Method for adjusting characteristics of device including electret, method for manufacturing device, and electret

Irradiating electrets with light allows for post-manufacturing adjustment of surface potential, addressing the fixed nature of electret characteristics and enabling precise control of device properties.

JP2024164750APending Publication Date: 2024-11-27THE RITSUMEIKAN TRUST +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023080453
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-15
Publication Date
2024-11-27

AI Technical Summary

Technical Problem

The surface potential of electrets, which affects the characteristics and performance of devices, is determined at the time of production and cannot be adjusted post-manufacturing, limiting the ability to fine-tune device properties.

Method used

A method involving irradiation with light to adjust the surface potential of electrets, allowing for precise control of device characteristics by changing the electret's surface potential distribution.

Benefits of technology

Enables post-manufacturing adjustment of device characteristics, compensating for manufacturing errors and achieving desired performance parameters by controlling the electret's surface potential distribution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024164750000001_ABST
    Figure 2024164750000001_ABST
Patent Text Reader

Abstract

To adjust the characteristics of a device that is sensitive to a surface potential of an electret.SOLUTION: A method for adjusting the characteristics of a device including an electret, the electret is made of a material whose surface potential changes when irradiated with light, the method includes irradiating the electret with light that changes the surface potential of the electret, thereby changing the surface potential and adjusting a device characteristic that depends on the surface potential.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for adjusting the characteristics of a device including an electret, a method for manufacturing the device, and an electret. [Background technology]

[0002] An electret is a material that is electrically polarized by applying an electric field to a highly dielectric insulator, and retains its charge even after the electric field is removed. By combining an electret with an electronic circuit or MEMS (Micro Electro Mechanical Systems), it is possible to create small microphones and vibration power generation elements.

[0003] Patent Documents 1 to 3 disclose devices equipped with electrets. Patent Document 1 discloses a vibration power generator equipped with an electret, Patent Document 2 discloses a vibration power generation element equipped with an electret, and Patent Document 3 discloses a MEMS element formed with an electret. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2020-036423 A [Patent Document 2] JP 2021-040389 A [Patent Document 3] Patent Publication No. 2022-29596 Summary of the Invention

[0005] Since electrets are electrically charged, they have a surface potential. The surface potential of an electret is determined by the electret material, dimensions, charging process, etc. Therefore, the surface potential of the electret is determined at the time of its manufacture. As a result, after the electret is manufactured, it is not possible to adjust the surface potential by any method other than recharging. Note that recharging the electret is a process of returning the attenuated surface potential to its original value, and cannot be applied to control the surface potential.

[0006] The surface potential of an electret can affect the characteristics and performance of a device that includes the electret. Therefore, it is possible to use an electret to adjust the characteristics of a device that is affected by its surface potential. However, if the surface potential cannot be adjusted after the electret is manufactured, it is difficult to adjust the device characteristics.

[0007] Therefore, it is desirable to provide a technique for solving such problems or a technique related thereto.

[0008] One aspect of the present disclosure is a device adjustment method for adjusting characteristics of a device including an electret, the electret being made of a material whose surface potential changes when irradiated with light, the method including irradiating the electret with light that changes the surface potential of the electret to change the surface potential and adjusting device characteristics that depend on the surface potential.

[0009] Another aspect of the present disclosure is a method for manufacturing a device. The disclosed method is a method for manufacturing a device including an electret, comprising: providing an electret, the surface potential of which can be changed by irradiation with light, in a device; and, after providing the electret in the device, irradiating the electret with light to change the surface electrons, thereby adjusting device characteristics that depend on the surface potential.

[0010] Another aspect of the present disclosure is an electret. The disclosed electret has a controlled surface potential distribution such that the surface potential varies depending on the in-plane position on the electret surface.

[0011] Further details will be described in the following embodiments. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a flowchart showing the procedure of a device manufacturing method according to an embodiment. [Diagram 2] FIG. 2 is an explanatory diagram showing a MEMS element having an electret and vacuum deposition onto the MEMS element. [Diagram 3] FIG. 3 is an explanatory diagram showing a field effect transistor including an electret and its threshold voltage characteristics. [Figure 4] FIG. 4 is a diagram showing another example of a field effect transistor including an electret. [Diagram 5] FIG. 5 is an explanatory diagram showing an experiment of irradiating light onto an electret. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] <1. Overview of the characteristic adjustment method for a device equipped with an electret, the manufacturing method for the device, and the electret>

[0014] (1) The method according to the embodiment may be a method for adjusting the characteristics of a device including an electret. In the method, the electret may be made of a material whose surface potential changes when irradiated with light. The method may include irradiating the electret with light that changes the surface potential of the electret, thereby changing the surface potential and adjusting device characteristics that depend on the surface potential. In this case, the device characteristics can be adjusted by changing the electret surface potential through light irradiation.

[0015] The electret may be provided in the device as a component essential to the operation and function of the device, or may be provided in the device solely for adjusting the device characteristics without being an essential component to the operation and function of the device. The adjustment of the device characteristics may be performed after the electret is provided, and may be performed during the manufacture of the device (before the device is completed) or after the device is manufactured (after the device is completed).

[0016] (2) The light irradiation may be performed by irradiating a region narrower than the entire region in which the electret is formed with the light. Also, the light irradiation may be performed by irradiating the light such that at least one of the light intensity and the irradiation time varies depending on the position in the region in which the electret is formed.

[0017] (3) The light irradiation is preferably performed by a maskless exposure machine.

[0018] (4) The electret is preferably a self-assembled electret.

[0019] (5) The device may include a MEMS element having the electret, and the device characteristics may include characteristics of the MEMS element.

[0020] (6) The device may include an electronic circuit including the electret. The electronic circuit is preferably an integrated circuit. The device characteristics may include circuit characteristics of the electronic circuit.

[0021] (7) A method according to an embodiment may be a method for manufacturing a device including an electret. The method may include providing an electret, the surface potential of which can be changed by irradiation with light, in a device, and irradiating the electret with light after providing the electret in the device to change the surface electrons and adjust device characteristics that depend on the surface potential.

[0022] The electret may be provided in the device as a component essential to the operation and function of the device, or may be provided in the device solely for adjusting the device characteristics without being an essential component to the operation and function of the device. The adjustment of the device characteristics may be performed after the electret is provided, and may be performed during the manufacture of the device (before the device is completed) or after the device is manufactured (after the device is completed).

[0023] (8) The electret according to the embodiment may have a surface potential distribution that is controlled so that the surface potential varies depending on the in-plane position on the electret surface.

[0024] <2. Method for adjusting characteristics of a device provided with an electret, method for manufacturing the device, and examples of electrets>

[0025] 1 shows a device manufacturing method according to an embodiment. This manufacturing method includes, for example, a device fabrication step (step S1) and a device characteristic adjustment step (step S2).

[0026] The device fabricated in step S1 includes an electret. The device fabricated in step S1 is, for example, a MEMS (Micro Electro Mechanical Systems) element. The MEMS element constitutes, for example, a mechanical element such as an energy harvester (power generation element), a pressure sensor, an acceleration sensor, a gyroscope, an optical scanner, a digital mirror device, an actuator, a power generation element, or an optical modulator. The power generation element is, for example, a vibration power generation element. The MEMS element is, for example, an integrated MEMS element. The integrated MEMS element is a semiconductor integrated circuit (LSI) and a MEMS structure formed on a single chip.

[0027] By providing a MEMS element with an electret, which is a dielectric material that semi-permanently holds an electric charge, it is possible to improve or adjust the characteristics and performance of the MEMS element, such as improving sensor sensitivity, reducing power consumption, and providing a power generation function. The characteristics of the MEMS element that are improved or controlled by providing an electret are, for example, the mechanical characteristics of the MEMS element. The mechanical characteristics are, for example, the resonance frequency of the vibrating MEMS element, the distance between the electrodes, and the inclination of the electrodes. The characteristics of the MEMS element are not limited to these, and may be other characteristics that can change depending on the surface potential of the electret.

[0028] The MEMS element is formed, for example, on a semiconductor integrated circuit by performing microfabrication using semiconductor manufacturing technology.

[0029] The device fabricated in step S1 may be an electronic circuit such as an integrated circuit. The electronic circuit is, for example, a field effect transistor (FET). When the electronic circuit is a semiconductor integrated circuit, the electronic circuit is formed by semiconductor manufacturing technology.

[0030] By providing an electronic circuit with an electret, it is possible to improve or adjust the circuit characteristics of the electronic circuit. For example, if the electronic circuit is a FET, the characteristic of the electronic circuit that is improved or adjusted by providing the electret is the threshold voltage of the FET. The characteristic of the electronic circuit is not limited to the threshold voltage of the FET, and may be other circuit characteristics that can change depending on the surface potential of the electret.

[0031] The device fabrication process of step S1 includes an electret formation process (step S11). The electret formation process of step S11 is a process for providing an electret to a device. Note that step S1 includes, in addition to the electret formation process of step S11, a process for forming components of the device other than the electret.

[0032] In an embodiment, the electret provided on the device in step S11 may be made of a material whose surface potential changes when irradiated with light. Since the electret is a material whose surface changes when irradiated with light, it is possible to adjust or control the surface potential of the electret by irradiating it with light after the device is manufactured.

[0033] The electret provided on the device in step S11 is, for example, a self-assembled electret (SAE). The self-assembled electret is described in Patent Documents 1-3. The present disclosure incorporates all of the contents of Patent Documents 1-3 by reference. The self-assembled electret utilizes the fact that spontaneously oriented polar organic molecules function as an electret that does not require charging. The surface potential of the self-assembled electret increases in proportion to the film thickness, reaching several volts at 100 nm. This huge potential is called "giant surface potential (GSP)". In other words, the self-assembled electret can also be said to be an electret made of a material that exhibits GSP. There are many materials that can be used as the self-assembled electret, and examples include 2CzPN, 4CzIPN, Alq3, TPBi, OXD-7, and BCP.

[0034] As described above, the self-assembled electret does not require charging (charging treatment). Therefore, when the self-assembled electret is provided in a device, adverse effects on the device due to charging treatment can be avoided. That is, charging treatment requires high temperature and high voltage application, but when a self-assembled electret that does not require charging treatment is used, high temperature and high voltage application for charging treatment are not required. For example, when charging is performed to form an electret in a device such as a MEMS element or an electronic circuit, adverse effects such as destruction of the device may occur. However, when the self-assembled electret is formed in a device, charging treatment is not required, so adverse effects on the device can be suppressed. In addition, when the self-assembled electret is used, charging treatment is not required, so the productivity of the device is improved.

[0035] The self-assembled electret is formed, for example, by vacuum deposition. Vacuum deposition can be performed, for example, at room temperature. Therefore, even if the device on which the electret is to be formed is placed in a vacuum deposition apparatus for the formation of the electret, there is little effect on the device.

[0036] The surface potential of the material constituting the self-assembled electret changes when irradiated with light. For example, the surface potential of the aforementioned Alq3 decreases or disappears when irradiated with light (for the principle of the decrease in surface potential due to light irradiation, see Patent Document 2).

[0037] In the fabrication of the device of the embodiment, an electret whose surface potential can be changed by irradiation with light, such as Alq3, is used. Such an electret is, for example, the above-mentioned 2CzPN, 4CzIPN, Alq3, TPBi, OXD-7, or BCP. In general, the surface potential of a self-assembled electret changes when irradiated with light.

[0038] Here, light refers to electromagnetic waves having a wavelength of 1 nm to 1 mm, and is not limited to visible light, but also includes ultraviolet radiation (ultraviolet light). The wavelength of light for changing the surface potential is preferably short, for example, 450 nm or less, 400 nm or less, 350 nm or less, or 300 nm or less. The light for changing the surface potential is, for example, ultraviolet radiation.

[0039] The light irradiated to the electret preferably includes light having a wavelength (and a wavelength shorter than that) corresponding to the absorption peak in the absorption spectrum of the material constituting the irradiated electret. Light having a wavelength including the wavelength of the absorption peak of the electret material is absorbed by the electret, lowering the surface potential. For example, since Alq3 has an absorption peak of about 400 nm, the potential can be lowered by irradiation with light (blue light) having a wavelength of about 400 nm or less. Since 2CzPN has an absorption peak of about 380 nm, the potential can be lowered by irradiation with light (blue light) having a wavelength of about 380 nm or less. Since 4CzIPN has an absorption peak of about 390 nm, the potential can be lowered by irradiation with light (blue light) having a wavelength of about 390 nm or less.

[0040] In addition, TPBi has an absorption peak of about 310 nm, so the potential can be reduced by irradiation with light (ultraviolet rays) with a wavelength of about 310 nm or less. OXD-7 has an absorption peak of about 290 nm, so the potential can be reduced by irradiation with light (ultraviolet rays) with a wavelength of about 290 nm or less. BCP has an absorption peak of about 260 nm, so the potential can be reduced by irradiation with light (ultraviolet rays) with a wavelength of about 260 nm or less.

[0041] In addition, the electret does not need to be a self-assembled electret, and may be an electret obtained by a charging process, as long as the surface potential can be changed by irradiation with light. Furthermore, the electret is not limited to an electret whose surface potential is decreased by irradiation with light, and may be an electret whose surface potential is increased. An electret whose surface potential is increased by irradiation with light is, for example, TPBi formed on an insulator. This TPBi is SAE. When this TPBi is irradiated with light, the surface potential increases. The insulator is formed on a conductive substrate. The insulator is, for example, SiO2. The conductive substrate is, for example, ITO.

[0042] After the device is fabricated in step S1, the device characteristics are adjusted in step S2. The device characteristics adjusted in step S2 are, for example, the mechanical characteristics of the MEMS element or the circuit characteristics of the electronic circuit. In step S2, among the device characteristics, the device characteristics that depend on the surface potential of the electret included in the device can be adjusted.

[0043] The adjustment step of step S2 includes a step of irradiating the electret with light (step S21). By irradiating the electret with light, the surface potential of the electret can be adjusted. As a result of adjusting the surface potential, the device characteristics that depend on the surface potential can be adjusted.

[0044] The surface potential of a self-assembled electret is usually determined by the film thickness. Therefore, the surface potential is determined at the time when the self-assembled electret is formed. However, a self-assembled electret irradiated with light has a surface potential different from the surface potential determined by the film thickness. Therefore, even if the surface potential deviates from the desired value due to a manufacturing error in the film thickness, the surface potential can be adjusted to the desired value by irradiating with light after the electret is formed.

[0045] In this way, the surface potential of the electret can be set to a desired value by irradiating the electret after fabrication with light. In addition, in the case of conventional electrets, the surface potential of the electret is determined at the stage of fabricating the electret, but according to the present embodiment, the electret fabrication process can be separated from the process of determining the final surface potential or surface potential distribution of the electret.

[0046] For example, in the case of a self-assembled electret, the surface potential distribution in the film plane is determined by the film thickness distribution. However, a self-assembled electret irradiated with light has a controlled surface potential distribution that is different from the surface potential distribution determined by the film thickness distribution. Here, controlling the electret surface potential distribution after the electret is fabricated is called in-plane potential control. A controlled surface potential distribution is obtained by in-plane potential control. For example, an electret having a nearly uniform film thickness usually has a nearly uniform distribution of surface potential, but by applying in-plane potential control to an electret having a nearly uniform film thickness, a surface potential distribution in which the surface potential varies depending on the position in the plane is obtained.

[0047] The electric potential distribution in the electret surface can be controlled by varying at least one of the intensity and time of light irradiated in the electret surface. The light intensity may be expressed as the illuminance of the light. The electric potential distribution in the electret surface can be controlled by irradiating light locally in the electret surface.

[0048] In this way, the surface potential of the electret can be locally decreased or locally eliminated by controlling the in-plane potential of the electret after fabrication. Therefore, a desired surface potential distribution can be obtained by controlling the in-plane potential of the electret after fabrication.

[0049] When the potential is locally eliminated in an electret, it is possible to produce a portion in which the electret material is present but which does not function as an electret. Here, the term "trimming" refers to locally eliminating the potential or lowering the potential to a level where the electret does not substantially function by controlling the in-plane potential. Trimming allows the region that functions as an electret to be narrower than the region in which the electret material is present.

[0050] For example, if the region where the electret is formed is larger than the desired region due to an error during the electret production, the unnecessary region can be trimmed by light irradiation. Also, by trimming after the electret production, the region that functions as the electret can be made to have a shape different from the electret region obtained in the electret formation process (for example, a predetermined pattern shape).

[0051] Furthermore, when preparing the electret, the electret is formed without giving any particular consideration to the area to be made to function as the electret, and after preparing the electret, the area to be made to function as the electret is determined, and the areas other than the area to be made to function as the electret are trimmed.

[0052] In this way, by controlling the in-plane potential, it is possible to compensate for errors during the fabrication of the electret, and to set the region that functions as an electret after the electret is fabricated to a desired range.

[0053] Furthermore, by precisely controlling the in-plane potential, the surface potential distribution can be precisely controlled. Precise in-plane potential control can be performed, for example, by an exposure machine that generates a precise exposure pattern. By using the exposure machine, localized light irradiation of the electret is possible. The exposure machine is, for example, a semiconductor exposure machine used for manufacturing semiconductor circuits. The exposure machine is preferably a maskless exposure machine that does not require a photomask to form the exposure pattern.

[0054] The exposure machine is preferably capable of irradiating light having an exposure line width of 100 μm or less, 50 μm or less, 20 μm or less, or 10 μm or less. The minimum exposure line width of the exposure machine is preferably 10 μm or more, the minimum exposure line width of the exposure machine is preferably 1 μm or more, and the minimum exposure line width of the exposure machine is preferably 0.1 μm or more, or 0.01 μm or more.

[0055] As described above, when the surface potential of the electret included in the device is adjusted, the device characteristics that depend on the surface potential of the electret are adjusted. Therefore, the device characteristics can be adjusted to a desired value through the adjustment of the surface potential of the electret. For example, the manufacturing error of the device characteristics (e.g., the mechanical characteristics or circuit characteristics of the device) can be compensated for after the device is manufactured by adjusting the surface potential of the electret.

[0056] In particular, the use of an exposure machine that generates a precise exposure pattern enables in-plane potential control of electrets in microdevices such as MEMS elements or integrated circuits. Precision trimming is also possible. Precise in-plane potential control or precise trimming also enables precise control of device characteristics. Furthermore, the use of an exposure machine that generates a precise exposure pattern enables precise in-plane potential control to obtain a desired two-dimensional potential distribution.

[0057] The electric potential distribution obtained by the method of the embodiment includes, for example, an electric potential distribution that changes smoothly two-dimensionally, an electric potential distribution having locally different electric potentials, an electric potential distribution in which some electric potentials have disappeared, etc. It is expected that the use of an electret having such an electric potential distribution will lead to the creation of new MEMS devices or electronic devices.

[0058] The light irradiation does not necessarily have to be for reducing or eliminating the surface potential, and for an electret whose surface potential increases by light irradiation, the light irradiation can be used to increase the surface potential. In addition, in FIG. 1, the light irradiation in step S21 is performed after the device is fabricated, but the light irradiation in step S21 may be performed during the device fabrication. In other words, the device including the electret does not have to be a finished product, and may be in the middle of fabrication. Therefore, after step S2 or step S21, assembly or formation of other elements constituting the device may be performed.

[0059] FIG. 2 shows an example of a process for forming a self-organized electret on a MEMS element as an example of a device. In FIG. 2, a vacuum deposition apparatus 100 is used to form the self-organized electret. The vacuum deposition apparatus 100 is configured to evaporate a film-forming material 101 in a vacuum container 100A to form a film on the surface of a workpiece such as a device. The vacuum deposition apparatus 100 shown in FIG. 2 includes a holder 103 that holds the workpiece in the container 100A, and a shadow mask 105. The shadow mask 105 limits the film-forming range.

[0060] 2 uses a self-organizing electret material as a film forming material in the vacuum deposition apparatus 100. The self-organizing electret material used is, for example, Alq3.

[0061] 2, a device 50 including a MEMS element 54 is disposed as the workpiece. The device 50 is, for example, an integrated MEMS device. The integrated MEMS device is one in which a semiconductor integrated circuit and a MEMS element are formed on a single chip.

[0062] The device 50 includes a substrate 51. The substrate 51 is formed of a semiconductor substrate such as a silicon substrate, and includes a semiconductor integrated circuit 52 such as an LSI. The semiconductor integrated circuit 52 also includes a semiconductor sensor 53 other than a MEMS element 54. The MEMS element 54 is provided on the semiconductor integrated circuit 52. The semiconductor integrated circuit 52 may include various semiconductor elements such as a FET, a resistor element, and a capacitor element. The FET may constitute an arithmetic circuit, a memory circuit, an amplifier circuit, or the like.

[0063] 2 is a vibration power generating element, for example. The vibration power generating element 54 includes a movable electrode 61 and a fixed electrode 62. The fixed electrode 62 is fixed onto, for example, the semiconductor integrated circuit 52. The movable electrode 61 is provided at a distance from the fixed electrode 62. The movable electrode 61 is supported on the integrated circuit so as to be vibrable, for example, via a support portion 63 provided on the semiconductor integrated circuit 52. The support portion 63 includes a spring, and the spring enables the movable electrode 61 to vibrate. That is, the movable electrode 61 is provided so that the relative position of the movable electrode 61 with respect to the fixed electrode 62 can be changed.

[0064] In the MEMS element 54, a self-assembled electret 71 is formed by vacuum deposition using a vacuum deposition apparatus 100. In FIG. 2, as an example, the self-assembled electret 71 is disposed on a fixed electrode 62. The electrode 62 including the electret 71 is charged. When the electrode 62 including the electret 71 faces another electrode 61, an induced charge is generated in the electrode 61 by electrostatic induction. When the electrode 61 and the electrode 62 are displaced relative to each other, the induced charge changes in response to the displacement, and the induced charge can be outputted to the outside as an electrical signal.

[0065] The movable electrode 61 in Fig. 2 has a plurality of through holes 61a. The through holes 61a are for allowing the film forming material evaporated in the vacuum deposition apparatus 100 to pass through and reach the fixed electrode 62. The fixed electrode 62 has electrets 71 formed in a pattern corresponding to the formation pattern of the through holes 61a (for example, the grid pattern in Fig. 2).

[0066] 2, when the self-assembled electret 71 is disposed on the MEMS element 54, no charging process is required, which may adversely affect the semiconductor integrated circuit 52 or the MEMS element 54. A low-temperature process (approximately room temperature) using vacuum deposition is also unlikely to adversely affect the semiconductor integrated circuit 52 or the MEMS element 54. Details of such a MEMS element 54 and its manufacturing method are described in Patent Document 3. The present disclosure incorporates all of the contents of Patent Document 3 by reference.

[0067] When the electret 71 is formed, the electret is irradiated with light in order to adjust the characteristics of the MEMS element 54. The above-mentioned through-hole 61a is also used to allow light irradiated from above the electrode 61 to pass therethrough and reach the electrode 62.

[0068] By irradiating the electret 71 with light, the surface potential of the electret 71 can be controlled, and the strength of the electrostatic attraction force generated by the surface potential can be controlled. Here, the electrostatic attraction force is a force that acts in a direction in which structures attract each other when there is a potential difference between the structures across an air gap. Here, it is a force that acts between the electrodes 61 and 62. The electrostatic attraction force is one of the characteristics of the MEMS element 54.

[0069] By controlling the surface potential of the electret 71, it is possible to change the electrostatic attractive force generated by the surface potential, and therefore it is possible to change the resonance frequency or the distance between the electrodes 61, 62 of the MEMS element 54, which is a vibration power generation element. The resonance frequency and the distance between the electrodes are mechanical characteristics of the MEMS element 54. By irradiating light, it is possible to adjust the resonance frequency or the distance between the electrodes after the MEMS element 54 is fabricated.

[0070] By irradiating light locally within the entire region of the electret 71, it is possible to control the distribution of the surface potential of the electret 71. In other words, it is possible to make the surface potential different depending on the position. By controlling the distribution of the surface potential, it is possible to make the electrostatic attractive force different depending on the position, and therefore it is also possible to adjust the degree of inclination of the electrode 61. The inclination of the electrode 61 is a mechanical characteristic of the MEMS element 54.

[0071] The movable electrode 61 may not be parallel to the substrate 51 due to dimensional variations in the springs that hold it or the influence of elements. In this case, the inclination of the electrode 61 can be adjusted by controlling the distribution of the surface potential of the electret 71 below the movable electrode 61 and varying the strength of the electrostatic attraction depending on the position. Therefore, after the movable electrode 61 is fabricated, the inclination of the movable electrode 61 can be adjusted to make it parallel.

[0072] Alternatively, an electret may be formed on the side surface of the movable electrode 61 and / or on a fixed electrode arranged to the side of the movable electrode 61, and the electret may be irradiated with light. In this case, the electrostatic attraction also acts in a direction parallel to the surface of the movable electrode 61 (horizontal direction). Therefore, by controlling the electrostatic attraction in the horizontal direction by irradiating the electret with light, it is possible to adjust the horizontal position of the movable electrode 61. The horizontal position of the movable electrode 61 is also one of the mechanical characteristics of the MEMS element 54. To form an electret on the side surface of the movable electrode 61 and / or on a fixed electrode arranged to the side of the movable electrode 61, the MEMS element 54 in FIG. 2 may be tilted and placed in the vacuum deposition apparatus 100.

[0073] FIG. 3A shows an electronic circuit (semiconductor integrated circuit) including a FET as another example of a device. FIG. 3 shows an N-channel MOSFET 80 as an example. The FET 80 shown in FIG. 3 is made up of a p-type semiconductor (p-Si) 81 and an n-type semiconductor (N +The FET 80 includes n-type semiconductor layers 82 and 83, and a dielectric (insulating film) 84 made of an oxide film. The FET 80 includes a gate electrode 85 provided on the dielectric 84, a source electrode 86 provided on the n-type semiconductor 82, a drain electrode 87 provided on the n-type semiconductor 83, and a backgate electrode 89.

[0074] FET 80 illustratively comprises an electret 88 disposed between dielectric 84 and gate electrode 85. The electret in this case is a self-assembled electret (SAE).

[0075] By providing the FET 80 with the electret 88, the threshold voltage Vgs of the FET 80 changes as shown in FIG. 3B. Here, the threshold voltage Vgs is a voltage applied between the gate and source to form a conductive path between the source and drain. The threshold voltage Vgs is one of the circuit characteristics of the FET 80.

[0076] 3B, when an electret 88 with a negative surface potential is provided, Vgs is smaller than that without the electret due to the self-bias of the electret 88. Also, when an electret with a positive surface potential is provided, Vgs is larger than that without the electret due to the self-bias of the electret 88.

[0077] When the electret 88 is irradiated with light to change the surface potential, the threshold voltage Vgs changes because the self-bias of the electret 88 changes. Therefore, the threshold voltage Vgs of the FET 80 can be adjusted by irradiating it with light.

[0078] A semiconductor integrated circuit generally includes a large number of FETs. The threshold voltages Vgs of these FETs may vary due to manufacturing errors. When there is an FET whose threshold voltage Vgs is to be adjusted among the multiple FETs included in the semiconductor integrated circuit, it is possible to adjust only the threshold voltage Vgs of that FET without changing the threshold voltages of the other FETs by locally irradiating light only onto the electret 88 of that FET. It is preferable that the electrode 85 is light-transmitting.

[0079] As for a p-type MOSFET having an electret similar to that shown in FIG. 3, the threshold voltage Vgs can be adjusted in a similar manner.

[0080] Fig. 4 shows another example of a FET equipped with an electret. The FET 80 shown in Fig. 4 is different from the FET 80 in Fig. 3 in that an electret 88 is provided between a p-type semiconductor 81 and a backgate electrode 89. The FET 80 in Fig. 4 is otherwise similar to the FET 80 in Fig. 3.

[0081] 4, the threshold voltage Vgs changes due to the electret 88. That is, when an electret 88 with a negative surface potential is provided, Vgs becomes smaller than when no electret is provided due to the self-bias of the electret 88. Also, when an electret with a positive surface potential is provided, Vgs becomes larger than when no electret is provided due to the self-bias of the electret 88.

[0082] In the case of a semiconductor integrated circuit having multiple FETs, a structure for other FETs is also formed in the p-type semiconductor in Fig. 4. That is, multiple FETs 80 are provided on a semiconductor 81 (semiconductor substrate 81) in Fig. 4. The electret 88 is formed across the multiple FETs 80 by, for example, forming it on the entire surface of the semiconductor 81. Therefore, the electret 88 in Fig. 4 affects the threshold voltage Vgs of each of the multiple FETs 80.

[0083] The threshold voltage Vgs of a specific FET can be adjusted by locally irradiating light onto the electret 88, which affects the threshold voltage Vgs of each of the multiple FETs 80. For example, if there is a specific FET among the multiple FETs whose threshold voltage Vgs is to be adjusted, the electret 88 can be irradiated with light locally only at the position corresponding to that FET, thereby adjusting only the threshold voltage Vgs of that FET without changing the threshold voltages of the other FETs.

[0084] If the electrode 89 is light transmissible, the threshold voltage can be adjusted after the formation of the electrode 89. Moreover, if the threshold voltage is adjusted before the formation of the electrode 89 as described below, the electrode 89 does not need to be light transmissible.

[0085] First, in a semiconductor integrated circuit having the FET structure shown in FIG. 4, before the electret 88 and the back gate electrode 89 are formed, the FET 80 is operated using the top gate electrode 85 or the like to confirm the threshold voltage of the FET. As a result, if there is an FET among the multiple FETs whose threshold voltage is deviated from the threshold voltages of the other FETs, that FET is identified as a target FET. Then, the electret 88 shown in FIG. 4 is formed. Then, light is irradiated locally onto the electret 88 only at a position among the multiple FETs that corresponds to the target FET. This compensates for the deviation in the threshold voltage of the target FET. After that, the back gate electrode 89 can be formed.

[0086] If necessary, the surface potential of the electret 88 at positions corresponding to FETs other than the target FET may be eliminated by light irradiation. For example, light intensity or time is set so that the potential of the electret 88 is eliminated for positions corresponding to FETs other than the target FET in the entire area of ​​the electret 88. This makes it possible to prevent the threshold voltage of FETs other than the target FET from being changed by the electret 88.

[0087] Alternatively, the following may be performed. In a semiconductor integrated circuit, before the back gate electrode 89 is formed, an electret 88 is formed over a plurality of FETs on a semiconductor substrate 81 of a FET 80 shown in FIG. 4. The electret 88 is formed, for example, on the entire surface of one surface of the substrate 81. For example, the electret 88 is formed so as to lower the threshold voltage of all FETs included in the integrated circuit. This can reduce the power consumption of the semiconductor integrated circuit. Also, before or after the formation of the electret 88, the FETs are operated to identify the target FETs that require compensation for their threshold voltages. Then, light irradiation of the electret 88 is performed locally only at a position corresponding to the target FET among the plurality of FETs. This compensates for the deviation in the threshold voltage of the target FET. After that, the back gate electrode 89 may be formed. In this case, it is not necessary to eliminate the surface potential of the electret 88 at a position corresponding to the FETs other than the target FET.

[0088] FIG. 5 shows an experiment on in-plane potential control of an electret. FIG. 5(A) shows the experimental method. In the experiment, a film of Alq3, which is a self-organizing electret (SAE), was formed on an ITO film formed on glass. The ITO film was a square with a side of 30 mm, and the Alq3 film was a square with a side of 20 mm. This Alq3 film was irradiated with ultraviolet light (irradiation wavelength: 365 nm) using a maskless exposure machine with the exposure pattern 10 shown in FIG. 5. The maskless exposure machine used was a maskless exposure device "PALET" manufactured by Neoark Corporation. The exposure line width was 15 μm.

[0089] The exposure pattern 10 shown in FIG. 5(A) has 12 exposure areas in the in-plane range of the Alq3 film. The exposure areas are areas to which light is irradiated. In FIG. 5, the white areas A11, A12, A13, A21, A22, A23, A31, A32, A33, A41, A42, and A43 are the exposure areas. Each exposure area has a rectangular shape with a short vertical side length of 3 mm and a long horizontal side length of 5 mm. A space is secured between each exposure area in both the horizontal and vertical directions. In the exposure pattern 10 shown in FIG. 5, the gray non-exposed areas are areas to which light is not irradiated. In this way, in the experiment, light is irradiated locally within the plane of the electret.

[0090] In the experiment, the exposure conditions (light irradiation conditions) of each exposure area were different. That is, the illuminance (light intensity) was changed to three levels and the exposure time (irradiation time) was changed to four levels for the 12 exposure areas, and ultraviolet rays were irradiated. As shown in Fig. 5, the exposure time was set to 0.1 [sec] for the exposure areas A11, A12, and A13, 1.0 [sec] for the exposure areas A21, A22, and A23, 10 [sec] for the exposure areas A31, A32, and A33, and 100 [sec] for the exposure areas A41, A42, and A43. In addition, the illuminance (light intensity) of exposure areas A13, A23, A33, and A43 was set to 100%, the illuminance (light intensity) of exposure areas A11, A21, A31, and A41 was set to 10% of that, and the illuminance (light intensity) of exposure areas A12, A22, A32, and A42 was set to 50% of that.

[0091] The surface potential on the Alq3 film was measured before and after exposure, and the potential of each exposed area was evaluated after exposure. A scanning Kelvin probe was used to measure the surface potential. Before exposure, the surface potential of the Alq3 film was approximately 1800 mV, with a nearly uniform distribution across its surface.

[0092] After exposure, some of the exposed areas had a reduced or lost potential. The numbers [%] in each exposed area in Figure 5(B) indicate the potential retention rate of each exposed area. The potential retention rate indicates the ratio of the potential after exposure to the potential before exposure (approximately 1800 mV).

[0093] As shown in FIG. 5(B), the potential retention rate of the exposure area A11 is approximately 100%. The potential retention rate of the exposure area A12 is approximately 90%. The potential retention rate of the exposure area A13 is approximately 80%. The potential retention rate of the exposure area A21 is approximately 85%. The potential retention rate of the exposure area A22 is approximately 70%. The potential retention rate of the exposure area A23 is approximately 55%. The potential retention rate of the exposure area A31 is approximately 75%. The potential retention rate of the exposure area A32 is approximately 55%. The potential retention rate of the exposure area A33 is approximately 40%. The potential retention rates of the exposure areas A41, A42, and A43 are approximately 0%.

[0094] As shown in FIG. 5(B), it can be seen that the surface potential of the exposed area decreases in proportion to the increase in illuminance (light intensity) and / or exposure time. This experiment demonstrated that it is possible to control the in-plane potential of the electret. It can also be seen that the potential can be changed locally within the electret surface by locally changing the light intensity (illuminance) or irradiation time (exposure time). In this way, by controlling the irradiation pattern of the electret, it is possible to control the potential distribution within the electret surface to a desired distribution. The electret obtained in the experiment has a surface potential distribution controlled so that the surface potential differs depending on the in-plane position of the electret surface, as shown in FIG. 4(B).

[0095] The present invention is not limited to the above-described embodiment, and various modifications are possible. [Explanation of symbols]

[0096] 10: Exposure pattern 50 : Device 51: Substrate 52: Semiconductor integrated circuits 53: Semiconductor sensor 54: MEMS elements 61: Movable electrode 61a :Through hole 62: Fixed electrode 63: Support part 71: Electret 80:FET 81: p-type semiconductor 82: n-type semiconductor 83: n-type semiconductor 84: Dielectric 85: Gate electrode 86: Source electrode 87: Drain electrode 88: Electret 89: Back gate electrode 100: Vacuum deposition equipment 100A: Container 101: Film forming materials 103: Holder 105: Shadow Mask A11: Exposure area A12: Exposure area A13: Exposure area A21: Exposure area A22: Exposure area A23: Exposure area A31: Exposure area A32: Exposure area A33: Exposure area A41: Exposure area A42: Exposure area A43: Exposure area AA23: Exposure area

Claims

1. 1. A method for adjusting a property of a device comprising an electret, comprising: The electret is made of a material whose surface potential changes when irradiated with light, The method includes irradiating the electret with light that changes the surface potential of the electret, thereby changing the surface potential and adjusting a device characteristic that depends on the surface potential. How to characterize a device.

2. The irradiating with light includes Irradiating the light to an area narrower than the entire area in which the electret is formed, or The light is irradiated so that at least one of the light intensity and the irradiation time is different depending on the position in the region where the electret is formed. A method for adjusting characteristics of a device according to claim 1.

3. The light irradiation is performed by a maskless exposure machine. A method for adjusting characteristics of a device according to claim 1.

4. The electret is a self-assembled electret A method for adjusting characteristics of a device according to claim 1.

5. The device comprises a MEMS element comprising the electret, The device characteristics include characteristics of the MEMS element. A method for adjusting characteristics of a device according to any one of claims 1 to 4.

6. The device comprises an electronic circuit comprising the electret, The device characteristics include circuit characteristics of the electronic circuit. A method for adjusting characteristics of a device according to any one of claims 1 to 4.

7. A method for manufacturing a device comprising an electret, comprising the steps of: An electret whose surface potential can be changed by irradiation with light is provided on the device; After the electret is provided on the device, the electret is irradiated with the light to change the surface potential, thereby adjusting device characteristics that depend on the surface potential. A method for manufacturing a device, comprising:

8. An electret having a surface potential distribution controlled so that the surface potential varies depending on the in-plane position on the electret surface.

Citation Information

Patent Citations

  • Vibration power generator and electret

    JP2020036423A

  • Vibration power generating element

    JP2021040389A

  • Fine element manufacturing method and fine element

    JP2022029596A