Semiconductor manufacturing apparatus

The semiconductor manufacturing apparatus addresses the challenge of grinding both sides of wafers simultaneously by using a central holding mechanism and a grinding part to efficiently remove protrusions on both surfaces, enhancing processing efficiency.

JP2024166530AActive Publication Date: 2024-11-29MITSUBISHI ELECTRIC CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023082686
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2024-11-29
Estimated Expiration
2043-05-19

AI Technical Summary

Technical Problem

Conventional wafer grinding devices that remove back surface protrusions on wafers while holding the front surface cause issues with surface protrusions remaining unaddressed, as they cannot effectively grind both sides of the wafer simultaneously.

Method used

A semiconductor manufacturing apparatus that includes a first main surface holding part to hold the wafer centrally and a first grinding part to grind the outer circumference, allowing simultaneous grinding of both sides of the wafer.

Benefits of technology

Enables efficient grinding of both the back and front surfaces of wafers in a shorter time, improving throughput by eliminating the need to reverse and re-load the wafer, and facilitating simultaneous processing on the opposite surface.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024166530000001_ABST
    Figure 2024166530000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor manufacturing apparatus that is capable, while holding one surface of a wafer, grinding the holding surface.SOLUTION: A semiconductor manufacturing apparatus includes: a first main surface holding unit 1 which comes into contact with a center portion of a first main surface 10a of a wafer 10 in plan view and holds the wafer 10; and a first grinding unit 3 which rotates about a rotation axis 9 that overlaps a center of the wafer 10 in plan view and that extends in a direction perpendicular to the first main surface 10a, and which grinds an outer periphery of the first main surface 10a in contact with the outer periphery, the outer periphery being a region surrounding the center portion of the first main surface 10a.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to semiconductor manufacturing equipment. [Background technology]

[0002] When an epitaxial layer is formed by epitaxial growth on the surface of a wafer, which is a SiC substrate constituting a semiconductor device, a conical protrusion called a backside protrusion may occur on the backside of the wafer, particularly on the outer periphery, and a ring-shaped protrusion called an epicrown may occur along the outer periphery of the wafer, particularly on the outer periphery. The occurrence of a backside protrusion or epicrown can cause problems such as defocusing in the photolithography process of the semiconductor device manufacturing process.

[0003] Regarding protrusions on wafers, Patent Document 1 describes a grinding device that holds the wafer on the front side of the wafer and rotates a polishing plate with a cavity in the center to abut against the outer periphery of the back side of the wafer, thereby removing protrusions that occur on the outer periphery of the back side of the wafer. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 58-114849 Summary of the Invention [Problem to be solved by the invention]

[0005] The apparatus described in Patent Document 1 is an apparatus that grinds the back surface of a wafer while holding the front surface of the wafer, and there was a problem in that when removing back surface protrusions that have occurred on the back surface of the wafer, it was not possible to simultaneously perform other processes on the front surface, such as removing front surface protrusions that have occurred on the front surface.

[0006] The present disclosure has been made to solve the problems described above, and aims to provide a semiconductor manufacturing apparatus that is capable of holding one side of a wafer and grinding the surface that is being held. [Means for solving the problem]

[0007] The semiconductor manufacturing apparatus according to the present disclosure includes a first main surface holding unit that contacts a central portion of a first main surface of a wafer in a planar view and holds the wafer, and a first grinding unit that rotates about a rotation axis that overlaps with the center of the wafer in a planar view and extends in a direction perpendicular to the first main surface, and contacts an outer periphery, which is a region surrounding the central portion of the first main surface, to grind the outer periphery of the first main surface. Effect of the Invention

[0008] According to the present disclosure, the first grinding unit can grind the outer periphery of the first main surface while the first main surface holding unit holds the wafer in contact with the center of the first main surface of the wafer. This makes it possible to simultaneously perform another process on the surface opposite to the first main surface, thereby achieving the effect of processing both sides of the wafer in a short time. [Brief description of the drawings]

[0009] [Figure 1] 1 is a plan view showing an overview of a semiconductor manufacturing apparatus according to a first embodiment. [Diagram 2] 1 is a cross-sectional view showing an overview of a semiconductor manufacturing apparatus according to a first embodiment. [Diagram 3] 1A to 1C are cross-sectional views illustrating a semiconductor manufacturing process according to a first embodiment. [Figure 4] 1A to 1C are cross-sectional views illustrating a semiconductor manufacturing process according to a first embodiment. [Diagram 5] 1A to 1C are cross-sectional views illustrating a semiconductor manufacturing process according to a first embodiment. [Figure 6] 1A to 1C are cross-sectional views illustrating a semiconductor manufacturing process according to a first embodiment. [Figure 7] 1A to 1C are cross-sectional views illustrating a semiconductor manufacturing process according to a first embodiment. [Figure 8] 11 is a cross-sectional view showing an overview of a semiconductor manufacturing apparatus according to a second embodiment. [Figure 9] FIG. 11 is a cross-sectional view showing an overview of a semiconductor manufacturing apparatus according to a third embodiment.

[0010] In this disclosure, the first main surface of the wafer may be referred to as the wafer back surface, and the second main surface opposite the first main surface may be referred to as the wafer front surface. The upward direction in the vertical direction may be referred to as the up (upward direction), and the opposite direction may be referred to as the down (downward direction). The vertical direction is the direction perpendicular to the first and second main surfaces of the wafer when the wafer is placed on the device, and the horizontal direction is the direction perpendicular to the vertical direction. The plan view is the view from a direction perpendicular to the first and second main surfaces of the wafer when the wafer is placed on the device, and the cross-sectional view is the view from a direction parallel to the first and second main surfaces of the wafer.

[0011] <Embodiment 1> An overview of a semiconductor manufacturing apparatus 101 according to a first embodiment will be described. FIG. 1 is a plan view showing an overview of the semiconductor manufacturing apparatus 101 as viewed from above, and FIG. 2 is a cross-sectional view showing the AA section of the semiconductor manufacturing apparatus 101 in FIG. 1. Although FIG. 1 and FIG. 2 show the semiconductor manufacturing apparatus 101, they only show the main components for the structure, action, and effect of the present disclosure, and do not show the apparatus housing, driving unit (including motor and cylinder), etc., which may be optionally configured. Also, FIG. 2 shows the semiconductor manufacturing apparatus 101 in a state in which a wafer 10, indicated by a dotted line, is placed and held in the apparatus, in order to make the explanation of each component easier to understand.

[0012] 1 and 2, the semiconductor manufacturing apparatus 101 includes a back surface holding unit 1, which is a first main surface holding unit that holds the wafer 10 by contacting the wafer back surface 10a, which is the first main surface of the wafer 10, an end surface holding unit 2 that holds the wafer 10 by contacting the wafer end surface, which is the end surface of the outer periphery of the wafer 10, a first grinding unit 3 that is disposed facing the wafer back surface 10a and that grinds the outer periphery of the wafer back surface 10a, and a second grinding unit 6 that is disposed facing the wafer front surface 10b, which is the second main surface of the wafer 10 and is the opposite surface to the wafer back surface 10a, and that grinds the wafer front surface 10b by contacting the wafer front surface 10b. The wafer 10 includes a Si layer 11 on the wafer back surface 10a side, and an epitaxial layer 12 on the wafer front surface 10b side. Each of the configurations will be described in detail below.

[0013] The back surface holding part 1 is provided inside the device housing (not shown) and is a holding means that holds the wafer 10 by contacting the center of the wafer back surface 10a. The holding surface 1a of the back surface holding part 1 that contacts the wafer 10 is flat, and is further provided with a suction port (not shown) connected to a separately provided vacuum pump (not shown). When the holding surface 1a contacts the wafer back surface 10a, the vacuum pump is operated to vacuum-suck the wafer 10 onto the holding surface 1a and hold it. Note that the back surface holding part 1 is not limited to such a vacuum suction type, and may be any as long as it can hold the wafer 10.

[0014] The edge surface holding parts 2 are holding means that hold the wafer 10 by contacting the edge surface of the wafer. The edge surface holding parts 2 are attached to an apparatus housing (not shown), and hold the wafer 10 by pressing the edge surface of the wafer toward the center of the wafer 10 with an air cylinder (not shown) connected to an edge surface holding plate having the same thickness as the wafer 10. In FIG. 2, the edge surface holding parts 2 are shown holding the wafer 10, but when the holding is released, each edge surface holding part 2 retreats toward the outside from the wafer 10. The edge surface holding parts 2 do not need to contact the entire circumference of the wafer edge surface, and may be provided at multiple points so as to face each other with the wafer 10 in between. In this embodiment, the edge surface holding parts 2 are provided at four outside points of the outer peripheral end of the wafer 10 as shown in FIG. 1. The edge surface holding parts 2 prevent the outer peripheral part of the wafer 10 from moving up and down in the front-back direction and the wafer 10 from shifting laterally during grinding.

[0015] The edge surface holding part 2 is not limited to a structure in which an edge surface holding plate is pressed by an air cylinder, and may be a structure in which an elastic edge surface holding plate is pressed, for example. The edge surface holding part 2 may have a plurality of edge surface holding plates. Note that, as long as the wafer 10 can be held without coming off or shifting during grinding, if either the back surface holding part 1 or the edge surface holding part 2 has sufficient holding force, the other may not be provided.

[0016] The first grinding unit 3 is disposed facing the wafer back surface 10a and grinds the outer periphery of the wafer back surface 10a, and is composed of an abrasive, such as a grindstone containing diamond abrasive grains. The first grinding unit 3 is annular in plan view, and has a first cutout portion 5 which is a hollowed-out area in the center. The back surface holding unit 1 is disposed so as to overlap the first cutout portion 5 in plan view, and abuts against the center of the wafer back surface 10a to hold the wafer 10. The first grinding unit 3 is attached to a first grinding stage 4.

[0017] The first grinding stage 4 is connected to a first motor (not shown) that rotates the first grinding stage 4. When the first motor rotates, the first grinding stage 4 and the first grinding unit 3 attached thereto rotate about a rotation axis 9 that is perpendicular to the holding surface 1a of the backside holding unit 1, i.e., perpendicular to the wafer backside 10a. The first motor is connected to a control unit (not shown) that can arbitrarily set the rotation direction and rotation speed.

[0018] The first grinding stage 4 is also connected to a first vertical drive unit (not shown) that moves the position of the first grinding stage 4 up and down in a direction perpendicular to the holding surface 1a. When the first vertical drive unit is driven, the first grinding unit 3 moves up and down together with the first grinding stage 4, and the presence or absence of contact with the wafer back surface 10a is controlled. The semiconductor manufacturing equipment 101 further has a first sensor (not shown) that detects the position of the first grinding stage 4 in the direction perpendicular to the holding surface 1a. The first vertical drive unit and the first sensor are connected to a control unit, and the first vertical drive unit is controlled based on position information from the first sensor, making it possible to move the position of the first grinding stage 4 up and down.

[0019] The second grinding unit 6 is disposed facing the wafer surface 10b and grinds the outer periphery of the wafer surface 10b. The second grinding unit 6 is attached to a second grinding stage 7. The semiconductor manufacturing apparatus 101 further includes a second motor (not shown) that rotates the second grinding stage 7 around a rotation axis 9, a second vertical drive unit (not shown) that varies the position of the second grinding stage 7 in a direction perpendicular to the holding surface 1a, and a second sensor (not shown) that detects the position of the second grinding stage 7 in a direction perpendicular to the holding surface 1a. The configurations and functions of the second motor, the second vertical drive unit, and the second sensor are similar to those of the first motor, the first vertical drive unit, and the first sensor, respectively, and therefore will not be described.

[0020] While the first grinding unit 3 has a first cutout 5 in the center, the second grinding unit 6 also has a second cutout 8, which is an area obtained by cutting out the center of the second grinding unit 6 and the second grinding stage 7. However, instead of the second cutout 8, the second grinding unit 6 may have a recess in the area of ​​the second cutout 8, in which the second grinding unit 6 is recessed in a direction away from the second main surface. By providing the second cutout 8 or the recess, the second grinding unit 6 comes into contact only with the outer periphery of the wafer surface 10b, and only the outer periphery of the wafer surface 10b can be ground.

[0021] When the grinding of the wafer 10 is performed by a wet method, a water supply section (not shown) may be provided to supply a liquid such as water between the wafer back surface 10a and the first grinding section 3 and between the wafer front surface 10b and the second grinding section 6 during grinding.

[0022] Next, the operation of the semiconductor manufacturing apparatus 101 in the semiconductor manufacturing process will be described. The following description is of the wafer manufacturing process in the semiconductor manufacturing process, and more specifically, of the operation of the semiconductor manufacturing apparatus 101 in the wafer grinding process after the epitaxial growth process. Note that the figures shown in the description are cross-sectional views that show a schematic diagram of the wafer grinding process, and show the same cross section of the semiconductor manufacturing apparatus 101 as the AA cross section in FIG. 1, but only show the main components for the structure, action, and effect of the present disclosure, and do not show the device housing, driving unit (including motor, cylinder), etc., which may be configured arbitrarily.

[0023] In the wafer grinding process after the epitaxial growth process, first, a loading process is performed in which the wafer 10 is loaded into the semiconductor manufacturing equipment 101. Fig. 3 is a cross-sectional view showing the loading process before the wafer is loaded. As shown in Fig. 3, before the wafer 10 is loaded, the first grinding unit 3 and the second grinding unit 6 are retracted to positions away from each other in the vertical direction of the page, and the edge holding unit 2 is also retracted outward in the horizontal direction of the page.

[0024] Next, in this state, the wafer 10 is placed on the back surface holding part 1 by a transfer hand (not shown) and is held by the back surface holding part 1 and the edge surface holding part 2. Fig. 4 is a cross-sectional view that shows a schematic diagram of a loading process after the wafer is loaded. When the wafer 10 is loaded onto the holding surface 1a of the back surface holding part 1 as shown in Fig. 4, the vacuum pump of the back surface holding part 1 is turned on and the wafer 10 is sucked onto the holding surface 1a of the back surface holding part 1, and then the edge surface holding part 2 moves toward the center of the wafer 10 and abuts against the wafer edge surface to hold the wafer 10 from the lateral direction. At this time, the wafer 10 is held at a position where the center of the wafer 10 overlaps with the rotation axis 9 in a plan view.

[0025] The transfer hand may be provided in the semiconductor manufacturing equipment 101, but may also be provided in another device such as a transfer robot.

[0026] In the loading step, the wafer 10 is loaded so that the wafer back surface 10a faces the first grinding unit 3 and the wafer front surface 10b faces the second grinding unit 6. Here, the wafer back surface 10a is the surface that was the back surface in the epitaxial step, and is the surface of the wafer 10 on which the Si layer 11 is provided. The wafer front surface 10b is the surface that was the front surface in the epitaxial step, and is the surface of the wafer 10 on which the epitaxial layer 12 is provided. As will be described in more detail later, a protrusion 13 is generated on the outer periphery of the wafer back surface 10a, and a protrusion 14 is generated on the outer periphery of the wafer front surface 10b.

[0027] After the wafer 10 is loaded in the loading step, a grinding step is then performed to grind the protrusions 13 on the wafer back surface 10a and the protrusions 14 on the wafer front surface 10b. In the grinding step, the first motor and the second motor are first started to rotate the first grinding stage 4 and the second grinding stage 7 in opposite directions about the rotation axis 9. The rotation directions may be the same, but if they are opposite, it is possible to prevent the wafer 10 from rotating in the rotation direction of the upper and lower grinding stages and becoming misaligned.

[0028] Next, the first vertical drive unit and the second vertical drive unit are driven to bring the first grinding unit 3 and the second grinding unit 6 close to the wafer back surface 10a and the wafer front surface 10b, respectively, and abut against them to perform grinding. Figures 5 and 6 are cross-sectional views that typically show the wafer grinding process. When the first grinding stage 4 and the second grinding stage 7 approach the wafer back surface 10a and the wafer front surface 10b, respectively, the first grinding unit 3 and the protrusions 13 on the wafer back surface 10a and the second grinding unit 6 and the protrusions 14 on the wafer front surface 10b first abut against each other, as shown in Figure 5, and grinding of the protrusions 13 and the protrusions 14 is performed.

[0029] As the first grinding stage 4 and the second grinding stage 7 approach the wafer 10, the protrusions 13 and 14 are ground and removed, and the vertical distance between the first grinding unit 3 and the second grinding unit 6 becomes equal to the thickness of the wafer in the area where there are no protrusions, as shown in Fig. 6. At this point, the protrusions 13 and 14 are removed, and the control unit determines that grinding is complete. The distance between the first grinding unit 3 and the second grinding unit 6 is determined using position information from a first sensor and a second sensor that detect the positions of the first grinding stage 4 and the second grinding stage 7.

[0030] When the control unit determines that grinding is completed, the first vertical drive unit and the second vertical drive unit retract the first grinding stage 4 and the second grinding stage 7 that were in contact with the wafer 10. Then, the first motor and the second motor are stopped, and the rotation of the first grinding stage 4 and the second grinding stage 7 is stopped.

[0031] After the grinding process is completed, the wafer 10 is unloaded in the unloading process. Fig. 7 is a cross-sectional view that shows the unloading process. In the unloading process, as shown in Fig. 7, the first grinding stage 4 and the second grinding stage 7 are retracted so that the first grinding unit 3 and the second grinding unit 6 are moved away from the wafer 10, and the edge surface holding unit 2 is retracted to the outside of the wafer 10, releasing the holding of the edge surface of the wafer 10. Thereafter, the transfer hand moves onto the wafer 10 and holds the wafer 10, the vacuum suction of the back surface holding unit 1 is released, and the unloading hand unloads the wafer 10 from the apparatus.

[0032] The effects of the semiconductor manufacturing apparatus 101 of the first embodiment will be described. In explaining the effects, first, protrusions 13 and 14 that are generated on the wafer back surface 10a and wafer front surface 10b, respectively, during epitaxial growth will be described. Epitaxial growth is one of the thin film crystal growth techniques used in semiconductor device manufacturing, and is a process technique for growing a new single crystal thin film on a semiconductor single crystal substrate. One method of epitaxial growth is, for example, vapor phase epitaxy (VPE: Vapor Phase Epitaxy or CVD: Chemical Vapor Deposition), in which components in a gas phase are deposited on the substrate crystal surface.

[0033] For example, when epitaxial growth is performed on wafer 10, which is a SiC substrate containing SiC, a backside protrusion (corresponding to protrusion 13), which is a barnacle-like protrusion about 5 to 6 μm high, may occur on wafer backside 10a, particularly around the orientation flat, and an epicrown (corresponding to protrusion 14), which is a ring-shaped protrusion about 15 to 20 μm high, may occur on wafer frontside 10b. These backside protrusions and epicrowns impair the flatness of wafer 10 and may cause problems such as defocusing in the photolithography process of the semiconductor manufacturing process.

[0034] Therefore, in the wafer manufacturing process, a process of grinding the front surface of the wafer 10 with a wafer grinding device is sometimes provided to remove these back surface protrusions and epicrowns. However, conventional wafer grinding devices grind the opposite surface of the wafer 10 while holding one side of the wafer 10, so that in order to remove the back surface protrusions on the wafer back surface 10a and the epicrowns on the wafer front surface 10b, it was necessary to first polish one surface and then turn the wafer 10 over and grind the other surface. In contrast, the semiconductor manufacturing apparatus 101 according to the first embodiment grinds the outer periphery of the wafer back surface 10a with the first grinding unit 3 while holding the wafer 10 with the back surface holding unit abutting the center of the wafer back surface 10a, so that another process can be simultaneously performed on the wafer front surface 10b. Therefore, by providing a second grinding section 6 for grinding the wafer surface 10b, it becomes possible to simultaneously perform the grinding process of the outer periphery of the wafer surface 10b. Compared to conventional grinding devices, this reduces the grinding time for one side of the wafer 10 and the time required to flip the wafer 10 and load and unload it again, thereby improving throughput.

[0035] <Embodiment 2> In the first embodiment, a semiconductor manufacturing apparatus 101 capable of simultaneously grinding backside protrusions occurring on the outer periphery of the backside surface 10a of the wafer and epicrowns occurring on the outer periphery of the wafer front surface 10b has been described. In the second embodiment, a semiconductor manufacturing apparatus 102 capable of more easily grinding epicrowns occurring on the wafer front surface 10b will be described. Note that a description of the same configuration as in the first embodiment will be omitted.

[0036] Fig. 8 is a cross-sectional view showing a cross section of semiconductor manufacturing equipment 102, and shows a cross section at a position corresponding to the AA cross section of semiconductor manufacturing equipment 101 in embodiment 1. Note that while Fig. 8 shows semiconductor manufacturing equipment 102, it shows only the main components for the structure, action, and effect of the present disclosure, and does not show an equipment housing, driving unit (including a motor and a cylinder), etc., which may be optionally configured. Also, in order to make the explanation of each component easier to understand, Fig. 8 shows semiconductor manufacturing equipment 102 in a state in which wafer 10, indicated by a dotted line, is placed on and held by the equipment.

[0037] The semiconductor manufacturing equipment 102 differs from the semiconductor manufacturing equipment 101 in the shape of the second grinding unit 6 that grinds the wafer surface 10b. That is, the surface of the second grinding unit 6 of the semiconductor manufacturing equipment 101 that contacts the wafer surface 10b is parallel to the wafer surface 10b, whereas the surface of the second grinding unit 6 of the semiconductor manufacturing equipment 102 that contacts the wafer surface 10b is not parallel to the wafer surface 10b but is inclined as shown in FIG. 8, and more specifically, the second grinding unit 6 has a shape in which the distance between the second grinding unit 6 and the wafer surface 10b decreases as it becomes farther from the rotation axis 9. That is, the second grinding unit 6 has a region that approaches the second main surface in the direction in which the rotation axis 9 extends as it becomes farther from the rotation axis 9 in a plan view.

[0038] The effect of the second embodiment will be described. As shown in FIG. 8, the epicrown occurring on the outer periphery of the wafer surface 10b has a tendency that the height of the protrusion gradually increases in the direction from the center of the wafer 10 to the outer periphery, except for the area very close to the outer periphery of the wafer 10. Therefore, in order to grind and remove the epicrown, more grinding is required closer to the outer periphery of the wafer 10. In the semiconductor manufacturing apparatus 102 according to the second embodiment, the surface of the second grinding unit 6 that contacts the wafer surface 10b has an inclination that approaches the wafer surface 10b from the rotation axis 9 toward the outer periphery, so that the second grinding unit 6 can contact the wafer surface 10b earlier and with stronger pressure to perform grinding closer to the outer periphery of the wafer 10. As a result, the epicrown on the wafer surface 10b can be removed more efficiently in a short time.

[0039] <Embodiment 3> In the first embodiment, a semiconductor manufacturing apparatus 101 capable of simultaneously grinding backside protrusions occurring on the outer periphery of the backside surface 10a of the wafer and epi-crowns occurring on the outer periphery of the wafer front surface 10b has been described. In the third embodiment, a semiconductor manufacturing apparatus 103 capable of simultaneously grinding backside protrusions and epi-crowns as well as epi-defects occurring on the wafer front surface 10b will be described. Note that the description of the same configuration as in the first embodiment will be omitted.

[0040] Fig. 9 is a cross-sectional view showing a cross section of semiconductor manufacturing equipment 103, and shows a cross section at a position corresponding to the AA cross section of semiconductor manufacturing equipment 101 in embodiment 1. Note that while Fig. 9 shows semiconductor manufacturing equipment 103, it shows only the main components for the structure, action, and effect of the present disclosure, and does not show an equipment housing, driving unit (including a motor and a cylinder), etc., which may be optionally configured. Also, in order to make the explanation of each component easier to understand, Fig. 9 shows semiconductor manufacturing equipment 103 in a state in which wafer 10, indicated by a dotted line, is placed and held in the equipment.

[0041] The semiconductor manufacturing equipment 103 differs from the semiconductor manufacturing equipment 101 in the shape of the second grinding unit 6 and second grinding stage 7 that grind the wafer surface 10b. That is, the second grinding unit 6 and second grinding stage 7 of the semiconductor manufacturing equipment 101 have a second cutout portion 8 in the center, whereas the second grinding unit 6 and second grinding stage 7 of the semiconductor manufacturing equipment 103 do not have a cutout portion in the center, and the second grinding unit 6 is configured to abut against the entire surface of the wafer surface 10b.

[0042] In epitaxial growth, defects such as protrusions and recesses may occur on the wafer surface 10b in addition to the epicrown described above. These are called epitaxial defects. Unlike epicrowns that occur mainly on the outer periphery of the wafer surface 10b, epitaxial defects may occur on the entire surface including the center. In the semiconductor manufacturing apparatus 103, the second grinding unit 6 that grinds the wafer surface 10b is provided in an area corresponding to the entire surface of the wafer surface 10b without having a cutout portion, so that when the second grinding unit 6 rotates, it is possible to grind even epitaxial defects that occur in the center of the wafer surface 10b.

[0043] In the first to third embodiments, the surface of the first grinding unit 3 that contacts the wafer back surface 10a is parallel to the wafer 10, but is not limited thereto, and the surface that contacts the wafer 10 may have a shape that is inclined with respect to the wafer 10, as in the second grinding unit 6 in the second embodiment. In cases where the number of protrusions 13 on the wafer back surface 10a increases with increasing distance from the rotation axis 9, or the height of the protrusions 13 increases, the first grinding unit 3 may be shaped such that the distance between the first grinding unit 3 and the wafer back surface 10a decreases with increasing distance from the rotation axis 9, as in the case of the second grinding unit 6, so that the protrusions 13 can be more efficiently ground and removed.

[0044] In the first to third embodiments, the completion of grinding of the protrusions in the grinding process is determined by detecting that the distance between the first grinding unit 3 and the second grinding unit 6 is equal to the thickness of the wafer 10 without the protrusions, using the first sensor for detecting the position of the first grinding stage 4 and the second sensor for detecting the position of the second grinding stage 7. However, the present invention is not limited to this, and for example, an optical sensor for measuring the distance between the first grinding unit 3 and the flat portion of the wafer back surface 10a without the protrusions and the distance between the second grinding unit 7 and the flat portion of the wafer front surface 10b without the protrusions may be provided separately and used for the determination. Alternatively, for example, the current values ​​flowing through the first motor and the second motor may be monitored by the control unit, and the change in the load applied to the first grinding unit 3 and the second grinding unit 6 may be detected by the change in the current value during grinding to determine that the protrusions have been removed.

[0045] In the first to third embodiments, the rotation speed of the first grinding stage 4 and the second grinding stage 7, i.e., the number of rotations per unit time, can be changed. For example, epicrowns on the wafer front surface 10b may be more difficult to remove than backside protrusions on the wafer back surface 10a, and more time may be required for grinding. In such a case, the rotation speed of the second grinding unit 6 is made faster than the rotation speed of the first grinding unit 3, thereby shortening the grinding time for the wafer front surface 10b and improving throughput.

[0046] In the first to third embodiments, the first grinding unit 3 has an annular shape. However, the present invention is not limited to this, and the first grinding unit 3 may be arranged on the first grinding stage 4 in one or more blocks that are not continuous in a ring shape in the rotation direction. Even if the first grinding stage 4 is arranged in such a block shape, it is sufficient that the first grinding stage 4 can rotate to abut against a desired annular region on the outer periphery of the wafer back surface 10a. Similarly, the second grinding unit 6 has an annular shape in the first and second embodiments, and a circular shape in the third embodiment, but may be arranged in one or more blocks that are not continuous in a ring shape in the rotation direction.

[0047] In the first to third embodiments, the back surface holding part 1 is disposed below the wafer 10 in the vertical direction. Therefore, the wafer 10 is held so that the wafer front surface 10b is on top and the wafer back surface 10a is on the bottom in the vertical direction. However, the back surface holding part 1 may be disposed above the wafer 10 in the vertical direction, and the wafer 10 may be held so that the wafer front surface 10b is on the bottom and the wafer back surface 10a is on top in the vertical direction. This configuration reduces the amount of grinding waste generated during grinding of the wafer 10 that falls down due to gravity and gets between the first grinding stage 4 and the back surface holding part 1, thereby suppressing malfunctions of the first grinding stage 4 and the back surface holding part 1.

[0048] In the first to third embodiments, the wafer 10 is held by the back surface holding part 1, and the first grinding part 3 and the second grinding part 6 rotate to grind the wafer back surface 10a and the wafer front surface 10b. However, conversely, the wafer 10 held by the back surface holding part 1 may rotate together with the back surface holding part 1, and the first grinding part 3 and the second grinding part 6 may be fixed and not rotate. Also, even if the wafer 10 rotates together with the back surface holding part 1 and the first grinding part 3 and the second grinding part 6 also rotate, it is only necessary that the rotation speeds are different. These may be configured to make it easy to manufacture the device, for example.

[0049] In the first to third embodiments, the first grinding unit 3 grinds the outer periphery of the wafer back surface 10a while the back surface holding unit of the wafer front surface 10b abuts against the center of the wafer back surface 10a to hold the wafer 10, so that the second grinding unit 7 is disposed on the side facing the wafer front surface 10b, and grinding of the wafer front surface 10b can be performed at the same time. However, the processing performed on the wafer front surface 10b is not limited to grinding. For example, a cleaning processing mechanism such as an air blower or cleaning water (cleaning liquid) spray, which is a cleaning means for the wafer 10, may be disposed at a position facing the wafer front surface 10b, so that the cleaning processing of the wafer front surface 10b can be performed at the same time as grinding the wafer back surface 10a.

[0050] Although some embodiments of the present disclosure have been described, these embodiments are presented as examples. Various omissions, substitutions, and modifications can be made without departing from the gist of the disclosure. Each embodiment can be combined. The scope of the present disclosure is indicated by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims.

[0051] Various aspects of the present disclosure are summarized below as appendices.

[0052] (Appendix 1) a first main surface holding part that abuts against a central portion of a first main surface of a wafer in a plan view and holds the wafer; a first grinding unit that rotates about a rotation axis that overlaps with the center of the wafer in a plan view and extends in a direction perpendicular to the first main surface, and comes into contact with an outer periphery that is a region surrounding a central portion of the first main surface to grind the outer periphery of the first main surface; Semiconductor manufacturing equipment equipped with (Appendix 2) 2. The semiconductor manufacturing apparatus according to claim 1, wherein the first grinding unit has a first cutout portion which is a region cut out in the center in a plan view, and the first main surface holding unit is disposed so as to overlap the first cutout portion in a plan view. (Appendix 3) 3. The semiconductor manufacturing apparatus of claim 1, further comprising a second grinding unit that rotates about the rotation axis and comes into contact with a second main surface that is an opposite surface to the first main surface to grind the second main surface. (Appendix 4) 4. The semiconductor manufacturing apparatus of claim 3, wherein the second grinding unit has, in a center in a plan view, a second cutout portion that is a cutout region or a recessed portion that is a region recessed in a direction away from the second main surface. (Appendix 5) 5. The semiconductor manufacturing apparatus according to claim 3, wherein the second grinding unit has a region that approaches the second main surface in an extension direction of the rotation axis as it becomes farther from the rotation axis in a plan view. (Appendix 6) 4. The semiconductor manufacturing apparatus of claim 3, wherein the second grinding unit contacts the entire second main surface. (Appendix 7) 7. The semiconductor manufacturing apparatus according to claim 3, wherein the second grinding unit rotates in a direction opposite to the direction in which the first grinding unit rotates. (Appendix 8) 8. The semiconductor manufacturing apparatus according to claim 3, wherein the number of revolutions per unit time of the second grinding unit is greater than the number of revolutions per unit time of the first grinding unit. (Appendix 9) 9. The semiconductor manufacturing apparatus according to claim 1, wherein the first main surface holding part holds the wafer by suctioning the first main surface through vacuum suction. (Appendix 10) 10. The semiconductor manufacturing apparatus according to any one of claims 1 to 9, wherein the first main surface holding part holds the wafer so that the first main surface is downward in a vertical direction relative to the second main surface. (Appendix 11) 11. The semiconductor manufacturing apparatus according to any one of claims 1 to 10, further comprising an edge surface holding section that holds the wafer by contacting the edge surface of the wafer. [Explanation of symbols]

[0053] 101, 102, 103 semiconductor manufacturing equipment, 1 back surface holding part, 2 end surface holding part, 3 first grinding part, 4 first grinding stage, 5 first cutout part, 6 second grinding part, 7 second grinding stage, 8 second cutout part, 9 rotation shaft, 10 wafer, 10a wafer back surface, 10b wafer front surface

Claims

1. a first main surface holding part that holds the wafer by contacting a central portion of the first main surface of the wafer in a plan view; a first grinding unit that rotates about a rotation axis that overlaps with the center of the wafer in a plan view and extends in a direction perpendicular to the first main surface, and comes into contact with an outer periphery that is a region surrounding a central portion of the first main surface to grind the outer periphery of the first main surface; Semiconductor manufacturing equipment equipped with

2. 2. The semiconductor manufacturing apparatus of claim 1, wherein the first grinding portion has a first cutout portion which is a region cut out in the center in a plan view, and the first main surface holding portion is arranged to overlap the first cutout portion in a plan view.

3. 2. The semiconductor manufacturing apparatus according to claim 1, further comprising a second grinding section which rotates about said rotation axis and comes into contact with a second main surface opposite to said first main surface to grind said second main surface.

4. 4. The semiconductor manufacturing apparatus according to claim 3, wherein the second grinding portion has, in a center in a plan view, a second hollow portion which is a hollowed-out region or a recessed portion which is a region recessed in a direction away from the second main surface.

5. 4. The semiconductor manufacturing apparatus according to claim 3, wherein the second grinding portion has a region that approaches the second main surface in the extending direction of the rotation shaft as it becomes farther from the rotation shaft in a plan view.

6. 4. The semiconductor manufacturing apparatus according to claim 3, wherein said second grinding portion abuts against the entire surface of said second main surface.

7. 7. The semiconductor manufacturing apparatus according to claim 3, wherein the second grinding unit rotates in a direction opposite to the direction in which the first grinding unit rotates.

8. 7. The semiconductor manufacturing apparatus according to claim 3, wherein the number of revolutions per unit time of the second grinding section is greater than the number of revolutions per unit time of the first grinding section.

9. 7. The semiconductor manufacturing apparatus according to claim 1, wherein the first main surface holding part holds the wafer by suctioning the first main surface through vacuum suction.

10. 7. The semiconductor manufacturing apparatus according to claim 1, wherein the first main surface holding part holds the wafer so that the first main surface is downward in the vertical direction relative to the second main surface.

11. 7. The semiconductor manufacturing apparatus according to claim 1, further comprising an edge surface holder that holds the wafer by contacting the edge surface of the wafer.

Citation Information

Patent Citations

  • Method for working silicon wafer

    JP2004356252A

  • Method of manufacturing silicon epitaxial wafer

    JP2011091143A

  • Semiconductor wafer and method of manufacturing the same

    JP2011134828A

  • Chemical Mechanical Polishing Correction Tool

    JP2022545263A

  • grinder

    JP1983114849A