersion test on the liquid ejection head of Comparative Example 2, the SiOC film, which is an adhesion improving layer, dissolved and peeled off after a long period of ink immersion. In Comparative Example 2, the SiOC film is formed to a thickness of 30 nm so that the Si:O ratio is 100:55. Therefore, if the oxygen ratio is excessive, the ink resistance of the film itself decreases and it becomes easily dissolved by ink. It is thought that this will happen.

[0068] Example 2 An inkjet recording substrate and a liquid ejection head according to the second embodiment will be described. Fig. 1 shows a liquid ejection head formed by adhesively bonding a substrate 4 to a head bonding member 20. The structures of the substrate and the liquid ejection head are almost the same as those of the first embodiment, so only the differences from the first embodiment will be described.

[0069] The ejection port protection member 11 is a separate part, and its shape is first formed by resist formation and then processed by a photoetching method using wet etching, as in Example 1. Then, an adhesion improving layer 12 is formed on the back surface of the ejection port protection member 11 in order to strengthen the bonding by the adhesive.

[0070] Here, since the resistance to ink is important for this adhesion improving layer 12, unlike Example 1, a thin film containing silicon-based material containing carbon, i.e., silicon carbide, or silicon oxide, silicon nitride, or silicon oxynitride containing carbon is desirable. More specifically, any of SiC, SiOC, SiCN, and SiOCN may be used, and can be selected depending on the type of ink required. In this example, a thin film of SiC with a thickness of 50 μm is formed using SiH as the deposition gas. 4 and C.H. 4 The film thickness and compressive stress are also the same as those in the first embodiment, and therefore will not be described here.

[0071] In this case, triode deposition was selected for the plasma CVD film formation, in which a 13.56 MHz RF power source was applied to the shower head as HF and a 380 KHz RF power source was applied to the platen as LF.

[0072] Furthermore, in order to increase the adhesion to the stainless steel surface, the HF power applied to the shower head was reduced and the LF power applied to the platen was increased. The compressive stress was adjusted to 500 MPa, and the HF / LF / pressure conditions were set to 100 W / 200 W / 100 Pa, respectively, to perform film formation.

[0073] In the plasma CVD method, the pressure during film formation is about 100 Pa, which is not a very high degree of vacuum for film formation. This has the advantage that it is possible to maintain a constant degree of vacuum stably without relying on the degassing of contaminants, especially organic contaminants, on the stainless steel surface, and that film formation is stable.

[0074] In addition, triode deposition allows deposition at low temperatures of less than 100°C, which is close to room temperature. Deposition was performed at 60°C to avoid behavior that induces deposition and transportation problems, such as expansion and contraction and warping of stainless steel components due to temperature differences.

[0075] The formed SiC film had a thickness of only 50 nm, and therefore functioned satisfactorily as the adhesion improving layer 12 without causing any deformation of the stainless steel substrate even when the compressive stress was set to a high value of 500 MPa.

[0076] Even when the ejection head of this embodiment was subjected to an ink durability test and an ink immersion test, no peeling or product damage occurred.

[0077] For comparison, a stainless steel member serving as the ejection port protection member 11 was bonded to the ejection port forming member 2 using the adhesive 13 without forming a SiC film as an adhesion improving layer on the rear surface thereof, and the same ink durability test and ink immersion test were carried out.

[0078] The adhesive and the stainless steel material interface are then dissolved by the ink, and the adhesive is removed. It was confirmed that the adhesive strength of the stainless steel member was reduced by peeling it off. As a result, it was found that if the stainless steel member was used as the ejection port protection member 11 without forming a SiC film, the ejection port protection member 11 could not fully perform its function of protecting the ejection port.

[0079] For comparison, a discharge port protection member 11 was formed using a silicon substrate, which is originally low in resistance to ink, and a SiC film was formed on the back surface as an adhesion improving layer. The discharge port protection member 11 was then adhesively bonded to the discharge port forming member 2 using an adhesive 13, and the same ink durability test and ink immersion test were performed.

[0080] As a result, only the areas where the SiC film was formed did not dissolve, and the adhesive strength of the silicon substrate did not decrease.

[0081] However, the portions of the silicon substrate on which the SiC film was not formed were dissolved, and a decrease in performance as the ejection port protection member 11 was observed.

[0082] Example 3 3 and 4 are diagrams showing the structure and manufacturing method of a substrate 4 and a liquid ejection head corresponding to Example 3 of the present invention. Corresponding parts are given the same reference numerals. Below, the manufacturing method of the substrate and the head will be explained, but since it is basically the same as the manufacturing method in Comparative Example 1, differences will be explained.

[0083] The features of the third embodiment of the present invention will be described. In this embodiment, a SiC film is formed to a thickness of 100 nm as the adhesion improving layer 12. SiC is used as a film formation target, and film formation is performed by bias RF sputtering.

[0084] For sputtering, a parallel plate SiC target was prepared, and bias RF sputtering was performed by applying RF power and DC power. The RF power was set to 500 W, the bias power to 50 W, and the compressive stress was adjusted to 0.5 Pa to form the film.

[0085] Generally, reverse sputtering is performed as a pretreatment before sputtering to remove contaminants, especially organic contaminants, from the stainless steel surface. However, in the case of stainless steel, the chromium oxide on the surface is removed, reducing the corrosion resistance that is characteristic of stainless steel. Therefore, in this embodiment, the process is carried out without reverse sputtering.

[0086] Furthermore, in order to avoid behavior that induces problems in film formation and transportation, such as expansion, contraction, and warping of stainless steel components due to temperature differences, film formation was performed without heating the substrate.

[0087] In this embodiment, the SiC film formed had a thickness of 100 nm, which was thicker than that in Example 2, and therefore the compressive stress was set at a moderate limit of 300 MPa, and the SiC film functioned well as the adhesion improving layer 12 without causing any deformation of the stainless steel substrate.

[0088] In this embodiment, unlike the first embodiment, two substrates 4 are adhesively bonded to one head, and then one ejection port protection member 11 is adhesively bonded to the two substrates 4. At this time, not all surfaces of the ejection port protection member 11 that is adhesively bonded with the adhesive 13 face the ejection port forming member 2. In places where the ejection port forming member 2 is not present, there are surfaces that face the substrate 4, and there are also places where the ejection port protection member 11 is adhesively bonded to the substrate 4 via the adhesive 13.

[0089] However, by forming the adhesion improving layer 12 on the entire back surface of the ejection port protection member 11 as in this embodiment, the effect of the adhesion improving layer on the adhesive 13 remains good and unchanged even if the surface or material of the object to be joined changes.

[0090] When the ejection head of this embodiment was subjected to an ink durability test and an ink immersion test, similarly to the second embodiment, no peeling or product damage occurred.

[0091] Example 4 5 is a diagram showing the structure of the substrate and head corresponding to Example 4 of the present invention. In Example 4, the substrate 4, the ejection port forming member 2, and the ejection port protecting member 11 have the same structures as those used in Example 3, so the following will describe the parts that are different from the other examples.

[0092] In this embodiment shown in FIG. 5, a 30 nm SiC film was formed as the adhesion improving layer 12. In this embodiment, the film forming gas was SiH 4 and C.H. 4 The film was formed by plasma CVD using the above material.

[0093] As shown in FIG. 5, the head connecting member 20 is not flat, but the outer extension of the head connecting member 20 is elevated so that the substrate 4 can be accommodated therein, and the head connecting member 20 is joined to the rear surface of the ejection port protection member 11 with an adhesive 13.

[0094] The features of Example 4 of the present invention will be described. Since the formed SiC film has a thickness of 30 nm, which is thinner than that of Example 2, the compressive stress is set to 650 MPa to further increase the adhesion to the stainless steel surface. The film is formed under HF / LF / pressure conditions of 100 W / 200 W / 50 Pa, respectively.

[0095] Even so, the adhesion improving layer 12 functioned satisfactorily without causing any deformation of the stainless steel member of the substrate.

[0096] This embodiment is similar to embodiment 3, but unlike embodiment 1, after two substrates 4 are adhesively bonded to one head, one ejection port protection member 11 is adhesively bonded to the two substrates 4. At this time, not all surfaces of the ejection port protection member 11 that is adhesively bonded with the adhesive 13 face the ejection port forming member 2. In places where there is no ejection port forming member 2, there are surfaces that face the head joining member 20, and there are also places where the ejection port protection member 11 is adhesively bonded to the head joining member 20 via the adhesive 13.

[0097] By forming the adhesion improving layer 12 on the entire back surface of the discharge port protection member 11 as in this embodiment, the effect of the adhesion improving layer on the adhesive 13 remains good and unchanged even if the surface or material of the object to be joined changes.

[0098] Even when the ejection head of this embodiment was subjected to an ink durability test and an ink immersion test, no peeling or product damage occurred.

[0099] The disclosure of this embodiment includes the following configurations and methods. (Configuration 1) A substrate in which a flow path for the liquid to be discharged is formed; a discharge port forming member having a discharge port formed therein through which the liquid that has passed through the flow path is discharged; a discharge port protection member bonded to the discharge port forming member via an adhesive; a thin film formed on a surface of the ejection port protection member that is to be bonded to the ejection port formation member, the thin film including silicon carbide, or any one of silicon oxide containing carbon, silicon nitride, and silicon oxynitride; A liquid ejection head comprising: (Configuration 2) 2. The liquid ejection head according to configuration 1, wherein the thin film contains the silicon oxide, and the ratio of oxygen to silicon in the silicon oxide is 5% or more and 50% or less. (Configuration 3) the discharge port forming member is made of a material containing an epoxy resin, The discharge port protection member is made of a material containing silicon or metal. 3. The liquid ejection head according to configuration 1 or 2. (Configuration 4) 4. The liquid ejection head according to configuration 3, wherein the ejection port protection member is made of a material containing a corrosion-resistant metal. (Configuration 5) 5. The liquid ejection head according to configuration 4, wherein the ejection port protection member is made of a material containing any one of stainless steel, aluminum alloy, titanium alloy, and nickel alloy. (Configuration 6) 3. The liquid ejection head according to configuration 1 or 2, wherein the ejection port protection member has a thickness of 10 μm or more and 50 μm or less. (Configuration 7) 3. The liquid ejection head according to configuration 2, wherein the thin film has a ratio of silicon to oxygen of 100:25. (Configuration 8) 3. The liquid ejection head according to claim 1 or 2, wherein the thin film has a thickness of 30 nm or more and 100 nm or less. (Configuration 9) 3. The liquid ejection head according to configuration 1 or 2, wherein the film stress of the thin film is a compressive stress of 300 MPa or more and 700 MPa or less. (Method 1) A substrate in which a flow path for the liquid to be discharged is formed; a discharge port forming member having a discharge port formed therein through which the liquid that has passed through the flow path is discharged; a discharge port protection member that is bonded to the discharge port forming member via an adhesive in order to protect the discharge port; A method for manufacturing a liquid ejection head comprising the steps of: A method for manufacturing a liquid ejection head, comprising a step of forming a thin film containing silicon carbide or any one of silicon oxide containing carbon, silicon nitride, and silicon oxynitride on a surface of the ejection port protection member that is joined to the ejection port forming member. (Method 2) The method for producing a liquid ejection head according to Method 1, wherein the thin film contains the silicon oxide, and the ratio of oxygen to silicon in the silicon oxide is 5% or more and 50% or less. (Method 3) 3. The method for producing a liquid ejection head according to method 1 or 2, wherein the thin film is formed by vacuum film formation. (Method 4) The method for producing a liquid ejection head according to Method 3, wherein the thin film is formed by a plasma CVD method. (Method 5) The method for producing a liquid ejection head according to Method 3, wherein the thin film is formed by a bias RF sputtering method. [Explanation of symbols]

[0100] 2... discharge port forming member, 4... substrate, 11... discharge port protecting member, 12... adhesion improving layer, 13... adhesive

Claims

1. A substrate in which a flow path for the liquid to be discharged is formed; a discharge port forming member having a discharge port formed therein through which the liquid that has passed through the flow path is discharged; a discharge port protection member bonded to the discharge port forming member via an adhesive; a thin film formed on a surface of the ejection port protection member that is to be bonded to the ejection port formation member, the thin film including silicon carbide, or any one of silicon oxide containing carbon, silicon nitride, and silicon oxynitride; A liquid ejection head comprising:

2. The thin film contains the silicon oxide, and the ratio of oxygen to silicon in the silicon oxide is 5% or more and 50% or less.

2. The liquid ejection head according to claim 1.

3. the discharge port forming member is made of a material containing an epoxy resin, The discharge port protection member is made of a material containing silicon or metal.

3. The liquid ejection head according to claim 1, wherein the liquid ejection head is a liquid ejection head.

4. 4. The liquid ejection head according to claim 3, wherein the ejection port protection member is made of a material containing a corrosion-resistant metal.

5. 5. The liquid ejection head according to claim 4, wherein the ejection port protection member is made of a material containing any one of stainless steel, aluminum alloy, titanium alloy, and nickel alloy.

6. 3. The liquid ejection head according to claim 1, wherein the ejection port protection member has a thickness of 10 [mu]m or more and 50 [mu]m or less.

7. 3. The liquid ejection head according to claim 2, wherein the thin film has a ratio of silicon to oxygen of 100:

25.

8. 3. The liquid ejection head according to claim 1, wherein the thin film has a thickness of 30 nm to 100 nm.

9. 3. The liquid ejection head according to claim 1, wherein the thin film has a compressive stress of 300 MPa or more and 700 MPa or less.

10. A substrate in which a flow path for the liquid to be discharged is formed; a discharge port forming member having a discharge port formed therein through which the liquid that has passed through the flow path is discharged; a discharge port protection member that is bonded to the discharge port forming member via an adhesive in order to protect the discharge port; A method for manufacturing a liquid ejection head comprising the steps of: A method for manufacturing a liquid ejection head, comprising a step of forming a thin film containing silicon carbide or any one of silicon oxide containing carbon, silicon nitride, and silicon oxynitride on a surface of the ejection port protection member that is joined to the ejection port forming member.

11. 11. The method for manufacturing a liquid ejection head according to claim 10, wherein the thin film contains silicon oxide, and the ratio of oxygen to silicon in the silicon oxide is 5% or more and 50% or less.

12. 12. The method according to claim 10, wherein the thin film is formed by vacuum deposition. A method for manufacturing the above liquid ejection head.

13. 13. The method for manufacturing a liquid ejection head according to claim 12, wherein the thin film is formed by a plasma CVD method.

14. The method for manufacturing a liquid ejection head according to claim 12, wherein the thin film is formed by a bias RF sputtering method.

Citation Information

Patent Citations

  • inkjet recording head

    JP3108771B2