Light-emitting device

By incorporating a structure between the uncovered substrate and insulating layer, cracks in the coating film are redirected, ensuring the light emitting element is protected from degradation, thus maintaining the sealing integrity.

JP2024167425AInactive Publication Date: 2024-12-03PIONEER IP +1
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2024157467
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Cracks in the sealing film of light emitting elements, such as organic EL elements, can propagate from the edges towards the inside, potentially deteriorating the sealing properties and allowing gas and moisture to degrade the element.

Method used

A structure is introduced between the uncovered portion of the substrate and the insulating layer, which redirects cracks away from the light emitting element, using a coating film that does not cover the terminals and is reinforced by a structure extending in a specific direction to prevent crack propagation.

Benefits of technology

This design effectively prevents cracks from reaching the light emitting element, maintaining the sealing performance and protecting it from degradation by gas and moisture.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024167425000001_ABST
    Figure 2024167425000001_ABST
Patent Text Reader

Abstract

To suppress the degradation of a light-emitting element owing to a crack in a coating film even if the cracking propagates from an end of the coating film into the coating film on condition that the light-emitting element is covered with the coating film.SOLUTION: A light-emitting device 10 comprises: a substrate 100; an insulator layer 160; a light-emitting element 102; a coating film 140; and structures 150. The insulator layer 160 is formed on one face of the substrate 100, and has an opening 162. The light-emitting element 102 is formed in the opening 162. The coating film 140 is formed on the above one face of the substrate 100, and covers the light-emitting element 102, the insulator layer 160 and part of the above one face of the substrate 100. Another portion of the substrate 100, e.g. a part of an end of the substrate, hereinafter referred to as "first part", is not covered with the coating film 140. Each structure 150 is located between the corresponding first part of the substrate 100 and the insulator layer 160. The coating film 140 also covers the insulator layer 160.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a light emitting device. [Background technology]

[0002] In recent years, the development of light-emitting devices using organic EL elements as light sources has progressed. Organic EL elements require a sealing structure because they use an organic layer as the light-emitting layer. In general, organic EL elements are sealed using a sealing member made of glass, metal, or the like. The terminals connected to the organic EL elements are located outside the sealing member.

[0003] On the other hand, Patent Document 1 describes that an organic EL element is sealed by forming a sealing film using an ALD (Atomic Layer Deposition) method. Patent Document 1 also describes that stress is likely to concentrate in a portion having an inverse tapered shape such as a partition wall, and therefore cracks are likely to occur in the sealing film. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2013-097917 A Summary of the Invention [Problem to be solved by the invention]

[0005] When light-emitting elements such as organic EL elements are sealed by covering them with a film, cracks may develop from the edge of the film toward the inside of the film. If these cracks reach the insulating layer surrounding the light-emitting element, the sealing properties may deteriorate. If the sealing properties deteriorate, gases (e.g., oxygen) and moisture that deteriorate the light-emitting element may penetrate through the cracks and reach the light-emitting element through the insulating layer.

[0006] One example of a problem that the present invention aims to solve is, when a light-emitting element is covered with a coating film, how to suppress deterioration of the light-emitting element due to cracks that progress from the ends of the coating film toward the inside of the coating film. [Means for solving the problem]

[0007] One aspect of the present invention is a method for manufacturing a semiconductor device comprising: an insulating layer formed on the substrate and having an opening; A light emitting element formed in the opening; a coating film formed on the substrate and covering the light emitting element, the insulating layer, and a part of the substrate; Equipped with a first portion of the substrate that is a part of an area not covered with the insulating layer is not covered with the coating film; further comprising a structure located between the first portion and the insulating layer; The covering film is a light emitting device covering the structure. [Brief description of the drawings]

[0008] The above objects, as well as other objects, features and advantages, will become more apparent from the following preferred embodiments and the accompanying drawings.

[0009] [Figure 1] 1 is a cross-sectional view showing a configuration of a light emitting device according to an embodiment. [Diagram 2] FIG. 2 is a plan view of the light emitting device shown in FIG. [Diagram 3] 3 is a cross-sectional view of FIG. 2 taken along line B-B. [Figure 4] 1A to 1C are cross-sectional views for explaining a method for forming an area on a substrate that is not covered with a coating film. [Diagram 5] FIG. 1 is a plan view showing a configuration of a light emitting device according to a first embodiment. [Figure 6] FIG. 2 is a plan view for explaining a manufacturing method of the light emitting device according to the first embodiment. [Figure 7] FIG. 11 is a cross-sectional view showing the configuration of a light emitting device according to Example 2. [Figure 8] FIG. 11 is a plan view showing the configuration of a light emitting device according to Example 3. [Figure 9] FIG. 11 is a plan view showing the configuration of a light emitting device according to Example 4. [Figure 10] 10 is a diagram in which the second electrode and the partition wall are removed from FIG. [Figure 11] 10 is a cross-sectional view taken along CC in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In all the drawings, the same components are given the same reference numerals and the description will be omitted as appropriate.

[0011] Fig. 1 is a cross-sectional view showing the configuration of a light emitting device 10 according to an embodiment. Fig. 2 is a plan view of the light emitting device 10 shown in Fig. 1. Fig. 1 is a cross-sectional view taken along line AA in Fig. 2. Fig. 3 is a cross-sectional view taken along line BB in Fig. 2.

[0012] The light-emitting device 10 according to the embodiment is, for example, a lighting device or a display, and includes a substrate 100, an insulating layer 160, a light-emitting element 102, a coating film 140, and a structure 150. The insulating layer 160 is formed on one surface of the substrate 100, and has an opening 162. The light-emitting element 102 is formed in the opening 162. The coating film 140 is formed on the one surface of the substrate 100, and covers the light-emitting element 102, the insulating layer 160, and a part of the one surface of the substrate 100. Another part of the substrate 100 (for example, a part of an end portion: hereinafter, referred to as a first portion) is not covered by the coating film 140. The structure 150 is located between the first portion of the substrate 100 and the insulating layer 160. The coating film 140 also covers the insulating layer 160. The light-emitting element 102 is, for example, an organic EL element. This will be described in detail below.

[0013] The substrate 100 is a transparent substrate such as a glass substrate or a resin substrate. The substrate 100 may be flexible. In this case, the thickness of the substrate 100 is, for example, 10 μm or more and 1000 μm or less. Even in this case, the substrate 100 may be formed of either an inorganic material or an organic material. The substrate 100 is, for example, a polygon such as a rectangle. When the substrate 100 is a resin substrate, an inorganic material film such as a silicon oxide film is formed on the surface of the substrate 100 on which the light emitting element 102 is formed. This can prevent moisture and the like from penetrating the substrate 100 and reaching the light emitting element 102.

[0014] An insulating layer 160 is formed on the substrate 100. The insulating layer 160 has an opening 162. The light emitting element 102 is formed in the opening 162. In other words, the opening 162 defines an area in which the light emitting element 102 should be formed. The insulating layer 160 is made of a material such as polyimide, silicon oxide, or silicon nitride.

[0015] The light-emitting element 102 has a configuration in which an organic layer 120 is sandwiched between a first electrode 110 and a second electrode 130. At least one of the first electrode 110 and the second electrode 130 is a light-transmitting electrode. The remaining electrodes are formed of a metal layer made of a metal selected from a first group consisting of Al, Mg, Au, Ag, Pt, Sn, Zn, and In, or an alloy of a metal selected from this first group. The material of the light-transmitting electrode is, for example, an inorganic material such as ITO (Indium Tin Oxide) or IZO (Indium Zinc Oxide), a conductive polymer such as a polythiophene derivative, or a mesh-like electrode using nanowires made of silver or carbon. For example, in the case of a bottom-emission type light-emitting element 102 having a configuration in which the first electrode 110, the organic layer 120, and the second electrode 130 are laminated in this order on the substrate 100, the first electrode 110 is a light-transmitting electrode, and the second electrode 130 is an electrode that reflects light, such as Al. Furthermore, in the case of a top-emission type light-emitting element 102 having a configuration in which a first electrode 110, an organic layer 120, and a second electrode 130 are laminated in this order on a substrate 100, the first electrode 110 is an electrode that reflects light, such as Al, and the second electrode 130 is an electrode that is transparent. In addition, both electrodes (the first electrode 110, the second electrode 130) may be transparent electrodes to form a transparent light-emitting device (dual emission type).

[0016] The organic layer 120 has a structure in which, for example, a hole transport layer, a light emitting layer, and an electron transport layer are laminated in this order. A hole injection layer may be formed between the hole transport layer and the first electrode 110. Also, an electron injection layer may be formed between the electron transport layer and the second electrode 130. The layers of the organic layer 120 may be formed by a coating method or a vapor deposition method, or may be formed partly by the coating method and the rest by the vapor deposition method. The organic layer 120 may be formed by a vapor deposition method using a vapor deposition material, or may be formed by an ink jet method, a printing method, or a spray method using a coating material.

[0017] Terminals 112 and 132 are formed on the surface of the substrate 100 on which the light emitting element 102 is formed. The terminal 112 is electrically connected to the first electrode 110, and the terminal 132 is electrically connected to the second electrode 130. In detail, the organic layer 120 is not formed on a part of the first electrode 110, and the part is located outside the insulating layer 160. This part serves as the terminal 112. The terminal 132 has the same layer as the first electrode 110. In the example shown in the figure, the terminal 112 is connected to the first electrode 110 via the wiring 116, and the terminal 132 is connected to the second electrode 130 via the wiring 136. Both the wirings 116 and 136 have the same layer as the first electrode 110.

[0018] In the example shown in the figure, the terminal 112 has a configuration in which the second layer 114 is laminated on the first electrode 110. The terminal 132 has a configuration in which the second layer 134 is laminated on the same layer as the first electrode 110. The second layers 114, 134 are formed of a material, such as a metal, that has a lower resistance than the material forming the first electrode 110. The second layers 114, 134 have a configuration in which, for example, Mo, Al, and Mo are laminated in this order. Note that other metals may be added to Mo and Al. Note that the second layers 114, 134 may also be formed on at least a part of the wirings 116, 136. However, the second layers 114, 134 may not be formed on the terminals 112, 132.

[0019] The coating film 140 is formed by a film forming method, for example, the ALD method or the CVD method. When the coating film 140 is formed by the ALD method, the coating film 140 is formed by a metal oxide film such as aluminum oxide, and the thickness is, for example, 10 nm to 200 nm, preferably 50 nm to 100 nm. When the coating film 140 is formed by the CVD method, the coating film 140 is formed by an inorganic insulating film such as a silicon oxide film, and the thickness is, for example, 0.1 μm to 10 μm. By providing the coating film 140, the light emitting element 102 is protected from moisture and the like. The coating film 140 may be formed by a sputtering method. In this case, the coating film 140 is formed by an insulating film such as SiO2 or SiN. In this case, the thickness is 10 nm to 1000 nm.

[0020] The above-mentioned terminals 112, 132 are formed near the edge of the substrate 100. The coating film 140 is not formed on the portion of the edge of the substrate 100 that is located near the terminals 112, 132. Therefore, the terminals 112, 132 are not covered with the coating film 140. A structure 150 is formed between the portion of the substrate 100 that is not covered with the coating film 140 and the insulating layer 160. In the example shown in the figure, the structure 150 is formed between the terminal 112 and the insulating layer 160, and between the terminal 132 and the insulating layer 160.

[0021] The structure 150 is formed of an insulating material such as a resin or an inorganic material. When the structure 150 is formed of a photosensitive material, the structure 150 is formed by applying the material onto the substrate 100 to form a layer, and then exposing and developing the layer. When the structure 150 is formed of an inorganic material, the structure 150 is formed by forming a layer that will become the structure 150 by a CVD method or a sputtering method, and then selectively removing the layer.

[0022] The structure 150 extends in a first direction (Y direction in FIG. 2). In the first direction, the structure 150 is longer than the insulating layer 160. In the example shown in the figure, the structure 150 is formed so as to cross the wiring 116 or the wiring 136. Therefore, the lower surface of the structure 150 has a portion in contact with the substrate 100 and a portion in contact with the wiring 116 or the wiring 136.

[0023] 3, in the vicinity of the portion where the bottom surface of the structure 150 is in contact with the substrate 100, the coating film 140 is in contact with the substrate 100 at a portion of the substrate 100 located between the structure 150 and the terminal 112 (second portion) and at a portion of the substrate 100 located between the structure 150 and the insulating layer 160 (third portion). When the coating film 140 is made of an inorganic material, the bond between the substrate 100 and the coating film 140 is stronger than the bond between the coating film 140 and the insulating layer 160 because it is a bond between inorganic materials.

[0024] Next, a method for manufacturing the light emitting device 10 will be described. First, the first electrode 110 and the terminals 112, 132 are formed on the substrate 100. The first electrode 110 and the terminals 112, 132 are formed using, for example, a vapor deposition method or a sputtering method. Next, an insulating layer 160 is formed so as to cover the periphery of the first electrode 110 (see FIG. 2). Next, an organic layer 120 is formed on the first electrode 110. Also, a structure 150 is formed.

[0025] Next, the second electrode 130 is formed, and then the covering film 140 is formed. The second electrode 130 is formed by using, for example, a sputtering method or a vapor deposition method, and the covering film 140 is formed by using, for example, an ALD method or a CVD method.

[0026] FIG. 4 is a cross-sectional view for explaining a method for forming an area of ​​the substrate 100 that is not covered by the coating film 140. As described above, the coating film 140 does not cover the terminals 112, 132. In order to achieve this, for example, before forming the coating film 140, the area of ​​the substrate 100 where the terminals 112, 132 are formed is covered with a lift-off layer 200. The lift-off layer 200 is formed of, for example, an organic material. The glass transition temperature or phase transition temperature (e.g., melting point) of the lift-off layer 200 is lower than the glass transition temperature or phase transition temperature (e.g., melting point) of the coating film 140. Note that the linear expansion coefficient of the material constituting the lift-off layer 200 is preferably larger than the linear expansion coefficient of the material constituting the coating film 140.

[0027] Then, after coating film 140 is formed, substrate 100 is heated and cooled. At this time, cracks occur in the portion of coating film 140 located above lift-off layer 200. When the vicinity of terminals 112 and terminals 132 is washed with a solution that dissolves lift-off layer 200, the solution comes into contact with lift-off layer 200 through the cracks generated in coating film 140, and lift-off layer 200 is removed. At this time, the portion of lift-off layer 200 located above lift-off layer 200 is removed.

[0028] Cracks may occur at the end of the coating film 140. These cracks occur, for example, during the process of removing the lift-off layer 200 described above, or when connecting a conductive member such as an anisotropic conductive film, a lead terminal, or a bonding wire to the terminals 112 and 132. When a crack occurs at the end of the coating film 140, the crack advances toward the light-emitting element 102. In contrast, in this embodiment, a structure 150 is formed between the region of the substrate 100 where the coating film 140 is not formed and the insulating layer 160. The structure 150 extends in a first direction (y direction in FIG. 2), thereby changing a crack that advances in a second direction (x direction in FIG. 2) intersecting the first direction to the first direction. This makes it possible to prevent a crack that occurs in the coating film 140 from advancing to the light-emitting element 102. This makes it possible to prevent gas (e.g., oxygen) and moisture that deteriorate the light-emitting element from reaching the light-emitting element.

[0029] In particular, if the outer side surface of the insulating layer 160 (i.e., the side surface opposite to the opening 162) is inclined in the direction in which the bottom surface of the insulating layer 160 widens, when a crack in the coating film 140 reaches the edge of the insulating layer 160, moisture, gas, and the like will immediately progress through the insulating layer 160 to the light emitting element 102. Even in such a case, since the structure 150 is provided in this embodiment, it is possible to suppress deterioration of the light emitting element 102 caused by a crack occurring in the coating film 140. In other words, the sealing performance of the light emitting device 10 can be maintained.

[0030] Furthermore, a crack that has reached the structure 150 may progress in the direction in which the structure 150 extends. Even in this case, in the example shown in the figure, the length of the structure 150 is greater than the width of the insulating layer 160 in the first direction (Y direction in FIG. 2). Even if a crack that has been redirected in the second direction (x direction in FIG. 2) progresses along the length of the structure 150, the length of the structure 150 is greater than the width of the insulating layer 160, so that the crack that has occurred in the coating film 140 can be further prevented from progressing to the insulating layer 160.

[0031] Furthermore, the coating film 140 contacts the substrate 100 at a portion (second region) of the substrate 100 located between the structure 150 and the terminal 112, and at a portion (third region) located between the structure 150 and the insulating layer 160. For this reason, cracks in the coating film 140 are less likely to progress in the second and third regions. This further prevents a crack generated in the coating film 140 from reaching the insulating layer 160 and causing deterioration of the light emitting element 102 due to gas or moisture penetrating through the crack. EXAMPLES

[0032] Example 1 Fig. 5 is a plan view showing the configuration of the light emitting device 10 according to Example 1, and corresponds to Fig. 2 in the embodiment. The light emitting device 10 according to this example has the same configuration as the light emitting device 10 according to the embodiment, except for the following points.

[0033] First, the edge of the coating film 140 is located inside the edge of the substrate 100 over the entire periphery. The structure 150 surrounds the insulating layer 160 over the entire periphery.

[0034] FIG. 6 is a plan view for explaining a manufacturing method of the light emitting device 10 according to this embodiment. In this embodiment, a plurality of light emitting devices 10 are simultaneously formed with the substrates 100 connected to each other. Then, after the coating film 140 is formed, the plurality of light emitting devices 10 are separated from each other using a dicing blade or the like. As an example, if the coating film 140 is formed on the scribe line 12, there is a possibility that a large crack will occur in the coating film 140 when the light emitting devices 10 are separated from each other. For this reason, it is preferable that the coating film 140 is formed away from the scribe line 12 over the entire circumference. Specifically, before forming the coating film 140, a lift-off layer 200 is applied to the scribe line 12 and its vicinity.

[0035] Here, the structure 150 is formed so as to surround the entire periphery of the insulating layer 160. Therefore, even if a crack occurs in any part of the edge of the coating film 140, deterioration of the light emitting element 102 due to this crack can be suppressed.

[0036] Example 2 Fig. 7 is a cross-sectional view showing the configuration of the light emitting device 10 according to Example 2, and corresponds to Fig. 3 in the embodiment. The light emitting device 10 according to this example has the same configuration as the light emitting device 10 according to the embodiment or Example 1, except for the cross-sectional shape of the structure 150.

[0037] In this embodiment, in a cross section of the structure 150 in the width direction (second direction), the upper surface of the structure 150 is wider than the lower surface of the structure 150. Specifically, the cross section of the structure 150 is a trapezoid whose upper base is longer than its lower base. Such a structure can be realized by controlling the conditions for forming the structure 150 (for example, the exposure conditions when the structure 150 is formed of a photosensitive material).

[0038] This embodiment also makes it possible to prevent cracks occurring at the edge of the coating film 140 from reaching the light emitting element 102. In addition, since the side surface of the structure 150 is inclined in a direction in which the width of the structure 150 increases toward the top, it becomes easier for the cracks to change course from the first direction (y direction in FIG. 2) to the second direction (x direction in FIG. 2). Therefore, deterioration of the light emitting element 102 due to cracks occurring at the edge of the coating film 140 can be prevented.

[0039] Example 3 Fig. 8 is a plan view showing the configuration of the light emitting device 10 according to Example 3. The light emitting device 10 according to this example has the same configuration as the light emitting device 10 according to Example 1, except for the following points. Note that, for the sake of explanation, the second electrode 130 and the terminal 132 are not shown in Fig. 8.

[0040] In this embodiment, the light emitting device 10 has a plurality of light emitting elements 102. An insulating layer 160 is formed between adjacent light emitting elements 102. Terminals 112 are formed to electrically connect to each of the plurality of light emitting elements 102. The plurality of terminals 112 are arranged side by side on the edge of the substrate 100. All of the terminals 112 are exposed from the coating film 140. The structure 150 surrounds the entire periphery of the region in which the plurality of light emitting elements 102 are formed. The cross-sectional shape of the structure 150 may be the same as that of the second embodiment.

[0041] The terminal 132 is arranged in the same manner as the terminal 112.

[0042] This embodiment also makes it possible to prevent cracks occurring at the edge of the coating film 140 from reaching the light emitting element 102.

[0043] Example 4 Fig. 9 is a plan view showing the configuration of the light emitting device 10 according to Example 4. Fig. 10 is a view in which the second electrode 130 and the partition wall 135 have been removed from Fig. 9. In Fig. 10, the second electrode 130 is shown by a dotted line for the sake of explanation. Fig. 11 is a cross-sectional view taken along CC in Fig. 10. Fig. 10 corresponds to Fig. 8 in Example 3. The light emitting device 10 according to this example has the same configuration as the light emitting device 10 according to Example 3, except for the following points.

[0044] In this embodiment, the light emitting device 10 is a display and has a plurality of light emitting elements 102 arranged in a matrix. The structure 150 surrounds the plurality of light emitting elements 102. The cross-sectional shape of the structure 150 may be the same as that of the second embodiment.

[0045] In detail, a plurality of first electrodes 110 extend parallel to each other, and a plurality of second electrodes 130 extend parallel to each other and in a direction intersecting (for example, a direction perpendicular to) the first electrodes 110. A light emitting element 102 is formed at each of the intersections of the first electrodes 110 and the second electrodes 130. Specifically, an insulating layer 160 is formed straddling the plurality of first electrodes 110. An opening is formed in the insulating layer 160 at a portion located at the intersection of the first electrodes 110 and the second electrodes 130. An organic layer 120 is provided in this opening. That is, the light emitting element 102 is formed in the opening of the insulating layer.

[0046] The terminal 112 is electrically connected to each of the multiple first electrodes 110, and the terminal 132 is electrically connected to each of the multiple second electrodes 130. The multiple terminals 112, 132 are both arranged along the edge of the substrate 100. In the example shown in the figure, the multiple terminals 112, 132 are both arranged along the same side of the substrate 100. However, the terminals 112 and 132 may be arranged along different sides of the substrate 100.

[0047] Moreover, a partition wall 135 is formed on the insulating layer 160. The partition wall 135 is located between the second electrodes 130. The cross section of the partition wall 135 is a trapezoid whose upper base is longer than its lower base. A conductive layer made of the same material as the second electrodes 130 is formed on the upper surface of the partition wall 135. The partition wall 135 is provided to separate the adjacent second electrodes 130 from each other when the second electrodes 130 are formed by a vapor deposition method or a sputtering method. For this reason, the partition wall 135 is formed after the insulating layer 160 is formed and before the partition wall 135 is formed (preferably before the organic layer 120 is formed).

[0048] In this embodiment, the structure 150 is formed in the same process as the partition wall 135. Therefore, the structure 150 is formed from the same material as the partition wall 135, and the cross section of the structure 150 is also a trapezoid whose upper base is longer than its lower base. The structure 150 and the partition wall 135 are formed from, for example, a photosensitive material, and are formed into the above-mentioned cross-sectional shape by controlling the exposure conditions.

[0049] This embodiment also makes it possible to prevent cracks occurring at the edge of the coating film 140 from reaching the light emitting element 102. Moreover, since the structure 150 is formed in the same process as the partition wall 135, the number of manufacturing processes for the light emitting device 10 can be reduced. As a result, the manufacturing cost of the light emitting device 10 can be reduced. Since the cross-sectional shape of the structure 150 is trapezoidal, it becomes easier to change the progression direction of the crack (from the first direction to the second direction).

[0050] Although the embodiment and examples have been described above with reference to the drawings, these are merely examples of the present invention, and various configurations other than those described above can also be adopted.

Claims

[Claim 1] A substrate having an inorganic film; an insulating layer overlying the substrate and having an opening; a light emitting element located in the opening; a coating film located on the substrate and covering the light emitting element, the insulating layer, and a part of the substrate; A plurality of wirings electrically connected to the light emitting element; Equipped with a first portion of the substrate that is a part of an area not covered with the insulating layer is not covered with the coating film; further comprising a structure located between the first portion and the insulating layer; the coating film covers the structure and the plurality of wirings and is in contact with the inorganic film between the plurality of wirings; Further, a terminal is located along at least a first side of the substrate and electrically connected to the wiring, When the substrate is viewed from the surface on which the light emitting element is located, the plurality of wirings are arranged between a second side of the substrate, which is different from the first side, and the light emitting element, in a direction from the second side of the substrate to the light emitting element; A light-emitting device, in which, in the direction in which the light-emitting element is located from the second side of the substrate, an end of the coating film is located on the second side of the wiring that is farthest from the light-emitting element among the multiple wirings between the second side of the substrate and the light-emitting element, and is located away from the second side of the substrate.

Citation Information

Patent Citations

  • Display device and method of manufacturing the same

    CN104900675A

  • Luminescence equipment and its producing method

    JP2002093576A

  • Luminescence equipment and its producing method

    JP2002093586A

  • Display device

    JP2006054111A

  • Organic light-emitting device and its manufacturing method

    JP2009049001A