Shaft-integrated bond magnet and manufacturing method for the same

The shaft-integrated bonded magnet design with grooves on the shaft surface enhances bonding strength and durability by increasing the bonding area and minimizing moisture intrusion, addressing the challenge of weak adhesion in existing magnets.

JP2024166899APending Publication Date: 2024-11-29PROTERIAL LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023083315
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

Existing shaft-integrated bonded magnets face challenges in achieving high bonding strength between the shaft and the bonded magnet, which is crucial for motors with long life and high reliability.

Method used

The design incorporates a shaft with grooves on its circumferential surface, featuring tapered ends and a smooth inner surface, with the bonded magnet covering the entire length of the grooves, enhancing the bonding area and strength.

Benefits of technology

This configuration results in a shaft-integrated bonded magnet with improved bonding strength, reduced moisture intrusion, and increased durability, ensuring a long life and high reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024166899000001_ABST
    Figure 2024166899000001_ABST
Patent Text Reader

Abstract

To provide a shaft-integrated bond magnet that has high bonding strength between the shaft and the bonded magnet.SOLUTION: A shaft-integrated bond magnet 1 is composed of a cylindrical bond magnet 3 and a cylindrical shaft 2 that penetrates the bond magnet 3 coaxially and protrudes from the bond magnet. The shaft 2 has multiple grooves 13 on its circumference, and each of the grooves 13 has a tapered end and a smooth inner surface. The bond magnet 3 covers the entire length of the grooves 13.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a shaft-integrated bonded magnet and a method for manufacturing a shaft-integrated bonded magnet. [Background technology]

[0002] A shaft-integrated bonded magnet has been proposed in which a cylindrical bonded magnet is integrated with a cylindrical shaft by inserting it into the magnet (Patent Document 1). Shaft-integrated bonded magnets are used in the rotors of various motors. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 6-140235 Summary of the Invention [Problem to be solved by the invention]

[0004] Motors incorporating shaft-integrated bonded magnets have a wide variety of specifications, such as dimensions, rotational speed, rotational torque, and operating environment. Therefore, shaft-integrated bonded magnets with various specifications are provided to suit the motor specifications.

[0005] Generally speaking, however, in order to realize a motor with a long life and high reliability, it is desirable to provide a shaft-integrated bonded magnet in which the bond strength between the shaft and the bonded magnet is high.

[0006] In one aspect, an object is to provide a shaft-integrated bonded magnet in which the bond strength between the shaft and the bonded magnet is high. [Means for solving the problem]

[0007] In a shaft-integrated bonded magnet that is constructed integrally with a cylindrical bonded magnet and a cylindrical shaft that coaxially penetrates the bonded magnet and protrudes from the bonded magnet, the shaft has a number of grooves on its circumferential surface, each of which is tapered at both ends and has a gently sloping inner surface, and the bonded magnet covers the groove over its entire length. Effect of the Invention

[0008] In one aspect, it is possible to provide a shaft-integrated bonded magnet in which the bond strength between the shaft and the bonded magnet is high. [Brief description of the drawings]

[0009] [Figure 1] FIG. 2 is a perspective view of a shaft-integrated bonded magnet. [Diagram 2] FIG. [Diagram 3] FIG. 2 is a longitudinal cross-sectional view of a shaft-integrated bonded magnet. [Figure 4] FIG. 4 is an enlarged view of part IV in FIG. [Diagram 5] FIG. [Figure 6] FIG. 2 is a cross-sectional view of the shaft at the center. [Figure 7] FIG. 7 is an enlarged view of part VII in FIG. [Figure 8] 1A to 1C are explanatory diagrams illustrating the manufacturing process of a shaft-integrated bonded magnet. [Figure 9] 1A to 1C are explanatory diagrams illustrating the manufacturing process of a shaft-integrated bonded magnet. [Figure 10] 1A to 1C are explanatory diagrams illustrating the manufacturing process of a shaft-integrated bonded magnet. [Figure 11] FIG. 11 is an enlarged cross-sectional view of a shaft of a first modified example. [Figure 12] FIG. 11 is an enlarged cross-sectional view of a shaft of a second modified example. [Figure 13] FIG. 11 is a schematic diagram of a shaft according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] [Embodiment 1] FIG 1 is a perspective view of a shaft-integrated bonded magnet 1. The shaft-integrated bonded magnet 1 comprises a shaft 2 and a bonded magnet 3. The bonded magnet 3 is approximately cylindrical. The shaft 2 is approximately cylindrical and coaxially passes through the bonded magnet 3. The shaft 2 and the bonded magnet 3 are integrally configured.

[0011] When used as a rotor for a motor, shaft 2 is rotatably supported via bearings (not shown) etc. A rotating magnetic field is applied to bonded magnet 3 from a stator (not shown), causing bonded magnet 3 and shaft 2 to rotate together. Shaft 2 functions as the output shaft of the motor.

[0012] 2 is a perspective view of the shaft 2. In the central portion of the shaft 2, a groove portion 13 parallel to the axial direction of the shaft 2 is formed in the shape of a flat knurl over the entire circumference. The groove portion 13 is an example of a groove provided on the peripheral surface of the shaft 2. However, the shape of the groove portion 13 is different from the groove shape defined in the JIS (Japanese Industrial Standards) B951 knurling.

[0013] Fig. 3 is a longitudinal cross-sectional view of shaft-integrated bonded magnet 1. Fig. 4 is an enlarged view of part IV in Fig. 3. In this embodiment, an even number of grooves 13 are formed at equal intervals on shaft 2, and Fig. 3 is a cross-sectional view taken along a plane passing through two grooves 13 that are 180 degrees apart. Groove 13 gradually becomes shallower at both ends. As shown in Figs. 3 and 4, bonded magnet 3 covers groove 13 over its entire length. There may be an odd number of grooves 13.

[0014] Since groove portion 13 is not exposed to the outside of bonded magnet 3, the interface between bonded magnet 3 and shaft 2 exposed on the outer surface of shaft-integrated bonded magnet 1 is circular, corresponding to the outer circumference of shaft 2, as shown in Figure 1. By minimizing the length of the exposed interface, it is possible to prevent a decrease in the bonding strength between shaft 2 and bonded magnet 3 due to the intrusion of moisture or oil from the interface.

[0015] The presence of groove 13 increases the area of ​​the joint between shaft 2 and bonded magnet 3, making it possible to provide shaft-integrated bonded magnet 1 in which shaft 2 and bonded magnet 3 are firmly joined.

[0016] Fig. 5 is an enlarged side view of the shaft 2. Fig. 5 shows an enlarged view of the end of the groove 13. The groove 13 has a central portion 11 having a uniform cross-sectional shape, and tapered portions 12 that are continuous with both ends of the central portion 11. As shown in Figs. 2 and 5, in the tapered portions 12, the width of the groove 13 gradually narrows as it moves away from the central portion 11.

[0017] The center line of the central portion 11 on the circumferential surface of the shaft 2 and the center lines of the tapered portions 12 on both sides of the central portion 11 form a straight line. In the following description, the straight line formed by the center line of the central portion 11 on the circumferential surface of the shaft 2 and the center lines of the tapered portions 12 may be referred to as the center line of the groove portion 13. The multiple groove portions 13 are arranged such that the central portions 11 are parallel to each other. The center lines of the multiple groove portions 13 are also parallel to each other.

[0018] 6 is a cross-sectional view of the shaft 2 at the center portion 11. Approximately U-shaped grooves 13 with their openings facing outward are arranged around the entire circumference of the shaft 2. The shapes of the grooves 13 are the same. Details of the shapes of the grooves 13 will be described later.

[0019] The material of the shaft 2 is, for example, iron, silicon steel, magnetic stainless steel, or aluminum alloy. The material of the shaft 2 may be resin. The material of the shaft 2 may be a composite material in which resin is mixed with powder or fibers of an inorganic material. The inorganic material used in the composite material is, for example, pure metal, alloy, or ceramics, and the shape of the inorganic material is, for example, powder, flakes, whiskers, or the like.

[0020] The groove portion 13 of the shaft 2 is produced by machining the side surface of a shaft material, which is, for example, a cylindrical bar, using a hobbing machine. In Fig. 4, a hob 71 indicated by a two-dot chain line is a schematic representation of the outer diameter of the hob 71, which is a cutting tool of the hobbing machine. Cutting blades provided on the outer periphery of the hob 71 are not shown. With the hob 71 in contact with the side surface of the round bar, which is the material of the shaft 2, it is moved in the axial direction of the shaft material, specifically, downward in Fig. 4.

[0021] The portion ground while the hob 71 moves in the axial direction of the shaft blank is formed with a central portion 11 having a uniform cross-sectional shape. Tapered portions 12 that narrow toward the tip are formed at the start and end positions of grinding of the groove portion 13. As a result, the groove portion 13 is formed with a gentle inner surface where the central portion 11 and tapered portion 12 are continuous.

[0022] Fig. 7 is an enlarged view of part VII in Fig. 6. The cross section of groove 13 has a substantially arc-shaped bottom 135 and substantially linear side parts 136 each extending from both ends of bottom part 135 toward the circumferential surface of shaft 2. The boundary between side part 136 and the circumferential surface of shaft 2 has an R-shaped surface.

[0023] An inscribed circle 51 of groove portion 13 connecting the deepest parts of each groove portion 13 is indicated by a two-dot chain line. Circles dividing the distance between inscribed circle 51 and the circumferential surface of shaft 2 into four equal parts are indicated by three two-dot chain arcs. Of these, the arc closest to the circumferential surface of shaft 2 is defined as reference circle 54. Reference circle 54 is a circle that divides the distance between inscribed circle 51 and the circumferential surface of shaft 2 at a ratio of 3:1, starting from the side closest to inscribed circle 51.

[0024] The intersection point between reference circle 54 and groove portion 13 is defined as foot 561, and the angle between perpendicular lines 56 drawn toward the inside of groove portion 13 is defined as A. In FIG. 7, tangent line 57 is a tangent to groove portion 13 that passes through foot 561. In other words, perpendicular line 56 and tangent line 57 intersect at right angles at foot 561. When degrees are used as the unit of angle, the relationship between angle B between tangent lines 57 and the above-mentioned angle A is B=180-A.

[0025] In this embodiment, A is 156 degrees and B is 24 degrees. Note that Fig. 6 and Fig. 7 are examples of the cross-sectional shape of groove portion 13, and are not limited to the shapes shown in the drawings. Modified examples of the shape of groove portion 13 will be described later.

[0026] The bonded magnet 3 is manufactured by compressing and solidifying a magnetic composition, which is a mixture of magnetic powder and resin as a binder, into a predetermined shape. A rare earth magnetic powder can be used as the magnetic powder. As the rare earth magnetic powder, an RTB magnetic powder (R is at least one rare earth element and always contains either Nd or Pr, T is Fe or Fe and Co, and B is boron, which can be partially replaced by C (carbon)) is preferable. The shape of the RTB magnetic powder is a magnetic powder manufactured by a quenching method, and is preferably flat (for example, the aspect ratio of the shape of the powder particle = short diameter / long diameter is 0.3 or less). By using an RTB magnetic powder having a flat shape, the magnetic powder becomes easier to stack when the material (a mixture of magnetic powder and resin) is compressed and molded. In addition, it is relatively difficult for voids or resin pools to form between the magnetic powders during molding, making it possible to pack the magnetic powders densely. The particle size of the RTB magnetic powder is a mixture of a first magnet powder having a particle size of 20 μm or less and a second magnet powder having a particle size of more than 20 μm and less than 220 μm with a peak particle size of 80 to 120 μm, with the first magnet powder being 5 to 15 mass% and the second magnet powder being 85 to 95 mass%, for a total of 100 mass%. Here, the average particle size is the arithmetic mean diameter of the volume distribution, and is measured using a laser diffraction type particle size distribution measuring device.

[0027] On the other hand, the resin (resin for compact) used in bonded magnet 3 is a thermosetting resin or two-component resin used in general bonded magnets, and preferred resins include, for example, epoxy resin, phenol resin, and polyimide resin.

[0028] It is desirable to mix 1 to 2% by mass of resin when the magnetic powder is taken as 100% by mass. If it is less than 1% by mass, the strength of the molded product may decrease. If it is more than 2% by mass, the magnetic powder content is relatively low, and the magnetic properties may be deteriorated.

[0029] The density of the bonded magnet 3 in this embodiment is 5.8 to 6.2 g / cm 3 By using compression molding, the density of the magnetic powder is high and a bonded magnet 3 with excellent magnetic properties can be manufactured. The molding pressure during compression molding is preferably 1 to 2.5 GPa. Below 1 GPa, the strength of the green body decreases. Furthermore, even if it exceeds 2.5 GPa, no substantial increase in the strength of the green body can be expected, so a molding pressure of more than 2.5 GPa is not necessary.

[0030] The dimensions of the cross-sectional shape of the groove 13 shown in Fig. 6 are desirably such that the largest size of the second magnetic powder just fits inside the recess. In each cross section, one to several second magnetic powder particles are accommodated inside the groove 13, the first magnetic powder gets into the gaps between the second magnetic powder particles, and the inner surface of the groove 13, the first magnetic powder, and the second magnetic powder are bonded together with the resin, thereby firmly fixing the bonded magnet 3 with good characteristics to the outside of the shaft 2.

[0031] Figures 8 to 10 are explanatory diagrams illustrating the manufacturing process of shaft-integrated bonded magnet 1. Figures 8 to 10 all show vertical cross-sectional views including the central axis of shaft-integrated bonded magnet 1 to be manufactured.

[0032] First, the procedure for preparing the magnetic composition, which is a mixture of magnetic powder and resin as a binder, will be described. Magnetic powder with an average particle size of 150 μm is pulverized in a ball mill, and magnetic powder with a size of <20 μm is removed, and then pulverized again. In this manner, pulverization and classification are repeated, and the magnetic powder with a size of <20 μm is mixed with the remaining magnetic powder (peak particle size 100 μm) to adjust the magnetic powder with a size of <20 μm to 10 mass %.

[0033] The magnetic powder is mixed with a thermosetting epoxy resin (1% by mass relative to the magnetic powder) that is solid at room temperature and diluted with a solvent (MEK: Methyl Ethyl Ketone) to prepare a magnetic composition. In the following description, the magnetic composition may be referred to as material 42.

[0034] 8A shows the starting position (hereinafter referred to as the "home position") of the molding operation of the molding device used in the manufacturing process. This molding device includes a cylindrical die 10, an upper metal mold 20, and a lower metal mold 30.

[0035] The upper die 20 has a triple structure including a long cylindrical first upper punch 21 having an outer diameter approximately equal to the inner diameter of the die 10, a long cylindrical second upper punch 22 having an outer diameter approximately equal to the inner diameter of the first upper punch 21, and a long columnar upper core 23 having a diameter approximately equal to the inner diameter of the second upper punch 22, and can be inserted into the die 10 from above. The first upper punch 21 can be inserted into the die 10 in the vertical direction, the second upper punch 22 can be inserted into the first upper punch 21 in the vertical direction, and the upper core 23 can be inserted into the second upper punch 22 in the vertical direction. The movement (upward / downward) of the first upper punch 21, the movement (upward / downward) of the second upper punch 22, and the movement (upward / downward) of the upper core 23 can be performed independently of each other.

[0036] The lower die 30 has a triple structure including a long cylindrical first lower punch 31 having an outer diameter approximately equal to the inner diameter of the die 10, a long cylindrical second lower punch 32 having an outer diameter approximately equal to the inner diameter of the first lower punch 31, and a long columnar lower core 33 having a diameter approximately equal to the inner diameter of the second lower punch 32, and can be inserted into the die 10 from below. The first lower punch 31 can be inserted into the die 10 in the vertical direction, the second lower punch 32 can be inserted into the first lower punch 31 in the vertical direction, and the lower core 33 can be inserted into the second lower punch 32 in the vertical direction. The movement (up / down) of the first lower punch 31, the movement (up / down) of the second lower punch 32, and the movement (up / down) of the lower core 33 can be performed independently of each other.

[0037] First, as shown in Fig. 8B, first lower punch 31 is lowered to form space 41 between second lower punch 32 and die 10. The lowering distance d1 (depth of space 41) at this time is determined taking into consideration the length of bonded magnet 3 in shaft-integrated bonded magnet 1 to be manufactured and the compression rate of material 42 in the compression molding process described below. Next, as shown in Fig. 8C, material 42 of bonded magnet 3 (a mixture of magnetic powder and resin (magnetic composition)) is filled into space 41.

[0038] 8D, lower core 33 is lowered to form open portion 43 inside second lower punch 32. The lowering distance d2 (length of open portion 43) at this time is determined taking into consideration the length of the portion of shaft 2 that protrudes from the end face of bonded magnet 3.

[0039] 9A, the shaft 2, which has been prepared in advance, is inserted into the open portion 43. At this time, the shaft 2 is lowered until one end face of the shaft 2 abuts against the lower core 33. The shaft 2 may be lowered by its own weight, or may be lowered manually or by using a dedicated jig (dedicated device) or the like.

[0040] 9B, the first upper punch 21, the second upper punch 22, and the upper core 23 are lowered. The upper core 23 is lowered until it abuts against the other end face of the shaft 2, and the shaft 2 is sandwiched between the upper core 23 and the lower core 33. The first upper punch 21 and the second upper punch 22 are also lowered to a position where they cover a partial area of ​​the shaft 2. The lowering positions of the first upper punch 21 and the second upper punch 22 are determined taking into consideration the length of the portion of the shaft 2 that protrudes from the end face of the bonded magnet 3.

[0041] 8D to 9A, when lower core 33 is lowered to form open portion 43 inside second lower punch 32 in FIG. 8D, the lowering distance d2 (length of open portion 43) may be set to a length corresponding to the sum of the length of the portion of shaft 2 protruding from bond magnet 3 and the length of the portion of shaft 2 covered by bond magnet 3. At this time, in FIG. 8A, the portion of shaft 2 protruding from bond magnet 3 protrudes from second lower punch 32. As a result, the boundary between the portion of shaft 2 protruding from bond magnet 3 and the portion not protruding, the upper surface of filled material 42, the upper surface of second lower punch 32, and the upper surface of die 10 are at the same position in the vertical direction.

[0042] Next, as shown in Fig. 9C, the second lower punch 32, the upper core 23, and the lower core 33 are lowered in conjunction with each other. At this time, the first upper punch 21 and the second upper punch 22 are further lowered in conjunction with each other. Then, as shown in Fig. 9D, the part of the shaft 2 covered by the bonded magnet 3 is buried in the material 42. The lowering distance of the upper core 23 and the lower core 33 and the first upper punch 21 and the second upper punch 22 at this time (the distance from the position of the upper core 23 and the lower core 33 and the first upper punch 21 and the second upper punch 22 in Fig. 9B to the position of the upper core 23 and the lower core 33 and the first upper punch 21 and the second upper punch 22 in Fig. 9D) is determined in consideration of the length of the part of the shaft 2 that protrudes from the end face of the bonded magnet 3 and the compression ratio of the material 42 in the compression molding process described later.

[0043] 9D, the first upper punch 21 and the second upper punch 22 are lowered until they abut against the upper surface of the material 42 or to the upper surface of the die 10. As a result, the shaft 2 and the material 42 are sealed between the upper die 20 and the lower die 30.

[0044] In the embodiment based on Figures 9B to 9D, when second lower punch 32 is lowered, it is lowered to the lowered position of first lower punch 31 (lowered by the lowering distance d1 shown in Figure 8B), but depending on the shape of shaft-integrated bonded magnet 1, etc., the lowered position of second lower punch 32 may be positioned above or below the lowered position of first lower punch 31.

[0045] 9B to 9D, instead of the process of clamping shaft 2 between upper core 23 and lower core 33 in advance, and lowering upper core 23 and lower core 33 in conjunction with each other while lowering second lower punch 32 to embed the central portion of shaft 2 in material 42, it is also possible to lower only lower core 33 while lowering second lower punch 32 without clamping shaft 2 between upper core 23 and lower core 33 in advance, so that shaft 2 placed on lower core 33 is lowered by its own weight. Also, shaft 2 may be lowered manually or by using a dedicated jig (dedicated device) or the like.

[0046] Next, as shown in Fig. 10A, the first lower punch 31 is lowered and the second upper punch 22 is lowered. Here, in Fig. 10A, the first lower punch 31 is lowered and the second upper punch 22 is lowered, but the first lower punch 31 may be lowered and the second upper punch 22 and the first upper punch 21 may be lowered.

[0047] Thereafter, as shown in FIG. 10B, the die 10 is lowered, and the upper core 23, the lower core 33, the first upper punch 21, and the second upper punch 22 are lowered while the shaft 2 is sandwiched between the upper core 23 and the lower core 33. Here, the lowering amount of the first upper punch 21 and the second upper punch 22 is adjusted so that the height positions of the faces of the first upper punch 21 and the second upper punch 22 that contact the material 42 are the same. Also, the rising amount of the first lower punch 31 and the second lower punch 32 is adjusted so that the height positions of the faces of the first lower punch 31 and the second lower punch 32 that contact the material 42 are the same. The lowering of the die 10 causes the first lower punch 31 and the second lower punch 32 to rise relatively. Then, the material 42 is compressed from two directions, downward and upward, by the first upper punch 21 and the second upper punch 22 and the first lower punch 31 and the second lower punch 32, to integrally mold the shaft 2 and the material 42.

[0048] Although the die 10 is lowered in the above embodiment, the first lower punch 31 and the second lower punch 32 may be directly raised. In the embodiment based on Fig. 10A and Fig. 10B, the lowering distance of the die 10 and the lowering distance of the upper core 23 and the lower core 33 may be the same or different. The lowering distance of the die 10, the upper core 23 and the lower core 33, the first upper punch 21 and the second upper punch 22, or the raising distance when the first lower punch 31 and the second lower punch 32 are raised may be determined in consideration of the shape of the compact 44 described later, etc.

[0049] Next, as shown in FIG. 10C, the die 10, the first upper punch 21, the second upper punch 22, the upper core 23, the first lower punch 31, the second lower punch 32, and the lower core 33 are all raised. At this time, the die 10, the first lower punch 31, and the second lower punch 32 are raised until they return to their fixed positions. Next, as shown in FIG. 10D, the first upper punch 21, the second upper punch 22, and the upper core 23 are further raised and returned to their fixed positions. Thereafter, the compact 44 is removed from the die 10, and the molding process is completed. Note that instead of the embodiment based on FIG. 10C to FIG. 10D, after only the die 10 is lowered to remove the compact 44 from the die 10, all of the die 10, the first upper punch 21, the second upper punch 22, the upper core 23, the first lower punch 31, the second lower punch 32, and the lower core 33 may be operated to return to their fixed positions. In the first embodiment, the molding pressure is, for example, 2 GPa.

[0050] Since the resin in the extracted compact 44 is not yet hardened, the extracted compact 44 is subjected to a heat treatment, for example, at 200°C for 1 hour to harden the resin. This results in a shaft-integrated bonded magnet 1 having the desired density and shape.

[0051] Cured molded body 44 is impregnated with thermosetting epoxy resin (viscosity 100 to 600 mPa s) that is liquid at room temperature in a reduced pressure and then pressurized atmosphere, after which excess resin on the magnet surface is removed through processes such as washing and centrifugation, and the magnet is heated and cured at 200°C for 1 hour. In this manner, bonded magnet 3 is produced from molded body 44.

[0052] In the above embodiment, the bond magnet 3 is composed of a mixture (magnetic composition) of magnetic powder and thermosetting resin, but the bond magnet 3 may be composed of a mixture of magnetic powder and a two-liquid epoxy resin consisting of a base agent and a hardener. When a two-liquid resin is used, the molded body 44 hardens at room temperature, but hardening may be accelerated by heat treatment at 200°C for 1 hour, for example. Also, the bond magnet 3 is impregnated with a thermosetting epoxy resin, but the bond magnet 3 may be impregnated with a two-liquid epoxy resin. The impregnation may be performed by a known method, such as a reduced pressure method, a pressurized method, or a vacuum pressurized method.

[0053] A configuration containing such magnetic powder, thermosetting epoxy resin, and two-component epoxy resin can provide a shaft-integrated bonded magnet 1 with a high filling rate of magnetic powder and little variation in strength, thereby improving the magnetic properties.

[0054] The effect of impregnating resin into bonded magnet 3 integrally molded with shaft 2 will be further explained. The impregnated resin penetrates into the gaps between the magnetic powder and resin of bonded magnet 3, improving the strength of bonded magnet 3. Furthermore, the impregnated resin penetrates between the magnetic powder, resin, and shaft 2, providing the special effect of firmly bonding bonded magnet 3 and shaft 2.

[0055] Since the shaft 2 has a groove 13 on its outer periphery, the shaft 2 and the bonded magnet 3 are molded integrally with each other, and the magnetic powder and resin are molded to conform to the shape of the groove 13, so that the shaft 2 and the bonded magnet 3 are fixed together. Although the strength is sufficient in this state, if resin impregnation is performed when even higher fixing performance is required, the impregnated resin increases the adhesive strength between the bonded magnet 3 and the shaft 2, and even if there is a gap in the groove 13 of the shaft 2 where no magnetic powder or resin is present, the impregnated resin penetrates (fills) the gap between the bonded magnet 3 and the shaft 2, and exerts the effect of integrating the shaft 2 and the bonded magnet 3, thereby achieving even higher fixing performance. It also increases the weather resistance of the bonded magnet 3 and has the potential to reduce eddy current loss. Furthermore, by integrally molding the shaft 2 and the bonded magnet 3, the coaxiality between the shaft 2 and the bonded magnet 3 and the runout accuracy when the shaft-integrated bonded magnet 1 is rotated are improved.

[0056] Epoxy resin can be used as the resin for impregnation. Heat-curing type, two-part epoxy resin consisting of a base agent and a curing agent can be used as the epoxy resin. Even if it is two-part, it can be cured not only at room temperature, but also by heating to accelerate the curing.

[0057] Next, a combination of the resin for the molded body and the resin for impregnation will be described. A thermosetting epoxy resin can be used for the resin for the molded body, and a thermosetting resin can be used for the resin for impregnation. A thermosetting resin can be used for the resin for the molded body, and a two-liquid epoxy can be used for the resin for impregnation. Heating can be performed after impregnation with the two-liquid epoxy resin. Also, only the curing agent for the impregnation resin can be impregnated first, and the main agent can be impregnated later. When the curing agent is impregnated without mixing with the main agent, the curing of the main agent does not progress, so the main agent can be used for a long time. A two-liquid epoxy can be used for the resin for the molded body, and a heat-curing resin can be used for the resin for impregnation. A two-liquid epoxy can be used for the resin for the molded body, and a two-liquid epoxy can be used for the resin for impregnation. In the case of a two-liquid epoxy resin, it hardens without heating, but heating may be performed to promote hardening.

[0058] In the above-mentioned manufacturing procedure for the shaft-integrated bonded magnet 1, a lubricant may be added to the mixture of magnetic powder and resin, or to the material 42 which is magnetic powder only. By adding such a lubricant, friction between the material 42 and the die 10 is reduced, and the life of the molding device can be extended.

[0059] The bond strength between bonded magnet 3 and shaft 2 in shaft-integrated bonded magnet 1 described above will be explained below.

[0060] As described above, a plurality of grooves 13 are formed in parallel to the axial direction of shaft 2 on the circumferential surface of the central portion of shaft 2. Groove 13 is tapered at both ends as described using Figures 2 and 5, and is formed to be gradually shallow at both ends as described using Figures 3 and 4. The inner surface of groove 13 has no corners and is gently sloping.

[0061] In the manufacturing process using Figures 8 to 10, the shaft 2 is pressed into the material 42 along the axial direction. Therefore, the material 42 flows along the longitudinal direction of the groove 13, filling the inside of the groove 13. Since the inner surface of the groove 13 is formed gently, the material 42 flows smoothly. Even if air bubbles are trapped in the material 42, the material 42 flows without forming air pockets inside the groove 13.

[0062] As a result of the above, material 42 is stably filled inside groove 13, creating shaft-integrated bonded magnet 1 in which shaft 2 and bonded magnet 3 are firmly bonded. Furthermore, because there are no corners or the like on the inner surface of groove 13, it is less likely that strong pressure will be applied to some of the magnetic powder during filling, causing it to be crushed. Therefore, shaft-integrated bonded magnet 1 equipped with bonded magnet 3 having the desired magnetic properties can be stably created.

[0063] Shaft 2 has no parts that protrude outward from the circumferential surface, and has no surfaces perpendicular to the central axis other than both end surfaces. Therefore, the force required to press shaft 2 into material 42 can be kept to a minimum, and shaft-integrated bonded magnet 1 can be manufactured without wasting energy.

[0064] According to this embodiment, it is possible to provide a shaft-integrated bonded magnet 1 with high bonding strength between the shaft 2 and the bonded magnet 3. According to this embodiment, it is possible to provide a shaft-integrated bonded magnet 1 with a long lifespan because there is little deterioration due to moisture intrusion from the bonding interface between the shaft 2 and the bonded magnet 3.

[0065] The shaft 2 may be provided with a structure such as a D-cut or a key groove that is used for connecting a rotated object or a coupling to a motor. The end of the shaft 2 may be chamfered.

[0066] 2 and 5 show the case where the groove 13 is formed along the generatrix of the shaft 2, but the groove 13 may be formed in a spiral shape inclined with respect to the generatrix. By using a hobbing machine, a spiral groove 13 having any inclination can be formed.

[0067] By using the spiral groove 13, it is possible to provide a shaft-integrated bonded magnet 1 that has high strength against thrust loads, that is, in the direction parallel to the central axis of the shaft 2.

[0068] [Variation 1] Fig. 11 is an enlarged cross-sectional view of shaft 2 of modified example 1. In this modified example, compared to groove portion 13 of embodiment 1 described using Fig. 7, bottom portion 135 has a larger radius, and the joint between bottom portion 135 and side portion 136 is closer to the center of shaft 2. In this modified example, angle A between perpendicular lines 56 is 130 degrees, and angle B between tangent lines 57 is 50 degrees.

[0069] Fig. 11 shows the lower limit of the desirable angle A. As explained using Figs. 8 to 10, when bonded magnet 3 is formed on the outside of shaft 2 by compression molding, bonded magnet 3 and the portion of shaft 2 that was pressed by bonded magnet 3 will expand when a mold such as die 10 is removed. This expansion phenomenon is called springback.

[0070] 11, springback is likely to generate stress in a direction that pulls apart the interface between shaft 2 and bonded magnet 3. Therefore, when shaft 2 is rotated at high speed, there is an increased risk of bonded magnet 3 being damaged.

[0071] However, angle A may be set to less than 130 degrees if the bonding strength between shaft 2 and bonded magnet 3 can be increased, for example, by appropriately selecting the surface treatment of shaft 2 or the resin material used for bonded magnet 3. Angle A may also be set to less than 130 degrees when used in applications where the load applied to shaft 2 and bonded magnet 3 is small, such as for low-speed motors or low-torque motors.

[0072] [Variation 2] 12 is an enlarged cross-sectional view of shaft 2 of modification 2. In this modification, tangents 57 on both sides of groove portion 13 are approximately parallel to each other, and two perpendicular lines 56 form a straight line. In this modification, angle A is 180 degrees, and angle B is 0 degree.

[0073] 12 shows the upper limit of the desirable angle A. If the angle A exceeds 180 degrees, the groove portion 13 will have a so-called overhang shape, which makes machining by the hob 71 difficult.

[0074] However, for example, when creating the shaft 2 by a method such as MIM (Metal Injection Molding), it is possible to create a shaft 2 with angle A exceeding 180 degrees. Generally, MIM processing is more expensive than processing using a hobbing machine, but in the case of a shaft-integrated bonded magnet 1 for applications where a high price is acceptable, angle A may be set to be greater than 180 degrees. A shaft-integrated bonded magnet 1 with high bonding strength between the shaft 2 and the bonded magnet 3 can be realized.

[0075] [Embodiment 2] This embodiment relates to a shaft-integrated bonded magnet 1 having intersecting grooves 13. Explanation of parts common to embodiment 1 will be omitted.

[0076] Fig. 13 is a schematic diagram of a shaft 2 according to a second embodiment. A groove portion 13 is formed in a twill knurled pattern in the central portion of the shaft 2. The groove portion 13 includes a first groove 131 shown slanting downward to the right in Fig. 13 and a second groove 132 shown slanting downward to the left. The downward-to-right direction is an example of the first direction, and the downward-to-left direction is an example of the second direction.

[0077] Both the first groove 131 and the second groove 132 are formed in a spiral shape on the circumferential surface of the shaft 2. Like the groove portion 13 in the first embodiment, both the first groove 131 and the second groove 132 include a central portion 11 having a uniform cross-sectional shape and tapered portions 12 that are continuous with both ends of the central portion 11.

[0078] According to this embodiment, the area of ​​the joint between shaft 2 and bonded magnet 3 is even larger than in embodiment 1, so it is possible to provide a shaft-integrated bonded magnet 1 in which shaft 2 and bonded magnet 3 are firmly joined.

[0079] The technical features (constitutive elements) described in each embodiment can be combined with each other, and by combining them, new technical features can be formed. The embodiments disclosed herein are illustrative in all respects and should not be considered as limiting. The scope of the present invention is defined by the claims, not by the above meaning, and is intended to include all modifications within the scope and meaning equivalent to the claims.

[0080] Independent claims and dependent claims described in the claims may be combined with each other in any combination, regardless of the reference format. Furthermore, the claims may be written in a format in which a claim references two or more other claims (multiple claim format), but this is not limited to this format. The claims may also be written in a format in which a multiple claim references at least one other claim (multiple multiple claim format). [Explanation of symbols]

[0081] 1. Shaft integrated bonded magnet 2 Shaft 3 Bonded magnets 10 Die 11 Central part 12 Taper 13 Groove (groove) 131 First groove 132 2nd groove 135 Bottom 136 Side 20 Upper mold 21 First upper punch 22 Second upper punch 23 Upper Core 30 Lower mold 31 First lower punch 32 Second Lower Punch 33 Lower Core 41 Space 42 Material (magnetic composition) 44 Molded body 51 Inscribed Circle 54 Reference Circle 56 Perpendicular 561 Feet 57 Tangent line 71 Hob

Claims

1. A bonded magnet with an integrated shaft is constructed integrally with a cylindrical bonded magnet and a cylindrical shaft that coaxially penetrates the bonded magnet and protrudes from the bonded magnet. the shaft has a plurality of grooves on a circumferential surface; Each of the grooves has tapered ends and a smooth inner surface; The bonded magnet covers the entire length of the groove. Shaft integrated bonded magnet.

2. The groove is parallel to the axial direction of the shaft.

2. The shaft-integrated bonded magnet according to claim 1.

3. The grooves include a plurality of first grooves arranged parallel to a first direction and a plurality of second grooves arranged parallel to a second direction intersecting the first direction.

2. The shaft-integrated bonded magnet according to claim 1.

4. The groove has a central portion having a uniform cross-sectional shape, and tapered portions that are continuous with both ends of the central portion and that become narrower and shallower as they move away from the central portion.

4. The shaft-integrated bonded magnet according to claim 1.

5. 。 The grooves are arranged such that the central portions are parallel to each other.

5. The shaft-integrated bonded magnet according to claim 4.

6. The cross-sectional shape of the central portion is An arcuate bottom portion; and a side portion extending from each side of the bottom portion toward the circumferential surface of the shaft.

5. The shaft-integrated bonded magnet according to claim 4.

7. The cross-sectional shape of the central portion is The angle between the perpendicular lines to both sides is between 130 degrees and 180 degrees.

7. The shaft-integrated bonded magnet according to claim 6.

8. The perpendicular line has a foot at a depth obtained by dividing the distance between the bottom of the groove and the circumferential surface of the shaft in a ratio of 3:1 from the side closer to the bottom. The shaft-integrated bonded magnet according to claim 7.

9. A hob is used to form multiple grooves on the side of a cylindrical bar, A material made by kneading magnet powder and resin is molded into a cylindrical shape that covers the groove over its entire length and exposes the end of the bar material from the end face. Manufacturing method for shaft-integrated bonded magnet.

10. The groove is parallel to the axial direction of the bar. A method for producing the shaft-integrated bonded magnet according to claim 9.

11. The grooves include a plurality of first grooves arranged parallel to a first direction and a plurality of second grooves arranged parallel to a second direction intersecting the first direction. A method for producing the shaft-integrated bonded magnet according to claim 9.

Citation Information

Patent Citations

  • Manufacture of integrally formed magnet body and integrally formed magnet

    JP1994140235A