Heated aroma cartridge
The heated aroma-generating base material, using cellulose polysaccharides and cross-linked PVP, addresses non-uniform mixing issues in existing substrates, ensuring stable production and long-term aroma enjoyment by preventing deformation and dissipation, and maintaining aroma and smoke generation.
Patent Information
- Application Number
- JP2024150191
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing heated aroma-generating substrates for smoking devices suffer from non-uniform mixing of aroma source materials, aerosol formers, and binders, leading to issues such as falling off, deformation, and insufficient aroma and smoke production due to heterogeneity and chemical properties, as well as the dissipation of cooling agents over time.
A heated aroma-generating base material is developed through a molding process involving compressive shear force, using a combination of cellulose polysaccharides and other polysaccharides as binders, along with cross-linked polyvinylpyrrolidone (PVP) and microcrystalline cellulose, to ensure uniform dispersion and cohesion, preventing deformation and dissipation of cooling agents.
The solution ensures stable production and long-term aroma enjoyment, prevents the base material from falling off, and maintains aroma and smoke generation, even after long-term storage, while enhancing mechanical strength and reducing contamination risks.
Smart Images

Figure 2024167354000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a heated aroma-generating substrate to be provided in a heated aroma cartridge suitable for a heated smoking device, a heated aroma cartridge provided with the heated aroma-generating substrate, and a method for manufacturing the heated aroma-generating substrate.
[0002] In particular, the heated aroma-generating substrate of the present invention is a heated aroma-generating substrate that is manufactured by mixing at least an aroma source material, an aerosol former, and a binder, and then undergoing a molding process in which a compressive shear force is applied, and is characterized in that the aroma source material, the aerosol former, and the binder are uniformly dispersed and bound together. As a result, when a heated aroma cartridge equipped with a heated aroma source composed of the heated aroma-generating substrate of the present invention is attached to or detached from a heated smoking device, problems such as deformation, detachment, and falling of the heated aroma-generating substrate do not occur, and the aroma volatilized from the heated aroma source material can be fully enjoyed during smoking. In the manufacture of the heated aroma-generating substrate, the aroma source material, the aerosol former, and the binder are uniformly dispersed and bound together, and have the toughness and strength required for molding, allowing stable production.
[0003] Furthermore, the heated aroma-generating substrate of the present invention is characterized in that when a refreshing agent such as menthol or xylitol is added as an aromatic agent, the dispersion of the refreshing agent over time is suppressed, and this has the effect of allowing the aroma of the heated aroma-generating substrate to be fully enjoyed when smoking after a heated aroma cartridge equipped with a heated aroma-generating source containing the same has been stored for a long period of time and is attached to a heated smoking device.
[0004] Furthermore, the heated aroma-generating substrate of the present invention is characterized by little dimensional change due to drying, and even after a heated aroma cartridge equipped with a heated aroma-generating source composed of the heated aroma-generating substrate is attached to a heated smoking device and used for smoking, the heated aroma-generating substrate does not fall off or fall off from the heated aroma cartridge, and even after long-term storage, the heated aroma-generating substrate does not fall off or fall off from the heated aroma cartridge, making it easy to handle and effective in preventing contamination of the heat source of the heated smoking device.
[0005] Incidentally, in the past, the above-mentioned "heated aroma-generating substrate" was often called "aerosol-forming substrate", but since heating causes the aroma components of the aroma source material and the aromatic agent to volatilize together with the aerosol former that forms the aerosol, and the smoke of the aerosol and the aroma of the aroma source material and the aromatic agent are enjoyed by smoking, in the present invention, it is called "heated aroma-generating substrate". Based on this, an "aerosol-forming body" filled with an aerosol-forming substrate and an "electronic cigarette cartridge" equipped with an aerosol-forming body are called "heated aroma-generating source" and "heated aroma cartridge", respectively. However, the name "heated aroma cartridge" is not limited, and it may be called "smoking cartridge" or "electronic cigarette compatible cartridge".
[0006] In addition, the source of the aroma is not limited, and tobacco plants of the genus Nicotiana and its congeneric plants and non-tobacco plants that do not contain tobacco components can be used. "Aroma" means "good smell" and refers to the aroma (fragrance) that wafts from the material itself, the aroma (aroma) that wafts through the air when heated, the aroma (flavor) that wafts through the mouth when inhaled, and the like that can be sensed when smoking. "Smoking" generally means smoking cigarettes or cigars, but here it simply means "enjoying the smoke," "tasting the aroma," and "enjoying the smoke or aroma." Therefore, the "smoke" here does not refer to something that is generated by combustion, but rather "something that looks like smoke" or "something that is smoke-like," such as droplets dispersed in the air, such as aerosols. [Background technology]
[0007] In recent years, smoking bans on cigarettes have been spreading widely in places where people gather, such as workplaces and restaurants. In response to this, a cigarette manufacturer has developed a method of smoking a heated aroma cartridge that generates an aerosol by heat transferred from an electronically controlled blade-type heat source when it is attached to the chamber of a heated smoking device (Patent Document 1). This heated aroma cartridge is equipped with a heated aroma generating source formed using an aerosol former, an aroma source material including a tobacco plant of the Solanaceae family, and a heated aroma generating base material containing a binder, etc., and when the heated aroma generating base material is heated, volatile substances are generated, the volatile substances of the aerosol former are cooled and become smoke, and the volatile substances of the aroma source material become aroma, allowing smoking similar to that of a combustion cigarette to be enjoyed. According to this heated smoking, the inhalation of harmful substances generated by the thermal decomposition and combustion of conventional cigarettes is reduced, so that the number of people smoking combustion cigarettes has drastically decreased, while the number of people smoking heated cigarettes has rapidly increased. For this reason, technological developments to make heated smoking more enjoyable are being actively carried out (e.g., Patent Documents 1 to 12).
[0008] The mechanism of such heated smoking differs depending on the form of the heated smoking device, heated aroma cartridge, etc., but a typical example is shown below. A heated aroma cartridge has a heated aroma generation source filled with a heated aroma generation substrate at one end and a mouthpiece at the other end. When the heated aroma generation source is attached so that it comes into contact with the heat source of the heated smoking device and heated, an aerosol former and volatiles of the aroma source material are released from the heated aroma generation source. These volatiles are sucked into the mouthpiece at the other end together with air when the smoker inhales. In this volatiles transport process, the volatiles of the aerosol former cool and condense to form a smoke-like aerosol, and other volatiles impart an aroma to the smoker's mouth and nose, resulting in the enjoyment of smoking. Therefore, in the case of heated smoking, smoking can be performed at approximately 200 to 350°C, which is capable of volatilizing aerosol formers such as glycerin and propylene glycol contained in the heated aroma-generating base material, that is, at a temperature at which the tobacco leaves begin to decompose thermally. This not only prevents the generation of harmful substances due to combustion, but also reduces the generation of harmful substances due to thermal decomposition.
[0009] As can be seen from this mechanism, the heat source and its control method play an extremely important role in heated smoking devices, which have a significant impact on the generation of smoke and aroma, and as a result of many years of development, blade-type heat sources using heaters have been widely used up to the present day (e.g., Patent Documents 1-5). In contrast, omnidirectional heat sources using electromagnetic induction heating have recently been put to practical use. It is believed that the aim is to increase the generation of volatiles and provide a deep flavor, as the heating speed is fast and the contact area with the heated aroma-generating substrate is large (Non-Patent Document 1).
[0010] On the other hand, various efforts have been made in the technical development of heated aroma-generating substrates, which are the source of smoke and aroma (for example, Patent Documents 6 to 12). The essential component is an aerosol former with a boiling point of 180 to 300°C, such as glycerin or propylene glycol, which is the source of smoke, and it is necessary to mold it into a homogeneous viscoelastic body by mixing it with the aroma source material, which is the aroma source, such as tobacco plants, non-tobacco plants, and flavors. For this reason, linear, side-chain, and branched polysaccharide polymers, such as cellulose, guar gum, and gum arabic, are used as binders. In addition, wetting agents, etc., must be added to disperse these uniformly.
[0011] However, conventionally, the heated aroma-generating substrate is prepared by dispersing an aerosol former, an aroma source material, a binder, a wetting agent, etc. in water to produce an aqueous slurry, which is then subjected to a papermaking process, followed by a compression and heat drying process, followed by a cast molding process, or by extrusion molding a viscoelastic body obtained by adding an appropriate amount of lower alcohol or water to a mixture of an aerosol former, an aroma source material, a binder, a wetting agent, etc. (Patent Documents 6 and 7). However, these methods cannot produce a viscoelastic body in which the components constituting the heated aroma-generating substrate are homogenized, and the mechanical strength of the molded product is insufficient, so there is often a problem that the heated aroma-generating substrate is destroyed at the stage of processing the heated aroma-generating substrate into a heated aroma-generating source. In addition, the heated aroma-generating substrate that is not homogenized has an insufficient packing state of the aroma source and the binder, so it shrinks violently when heated and dried, and is destroyed during heat drying at the stage of processing into a heated aroma-generating source, or the heated aroma-generating substrate falls off or falls off after smoking.
[0012] Regarding the falling off or falling off, or cracking or breaking of the heated aroma-generating substrate after smoking, the effectiveness of an inorganic binder has been disclosed (Patent Document 8). This solution is based on the fact that the inorganic binder does not improve the heterogeneity, but rather improves the heat resistance to the heat source, thereby suppressing the combustion of the heated aroma-generating material, and furthermore, there is a problem in that the relative proportions of the aroma source material and aerosol former in the heated aroma-generating substrate are reduced, which leads to a decrease in the amount of aroma and smoke produced.
[0013] In addition, the heterogeneity resulting from the chemical properties of the components constituting the heated aroma-generating substrate also leads to a decrease in the amount of aroma and smoke produced. In particular, the chemical affinity between the aroma source material and the aerosol former is low, and the aroma source material is not dissolved in the aerosol former and must be dispersed, so that aerosol formers of various volumes and lumps of aroma source material of various sizes are irregularly present. Therefore, even in the case of such a heterogeneous heated aroma-generating substrate, even if it is heated by a heat source, heat is not uniformly transferred to the aroma source material and the aerosol former, so that the aroma components of the aroma source material are not sufficiently volatilized, resulting in an insufficient taste when smoking, and the aerosol former is also not sufficiently volatilized, so that it is not possible to produce smoke sufficient to please the smoker's eyes. To address this problem, a solution has been proposed in which wax is added to increase the fluidity of the volatile components of the aroma source material and the aerosol former, and to promote the dissipation of volatile substances from the heated aroma-generating substrate (Patent Documents 9 and 10). However, since wax is hydrophobic, it is difficult to produce a homogenized heated aroma-generating base material, particularly by a production method using a cast method, and a significant improvement effect cannot be expected. In addition, the wax causes a problem of mechanical strength in that the heated aroma-generating base material becomes brittle.
[0014] Furthermore, in the case of heated tobacco, as in the case of combustible tobacco, in order to obtain a refreshing feeling when smoking, a freshening agent such as menthol or xylitol may be added as an aromatic. In addition, flavorings may be added to add the flavor of fruits, nuts, etc. In such cases, in the heat drying process for producing the aroma-generating substrate to be heated by the casting method described above, there is a problem that the freshening agent and flavoring are scattered, and there is also a problem that the freshening agent and flavoring are scattered over time due to the balance of hydrophilicity and hydrophobicity of the components constituting the aroma-generating substrate to be heated, including the freshening agent and flavoring, and the aerosol former contains a large amount of components that are not soluble in the aerosol former and is not homogenized. In response to these problems, inclusion of the freshening agent and flavoring with various cyclodextrins and encapsulation of the freshening agent and flavoring with wax have been disclosed as means for solving these problems (Patent Documents 11 and 12). In order to form the former inclusion compound, it is necessary to find a suitable combination of a freshening agent and a flavoring with a cyclodextrin, select a suitable solvent, homogenize the freshening agent and the flavoring with the cyclodextrin in a homogenizer, and then spray-dry, freeze-dry, or vacuum-dry. Therefore, applicable freshening agents and flavorings are limited, and production requires a great deal of effort.
[0015] As mentioned above, the heated aroma-generating substrate has a problem of non-homogenization due to the manufacturing methods of cast molding and extrusion molding and the chemical properties of the constituent components. This problem may be solved by adopting a compression and shear processing method as a manufacturing method. For example, a method using a three-roll mill that can uniformly knead and disperse a high-viscosity paste by compression by being forced between narrow rolls and shearing by the roll speed difference, and can also be formed into a sheet, is considered. However, in this case, the sheet that becomes the heated aroma-generating substrate has a problem of being difficult to process into a sheet because of cohesive failure and adhesion to the metal roll due to the insufficient strength and high adhesiveness of the sheet.
[0016] Thus, in order to enjoy smoking heated tobacco, that is, by attaching a heated aroma cartridge to a heated smoking device, it is necessary to not only improve the heated smoking device, but also to further resolve various issues arising from the composition of the heated aroma-generating substrate that constitutes the heated aroma-generating source of the heated aroma cartridge. [Prior art documents] [Patent documents]
[0017] [Patent Document 1] Special Publication No. 2015-503335 [Patent Document 2] Special Publication No. 2013-511962 [Patent Document 3] Special Publication No. 2013-515465 [Patent Document 4] Special Publication No. 2015-506170 [Patent Document 5] Special Publication No. 2015-503916 [Patent Document 6] Special Publication No. 2010-520764 [Patent Document 7] Special Publication No. 2013-519384 [Patent Document 8] Special Publication No. 2015-525565 [Patent Document 9] Special Publication No. 2018-531019 [Patent Document 10] Special Publication No. 2018-533950 [Patent Document 11] Special Publication No. 2008-518614 [Patent Document 12] Special Publication No. 2017-500850 [Non-patent literature]
[0018] [Non-Patent Document 1] Ruri Oizumi, "The momentum of the heated tobacco "Glo" is unstoppable! We have seen the new devices "Glo Pro" and "Glo Nano", Kakaku.com Magazine, https: / / kakakumag.com / hobby / ?id=14328 [Non-Patent Document 2] "What is cyclodextrin?", CycloChem Co., Ltd. website, http: / / www.cycrochem.com / cd / 001.html [Non-Patent Document 3] "Cyclodextrin | Purpose of inclusion and preparation method of inclusion products", Ensuiko Sugar Refining Co., Ltd. website, https: / / www.ensuiko.co.jp / product / cd / cd07.html Summary of the Invention [Problem to be solved by the invention]
[0019] The present invention aims to provide a heated aroma-generating substrate to be provided in a heated aroma cartridge suitable for a heated smoking device, which contains at least an aroma source material, an aerosol former, and a binder, and is manufactured by mixing these and then subjecting them to a molding process in which compressive shear force is applied, wherein the aroma source material, aerosol former, and binder are uniformly dispersed and bound together.
[0020] As a result, problems such as deformation of the heated aroma generating source and falling off or dropping of the heated aroma generating substrate when attaching or detaching a heated aroma cartridge equipped with a heated aroma source composed of the heated aroma generating substrate of the present invention to a heated smoking device can be solved, and a heated aroma generating substrate can be provided that is imparted with the toughness and strength required for this molding process and allows the aroma volatilized from the heated aroma source material to be fully enjoyed.
[0021] Furthermore, the heated aroma-generating substrate of the present invention is intended to provide a heated aroma-generating substrate in which, when a freshening agent such as menthol or xylitol is added as an aromatic agent, the dispersion of the aromatic agent or freshening agent over time is suppressed, and even after a heated aroma cartridge equipped with a heated aroma-generating source containing the same is stored for a long period of time, the aroma of the heated aroma-generating substrate can be fully enjoyed when the heated aroma-generating substrate is attached to a heated smoking device and used for smoking.
[0022] Furthermore, the heated aroma-generating substrate of the present invention undergoes little dimensional change due to drying, and even after a heated aroma cartridge containing a heated aroma-generating source containing the heated aroma-generating substrate is attached to a heated smoking device and used for smoking, the heated aroma-generating substrate does not fall off or fall off from the heated aroma cartridge, and even after long-term storage, the heated aroma-generating substrate does not fall off or fall off from the heated aroma cartridge, making it easy to handle and capable of preventing contamination of the heat source of the heated smoking device.
[0023] Thus, the main problem that the present invention aims to solve is to homogeneously mix and disperse materials with different properties, such as fragrance source material, aerosol former, binder, and fragrance, which are found in conventional heated fragrance-generating substrates, as well as to easily prevent the fragrance from dissipating over time and to prevent the shape from shrinking over time and due to heat. [Means for solving the problem]
[0024] The inventors have examined a wide variety of materials in addition to the aroma source material, aerosol former, binder, and fragrance that constitute the heated aroma-generating base material, and have found that the above-mentioned problems can be solved by selecting two types of binders and an appropriate method for blending them, as well as by adding cross-linked polyvinylpyrrolidone (PVP) and microcrystalline cellulose, thereby completing the present invention.
[0025] That is, the present invention is a heated aroma-generating substrate containing at least an aroma source material, an aerosol former, and a binder, wherein the binders include a first binder and a second binder, the first binder being at least one type of cellulose polysaccharide selected from the group consisting of methyl cellulose, ethyl cellulose, carboxymethyl cellulose, carboxyethyl cellulose, hydroxymethyl cellulose, hydroxyethyl cellulose, hydroxypropyl cellulose, and their sodium salts, potassium salts, and calcium salts, and the second binder being at least one polysaccharide other than a cellulose polysaccharide selected from the group consisting of glucomannan, guar gum, pectin, carrageenan, locust bean gum, and agar.
[0026] By using such a first binder and a second binder in combination, the aroma source material and the aerosol former constituting the heated aroma-generating substrate are homogeneously mixed and dispersed, and the binding force between the two is enhanced, resulting in a heated aroma-generating substrate having the toughness and strength required for molding. As a result, the heated aroma-generating substrate can be attached to and detached from the heated aroma-generating substrate without falling off, dropping, or deforming, even immediately after the heated aroma cartridge including the heated aroma-generating substrate is manufactured, or after it has been stored for a long period of time. In addition, aroma from the aroma source material and smoke from the aerosol former are sufficiently generated during smoking. Furthermore, since the aroma source material and the aerosol former are homogeneously mixed and dispersed via the binder, even in molding using compressive shear force, for example, when a three-roll roll is used, it is possible to mold the heated aroma-generating substrate into a sheet-shaped heated aroma substrate without causing cohesive failure. In order for the heated aroma-generating substrate to achieve such effects, the breaking strength in a tensile strength test must be 0.167 N / mm 2 It was confirmed that this was the case.
[0027] In order to stably exert the above-mentioned effect by using the first binder and the second binder in combination, it is preferable to use a stepwise binder mixing manufacturing process including a first mixing process of mixing the aroma source material, the aerosol former, and the first binder, and a second mixing process of mixing the mixture produced in the first mixing process with the second binder, or a first mixing process of mixing the aroma source material, the aerosol former, and the first binder, and a mixing and molding process of mixing the mixture produced in the first mixing process with the second binder and molding it into a heated aroma-generating substrate. The reason for this is unclear, but it is thought that the first binder, which is a cellulose-based polysaccharide, promotes uniform mixing and dispersion of the aroma source material and the aerosol former to form a stable sol state, and then the second binder, which is a polysaccharide other than the cellulose-based polysaccharide, forms a gel state that enhances the bond between them.
[0028] Supporting this hypothesis, it was observed that when the first binder and the second binder were mixed interchangeably, partially gelled lumps were formed in the mixture of the fragrance source material, aerosol former, and binder, making it impossible to achieve a uniformly dispersed state.
[0029] Furthermore, it is more preferable to add a curing step for curing the mixture produced in the first mixing step immediately after the first mixing step, and when the temperature of the curing step is 15°C or higher and 30°C or lower, and the time of the curing step is 72 hours or higher and 336 hours or lower, the combined effect of the first binder and the second binder is maximized. It is presumed that this curing step has the effect of increasing and stabilizing the dispersion degree of the aroma source material in the sol state formed by promoting the uniform mixing and dispersion of the aroma source material and the aerosol former, by the first binder of cellulose polysaccharide. This is because the volume of the mixture increases in the curing step. And, at temperatures below 15°C, the volume increase is also small, and the curing step has no effect on the quality of the heated aroma-generating base material, and at temperatures above 30°C, the mixture begins to gel, although the cause is unknown. Furthermore, if the curing time is less than 72 hours, the volume increase is slight and no effect of the curing process on the quality of the heated aroma-generating substrate is observed. If the curing time exceeds 336 hours, this volume increase stops and the effect of the curing process on the quality of the heated aroma-generating substrate becomes saturated, and curing for a longer period of time may result in gelation.
[0030] When such a curing step is performed, it is not necessary to add the first binder and the second binder stepwise, and the manufacturing process can include a third mixing step in which the aroma source material, the aerosol former, the first binder, and the second binder are mixed, and a curing step in which the mixture produced in the third mixing step is cured. In this curing step, it is believed that the effect of increasing the dispersion of the aroma source material by the first binder and the effect of increasing the cohesion by the second binder occur in parallel.
[0031] The binder is preferably a combination of the above-mentioned cellulose polysaccharides and other polysaccharides, and more preferably, cellulose fibers extracted from plants containing a large amount of cellulose fibers are further added. In particular, cellulose fibers of hemp such as linen, jute, mulukhiyah (Coleoptera), kenaf, hemp, Manila hemp, and sisal, and graminaceous plants such as rice, oats, barley, wheat, oats, pearl barley, rye, sugarcane, esparto, and bamboo, which have a fiber diameter of 10 to 50 μm, can homogeneously mix, disperse, and bind the materials constituting the heated aroma-generating substrate, impart the toughness and strength required for molding, and are highly effective in preventing deformation, falling off, and falling off. In particular, rice, wheat, and sugarcane are even more preferable because they release their aroma when heated.
[0032] Materials that are preferably used as aroma source materials are substances that emit aromas by themselves and substances that emit aromas by heating, and plants and processed products obtained by drying, fermenting, etc. of them are preferred. Aroma source materials are broadly classified into tobacco, which belongs to the Nicotiana genus of the Solanaceae family, aboveground stems and leaves of plants of the same genus, and their components, as well as flowers, roots, underground stems, trunks, branches, seeds, fruits, and aboveground stems and leaves of angiosperms, as well as teas, spore-bearing plants, sprouted vegetables, and fermented grains and beans. It is more preferred to mix two or more aroma source materials, and it is more preferred to mix three or more materials that have a fragrance defined as an aroma that wafts from the aroma source material itself, a material that has an aroma defined as an aroma that wafts through space when the aroma source material is heated, and a material that has a flavor defined as an aroma that wafts through the mouth when the aroma source material is heated. Specific examples of these are listed below.
[0033] From the viewpoint of preventing the inhalation of harmful substances, it is desirable to use as little as possible of tobacco (a member of the Nicotiana genus in the Solanaceae family) and the above-ground stems and leaves of related plants, as well as their components. However, former smokers of cigarettes tend to crave the aroma of nicotine, etc., so it is preferable to use the minimum amount necessary.
[0034] Non-tobacco plants are selected based on the aroma of the plant itself and the aroma released by heating, since there is little need to consider the inhalation of harmful substances. As for the flowers of angiosperms, among the countless flowers of angiosperms, the following are included: sophora japonica, ginger, chamomile, coltsfoot, Asteraceae (house daisy, daisy, corn daisy, sea daisy, Japanese daisy, etc.), Ardisia crenata, honeysuckle, plants of the Dianthus genus of the Caryophyllaceae family (dianthus arvensis, dianthus anguicus, dianthus anguicus, Japanese chinchilla, etc.), plants of the Mint genus of the Lamiaceae family (mint serrata, mint serrata, mint serrata, etc.), and various peppermint-type plants of the Mint genus of the Lamiaceae family (peppermint, pepper ... Parmint, Japanese mint, apple mint, water mint, Corsican mint, pennyroyal mint, etc.), various spearmint plants of the genus Mentha in the family Lamiaceae (spearmint, horse mint, green mentha, chili pepper, ginger mint, etc.), catnip, lemon balm, savory, willow mint (hyssop), Hypericum, pitcher plant, patchouli, mugwort, burdock, legume (Camellia sinensis), lamiaceae (Camellia arborescens), cactus Bamboo, Japanese laurel, safflower, narrow-leaved mountain fern, long-leaved oak, plants of the Plantaginaceae family (Plantago major, Plantago lutea, and Plantago major), plants of the Leguminosae family (Scutellaria verum, Scutellaria verum, etc.), bitter orange, rose, lotus, plants of the Magnoliaceae family (Magnolia japonica, Magnolia kobushi, Magnolia japonica, White Magnolia, and Sara) Plants of the Asteraceae family (Inula japonica, Inula nigra, etc.), plants of the Iridaceae family (Iris, Ehime iris, Iris amplexicaule, Wild iris, Japanese iris, Japanese iris, etc.), skullcap, firefly, Japanese iris, oregano, clove, plants of the Elder family (Sambucus nigra, Elderberry, Elderberry, etc.), Flowers of the following plants are preferred: Osmanthus nigra, Elderberry, Elderberry, etc., Oleaceae Osmanthus genus plants (Osmanthus australis, Osmanthus grandiflorus, Osmanthus holly, etc.), Illicium verum, Marshmallow, Pear tree, Common laurel, Red clover, Achillea millefolium, Celery, Lamiaceae Thymus genus plants (Common thyme, Citrus thyme, Wild thyme, etc.), Artichoke, Asteraceae Thymus genus plants (Marigold, African marigold, French marigold, Mexican marigold, lemon marigold, etc.), Lavender, Echinacea purpurea, Saffron, and Typha genus plants (Typha typha, Typha koenig, Typha koenig, etc.). However, in some cases, flower buds are preferred, not just flowers in bloom. Furthermore, it is not necessary to use all the parts that make up the flower; it is possible to use only the parts that have a particularly strong scent, such as the petals, pistils, and stamens.
[0035] There are countless roots of angiosperms, but the tuberous roots of dahlias, sweet potatoes, cassava, Jerusalem artichoke, yacon, Houttuynia cordata, Triticum vulgare, and plants of the Campanulaceae family (such as Lycopersicon esculentum, Lycopersicon esculentum, and Baasob), and the roots of Chinese yam and Chinese yam, which are rhizomes, are preferred. Common roots include Eleuthero, burdock, plants of the Thistle genus of the Asteraceae family (wood thistle, field thistle, Thai thistle, Fuji thistle, Nohara thistle, sea thistle, etc.), carrots, radishes, turnips, Panax ginseng, madder root, Japanese laurel, Japanese laurel, Sakishima buttonberry, Cinderella, Tendaiyaku, Astragalus membranaceus, Astragalus nigra, Scutellaria, Polygala tenuifolia, plants of the Pueraria genus of the Leguminosae family (kudzu, Chinese kudzu, Taiwan kudzu, Japanese kudzu, Japanese kudzu, white kudzu, etc.), plants of the Licorice genus of the Leguminosae family (Pueraria vine, Chinese kudzu, Taiwan kudzu, Japanese kudzu, Japanese kudzu, white kudzu, etc.), Licorice, Chinese tallow tree, Chinese lily, etc.), bellflower, Ardisia crenata, Sophora arvensis, Japanese cinnamon, wolfberry, plants of the Cinnamon genus of the Lauraceae family (Cinnamon, Ceylon cinnamon, Java cinnamon, Chinese cinnamon, round cinnamon, etc.), Scrophulariaceae, Dalbergia, Large-leaved tree, Japanese ginseng, Japanese laurel, Cnidium amplexicaule, Ardisia crenata, Atractylodes macrocarpa, Japanese knotweed, Bupleurum falcatum, plants of the Asarum genus of the Plantaceae family (Ursula arvensis, Okuzo arvensis, Togo arvensis, etc.). , Mikunisaishin, etc.), plants of the Parsley family (Parsley, Cinnamon, etc.), bat vine, plants of the Taraxacum family (Taraceae, Chinese dandelion, Odasam dandelion, Cinnamon, Kansai dandelion, Common dandelion, etc.), Rehmannia oleracea, Rehmannia verum, Chinese peony, purple, Chinese peony, Siberian peony, Japanese radish, Glehnia littoralis, plants of the Gentianaceae family (Gentiana nigricans, Gentiana serrata, Kirishi gentian, Kumagawa gentian, Akebono gentian, Large-leaved gentian, Jacques gentiana, Tibetan gentian, Siberian gentian, etc.), Nodake, Shaku, plants of the Nymphaeaceae family (Splash, Nuphar japonica, Common water lily, etc.), Ducks, Tounbana, mulberry, Salvia miltiorrhiza, Sanguisorba japonica, plants of the Apiaceae family (Angelica quince, Hokkai Angelica, Japanese Angelica, Angelica dahurica, etc.), Ophiopogon, plants of the Asparagaceae family (Lilium longiflorum, Lilium longiflorum, Lilium sieboldii, Lilium nigra, Lilium nigra, Lilium nigra, etc.),The roots of parsley, cassia grass, plants of the genus Rheum of the Polygonaceae family (Rheum officinalis, Rheum officinalis, Rheum chinense, etc.), Ryukyu eye, armoured weed, Chinese angelica, plants of the genus Rheum of the Polygonaceae family (Rheum officinalis, Rheum officinalis, Rheum chinense, Rheum chinense, etc.), plants of the genus Asteraceae (Asteraceae family, Acer nigra, Acer chinense, Acer nigra, etc.), Imperata cylindrica, Scutellaria baicalensis, tree peony, Akebia japonica, Akebia trifoliata, plants of the genus Aristolochiae family (Aristolochiae, Aristolochiae, etc.), Elephant grass, Gentian, and Echinacea purpurea are preferred. As for the roots, the whole root may be used, or only the part with the root bark removed may be used.
[0036] There are countless underground stems of angiosperms, but the preferred ones are the bulbous rhizomes of tulips, hyacinths, garlic, shallots, onions, red spider lilies, Japanese lilies, and daffodils, as well as the corms of crocuses, gladioli, freesias, Iridaceae plants (iris, Japanese iris, Iris amplexicaule, Japanese iris, Japanese iris, Japanese iris pseudacorus, etc.), taro, and konjac. Also preferred are the underground stems of tubers such as cyclamen, anemone, begonia, Chinese chilon, potato, American hogweed, Corydalis japonica, Sarmientobar bark, plants of the genus Eucalyptus (Eucalyptus, Ezo Eucalyptus, Deutzia gracilis, etc.), Japanese laurel, plants of the genus Arisaema (Araceae) (Maizuru Arisaema, Korean Arisaema, Korean Arisaema, etc.), coral reed, Asparagus vine, and Pinellia ternata, as well as rhizomes such as canna, lotus, ginger, wasabi, horseradish, turmeric, plants of the genus Polygonaceae (Polygonaceae) (Polygonaceae, Narcissus japonica, Japanese narcissus, etc.), coptis japonica, zedoary, kudzu, Japanese laurel, Chinese laurel, Japanese ginseng, Japanese lantern plant, Japanese knotweed, Japanese knotweed, Chinese sedge, Glehnia littoralis, Japanese citron, Japanese calamus, Japanese snowbell, Cnidium, plants of the Asteraceae family (narrow-leaved cricket, Chinese cricket, large-flowered cricket, cricket, etc.), plants of the Polygonaceae family (rheum, medicinal rheum, Korean rheum, etc.), Japanese ginseng, anemone sedge, Sanguinea japonica, Brassicaceae family, Tahitian Also preferred are plants of the genus Menispermum (such as narrow-leaved Menispermum and Menispermum tschonoskii), Ryukyu eyelashes, plants of the family Menispermaceae (such as Menispermum macrocarpa and Striped Leaf Vine), Menispermum umbellata, Imperata cylindrica, Sarcocarpus, plants of the family Ephedrae (such as Ephedra chinensis, Ephedra chinensis, Ephedra bracteatum, etc.), Belamcanda japonica, Gentian, Chinese laurel, and the rhizomes of reeds.
[0037] With regard to the trunks and branches of angiosperms, many are preferable for coniferous plants, but particularly preferable are the trunks and branches of cypress, pine, cedar, asarum, camellia, elm, Japanese elm, American wax tree, Mallotus japonicus, Chinese oak, Phellodendron amplexicaule, cherry tree, China tree, Japanese cinnamon, plants of the Cinnamon genus of the Lauraceae family (Cinnamon, Ceylon cinnamon, Java cinnamon, Chinese cinnamon, round cinnamon, etc.), Magnolia obovata, Japanese laurel, Machilus thunbergii, Ash tree, Oriental ash, Japanese oak, Suoh, Hachiku, Eucommia ulmoides, and Illicium verum.
[0038] There are also countless seeds and / or fruits of angiosperms, particularly American wax tree, fennel, wild rose, myrobalan, Chinese laurel, Chinese hawthorn, plants of the Gardenia genus of the Rubiaceae family (Gardenia, Cornus jasmine, Gardenia jasmine, etc.), Cornus japonicus, plants of the Ligustrum genus of the Oleaceae family (Ligustrum persica, Ligustrum jasmine, etc.), roses, plants of the Lamiaceae family (Perilla frutescens, Perilla frutescens, Perilla jasmine, Perilla jasmine, etc.), Tribulus terrestris, Kochia jasmine, water lily, and Yam. Buttercup (fruit), plants of the Palm family (Washuro, Tojuro, Aijuro, etc.), Amomum, Tsusaoko, Asarum, Cocklebur, Mulberry, Honey locust, Betel nut, plants of the Cuscuta family (Sea vine, Mamedaoshi, Cuscuta, White dodder, American dodder, etc.), Oriental grass, plants of the Typha family (Typha, Typha, Typha, etc.), Cannabis, plants of the Vicia family (Vitis vinifera, Vicia faba, etc.), Akebia, Akebia trifoliata, Kaba Phosphorus, plants of the Aristolochiae family (Aristolochiae, Marlborough, etc.), Longan, plants of the Forsythia genus of the Oleaceae family (Forsythia, Chinese Forsythia, Korean Forsythia, Forsythia suavea, etc.), Kenponashi, plants of the Citrus genus of the Rutaceae family (Bitter orange, Satsuma mandarin, Natsudaidai, Ponkan, Hassaku, Iyokan, Yichang lemon, Trifoliate orange, Orange, Mandarin orange, Kabosu, Kishu mandarin, Kinotto Grapefruit, Koji, Sanboukan, Citron, Jabara, Sudachi, Tachibana, Tangor, Natsumikan, Hanayuzu, Hyuganatsu, Hirami Lemon (Shikwasa), Buntan (Pomelo), Yuzu, Lime, Lemon, Kaffir lime, etc.), Apricot, Rosaceae (Peach, Japanese peach, etc.), Blueberry, Dutch strawberry, Raspberry, Apple, Banana, Pineapple, Mango, Grape, Kumquat, Melon, Persimmon, Kaki, Apricot, Olive, Pomegranate, Socotra Pomegranate, Chinese laurel, betel nut, trillium melon, plum, tomato, various non-spicy chili peppers (paprika, green pepper, shishito pepper, etc.) from the Capsicum genus of the Solanaceae family, Monk fruit, lotus, wax gourd, ginger, burdock, plants from the Senna genus of the Fabaceae family (shrimp grass, shrimp grass), plants from the Plantago genus of the Plantaginaceae family (plantago ovata, plantain ovata, European plantain, etc.), Chinese laurel, Chinese hazel, blue hazel, amplexicaule, amplexicaule, cashew nut. Tree, macadamia, chestnut, oak, Japanese oak, oak tree, Japanese beech, wolfberry, jujube, jujube, horse chestnut, nutmeg, plants of the Ipomoea genus (morning glory, morning glory, Ipomoea orbiculatus, etc.), sunflower, plants of the Poaceae family (indica rice, japonica rice, javanica rice, glaberrima rice, nerica rice, etc.), plants of the Poaceae family (oats, wild oats, etc.), barley, plants of the Poaceae family (wheat, bread wheat, club wheat, durum wheat, etc.), rye, pearl barley, jute Rice bran, corn, foxtail millet, barnyard millet, millet, finger millet, kodra, pearl millet, fonio, wild rice, teff, buckwheat, tartary buckwheat, quinoa, amaranth, adzuki beans, carob, plants of the Phaseolus genus (kidney beans, runner beans, tepary beans, etc.), grass pea, plants of the Vigna genus (black gram, cowpea, bambara groundnut, mung bean, etc.), winged beans, zeocarpa beans, broad beans, soybeans, bamboo beans, plants of the Sword Bean genus (sword beans, jack beans, red sword beans, white sword beans, beach sword beans, etc.) rice, takanata beans, etc.), tamarind, mucuna pruriens, chickpeas, hyacinth beans, horse gram, moth beans, lima beans, peanuts, lupine beans, peas, kumquat, Dutch ibis, plants of the genus Zanthoxylum in the Rutaceae family (Zanthoxylum japonicum, Zanthoxylum asakura, Zanthoxylum bracteatum, Zanthoxylum ryujinensis, Zanthoxylum takaharaensis, etc.), allspice, ajowan, plants of the genus Piperaceae (pepper, long pepper, pseudo-piper rhizome, amplexicaule, etc.), fenugreek, sesame, castor bean,Preferred are seeds and / or fruits of various hot peppers (capsicum, habanero, jalapeno, capsicum, Trinidad scorpion, Trinidad scorpion Butch Taylor, Bhut Jolokia, Pimon Espelette, Long Viper, etc.) belonging to the Capsicum genus of the Solanaceae family, cumin, anise, cardamom, Illicium verum, Juniperus communis, celery, dill, coriander, plants belonging to the Nigella genus of the Ranunculaceae family (Nigella sativa, Nigella sargentea, etc.), poppy, Aframomum melegueta, and yakuchi. In this case, both the seeds and the fruits may be used, or only the seeds or only the fruits may be used.
[0039] The above-ground stems and leaves of angiosperms are generally called herbs, such as tarragon, allspice, kaffir lime, bitter orange, fenugreek, peppermint plants (peppermint, Japanese mentha, apple mint, water mint, Corsican mint, pennyroyal mint, etc.), spearmints of the Mentha genus of the Lamiaceae family (spearmint, horse mint, green mentha, chili pepper, ginger mint, etc.), catnip, lemon balm, savory pepper, willow mint (hyssop), curry plant, oregano, curry leaf, and plants of the Zanthoxylum genus of the Rutaceae family (Zanthoxylum piperitum, Zanthoxylum aspergillum, Zanthoxylum gracilis, Zanthoxylum umbellata ... Preferably usable are the above-ground stems and leaves of: Japanese pepper, Chinese pepper, Japanese pepper, lemongrass, Chinese laurel, bay leaf, rosemary, red clover, yarrow, celery, plants of the Thymus genus of the Lamiaceae family (common thyme, citrus thyme, wild thyme, etc.), chervil, chives, dill, coriander, basil, parsley, marjoram, plants of the Thymus genus of the Asteraceae family (marigold, African marigold, French marigold, Mexican marigold, lemon marigold, etc.), and lavender.
[0040] Without being limited to these, above-ground stems and leaves of various plants such as the following can also be used. Among them, loquat, persimmon, red pine, plants of the Palmaceae family (washuro, tojuro, aijuro, etc.), Japanese laurel, plants of the Leguminosae family (scutellaria, scutellaria, etc.), Japanese bead tree, plants of the Plantago genus of the Plantaginaceae family (plantago asiatica, plantago major, etc.), madder, Mallotus japonicus, gambir tree, mugwort, Quercus salicina, plants of the Lamiaceae family (mint, scutellaria, scutellaria, etc.), Japanese knotweed, etc.), Hypericum, Prunella, Patchouli, Artemisia, Ardisia crenata, Fabaceae (Japanese knotweed), Lamiaceae (Japanese knotweed), Japanese spicebush, plants of the Dianthus genus of the Caryophyllaceae family (Dianthus campanulata, Dianthus nigricans, Dianthus umbellata, Dianthus quinquefolia, etc.), Japanese holly, Narrow-leaved mountain shiso, Lamiaceae (Philadelphus umbellata, Philadelphus nigricans, Magnolia elata, Aralia aralia, plants of the Asarum genus of the Platycodon family (Philadelphus umbellata, Philadelphus nigricans, Philadelphus umbellata, etc.), Philadelphus umbellata of the Platycodon family Plants of the genus Ipomoea (such as Sedge and Glaucian, etc.), plants of the Lamiaceae family (Perilla, Chirimensho, Madara, Akamiso, Aojiso, etc.), Maidenhair tree, Dendrobium, plants of the genus Sambucus of the family Salicaceae (Sanbu, Western Elder, Elderberry, American Elderberry, etc.), mistletoe, Asian mistletoe, honeysuckle, Japanese honeysuckle, Japanese honeysuckle, Japanese firefly, Japanese bark grass, Japanese hawkweed The above-ground stems and leaves of plants of the Menispermaceae family (Menispermum gracilis, Menispermum japonica, etc.), Menispermum japonica, Akebia japonica, Akebia trifoliata, Japanese laurel, Ardisia crenata, Houttuynia cordata, Japanese laurel, Echinacea purpurea, carrot, Gymnema sylvestre, Gynostemma pentaphyllum, Chinese wolfberry, Japanese laurel, ginkgo, mulberry, Houttuynia cordata, Japanese laurel, cowpea, watermelon, Japanese laurel, rooibos, and Angelica keiskei are preferred. As for the above-ground stems and leaves, either the stems or the leaves alone may be used.
[0041] There are countless types of tea, but preferred are Japanese tea, black tea, Chinese tea, Angelica leaf tea, sweet tea, Gynostemma tea, Ginkgo leaf tea, turmeric tea, Quercus salicina tea, Eleuthero tea, Plantain tea, Kakidooshi tea, Persimmon leaf tea, Kawara Kesmei tea, Bean tea, Gymnema tea, guava tea, Goji berry tea, mulberry leaf tea, Black bean tea, Burdock tea, Cherry blossom tea, Shiso tea, ginger tea, Horsetail tea, Buckwheat tea, Aralia aralia tea, Dandelion tea, Sweet tea, Houttuynia cordata tea, Eucommia tea, Sword bean tea, Elderberry tea, Job's tears tea, Habu tea, Loquat leaf tea, Pine needle tea, Roasted mate tea, Barley tea, Megusurinoki tea, Mugwort tea, Rooibos tea, and Bitter melon tea.
[0042] Teas that are made by heating and drying the stems and leaves of plants, followed by rolling, roasting, steaming, fermentation, etc., have a strong aroma, and Japanese tea, Chinese tea, and black tea are more preferably used. Examples of Japanese tea include sencha, deep-steamed sencha, gyokuro, kabusecha, matcha, tencha, tamaryokucha, nobicha, kamai-iri tamaryokucha, kukicha, budcha, powdered tea, genmaicha, roasted tea, and bancha (ichibancha, akifuyubancha, toyanagi).
[0043] Furthermore, among teas, fermented Chinese tea and black tea (black tea) are more preferable than unfermented Japanese tea. Examples of Chinese tea include oolong tea (Tieguanyin, Golden Catalogue, Narcissus, and Colored), Pu-erh tea, and Jasmine tea, while examples of black tea include Darjeeling, Assam, Uva, Nuwara Eliya, and Keemun. Among them, black tea is the most preferable from the viewpoint of aroma.
[0044] Examples of spore-bearing plants include mushrooms, mosses, seaweeds, and ferns, each of which has a very large variety, but the following plants are preferably used. Mushrooms are edible mushrooms, and parts other than the mushroom pits are preferred, such as Matsutake, Shiitake, Hatutake, Shoro, Agaricus, Tsukuritake, Shimeji, Porcini, Akamomitake, and parts other than the pits of Reishi mushrooms. Mosses are preferably Marchantia polymorpha, Delphaciformes, Polytrichum commune, Polytrichum arbuscula, Lucidum luminosum, Sphagnum moss, Silver moss, Polytrichum formosum, Polytrichum nigricans ... As the seaweed, parts other than the rhizoids of the following seaweeds are preferred: green laver, single-eared rockweed, susabinoori, asakusanori, bouaonoori, iwanori, chishimakurowori, habanori, egonori, ogonori, akamoku, kelp (gagome kombu, macunbu, risori kombu, rausu kombu, hidaka kombu, naga kombu, atsuba kombu, narrow-skinned kombu), Eisenia bicolor, tsuruarame, Ecklonia japonica, kojime, kurome, wakame, undaeme, kubirezuta, dulse, hijiki, funori, makusa, and mozuku. As for ferns, the leaves of field horsetail, pine orchid, Japanese fern, horsetail, fern, salicylate, bracken, holly fern, Japanese holly fern, Japanese bracken, holly fern, Japanese holly fern, Japanese cycad, red fern, Japanese holly fern, star fern, and bracken fern are preferred.
[0045] Preferred sprouted vegetables are legume-type sprouts, such as soybean, mung bean, and fenugreek, and cruciferous-type radish sprouts, such as radish, broccoli, cabbage, mustard, white mustard, watercress, and buckwheat.
[0046] Finally, with regard to fermented grains or beans, the selection is quite limited, with koushi, natto, and shinkiku being preferred.
[0047] The aerosol former preferably contains at least one selected from propylene glycol, 1,3-butanediol, sorbitol, ethylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, glycerin, lactic acid, monoacetin (glycerin monoacetate), diacetin (glycerin diacetate), triacetin (glycerin triacetate), triethylene glycol diacetate, triethyl citrate, isopropyl myristate, methyl stearate, dimethyl dodecanediate, and dimethyl tetradecanediate. In particular, propylene glycol, glycerin, and a mixture of propylene glycol and glycerin are preferred.
[0048] It is preferable to add a freshening agent and crosslinked PVP to the heated aroma generating base material containing at least such aroma source material, aerosol former, and binder. This is because the flavor in the mouth due to the volatile components of the freshening agent brings about a refreshing smoking experience. The crosslinked PVP has a function of sorbing the freshening agent, and can prevent the freshening agent from dissipating over time. Moreover, the freshening agent is sorbed to the crosslinked PVP simply by providing a process of mixing the freshening agent dissolved in a lower alcohol with the crosslinked PVP, so that a process of sorbing the freshening agent to cyclodextrin is not required.
[0049] Examples of the cooling agents include menthol, menthol derivatives such as menthyl ether, menthyl ester, and menthyl carbonate, menthone and its derivatives, menthane and its derivatives, menthane amides such as menthanecarboxylic acid-N-ethylamide [WS3], Nα-(menthanecarbonyl)glycine ethyl ester [WS5], menthanecarboxylic acid-N-(4-cyanophenyl)amide, menthanecarboxylic acid-N-(4-cyanomethylphenyl)amide, and menthanecarboxylic acid-N-(alkoxyalkyl)amide, and methyldiisopropylpropionamide [2,3-dimethyl-2-(2-propyl)-butyric acid-N-methylamide [WS 23], isopulegol and its esters such as (l(-)-isopulegol, l(-)-isopulegol acetate, carboxamides such as N-(2-(pyridin-2-yl)ethyl)-3-p-menthanecarboxamide, (1R,2S,5R)-N-(4-methoxyphenyl)-5-methyl-2-(1-isopropyl)cyclohexane-carboxamide [WS12] and oxamate, and L-carvone, xylitol, thymol, spilanthol, etc. can be used. In particular, menthol and / or xylitol produce a mouth-watering flavor suitable for smoking a heated aromatic cartridge using a heated smoking device.
[0050] Furthermore, it is preferable that the heated aroma-generating substrate contains microcrystalline cellulose. Microcrystalline cellulose is a high-purity microcrystalline cellulose obtained by hydrolyzing and purifying pulp with acid, and is a flowable powder that does not dissolve solvents such as water and ethanol, and is used as an excipient for pharmaceutical tablet molding. This is because the flowability and high compressibility of microcrystalline cellulose, which has a large volume change, are effective in preventing cohesive failure and adhesion to a mold when forming tablets by direct compression. In the present invention, too, by adding microcrystalline cellulose, the aroma source material and the aerosol former are homogeneously mixed and dispersed via a binder, so that in the sheet production of the heated aroma-generating substrate by a three-roll mill that can be formed into a sheet by compression and shear, the cohesive failure of the sheet and adhesion to a metal roll can be effectively prevented.
[0051] In addition, since it does not absorb solvents such as water or ethanol, and exists in powder form within the heated aroma-generating substrate, it is possible to reduce volumetric shrinkage over time due to drying of the heated aroma-generating substrate, etc. Furthermore, it acts as a reinforcing material and can improve the strength of the heated aroma-generating substrate, which makes it possible to prevent the heated aroma-generating substrate from falling off, dropping, deforming, etc. before and after smoking and after long-term storage.
[0052] The heated aroma-generating substrate must contain at least an aroma source material, an aerosol former, and a binder, and in order for these to be homogeneously mixed and dispersed, have enhanced cohesion, and be a high-quality heated aroma-generating substrate with the toughness and strength required for molding, there is a specific blending amount, which was experimentally determined from among many blending amounts. That is, it was found that the aroma source material and the aerosol former must be contained in the heated aroma-generating substrate at 30 to 90 mass% and 10 to 40 mass%, respectively, and the binder must contain the first binder and the second binder at 1 to 30 mass parts and 0.1 to 5 mass parts, respectively, per 100 mass parts of the aroma source material. It was also found that the binder can further improve quality by containing 1 to 25 mass parts of cellulose fiber per 100 mass parts of the aroma source material.
[0053] By appropriately blending suitable amounts of a cooling agent and crosslinked PVP into the basic composition of such a heated aroma-generating substrate, and by adding a suitable amount of microcrystalline cellulose, the quality of the heated aroma-generating substrate can be further improved as described above.
[0054] In order to enjoy the refreshing sensation of the cooling agent and prevent its dissipation over time, the cooling agent and crosslinked PVP must be present in an amount of 1 to 10% by mass and 2 to 10% by mass, respectively, in the heated aroma-generating base material, and the crosslinked PVP must be present in an amount 1 to 6 times the cooling agent content. In addition, the mixing of the freshening agent and the crosslinked PVP requires that the freshening agent is dissolved in a lower alcohol and then mixed with the crosslinked PVP. In this content and mixing method, the aroma of the freshening agent can be enjoyed during smoking, and the crosslinked PVP can sorb the freshening agent and prevent it from dissipating over time. A quantitative index that can determine whether the heated aroma-generating substrate has this dissipation prevention effect was found by comparing the heated aroma-generating substrate of the present invention, which uses menthol as the freshening agent, with the conventional heated aroma-generating substrate. This is the menthol reduction rate d={(d(24)-d(48)} / d(0), where d(0) is the menthol content in a heated aroma-generating substrate weighed out in an amount of about 5 g to 10 g in an environment of 17°C and a relative humidity of 65% RH, d(24) is the mass of the precisely weighed heated aroma-generating substrate after being left for 24 hours at 5°C, and d(48) is the mass of the precisely weighed heated aroma-generating substrate after being left for 48 hours at 5°C, and the menthol loss prevention effect is significant when d≦0.20. Therefore, the heated aroma-generating substrate of the present invention is characterized in that its menthol loss prevention rate d is d≦0.20. The refreshing agents already exemplified exhibit the effect of preventing loss of the refreshing agent when blended in the above-mentioned amounts and by the above-mentioned blending method.
[0055] Microcrystalline cellulose must be contained in the aroma-generating substrate at 2 to 15% by mass in order to improve the strength of the aroma-generating substrate and effectively prevent the aroma-generating substrate from falling off, falling off, or deforming before and after smoking or after long-term storage, and to effectively prevent the sheet from cohesive failure and adhesion to a metal roll when the aroma-generating substrate is produced by compression and shear processing. Although the effect of microcrystalline cellulose can be achieved by being contained within this range, it is more effective if the microcrystalline cellulose has an average particle size of 70 μm or more and 120 μm or less and / or a mass average molecular weight (Mw) of 20,000 or more and 60,000 or less, and it is even more effective if the microcrystalline cellulose has a narrow particle size distribution, with a sieve residue of 250 μm or less and a sieve residue of 75 μm or more and a sieve residue of 45% or more by mass of the total amount of microcrystalline cellulose.
[0056] Since microcrystalline cellulose does not dissolve in water, lower alcohols, aerosol formers, etc., it can be treated in the same way as a fragrance source material, so it is preferable to mix microcrystalline cellulose together with the fragrance source material and the aerosol former.
[0057] In the present invention, microcrystalline cellulose can improve the strength of a heated aroma-generating substrate, prevent the heated aroma-generating substrate from falling off, dropping, or deforming before and after smoking and after long-term storage, and can prevent the sheet from cohesive failure and adhesion to a metal roll when the heated aroma-generating substrate is produced by a compression / shear processing method, and a quantitative index capable of determining whether the heated aroma-generating substrate has this effect has been found. The first quantitative index is the rate of shape change that occurs between a heated aroma-generating substrate before drying that is shaped to a length of 50 mm, a width of 15 mm, and a thickness of 0.3 mm, and a heated aroma-generating substrate after drying the heated aroma-generating substrate before drying at 105° C. for 10 minutes. The second quantitative index is the rate of change in shape between a heated aroma-generating substrate having a width of 50 mm, a width of 15 mm, and a thickness of 0.3 mm before drying and a heated aroma-generating substrate having the same shape after drying for 15 minutes at 105° C. The third quantitative index is the rate of change in shape between a heated aroma-generating substrate having a length of 12 mm, a width of 1.5 mm, and a thickness of 0.3 mm before drying and a heated aroma-generating substrate having the same shape after drying for 10 minutes at 105° C. The fourth quantitative index is the rate of change in shape between a heated aroma-generating substrate having a length of 12 mm, a width of 1.5 mm, and a thickness of 0.3 mm before drying and a heated aroma-generating substrate having the same shape after drying for 15 minutes at 105° C. As a result of comparing the heated aroma-generating substrate of the present invention with conventional heated aroma-generating substrates, it was found that a heated aroma-generating substrate whose shape change rate is below a certain limit value is a heated aroma-generating substrate that exhibits the desired strength, the effect of preventing the heated aroma-generating substrate from falling off, dropping, and deformation before and after smoking and after long-term storage, and the effect of preventing the sheet from cohesively failing and adhering to metal rolls in compression and shear processing. Below, the allowable ranges of the change rates of length, width, and thickness are shown as specific shape change rates for the first to fourth quantitative indicators.
[0058] The first quantitative index of the heated aroma-generating substrate of the present invention uses a heated aroma-generating substrate having a shape of 50 mm in length, 15 mm in width and 0.3 mm in thickness, and defines the length, width, thickness and volume of the heated aroma-generating substrate before drying as L0 (=50 mm), W0 (=15 mm) and T0 (=0.3 mm), respectively, and defines the length, width and thickness of the heated aroma-generating substrate after drying for 10 minutes at 105°C as When L is 10 mm, W is 10 mm, and T is 10 mm, the length change rate La (%) is defined as = {(L0-L10) / L0} x 100, the width change rate Wa (%) is defined as = {(W0-W10) / W0} x 100, and the thickness change rate Ta (%) is defined as = {(T0-T10) / T0} x 100, and are characterized in that they satisfy 0%≦La≦7.2%, 0%≦Wa≦5.7%, and 0%≦Ta≦1.2%, respectively.
[0059] The second quantitative index of the heated aroma-generating substrate of the present invention is a substrate having a length of 50 mm, a width of 15 mm and a thickness of 0.3 mm. The length, width, thickness and volume of the heated aroma-generating substrate before drying are L0 (=50 mm), W0 (=15 mm) and T0 (=0.3 mm), respectively, and the length, width and thickness of the heated aroma-generating substrate after drying for 15 minutes at 105°C are L15 mm, W15 mm and T2 (=0.3 mm), respectively. where L0 is 15 mm and T is 15 mm, the length change rate Lb (%) is defined as = {(L0-L15) / L0} x 100, the width change rate Wb (%) is defined as = {(W0-W15) / W0} x 100, and the thickness change rate Tb (%) is defined as = {(T0-T15) / T0} x 100, and they are characterized in that they satisfy 0%≦Lb≦8.1%, 0%≦Wb≦6.1%, 0%≦Tb≦1.5%, and 0%≦Vb≦14.3%, respectively.
[0060] The third quantitative index of the heated aroma-generating substrate of the present invention is determined by using a heated aroma-generating substrate having a length of 12 mm, a width of 1.5 mm and a thickness of 0.3 mm, and defining the length, width, thickness and volume of the heated aroma-generating substrate before drying as L'0 (=12 mm), W'0 (=1.5 mm) and T'0 (=0.3 mm), respectively, and defining the length, width and thickness of the heated aroma-generating substrate after drying for 10 minutes at 105°C as L'10mm, respectively. , W'10mm, and T'10mm, the length change rate L'a (%) is defined as = {(L'0-L'10) / L'0} x 100, the width change rate W'a (%) = {(W'0-W'10) / W0} x 100, and the thickness change rate T'a (%) = {(T'0-T'10) / T'0} x 100, and are characterized by satisfying 0%≦L'a≦4.8%, 0%≦W'a≦5.0%, and 0%≦T'a≦1.2%, respectively.
[0061] The fourth quantitative index of the heated aroma-generating substrate of the present invention is determined by using a heated aroma-generating substrate having a length of 12 mm, a width of 1.5 mm and a thickness of 0.3 mm, and defining the length, width, thickness and volume of the heated aroma-generating substrate before drying as L'0 (=12 mm), W'0 (=1.5 mm) and T'0 (=0.3 mm), respectively, and defining the length, width and thickness of the heated aroma-generating substrate after drying for 15 minutes at 105°C as L'15mm, respectively. , W'15mm, and T'15mm, the length change rate L'b (%) is defined as {(L'0-L'15) / L'0}×100, the width change rate W'b (%) is defined as {(W'0-W15) / W'0}×100, and the thickness change rate T'b (%) is defined as {(T'0-T15) / T'0}×100, and are characterized in that they satisfy 0%≦L'b≦5.8%, 0%≦W'b≦5.1%, and 0%≦T'b≦1.5%, respectively.
[0062] As described above, the components, composition, properties, etc. of the heated aroma-generating substrate of the present invention have been explained, but as already described, the properties of the heated aroma-generating substrate are affected by the manufacturing method. Therefore, it is an object of the present invention to provide a manufacturing method that is preferable for a high-quality heated aroma-generating substrate.
[0063] First, the method for producing a heated aroma-generating substrate of the present invention is characterized by comprising a first mixing step of mixing an aroma source material, an aerosol former, and a first binder, a second mixing step of mixing a second binder with the mixture produced in the first mixing step, and a molding step of molding the mixture produced in the second mixing step into a heated aroma-generating substrate. The reason why such a manufacturing step of mixing different binders stepwise is preferable is unclear, but as already explained, it is believed that the cellulose-based first binder promotes uniform mixing and dispersion of the aroma source material and the aerosol former to form a stable sol state, and then the polysaccharide-based second binder forms a gel state that enhances the binding of these.
[0064] Secondly, the manufacturing method of the heated aroma-generating substrate of the present invention is characterized by comprising a first mixing step of mixing an aroma source material, an aerosol former, and a first binder, and a mixing and molding step of molding the mixture produced in the first mixing step into a heated aroma-generating substrate while mixing a second binder. This is because the compression-shear molding method can uniformly mix and disperse the second binder and can mold the heated aroma-generating substrate into a sheet-like heated aroma-generating substrate, and therefore has the effect of omitting the second mixing step and shortening the manufacturing process.
[0065] Thirdly, the method for producing the heated aroma-generating substrate of the present invention is characterized in that a curing step is provided immediately after the first mixing step, in which the mixture produced in the first mixing step is cured. In particular, the curing step is preferably performed at a temperature of 15°C or more and 30°C or less, and for a time of 72 hours or more and 336 hours or less. As already explained, it is presumed that the curing step has an effect of increasing and stabilizing the dispersion degree of the aroma source material in the sol state formed by promoting the uniform mixing and dispersion of the aroma source material and the aerosol former with the cellulose-based first binder. This is because the volume of the mixture is increased in the curing step. And, at a temperature below 15°C, the volume increase is also small, and the curing step has no effect on the quality of the heated aroma-generating substrate, and at a temperature above 30°C, the mixture becomes gelled, although the cause is unknown. Furthermore, if the curing time is less than 72 hours, the volume increase is slight and no effect of the curing process on the quality of the heated aroma-generating substrate is observed. If the curing time exceeds 336 hours, this volume increase stops and the effect of the curing process on the quality of the heated aroma-generating substrate becomes saturated, and curing for a longer period of time may result in gelation.
[0066] Fourthly, the method for producing a heated aroma-generating substrate of the present invention is characterized by comprising a third mixing step of mixing an aroma source material, an aerosol former, a first binder, and a second binder, a curing step (Y) of curing the mixture produced in the third mixing step, and a molding step of molding the mixture produced in the curing step into a heated aroma-generating substrate. When the curing step is performed, it is not necessary to add the first binder and the second binder step by step, and the manufacturing process can include a third mixing step of mixing an aroma source material, an aerosol former, a first binder, and a second binder, and a curing step of curing the mixture produced in the third mixing step. In this curing step, it is considered that the effect of increasing the dispersion degree of the aroma source material by the first binder and the effect of increasing the cohesion by the second binder occur in parallel.
[0067] Fifth, the manufacturing method for a heated aroma-generating substrate of the present invention is characterized in that, in the manufacturing methods described in the first to fourth paragraphs, when a refreshing agent is added to the heated aroma-generating substrate, a fourth mixing step is added in which crosslinked PVP is mixed into a lower alcohol solution of the refreshing agent in order to mix the refreshing agent in the first mixing step, the second mixing step, the third mixing step, and the mixing and molding step.
[0068] Finally, the heated aroma-emitting source of the present invention and the heated aroma cartridge of the present invention, which use the high-quality heated aroma-emitting substrate of the present invention produced by the above-mentioned components, composition and method, will be described.
[0069] The heated aroma generating source constituting the heated aroma cartridge of the present invention is characterized in that it is a single heated aroma generating substrate or an aggregate of heated aroma generating substrates. In the case of a single heated aroma generating source, it is preferable that the heated aroma generating source is in the form of a sheet, and in the case of an aggregate, it is preferable that a suitable amount of sheet-shaped or cut heated aroma generating substrates are bundled. In particular, the shape of the cut heated aroma generating substrate is not limited to a prismatic, flat, cylindrical, granular, etc., but is preferably a prismatic shape from the viewpoint of forming a gas flow path. However, whether in the form of a sheet or a prismatic shape, in order to more sufficiently secure the gas flow path, it is required that the heated aroma generating source is arranged with the heated aroma generating substrate so that the voids are communicated in the longitudinal direction of the heated aroma cartridge equipped with the heated aroma generating source.
[0070] Such a heated aroma generating source may be stored as it is in an exterior member that wraps the entire heated aroma cartridge, or may be wrapped in a heated aroma generating substrate wrapping member that is a cylindrical scroll. In the former case, the heated aroma generating substrate is packed in an exterior member, while in the latter case, for example, it is sufficient to simply wrap it in an exterior member, which is efficient in manufacturing a heated aroma cartridge. The heated aroma generating substrate wrapping member can be made of paper as in the conventional technology, but in the case of a heated smoking device equipped with a blade-type heat source using a heater, there is no contact with the heat source and the heated aroma generating substrate needs to be aerosol former resistant, so a plastic film is more suitable. In particular, from the viewpoint of environmental protection, a biodegradable plastic film is more preferable. Examples of plastics include plastics such as polyolefin, polyester, and nylon, and engineering plastics, and examples of biodegradable plastics include poly(3-hydroxybutyrate) (PHB), poly(ε-caprolactone) (PCL), poly(butylene succinate) (PBS), poly(L-lactide) (PLA However, in the case of an omnidirectional heat source using electromagnetic induction heating, the entire heated aroma generating source of the heated aroma cartridge is heated to about 240°C, so when using plastic as the heated aroma generating substrate wrapping member, it is necessary to apply a film of a special engineering plastic that has the same heat resistance as cellulose fibers (which constitute paper) that begin to undergo glass transition or thermal decomposition at about 300°C, that is, a glass transition temperature of 240°C or higher. Examples of such special engineering plastics include polyamide-imide, polyarylate, polyimide, polytriazine, and liquid crystal polymer.
[0071] Next, the heated aroma generating cartridge of the present invention is characterized in that the heated aroma generating source is stored in a heated aroma cartridge exterior member which is a cylindrical body, and the heated aroma cartridge exterior member itself forms a mouthpiece. The heated aroma cartridge does not necessarily require a filter member for filtering carbon monoxide, nicotine, tar, etc., which are contained in gas components and particulate components contained in smoke generated by the combustion of tobacco leaves and cigarette paper and which have adverse effects on the body, as in cigarettes, and unpleasant taste components, so the mouthpiece may be simply hollow. However, since the heated aroma cartridge exterior member which is a cylindrical body needs to have a strength sufficient to be held in the mouth, it is more preferable that it is made of thick paper, or a plastic or engineering plastic with a moderate thickness, and from the viewpoint of environmental protection, it is even more preferable that it is made of a biodegradable plastic film. As the plastic and biodegradable plastic, those listed in the heated aroma generating substrate wrapping member can be used. However, while this is also applicable to heated smoking devices equipped with a blade-type heat source using a heater, in the case of an omnidirectional heat source using electromagnetic induction heating, the entire heated aroma generating source of the heated aroma cartridge is heated to approximately 240°C, so when using plastic as the exterior component of the heated aroma cartridge, it is necessary to use a special engineering plastic with a glass transition temperature of 240°C or higher, as already mentioned.
[0072] In addition, the heated aroma cartridge of the present invention can be configured such that the mouthpiece is attached to the heated aroma generating source in the longitudinal direction and is stored in a cylindrical heated aroma cartridge exterior member, and for the same reason, the mouthpiece may be a simple hollow tube. In this case, the heated aroma cartridge exterior member can be made of thin paper used in conventional cigarettes, but the hollow tube is more preferably made of thick paper, or a plastic or engineering plastic with a suitable thickness, and from the viewpoint of environmental protection, it is even more preferably made of a biodegradable plastic film. In this case, as already mentioned, it is necessary to select a plastic suitable for the heat source for the heated aroma cartridge exterior member.
[0073] In any of these mouthpieces, it is preferable that the mouthpiece is equipped with at least one of the following: a support member for preventing movement of the heated aroma source toward the mouthpiece due to smoking; a cooling member for actively cooling the volatiles in the aerosol former to increase the amount of aerosol produced; and a filter member for filtering out, albeit to a small extent, carbon monoxide, nicotine, tar, etc., and unpleasant flavor components that are generated by heating the heated aroma source.
[0074] Furthermore, in any of these mouthpieces, the support member and cooling member are arranged in the stated order in the longitudinal direction from the heated aroma generation source, the support member and filter member are arranged in the stated order in the longitudinal direction from the heated aroma generation source, the cooling member and filter member are arranged in the stated order in the longitudinal direction from the heated aroma generation source, or the support member, cooling member and filter member are arranged in the stated order in the longitudinal direction from the heated aroma generation source, thereby allowing the taste of the heated aroma cartridge to be variously adjusted.
[0075] The mouthpiece having at least one selected from the support member, the cooling member, and the filter member can be directly attached to the heated aroma cartridge exterior member, but it is preferable to have the support member, the cooling member, and the filter member wrapped in a cylindrically wound mouthpiece wrapping member in advance, which makes it easier to assemble the heated aroma cartridge. Also, the support member, the cooling member, and the filter member selected for attachment to the mouthpiece may be individually wrapped in a cylindrically wound mouthpiece wrapping member. For such members that do not transmit the temperature of the heat source, the paper that has been used in the past can be replaced with plastic or engineering plastic, and it is particularly preferable that the paper is biodegradable plastic.
[0076] Furthermore, forming at least one hole on the outer peripheral surface of the mouthpiece is also an effective means for adjusting the taste, amount of inhalation, etc. of the heated aroma cartridge. Effect of the Invention
[0077] According to the heated aroma-generating substrate of the present invention, when a heated aroma cartridge equipped with a heated aroma source made from it is attached to or detached from a heated smoking device, problems such as deformation, detachment, or falling of the heated aroma-generating substrate do not occur, and when smoking, the aroma volatilized from the heated aroma source material can be fully enjoyed.In the manufacture of the heated aroma-generating substrate, the aroma source material, aerosol former, and binder are uniformly dispersed and bound, and have the toughness and strength required for molding processing, allowing stable production.
[0078] Furthermore, the heated aroma-generating substrate of the present invention is characterized in that when a refreshing agent such as menthol or xylitol is added as an aromatic agent, the dispersion of the refreshing agent over time is suppressed, and this has the effect of allowing the aroma of the heated aroma-generating substrate to be fully enjoyed when smoking after a heated aroma cartridge equipped with a heated aroma-generating source containing the same has been stored for a long period of time and is attached to a heated smoking device.
[0079] Furthermore, the heated aroma-generating substrate of the present invention is characterized by little dimensional change due to drying, and even after a heated aroma cartridge equipped with a heated aroma-generating source composed of the heated aroma-generating substrate is attached to a heated smoking device and used for smoking, the heated aroma-generating substrate does not fall off or fall off from the heated aroma cartridge, and even after long-term storage, the heated aroma-generating substrate does not fall off or fall off from the heated aroma cartridge, making it easy to handle and effective in preventing contamination of the heat source of the heated smoking device. [Brief description of the drawings]
[0080] [Figure 1] In order to evaluate a heated aroma cartridge equipped with a heated aroma generating substrate according to one embodiment of the present invention, a heated aroma cartridge for a blade-type heat source was manufactured and attached to a blade-type heated smoking device, as shown in this schematic cross-sectional diagram cut through the central axis of a cylinder. [Diagram 2]In order to evaluate a heated aroma cartridge equipped with a heated aroma-generating substrate according to one embodiment of the present invention, a heated aroma cartridge for an omnidirectional heat source was manufactured and attached to an omnidirectional heated smoking device. This is a schematic cross-sectional diagram cut through the central axis of the cylinder. [Diagram 3] This is a schematic cross-sectional diagram perpendicular to the longitudinal direction showing the arrangement of heated aroma-generating sources in a heated aroma-generating source in which a heated aroma-generating substrate assembly is wrapped with a heated aroma-generating substrate wrapping member according to one embodiment of the present invention, and the gas flow path generated by this arrangement. [Figure 4] FIG. 2 is a schematic perspective view showing an example of a support member, a cooling member, and a filter member that constitute a heated aroma cartridge together with a heated aroma-generating substrate according to one embodiment of the present invention. [Diagram 5] This is a schematic cross-sectional diagram cut through the central axis of a cylinder, showing the configuration of a heated aroma cartridge in one embodiment of the present invention, in which the heated aroma generation source of the present invention is stored in a cylindrical heated aroma cartridge outer casing member, and the heated aroma cartridge outer casing member forms the mouthpiece. [Figure 6] This is a schematic cross-sectional diagram cut through the central axis of a cylinder, showing the configuration of a heated aroma cartridge in one embodiment of the present invention, in which a mouthpiece is attached in the longitudinal direction of a heated aroma generation source and is housed in a cylindrical heated aroma cartridge outer casing. [Figure 7] This is a schematic cross-sectional diagram cut through the central axis of a cylinder showing the configuration of a heated aroma cartridge in one embodiment of the present invention, in which a mouthpiece is attached in the longitudinal direction of a heated aroma generating source of the present invention, the mouthpiece comprises a support member, a cooling member, and a filter member, and is arranged in that order in the longitudinal direction from the heated aroma generating source, and further, a portion of the mouthpiece is wrapped with a mouthpiece reinforcing member. [Figure 8]1 is a flow chart showing steps of producing a heated aroma-generating substrate according to one embodiment of the present invention, comprising a first mixing step of mixing an aroma source material, an aerosol former, and a first binder, a second mixing step of mixing a second binder with the mixture produced in the first mixing step, and first and second shaping steps of shaping the mixture produced in the second mixing step into a heated aroma-generating substrate, wherein the first shaping step is a step of shaping into a sheet-like heated aroma-generating substrate and the second shaping step is a step of cutting into a long rectangular columnar heated aroma-generating substrate. [Figure 9] 1 is a flow chart showing a process for producing a heated aroma-generating substrate according to one embodiment of the present invention, comprising a first mixing step of mixing an aroma source material, an aerosol former, and a first binder, a mixing and molding step of molding the mixture produced in the first mixing step into a heated aroma-generating substrate while mixing a second binder, and a second molding step, in which the first molding step is a step of molding into a sheet-like heated aroma-generating substrate, and the second molding step is a step of cutting into long rectangular column-shaped heated aroma-generating substrates. [Figure 10] 1 is a flow chart showing a process for producing a heated aroma-generating substrate according to one embodiment of the present invention, which includes an additional curing process for curing the mixture produced in the first mixing process immediately after the first mixing process, a mixing and molding process for molding the mixture produced in the first mixing process into a heated aroma-generating substrate while mixing a second binder, and a second molding process, in which the first molding process is a process for molding into a sheet-like heated aroma-generating substrate, and the second molding process is a process for cutting into long rectangular column-shaped heated aroma-generating substrates. [Figure 11] 1 is a flow chart showing steps of producing a heated aroma-generating substrate according to one embodiment of the present invention, including a third mixing step of mixing an aroma source material, an aerosol former, a first binder, and a second binder, a curing step of curing the mixture produced in the third mixing step, and first and second molding steps of molding the mixture produced in the curing step into a heated aroma-generating substrate, where the first molding step is a step of molding into a sheet-like heated aroma-generating substrate and the second molding step is a step of cutting into a long rectangular column-shaped heated aroma-generating substrate. [Figure 12] FIG. 11 is a flow chart showing a process for producing a heated aroma-generating base material by adding a fourth mixing step of mixing a crosslinked PVP into a lower alcohol solution of menthol and / or xylitol in order to mix menthol and / or xylitol in the first mixing step shown in FIG. 10 according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0081] The present invention will be described in more detail below with reference to examples, comparative examples, figures, etc. The present invention is not limited to these examples, and various modifications and variations are possible without departing from the spirit and scope of the present invention. It is possible to make the above-mentioned invention, and it is limited only by the technical idea described in the claims. It is.
[0082] First, in order to concretely show the effect of the type of binder and the method of adding the binder, Examples 1 to 10 are given. Additionally, experiments for Comparative Examples 1 to 4 were carried out. Example 1
[0083] The first binder, methylcellulose and sodium carboxymethylcellulose (CM C) and the second binder, glucomannan, are mixed stepwise by the method shown in FIG. A heated aroma-generating base material was produced. Xylitol was added as a cooling agent in the first mixing step. For this reason, the xylitol solution is Xylitol 100 parts by weight 400 parts by mass of water was mixed and stirred to produce the product.
[0084] On the other hand, the aroma source materials, black tea leaves and sweet tea vine leaves, are soaked in water so that their moisture content is about 2% by mass. The powder was dried at 70°C, crushed, and passed through a 80 mesh sieve. The temperature is preferably in the range of 60°C to 80°C. It is easy to achieve a desired moisture content while avoiding the loss of flavor components. It is more preferable that the temperature is 65° C. or more and 75° C. or less. To facilitate this, the dried ground material must absorb moisture, and the moisture content must be less than 5% by mass. It is preferably 0.1% by mass or less, more preferably 3% by mass or less, and more preferably 0.1% by mass or more. It is even more preferable.
[0085] In the first mixing step shown in FIG. Dried and ground black tea leaves 80 parts by weight Dried and crushed sweet potato vine leaves 20 parts by weight Glycerin 30 parts by weight Propylene glycol 30 parts by weight Methylcellulose 15 parts by weight Sodium carboxymethylcellulose (CMC) 4 parts by weight Xylitol / water solution 8 parts by weight were charged into a mixer and mixed for 15 minutes to produce a first mixture.
[0086] The first mixture is mixed with a second binder in a second mixing step, and then the heated aroma-emitting sheet is formed. The raw material was then put into the mixing and molding process, which also serves as the first molding process. In the step, 0.5 parts by mass of glucomannan, which is a second binder, is added to 100 parts by mass of the first mixture. While adding 20 parts by weight of water, the doctor blade is pressed against the roll to form a sheet. The triple roll milling process is repeated to produce a second mixture, which is the composition of the heated aroma-generating substrate. The mixture is mixed and molded into a sheet-shaped heated aroma-emitting substrate. During the process, the moisture evaporates moderately, forming a heated sheet-shaped aroma-emitting substrate with a thickness of 0.3 mm. The three-roll mill was operated eight times with the roll interval and roll speed ratio adjusted so that the powder was formed. This mixing and molding step is the second mixing step ( 100 parts by mass of the first mixture, 0.5 parts by mass of glucomannan as the second binder, and 20 parts by mass of water. The process combines the first step of mixing the ingredients and the second step of forming the mixture into a sheet using a three-roll mill. This has the advantage of simplifying the manufacturing process shown in FIG. 8, but the resulting sheet-like There is no difference in the mixing and dispersion state of the heated aroma-generating base material.
[0087] Next, in the second forming step shown in FIG. 9, the sheet is molded into a 150 mm long and 240 mm wide sheet. The pieces are then cut into rectangles measuring 240 mm in length and 1 mm in width using a rotary cutter. The product is cut into a shape with a diameter of 0.5 mm and a thickness of 0.3 mm to produce a long rectangular columnar heated aroma-emitting substrate. The longitudinal and transverse directions of this sheet were parallel and perpendicular to the rotation axis of the roll, respectively. It is in the direction.
[0088] The 50 long rectangular column-shaped heated aroma-emitting substrates 3211 (FIG. 3) thus manufactured were After being aligned in the hand direction, the heated aroma generating substrate wrapping member 322 is made of 34 g / m2 of paper is wrapped around it and glued to create a cylindrical roll with an outer diameter of 6.9 mm. After the product was manufactured, it was cut into a length of 12.0 mm to produce the heated aroma source 320. As a result, the heated aroma-emitting substrate 3, which was 12.0 mm long, 1.5 mm wide, and 0.3 mm thick, was 211 (FIG. 3) 50 pieces of the heated aroma source 320 wrapped in paper are heated aroma source 3 Each of the heated aroma generating substrates 321 contains 0.29 g of the heated aroma generating source. The volumetric filling ratio of the heated aroma-emitting substrate assembly 321 (FIG. 3) to the volume of 320 is 0.60 In addition, the aroma generating substrate 3211 (FIG. 3) had a temperature of 100 mass parts of the aroma source material. The aerosol former is 60 parts by mass, the first binder is methylcellulose and CM C was 15 parts by mass and 4 parts by mass, respectively, and glucomannan, which was the second binder, was 0.9 Parts by weight included.
[0089] Here, the heated aroma-emitting substrate wrapping material for wrapping the heated aroma-emitting substrate assembly 321 is 322 does not have to be paper, but it should have a strength equivalent to that of paper with a basis weight of 30g / m2 to 40g / m2. A plastic film can be used. As described later, the aroma generating substrate 3 is heated without coming into contact with the heat source of the heated smoking device. Since it comes into contact with the aerosol former, which is also an organic solvent contained in 211 (Figure 3), It is preferable to use plastic films that have the same strength as the paper. From the viewpoint of protection, it is more preferable to use a biodegradable plastic film. In the case of plastic films, the film thickness must be selected according to the material. The same is true for the heated aroma-generating substrate wrapping members of the examples and comparative examples. Selection for heated aroma cartridges to be used in heated smoking devices equipped with a heat source of a heat source It is a selectable material.
[0090] In Examples 1 to 5 and Comparative Examples 1 and 2, the outer diameter and length are subjected to the above-mentioned load. The source of the hot aroma is the heater used in the smoking test described below. IQOS (registered trademark, manufactured by Philip Morris) is a heated smoking device equipped with a handheld heat source. For use. Example 2
[0091] Example 2 is a composition exactly the same as Example 1, but in order to concretely demonstrate the effect of curing, The aroma-emitting substrate was manufactured according to the manufacturing process shown in FIG. 10, to which a curing process was added. The first mixture was produced in the same manner as in Example 1 up to the mixing step, but the second mixing step and Prior to the mixing and molding step, which also serves as the first molding step, the first mixture is sealed in a polyethylene bag; A curing process was carried out at 20°C for 144 hours (6 days). Through this curing process, The apparent volume is about 1.5 times larger, and the curing mixture after the curing process is smaller than before curing. It was visually observed that the amount of tea powder that was released was reduced. The raw material is a fragrance source material, an aerosol former, and a first binder, methylcellulose. This is believed to be due to the improved dispersion of the powder and CMC.
[0092] The curing mixture thus produced was subjected to the mixing and molding step, the second forming step, and the third forming step, as in Example 1. Through the forming process, the heated aroma source 320 was manufactured. 50 pieces of heated aroma-emitting substrates 321 each having a diameter of 1.5 mm and a thickness of 0.3 mm are placed on a paper substrate. The heated aroma generating source 320 wrapped around the heated aroma generating substrate wrapping member 322 is Each aroma generating source 320 contains 0.29 g of heated aroma generating substrate aggregate 321. The volumetric filling ratio of the heated aroma-emitting substrate assembly 321 to the volume of the thermal aroma-emitting source 320 is 0. 60. As in Example 1, the aroma-generating substrate 3211 to be heated (FIG. 3) For 100 parts by mass of the source material, 60 parts by mass of the aerosol former and methyl The second binder, 15 parts by weight of cellulose and 4 parts by weight of CMC, Contains 0.9 parts by mass of lacomannan. <Comparative Example 1>
[0093] Comparative Example 1 was conducted to specifically demonstrate the effect of adding the first binder and the second binder in two separate steps. The second binder, glucomannan, was added in the first mixing step instead of the mixing and molding step in Example 1. The procedure was carried out except that the first binder, methyl cellulose, and CMC were mixed simultaneously in the first step. A heated aroma source was prepared as in Example 1.
[0094] A xylitol aqueous solution for adding xylitol as a cooling agent in the first mixing step teeth, Xylitol 100 parts by weight 400 parts by mass of water The aromatic materials, black tea leaves and sweet tea vine leaves, were mixed and stirred for 7 After drying at 0°C, the material was crushed and passed through a 80 mesh sieve. The moisture content of the dried ground product was about 2% by mass.
[0095] In the first mixing step, Dried and ground black tea leaves 80 parts by weight Dried and crushed sweet potato vine leaves 20 parts by weight Glycerin 30 parts by weight Propylene glycol 30 parts by weight Methylcellulose 15 parts by weight Sodium carboxymethylcellulose (CMC) 4 parts by weight Glucomannan 0.9 parts by weight Xylitol / water solution 8 parts by weight Water 37 parts by mass were charged into a mixer and mixed for 15 minutes to produce a first mixture.
[0096] The first mixture thus prepared was different from Example 1 in that it did not contain a second binder. The doctor blade is pressed against the roll to form the sheet. The molten steel is then fed into the first forming process, in which the roll gap and the roll speed ratio are adjusted. The roll mill was repeated eight times to obtain a sheet of heated material with a thickness of 0.3 mm, after which the moisture had evaporated to an appropriate level. The fragrance-generating substrate was molded.
[0097] Next, similarly to Example 1, a heated aroma emitting source was produced through a second molding step. As a result, 50 heated aromatic sticks measuring 12.0 mm in length, 1.5 mm in width, and 0.3 mm in thickness were The aroma generating substrate assembly 321 is wrapped around a heated aroma generating substrate wrapping member 322 made of paper. The heated aroma source 320 is a heated aroma source having a capacity of 0.29 g per heated aroma source 320. The volume of the heated aroma-emitting substrate relative to the volume of the heated aroma-emitting source 320, including the raw substrate mass 321 The volume filling rate of the assembly 321 was 0.60. The raw base material 3211 (FIG. 3) is a mixture of 60 parts by mass of the aerosol former and 100 parts by mass of the fragrance source material. parts by weight, methyl cellulose and CMC as the first binder, respectively, 15 parts by weight and 4 parts by mass, and 0.9 parts by mass of the second binder, glucomannan. Example 3
[0098] Example 3 shows that the effect of the present invention does not depend on the cross-sectional shape perpendicular to the longitudinal direction of the aroma-generating substrate to be heated. In order to specifically show that the aroma generating substrate is heated, the width and thickness are made smaller than those of Example 2. In the same manner as in Example 2, the first mixing step, the curing step, and the second mixing step were carried out. The second mixture is produced in a mixing and molding process which also serves as the first molding process, and the sheet-shaped heated The aroma-emitting substrate was formed. However, in Example 3, the position of the doctor blade and the roll interval were A three-roll mill in which the speed ratio between the rolls and other factors were adjusted differently from those in Example 2 The process was repeated eight times to form a sheet-shaped heated aroma-emitting substrate having a thickness of 0.1 mm. As in Example 1, in the second molding process, the sheet is cut into a rectangle of 150 mm in length and 240 mm in width. After that, a rotary cutter was used to cut the sheet into pieces 240 mm long, 1.0 mm wide and 0.1 mm thick. The substrate was cut into a shape of m to produce a long rectangular columnar heated aroma-emitting substrate.
[0099] In the case of this heated aroma-generating substrate, 225 pieces are aligned in the longitudinal direction and the basis weight is 34 g / m The roll is then wrapped in paper No. 2 and glued together to form a cylindrical roll with an outer diameter of 6.9 mm. After the object was manufactured, it was cut into pieces of 12.0 mm in length. The heated aroma-emitting substrate assembly 321 is made of paper and has a diameter of 1.0 mm and a thickness of 0.1 mm. The heated aroma source 320 wrapped around the heated aroma-emitting substrate wrapping member 322 is Each of the thermal aroma generating sources 320 contains 0.29 g of the heated aroma generating substrate aggregate 321. The volumetric filling ratio of the heated aroma-emitting substrate assembly 321 to the volume of the heated aroma source 320 is 0.6 0. Naturally, the composition of the heated aroma-generating substrate 3211 (FIG. 3) in this case was the same as that in Example 1. and 2, and Comparative Example 1. Example 4
[0100] In Example 4, the effect of the present invention does not depend on the cross-sectional shape perpendicular to the longitudinal direction of the aroma-generating substrate to be heated. In order to specifically show that the aroma generating substrate is heated, the width and thickness of the heated aroma generating substrate are made larger than those of Example 2. In the same manner as in Example 2, the first mixing step, the curing step, and the second mixing step were carried out. The second mixture is produced in a mixing and molding process which also serves as the first molding process, and the sheet-shaped heated The aroma-emitting substrate was formed. However, in Example 4, the position of the doctor blade and the roll interval were A three-roll mill in which the speed ratio between the rolls and other factors were adjusted differently from those in Example 2 The process was repeated eight times to form a sheet-shaped heated aroma-emitting substrate having a thickness of 0.5 mm. As in Example 1, in the second molding process, the sheet is cut into a rectangle of 150 mm in length and 240 mm in width. After that, a rotary cutter was used to cut the sheet into pieces 240 mm long, 2.0 mm wide and 0.5 mm thick. The substrate was cut into a shape of m to produce a long rectangular columnar heated aroma-emitting substrate.
[0101] In the case of this heated aroma-generating substrate, 23 pieces are aligned in the longitudinal direction and have a basis weight of 34 g / m The roll is then wrapped in paper No. 2 and glued together to form a cylindrical roll with an outer diameter of 6.9 mm. After the object was manufactured, it was cut into pieces of 12.0 mm in length. 23 heated aroma generating substrates 321 each having a diameter of 2.0 mm and a thickness of 0.5 mm were placed on the heated aroma generating substrate 321 made of paper. The heated aroma source 320 wrapped around the aroma-generating substrate wrapping member 322 is Each raw material source 320 contains 0.30 g of the heated aroma generating substrate aggregate 321. The volumetric filling ratio of the heated aroma-generating substrate assembly 321 to the volume of the source 320 was 0.62. Naturally, the composition of the heated aroma-generating substrate 3211 (FIG. 3) in this case was the same as that in Examples 1 and 2, Also, the same as in Comparative Example 1. <Comparative Example 2>
[0102] In Comparative Example 2, glucomannan was not used in order to confirm the effect of the second binder. In the same manner as in Comparative Example 1, an attempt was made to produce a heated aroma-generating base material, but a three-roll mill was used. In the first molding step, breakage and peeling occur, making it difficult to form the glucomannan into a sheet. It was found that it is an essential binder for the heated aroma generating substrate and its manufacture. In order to carry out the smoke test, heated aroma sources of the same size as those in Examples 1 and 2 and Comparative Example 1 were used. was manufactured. Example 5
[0103] In Example 5, in order to concretely demonstrate the influence of curing, curing was added to the manufacturing process of Comparative Example 1. A new process was added. That is, the first mixture in Comparative Example 1 was sealed in a polyethylene bag. The material was then left to cure at 20°C for 144 hours (6 days). The apparent volume of the curing mixture after the curing process is about 1.4 times that of the original volume before curing. It was visually observed that the amount of ground tea powder released was reduced. It was molded in the same manner as in Example 1, and had a length of 12.0 mm, a width of 1.5 mm, and a thickness of 0.3 mm. The heated aroma-emitting substrate assembly 321 is wrapped in a paper heated aroma-emitting substrate wrapping material. A heated aroma source 320 wrapped around a material 322 is manufactured, and one heated aroma source 320 The heated aroma generating source 320 includes 0.29 g of the heated aroma generating substrate 321 per unit area. The volumetric packing ratio of the heated aroma-generating substrate assembly 321 to the volume was 0.60. As in Examples 1 to 4 and Comparative Example 1, the heated aroma-generating substrate 3211 (FIG. 3) is an aroma source material. 60 parts by mass of aerosol former, methyl cellulose as a first binder, and The CMC was 15 parts by mass and 4 parts by mass, respectively, and the second binder, glucomannan, was 0. Contains .9 parts by mass.
[0104] In the above Examples 1 to 5 and Comparative Examples 1 and 2, the heater The blade-type heat source was molded for evaluation using ICOS (registered trademark) However, depending on the heat source, the heating method, the maximum temperature reached, and the heated aroma source and heated The composition of the fragrance cartridges is different, which may affect the evaluation results. Therefore, although it is the same heated smoking device, it uses an omnidirectional heat source, Glow (registered trademark), which uses electromagnetic induction heating. In Examples 6 to 10 and Comparative Examples 3 and 4, the aroma generated by heating was evaluated. The composition of the substrate and the manufacturing method thereof are described in Examples 1 to 5 and Comparative Example 1 and 2, but has been molded into a heated aroma source compatible with Glo (registered trademark) . Example 6
[0105] The heated aroma-emitting sheet substrate having a thickness of 0.3 mm was prepared in the same manner as in Example 1. In the forming process in step 2, the material is cut into a rectangle measuring 150 mm in length and 210 mm in width, and then passed through a rotary Using a cutter, it is cut into a shape of 210 mm in length, 1.5 mm in width, and 0.3 mm in thickness. A long prismatic heated aroma-generating substrate was produced.
[0106] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After being manufactured, it was cut to a length of 42.0 mm to manufacture the heated aroma source 420. As a result, 31 heated pieces measuring 42.0 mm in length, 1.5 mm in width, and 0.3 mm in thickness were released. The substrate assembly 421 is wrapped around a heated aroma-generating substrate wrapping member 422 made of paper. The aroma source 420 is heated with 0.63 g of aroma generating group per heated aroma source 420. The volume of the heated aroma emitting source 420 includes a volume of the heated aroma emitting substrate 421. The volumetric filling factor of the body 421 was 0.59. The composition of the heated aroma-generating base material did not change. For 100 parts by mass of the fragrance source material, 60 parts by mass of the aerosol former and 1st binder are Methylcellulose and CMC were 15 parts by weight and 4 parts by weight, respectively, as the second binder. It contains 0.9 parts by mass of glucomannan.
[0107] Here, the heated aroma emitting substrate wrapping material for wrapping the heated aroma emitting substrate assembly 421 is 422 does not have to be paper, but it should be of a strength equivalent to that of paper with a basis weight of 30g / m2 to 40g / m2. Plastic film can be used. However, the omnidirectional heat source by electromagnetic induction heating is In the case of the heated aroma cartridge, unlike the blade-type heat source using a heater, The source 420 and the heated aroma cartridge exterior member 410 are heated to about 240° C. In order to prevent this, plastic films, engineering plastic films, biodegradable plastics Stick film cannot be used as a substitute for paper. In this case, heat When using plastic as a fragrance-generating substrate wrapping material, it is heated to about 300°C until it turns into glass. Heat resistance equivalent to that of the cellulose fibers (which make up the paper) at which migration or thermal decomposition begins, i.e. A film of special engineering plastic with a glass transition temperature of 240℃ or higher is applied. Such special engineering plastics include, for example, polyamide isomers. Examples of the polymerizable compound include polyamide, polyarylate, polyimide, polytriazine, and liquid crystal polymer. Cut. Example 7
[0108] Example 7 also confirms the effect of curing in order to concretely show the effect of curing in comparison with Example 6. The heated aroma-emitting sheet substrate having a thickness of 0.3 mm was prepared in the same manner as in Example 2. In the molding process of 2, the product was cut in exactly the same manner as in Example 6, and then heated aroma source 4 was added in exactly the same manner. 20 were manufactured. The result was a length of 42.0 mm, width of 1.5 mm, and thickness of 0.3 mm. The 31 heated aroma-emitting substrate aggregates 421 are wrapped around a paper heated aroma-emitting substrate wrapping member 4 The heated aroma source 420 wrapped around the 22 is 0.6 3 g of the heated aroma generating substrate assembly 421, and the volume of the heated aroma generating source 420 The volumetric packing ratio of the heated aroma-emitting substrate assembly 421 was 0.59. It has the same composition as the heated aroma-generating substrate. <Comparative Example 3>
[0109] Comparative Example 3 was also conducted to specifically demonstrate the effect of adding the first binder and the second binder in two separate steps. A 0.3 mm thick sheet was manufactured in exactly the same manner as in Comparative Example 1 to confirm the effect of two-stage divided addition. The heated aroma-emitting substrate in the form of a sheet was cut in the same manner as in Example 6 in the second molding step. After that, the heated aroma source 420 was produced in exactly the same manner. The heated aroma-emitting substrate assembly 421 is made of paper and has a diameter of 0.5 mm and a thickness of 0.3 mm. The heated aroma source 420 wrapped around the thermal aroma generating substrate wrapping member 422 is Each aroma generating source 420 contains 0.63 g of heated aroma generating substrate aggregate 421. The volumetric filling ratio of the heated aroma-emitting substrate assembly 421 to the volume of the aroma-emitting source 420 is 0.5 The composition was the same as that of the heated aroma-generating substrate of Example 6. Example 8
[0110] In Example 8, compared with Example 7, the effect of the cross-sectional shape perpendicular to the longitudinal direction of the heated aroma-generating substrate was also examined. In order to confirm the effect of the cross-sectional shape perpendicular to the longitudinal direction of the heated aroma-emitting substrate, A sheet-shaped heated aroma generating base having a thickness of 0.1 mm was prepared in the same manner as in Example 3. In the second forming process, the material is cut into a rectangle measuring 150 mm in length and 210 mm in width. Using a rotary cutter, cut into a shape with a length of 210 mm, width of 1.0 mm, and thickness of 0.1 mm. The aroma-generating substrate was cut into a long rectangular column shape to be heated. The 42 pieces are aligned lengthwise, wrapped in paper with a basis weight of 34g / m2, and then glued. By this process, a cylindrical roll with an outer diameter of 5.5 mm was produced, and then cut into a length of 42.0 m. The heated aroma source 420 was manufactured by cutting the heated aroma source 420 into pieces each having a length of 42.0 mm and a width of 42.0 mm. The heated aroma-emitting substrate assembly 421 is made of paper and has a diameter of 1.0 mm and a thickness of 0.1 mm. The heated aroma source 420 wrapped around the heated aroma-emitting substrate wrapping member 422 is Each of the thermal aroma generating sources 420 contains 0.64 g of the heated aroma generating substrate assembly 421. The volumetric filling rate of the heated aroma-emitting substrate assembly 421 relative to the volume of the heated aroma-emitting source 420 is 0. The composition was the same as that of the heated aroma-generating substrate of Example 6. Example 9
[0111] In Example 9, compared with Example 7, the effect of the cross-sectional shape perpendicular to the longitudinal direction of the heated aroma-generating substrate was also examined. In order to confirm the effect of the cross-sectional shape perpendicular to the longitudinal direction of the heated aroma-emitting substrate, A sheet-shaped heated aroma generating base having a thickness of 0.5 mm was prepared in the same manner as in Example 4. In the second forming process, the material is cut into a rectangle measuring 150 mm in length and 210 mm in width. Using a rotary cutter, cut into a shape with a length of 210 mm, width of 2.0 mm, and thickness of 0.5 mm. Cutting was performed to produce long prismatic heated aroma generating substrates.
[0112] The heated aroma-generating substrate is made of 14 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. 142 heated aroma-emitting substrates, each 42.0 mm long, 2.0 mm wide, and 0.5 mm thick The assembly 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The source 420 is a heated aroma generating material collection of 0.63 g per heated aroma generating source 420. The volume of the heated aroma generating substrate assembly 420 including the combination 421 is The volume filling rate of 21 was 0.59. The composition was the same as that of the heated aroma-generating substrate of Example 6. It is a completion. <Comparative Example 4>
[0113] Since the composition is the same as that of Comparative Example 2, which confirms the effect of the second binder, the results shown in Comparative Example 2 were obtained. In order to confirm the effect of the heat source by performing a smoking test, Heated aroma sources of the same size as those in Example 7 and Comparative Example 3 were manufactured. Example 10
[0114] Example 10 also aims to confirm the influence of curing. Confirm that the aroma-generating sheet of 0.3 mm thick heated product was manufactured in exactly the same manner as in Example 5. In the second molding step, the substrate was cut in exactly the same manner as in Example 6, and then subjected to the same processing. A thermal aroma source was produced. The result was a tube measuring 42.0 mm in length, 1.5 mm in width, and 0.3 mm in thickness. The 31 heated aroma-emitting substrates 421 are wrapped in a paper heated aroma-emitting substrate wrapping material. The heated aroma source 420 wrapped around the material 422 is 0 0.64g of heated aroma-emitting substrate assembly 421, and the volume of heated aroma-emitting source 420 The volumetric filling rate of the heated aroma-emitting substrate assembly 421 was 0.60. It has the same composition as the heated aroma-generating substrate of 5.
[0115] In order to specifically show the effects of the type of binder and the method of addition, Examples 1 to 10 and In the comparative examples 1 to 4, the heated aroma sources were manufactured, and further, the mixtures of different types of binders were used. When we tried to examine the order of mixing, we found that in the first mixing, similar to that in Example 1, The first binder, which is a cellulose polysaccharide, is replaced with a second binder, which is a polysaccharide other than a cellulose polysaccharide. When the agent was replaced, a gelled mass was formed, and in the subsequent process Since the aromatic substance remained even after heating, it was not possible to produce a uniform aromatic substance when heated. The description has been omitted.
[0116] Using the heated aroma sources of Examples 1 to 10 and Comparative Examples 1 to 4, the first binder and To concretely demonstrate the effect of the stepwise addition of the second binder, and the effect and impact of curing. The following evaluations 1 to 3 were carried out. [Rating 1-1]
[0117] In order to evaluate the heated aroma sources of Examples 1 to 5 and Comparative Examples 1 and 2, the following was performed. The heated smoking area is equipped with a blade-type heat source 130 made by Philip Morris. The smoking device used was the IQOS (registered trademark) 100. The smoking device 100 has a heat source 130, A blade type heater with a width of 4.5 mm, a length of 12 mm to the tip, and a thickness of 0.4 mm. A heat source 130 is provided on the opposite side of the body 110 from the chamber (not shown). The power supplied from the battery generates heat, reaching approximately 300 to 350°C. The heated aroma cartridge 300 has a chamber with an inner diameter of 7.0 mm provided in the body 110. After being attached to the inner surface of the body 110 along the line 120, the control system The stem allows one heated aroma cartridge 300 to be smoked with 14 puffs. In addition, when the heated aroma cartridge 300 of this embodiment and this comparative example was inserted, The length of the part protruding outward from the hole 110 is about 20 mm.
[0118] On the other hand, the heated aroma cartridge 300 to be attached to the smoking article is, as shown in FIG. The heated aroma generating source 320, the support member 331, and the filter member 333 are placed in a heated aroma chamber. The cartridge is wrapped with an exterior member 310, and the mouthpiece is wrapped with a mouthpiece reinforcing member 3301. More specifically, the structures of Examples 1 to 5 and Comparative Examples 1 and 2 were The heated aroma source 320 is a cylinder with a length of 12 mm, an outer diameter of 6.9 mm, and an inner diameter of 4 mm. A support member 331 is a hollow tube having a length of 8 mm and an outer diameter of 6.9 mm and having a through hole. A cellulose acetate fiber sheet formed into a cylindrical shape with a length of 23 mm and an outer diameter of 6.9 mm. The filter members 333 are attached in this order in the longitudinal direction, and the inner surfaces of the filter members 333 are aligned in predetermined positions. The heated fragrance cartridge outer packaging is made of paper with a basis weight of 38 g / m2 and a certain amount of adhesive applied. The member 310 is wound so that the outer diameter is slightly less than 7.0 mm, and the mouthpiece 330 is wound around the The inner surface of the paper is coated with adhesive and has a basis weight of 40 g / m2 so that it overlaps with the filter member 333. The heated aroma cartridge exterior member 310 in this case has a basis weight of 32g / m2~45g / m2 paper or plastic film with equivalent strength It is preferable to use a material that maintains the minimum necessary strength, but for the part that is held in the lips, To prevent damage caused by saliva penetration, it is preferable to reinforce the paper with a basis weight of 40 g / m2 or more. The heated aroma cartridge exterior member 310 does not come into contact with the heat source 130. Plastic films can be used according to the strength of each paper. The mouthpiece film does not allow saliva to penetrate and does not require a mouthpiece reinforcing member 3301. It is particularly preferable to use a biodegradable plastic film from the viewpoint of environmental protection. However, in the case of a plastic film, the thickness of the film should be selected according to the material. It is necessary to do so.
[0119] In the case of the blade-type heat source 240, a drop test of the heated aroma-emitting substrate 3211 (FIG. 3) was carried out. The effects of the binder and curing were confirmed. This was done by using a blade-type heat source 130 as shown in FIG. In this case, the aroma-emitting substrate assembly 321 is heated by contacting the blade-type heat source 240. Therefore, the heated aroma-generating substrate 3211 (Fig. 3) tends to shrink and fall off after smoking. The aroma generating substrate assembly 321 to be heated during smoking has a blade-type heat source 130 and This is based on the tendency of the material to contaminate the chamber inner wall 120. , and the heated aroma car equipped with the heated aroma generating source 320 manufactured in Comparative Examples 1 and 2. The cartridge 300 is attached to a heated smoking device 100 having a blade-type heat source 130, and a smoking After this, the heated aroma cartridge 300 is removed, and the heated aroma source 320 is By pointing it directly downward, it is possible to check whether the heated aroma-emitting substrate 3211 (Figure 3) falls or not. It was held.
[0120] The criteria for this evaluation are as follows: Rank A: The heated aroma-generating substrate does not fall off, and the blade-type heat source and the inner wall of the chamber are not soiled. Dye few Rank B: Part of the heated aroma-generating substrate fell off and hit the blade-type heat source and the inner wall of the chamber. pollution is noticeable [Rating 1-2]
[0121] In order to evaluate the heated aroma sources of Examples 6 to 10 and Comparative Examples 3 and 4, As shown in Figure 2, the British The smoking device 200 used was a Glo (registered trademark) 200 manufactured by American Tobacco Co. An omnidirectional heat source 24 using electromagnetic induction heating is provided along the inner surface 220 of the chamber of the oven 210. The heated aroma cartridge 400 is attached to the heat source 240. The area around the scent source 420 is heated. It heats up with electricity and reaches a temperature of about 240-280°C in about 3-4 minutes of smoking time. The heated aroma cartridge 400 has an air hole 230 at the bottom, no lid, and an inner diameter of 5. After being attached to a heat source 240 having a cylindrical shape of 6 mm, the heat source control unit 250 heated the heat source. The aerosol former evaporates from the heated aroma source 420 surrounded by the heat source 240 and is inhaled. Then, the air flowing in from the ventilation hole 230 cools the aerosol former, generating smoke and causing smoking. You can smoke.
[0122] On the other hand, the heated aroma cartridge 400 to be attached to the smoking article is, as shown in FIG. A heating aroma generating source 420, a cooling member 432, a filter member 433, and a hollow tube 434 The mouthpiece 430 is wrapped in the heated aroma cartridge exterior member 410. More specifically, the long fibers produced in Examples 6 to 10 and Comparative Examples 3 and 4 were Heated aroma source 420, 42 mm in diameter, 5.5 mm in outer diameter, 25 mm in length, 0.5 mm in thickness The cooling member 432 is a cylinder made of cardboard rolled up to an outer diameter of 5.5 mm, with a length of 8 mm and an outer diameter of 5. Filter material 433 made of cellulose acetate fiber molded into a 5 mm cylindrical shape , and a cardboard 8 mm long and 0.5 mm thick rolled up into a cylindrical shape with an outer diameter of 5.5 mm. The hollow tubes 434 are attached in this order in the longitudinal direction, and a predetermined amount of adhesive is applied to the predetermined positions on the inner surface. The heated fragrance cartridge is a paper cartridge with a length of 20 mm, a width of 83 mm and a basis weight of 38 g / m2. The wire was wrapped with a wire-rimmed outer casing 410 so that the outer diameter was just under 5.6 mm.
[0123] In the case of the omnidirectional heat source 240, a test is performed to insert the heated aroma cartridge 400 and to determine whether it is connected properly. As shown in Figure 2, the effect of the agent and curing was confirmed. In the case of 0, the elongated heated aroma cartridge 400 is inserted into the elongated cylindrical can. Therefore, it is difficult to attach the heated aroma cartridge 400. The evaluation is based on the fact that the heating and Five subjects were asked about the comfort of fitting the heated aroma cartridge 400 to the smoking device 400. was carried out by.
[0124] The criteria for this evaluation are as follows: Rank A: No problem with installing the heated aromatic cartridge Rank B: It is difficult to install the heated aroma cartridge, and in some cases, it may break. [Rating 2-1]
[0125] In the smoking conducted in [Evaluation 1-1], a sensory test was conducted by five subjects, and the combination The sensory evaluation was conducted with a focus on the delicate aroma of tea. It was said.
[0126] The criteria for this evaluation are as follows: Rank A: The level at which you can enjoy the aroma of tea when smoking. Rank B: The tea aroma is unsatisfactory when smoking. [Rating 2-2]
[0127] In the case of the omnidirectional heat source 240, as in the case of the blade heat source 130, the state shown in FIG. Five subjects smoked and conducted a sensory test to confirm the effectiveness of the binder and curing. Again, the sensory test focused on the delicate aromas of the teas.
[0128] The criteria for this evaluation are as follows: Rank A: The level at which you can enjoy the aroma of tea when smoking. Rank B: The tea aroma is unsatisfactory when smoking. [Rating 3]
[0129] The effects of the binder and curing were evaluated in evaluations 1 and 2 by drop tests of the heated aroma-generating substrate, and These effects were confirmed by inserting heated aroma cartridges and by smoking tests. The power of the heated aroma-generating sheet-shaped substrates produced in Examples 1 to 10 and Comparative Examples 1 to 4 We found that there was a correlation between the chemical composition and the biological strength.
[0130] In practice, Examples 1, 2, 5, 6, 7, and 10 were manufactured to a thickness of 0.3 mm. The sheet-shaped heated aroma-generating substrates of Comparative Examples 1 to 4 were used, and the heated aroma-generating substrates were placed in a 10.0 cm wide x 22.0 cm long box. A general tensile strength test is performed using test pieces cut to 1.0 mm in length, and the measured breaking strength is evaluated. The tensile strength test was performed with the test piece clamped at a distance of 20.0 cm in the vertical direction. The test was carried out in a temperature environment of ℃ and 50% RH. The breaking strength was measured when the test piece started to break. was defined as the intensity of
[0131] The compositions of Examples 1 to 10 and Comparative Examples 1 to 4 used in Evaluations 1 to 3, as well as Participant [Table 1-1] The shape and number of heated aroma-emitting substrates used in the thermal aroma source are shown in Table 1-1. The production conditions for the raw substrate composition and the results of evaluations 1 to 3 are shown in Table 1-2. [Table 1-2]
[0132] The method of adding the binder is compared between Example 1 and Comparative Example 1, and between Example 6 and Comparative Example 3. It was confirmed that it is preferable to add the first and second binders in stages. In Example 1 and Comparative Example 1, the first binder and the second binder were added in two stages, The latter is a heated aroma-generating base material manufactured under exactly the same conditions, except that it is added all at once. A drop test and a smoking test were performed using a heated smoking device 100 equipped with a blade-type heat source 130. In addition, the former obtained better results. 1 and Comparative Example 1, and a heated smoking device 200 equipped with an omnidirectional heat source 240. In the insert and smoking tests used, compositions prepared by two-stage addition of binder Better results have been obtained with heated aroma-generating substrates made from
[0133] The reason for this is unclear, but it is thought that the first binder of the cellulose polysaccharide is the aromatic source material and aerobic Promote uniform mixing and dispersion of the sol former to form a stable sol state, and then add the cellulosic acid to the sol. The second binder, a polysaccharide other than the sugar-based polysaccharide, forms a gel state that enhances the bonds between the two. In order to achieve this, the fine dispersion enhances the evaporation of the aromatic components of tea when heated, and the cohesiveness is increased. It is believed that this reduces the shrinkage caused by the heating and improves the mechanical strength of the aroma-generating substrate. This hypothesis is based on the fact that when the first binder and the second binder are mixed in an interchangeable manner, the fragrance source material, enamel, A partially gelled mass is formed in the mixture of the aerosol former and the binder, and the mixture is uniformly dispersed. This is supported by the phenomenon of being unable to generate states.
[0134] The effect of curing was compared between Example 1 and Examples 2 to 4, and Example 5 and Comparative Example 1, with and without curing. For Example 6, Examples 7 to 9, and Example 10 and Comparative Example 3, the evaluations were 1-1 and 1 The results of -2, Evaluation 2-1, and Evaluation 2-2 are clear. As with the addition of Example 5, the quality of the aroma-generating substrate when heated can be greatly improved. As can be seen from a comparison of the evaluation results of Comparative Example 1, Example 10, and Comparative Example 3, the curing process In this case, it is not necessary to add the first and second binders step by step, and the curing effect is improved. It is thought to be quite large.
[0135] The cause of this curing effect is unclear, but it is thought that the cellulose-based first binder acts as a fragrance source material and Aromatic source material in a sol state formed by promoting uniform mixing and dispersion of the aerosol former This is presumably due to the fact that the degree of dispersion of the granules is increased and stabilized. It was found that the volume increase of the mixture during curing depends on the temperature and time of curing. As a result, the aroma of the aroma-generating substrate produced by the curing process was The denser dispersion structure of the aromatic ingredients enhances the volatilization of the aromatic components of tea when heated, and the aromatic components of the tea are retained in the heated tea. The shrinkage of the fragrance-generating base material caused by heating has been reduced, and its mechanical strength has been improved. It is possible.
[0136] In addition, the evaluation results of Comparative Examples 2 and 4, in which glucomannan was not added, showed that the second binder The polysaccharides other than the cellulose polysaccharides used as the oxidizing agent were added in small amounts, but they had a significant effect on the aromatic properties of the heated food. It is considered essential to improve the quality of the generating substrate. The addition of a large amount of polysaccharide, which is a binder, destroys the dispersion system of the composition of the heated aroma-generating base material, It tends to gel, so it is recommended to use it in conjunction with the cellulosic polysaccharides used as the first binder. It is necessary to improve the dispersibility and cohesiveness of the heated aroma-generating base material by this.
[0137] Furthermore, to support the causal relationship of such drop tests, insertion tests, and smoking tests, These evaluation results were obtained for the sheet-shaped applied heat exchangers manufactured in Examples 1 to 10 and Comparative Examples 1 to 4. It was found that there was a good correlation with the breaking strength of the thermal aroma-emitting substrate. The results are shown in Table 1-2. The tensile test series shown in Examples 1, 2, 5, 6, 7, and 10 and Comparative Examples 1 and 2. When comparing this evaluation 3 with the evaluation results 1-1, 1-2, 2-1, and 2-2, The breaking strength of the heated aroma-emitting sheet-shaped substrate produced by two-step addition of binder and curing The degree is high, and the cross-sectional area of the test piece (0.3 × 100 mm 2 ) at least 5N or more, i.e. 0.167N / mm 2 The heated aroma cartridge has a breaking strength of the above. The mechanical strength required for the above, low heat shrinkage after smoking, and aroma due to heating during smoking are required. It is believed that this is an index for expressing the volatility of the components. The effects of stepwise addition of binder and curing are not inconsistent with, but rather correlate with, the effect of curing.
[0138] Secondly, the crosslinked PVP can sorb the cooling agent in a simple process, and the aroma generated by heating is reduced. A heated aroma source is provided that suppresses the dissipation of a freshening agent from a base material over time and contains the same. Even after storing the aroma cartridge for a long period of time, it will not be heated when you attach it to a heated smoking device and smoke it. In order to concretely demonstrate the effect of being able to fully enjoy the aroma of the aroma-generating material, Examples 11 to 18 and Comparative Examples 5 to 12 in which menthol and xylitol were used as the stimulants An experiment was conducted.
[0139] As a method for producing the aroma-generating substrate to be heated according to the present invention, as shown in FIG. 12, a first binder and A first mixing step in which the first binder is added while the second binder is added stepwise, and a second mixing step in which the first binder is added stepwise. It is best to provide a curing step between the first mixing step and the second mixing step in which the binder is added. In the following examples and comparative examples, the focus is on verifying the effect of crosslinked PVP, and the experiments are simplified. In order to achieve this, the first binder and the second binder are added at once, the curing step is omitted, and Only menthol was used as a cooling agent. The process diagram in Figure 11, which does not include the curing process, is shown in Figure 12. A manufacturing process was adopted that introduced a fourth mixing step. Example 11
[0140] The fourth mixing step, in which the lower alcohol in which the cooling agent is dissolved and the crosslinked PVP are mixed, is as follows: And so he went. Menthol 100 parts by weight Ethyl alcohol 200 parts by weight Cross-linked polyvinylpyrrolidone (PVP) 200 parts by weight Weigh out the menthol, dissolve it in ethyl alcohol, and prepare a menthol / ethyl alcohol solution. After preparing the solution, add the cross-linked PVP to the menthol / ethyl alcohol solution and mix with stirring. A menthol / ethyl alcohol / crosslinked PVP mixture was prepared in which the crosslinked PVP was swollen.
[0141] On the other hand, xylitol is added to the third mixing process, so the following mixing ratio of xylitol / An aqueous solution was prepared. Xylitol 100 parts by weight 400 parts by mass of water
[0142] The fragrance source material is black tea leaves, which are dried at 70℃ so that the moisture content is about 2%, The mixture was crushed and passed through a 80 mesh sieve, and mixed in the third mixing step in the following ratio: The mixture was then placed in a wet mixer and processed for 15 minutes to produce a heated aroma-generating base material composition. 100 parts by weight of dried and ground black tea leaves Menthol / ethyl alcohol / crosslinked PVP mixture 25 parts by weight Glycerin 30 parts by weight Propylene glycol 30 parts by weight Sodium carboxymethylcellulose (CMC) 4 parts by weight Methylcellulose 15 parts by weight Glucomannan 1 part by weight Xylitol / water solution 8 parts by weight
[0143] The composition produced in the third mixing step is fed into a three-roll mill in the first molding step. The material was compressed between the narrow rolls and sheared by the difference in roll speed. The ingredients were mixed and dispersed together to produce a sheet-shaped heated aroma-emitting substrate having a predetermined thickness. In the first molding process, the composition becomes a highly viscous paste, so the sheet is carefully cooled by adding pure water while observing its condition. While adding an appropriate amount of water, the doctor blade is pressed against the roll to form the mixture into a sheet. In this molding process, the moisture evaporates moderately, and the heated aromatic sheet with a thickness of 0.3 mm is formed. A three-roll machine with the roll interval and roll speed ratio adjusted to form the fragrance-generating base material. The mill was repeated eight times.
[0144] The sheet-shaped heated aroma-emitting substrate produced in the first molding step is put into the second molding step. First, it was cut into a rectangle measuring 150 mm in length and 240 mm in width. The cut sheet is cut into a length of 240 mm, width of 1.5 mm, and thickness of 0.0 mm using a rotary cutter. The material was cut to 0.3mm to produce long rectangular prismatic heated aroma-emitting substrates.
[0145] The 50 long rectangular pillar-shaped heated aroma-emitting substrates thus produced were aligned in the longitudinal direction. Then, a paper with a basis weight of 34 g / m2 was used as the heated aroma generating substrate wrapping member 322. After being rolled and glued, a cylindrical roll with an outer diameter of 6.9 mm is produced. The heated aroma source 320 was manufactured by cutting the heated aroma source 320 into a length of 12.0 mm. A collection of 50 heated aroma-emitting substrates, each measuring 12.0 mm in diameter, 1.5 mm in width, and 0.3 mm in thickness. 321 is a heated aroma source wrapped around a heated aroma-emitting substrate wrapping member 322 made of paper 320 is a heated aroma generating substrate assembly 3 of 0.29 g per heated aroma generating source 320 21, and the volume of the heated aroma-emitting substrate assembly 321 relative to the volume of the heated aroma-emitting source 320 The volume filling rate was 0.60. In addition, the aroma-generating substrate 3211 (FIG. 3) was For 100 parts by mass of the source material, 60 parts by mass of the aerosol former and methyl The second binder, 15 parts by weight of cellulose and 4 parts by weight of CMC, 1 part by mass of alcomannan, 10 parts by mass of crosslinked PVP, 5 parts by mass of menthol, and xylitol. It contains 1.6 parts by mass of ritol.
[0146] In Examples 11 to 15 and Comparative Examples 5 to 8, the outer diameter and length of the The heating aroma source is a product that emits a pulsating heat generated by a heater during the smoking test described below. The IQOS (registered trademark, manufactured by Philip Morris) equipped with a card-type heat source was used as a heated smoking device. This is for use. Example 12
[0147] A heated aroma-emitting base composition was prepared in exactly the same manner as in Example 11. To confirm the effect of the shape, i.e., specific surface area, of the heated aroma-generating substrate on torr dissipation. Therefore, in the first molding step, the position of the doctor blade, the roll interval, and the roll The three-roll mill, the speed ratio of which was adjusted differently from that of Example 11, was repeated eight times to obtain the thickness. It was molded into a sheet-like heated aroma-emitting substrate having a thickness of 0.1 mm, which is thinner than that of Example 11.
[0148] The sheet-shaped heated aroma-emitting substrate produced in the first molding step is put into the second molding step. First, it was cut into a rectangle measuring 150 mm in length and 240 mm in width. The sheet was cut into a length of 240 mm using a rotary cutter, narrower than that of Example 11. The heated aroma-emitting substrate is manufactured in a long rectangular column shape with a diameter of 1.0 mm, width of 1.0 mm and thickness of 0.1 mm. It was done.
[0149] The 225 long rectangular pillar-shaped heated aroma-emitting substrates thus produced were aligned in the longitudinal direction. Then, a paper with a basis weight of 34 g / m2 was used as the heated aroma generating substrate wrapping member 322. The roll is then rolled and glued to produce a cylindrical roll with an outer diameter of 6.9 mm. Then, the heated aroma source 320 was manufactured by cutting the heated aroma source 320 into a length of 12.0 mm. A collection of 225 heated aroma-emitting substrates, each 12.0 mm long, 1.0 mm wide, and 0.1 mm thick. The combination 321 is wrapped around a heated aroma generating substrate wrapping member 322 made of paper. The raw source 320 is a heated aroma-emitting substrate aggregate of 0.29 g per heated aroma-emitting source 320. The heated aroma-emitting substrate assembly 32 includes a body 321, and the heated aroma-emitting source 320 has a volume of The volume filling factor of 1 was 0.60. Example 13
[0150] A heated aroma-emitting base composition was prepared in exactly the same manner as in Example 11. To confirm the effect of the shape, i.e., specific surface area, of the heated aroma-generating substrate on torr dissipation. Therefore, in the first molding step, the position of the doctor blade, the roll interval, and the roll The three-roll mill, the speed ratio of which was adjusted differently from that of Example 11, was repeated eight times to obtain the thickness. A sheet-like heated aroma-generating substrate having a thickness of 0.5 mm, which is thicker than that of Example 11, was formed.
[0151] The sheet-shaped heated aroma-emitting substrate produced in the first molding step is put into the second molding step. First, it was cut into a rectangle measuring 150 mm in length and 240 mm in width. The sheet was cut into a length of 240 mm using a rotary cutter, which was wider than that of Example 11. The heated aroma-emitting substrate is manufactured in a long rectangular column shape with a diameter of 2.0 mm, width of 2.0 mm and thickness of 0.5 mm. It was done.
[0152] The 23 long rectangular pillar-shaped heated aroma-emitting substrates thus produced were aligned in the longitudinal direction. Then, a paper with a basis weight of 34 g / m2 was used as the heated aroma generating substrate wrapping member 322. After being rolled and glued, a cylindrical roll with an outer diameter of 6.9 mm is produced. The heated aroma source 320 was manufactured by cutting the heated aroma source 320 into a length of 12.0 mm. A collection of 23 heated aroma-emitting substrates, each measuring 12.0 mm in diameter, 2.0 mm in width, and 0.5 mm in thickness. 321 is a heated aroma source wrapped around a heated aroma-emitting substrate wrapping member 322 made of paper 320 is a heated aroma generating substrate assembly 3 of 0.29 g per heated aroma generating source 320 21, and the volume of the heated aroma-emitting substrate assembly 321 relative to the volume of the heated aroma-emitting source 320 The volume filling factor was 0.60. <Comparative Example 5>
[0153] In order to clarify the effect of crosslinked PVP, the aromatic group generated by heating was measured without using crosslinked PVP. The material was manufactured.
[0154] In the fourth mixing step, menthol is dissolved in ethyl alcohol in the following mixing ratio, and the menthol is mixed with ethyl alcohol. A methanol / ethyl alcohol solution was prepared. Menthol 100 parts by weight Ethyl alcohol 400 parts by weight
[0155] On the other hand, xylitol is added to the third mixing process, so the following mixing ratio of xylitol / An aqueous solution was prepared. Xylitol 100 parts by weight 400 parts by mass of water
[0156] The fragrance source material was treated in the same manner as in Example 11, and mixed in the following ratio in the third mixing step: The mixture was then placed in a wet mixer and processed for 15 minutes to produce a heated aroma-generating base material composition. 100 parts by weight of dried and ground black tea leaves Menthol / ethyl alcohol solution 25 parts by weight Glycerin 30 parts by weight Propylene glycol 30 parts by weight Methylcellulose 15 parts by weight Sodium carboxymethylcellulose (CMC) 4 parts by weight Glucomannan 1 part by weight Xylitol / water solution 8 parts by weight
[0157] The composition of the heated aroma-generating base material produced in the third mixing step was mixed with the first mixture in the same manner as in Example 12. After the first and second molding processes, the final product is 12.0 mm long, 1.0 mm wide, and 1.0 mm thick. The heated aroma-emitting substrate assembly 321 is made of paper and has a thickness of 0.1 mm. A heated aroma source 320 having an outer diameter of 6.9 mm was manufactured and wrapped around a substrate wrapping member 322. Each heated aroma source 320 produces 0.29g of heated aroma. The volume of the heated aroma-emitting source 320 includes a substrate assembly 321. The volumetric filling rate of the combined body 321 was 0.60. In addition, the heated aroma-generating base material 3211 (FIG. 3 ) does not contain cross-linked PVP and is aerosol-based for 100 parts by mass of fragrance source material. The first binder, methyl cellulose, and CMC, were each 15 parts by mass. parts by weight and 4 parts by weight of the second binder, 1 part by weight of glucomannan, and 5 parts by weight of menthol. It contains 1.6 parts by mass of xylitol. <Comparative Example 6>
[0158] As in Comparative Example 5, in order to clarify the effect of crosslinked PVP, uncrosslinked water-soluble Using the hydrophilic PVP, a heated aroma source 320 was produced in the same manner as in Example 12. Fruit, 225 pieces of heated aromatic fruit, each 12.0 mm long, 1.0 mm wide, and 0.1 mm thick. The substrate assembly 321 is wrapped around a heated aroma-generating substrate wrapping member 322 made of paper. The aroma generating source 320 was manufactured. And, 0.2 9 g of the heated aroma generating substrate assembly 321, The volumetric filling rate of the heated aroma-emitting substrate assembly 321 was 0.60. The raw base material 3211 (Figure 3) does not contain cross-linked PVP and has a The aerosol former is 60 parts by mass, the first binder is methylcellulose and CM C is 15 parts by mass and 4 parts by mass, respectively, and glucomannan as the second binder is 1 part by mass. parts by weight, 10 parts by weight of PVP, 5 parts by weight of menthol, and 1.6 parts by weight of xylitol Included. <Comparative Example 7>
[0159] In Comparative Example 7, the timing of contacting the crosslinked PVP with the menthol was As an example showing the effect of menthol / ethyl alcohol / crosslinked PV Effect of the mixing order in the fourth mixing step of producing the P mixture on the quality of the heated aroma-generating substrate The purpose of this study was to demonstrate the effect of dissolving the cellulose in ethyl alcohol as in Example 11. The menthol / ethyl alcohol mixture was mixed with the crosslinked PVP to obtain a menthol / ethyl alcohol mixture with swollen crosslinked PVP. Instead of preparing a menthol / crosslinked PVP mixture, the menthol was swollen with ethyl alcohol. By mixing with the crosslinked PVP, the crosslinked PVP was swollen and the menthol / ethyl alcohol was A mixture of 1,2-diol / crosslinked PVP was prepared. The mixing ratio was the same as in Example 11.
[0160] Except for the order of mixing in this fourth step, the third mixing step and subsequent steps were performed in exactly the same manner as in Example 11. The heated aroma source 320 was manufactured. As a result, the length was 12.0 mm, the width was 1.5 mm, and the thickness was 1.5 mm. The heated aroma-emitting substrate assembly 321 is made of 50 pieces of paper with a diameter of 0.3 mm. The heated aroma source 320, which is wrapped around a wrapping member 322 and has an outer diameter of 6.9 mm, is Each of the thermal aroma generating sources 320 contains 0.29 g of the heated aroma generating substrate aggregate 321. The volumetric filling rate of the heated aroma-emitting substrate assembly 321 relative to the volume of the heated aroma-emitting source 320 is 0. The aroma source material was 100 mass .60. 60 parts by weight of aerosol former, methyl cellulose as a first binder, and and CMC were 15 parts by mass and 4 parts by mass, respectively, and glucomannan, which was the second binder, was 1 part by weight, 10 parts by weight of crosslinked PVP, 5 parts by weight of menthol, and 1 part by weight of xylitol. Contains .6 parts by mass. <Comparative Example 8>
[0161] In Comparative Example 8, similar to Comparative Example 7, the method of contacting crosslinked PVP with menthol was used to produce a heated aromatic compound. As an example showing the effect on the quality of the generated substrate, the cross-linked PV in the fourth mixing step Instead of adding P, we changed the mixing process to add crosslinked PVP in the third mixing step. A heated aroma-generating substrate composition was prepared in this manner.
[0162] In the fourth mixing step, menthol is dissolved in ethyl alcohol in the following mixing ratio to obtain a menthol mixture. A ethanol / ethyl alcohol solution was prepared. Menthol 100 parts by weight Ethyl alcohol 400 parts by weight
[0163] On the other hand, xylitol is added to the third mixing process, so the following mixing ratio of xylitol / An aqueous solution was prepared. Xylitol 100 parts by weight 400 parts by mass of water
[0164] In the third mixing step, the fragrance source material and the aerosol powder treated in the same manner as in Example 11 were mixed. Add the crosslinked PVP to the wet mixer together with the former and process for 15 minutes to prepare the heated aroma-generating base material. The composition was prepared. 100 parts by weight of dried and ground black tea leaves Menthol / ethyl alcohol solution 25 parts by weight Glycerin 30 parts by weight Propylene glycol 30 parts by weight Methylcellulose 15 parts by weight Sodium carboxymethylcellulose (CMC) 4 parts by weight Glucomannan 1 part by weight Crosslinked polyvinylpyrrolidone (PVP) 10 parts by weight Xylitol / water solution 8 parts by weight
[0165] After this third mixing step, the heated aroma source 320 was produced in exactly the same manner as in Example 11. As a result, 50 heated rods measuring 12.0 mm in length, 1.5 mm in width, and 0.3 mm in thickness were The aroma-emitting substrate assembly 321 is wrapped around a heated aroma-emitting substrate wrapping member 322 made of paper. , the heated aroma source 320 with an outer diameter of 6.9 mm is 0. The heated aroma generating source 320 includes a heated aroma generating substrate assembly 321 of 29 g. The volumetric filling rate of the aroma-generating substrate 321 to be heated was 0.60. Material 3211 (Figure 3) contains 60 parts by mass of aerosol former for every 100 parts by mass of fragrance source material. parts by weight, methyl cellulose and CMC as the first binder were 15 parts by weight and 4 parts by weight, respectively. parts by weight, 1 part by weight of glucomannan as the second binder, 10 parts by weight of cross-linked PVP, It contains 5 parts by mass of tallow and 1.6 parts by mass of xylitol.
[0166] In order to enjoy the refreshing sensation of the cooling agent and prevent its dissipation over time, the aroma-generating substrate that is heated must be The content of the cooling agent and crosslinked PVP, as well as the content of the crosslinked PVP relative to the cooling agent, are also important. It is necessary to cover all of these points, but a representative example is the When the content of cross-linked PVP is doubled, the content of menthol and cross-linked PVP is The results of the investigation are shown in Examples 14 and 15. The required content in the scent-generating base material is 1 to 10% by mass and 2 to 10% by mass, respectively; In addition, the content of the crosslinked PVP relative to the cooling agent is preferably 1 to 6 times. Many of the heated aroma cartridges with heated aroma generating sources are equipped with blade-type heat sources. The results were determined by sensory testing using heated smoking devices. Example 14
[0167] The menthol / ethyl alcohol / crosslinked PVP mixture to be mixed in the third mixing step is 10 mass The heated aroma source 320 was manufactured in the same manner as in Example 11, except that the heated aroma source 320 was used as the heating source 320. As a result, 50 pieces of specimens with a length of 12.0 mm, a width of 1.5 mm, and a thickness of 0.3 mm were The heat-emitting aroma-generating substrate assembly 321 is wrapped around a heat-emitting aroma-generating substrate wrapping member 322 made of paper. The heated aroma source 320 is heated with 0.29 g of aroma per heated aroma source 320. The aroma generating substrate assembly 321 is included, and the heated aroma generating material is heated relative to the volume of the heated aroma generating source 320. The volumetric packing ratio of the raw substrate assembly 321 was 0.60. In the example shown in FIG. 3, the aerosol former is 60 parts by mass per 100 parts by mass of the fragrance source material, and the third 1, the binders methylcellulose and CMC, were 15 parts by weight and 4 parts by weight, respectively; The second binder is 1 part by weight of glucomannan, 4 parts by weight of cross-linked PVP, and 2 parts by weight of menthol. It contains 1.6 parts by mass of xylitol. Example 15
[0168] The menthol / ethyl alcohol / crosslinked PVP mixture to be mixed in the third mixing step is 50 mass%. The heated aroma source 320 was manufactured in the same manner as in Example 11, except that the heated aroma source 320 was used as the heating source 320. As a result, 50 pieces of specimens with a length of 12.0 mm, a width of 1.5 mm, and a thickness of 0.3 mm were The heat-emitting aroma-generating substrate assembly 321 is wrapped around a heat-emitting aroma-generating substrate wrapping member 322 made of paper. The heated aroma source 320 is heated with 0.29 g of aroma per heated aroma source 320. The aroma generating substrate assembly 321 is included, and the heated aroma generating material is heated relative to the volume of the heated aroma generating source 320. The volumetric packing ratio of the raw substrate assembly 321 was 0.60. In the example shown in FIG. 3, the aerosol former is 60 parts by mass per 100 parts by mass of the fragrance source material, and the third 1, the binders methylcellulose and CMC, were 15 parts by weight and 4 parts by weight, respectively; The second binder is 1 part by weight of glucomannan, 20 parts by weight of cross-linked PVP, and menthol. It contains 10 parts by mass of glycerin and 1.6 parts by mass of xylitol.
[0169] In the above Examples 11 to 15 and Comparative Examples 5 to 8, the heater The blade-type heat source ICOS (registered trademark) was used for evaluation. However, the heating method, maximum temperature, and the aroma source and the heat source are different depending on the heat source. The composition of the thermal aroma cartridge is different, which may affect the evaluation results. Therefore, although it is the same heated smoking device, it uses an omnidirectional heat source glow (registered trademark) that uses electromagnetic induction heating. In Examples 16 to 18 and Comparative Examples 9 to 12, the heated aromatic The composition of the generating substrate and the cross-sectional shape perpendicular to the longitudinal direction are the same as those of Examples 11 to 1. 3 and Comparative Examples 5 to 8, but the heated aroma corresponds to Glo (registered trademark). The length and outer diameter of the source were formed. Example 16
[0170] In the same manner as in Example 11, a sheet-shaped heated material having a thickness of 0.3 mm was produced in the first molding step. In the second molding process, the aroma-emitting substrate is cut into a rectangle of 150 mm length and 210 mm width. After being cut by a rotary cutter, the sheet is cut into pieces 210 mm long, 1.5 mm wide, A shape of 0.3 mm thickness was cut to produce a long rectangular columnar heated aroma-emitting substrate.
[0171] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 31 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.3 mm thick. The combination 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The raw source 420 is a heated aroma-emitting substrate aggregate of 0.63 g per heated aroma-emitting source 420. The heated aroma-emitting substrate assembly 42 includes a body 421, and the heated aroma-emitting substrate assembly 42 includes a body 422. The volume filling factor of 1 was 0.59. Example 17
[0172] In the same manner as in Example 12, a 0.1 mm thick molded product was produced in the first molding process. The heated aroma-emitting sheet substrate is then molded into a sheet having a length of 150 mm and a width of 210 mm in the second molding process. After cutting into a rectangle of 210 mm using a cutter, a rotary cutter was used to cut the The heated aroma-emitting substrate is cut into a shape of 1.0 mm in width and 0.1 mm in thickness to produce a long rectangular columnar shape. It was created.
[0173] This heated aroma-generating substrate has 142 pieces aligned in the lengthwise direction and a basis weight of 34 g / m2. The paper is wrapped around the roll and glued to create a cylindrical scroll with an outer diameter of 5.5 mm. After being manufactured, it was cut into a length of 42.0 mm to produce a heated aroma source. 142 heated aroma emitters, each measuring 42.0 mm in length, 1.0 mm in width, and 0.1 mm in thickness. The aroma generating material assembly 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The aroma generating source 420 is a heated aroma generating base material of 0.64 g per heated aroma generating source 420. A heated aroma-emitting substrate assembly including the assembly 421 relative to the volume of the heated aroma-emitting source 420 The volume filling factor of 421 was 0.59. Example 18
[0174] In the same manner as in Example 13, a 0.5 mm thick molded product was produced in the first molding process. The heated aroma-emitting sheet substrate is then molded into a sheet having a length of 150 mm and a width of 210 mm in the second molding process. After cutting into a rectangle of 210 mm using a cutter, a rotary cutter was used to cut the The heated aroma-emitting substrate is cut into a shape of 2.0 mm in width and 0.5 mm in thickness to produce a long rectangular columnar shape. It was created.
[0175] The heated aroma-generating substrate is made of 14 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 14 heated aroma-emitting substrates, each 42.0 mm long, 2.0 mm wide, and 0.5 mm thick. The combination 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The raw source 420 is a heated aroma-emitting substrate aggregate of 0.63 g per heated aroma-emitting source 420. The heated aroma-emitting substrate assembly 42 includes a body 421, and the heated aroma-emitting substrate assembly 42 includes a body 422. The volume filling factor of 1 was 0.59. <Comparative Example 9>
[0176] In the same manner as in Comparative Example 5, a 0.1 mm thick sintered body was manufactured in the first molding step. In the second molding step, the sheet-shaped heated aroma-emitting substrate is molded into a size of 150 mm long and 210 mm wide. After cutting into a rectangle with a cutter, a rotary cutter is used to cut into a length of 210 mm and The product is cut into a shape with a width of 1.0 mm and a thickness of 0.1 mm to produce a long rectangular columnar heated aroma-emitting substrate. It was done.
[0177] This heated aroma-generating substrate has 142 pieces aligned in the lengthwise direction and a basis weight of 34 g / m2. The paper is wrapped around the roll and glued to create a cylindrical scroll with an outer diameter of 5.5 mm. After being manufactured, it was cut into a length of 42.0 mm to produce a heated aroma source. 142 heated aroma emitters, each measuring 42.0 mm in length, 1.0 mm in width, and 0.1 mm in thickness. The aroma generating material assembly 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The aroma generating source 420 is a heated aroma generating base material of 0.64 g per heated aroma generating source 420. A heated aroma-emitting substrate assembly including the assembly 421 relative to the volume of the heated aroma-emitting source 420 The volume filling factor of 421 was 0.60. <Comparative Example 10>
[0178] In the same manner as in Comparative Example 6, a 0.1 mm thick sintered body was manufactured in the first molding step. In the second molding step, the sheet-shaped heated aroma-emitting substrate is molded into a size of 150 mm long and 210 mm wide. After cutting into a rectangle with a cutter, a rotary cutter is used to cut into a length of 210 mm and The product is cut into a shape with a width of 1.0 mm and a thickness of 0.1 mm to produce a long rectangular columnar heated aroma-emitting substrate. It was done.
[0179] This heated aroma-generating substrate has 142 pieces aligned in the lengthwise direction and a basis weight of 34 g / m2. The paper is wrapped around the roll and glued to create a cylindrical scroll with an outer diameter of 5.5 mm. After being manufactured, it was cut into a length of 42.0 mm to produce a heated aroma source. 142 heated aroma emitters, each measuring 42.0 mm in length, 1.0 mm in width, and 0.1 mm in thickness. The aroma generating material assembly 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The aroma generating source 420 is a heated aroma generating base material of 0.64 g per heated aroma generating source 420. A heated aroma-emitting substrate assembly including the assembly 421 relative to the volume of the heated aroma-emitting source 420 The volume filling factor of 421 was 0.60. <Comparative Example 11>
[0180] In the same manner as in Comparative Example 7, a sheet-shaped heated aromatic fiber having a thickness of 0.3 mm was produced in the first molding step. In the second molding process, the scent-generating base material is cut into a rectangle 150 mm long and 210 mm wide. After being cut by a rotary cutter, the length is 210 mm, width is 1.5 mm, and thickness is The heated aroma-emitting substrate was cut into a shape having a length of 0.3 mm to produce a long rectangular columnar shape.
[0181] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 31 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.3 mm thick. The combination 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The raw source 420 is a heated aroma-emitting substrate aggregate of 0.63 g per heated aroma-emitting source 420. The heated aroma-emitting substrate assembly 42 includes a body 421, and the heated aroma-emitting substrate assembly 42 includes a body 422. The volume filling factor of 1 was 0.59. <Comparative Example 12>
[0182] In the same manner as in Comparative Example 7, a sheet-shaped heated aromatic fiber having a thickness of 0.3 mm was produced in the first molding step. In the second molding process, the scent-generating base material is cut into a rectangle 150 mm long and 210 mm wide. After being cut by a rotary cutter, the length is 210 mm, width is 1.5 mm, and thickness is The heated aroma-emitting substrate was cut into a shape having a length of 0.3 mm to produce a long rectangular columnar shape.
[0183] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 31 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.3 mm thick. The combination 421 is wrapped around a heated aroma generating substrate wrapping member 422 made of paper. The raw source 420 is a heated aroma-emitting substrate aggregate of 0.63 g per heated aroma-emitting source 420. The heated aroma-emitting substrate assembly 42 includes a body 421, and the heated aroma-emitting substrate assembly 42 includes a body 422. The volume filling factor of 1 was 0.59.
[0184] In order to confirm the cooling agent sorption ability of the crosslinked PVP, menthol was used as a cooling agent. The heated aroma sources of Examples 11 to 18 and Comparative Examples 5 to 12 were used to carry out the following evaluation 4. ~6 was carried out. [Rating 4-1]
[0185] Conventionally, aroma-generating substrates containing menthol that are heated have been known to lose their aroma when left for a long period of time. Menthol is soluble in ethyl alcohol but poorly soluble in water. In the evaluation 4-1, the white crystals of menthol were precipitated. The white crystal precipitation test was carried out as follows.
[0186] Using the heated aroma sources manufactured in Examples 11 to 15 and Comparative Examples 5 to 8, evaluation 1 was performed. The heated smoking device 100 is equipped with a blade-type heat source 130 as described in A heated aroma cartridge 300 that can be attached to a cigarette lighter (trademark) and smoked has been manufactured. 20 heated aromatic cartridges 300, each with a long side of 70 mm, a short side of 14 mm, and a height of 45 mm The heated aroma source 320 is placed in contact with the bottom of a paper box and packed vertically. The product was left wrapped in polyethylene bags at 5°C for 48 hours. The cartridge 300 is taken out and left in a room temperature and humidity environment for one day. The end surface of the combined 321 that was in contact with the bottom of the box was observed using a 5x magnifying glass. The number of white crystals of menthol precipitated was counted and 20 heated aroma cartridges were The average value of the 300 points was calculated and evaluated according to the following criteria. Therefore, menthol dissipates outside the aroma-generating substrate, and even if the aroma-generating substrate is heated, There is a high possibility that the cooling sensation will be impaired, and it is assumed that a rank of B or A would be usable. . Rank A: 0 white crystals Rank B: 1-4 white crystals Rank C: 5 or more white crystals
[0187] In addition, the conditions for leaving the heated aroma cartridge in Evaluation 4-1 were as follows: This was established after extensive investigation into the conditions under which crystals are likely to precipitate. [Rating 4-2]
[0188] The purpose is the same as Evaluation 4-1, but it may be affected by the shape of the heated aroma-emitting substrate. Therefore, the heated aroma sources manufactured in Examples 16 to 18 and Comparative Examples 9 to 12 were The heated smoking device 200 is equipped with the omnidirectional heat source 240 described in Evaluation 1-2. A heated aroma cartridge 400 that can be attached to a cigarette lighter (registered trademark) and smoked was manufactured. The 20 heated aroma cartridges 400 have a long side of 55 mm, a short side of 12 mm, and a height of The heated aroma source 420 is placed in contact with the bottom of a paper box having a thickness of 85 mm and packed vertically. Ta.
[0189] After that, it was left under exactly the same conditions as in Evaluation 4-1, and then it was subjected to exactly the same methods and and evaluated based on the following criteria. [Rating 5-1]
[0190] The main purpose of the study was to determine the correlation between the precipitation test and the smoking test. The heated aroma cartridge in which the test was conducted was smoked in the manner described in Evaluation 1-1. As described in Evaluation 2-1, the sensory evaluation of the cooling sensation of menthol by five subjects was conducted. An investigation was conducted.
[0191] The smoking test was carried out as follows. Using the heated aroma generating source, a heated aroma cartridge 300 was manufactured in the same manner as in Evaluation 1-1. The 20 heated aroma cartridges 300 are made of a 70 mm long side, 14 mm short side, The heated aroma source 320 is placed in contact with the bottom of a paper box with a height of 45 mm and packed vertically into the box. In this smoking test, a box filled with heated aroma cartridges was The cigarettes were then left at 25°C for two weeks, similar to the conditions that smokers would find them in. Using the heated aroma cartridge before and after leaving it, subjects compared the refreshing sensation of menthol. The pricing standards are as follows: Rank A: No change in the refreshing sensation of menthol before and after leaving it Rank B: The refreshing feeling of menthol after leaving it alone is slightly less than before leaving it alone Rank C: The refreshing feeling of menthol after leaving it for a while is clearly less than before leaving it for a while. [Rating 5-2]
[0192] Regarding the smoking test, in addition to the same objectives as Evaluation 5-1, the shape of the heated aroma-generating substrate, The structure of the thermal aroma cartridge, the heat source method of the heated smoking device and the heated aroma It is highly likely that the shape of the fragrance source will have an effect, so it is also important to check whether or not this has an effect. The purpose of the evaluation was to evaluate the heated aroma cartridge in which the precipitation test in Evaluation 4-2 was carried out. Smoking was performed in the manner described in 1-2, and five subjects were evaluated as described in Evaluation 2-2. A sensory survey was conducted on the cooling sensation of menthol.
[0193] The smoking test was carried out as follows. Using the heated aroma generating source, the heated aroma cartridge 400 was 20 of the heated aroma cartridges 400 are manufactured, each having a long side of 55 mm and a short side of 12 mm. The heated aroma source 420 is placed in contact with the bottom of a paper box having a height of 85 mm and packed vertically. In this smoking test, a box filled with heated aroma cartridges was They were left at 25°C for two weeks, similar to the conditions a regular smoker would find them in, and The subjects compared the refreshing sensation of menthol using the heated aromatic cartridge before and after it was left standing. The evaluation criteria are as follows: Rank A: No change in the refreshing feeling of menthol before and after leaving it Rank B: The refreshing feeling of menthol after leaving it alone is slightly less than before leaving it alone Rank C: The refreshing feeling of menthol after leaving it for a while is clearly less than before leaving it for a while. [Rating 6]
[0194] The precipitation test and the smoking test are correlated to reveal the results of the smoking test. The factors that cause this are clarified, and smoking tests that require the manufacture of heated aroma cartridges are carried out. It is believed that it is possible to judge the results of smoking tests by precipitation tests without performing However, the deposition test was carried out to measure the amount of menthol deposited on the end surface of the heated aroma-emitting substrate of the heated aroma-emitting source. The number of white crystals in the bottle determines the temperature and does not depend on the internal condition of the heated aroma source. Therefore, in order to find a more accurate standard for judging the results of the smoking test, the menthol reduction rate was measured.
[0195] The menthol reduction rate was measured in an environment of 17°C and 65% relative humidity. The amount of menthol contained in the aroma-generating base material when the base material is precisely weighed out at about 5g to 10g. The mass of the aroma-generating substrate is taken as d(0), and the mass is calculated from the composition of the components constituting the aroma-generating substrate to be heated. The rate of decrease in the amount of the aroma generated by heating the precisely weighed substrate after it is left at 5°C for 24 hours is called the rate of decrease in the amount of the aroma generated by heating the substrate. The mass is d(24), and the mass after being left at 5°C for 48 hours is d(48), and the following formula is used: ) Here, the reason for subtracting d(48) from d(24) in the above formula is that When the precipitation test of the ole was observed in detail, the precipitation of white crystals was observed after 24 hours. Therefore, we excluded other dissipated components than menthol to better reflect the dissipation of menthol. It is significant that this can be done. d = {(d(24) - d(48)} / d(0) (1)
[0196] The compositions of Examples 11 to 18 and Comparative Examples 5 to 12 used in Evaluations 4 to 6 and The shape and number of the heated aroma-emitting substrates used in the heated aroma-emitting source are shown in Table 2-1. The production conditions for the composition of the thermal aroma-emitting base material and the results of evaluations 4 to 6 are shown in Table 2-2. [Table 2-1] [Table 2-2]
[0197] As is clear from the results in Table 2-2, the cross-sectional shape perpendicular to the longitudinal direction of the heated aroma-generating substrate, Regardless of the physical characteristics of the heated aroma-generating substrate, such as length and number, and regardless of the type of heated smoking device, Regardless of the heat source method of the ingredients, there was a good correlation between the precipitation test, smoking test, and menthol reduction rate. In particular, when the menthol reduction rate is 0.200 or less, the crosslinked PVP is the menthol The menthol is absorbed and effectively prevented from dissipating over time. The reason why such a heated aroma generating substrate can be manufactured is that menthol is used as a heated aroma generating substrate. To be mixed into the generating base composition, menthol was dissolved in ethanol to prepare a menthol / ethanol solution. A method for producing a heated aroma-generating substrate, comprising the step of mixing crosslinked PVP as an alcohol solution. In addition, the menthol content in the heated aroma-generating base material is 1 to 20%. 10% by mass, and the content of crosslinked PVP in the heated aroma-generating base material is 2 to 10% by mass. and 1 to 6 times the menthol content, particularly when the menthol content is increased This can prevent the risk of loss of information.
[0198] The crosslinked PVP that can prevent the dissipation of menthol over time is Cooling agents other than menthol, such as menthyl ethers, menthyl esters, and menthol derivatives such as menthyl carbonate, as well as menthone and its derivatives; and menthane and its derivatives, and menthanecarboxylic acid-N-ethylamide [W S3], Nα-(menthanecarbonyl)glycine ethyl ester [WS5], Mentha Menthanecarboxylic acid-N-(4-cyanophenyl)amide, Methylphenyl)amide and Menthanecarboxylic acid-N-(alkoxyalkyl)amide Menthane carboxylic acid amides such as methyldiisopropylpropionamide [ 2,3-Dimethyl-2-(2-propyl)-butyric acid-N-methylamide [WS23] etc. ,3-Dimethyl-2-(2-propyl)-butyric acid derivatives, and (l(-)-isopregon isopulegol and its esters such as l(-)-isopulegol acetate, N- (2-(pyridin-2-yl)ethyl)-3-p-menthane carboxamide, (1R, 2S,5R)-N-(4-methoxyphenyl)-5-methyl-2-(1-isopropyl) Cyclohexane-carboxamide [WS12] and carboxamides such as oxamate It is also effective against L-carvone, xylitol, thymol, spilanthol, etc. It has been confirmed that:
[0199] Thirdly, by incorporating microcrystalline cellulose into the heated aroma-generating substrate, The aerosol former and the binder are mixed and dispersed homogeneously, so that the mixture is not subject to compression and shear. For example, in the sheet forming process using a three-roll mill, the sheet aggregates. It is possible to effectively prevent breakage and adhesion to the metal roll, and the aroma-emitting substrate to be heated can be It reduces the volumetric shrinkage caused by drying and acts as a reinforcing material to enhance the aroma-generating substrate when heated. The strength is improved, so the aroma-emitting substrate to be heated is less likely to fall off, fall off, or fall off before and after smoking and after long-term storage. In order to specifically show that the deformation and the like can be prevented, Examples 19 to 26 and Experiments for Comparative Examples 13 to 18 were carried out. Example 19
[0200] As in Examples 11 to 13 and Examples 16 to 18, black tea leaves and aerosols were used as the aroma source materials. Solformer, CMC and glucomannan as binders, menthol and Cross-linked PVP is used as a sorbent for xylitol, a cooling agent. In this example, methyl The effect of using microcrystalline cellulose instead of cellulose was confirmed. The ingredients are mixed together in a mixer and stirred for 15 minutes to form the heated aroma-generating base material. The composition was prepared. 100 parts by weight of dried and ground black tea leaves Glycerin 30 parts by weight Propylene glycol 30 parts by weight Sodium carboxymethylcellulose (CMC) 4 parts by weight Glucomannan 1 part by weight Microcrystalline cellulose 15 parts by weight Crosslinked polyvinylpyrrolidone (PVP) 10 parts by weight Menthol 5 parts by weight Xylitol 1.5 parts by weight
[0201] The black tea leaves were dried at 70°C so that the moisture content was approximately 2% by mass, crushed, and then cooled to 80°C. The microcrystalline cellulose used had an average particle size of 90 μm. m and the mass average molecular weight (Mw) was 36,000. However, the average particle size was 90μm, but the residue on the sieve with 75μm openings accounts for 5% of the total amount of microcrystalline cellulose. 2% by mass, and the residue on a sieve with an opening of 250 μm is based on the total amount of microcrystalline cellulose. The particle size distribution is narrow, with a particle size of 1% by mass, and the effect of microcrystalline cellulose is significantly expressed. We chose the one that was best for our needs.
[0202] The heated aroma-generating substrate composition thus produced is forced between narrow rolls. The compression caused by the rolling and the shear caused by the difference in roll speeds uniformly knead and break down the high viscosity paste. The material can be dispersed and formed into a sheet using a three-roll mill to produce a desired thickness. In this example, the roll gap was adjusted in advance. and a step of pressing a doctor blade against the roll at a roll speed ratio of 0.01 to 0.01 and forming the material into a sheet. By repeating this process eight times, a sheet-shaped heated aroma-emitting substrate with a thickness of 0.1 mm was produced. During this time, water was provided appropriately depending on the condition of the sheet.
[0203] This sheet-shaped heated aroma-emitting substrate is 0.1 mm thick and has a length of 150 mm in height and 240 mm in width. After cutting into a square, a rotary cutter was used to cut the square into pieces 240 mm long, 1.5 mm wide, and 1.5 mm thick. Long prismatic heated aroma-emitting substrates with a length of 0.1 mm were prepared.
[0204] The 150 long rectangular column-shaped heated aroma-emitting substrates thus produced were aligned in the longitudinal direction. Then, a paper with a basis weight of 34 g / m2 was used as the heated aroma generating substrate wrapping member 322. The roll is then rolled and glued to produce a cylindrical roll with an outer diameter of 6.9 mm. After that, it was cut into a length of 12.0 mm to produce a heated aroma source. A set of 150 heated aroma-emitting substrates, each measuring 3.0 mm in diameter, 1.5 mm in width, and 0.1 mm in thickness. 21 is a heated aroma source 3 wrapped around a heated aroma-emitting substrate wrapping member 322 made of paper. 20 is a heated aroma generating substrate assembly 320 of 0.29 g per heated aroma generating source 320 1, and the volume of the heated aroma-emitting substrate assembly 321 relative to the volume of the heated aroma-emitting source 320 The volume packing ratio was 0.60. In addition, the aroma source was For 100 parts by mass of the material, 60 parts by mass of aerosol former, CMC and Glu as binders The alcomannan was 4 parts by mass and 1 part by mass, the microcrystalline cellulose was 15 parts by mass, and the crosslinked The bridged PVP was 10 parts by weight, and the menthol and xylitol were 5 parts by weight and 5 parts by weight, respectively. and 1.5 parts by mass. Example 20
[0205] In Example 20, the effect of microcrystalline cellulose was examined in a cross section perpendicular to the longitudinal direction of the heated aroma-generating substrate. In order to concretely demonstrate that the aroma generating effect does not depend on the surface shape, the aroma generating effect of the heated aroma generating substrate is compared with that of Example 19. The thickness of the heated aroma-generating substrate was increased. The composition was used to produce a sheet-shaped applied powder using a three-roll mill in which compression and shear were repeated. A thermal aroma generating substrate was prepared. In Example 20, the position of the doctor blade, the roll gap, In addition, the speed ratio between the rolls and the like were adjusted differently from those in Example 19. The process was repeated eight times to form a 0.3 mm thick sheet of the heated aroma-emitting substrate.
[0206] This sheet-shaped heated aroma-emitting substrate is 0.3 mm thick and has a length of 150 mm in height and 240 mm in width. After cutting into a square, a rotary cutter was used to cut the square into pieces 240 mm long, 1.5 mm wide, and 1.5 mm thick. Long prismatic heated aroma-emitting substrates with a length of 0.3 mm were prepared.
[0207] The 50 long rectangular pillar-shaped heated aroma-emitting substrates thus produced were aligned in the longitudinal direction. Then, a paper with a basis weight of 34 g / m2 was used as the heated aroma generating substrate wrapping member 322. After being rolled and glued, a cylindrical roll with an outer diameter of 6.9 mm is produced. , and cut into a length of 12.0 mm to produce a heated aroma source. 50 pieces of heated aroma-emitting substrates each having a diameter of 0.0 mm, width of 1.5 mm, and thickness of 0.3 mm. The heated aroma generating source 320 is wrapped around a heated aroma generating substrate wrapping member 322 made of paper. For each heated aroma generating source 320, 0.29 g of the heated aroma generating substrate aggregate 321 is used. The volumetric filling ratio of the heated aroma-emitting substrate assembly 321 to the volume of the heated aroma-emitting source 320 is also included. The filling rate was 0.60. The composition contained in the heated aroma-generating substrate 3211 (FIG. 3) is the same as in Example 19. Example 21
[0208] In Example 21, the effect of the microcrystalline cellulose was also observed in the cross section perpendicular to the longitudinal direction of the heated aroma-generating substrate. In order to concretely demonstrate that the aroma generating property is not dependent on the shape, the aroma generating property of the heated aroma generating substrate is further increased from that of Example 20. The thickness was increased. Therefore, the aroma-generating substrate to be heated was manufactured in exactly the same manner as in Example 29. The composition is used to produce a sheet-shaped heated product using a three-roll mill in which compression and shear are repeated. An aroma-generating substrate was produced. In Example 21, the position of the doctor blade, the distance between the rolls, The three-roll mill was designed with adjustments different from those in Example 20 with respect to the roll spacing, roll speed ratio, etc. The mixture was milled eight times to form a 0.5 mm thick sheet of the aroma-releasing substrate to be heated.
[0209] This sheet-shaped heated aroma-emitting substrate is 0.5 mm thick and has a length of 150 mm in height and 240 mm in width. After cutting into a square, a rotary cutter was used to cut the square into pieces 240 mm long, 1.5 mm wide, and 1.5 mm thick. Long prismatic heated aroma-emitting substrates 0.5 mm in length were prepared.
[0210] The 30 long rectangular pillar-shaped heated aroma-emitting substrates thus produced were aligned in the longitudinal direction. Then, a paper with a basis weight of 34 g / m2 was used as the heated aroma generating substrate wrapping member 322. After being rolled and glued, a cylindrical roll with an outer diameter of 6.9 mm is produced. The heated aroma source 320 was manufactured by cutting the heated aroma source 320 into a length of 12.0 mm. A collection of 30 heated aroma-emitting substrates, each measuring 12.0 mm in diameter, 1.5 mm in width, and 0.5 mm in thickness. 321 is a heated aroma source wrapped around a heated aroma-emitting substrate wrapping member 322 made of paper 320 is a heated aroma generating substrate assembly 3 of 0.29 g per heated aroma generating source 320 21, and the volume of the heated aroma-emitting substrate assembly 321 relative to the volume of the heated aroma-emitting source 320 The volume filling rate was 0.60. In addition, the aroma-generating substrate 3211 (FIG. 3) contained The composition is the same as in Example 19. Example 22
[0211] To examine the effect of the content of microcrystalline cellulose, we use microcrystalline cellulose as an example. The amount of the flavoring agent was set to 4 parts by mass relative to the amount of black tea leaves used as the aroma source. The heated aroma source was manufactured. The result was a length of 12.0 mm, width of 1.5 mm, and thickness of 0. 50 pieces of the heated aroma-emitting substrate assembly 321, each having a diameter of 3 mm, are wrapped in a paper heated aroma-emitting substrate wrapper. The heated aroma source 320 wrapped around the pin member 322 is a single heated aroma source 320. The heated aroma generating source 320 includes 0.29 g of the heated aroma generating substrate 321 per unit area. The volumetric packing ratio of the heated aroma-emitting substrate assembly 321 to the volume was 0.60. In the aroma generating substrate 3211 of Example 22 (FIG. 3), The aerosol former is 60 parts by mass, and the binders CMC and glucomannan are 4 parts by weight and 1 part by weight, respectively, 4 parts by weight of microcrystalline cellulose, 10 parts by weight of crosslinked PVP, and menthol and xylitol are contained in amounts of 5 parts by mass and 1.5 parts by mass, respectively. There are. <Comparative Example 13>
[0212] The aroma-producing product was heated in the same manner as in Example 19, except that microcrystalline cellulose was not used. The result was a 12.0 mm long, 1.5 mm wide, and 0.1 mm thick source. The 50 pieces of the heated aroma-emitting substrate assembly 321 are wrapped in a paper heated aroma-emitting substrate wrapping member 3 The heated aroma source 320 wound around the heating element 22 is 0.2 9 g of the heated aroma generating substrate assembly 321, The volumetric packing ratio of the heated aroma-generating substrate assembly 321 was 0.60. The heated aroma generating substrate 3211 (FIG. 3) is aerosolized with respect to 100 parts by mass of the aroma source material. The mixture was 60 parts by mass of Luforma, 4 parts by mass of CMC and 4 parts by mass of glucomannan as binders. parts by mass and 1 part by mass of crosslinked PVP, and menthol and xylitol are The components are contained in the compositions of the present invention at 5 parts by mass and 1.5 parts by mass, respectively. <Comparative Example 14>
[0213] The heated aroma was produced in exactly the same manner as in Example 20, except that microcrystalline cellulose was not used. As a result, a 5 mm long, 1.5 mm wide, and 0.3 mm thick source was produced. The heated aroma-emitting substrate assembly 321 is wrapped in a paper heated aroma-emitting substrate wrapping member 32 The heated aroma source 320 wrapped around the 2 is 0.29 g of the heated aroma-emitting substrate assembly 321, The volumetric filling rate of the heated aroma-generating substrate assembly 321 was 0.60. The composition contained in the substrate 3211 (FIG. 3) is the same as that in Comparative Example 13. <Comparative Example 15>
[0214] The heated aroma was prepared in exactly the same manner as in Example 21, except that microcrystalline cellulose was not used. The source was manufactured. The result was a length of 12.0 mm, width of 1.5 mm, and thickness of 0.5 mm. The 50 pieces of the heated aroma-emitting substrate assembly 321 are wrapped in a paper heated aroma-emitting substrate wrapping member 3 The heated aroma source 320 wound around the heating element 22 is 0.2 9 g of the heated aroma generating substrate assembly 321, The volumetric filling rate of the heated aroma-emitting substrate assembly 321 was 0.60. The composition contained in the green substrate 3211 (FIG. 3) is the same as in Comparative Example 13. <Comparative Example 16>
[0215] Except for the use of methylcellulose instead of microcrystalline cellulose, the entire procedure was the same as in Example 20. The heated aroma source was manufactured in the same manner. The result was a length of 12.0 mm, width of 1.5 mm, and thickness of The heated aroma-emitting substrate assembly 321 is made of paper and has a thickness of 0.3 mm. The heated aroma source 320 wrapped around the material wrapping member 322 is heated aroma source 32 Each of the heated aroma generating sources 321 contains 0.29 g of the heated aroma generating substrate aggregate 321. The volumetric filling rate of the heated aroma-generating substrate assembly 321 relative to the volume of the container 20 was 0.60. The aroma generating substrate 3211 to be heated in Comparative Example 16 (FIG. 3) contains 100 parts by mass of the aroma source material. 60 parts by mass of aerosol former, CMC and glucomannan as binders , 4 parts by mass and 1 part by mass, respectively, methylcellulose was 15 parts by mass, and crosslinked PVP was 10 parts by weight, and menthol and xylitol are 5 parts by weight and 1.5 parts by weight, respectively. Included.
[0216] The above Examples 19 to 22 and Comparative Examples 13 to 16 were found to be effective in preventing smoking in the smoking test described below. The blade-type heat source ICOS (registered trademark) was used for evaluation. However, the heating method, maximum temperature, and the heated aroma source and The composition of the heated aroma cartridges is different, which may affect the evaluation results. Therefore, it is the same heated smoking device, but the glow of the omnidirectional heat source by electromagnetic induction heating (registered trademark) In Examples 23 to 26 and Comparative Examples 17 and 18, The composition of the heat-generating aroma base material and its cross-sectional shape perpendicular to the longitudinal direction are the same as those of Examples 19 to 22 and The comparison corresponds to Comparative Examples 14 and 16, but the heated aroma release corresponds to Glo (registered trademark). The length and outer diameter of the raw material were then formed. Example 23
[0217] The heated aroma-generating sheet substrate having a thickness of 0.1 mm was prepared in the same manner as in Example 19. After cutting into a rectangle measuring 150 mm by 210 mm, the material is cut using a rotary cutter. The material is cut into a long rectangular column shape with a length of 210 mm, a width of 1.5 mm, and a thickness of 0.1 mm. A heated aroma-generating substrate was prepared.
[0218] The heated aroma generating substrate is made of 93 pieces aligned lengthwise and made of paper with a basis weight of 34g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 93 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.1 mm thick. The combination 421 is a heated aroma generating substrate wrapped around a paper wrapping member 422. The source 420 is a heated aroma generating material collection of 0.63 g per heated aroma generating source 420. The volume of the heated aroma generating substrate assembly 420 including the combination 421 is The volume filling factor of 21 was 0.59. Example 24
[0219] The heated aroma-emitting sheet substrate having a thickness of 0.3 mm was prepared in the same manner as in Example 20. After cutting into a rectangle measuring 150 mm by 210 mm, the material is cut using a rotary cutter. The material is cut into a long rectangular column shape with a length of 210 mm, a width of 1.5 mm, and a thickness of 0.3 mm. A heated aroma-generating substrate was prepared.
[0220] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 31 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.3 mm thick. The combination 421 is a heated aroma generating substrate wrapped around a paper wrapping member 422. The source 420 is a heated aroma generating material collection of 0.63 g per heated aroma generating source 420. The volume of the heated aroma generating substrate assembly 420 including the combination 421 is The volume filling factor of 21 was 0.59. Example 25
[0221] The heated aroma-generating sheet substrate having a thickness of 0.5 mm was prepared in the same manner as in Example 21. After cutting into a rectangle measuring 150 mm by 210 mm, the material is cut using a rotary cutter. The material is cut into a long rectangular column shape with a length of 210 mm, width of 1.5 mm, and thickness of 0.5 mm. A heated aroma-generating substrate was prepared.
[0222] The heated aroma-generating substrate is made of 19 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 19 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.5 mm thick. The combination 421 is a heated aroma generating substrate wrapped around a paper wrapping member 422. The source 420 is a heated aroma generating material collection of 0.64 g per heated aroma generating source 420. The volume of the heated aroma generating substrate assembly 420 including the combination 421 is The volume filling factor of 21 was 0.60. Example 26
[0223] The heated aroma-generating sheet substrate having a thickness of 0.3 mm was prepared in the same manner as in Example 22. After cutting into a rectangle measuring 150 mm by 210 mm, the material is cut using a rotary cutter. The material is cut into a long rectangular column shape with a length of 210 mm, a width of 1.5 mm, and a thickness of 0.3 mm. A heated aroma-generating substrate was prepared.
[0224] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 31 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.3 mm thick. The combination 421 is a heated aroma generating substrate wrapped around a paper wrapping member 422. The source 420 is a heated aroma generating material collection of 0.63 g per heated aroma generating source 420. The volume of the heated aroma generating substrate assembly 420 including the combination 421 is The volume filling factor of 21 was 0.59. <Comparative Example 17>
[0225] The heated aroma-emitting sheet substrate having a thickness of 0.3 mm was prepared in the same manner as in Comparative Example 14. After cutting into a rectangle measuring 150 mm by 210 mm, the material is cut using a rotary cutter. The material is cut into a long rectangular column shape with a length of 210 mm, a width of 1.5 mm, and a thickness of 0.3 mm. A heated aroma-generating substrate was prepared.
[0226] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 31 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.3 mm thick. The combination 421 is a heated aroma generating substrate wrapped around a paper wrapping member 422. The source 420 is a heated aroma generating material collection of 0.63 g per heated aroma generating source 420. The volume of the heated aroma generating substrate assembly 420 including the combination 421 is The volume filling factor of 21 was 0.59. <Comparative Example 18>
[0227] The heated aroma-generating sheet substrate having a thickness of 0.3 mm, which was produced in the same manner as in Comparative Example 16, was After cutting into a rectangle measuring 150 mm by 210 mm, the material is cut using a rotary cutter. The material is cut into a long rectangular column shape with a length of 210 mm, width of 1.5 mm, and thickness of 0.3 mm. A heated aroma-generating substrate was prepared.
[0228] The heated aroma-generating substrate is made of 31 pieces aligned lengthwise and made of paper with a basis weight of 34 g / m2. The roll is then wrapped around the material and glued to create a cylindrical roll with an outer diameter of 5.5 mm. After the heating, the heated aroma source was cut to a length of 42.0 mm. A collection of 31 heated aroma-emitting substrates, each 42.0 mm long, 1.5 mm wide, and 0.3 mm thick. The combination 421 is a heated aroma generating substrate wrapped around a paper wrapping member 422. The source 420 is a heated aroma generating material collection of 0.63 g per heated aroma generating source 420. The volume of the heated aroma generating substrate assembly 420 including the combination 421 is The volume filling factor of 21 was 0.59.
[0229] The heated aroma sources produced in Examples 19 to 26 and Comparative Examples 13 to 18 were used to produce microcrystals. It is possible to concretely demonstrate the effects of crystalline cellulose. The following evaluations 7 to 11 were carried out. did. [Rating 7]
[0230] The heated aroma sources 320 of Examples 19 to 22 and Comparative Examples 13 to 16 were used for evaluation. As shown in FIG. 1-1 and FIG. 1, the heated smoking device 100 is equipped with a blade-type heat source. The heated aroma cartridge 300 for smoking is manufactured, and after one smoking session, the heated aroma cartridge is The heated aroma cartridge 300 is removed from the device 100, and the heated aroma generating substrate 3211 ( A drop test was conducted as shown in Figure 3.
[0231] The drop test was carried out by dropping the heated aroma generating source 320 of the heated aroma cartridge 300 vertically after smoking. By shaking it up and down three times in the direction of the heated aroma source 320, a heated aroma source made of paper is The heated aroma-emitting substrate 3211 wrapped in the aroma-emitting substrate wrapping material 322 (FIG. 3) The presence or absence of falling off or dropping off was observed. The evaluation criteria are as follows. Rank A: No falling off or falling off Rank B: Falling or falling off [Rating 8]
[0232] As in Evaluation 7, the heated aroma generating sources 320 of Examples 19 to 22 and Comparative Examples 13 to 16 were As described in Evaluation 1-1 and FIG. 1, a heated smoking device 1 equipped with a blade-type heat source was used. A heated aroma cartridge 300 for smoking by attaching it to the cigarette lighter cigar cigar cigar 00 was manufactured.
[0233] The 20 heated aroma cartridges 300 are arranged in a size of 70 mm long, 14 mm short, and 45 mm high. The heated aroma source 320 is placed in contact with the bottom of a paper box measuring 1.5 mm in diameter and then packed vertically in the box. The heated aroma cartridge 300 was then removed from the box and left at 45° C. for two weeks. The heated aroma generating source of the heated aroma cartridge 300 is shaken up and down three times vertically downward. As a result, the heated aroma generating source 320 is a paper-made heated aroma generating substrate wrapping material. Observe whether the heated aroma generating substrate 3211 (FIG. 3) wrapped with 322 falls off or falls off. The evaluation criteria are as follows: Rank A: No falling off or falling off Rank B: Falling or falling off [Rating 9]
[0234] The heated aroma generating sources 420 of Examples 23 to 26 and Comparative Examples 17 and 18 were used for evaluation. As shown in Figure 1-2 and Figure 2, the device is attached to a heated smoking device 200 equipped with an omnidirectional heat source. After manufacturing the heated aroma cartridge 400 to be smoked, 20 pieces of 00 are attached to the bottom of a paper box with a long side of 55 mm, a short side of 12 mm, and a height of 85 mm. After being vertically packed in a box with the heated aroma source 420 in contact, the box was left at 45° C. for two weeks.
[0235] The heated aroma cartridge 400 was removed from the box, and then placed in the same container as shown in FIG. The heated aroma cartridge 400 is attached to the heated smoking device 200, and after smoking, it is removed. The series of operations of attaching, detaching, and removing the heated aroma cartridge 400 are carried out to evaluate the operability of the heated aroma cartridge 400. The test was carried out and the evaluation criteria were as follows: Rank A: No deformation of the heated aroma cartridge or falling off of the heated aroma generating base material when removed. Rank B: When removing or attaching the heated aroma cartridge, deformation occurs and the heated aroma generating base material falls off. [Rating 10]
[0236] As in Evaluation 9, the heated aroma cartridge 400 was packed in a box and left at 45°C for two weeks. After that, the heated aroma cartridge 400 is taken out of the box, and the heated aroma source 420 is vertically By shaking it up and down three times, a heated aroma source 420 made of paper is used as the heated aroma source 420. The aroma-emitting substrate to be heated, which is wrapped with the aroma-emitting substrate wrapping member 422, falls off or falls off. The presence or absence was observed. The evaluation criteria were as follows: Rank A: No falling off or falling off Rank B: Falling or falling off [Rating 11-1]
[0237] The reasons for the results of 7 to 10 are considered to be as follows: Fragrance source material and aerosol The former is mixed and dispersed through the binder, so it can be formed into a sheet by compression and shear. For example, in the sheeting of heated aroma-generating substrates using a three-roll mill, The addition of cellulose effectively prevents the sheet from cohesively breaking and sticking to the metal roll. The resulting mixture is then mixed and dispersed in a uniform manner, producing a dense, heated aroma-generating substrate. In addition, the microcrystalline cellulosic acid does not absorb solvents such as water or ethanol. The cellulose is present in the heated aroma-generating substrate in powder form, and microcrystalline cellulose acts as a reinforcing material. It is believed that this function produces a strong aroma-emitting substrate when heated. The heated aroma-generating substrate containing microcrystalline cellulose exhibits a volumetric shrinkage over time due to drying, etc. It is assumed that shrinkage will be reduced.
[0238] Therefore, the shape of the heated aroma-generating substrate due to the volumetric shrinkage caused by the heating and drying of the heated aroma-generating substrate The rate of change was measured and the correlation with the ratings of 7 to 10 was examined. The specific method for measuring the rate of change is as follows. The aroma-emitting heated sheet substrates manufactured in steps 16 and 17 were placed in a container with a length of 50 mm. A test piece for measuring the volumetric shrinkage of a heated aroma-generating substrate cut into a rectangular shape with a width of 15 mm. Heat drying was performed using a halogen moisture meter (electronic halogen moisture meter) (Bangxi In Manufactured by Instrument Technology Co., Ltd., Model No.: DHS-50- 5) was used, the test piece was placed on the sample dish of the halogen moisture meter, and the halogen The test piece was heated from above the sample dish by a lamp. The heating temperature was 105°C. The length, width, and thickness of the test piece were measured at 0, 10, and 15 minutes. Using the measured values, the rate of change was calculated from the formula shown in Table 4-1. The length change rate La (%), width change rate Wa (%), and width of a 0.3 mm test piece after drying for 10 minutes Change rate Wa (%) and thickness change rate Ta (%), and length 50 mm, width 15 mm, The length change rate Lb (%) and width change rate Wb (%) of a 0.3 mm thick test piece after drying for 15 minutes. The width change rate Wb (%) and the thickness change rate Tb (%) were calculated. The length, width, and thickness of the test piece are measured at a temperature of 28℃ to 30℃ and a relative humidity of about 40%. Measurement when the moisture content is 15-20% by mass, adjusted by storing in an atmospheric condition. values were used. [Rating 11-2]
[0239] The purpose is the same as Evaluation 11-1, but the specific surface area varies depending on the shape of the test piece, and the volume yield Since this may affect the shrinkage of the specimens, the correlation between the scores 7 to 10 and the volumetric shrinkage was examined. The shape dependency of was investigated. That is, in the same manner as in Evaluation 1-1, Examples 20 and 22, and The heated aroma-emitting substrates of 0.3 mm thickness were prepared in Comparative Examples 14 and 16. The aroma-generating base is cut into a rectangular shape with a length of 12 mm and a width of 1.5 mm. The material was used as a test piece for measuring volumetric shrinkage.
[0240] The measurement method is exactly the same as in Evaluation 1-1, and the length is calculated from the definition of the rate of change shown in Table 5-1. The length change rate La (%) of a test piece with a length of 12 mm, width of 1.5 mm, and thickness of 0.3 mm after drying for 10 minutes ), width change rate Wa (%), width change rate Wa (%), and thickness change rate Ta (%), and The length change rate Lb( of a test piece with a length of 50 mm, width of 15 mm, and thickness of 0.3 mm after drying for 15 minutes %), width change rate Wb(%), width change rate Wb(%), and thickness change rate Tb(%) were calculated. Here, the length, width, and thickness of the test piece with a drying time of 0 minutes were measured at temperatures of 28°C to 30°C. The moisture content was adjusted by storing the product in an atmosphere with a relative humidity of about 40%. This is the measured value when the content is 20 mass % or less.
[0241] The compositions of Examples 19 to 26 and Comparative Examples 13 to 18 used in Evaluations 7 to 11 above, The shape and number of the heated aroma-emitting substrates used in the heated aroma-emitting source are shown in Table 3-1. The results of evaluations 7 to 11 are shown in Table 3-2. The calculated rate of shape change due to volumetric shrinkage of the aroma-generating substrate when heated is shown in Tables 4-2 and 5-2. .
[0242] The results of the drop tests and the attachment / detachment tests shown in Table 3-2 are shown in Examples 19 to 22 and Comparative Example 14. As is apparent from a comparison between Examples 23 to 26 and Comparative Examples 17 and 18, As described above, regardless of the cross-sectional shape perpendicular to the longitudinal direction of the heated aroma-generating substrate, microcrystalline cellulose A heated aroma generating source comprising a heated aroma generating substrate containing The cartridges do not shrink due to volumetric shrinkage even when exposed to drying over time and heat drying caused by smoking. This has solved the problem of the aroma-emitting substrate falling off or falling off when heated. The problem is different between a blade-type heat source using a heater and an omnidirectional heat source using electromagnetic induction heating. , heating method, maximum temperature reached, and the structure of the heated aroma source and the heated aroma cartridge Regardless of composition, the problem was resolved by the addition of microcrystalline cellulose. [Table 3-1] [Table 3-2]
[0243] The effect of this microcrystalline cellulose was examined on a test piece 50 mm long, 15 mm wide, and 0.3 mm thick. As can be seen from Table 4-2, which shows the shape change rate in the case of the test sample containing 2% by mass of microcrystalline cellulose, After drying for 10 minutes, the length change rate of the heated aroma-emitting substrate was La = 7.2%, and the width change rate Wa = 5.7%. , and the thickness change rate Ta=1.2%, and the length change rate Lb after drying for 15 minutes=8.1%. At least one of the following: a width change rate Wb=6.1%; and a thickness change rate Tb=1.5%. It is not necessary to satisfy all of these thresholds at the same time. As shown in Fig. 1, if this shape change rate is satisfied, there is a good correlation with the results of each drop test and attachment / detachment test. The reason why it is sufficient to satisfy only one of the length, width, and thickness is Although not clearly recognized in Table 4-2, the area of the cross section perpendicular to the longitudinal direction is smaller than that of the load. When the thermal fragrance generating substrate is dried, it becomes distorted, and the stems and leaves of plants are dispersed as fragrance source materials. This is because the heated aroma-generating substrate has anisotropy. [Table 4-1] [Table 4-2]
[0244] This correlation was observed for a test piece with a length of 12 mm, width of 1.5 mm, and thickness of 0.3 mm. In Table 5-2 showing the ratio, the heated aroma-generating substrate containing 2% by mass of microcrystalline cellulose After drying for 10 minutes, the length change rate La' is 4.8%, the width change rate Wa' is 5.0%, and the thickness The rate of change Ta' is 1.2%, and the rate of change in length Lb' after 15 minutes of drying is 5.8%, and the rate of change in width At least one of Wb'=5.1% and the thickness change rate Tb'=1.5% is set as the threshold value. It is not necessary to satisfy all of these thresholds at the same time. As shown in the figure, if this shape change rate is satisfied, there is a good correlation with the results of each drop test and attachment / detachment test. is obtained. [Table 5-1] [Table 5-2]
[0245] In this way, the heated aroma-emitting substrate of the present invention comprises an aroma source material, an aerosol former, and a resultant It is made of materials with different properties such as mixtures, but the types of additives and their addition methods, as well as The manufacturing method of the composition, such as curing, the addition of crosslinked PVP and the method of adding the same, and the microcrystals The addition of cellulose allows the fragrance source material, aerosol former, and binder to be mixed homogeneously. This allows for easy mixing and dispersion, preventing the fragrance from easily scattering over time, and preventing the shape from shrinking over time. The present invention provides a high-quality, heated aroma-emitting substrate that prevents shrinkage of its shape due to heating. That is why.
[0246] As a result, a heated aroma source comprising the heated aroma generating substrate of the present invention is provided. Deformation of the heated aroma source and the heated aroma emission when inserting and removing the cartridge into the heated smoking device Solves problems such as the base material falling off and dropping, and provides the toughness and strength required for this molding process. At the same time, the heated aroma generating substrate is capable of fully enjoying the aroma volatilized from the heated aroma source material. can be provided.
[0247] In addition, the heated aroma-generating substrate of the present invention may contain a cooling agent such as menthol or xylitol as an aromatic agent. When a fragrance or freshener is added, the dispersion of the fragrance or freshener over time is suppressed, and the heated fragrance containing the fragrance or freshener is Even after storing a heated aroma cartridge equipped with a fragrance source for a long period of time, it can still be attached to a heated smoking device. When smoking the aroma generating substrate, the aroma of the heated aroma generating substrate can be fully enjoyed.
[0248] Furthermore, the heated aroma-generating substrate of the present invention undergoes little dimensional change upon drying, and the heated aroma-generating substrate After a heated aroma cartridge equipped with an aroma generating source is attached to a heated smoking device and smoking is performed, Even if heated, the aroma generating base material will not fall off or fall out of the heated aroma cartridge, and can be stored for a long time. Even after the heating, the heated aroma generating base material does not fall off or fall off from the heated aroma cartridge. It is easy to handle and does not contaminate the heat source of heated smoking devices. Materials can be provided.
[0249] The present invention further relates to a heated aroma-emitting source using such a heated aroma-emitting substrate, The object of the present invention is to provide a heated aroma cartridge having an aroma generating source, The heated aroma generating source and the heated aroma cartridge of the present invention will be described in detail with reference to the drawings. The contents are not limited to these, and may be modified in various ways without departing from the spirit of the present invention. It is possible to carry out the present invention, and is limited only by the technical ideas described in the claims. It is something.
[0250] FIG. 1 shows the heating element used in the above examples and comparative examples, which is suitable for a blade-type heat source using a heater. An example of a thermal aroma cartridge 300 is shown. The scent cartridge 300 is an assembly 321 of heated aroma-emitting substrates 3211 (FIG. 3) of the present invention. A heated aroma generating source 320 wrapped around a heated aroma generating substrate wrapping member 322; A support member 331 is attached to one end of the heated aroma source 320 on the suction side in the longitudinal direction, The filter member 333 is attached to one end of the support member 331 on the suction side in the longitudinal direction. In a state where the heated aroma cartridge exterior member 310 is wrapped around the support member 331 and the filter, The mouthpiece 330 is made up of a filter member 333 and a mouthpiece 334. It is wrapped with a piece reinforcement member 3301.
[0251] FIG. 2 shows the heating conditions used in the above examples and comparative examples, which are suitable for an omnidirectional heat source using electromagnetic induction heating. 4 shows an example of a heated aroma cartridge 400. The aroma cartridge 400 is a heated aroma emitting device comprising an assembly 421 of the aroma emitting substrate of the present invention. A heated aroma source 420 wrapped around a raw substrate wrapping member 422 and the heated aroma source A cooling member 432 is attached to one end of the suction side of the heat source 420 in the longitudinal direction, and the cooling member 43 A filter member 433 is attached to one end of the suction side of the longitudinal direction of the filter member 2, and this filter member A hollow tube 434 is attached to one end of the suction side of the longitudinal direction of the 433, and a heated aroma cartridge is connected to the hollow tube 434. The coil spring 410 is wrapped around the coil spring 410 .
[0252] However, the heated aroma cartridge of the present invention is not limited to this configuration. The product can be made in a variety of configurations to meet the smoker's preferences regarding flavor, smoke, inhalation amount, cost, etc. It is characterized by the fact that it is possible to
[0253] The various configurations are shown in FIG. 1 using the heated aroma cartridge 300 suitable for the blade-type heat source. However, the heated aroma cartridge of the present invention is not limited to these. The present invention is limited only by the technical ideas described in the claims.
[0254] First, the heated aroma generating source 320 constituting the heated aroma cartridge 300 of the present invention is shown in FIG. As shown in FIG. 1, the assembly 321 of the aroma-generating substrate 3211 (FIG. 3) is an aroma-generating device. The aroma emitting device is characterized in that it is wrapped around a base wrapping member 322. As is clear from the cross-sectional view perpendicular to the longitudinal direction of the source, the heated aroma-generating substrate assembly of the present invention 321 is a rectangular columnar aroma-generating substrate (single unit) 3211 to be heated, and this aroma-generating substrate 3 211 and the heated aroma-generating base material primary aggregate 3212 formed by irregular contact. The inside of the heated aroma-emitting substrate assembly 321 and the heated aroma-emitting substrate assembly 3 Between the primary aggregate 21 and the heated aroma-generating substrate wrapping member 322, a gas flow path 321 is provided within the primary aggregate. A, gas flow path between primary aggregates 321B, gas flow path between substrate and primary aggregate 321C, A heated aroma-generating substrate that is easy to form a gas flow path 321D between the combined / wrapping members. It is characterized by its cross-sectional shape of 3211 and its arrangement parallel to the longitudinal direction.
[0255] However, the cross-sectional shape of the heated aroma-generating substrate is preferably a rectangle as shown in FIG. In order to achieve both a good balance between the formation of a gas flow path and the shape of the gas flow path, a polygonal or star-shaped polygon is preferable. It is more preferable from the viewpoint of composition. Furthermore, it is more preferable that the heated aroma-generating substrate is hollow. preferable.
[0256] In addition, the shape does not necessarily have to be a rectangular column, but may be a sheet. In this case, It is preferable for the aroma source to be folded irregularly in parallel with the longitudinal direction in order to form a gas flow path. .
[0257] Furthermore, as described below, the heated aroma generating source does not necessarily have to be a heated aroma generating substrate wrapping part. For example, the heated aroma cartridge exterior member 3 in FIG. The aromatic substance to be heated may be directly wrapped around the exterior member corresponding to 10. In this case, the exterior member may be In constructing the cartridge, it is preferable that the material has strength.
[0258] The heated aroma wrapping material does not necessarily have to be paper. Since the heated fragrance-generating substrate must be resistant to aerosol formers, Plastic film is more suitable than paper. Especially in terms of environmental protection, it is biodegradable. It is preferable to use a plastic film. The plastic is polyolefin. Plastics such as polyester, nylon, and engineering plastics are Degradable plastics include poly(3-hydroxybutyrate) (PHB), poly(ε- caprolactone) (PCL), poly(butylene succinate) (PBS), poly(L-la These materials are suitable for use in the heated aromatic capsules described below. The cartridge exterior member 310, the support member 331, the cooling member 332, and the filter member 333 This can also be applied to the filter wrapping member 3331 and the hollow tube 334, They need to be molded into shapes that will provide the functionality required for each application.
[0259] The heated aroma cartridge 300 of FIG. 1 according to one embodiment of the present invention includes a heated aroma source 3 20, and a support member 3 attached to one end of the heated aroma source 320 on the suction side in the longitudinal direction. 31, and a filter member 33 attached to one end of the support member 331 on the suction side in the longitudinal direction. 3, and in a state where it is wrapped with the heated aroma cartridge exterior member 310, Furthermore, the filter of the mouthpiece 330 consisting of the support member 331 and the filter member 333 The mouthpiece is wrapped around the mouthpiece member 333 with a reinforcing member 3301. The piece reinforcement member 3301 is not necessarily required, but at least the heated aroma cartridge In other words, the required component is the heat-resistant member 310. Except for the thermal aroma source, the main purpose is to prevent the heated aroma source from moving to the suction side as shown in Figure 4. The support member 331 has a function of cooling the volatilized aerosol former to produce smoke. A cooling member 332 having a function of promoting the generation of an aerosol, mainly a heated aroma generating member A filter section that has the function of filtering out volatile components generated from the source and components that cause unpleasant flavors from smoke. At least one selected from a hollow tube 334 having a function of being easily held in the mouth. As shown in FIG. 4, the support member 331 and the cooling unit At least one selected from the group consisting of a material 332, a filter member 333, and a hollow tube 334. The mouthpiece 330 is configured. However, two or more of these may be provided as a mouthpiece. In the case of the aroma generating source, the aroma generating device is arranged on the suction side in the longitudinal direction from the aroma generating source. The positional relationship of the material 331, the cooling member 332, the filter member 333, and the hollow tube 334 is observed. It is preferable that the above is done.
[0260] For example, a heated aroma cartridge 300 according to an embodiment of the present invention is as shown in FIG. The heated aroma-emitting substrate assembly 321 is wrapped with a heated aroma-emitting substrate wrapping material 322. The heated aroma source 320 has water resistance and pressure resistance so that it can maintain its shape even when held between the lips. It is characterized by being fixed to one end of the heated aroma cartridge exterior member 310. A simple device consisting of only a heated aroma generating source 320 and a heated aroma cartridge exterior member 310. In this case, the heated aroma source 320 is not included. The heated aroma cartridge exterior member 310 in this portion serves as the mouthpiece 330. It is a hollow tube 334 .
[0261] The simplest heated aroma cartridge is the heated aroma source 320 of FIG. The substrate wrapping member 322 is not provided, but the heated aroma generating substrate wrapper The heated aroma generating source 320 wrapped with the wrapping member 322 is heated by the aroma cartridge. This is preferable because it is easy to handle in production.
[0262] For example, a heated aroma cartridge 300 according to an embodiment of the present invention is shown in FIG. In this way, the aroma-emitting substrate assembly 321 is wrapped in the aroma-emitting substrate wrapping member 322. The heated aroma source 320 is wound around one end of the suction side in the longitudinal direction, and is attached with a piece of paper that can be held in the mouth by the lips and maintains its shape. The hollow tube 334 is made of a material having water resistance and pressure resistance that can be supported by the body. The heating aroma cartridge is characterized in that it is wrapped around an exterior member 310, and the hollow tube 3 34 serves as a mouthpiece 330.
[0263] Based on the heated aroma cartridge 300 shown in FIG. The cartridge can be a heated aroma cartridge of various configurations. The empty tube 334 is connected to the support member 331, the cooling member 332, and the filter member 333 shown in FIG. At least one of the hollow tubes 33 may be replaced. 4. The support member 331, the cooling member 332, and the filter member 334 are left as shown in FIG. 33. At least one or more selected from the following can be added. When two or more mouthpieces are used, the heated aroma source is located on the inhalation side in the longitudinal direction. There is a rule that the support member 331, the cooling member 332, the filter member 333, It is preferred that the positional relationship of hollow tube 334 be respected.
[0264] When the heated aroma cartridge is constructed in this manner, it can be used as a mouthpiece 330. A support member 331, a cooling member 332, a filter member 333, and a hollow tube 334 are used. Depending on the material and structure of the heated aroma source, the heated aroma source is wrapped with an individual wrapping material. 320, and the heated aroma cartridge outer casing 310 can be wrapped around it. In addition, the mouthpiece 330 includes a support member 331, a cooling member 332, and a filter. The member 333 and the hollow tube 334 are wrapped together with a wrapping material and then heated. The aroma generating source 320 is wrapped in the heated aroma cartridge exterior member 310. However, the method of constructing the heated aroma cartridge is not limited to these. There is none.
[0265] FIG. 7 shows a mouthpiece 330 including a mouthpiece reinforcing member 3301 and a support member 331. In one embodiment of the present invention, the cooling member 332, the filter member 333, and the hollow tube 334 are provided. The heated aroma cartridge 300 according to the embodiment is shown. The heated aroma generating source 320 wrapped in the heated aroma generating substrate wrapping material 322 is A support member 331 is attached to one end of the suction side of the support member 331, and the suction in the longitudinal direction of the support member 331 is A hollow cylindrical cooling member 332 is attached to one end of the cooling member 332, and the cooling member 332 is suctioned in the longitudinal direction. At one end of the pull side, a filter member 333 wrapped with a filter wrapping member 3331 is provided. The hollow tube 33 is attached to one end of the filter member 333 on the suction side in the longitudinal direction. 4 are attached, and these are all wrapped in the heated aroma cartridge exterior member 310. Then, the filter member 333 and the hollow tube 334 of the mouthpiece 330 are The heated aroma cartridge is characterized by being reinforced with a reinforcing member (3301).
[0266] The heated aroma cartridge 300 shown in FIG. 7 is not limited to this configuration. 1. The cooling member 332 and the hollow tube 334 are wrapped with a wrapping material suitable for each. The heated aroma source 320 and the filter member 333 may be provided with The heating aroma generating substrate wrapping member 322 and the filter wrapping member 3331 are wrapped around the In addition, the support member 331, the cooling member 332, the filter member 333, After the hollow tube 334 is wrapped with a mouthpiece wrapping material, the support member After one end of 331 and one end of the heated aroma source 320 are attached to each other, the whole is made into a heated aroma source. The incense cartridge may be wrapped with wrapping material 310. Depending on the construction and method, a variety of heated aroma cartridges can be manufactured.
[0267] The above is a heated smoking device that is equipped with a blade-type heat source using a heater. The heated aroma cartridge of the present invention has been described by taking the aroma cartridge 300 as an example. However, these are used by attaching them to heated smoking devices equipped with an omnidirectional heat source that uses electromagnetic induction heating. However, this technology is applicable to the heated aroma cartridge 400 that is equipped with an omnidirectional heat source. The heated aroma cartridge 400 is used by being attached to the heated smoking device. The entire aroma source 320 is heated to about 240° C., so that the aroma generating substrate wrapping member and As a substitute for paper for the exterior parts of heated aroma cartridges, plastics, engineering Plastics, biodegradable plastics, etc. cannot be used. Heat resistance equivalent to that of cellulose fibers (which make up paper), at which point glass transition or thermal decomposition begins. In other words, special engineering plastics with a glass transition temperature of 240°C or higher are used. Such special engineering plastics include, for example, polyamide isomers. Examples of the polymerizable compound include polyamide, polyarylate, polyimide, polytriazine, and liquid crystal polymer. Cut.
[0268] However, the heat of the heat source in all directions is not transmitted to the support members, cooling members, and filter members. -Wrapping materials and hollow tubes are made of plastic, engineering plastics From the viewpoint of environmental conservation, biodegradable plastics can be used. However, it is preferable to use plastic in a form that expresses the function according to each application. It is necessary to form it into a shape. [Industrial Applicability]
[0269] The present invention relates to tobacco and its related plants, which belong to the genus Nicotiana in the family Solanaceae, as well as the roots and stems of various plants. The aroma derived from the leaves, etc., and the smoke-like aerosol are enjoyed using heated smoking devices. Therefore, it has the same fragrance, aroma, and flavor as tobacco. You can enjoy smoking. Therefore, it is not only the smoker but also the non-smokers around them. You can enjoy smoking without any negative effects on your health, and it has a soothing effect that brings alpha waves to the brain. This is a new smoking technology that is useful for improving health and beauty. It has the potential to be widely used in incense sticks, burning incense, powdered incense, ointments, and aromatherapy. [Explanation of symbols]
[0270] 100 Blade-type heated smoking device 110 Body 120 Chamber inner wall 130 Blade type heat source 200 All-directional heated smoking device 210 Body 220 Chamber inner wall 230 Ventilation hole 240 Omnidirectional heat source 250 Heat source control unit 300 Heated aroma cartridge for blade type heat source 310 Heated aromatic cartridge exterior material 320 Heated aroma source 321 Heated aroma generating base material aggregate 3211 Heated aroma-generating substrate (single unit) 3212 Heated aroma generating base material primary aggregate 321A Gas flow path in primary aggregate 321B Gas flow path between primary aggregates 321C Gas flow path between substrate and primary aggregate 321D Gas flow path between substrate assembly and wrapping component 322 Heated aroma-generating substrate wrapping material 330 Mouthpiece 3301 Mouthpiece reinforcement material 331 Supporting member 332 Cooling Materials 333 Filter parts 3331 Filter wrapping materials 334 Hollow tube 400 Heated aroma cartridge for omnidirectional heat source 410 Heated aromatic cartridge exterior material 420 Heated aroma source 421 Heated aroma generating base material 422 Heated aroma-generating substrate wrapping material 430 Mouthpiece 432 Cooling material 433 Filter parts 434 Hollow tube
Claims
1. a heated aroma generating source filled with a heated aroma generating base material, a support member, a cooling member, and a filter member are arranged in this order in the longitudinal direction from the heated aroma generating source side; The heated aroma-generating source is obtained by wrapping the heated aroma-generating substrate with a heated aroma-generating substrate wrapping member which is a cylindrical roll, The support member and the filter member are wrapped with individual wrapping members, The support member is a hollow tube, and the cooling member is a hollow cylinder. A heated aroma cartridge.
2. The inner diameter of the through hole of the cooling member is larger than the inner diameter of the through hole of the support member. The heated aroma cartridge according to claim 1 .
Citation Information
Patent Citations
Cooling filter rod and cigarette
CN109588768A
Electrically heated cigarettes containing controlled-release flavorants
JP2006504431A
Non-tobacco nicotine-containing articles
JP2017501676A
Articles for use in devices for heating smoking material
JP2019523639A
Tobacco filler assembly and electronic cigarette cartridge
JP6516907B1