Sensor element and odor measurement device
The sensor element with a resin composition and odorant-permeable layer addresses the challenges of sensitivity and responsiveness in chemiresistor sensors by improving odorant detection accuracy and speed.
Patent Information
- Application Number
- JP2024082769
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-25
- Filing Date
- 2024-05-21
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2044-05-21
AI Technical Summary
Conventional chemiresistor type odor sensors face challenges in achieving simultaneous improvements in sensitivity to low-concentration odorants, measurement accuracy in repeated measurements, and responsiveness to changes in odorant concentration, as extending measurement time enhances sensitivity but reduces responsiveness, while shortening measurement time decreases sensitivity.
A sensor element with an odorant-receiving layer containing a resin composition and a filler, separated metal wirings, and an odorant-permeable layer made of R1-SiO 3/2 and R2-SiO 1 structures, which allows for improved odorant permeation and protection, enhancing sensitivity and responsiveness.
The sensor element achieves improved sensitivity to low-concentration odorants, enhanced measurement accuracy in repeated measurements, and increased responsiveness by optimizing the odorant-receiving layer composition and structure.
Smart Images

Figure 2024169365000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an odor measuring device. [Background technology]
[0002] With recent developments in information processing technology, if it were possible to somehow quantify the sense of smell, which is one of the five human senses that cannot be adequately measured mechanically, it is expected that this technology could be used in a wide range of industrial fields, including the medical field, the environmental field, the field of biogas utilization, the field of safety, the field of food, and the field of marketing. Such technology relating to the sense of smell can be used for a variety of purposes, for example, as follows: Medical field: Nursing care, assistance, preventive diagnosis and disease testing, etc. ·Environmental field: Odor control in factories, etc. - Biogas utilization: Fermentation process management, wastewater treatment management, etc. Safety field: Predicting landslides and floods, detecting deterioration of engine oil and machine operating oil, etc. Food industry: Detection of the maturity state of plants (e.g. vegetables and grains) and meat, process management of fermented foods such as alcoholic beverages, plant cultivation management, and quality control during the production, storage, and distribution of food. Marketing field: Cosmetics, body odor countermeasures, scented environments, product scent production, etc.
[0003] The invention described in Patent Document 1 proposes a mechanism for detecting the adsorption of odor components on the surface of a conductive polymer by replacing the semiconductor of a semiconductor gas sensor with a conductive polymer. Patent Document 1 reports that it is possible to detect odor components that are easily thermally decomposed and substances that do not cause an oxidation-reduction reaction on the surface of the detection part of the sensor.
[0004] Patent Document 2 also focuses on the property that the electrical resistance of a mixture of an organic polymer and a conductive material changes when exposed to an organic gas. Patent Document 2 describes that when a plurality of combinations of organic polymer / conductive material in which the organic polymer composition is different from that of the above mixture is prepared and these are used as an electrical resistance array in a sensor, the electrical resistance changes when exposed to the same organic gas are different for each combination. Patent Document 2 reports that this can be used to identify odors by attributing the pattern of electrical resistance changes to the type of odor (= organic gas mixture).
[0005] Furthermore, Patent Document 3 reports that the response speed of the sensor is improved by adding a plasticizer to the above organic polymer. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Japanese Patent Application Publication No. 11-23508 [Patent Document 2] Special Publication No. 11-503231 [Patent Document 3] Patent Publication No. 2002-519633 Summary of the Invention [Problem to be solved by the invention]
[0007] In the case of an odor measuring device equipped with a chemiresistor type odor sensor, the change in electrical conductivity of the odorant receiving layer caused by the volume change caused by the odorant adsorbing the odorant is detected as an electrical signal to measure the odorant. In an odor measuring device equipped with a chemiresistor type odor sensor, in order to improve the measurement sensitivity for low concentrations of odorants, a method of simply extending the measurement time may be adopted. However, if the measurement time per measurement is extended, the responsiveness to the concentration change of the odorant decreases. In order to maintain the responsiveness to the concentration change of the odorant, a method of shortening the measurement time per measurement may be adopted. However, if this method is adopted, the measurement sensitivity to low concentrations of odorants decreases. Thus, in an odor measuring device equipped with a conventional chemiresistor type odor sensor, it was difficult to simultaneously achieve an improvement in sensitivity for measuring low concentrations of odorants and an improvement in measurement accuracy and responsiveness to the concentration change of the odorant in repeated measurements.
[0008] An object of one aspect of the present invention is to provide a sensor element or the like that realizes improved sensitivity to low concentration components in odor measurement, improved measurement accuracy in repeated measurements, and improved responsiveness. [Means for solving the problem]
[0009] One aspect of the present invention is an odorant receiving layer comprising a resin composition including a resin (A) and a filler (B), a first metal wiring in contact with at least a portion of the odorant receiving layer, a second metal wiring spaced apart from the first metal wiring and in contact with at least a portion of the odorant receiving layer, and an odorant permeation layer covering at least a portion of the odorant receiving layer opposite the side in contact with the first metal wiring and the second metal wiring, wherein the odorant permeation layer is made of R1-SiO 3 / 2 and R2-SiO 1 wherein R1 is a hydrocarbon group having 1 to 18 carbon atoms; and an odor measuring device including a plurality of such sensor elements. Effect of the Invention
[0010] According to one aspect of the present invention, it is possible to provide a sensor element that realizes improved sensitivity to low concentration components in odor measurement, improved measurement accuracy by enabling repeated measurements in a short measurement time, and improved responsiveness. [Brief description of the drawings]
[0011] [Figure 1] 1 is a schematic diagram showing an example of the configuration of an odor sensor according to one embodiment of the present invention. [Diagram 2] This is an SEM image of a cross section of a sensor element. [Diagram 3] FIG. 2 is a top view showing an example of the configuration of a sensor element. [Figure 4] 4 is a cross-sectional view showing an example of the configuration of the sensor element shown in FIG. 3. [Diagram 5] 1 is a schematic diagram showing an example of the configuration of an odor measurement device according to one embodiment of the present invention. [Figure 6] 1 is a functional block diagram showing an example of the configuration of an odor measurement device. [Figure 7] 11 is a flowchart showing an example of a process flow in which the estimation device generates an estimation model. [Figure 8] 1 is a functional block diagram showing an example of the configuration of an odor measurement device. [Figure 9] 11 is a flowchart showing an example of a process flow in which the estimation device estimates an odor substance. [Figure 10] FIG. 2 is a top view showing an example of the configuration of a sensor element of the present invention. [Figure 11] FIG. 2 is a top view showing an example of the configuration of a sensor element of the present invention. [Figure 12] FIG. 2 is a perspective view showing an example of the configuration of a sensor element of the present invention. [Figure 13] 13 is a graph for explaining an operation for determining Tz. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] An embodiment of the present invention will be described below, but the present invention is not limited thereto. In addition, unless otherwise specified in this specification, "A to B" representing a numerical range means "A or more and B or less."
[0013] [1. Sensor element 31] As a result of investigations aimed at achieving the above object, the present inventors arrived at the present invention.
[0014] The sensor element 31 for an odor measuring device according to one embodiment of the present invention is a chemiresistor type odor sensor. The sensor element 31 includes an odorant receiving layer 315 containing a resin composition, a first metal wiring 313A and a second metal wiring 313B each in contact with at least a portion of the odorant receiving layer 315, and an odorant permeable layer 317. Here, the resin composition includes a resin (A) and a filler (B). The first metal wiring 313A is spaced apart from the second metal wiring 313B.
[0015] The odorant permeation layer 317 covers at least a portion of the odorant receiving layer 315 on the side opposite to the side in contact with the first metal wiring 313A and the second metal wiring 313B. The odorant permeation layer 317 is not in contact with the first metal wiring 313A and the second metal wiring 313B. The odorant permeation layer 317 is made of R1-SiO 3 / 2 and R2-SiO 1 The odorant permeation layer 317 includes a composition having at least one of the structures represented by the formula: where R1 and R2 are hydrocarbon groups having 1 to 18 carbon atoms bonded to a silicon atom (Si). For example, the odorant permeation layer 317 may be provided so as to completely cover the side of the odorant receiving layer 315 opposite to the side in contact with the first metal wiring 313A and the second metal wiring 313B. The odorant permeation layer 317 and the odorant receiving layer 315 are in contact with each other on a surface other than the surface including the contact surface of the odorant receiving layer 315 with the first metal wiring 313A and the second metal wiring 313B. The odorant permeation layer 317 is not in contact with the first metal wiring 313A and the second metal wiring 313B.
[0016] [2-1. Odor-permeable layer] The odorant permeable layer 317 of the sensor element 31 is made of R1-SiO 3 / 2 and R2-SiO 1 The odorant-permeable layer 317 includes a composition having at least one of the structures represented by R1-SiO 3 / 2 and R2-SiO 1 In the case where the odorant-permeable layer 317 includes both of the structures represented by R2-SiO 1 When the odorant-permeable layer 317 does not include the structure represented by R1-SiO, the odorant-permeable layer 317 becomes hard, the time required for the odorant to desorb is shortened, and the measurement speed is improved. 3 / 2 and R2-SiO 1 The mixing ratio of R1-SiO 3 / 2 :R2-SiO 1=0.9:0.1-0.7:0.3. Here, R1 is a hydrocarbon group having a carbon number of 1 or more and 18 or less. In the present invention, a hydrocarbon group is a group consisting of carbon atoms and hydrogen atoms. From the viewpoint of solubility during slurry preparation, the carbon number of R1 is preferably 1 or more and 12 or less, more preferably 1 or more and 10 or less, even more preferably 1 or more and 8 or less, and even more preferably 1 or more and 6 or less. Here, R1 may contain one or more functional groups selected from aliphatic hydrocarbon groups and aromatic groups, and more preferably contains a methyl group and / or an aromatic group. This improves the adhesion between the odorant permeation layer and the odorant reception layer, so that the sensor element 31 can obtain a characteristic with excellent accuracy in repeated measurements. Therefore, the sensor element 31 having the odorant permeation layer 317 according to the present disclosure can achieve both high measurement accuracy and high responsiveness in repeated measurements. Here, the responsiveness refers to the time until the next measurement can be performed continuously using the same sensor element 31 after a measurement using the sensor element 31. The sensor element 31 according to the present disclosure can perform multiple measurements in a shorter time. Examples of the aliphatic hydrocarbon group include "alkyl groups having 1 to 18 carbon atoms". The "alkyl groups having 1 to 18 carbon atoms" may be linear or branched. Examples of linear alkyl groups include methyl, ethyl, propyl, butyl, hexyl, heptyl, octyl, nonyl, decyl, dodecyl, tridecyl, tetradecyl, pentadecyl, hexadecyl, heptadecyl, and octadecyl. Examples of branched alkyl groups include isopropyl, sec-butyl, tert-butyl, isobutyl, isopentyl, tert-pentyl, 2-hexyl, 3-hexyl, 2-heptyl, 3-heptyl, isoheptyl, tert-heptyl, isooctyl, tert-octyl, 2-ethylhexyl, and isononyl. Examples of the aromatic group having 6 to 18 carbon atoms include a phenyl group, an indenyl group, a naphthyl group, a biphenylyl group, a fluorenyl group, a phenanthrenyl group, and an anthracenyl group.R2 may contain one or more functional groups selected from the group consisting of a hydrogen atom, a methyl group, an alkyl group having 1 to 12 carbon atoms, an amino group, a hydroxyl group, a carboxyl group, a fluoromethyl group, a polyester group, a polyether group, an amide group, and an aralkyl group having 1 to 12 carbon atoms.
[0017] It is preferable that R2 contains one or more functional groups selected from the group consisting of a carboxyl group, an amide group, an alkyl group, and a fluoromethyl group. In particular, it is preferable that R2 contains one or more functional groups selected from the group consisting of a hydrogen atom, an amide group, a methyl group, an alkyl group having 1 to 12 carbon atoms, an aralkyl group having 1 to 12 carbon atoms, a carboxyl group, and a fluoromethyl group. When R2 contains the above-mentioned functional group, the degree to which R2 inhibits the gas permeability specific to silicone is reduced. When the odorant permeable layer 317 contains the above-mentioned R2, Tz, which is the time from the completion of one measurement to the time when the next measurement can be performed, tends to be shortened. Therefore, when the odorant permeable layer 317 contains the above-mentioned R2, a permeable layer with excellent characteristics can be realized.
[0018] The odorant permeable layer 317 containing this composition may be a layer having the function of selectively allowing the odorant to reach the odorant receiving layer 315. The odorant permeable layer 317 may also function as a protective layer that reduces the rate at which the odorant receiving layer 315 deteriorates due to the humidity of the measurement environment.
[0019] The odorant permeable layer 317 may be a thin film having a thickness of 0.1 μm or more and 50 μm or less, with the lower limit of the thickness being more preferably 0.5 μm or more and the upper limit of the thickness being more preferably 20 μm or less. The thickness of the odorant permeable layer 317 may be within the above numerical range throughout the entire odorant permeable layer 317, or the average value of the entire thickness of the odorant permeable layer 317 may be within the above numerical range. When creating the odorant permeable layer 317, the area of the film to be coated is regulated by the electrode shape, etc., and the evaporation residue of the solution of the odorant permeable layer to be dispensed and the dispensed amount are controlled to control the thickness of the odorant permeable layer 317. The odorant that has permeated the odorant permeable layer 317 can reach the odorant receiving layer 315, but the odorant that cannot permeate the odorant permeable layer 317 cannot reach the odorant receiving layer 315. If the thickness of the odorant permeable layer 317 is excessively thick, less odorant reaches the odorant receiving layer 315, resulting in a decrease in measurement sensitivity. Furthermore, if the odorant permeation layer 317 inhibits the volume change of the odorant reception layer 315, the change in electrical conductivity of the odorant reception layer 315 caused by the odorant reception layer 315's adsorption will be small, and the measurement sensitivity will decrease. On the other hand, if the odorant permeation layer 317 is not thick enough, most of the odorant will reach the odorant reception layer 315. Therefore, the odorant permeation layer 317 cannot fully perform the function of selectively allowing the odorant to reach the odorant reception layer 315. Furthermore, an odorant permeation layer 317 that is not thick enough cannot fully protect the odorant reception layer 315. Therefore, it is preferable that the thickness of the odorant permeation layer 317 of the sensor element 31 according to the present invention is within the above-mentioned range.
[0020] <Method for measuring the thickness of the odorant permeable layer 317> The method for measuring the thickness of the odorant permeation layer 317 will be described below with reference to FIG. 2. FIG. 2 is a scanning electron microscope (SEM) image of the cross section of the sensor element 31 including the odorant reception layer 315 and the odorant permeation layer 317, observed at 25,000 times magnification. The cross section of the sensor element 31 including the odorant reception layer 315 and the odorant permeation layer 317 is formed, for example, using a cross-section polisher, specifically IB-19530CP (product name manufactured by JEOL Ltd.). The lines indicated by symbols L1 to L20 in FIG. 2 indicate the length from the boundary between the odorant reception layer 315 and the odorant permeation layer 317 at each location to the surface of the odorant permeation layer 317. Hereinafter, the length from the boundary between the odorant reception layer 315 and the odorant permeation layer 317 to the surface of the odorant permeation layer 317 is referred to as the cross-sectional length of the odorant permeation layer 317. The boundary between the odorant receiving layer 315 and the odorant permeable layer 317 can be determined, for example, using SEM reflection observation, electron image SEM-EDX, or STEM.
[0021] The thickness of the odorant-permeable layer 317 may be the average value of the cross-sectional length at multiple points of the odorant-permeable layer 317. The measurement points of the cross-sectional length that are the calculation basis for the thickness of the odorant-permeable layer 317 may be two points, the thickest and the thinnest, or may be 10 points arbitrarily selected from the odorant-permeable layer 317, or may be even more. As an example, the average value of the cross-sectional lengths at 20 points indicated by symbols L1 to L20 in the example shown in FIG. 2 may be the thickness of the odorant-permeable layer 317. The thickness of the odorant-permeable layer 317 may be the average value of the cross-sectional lengths at multiple points that fall within the above-mentioned numerical range.
[0022] [2-2. Odor Receptor Layer] The odorant receiving layer 315 of the sensor element 31 includes a resin composition containing a resin (A) and a filler (B). This resin composition may further include a surfactant (C). This resin composition is applied onto a sensor element substrate, heated and dried to a dry solid, and then used as the odorant receiving layer 315. The resin (A), filler (B), and surfactant (C) will be described later with specific examples.
[0023] <Resin composition> In this specification, "odor substance" refers in a broad sense to a substance that can be adsorbed to the odor substance receiving layer 315. Therefore, it also includes substances that are not generally considered to be the cause of odor. "Odor" often contains multiple odor substances that cause it, and there are also substances that are not recognized as odor substances or unknown odor substances. One embodiment of the present invention focuses on the fact that the amount of odor substance adsorbed to the odor substance receiving layer 315 varies depending on the type of odor substance.
[0024] In addition, even when the term "odor substance" is simply used in this specification, it may mean a "collection of odor substances" that may contain multiple odor substances, rather than an individual odor substance.
[0025] Examples of "odor substances" include, but are not limited to, hexane, ethyl acetate, methanol, diethyl carbonate, toluene, d-limonene, bornan-2-one, cis-3-hexenol, β-phenylethyl alcohol, citral, L-carvone, γ-undecalactone, eugenol, linalyl acetate, menthol, benzaldehyde, vanillin, hexanal, ethanol, pentyl valerate, linalool, and 2-propanol.
[0026] In addition, in this specification, the term "odor substance receiving layer" refers to a layer that adsorbs the odor substance to be recognized. The odor substance receiving layer 315 is formed from the above-mentioned resin composition. The odor substance receiving layer 315 can be provided as a part of the sensor element 31 described below.
[0027] It is believed that the sensor described in the cited document 1 can detect odors consisting of single compounds. On the other hand, many odors are mixtures of multiple substances. The sensor described in the cited document 1 does not have a function to distinguish odor components in the detection unit, so the odor discrimination performance for mixtures is insufficient. In the cited document 2, it is shown that it is possible to recognize odors as mixtures by making the response of the detection unit to various compounds different through each conductive polymer by utilizing the difference in the chemical structure of the conductive polymer used in the detection unit. However, the chemical structure of the conductive polymer is limited, and it is difficult to separate the response of the detection unit to any odor component with high sensitivity, and it is difficult to distinguish between odors consisting of similar components. In the cited document 3, a method is proposed in which a mixture consisting of an organic polymer, a plasticizer, and a conductive substance is used as a detection material in the detection unit, and the penetration of odor components into the organic polymer is detected as a change in the electrical resistance of the mixture. By utilizing the fact that the odor components that penetrate are different when organic polymers of different compositions are used, it is possible to recognize odors as mixtures by using multiple detection units consisting of the above detection material containing organic polymers of different compositions in parallel to form an array. However, in the case of the above organic polymers and organic polymers containing plasticizers, even if multiple combinations of organic polymers and conductive materials are prepared, the difference in chemical properties between the organic polymers is small, so the odor discrimination performance is insufficient. These conventional techniques cannot accurately detect, for example, real odor patterns in which multiple substances interact with each other or real odor patterns caused by substances with unknown compositions.
[0028] The electrical conductivity of the resin composition described above changes depending on the amount of odorant adsorbed to the resin composition. In addition, the adsorption process of odorants to the resin composition described above differs for each odorant. Therefore, by using such a resin composition, the sensor element 31 according to one embodiment of the present invention can improve the odor discrimination performance. For example, it can discriminate a real odor pattern in which multiple substances interact with each other or a real odor pattern caused by a substance whose composition is unknown.
[0029] <Resin (A)> The resin (A) contained in the resin composition according to one embodiment of the present invention is not particularly limited, and may be a urethane resin, a polyalkylene oxide, an acrylic resin, a fluorine-containing resin, a vinyl polymer resin (e.g., polyvinylpyrrolidone, polyvinyl butyral, etc.), a silicone resin, a polyamide resin, a polypropylene resin, paraffin wax, a polyester resin, etc. However, the resin (A) may be R-SiO n (n is 1 or more and 3 / 2 or less) is not included.
[0030] <Filler (B)> The resin composition according to one embodiment of the present invention contains a filler (B). In this specification, the filler (B) is a conductive carbon material, more specifically, a carbon material having a volume resistivity of 0.1 Ω·cm or less. The above-mentioned resin composition is in a state in which the filler (B) is dispersed in the resin (A). The fillers (B) come into contact with each other to form a conductive path, which makes the resin composition conductive.
[0031] Examples of the filler (B) include conductive carbon materials such as carbon black, carbon nanotubes, and graphene, pigments, silica, and metal powders.
[0032] Commercially available carbon black products include Ketjen Black EC (trade name manufactured by Akzo Co., Ltd., Netherlands), Ketjen Black EC-300J (trade name manufactured by Lion Specialty Chemicals Co., Ltd.), Ketjen Black EC-600JD (trade name manufactured by Lion Specialty Chemicals Co., Ltd.), Seast G116, 116 (trade names manufactured by Tokai Carbon Co., Ltd.), Niteron #10 (trade name manufactured by Nippon Steel Chemical Co., Ltd.), Denka Black (trade name manufactured by Denka Co., Ltd.), Toka Black (trade name manufactured by Tokai Carbon Co., Ltd.), and SUPER C-65 (trade name manufactured by MTI Corporation, USA).
[0033] Commercially available carbon nanotubes include VGCF-H (product name manufactured by Showa Denko KK).
[0034] Commercially available graphene products include those manufactured by Sigma-Aldrich.
[0035] The conductive carbon material is preferably in the form of fibers or spheres.
[0036] In the case of a fibrous form, the fiber diameter is preferably 0.1 to 10 μm, more preferably 0.1 to 5 μm, and the fiber length is preferably 0.1 to 10 μm, more preferably 1 to 10 μm.
[0037] When it is spherical, the primary particle size is preferably 10 nm to 200 nm, and more preferably 20 nm to 150 nm.
[0038] In addition, the conductive carbon material preferably has a primary particle diameter of 100 nm or less from the viewpoint of conductivity in the resin composition and sensor sensitivity. The particle diameter of the conductive carbon material can be determined by a known method. For example, the particle diameter of the conductive carbon material can be measured by observing with a transmission electron microscope (TEM) and analyzing the image using an image processing device (for example, a digital microscope VHX-700F manufactured by Keyence). When the conductive carbon material is a known or commercially available product, the particle diameter may be a literature value or a catalog value.
[0039] The content of the filler (B) is preferably 10 to 60% by weight, where the total amount of the resin (A) and the filler (B) is taken as 100% by weight, from the viewpoint of the sensor element formed from the resin composition exhibiting sufficient conductivity as an odor sensor, and exhibiting sufficient sensitivity as the odor sensor. The content of the carbon black in the odorant receiving layer 315 may more preferably be 10 to 55% by weight, where the total amount of the resin (A) and the filler (B) is taken as 100% by weight.
[0040] The resin composition may further contain other components other than the above-mentioned resin (A), filler (B) and surfactant (C) within the range in which the effects of the present invention can be obtained. Examples of other components include a solvent (D). The other components can be suitably used within the range in which both the effects of the present invention and the effects of the other components can be obtained.
[0041] The solvent (D) can be added to the resin composition from the viewpoint of increasing the compatibility between the resin (A) and the filler (B), increasing the dispersibility of the surfactant (C) in the resin composition, or increasing the coatability of the resin composition. Examples of the solvent (D) include N-methylpyrrolidone (also called NMP), propylene glycol monomethyl ether acetate, ethyl butyrate, butyl butyrate, ethyl acetate, N,N-dimethylformamide, N,N-dimethylacetamide, toluene, and xylene.
[0042] The content of the solvent (D) in the resin composition can be appropriately determined from the above viewpoints.
[0043] <Surfactant (C)> The resin composition according to one embodiment of the present invention may contain a surfactant (C) as described below. The surfactant (C) acts as a dispersant for the filler (B). The surfactant (C) can be appropriately selected from known surfactants within the range in which the resin composition exerts the above-mentioned function.
[0044] The surfactant (C) is not particularly limited, but preferably has an HLB value of 8 to 18, more preferably 9 to 17, and particularly preferably 10 to 16. By using a surfactant (C) having such an HLB value, odor discrimination performance is improved.
[0045] The "HLB value" here is an index showing the balance between hydrophilicity and lipophilicity, and is known as a value calculated by the Oda method described, for example, in "Introduction to Surfactants" [published by Sanyo Chemical Industries, Ltd. in 2007, written by Takehiko Fujimoto], page 212, and is not a value calculated by the Griffin method.
[0046] The HLB value can be calculated from the ratio of the organic value to the inorganic value of an organic compound.
[0047] HLB=10×Inorganic / Organic Here, the inorganic and organic values in the above formula represent index values expressing organic and inorganic properties proposed by Fujita et al., and can be calculated using the values in the table on page 213 of the aforementioned "Introduction to Surfactants."
[0048] Examples of the ionic surfactant include anionic surfactants, cationic surfactants, amphoteric surfactants, and nonionic surfactants.
[0049] Examples of the anionic surfactant include alkali metal salts of carboxylic acids having 10 to 24 carbon atoms, alkali metal salts of alkylsulfonic acids having 14 to 24 carbon atoms, and amine salts of polyether acid esters.
[0050] Examples of the carboxylic acid having 10 to 24 carbon atoms include decanoic acid, undecanoic acid, dodecanoic acid, tridecanoic acid, tetradecanoic acid, hexadecanoic acid, heptadecanoic acid, octadecanoic acid, pentadecanoic acid, nonadecanoic acid, icosanoic acid, henicosanoic acid, docosanoic acid, tricosanoic acid, and tetracosanoic acid.
[0051] Examples of the alkyl group contained in the alkylsulfonic acid having 14 to 24 carbon atoms include a tetradecyl group, a pentadecyl group, a hexadecyl group, a heptadecyl group, an octadecyl group, a nonadecyl group, an icosyl group, a henicosyl group, a docosyl group, a tricosyl group, and a tetracosyl group.
[0052] Examples of the alkali metal contained in the alkali metal salt include sodium and potassium.
[0053] Examples of the cationic surfactant include halide salts of quaternary ammonium having an alkyl group having 12 to 24 carbon atoms.
[0054] Examples of the quaternary ammonium having an alkyl group having 12 to 24 carbon atoms include tetrapropylammonium, tetrabutylammonium, tetrapentylammonium, tetrahexylammonium, dimethyldioctylammonium, didecyldimethylammonium, decyltrimethylammonium, dodecyltrimethylammonium, tridecyltrimethylammonium, hexadecyltrimethylammonium, methyltrioctylammonium, octyltrimethylammonium, tributylmethylammonium, octadecyltrimethylammonium, tetradecyltrimethylammonium, nonadecyltrimethylammonium, icosyltrimethylammonium, henicosyltrimethylammonium, heptadecyltrimethylammonium, and pentadecyltrimethylammonium.
[0055] The halide salts include, for example, fluoride salts, chloride salts, bromide salts, and iodide salts.
[0056] Examples of amphoteric surfactants include dimethyl(3-sulfopropyl)ammonium inner salts having an alkyl group with 10 to 22 carbon atoms, and N-alkyl-N,N-dimethylglycines having an alkyl group with 10 to 22 carbon atoms.
[0057] Examples of dimethyl(3-sulfopropyl)ammonium hydroxide inner salts having an alkyl group having 10 to 22 carbon atoms include decyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, undecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, dodecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, tridecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, tetradecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, pentadecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, Examples of such ammonium hydroxide inner salt include hexadecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, heptadecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, octadecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, nonadecyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, icosyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, henicosyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt, and docosyldimethyl(3-sulfopropyl)ammonium hydroxide inner salt.
[0058] Examples of N-alkyl-N,N-dimethylglycines having an alkyl group having 10 to 22 carbon atoms include N-dodecyl-N,N-dimethylglycine and N-octadecyl-N,N-dimethylglycine.
[0059] Examples of nonionic surfactants include higher alcohol ethylene oxide adducts.
[0060] Examples of higher alcohols include 1-hexyl alcohol, 1-heptyl alcohol, 1-octyl alcohol, 1-nonyl alcohol, 1-decyl alcohol, 1-undecyl alcohol, 1-dodecyl alcohol, 1-tridecyl alcohol, 1-tetradecyl alcohol, 1-pentadecyl alcohol, 1-hexadecyl alcohol, 1-heptadecyl alcohol, and 1-octadecyl alcohol.
[0061] The number of moles of ethylene oxide added is preferably 5 to 50, more preferably 5 to 40, and even more preferably 5 to 30, from the viewpoint of odor discrimination performance.
[0062] The resin (A) and the filler (B) may or may not be compatible with each other.
[0063] The content of the surfactant is preferably 0 to 50% by weight, more preferably 10 to 40% by weight, and most preferably 20 to 30% by weight, based on 100% by weight of the total of the resin (A), the filler (B) and the surfactant (C), from the viewpoint of receptive sensitivity to odorous substances.
[0064] <Method of producing resin composition> A specific example of the method for producing a resin composition according to one embodiment of the present invention is as follows.
[0065] The resin composition is obtained as a slurry by mixing the resin (A) and the filler (B) and kneading them uniformly with a stirrer. When mixing the resin (A) and the filler (B), a surfactant (C) and a solvent (D) may be added as necessary. As the stirrer, for example, a centrifugal mixer is used. As the centrifugal mixer, for example, ARE-310 (trade name of Thinky Corporation) or HR003-04A / V (trade name of Samsung Industries Co., Ltd.) can be mentioned. The resin composition is obtained as a slurry having a desired porosity by mixing the resin (A) and the filler (B) and kneading them with a stirrer at a rotation speed of, for example, 2000 rpm and a rotation time of about 10 to 60 minutes. When the surfactant (C) and the solvent (D) are added as necessary to the resin composition, the solvent (D) is distilled off from the resin composition. The solvent (D) may be removed by distillation from a resin composition formed by uniformly mixing, or may be removed by distillation from a coating film formed during the production of the sensor element 31.
[0066] [2. Sensor element 31] The above-mentioned resin composition exhibits different changes in electrical conductivity over time when odorant A is adsorbed to the resin composition than when odorant B, which is different from odorant A, is adsorbed to the resin composition. By utilizing this property, a sensor element 31 capable of detecting and identifying odorants can be realized.
[0067] The outline and effects of a sensor element 31 to which a resin composition according to one embodiment of the present invention is applied will be described below.
[0068] The sensor element 31 includes an odorant receiving layer 315 containing the above-mentioned resin composition, a first metal wiring 313A, a second metal wiring 313B, and an odorant permeable layer 317. In the following description, when there is no need to distinguish between the first metal wiring 313A and the second metal wiring 313B, they may be referred to as metal wiring 313.
[0069] Here, the first metal wiring 313A and the second metal wiring 313B will be described with reference to Fig. 3 and Fig. 4. Fig. 3 is a top view showing an example of the configuration of sensor element 31, and Fig. 4 is a cross-sectional view showing an example of the configuration of sensor element 31 shown in Fig. 3.
[0070] The first metal wiring 313A and the second metal wiring 313B are metal wirings that function as electrodes for measuring changes in the electrical conductivity of the odorant receiving layer 315 (i.e., the resin composition). That is, the first metal wiring 313A and the second metal wiring 313B are spaced apart from each other, and the odorant receiving layer 315 is in contact with at least a portion of the first metal wiring and at least a portion of the second metal wiring. In one example, the first metal wiring 313A and the second metal wiring 313B are metal wirings that are not in direct contact with each other, and may be metal wirings that are approximately parallel to each other, as shown in FIG. 3.
[0071] As shown in FIG. 3, the metal wiring 313 including the first metal wiring 313A and the second metal wiring 313B may be disposed on a substrate 311. The substrate 311 may be a substrate such as glass epoxy generally used for electronic circuits. The substrate 311 is not limited to glass epoxy, and may be a substrate of paper phenol, glass composite, polyimide, PET, glass ceramic, alumina, or aluminum. The metal wiring 313 may be a metal wiring such as copper or gold. The thickness of each of the first metal wiring 313A and the second metal wiring 313B as viewed from a direction perpendicular to the surface of the substrate is preferably 10 μm to 2 mm, and more preferably 10 μm to 1 mm. The height, i.e., thickness, of each of the first metal wiring 313A and the second metal wiring 313B as viewed from a direction parallel to the surface of the substrate is preferably 1 μm to 100 μm, and more preferably 10 μm to 50 μm. The distance between first metal wiring 313A and second metal wiring 313B is preferably 1 μm to 3 mm, and more preferably 1 μm to 1.5 mm. The length of metal wiring 313 is preferably 100 μm to 50 mm, and more preferably 500 μm to 30 mm.
[0072] FIG. 4 shows the AA cross section of FIG. 3. The odorant receiving layer 315 may be in contact with at least a part of the first metal wiring 313A and at least a part of the second metal wiring 313B. The odorant receiving layer 315 may be arranged to completely cover the first metal wiring 313A and the second metal wiring 313B, for example, as shown in FIG. 3 and FIG. 4. At least a part of the odorant receiving layer 315 may be a thin film having a thickness of 1 μm or more and 50 μm or less, and the lower limit of the thickness is more preferably 3 μm or more, and the upper limit of the thickness is more preferably 10 μm or less. If the thickness is 1 μm or less, the electrical resistance becomes too large, making it difficult to obtain a signal S / N ratio. In addition, if the thickness is 50 μm or more, it takes a long time for the odorant to diffuse into the film, so the responsiveness to changes in the concentration of the odorant deteriorates. With this configuration, the change in the electrical conductivity of the odorant receiving layer 315 caused by the odorant being adsorbed by the odorant receiving layer 315 can be accurately detected as an electrical signal. Furthermore, when creating the odorant receiving layer 315, it is possible to control the thickness of the odorant receiving layer 315 by regulating the area of the film to be applied using the electrode shape, etc., and by controlling the evaporation residue and the amount of the odorant permeable layer solution dispensed.
[0073] When the electrical conductivity of the odorant receiving layer 315 (ie, the electrical conductivity of the sensor element 31) is low, it is desirable that the distance between the first metal wiring 313A and the second metal wiring 313B be a predetermined distance (eg, 500 μm) or less.
[0074] The sensor element 31 can detect and distinguish various odorants by applying a resin composition that exhibits different changes in electrical conductivity over time when odorant A is adsorbed and when odorant B, which is different from odorant A, is adsorbed. In the odor sensor 30 described later, a plurality of sensor elements 31 each having a substrate 311 provided with a configuration for detecting an odorant (metal wiring 313 and an odorant receiving layer 315) may be arranged. Each substrate 311 may be provided with a plurality of sets including an odorant receiving layer 315 of the same composition. When a plurality of sensor elements 31 are arranged, a constant voltage power supply and a voltmeter are provided for each sensor element 31. In the odor sensor 30, one configuration for detecting an odorant (metal wiring 313 and an odorant receiving layer 315) may be arranged on each substrate 311. Alternatively, in the odor sensor 30, a plurality of sets of a configuration for detecting an odorant (metal wiring 313 and an odorant receiving layer 315) may be arranged on one substrate 311. In the latter case, a constant voltage power supply and a voltmeter are connected to each of the sets provided on the substrate 311.
[0075] The composition of each of the multiple odorant receiving layers 315 included in the odor sensor 30 may be the same or different. When the odor sensor 30 includes odorant receiving layers 315 with the same composition, the same odorant can be detected in each of the multiple odorant receiving layers 315. When the odor sensor 30 includes odorant receiving layers 315 with different compositions, each of the multiple odorant receiving layers 315 responds differently to the odorant. In this way, by providing multiple sets of configurations for detecting odorants, the accuracy of odorant identification in the odor sensor 30 can be improved.
[0076] [3. Odor Sensor 30] The outline and effects of the odor sensor 30 to which the sensor element 31 is applied will be described below with reference to Fig. 5. Fig. 5 is a block diagram showing an example of the configuration of the odor sensor 30 to which the sensor element 31 is applied.
[0077] The odor sensor 30 includes a sensor element 31 that detects odor substances, a constant-voltage power supply 32 (power supply), and a voltmeter 33 (measuring device).
[0078] The first metal wiring 313A and the second metal wiring 313B of the sensor element 31 are connected by a lead wire W. An example in which a constant voltage power supply 32 and a voltmeter 33 are provided on the lead wire W is shown in FIG.
[0079] The constant voltage power supply 32 is a power supply for supplying power to the sensor element 31. The constant voltage power supply 32 supplies a constant voltage via lead wires to the sensor element 31. The voltage value supplied by the constant voltage power supply 32 is 0.5V to 10V, for example, 2.5V.
[0080] The voltmeter 33 measures the potential difference generated between the first metal wiring 313A and the second metal wiring 313B when a constant voltage supplied from the constant voltage power supply 32 is supplied to the odorant receiving layer 315.
[0081] In addition, the odor sensor 30 includes an amplifier (not shown) in front of the voltmeter 33 in the circuit for measuring odor substances, and the amplifier amplifies the acquired signal and supplies it to the voltmeter 33.
[0082] In addition, the odor sensor 30 is equipped with a reference circuit in addition to the circuit for measuring odorous substances, and the voltmeter 33 acquires the difference (potential difference) between the value acquired in the circuit for measuring odorous substances and the value acquired in the reference circuit as a voltage value.
[0083] Although not a required component, the odor sensor 30 may further include a housing 34. The housing 34 is a container capable of containing air containing an odor substance. When the odor sensor 30 includes the housing 34, the sensor element 31 is disposed within the housing 34.
[0084] The housing 34 has an inlet 341 for introducing an odorant and an outlet 342 for discharging air containing the odorant. The odorant may be introduced by introducing filter paper or the like soaked in the odorant into the housing 34 from the inlet 341, or by introducing air containing the odorant into the housing 34 from the inlet 341. The housing 34 is a container for containing air containing the odorant at a predetermined concentration (e.g., 200 ppm) or more.
[0085] Although not essential, an airflow generating fan 35 may be provided at the exhaust port 342 of the housing 34. The airflow generating fan 35 is for generating an airflow inside the housing 34 and discharging the gas inside the housing 34 from the exhaust port 342 to the outside of the housing 34.
[0086] The odor sensor 30 may include a constant current source (power supply) (not shown) instead of the constant voltage power supply 32, and an ammeter (measuring device) (not shown) instead of the voltmeter 33. In this case, the constant current source functions as a power supply for supplying power to the sensor element 31, and applies a constant current to the sensor element 31 via a lead wire. Meanwhile, the ammeter measures the value of the current flowing between the first metal wiring 313A and the second metal wiring 313B when a constant current is applied to the odorant receiving layer 315. Both the first metal wiring 313A and the second metal wiring 313B can function as electrodes. Hereinafter, when the metal wiring 313 functions as an electrode, it may be referred to as "electrode 313".
[0087] The odor sensor 30 outputs a measurement value that indicates the change over time in the electrical conductivity of the sensor element 31 before and after an odor substance is adsorbed to the sensor element 31. This makes it possible to detect and identify various odor substances.
[0088] 4. Odor measuring device 100 The odor sensor 30 described above can output the change over time in the electrical conductivity of the sensor element 31 for each odor substance when various odor substances are adsorbed to the sensor element 31. By applying this odor sensor 30, it is possible to compare the change over time in the electrical conductivity of the sensor element 31 when odor substance A is adsorbed to the sensor element 31 with the change over time in the electrical conductivity of the sensor element 31 when odor substance B is adsorbed to the sensor element 31. Based on such a comparison result, it is possible to realize an odor measurement device 100 that can estimate the odor substance adsorbed to the sensor element 31.
[0089] Furthermore, the odor measuring device 100 can estimate odor substances with high accuracy by using the estimation model 22 generated by machine learning. The estimation model 22 can be generated using learning data including a combination of measurement values measured when each of a plurality of odor substances is adsorbed to at least one sensor element 31, and identification information unique to the odor substance that provided the measurement value.
[0090] The following describes the outline and effects of an odor measuring device 100 that uses the odor sensor 30. The odor measuring device 100 is a device that estimates the odor substance adsorbed to a sensor element 31 based on a change in electrical conductivity that occurs in the sensor element 31 to which the above-mentioned resin composition is applied.
[0091] The odor measuring device 100 of this embodiment is separately provided with a sensor chamber 60 including a plurality of sensor elements 31A (hereinafter also referred to as a "sensor element group 31A"), and a target sample receiving section 50 into which a target sample containing an odorant is introduced and into which gas containing the odorant generated from the target sample is enclosed. In this embodiment, each sensor element 31 included in the sensor element group 31A will be simply referred to as a "sensor element 31".
[0092] The odor measuring device 100 of this embodiment employs a configuration in which the gas containing the odorant inside the target sample receiving section 50 is pushed toward the sensor chamber 60 by using a gas other than the gas containing the odorant. In this embodiment, the gas inside the target sample receiving section 50 when the target sample is introduced into the target sample receiving section 50 (i.e., the gas containing the odorant to be detected) is referred to as the first gas. Meanwhile, the gas for pushing the first gas toward the sensor chamber 60 is referred to as the second gas.
[0093] Fig. 1 is a schematic diagram of an odor measurement device 100. As shown in Fig. 1, the odor measurement device 100 includes an odor sensor 30, a target sample receiving section 50, a sensor chamber 60, a gas supply section 80, and an estimation device 10. The odor measurement device 100 may further include an adjustment section 51. The odor measurement device 100 may further include an estimation device 10a.
[0094] 1 shows, as an example, an example in which gas flows from gas supply unit 80 to target sample receiving unit 50 and sensor chamber 60 in that order. Gas supply unit 80, target sample receiving unit 50, and sensor chamber 60 are each connected by a tube.
[0095] [Target sample receiving section 50] The target sample receiving section 50 can receive a target sample containing an odorant and hold a first gas. The target sample receiving section 50 has a first port 501 through which the second gas entering the inside passes, and a second port 502 through which the first gas and the second gas leaving the inside can pass. In FIG. 1, the first port 501 is installed at the upper part of the target sample receiving section 50 and the second port 502 is installed at the lower part of the target sample receiving section 50, but is not limited to this. For example, the positions of the first port 501 and the second port 502 can be appropriately set depending on the type and combination of odor components contained in the first gas. For example, the positions of the first port 501 and the second port 502 may be changed depending on whether the weight per unit volume of the odor components contained in the first gas (i.e., specific gravity) is heavier or lighter than that of the second gas. Furthermore, the target sample receiving section 50 may include an airflow generating fan 35 therein, as in FIG.
[0096] The target sample receiving section 50 includes a sample inlet 503 for receiving a liquid or solid target sample. The target sample receiving section 50 may include a placement section (not shown) for placing the target sample. When the target sample is liquid, the placement section may be a cup for holding the liquid, and when the target sample is solid, the placement section may be a petri dish on which the solid is placed. The target sample may be introduced into the target sample receiving section 50 in a gaseous state as a first gas from the sample inlet 503. In this way, since the target sample receiving section 50 can receive a liquid or solid target sample, it is possible to adjust the concentration of the odorant in the first gas. For example, even if the odorant is the same, it is easy to adjust the concentration of the odorant in the first gas.
[0097] A material inactive to odorants may be disposed on the inner surface of the target sample receiving portion 50. A material inactive to odorants is a material that does not significantly change the concentration of each odorant contained in the gas sent to the sensor chamber 60. For example, a material inactive to odorants is a material in which odorants are unlikely to be adsorbed or dissolved. Examples of materials inactive to odorants include glass, metal, and resin. When metal is used, stainless steel (SUS) is preferable, and when resin is used, fluorine-based resin, polypropylene (PP), polyethylene (PE), ABS resin, and polyethylene terephthalate (PET) are preferable.
[0098] If the inner surface of target sample receiving portion 50 is made of a material that adsorbs odorous substances contained in the first gas, the odorous substances may be adsorbed to various portions, which may affect subsequent measurements.
[0099] In this way, the inner surface of the target sample receiving portion 50 is made of a material that is inactive against odorants, thereby reducing the risk that the material of the inner surface will react with the odorants contained in the first gas, or that the odorants will be adsorbed onto the inner surface. This reduces the risk that the odorants contained in the first gas supplied to the sensor chamber 60 will change while contained in the target sample receiving portion 50, or that the concentration of the odorants will be diluted.
[0100] Even if the target sample is a liquid or solid, the odor measurement device 100 is provided with the target sample receiving section 50, thereby making the concentration of the first gas uniform in the target sample receiving section 50 before the first gas is sent to the sensor chamber 60. Furthermore, by providing the target sample receiving section 50, the odor measurement device 100 is able to push the first gas into the sensor chamber 60 at a constant flow rate. As a result, even when measurements are repeated, the odor measurement device 100 can send the first gas to the sensor chamber 60 under the same conditions each time, thereby enabling repeated and stable measurements to be performed.
[0101] The volume of the target sample receiving section 50 is preferably 1 to 200 times the volume of the sensor chamber 60. In particular, the volume of the target sample receiving section 50 is preferably larger than the volume of the sensor chamber 60. The volume of the target sample receiving section 50 is more preferably 2 or more times the volume of the sensor chamber 60, and more preferably 4 or more times. In addition, the volume of the target sample receiving section 50 is preferably 100 or less times the volume of the sensor chamber 60, and more preferably 60 or less times. By having the volume of the target sample receiving section 50 be 1 or more times the volume of the sensor chamber 60, the concentration of the odor substance in the sensor chamber 60 is appropriately adjusted, and the measurement result by the sensor provided in the sensor chamber 60 is stably output. In addition, by having the volume of the target sample receiving section 50 be 200 or less times the volume of the sensor chamber 60, it is easy to adjust the temperature and humidity in the target sample receiving section 50, so that the measurement result by the sensor is stably output and the size of the odor measuring device 100 can be kept compact.
[0102] If the volume of the target sample receiving section 50 is less than one time the volume of the sensor chamber 60, the odorant generated in the target sample receiving section 50 may be diluted in the sensor chamber 60, and the measurement sensitivity of the sensor may decrease. If the volume of the target sample receiving section 50 is more than 200 times the volume of the sensor chamber 60, the volume of the target sample receiving section 50 is too large, so the uniformity of the concentration, temperature, and humidity of the first gas may decrease, and when measurements are repeated, the first gas may not be sent to the sensor chamber 60 under the same conditions. Furthermore, the overall size of the odor measuring device 100 may become large.
[0103] FIG. 1 shows an example in which the volume of the target sample receiving portion 50 is eight times the volume of the sensor chamber 60 .
[0104] For example, if the inner surface of the tube 93 is made of a material that adsorbs odorous substances contained in the first gas, the odorous substances may be adsorbed to various parts, which may affect the subsequent measurement. Therefore, it is preferable that a material that is inactive to odorous substances is arranged on the inner surface of the tube 93 that guides the first gas from the target sample receiving section 50 to the sensor chamber 60, similar to the inner surface of the target sample receiving section 50. Examples of materials that are inactive to odorous substances include glass, metal, and resin. When metal is used, stainless steel (SUS) is preferable, and when resin is used, fluorine-based resin, polypropylene (PP), polyethylene (PE), ABS resin, and polyethylene terephthalate (PET) are preferable.
[0105] The target sample receiving section 50 may be configured to be detachable from the tubes 92 and 93. In this manner, since the target sample receiving section 50 is detachable, when the previous measurement is completed and the next measurement is to be performed, a new target sample receiving section 50 can be attached without purging the inside of the target sample receiving section 50. This allows the odor measuring device 100 to perform multiple measurements in a short period of time.
[0106] Furthermore, because the target sample receiving section 50 is detachable, the target sample receiving section 50 into which the target sample has been introduced can be maintained at a desired temperature using a heat retention chamber separate from the odor measurement device 100. This allows the odor measurement device 100 to adjust the temperature of the target sample receiving section 50, even if it is not possible to provide the adjustment section 51 described below in the odor measurement device 100. As the heat retention chamber, for example, a water bath, a dry bath, a heat jacket, a silicon heater, a forward air dryer, a thermo-hygrostat, a sprayer, or the like may be used.
[0107] [Adjustment section 51] The adjustment unit 51 adjusts at least one of the temperature and humidity of the first gas contained in the target sample receiving section 50. When the adjustment unit 51 adjusts the temperature, the adjustment unit 51 is, for example, a heater or a cooler. In this case, the adjustment unit 51 may be configured to cover the entire target sample receiving section 50. When the adjustment unit 51 adjusts the humidity, the adjustment unit 51 is, for example, a humidifier or a dehumidifier. The adjustment unit 51 may adjust at least one of the temperature and humidity for each type of first gas, or may change at least one of the temperature and humidity at predetermined time intervals during measurement of the same first gas. As the adjustment unit 51, for example, a water bath, a dry bath, a heat jacket, a silicon heater, a wind dryer, a thermohygrostat, a sprayer, or the like capable of changing at least one of the temperature and humidity may be used.
[0108] The adjustment unit 51 adjusts at least one of the temperature and humidity of the first gas in the target sample receiving unit 50, so that the odor measuring device 100 can send the first gas to the sensor chamber 60 using conditions according to, for example, the type of the first gas (such as the weight or volatility of the gas). This also allows the odor measuring device 100 to send a stable concentration of the first gas to the sensor chamber 60, improving the accuracy of the measurement.
[0109] [Sensor chamber 60] The sensor chamber 60 is a space for storing the sensor element 31 for measuring odor substances. The sensor chamber 60 is connected to the second port 502 of the target sample receiving portion 50. Specifically, the sensor chamber 60 includes a gas supply port 601 and a gas exhaust port 602, and the second port 502 of the target sample receiving portion 50 is connected to the gas supply port 601.
[0110] The sensor chamber 60 includes a plurality of sensor elements 31A capable of outputting a measurement result according to an odor substance contained in the first gas. The plurality of sensor elements 31A may be sensor elements 31 each having a different resin composition as a substance receiving layer. That is, the plurality of sensor elements 31A may have different sensitivities and specificities to the odor substance. The sensor chamber 60 in FIG. 1 includes, as an example, a sensor element 31 and a sensor element 31b, but is not limited thereto. The sensor chamber 60 in FIG. 1 also includes a sensor element 31c having a resin composition different from the sensor elements 31 and 31b as a substance receiving layer. The sensor element 31 and the sensor element 31b are capable of outputting a measurement result according to the same odor substance contained in the first gas, but the measurement results output by each of them are different. The measurement result according to the odor substance is, for example, a measurement result according to the concentration of the odor substance. In the following description, when there is no particular distinction between the sensor elements 31, 31b, 31c and the sensor element 31d described later, they are collectively referred to as "sensor element 31".
[0111] The sensor elements 31 each having a different resin composition as a substance receiving layer may be installed in any combination and in any arrangement in the sensor chamber 60. Furthermore, the sensor chamber 60 may be installed with a plurality of sensor elements 31 each having the same resin composition as a substance receiving layer.
[0112] Here, the sensor element 31 and the sensor element 31b may be sensor elements capable of outputting measurement results corresponding to different odor substances. For example, the sensor chamber 60 may be provided with a sensor element 31 capable of outputting measurement results corresponding to an odor substance contained in a first gas, and a sensor element 31b capable of outputting measurement results corresponding to a second odor substance different from the odor substance contained in the first gas. For example, the odor sensor 30 may include sensor elements 31 and 31b having different resin compositions used in the odor substance receiving layer 315.
[0113] By providing multiple sensor elements 31 in which resin compositions with different odorant adsorption properties are used in the odorant receiving layer 315, the odor measuring device 100 can simultaneously perform estimations for multiple odorants. Note that as a sensor element 31 according to one embodiment of the present invention, a sensor element 31 that does not contain a surfactant (C) in the odorant receiving layer 315 and a sensor element 31 that contains a surfactant (C) in the odorant receiving layer 315 may be used in combination.
[0114] Furthermore, by using the odor measurement device 100, it is possible to obtain a first change pattern indicating a change in the electrical conductivity of the sensor element 31 and a second change pattern indicating a change in the electrical conductivity of the sensor element 31b for each known odor substance. The estimation model 22 may be generated by machine learning using both the first change pattern and the second change pattern. The odor measurement device 100 estimates odor substances using the estimation model 22 generated in this way, and therefore is able to more precisely identify each odor substance.
[0115] 1 includes a plurality of sensor elements 31A arranged in a 4×4 array, as an example. The number of sensor elements 31A and the manner in which the sensor elements 31A are arranged are not limited. The total number of sensor elements 31A included in the sensor chamber 60 is also not particularly limited, and may be, for example, 2, 8, 16, or 64. The total number of sensor elements 31A may be 8 or more and 16 or less.
[0116] The material of the inner surface of the sensor chamber 60 is preferably a material that is inactive to odorants, similar to the target sample receiving section 50. Examples of materials that are inactive to odorants include glass, metal, and resin. When metal is used, stainless steel (SUS) is preferable, and when resin is used, fluororesin, polypropylene (PP), polyethylene (PE), ABS resin, and polyethylene terephthalate (PET) are preferable. When the material of the inner surface of the sensor chamber 60 is a material that adsorbs odorants contained in the first gas, the odorants adsorbed in the sensor chamber may reduce the amount of change in output from the sensor element 31 in a subsequent measurement, and the odor measuring device 100 may not be able to perform an accurate measurement.
[0117] [Multiple sensor elements 31A (sensor element group 31A)] The sensor elements 31A may include a thin film. As an example, the odorant receiving layer 315 and the odorant permeable layer 317 in FIG. 2 and FIG. 3 are thin films.
[0118] As an embodiment for sending the first gas containing an odorant into the sensor chamber 60, for example, a vacuum pump may be installed on the gas exhaust port 602 side of the sensor chamber 60, and the gas may be drawn using the vacuum pump to send the odorant into the sensor chamber 60 from the gas supply port 601 side of the sensor chamber 60. However, if the sensor elements 31 and 31b have a thin film, the thin film may expand if the pressure inside the sensor chamber 60 is negative, and the sensor elements 31 and 31b may not be able to output a stable measurement result. In the odor measurement device 100 according to this embodiment, the gas supply unit 80 pushes the gas from the first port 501 side of the sensor chamber 60 and the target sample receiving unit 50 to send the first gas into the sensor chamber 60, so the pressure inside the sensor chamber 60 is positive. Therefore, the odor measurement device 100 can obtain a stable measurement result even if multiple sensor elements 31A have thin films. In contrast, if the gas supply unit 80 sends the first gas into the sensor chamber 60 by pushing the gas from the sensor chamber 60 and the first port 501 side of the target sample receiving unit 50, the pressure inside the sensor chamber 60 will be positive. Therefore, it is preferable for the odor measurement device 100 according to this embodiment to adopt a configuration in which the gas supply unit 80 sends the first gas into the sensor chamber 60 by pushing the gas from the sensor chamber 60 and the first port 501 side of the target sample receiving unit 50. This allows the odor measurement device 100 to obtain stable measurement results even if multiple sensor elements 31A are equipped with thin films.
[0119] The thin film of the plurality of sensor elements 31A may contain a conductive carbon material, a resin composition, and a surfactant.
[0120] [Gas supply unit 80] The gas supply unit 80 is connected to the first port 501 of the target sample receiving portion 50, and by sending a second gas into the inside of the target sample receiving portion 50, the first gas is sent from within the target sample receiving portion 50 toward the sensor chamber 60.
[0121] A valve 81 may be provided between the gas supply unit 80 and the target sample receiving unit 50. By opening and closing the valve 81, start and stop of gas supply from the gas supply unit 80 may be adjusted.
[0122] In this way, the gas supply unit 80 pushes the gas from the first port 501 side of the target sample receiving unit 50 to send the first gas into the sensor chamber 60, so the pressure inside the sensor chamber 60 is positive. This allows the odor measurement device 100 to obtain stable measurement results. In addition, since the second gas can be sent by opening and closing the valve 81, the odor measurement device 100 can send the first gas from the target sample receiving unit 50 toward the sensor chamber 60 at any timing. This allows the odor measurement device 100 to improve the reproducibility of the waveform shape output by each sensor element 31 when repeatedly measuring odor substances contained in the first gas using the sensor element group 31A.
[0123] The second gas may be an inert gas or air. Examples of the inert gas include argon and nitrogen. When the second gas is an inert gas, the gas supply unit 80 may be a gas cylinder.
[0124] Furthermore, when the second gas is air, the gas supply unit 80 may be a pump. In this case, in order to remove components that react with the first gas contained in the target sample receiving unit 50, the odor measuring device 100 may be provided with, for example, an activated carbon filter, a dehumidifier, a silica gel column, or a dust filter on the first port 501 side of the target sample receiving unit 50.
[0125] The odor measuring device 100 may further include a mass flow controller on the side of the first port 501 of the target sample receiving section 50, more specifically, between the valve 81 and the gas supply section 80. The odor measuring device 100 employing this configuration can send the first gas from the target sample receiving section 50 to the sensor chamber 60 at a constant flow rate, and the multiple sensor elements 31A can provide stable outputs.
[0126] 1 shows a configuration in which the first gas and the second gas leaving the inside of the target sample receiving part 50 pass through the tube 93 and the sensor chamber 60, but the configuration is not limited to this. Since the target sample receiving part 50 of the odor measurement device 100 has a larger volume than the sensor chamber 60, it is not necessary to send the entire amount of the first gas inside the target sample receiving part 50 to the sensor chamber 60 during measurement. Furthermore, when the inside of the target sample receiving part 50 is purged with the second gas after the measurement, it is not necessary for the target sample receiving part 50 and the sensor chamber 60 to be connected. Therefore, the odor measurement device 100 may be configured such that a valve (not shown) is arranged in the tube 93 so that the first gas and the second gas leaving the inside of the target sample receiving part 50 can be exhausted without passing through the sensor chamber 60.
[0127] [Estimation device 10] The estimation device 10 is a device that estimates an odor substance detected by the odor sensor 30. The estimation device 10 is, for example, a computer, and includes a CPU and a memory (not shown). The estimation device 10 is connected to the odor sensor 30 so that it can communicate with the odor sensor 30. Specifically, the estimation device 10 performs estimation of the odor substance by analyzing the measurement value acquired from the odor sensor 30. If the sensor chamber 60 further includes a sensor element 31c in which a resin composition different from that of the sensor element 31 and the sensor element 31b is used in the substance receiving layer 315, the estimation device 10 may further acquire and analyze a measurement value measured by a voltmeter by supplying a constant voltage to the sensor element 31c. The estimation device 10 may also display the measurement value itself, a waveform in which the measurement value is plotted, and an estimation result of an unknown odor substance based on an estimation model. The estimation device 10 may also display a numerical value and a graph indicating the change in the presence ratio of each odor substance for a gas containing multiple odor substances. The estimation device 10 may also generate an estimation model 22 used to estimate an odor substance.
[0128] <Generation of Estimation Model 22> Next, the configuration of the odor measuring device 100 that performs the process of generating the estimation model 22 used to estimate odor substances, and the process of generating the estimation model 22 will be described with reference to FIGS. 6 and 7. FIG.
[0129] The estimation model 22 is generated by machine learning using learning data including a combination of measurement values measured by the voltmeter 33 when each of a plurality of odor substances is adsorbed to at least one sensor element 31, and identification information unique to the odor substance that gave the measurement value. Here, the identification information unique to the odor substance may be, for example, the name, CAS number, and chemical formula of the odor substance.
[0130] (Configuration of the Estimation Device 10 (Generation of Estimation Model 22)) Fig. 6 is a functional block diagram showing an example of the configuration of the odor measuring device 100. For ease of explanation, the same reference numerals are given to members having the same functions as those described in Fig. 1, and the explanation thereof will not be repeated.
[0131] As shown in FIG. 6, the estimation device 10 includes an input unit 15, a control unit 1, and a storage unit 2.
[0132] The input unit 15 is for accepting various input operations from a user, and may be, for example, a keyboard, a mouse, a touch panel, or the like.
[0133] The control unit 1 includes a measurement value acquiring unit 11 (acquiring unit), a change pattern analyzing unit 12 (analyzing unit), a learning control unit 13, and an estimation model generating unit .
[0134] The measurement value acquiring unit 11 acquires a measurement value from the voltmeter 33. Furthermore, the measurement value acquiring unit 11 uses the acquired measurement value to calculate a value (e.g., resistance value, impedance, etc.) indicating the electrical conductivity of the sensor element 31. The measurement value acquiring unit 11 may acquire the measurement value from the voltmeter 33 at a predetermined time interval (e.g., 0.1 second interval).
[0135] The change pattern analysis unit 12 analyzes the change over time in the electrical conductivity of at least one sensor element 31. Using the resistance value calculated by the measurement value acquisition unit 11, the change pattern analysis unit 12 calculates a value indicating the amount of change in the electrical conductivity of the sensor element 31 due to the adsorption of an odorant. The change pattern analysis unit 12 generates data indicating a change pattern indicating the time change in the calculated amount of change in electrical conductivity. When the generated change pattern is a known odorant, the change pattern analysis unit 12 may store the generated change pattern in the change pattern database 21 (learning data) in association with identification information specific to the known odorant.
[0136] The learning control unit 13 reads out the change pattern database 21 from the storage unit 2 and controls the generation of the estimation model 22 by machine learning. Here, the change pattern database 21 is a database that includes combinations of measurement values measured when multiple odor substances are adsorbed to the sensor element 31 and identification information unique to the known odor substances that provided the measurement values. The learning control unit 13 inputs the change pattern read out from the change pattern database 21 to the estimation model generation unit 14. In addition, the learning control unit 13 compares the identification information of the odor substance corresponding to the change pattern input to the estimation model generation unit 14 with the estimation result output from the estimation model generation unit 14, and outputs a correction instruction according to the comparison result to the estimation model generation unit 14.
[0137] The estimation model generation unit 14 generates the estimation model 22 by a machine learning algorithm using the change patterns stored in the change pattern database 21. The estimation model generation unit 14 may be configured to generate the estimation model 22 by using a known supervised machine learning algorithm. Examples of machine learning algorithms that can be applied to the estimation model generation unit 14 include the k-nearest neighbor method, logistic regression, support vector machine, random forest, and neural network.
[0138] Feature extraction method When generating an estimation model by machine learning, the data on which the model is based may be the measurement value itself, or may be data extracted from the feature of the measurement value, such as a statistical quantity of the measurement value, a differential integral value, a peak detection value, or an autocorrelation value. Examples of the statistical quantity include an average value, a variance value, a maximum value, a minimum value, a difference between a maximum value and a minimum value, and a standard deviation. Examples of the differential integral include a slope and an area. Examples of the peak detection value include the number of peaks and the height. Examples of the autocorrelation value include a step difference.
[0139] Pretreatment method When generating an estimation model by machine learning, the base data may be used for machine learning as it is, or the base data may be pre-processed as necessary. When pre-processing is performed, the pre-processing may be performed before feature extraction, after feature extraction, or both before and after feature extraction. The pre-processing may be performed by a known method, and may include correction, noise removal, standardization, data conversion, smoothing, data expansion, and other methods. Correction may be performed based on the measurement results of multiple elements, commercially available sensors (for example, temperature sensors, humidity sensors, and the like), and standard gases. For example, correction may be performed by output ratio calculation, independent component analysis (ICA), statistical calculation, integration, addition, subtraction, division, and other methods. Examples of noise removal include removal of outliers and white noise. Examples of standardization include normalization and regularization. Examples of data transformation include trend removal, frequency conversion, logarithmic conversion, and the like. Examples of smoothing include moving average, difference, and the like. Examples of data augmentation include adding the same sample data (for example, assuming a normal distribution) and adding new sample data (for example, adding using a vector mixture ratio).
[0140] Machine learning algorithms Machine learning algorithms applicable to the estimation model generation unit 14 include regression analysis, classification, tree, time series analysis, neural network, clustering, etc. Examples of regression analysis include logistic regression, Lasso, elastic net, support vector regression (SVR), linear, Ridge, ensemble regression, etc. Examples of classification include k-nearest neighbor method, support vector classification (SVC), Naibe Bayes classifier, stochastic gradient descent (SGD), kernel approximation, etc. Examples of trees include decision trees, regression trees, random forests, boosting (lightGBM, XGboost), stacking, etc. Examples of time series include AR, MA, ARIMA, state space, etc. Examples of neural networks include multi-layer perceptrons (MLPs), convolutional neural networks (CNNs), recurrent neural networks (RNNs), residual neural networks (ResNets), transformers, graph neural networks (GNNs), etc. Examples of clustering include Gaussian mixture models (GMMs), k-means methods (kmeas), minikmeans, variational Gaussian mixture models (VBGMMs), kernel approximations, etc.
[0141] (Process for generating estimation model 22) The process of generating the estimation model 22 using the odor measurement device 100 will be described below with reference to Fig. 7. Fig. 7 is a flow chart showing an example of the process flow in which the estimation device 10 of the odor measurement device 100 generates the estimation model 22. The estimation model 22 is generated by machine learning using learning data including a combination of measurement values measured by the voltmeter 33 when each of a plurality of odor substances is adsorbed to at least one sensor element 31, and identification information unique to the odor substance that gave the measurement value. Here, the identification information unique to the odor substance may be, for example, the name, CAS number, and chemical formula of the odor substance.
[0142] First, the measurement value acquiring unit 11 acquires the voltage value V0 measured by the odor sensor 30 before the odor substance is introduced into the target sample receiving unit 50, and calculates the resistance value R0. The resistance value R0 is preferably 500 to 3000 Ω, more preferably 800 to 2800 Ω, and most preferably 1000 to 2500 Ω. Then, the odor substance is introduced into the target sample receiving unit 50 (step S1).
[0143] Meanwhile, the input unit 15 receives an input of the name of the known odor substance introduced into the target sample receiving unit 50 (step S2). The process of step S2 may be performed before step S1.
[0144] Next, the measurement value acquiring unit 11 acquires data (waveform or pattern of change over time) of the amount of change (ΔV) in the voltage value V before and after the odor substance is adsorbed and desorbed to the sensor element 31 (step S3).
[0145] Next, the change pattern analysis unit 12 associates the change (ΔV) data (waveform or change pattern over time) in the voltage value V before and after the odor substance adsorption and desorption with the name of the input known odor substance and stores it in the change pattern database (step S4).
[0146] If no change pattern has been stored for a given type of existing odor substance (NO in step S5), that is, if there is still insufficient data to use for machine learning, the process returns to step S1.
[0147] If a change pattern is stored for a predetermined type of existing odor substance (YES in step S5), the learning control unit 13 reads out the change pattern for the known odor substance stored in the change pattern database 21 and inputs it to the estimation model generation unit 14. The estimation model generation unit 14 generates an estimation model 22 by machine learning based on the time-dependent change pattern (or feature amount extracted from the change pattern) stored in the change pattern database 21 (step S6).
[0148] The estimation model generating unit 14 stores the estimation model 22 generated by a predetermined machine learning in the storage unit 2 (step S7).
[0149] 6 and 7, the estimation device 10 generates the estimation model 22, but is not limited to this. For example, the estimation device 10 may provide an external computer different from the estimation device 10, which has the same functions as the learning control unit 13 and the estimation model generation unit 14, with the same data as the change pattern database 21 to generate the estimation model 22.
[0150] <Identification of odor substances> Next, the configuration of the odor measuring device 100a that estimates an odor substance using the estimation model 22 and the estimation process will be described with reference to FIGS.
[0151] (Configuration of Estimation Device 10a (Execution of Estimation Process)) Fig. 8 is a functional block diagram showing an example of the configuration of an odor measuring device 100a. For ease of explanation, the same reference numerals are given to members having the same functions as those described in Fig. 1 and Fig. 6, and the description thereof will not be repeated.
[0152] As shown in Fig. 8, the estimation device 10a includes a control unit 1a, a storage unit 2a, and an output unit 18. Here, Fig. 8 shows a configuration example in which the estimation device 10 shown in Fig. 6 is used for odor substance estimation processing. That is, the estimation device 10 shown in Fig. 6 and the estimation device 10a shown in Fig. 8 may be computers having the same hardware configuration.
[0153] The output unit 18 is for presenting the estimation result to the user, and may be, for example, a display, a speaker, a lamp, or the like.
[0154] The control unit 1 a includes a measurement value acquiring unit 11 (acquiring unit), a change pattern analyzing unit 12 (analyzing unit), an estimating unit 16, and an output control unit 17.
[0155] The estimation unit 16 uses the estimation model 22 to estimate the odor substance from the analysis results obtained by analyzing the measurement values obtained from the odor sensor 30.
[0156] The output control unit 17 controls the output unit 18 to output the estimation result.
[0157] (Estimation process) Hereinafter, specific processing performed by each part of the control unit 1a will be described with reference to Fig. 9. Fig. 9 is a flow chart showing an example of the flow of processing performed by the estimation device 10a to estimate an odor substance.
[0158] First, the measurement value acquiring unit 11 acquires the voltage value V0 measured by the odor sensor 30 before the odor substance is introduced into the target sample receiving unit 50, and calculates the resistance value R0. After that, an unknown odor substance (regardless of its properties) is introduced into the target sample receiving unit 50 (step S11).
[0159] Next, the measurement acquisition unit 11 acquires data (waveform or pattern of change over time) of the change (ΔV) in the voltage value V before and after the adsorption and desorption of the unknown (i.e., the target) odor substance to the sensor element 31 (step S12).
[0160] Next, the estimation unit 16 estimates the unknown odor substance from the time-dependent change pattern (or the feature amount extracted from the change pattern) based on the estimation model 22 (step S13).
[0161] The output control unit 17 controls the output unit to output the estimation result (step S14).
[0162] In the above embodiment, the estimation device 10 that generates the estimation model 22 and the estimation device 10a that estimates odor substances using the estimation model 22 have been described. Note that the estimation device 10 and the estimation device 10a may be separate devices or may be a single device.
[0163] <Configuration example of sensor element 31c> FIG. 10 is a top view showing an example of the configuration of one sensor element 31c included in the sensor element group 31A. The sensor element 31c includes an electrode 313, which is a metal wiring arranged on the substrate 311, and a circular odorant receiving layer 315c formed on the electrode 313. The electrode 313 includes a first metal wiring 313C and a second metal wiring 313D. The first metal wiring 313C and the second metal wiring 313D are metal wirings that function as electrodes for measuring changes in the electrical conductivity of the odorant receiving layer 315c. In FIG. 10, the metal wiring 313a and the metal wiring 313d are arranged on the front side of the substrate 311 (i.e., the front side of the paper) and are in contact with the odorant receiving layer 315c. On the other hand, the metal wiring 313b and the metal wiring 313c are connected to the metal wiring 313a and the metal wiring 313d, respectively, on the front side of the substrate 311 and penetrate the substrate 311 toward the back side. Therefore, the metal wiring 313b and the metal wiring 313c are not in contact with the odorant receiving layer 315c. The diameter R of the odorant receiving layer 315c is 0.2 mm or more and 5 mm or less. In FIG. 10, the shape of the odorant receiving layer 315c provided in the sensor element 31c is elliptical as an example, but is not limited to this. When the shape of the odorant receiving layer 315c is elliptical, the average of the minor axis and the major axis may be 0.2 mm or more and 5 mm or less. The shape of the odorant receiving layer 315c may also be a perfect circle.
[0164] As shown in FIG. 10, the metal wiring 313a and the metal wiring 313d are in contact with the odorant receiving layer 315c but are not in contact with the odorant permeable layer 317.
[0165] 11 is a top view showing an example of the configuration of one sensor element 31d included in the sensor element group 31A. The sensor element 31d comprises an electrode 313 (first metal wiring 313C, second metal wiring 313D) arranged on the substrate 311, and a strip-shaped odorant receiving layer 315d formed on the electrode 313. The length W of the short width of the odorant receiving layer 315d is 0.2 mm or more and 5 mm or less. In the following description, when there is no particular distinction between the odorant receiving layers 315c and 315d, they will be collectively referred to as "odorant receiving layer 315."
[0166] The electrodes of the sensor elements 31 included in the sensor element group 31A each have a first electrode and a second electrode, and the first and second electrodes may be arranged in parallel lines, parallel curves, a comb shape, or a concentric circle shape. Regardless of which shape is adopted, the first and second electrodes are preferably arranged in line symmetry or point symmetry with each other. By arranging the first and second electrodes in this way, the odor measuring device 100 can measure odor substances contained in the gas with high accuracy.
[0167] The sensor element 31c in FIG. 10 has a first metal wiring 313C and a second metal wiring 313D. As an example, the first metal wiring 313C is a first electrode composed of a metal wiring 313a and a metal wiring 313b, and the two metal wirings are arranged in a T-shape so as to be perpendicular to each other. The second metal wiring 313D is a second electrode composed of two metal wirings 313c and 313d like the first metal wiring 313C, and is configured so as to be arranged in a T-shape so as to be perpendicular to each other. The first metal wiring 313C and the second metal wiring 313D are arranged in parallel lines so that the metal wiring 313a and the metal wiring 313c face each other.
[0168] The first metal wiring 313C and the second metal wiring 313D are arranged in a T-shape, so that the first metal wiring 313C and the second metal wiring 313D can be arranged at a suitable distance, and the resistance value of the electrodes can be stabilized. For example, if the electrodes are arranged in a comb shape, the distance between the electrodes is short, and the resistance value of the electrodes may become too small. In addition, since the first metal wiring 313C and the second metal wiring 313D are arranged in a T-shape, in the application process of the manufacturing method of the sensor element 31 described later, there is no uneven part of the electrode that can hinder the slurry from spreading in the area where the slurry spreads, so the slurry spreads easily. In addition, since the slurry spreads easily, the thickness of the odorant receiving layer 315 after drying is uniform.
[0169] 12 is a perspective view showing an example of the configuration of one sensor element 31c included in the sensor element group 31A. As shown in FIG. 12, in the sensor element 31c, the first metal wiring 313C and the second metal wiring 313D are connected to pins 316 at the ends where the first metal wiring 313C and the second metal wiring 313D do not face each other. The pins 316 are conductive members for electrically connecting the first metal wiring 313C and the second metal wiring 313D to other members of the odor sensor 30. Although not shown, the sensor elements 31c and 31d shown in FIG. 10 and FIG. 11 also include the pins 316 shown in FIG. 12.
[0170] <Method of manufacturing sensor element 31> The following describes a method for manufacturing a variety of types of sensor elements 31 used in the odor measuring device 100. The odorant receiving layer 315 of the sensor element 31 may use slurries having various compositions as its raw material.
[0171] (Slurry preparation process) First, a plurality of types of slurries with different mixing ratios of the conductive carbon material and the resin composition are prepared. The mixing ratio of the conductive carbon material and the resin composition may be appropriately set according to the desired sensitivity and detection specificity of the odorant receiving layer 315. The slurry may contain a solvent, an additive, and a surfactant in addition to the conductive carbon material and the resin composition. When preparing / kneading a slurry of the resin composition containing the filler and the resin composition, NMP as a solvent may be added to the mixture of the filler and the resin composition in multiple batches, and kneading may be repeated. Note that by increasing the number of times of kneading, the porosity in the cross section of the odorant receiving layer 315 decreases.
[0172] (Electrode placement process) Next, electrodes are arranged on the substrate. The electrodes may include a first electrode and a second electrode. The first electrode and the second electrode may be arranged in a parallel straight line shape, a parallel curved line shape, a comb shape, or a concentric circle shape. In addition, the first electrode and the second electrode are preferably arranged in line symmetry or point symmetry with each other, regardless of which shape is adopted. Furthermore, it is more preferable that the first electrode and the second electrode are arranged in a parallel straight line shape or a parallel curved line shape. It is particularly preferable that the first electrode and the second electrode are arranged in a shape as shown in FIG. 10 and FIG. 11. Specifically, it is preferable that the first metal wiring 313C is composed of two metal wirings (313a and metal wiring 313c) arranged perpendicular to each other in a T-shape, the second metal wiring 313D is composed of two metal wirings (313c and metal wiring 313d) arranged perpendicular to each other in a T-shape, and the first metal wiring 313C and the second metal wiring 313D are arranged in parallel lines such that the metal wiring 313a and the metal wiring 313c face each other. By arranging the first metal wiring and the second metal wiring in this way, the odor measuring device 100 can measure odor substances contained in the gas with high accuracy.
[0173] As an example, in Figures 10 and 11, a set of electrodes (first metal wiring 313C and second metal wiring 313D) is arranged on a single substrate 311, but multiple sets of electrodes may be arranged side by side on a single substrate.
[0174] (Area definition process) Next, coating regions for coating each of the multiple types of slurries are defined on the substrate on which the electrodes are disposed. The coating regions may be defined, for example, by disposing a resist. Furthermore, in the coating step, when the slurry is dropped from a nozzle, the coating regions may be defined in accordance with the nozzle diameter. The resist M is disposed so as to define the coating region 330. In the coating region 330, the substrate 311 is exposed.
[0175] The size of the coating area 330 may be specified to be the same for each of the multiple types of slurries. That is, even if the mixing ratio of the conductive carbon material and the resin composition is different for each slurry, the area of the coating area 330 for coating the slurry may be uniform. In this way, even if multiple types of slurries with different mixing ratios are used, the variation in the area of the multiple types of odorant receiving layers 315 after drying is reduced.
[0176] The coated area 330 is circular as an example, but the shape of the coated area 330 is not limited thereto. The coated area 330 may be circular or strip-shaped. This forms a circular or strip-shaped odorant receiving layer 315.
[0177] When the shape of the coating region 330 is circular, the diameter of the circle may be 0.2 mm or more and 5 mm or less, and when the shape of the coating region 330 is strip-shaped, the length of the strip in the short direction may be 0.2 mm or more and 5 mm or less. This forms a circular odorant receiving layer 315c with a diameter of 0.2 mm or more and 5 mm or less, and a circular odorant receiving layer 315d with a strip length in the short direction of 0.2 mm or more and 5 mm or less.
[0178] The method by which the resist M is applied is not particularly limited, but examples include a method in which the solder resist is silk-screened in a specified area and then UV-cured, a method in which a resist film is attached to a substrate, and a method in which only the resist in a specified area is cured and the uncured portion is removed.
[0179] (Coating process) Next, each of the multiple types of slurries is applied to the application region 330. The method of applying the slurry can be a conventionally known method, and the slurry may be dropped from a nozzle, sprayed, or spin-coated. The method of applying the slurry is particularly preferably a method of dropping the slurry from a nozzle, and a desired application shape can be obtained by using, for example, a SUS metal needle nozzle (inner diameter 0.1 mmΦ, outer diameter 0.23 mm) on an IMAGE MASTER 350 PC Smart manufactured by Musashi Engineering Co., Ltd.
[0180] (drying process) Finally, the slurry applied to the application area 330 is dried to form the odorant receiving layer 315. The method for drying the slurry is not particularly limited, but for example, a method can be used in which the slurry is heated at 100°C at normal pressure for 1 hour by infrared heating, and then heated at 100°C for 1 hour while reducing the pressure in a vacuum dryer.
[0181] (Odor permeable layer adjustment process) By kneading various resin compositions with NMP, a solution containing the resin for the odorant-permeable layer 317 is prepared. Note that by repeating the kneading process many times, the porosity of the cross section of the odorant-permeable layer 317 decreases.
[0182] (Overlay of odorant permeable layer 317) A solution of resin for the odorant permeation layer 317 is applied onto the dried odorant reception layer 315. At this time, care is taken to ensure that no gaps are formed between the odorant reception layer 315 and the odorant permeation layer 317. The application method can be the same as the method described above in the (application step). The drying method after application can also be the same as the method described above in the (drying step).
[0183] <Example of software implementation> The control block (particularly the control unit 1) of the estimation device 10, 10a may be realized by a logic circuit (hardware) formed on an integrated circuit (IC chip) or the like, or may be realized by software.
[0184] In the latter case, the estimation device 10, 10a includes a computer that executes instructions of a program, which is software that realizes each function. The computer includes, for example, one or more processors, and a computer-readable recording medium that stores the program. The object of the present invention is achieved by the processor reading the program from the recording medium and executing it in the computer. The processor may be, for example, a CPU (Central Processing Unit). The recording medium may be a "non-transient tangible medium", such as a ROM (Read Only Memory), a tape, a disk, a card, a semiconductor memory, a programmable logic circuit, or the like. The device may further include a RAM (Random Access Memory) that expands the program. The program may be supplied to the computer via any transmission medium (such as a communication network or a broadcast wave) that can transmit the program. Note that one aspect of the present invention may also be realized in the form of a data signal embedded in a carrier wave, in which the program is embodied by electronic transmission.
[0185] 〔summary〕 The sensor element according to the first aspect of the present disclosure comprises an odorant receiving layer including a resin composition including a resin (A) and a filler (B), a first metal wiring in contact with at least a portion of the odorant receiving layer, a second metal wiring spaced apart from the first metal wiring and in contact with at least a portion of the odorant receiving layer, and an odorant permeation layer covering at least a portion of the odorant receiving layer opposite the side in contact with the first metal wiring and the second metal wiring, wherein the odorant permeation layer is made of R1-SiO 3 / 2 and R2-SiO 1 wherein R1 is a hydrocarbon group having 1 to 18 carbon atoms.
[0186] The sensor element according to aspect 2 of the present disclosure is the sensor element according to aspect 1, wherein at least a portion of the odorant-permeable layer is in the form of a thin film having a thickness of 0.1 μm or more and 50 μm or less.
[0187] The sensor element according to aspect 3 of the present disclosure is the sensor element according to aspect 1 or 2, wherein the odorant receptive layer is made of R-SiO 3 / 2 The composition may not include a composition having a structure represented by the formula:
[0188] The sensor element according to aspect 4 of the present disclosure is any one of aspects 1 to 3, wherein at least a portion of the odorant receiving layer is in the form of a thin film having a thickness of 1 μm or more and 50 μm or less.
[0189] A sensor element according to a fifth aspect of the present disclosure is the sensor element according to any one of the first to fourth aspects, in which the filler (B) is a conductive carbon material.
[0190] A sensor element according to a sixth aspect of the present disclosure is any one of the first to fifth aspects, wherein R1 may be one or more of a methyl group, an aliphatic hydrocarbon group, and an aromatic group.
[0191] A sensor element according to aspect 7 of the present disclosure is any one of aspects 1 to 6 above, wherein R2 may be one or more of a hydrogen atom, a methyl group, an alkyl group, an amino group, a hydroxyl group, a carboxyl group, a fluoromethyl group, a polyester group, and a polyether group.
[0192] The sensor element according to aspect 8 of the present disclosure, in any one of aspects 1 to 7 above, may have a content of the filler (B) of 10 to 50% by weight, where the total amount of the resin (A) and the filler (B) is taken as 100% by weight.
[0193] An odor measuring device according to a ninth aspect of the present disclosure includes a plurality of sensor elements according to any one of the first to eighth aspects. EXAMPLES
[0194] The present invention will be further described below with reference to Examples and Comparative Examples, but the present invention is not limited thereto. Unless otherwise specified, % represents % by weight and part represents part by weight.
[0195] <R1-SiO 3 / 2 > The following were used. S1: KR-271 (methyl / phenyl silicone resin) S2: KR-480 (methyl / phenyl silicone resin) S3: KR-251 (methyl silicone resin) All of the above are manufactured by Shin-Etsu Chemical Co., Ltd.
[0196] <R2-SiO 1 > The following were used. S4: KF3935 (side-chain higher aliphatic amide-modified silicone oil) S5: X22-3710 (one-terminal carboxyl group-modified silicone oil) S6: X22-1877 (side-chain alkyl·aralkyl-modified silicone oil) S7: FL-100-1000cs (fluoromethyl-containing modified silicone oil) S8: KF-6123 (polyether, hydroxyl group-containing modified silicone oil) All of the above are manufactured by Shin-Etsu Chemical Co., Ltd.
[0197] Also, as R2-SiO 1 S9 obtained as follows was used. <Preparation of S9> Into a glass flask, 300 parts of xylene, 20 parts of KF-101 (glycidyl group-modified silicone oil) manufactured by Shin-Etsu Chemical Co., Ltd., and 0.04 part of dibutyltin were added to 100 parts of FINEDIC FD-305 (polyester resin) manufactured by DIC Corporation. After reacting for 12 hours under reflux conditions at 140 °C, it was cooled and isopropyl alcohol was gradually added. When it became cloudy, the unnecessary components were filtered off and dried. When the structure was confirmed by NMR, it was confirmed that the obtained product was polyester-modified silicone oil (S9).
[0198] <Other resins> Z1: PEG4000 (polyethylene glycol) manufactured by Fujifilm Wako Pure Chemical Corporation.
[0199] <Resin (A)> A5: Mobilta B14S (polyvinyl butyral resin) manufactured by Kuraray Co., Ltd.
[0200] <Preparation of A6> [Preparation of polyester amide (A6)] Into a reaction vessel equipped with a condenser, a water separator, a heating and cooling device, a thermometer, a stirrer, and a nitrogen inlet tube, 150 parts of xylene and 120 parts of a 20% aqueous solution of polyallylamine (「PAA-03」manufactured by Nittobo Medical Co., Ltd., average molecular weight of about 3,000) were charged, and the temperature was raised to 160 °C. Water was distilled off using the water separator. At this time, the xylene separated from the water flowed back into the reaction solution. Then, 72 parts of the polyester resin (PE-1) obtained in Production Example 1, which had been heated to 160 °C, was charged, and the reaction was carried out at 160 °C for 2 hours. Next, it was heated at 160 °C for 0.5 hour, the xylene was distilled off, and the remaining resin was taken out. The taken-out resin was cooled to room temperature and then pulverized into particles to obtain a polyester amide resin (A6). The number average molecular weight (Mn) of the polyester amide resin (A6) was 10,000, and the acid value was 0.3 mg KOH / g.
[0201] <Solvent> Ethanol, d-limonene, ethyl acetate, and NMP (N-methylpyrrolidone) manufactured by Tokyo Chemical Industry Co., Ltd. were used.
[0202] <Filler> CB: Carbon Black SUPER C65 Made by MTI Corporation.
[0203] <Receptor layer resin composition 1> Table 1 shows the substances contained in the resin compositions 1 to 4 used in the odorant receiving layer (hereinafter, receiving layer resin compositions) and the composition ratios of the substances. Resin for receiving layer: A1 70 parts by weight Filler: CB 30 parts by weight NMP: 400 parts by weight The mixture of the above-mentioned receiving layer resin, filler and NMP was stirred at 2000 rpm for 20 minutes using a centrifugal mixer (ARE-310 manufactured by Thinky Corporation) to obtain receiving layer resin composition 1 as a slurry.
[0204] For receiving layer resin compositions 2 to 4, which have different compositional ratios of the substances contained therein, slurries were prepared in the same manner as for receiving layer resin composition 1, with the composition ratios shown in Table 1.
[0205] [Table 1]
[0206] <Creating sensor element E1-5> Table 2 shows the correspondence between the sensor elements (E1-5) to (E-25) and the compositions of the odorant receiving layer and odorant permeation layer. An odorant receiving layer was formed on the sensor substrate K-1 prepared using a coating device equipped with a SUS metal needle nozzle (inner diameter 0.1 mmΦ, outer diameter 0.23 mm) attached to an IMAGE MASTER 350 PC Smart manufactured by Musashi Engineering Co., Ltd. An appropriate amount of the receiving layer resin composition 1 was dropped and applied to the metal wiring portion. After application, the coating was dried for 3 hours in a circulating air dryer heated to 100°C.
[0207] Next, using the same coating equipment, R1-SiO 3 / 2An appropriate amount of composition S1 represented by the formula (I) was applied to the film to obtain the thickness shown in Table 2, and an odorant permeable layer was arranged to cover the odorant receiving layer. After application, the film was dried for 3 hours in a circulating air dryer heated to 100°C. After drying, the film was cooled to room temperature to prepare a sensor element (E1-5). The same operation was repeated 10 times to prepare 10 pieces for each sensor element.
[0208] <Fabrication of sensor elements E1-6 to E1-13, E1-17, E1-18, and E1-20> Sensor elements E1-6 to E1-13, E1-17, E1-18, and E1-20 were produced in the same manner as sensor element E1-5, except that the odorant receiving layer and odorant permeation layer had the compositions shown in Table 2.
[0209] <Fabrication of sensor elements E1-14 to E1-16, E1-21 to E1-24> R1-SiO for odorant permeation layer 3 / 2 Instead of the composition S1 represented by the formula: R1-SiO 3 / 2 and 8 parts of the composition S1 represented by the formula: 1 Two parts of each of compositions S4 to S9 represented by the formula: were premixed to obtain mixtures. Except for using these mixtures, sensor elements E1-14 to E1-16 and E1-21 to E1-24 were produced with odorant receiving layers and odorant permeation layers having the compositions shown in Table 2 in the same manner as in producing sensor element E1-5.
[0210] <Fabrication of sensor element E1-19> Sensor element E1-19 was produced in the same manner as sensor element E1-5, except that only the odorant receptive layer was formed and no odorant permeable layer was formed.
[0211] <Preparation of sensor element E1-25> Sensor element E1-25 was produced in the same manner as sensor element E1-24, except that only the odorant receptive layer was formed and no odorant permeable layer was formed.
[0212] [Table 2]
[0213] <Construction of odor sensors 13 to 33> We created a housing equipped with a target sample receiving section equipped with an inlet for introducing the sample (odor substance) and an aluminum block thermostatic bath for temperature control, a nitrogen gas cylinder for gas supply, a mass flow controller, and a sensor chamber. The volume of the target sample receiving section was designed to be five times the volume of the sensor chamber.
[0214] Lead wires for taking out the sensor terminals to the outside were soldered to each of the sensor elements (E1-5) to (E1-25), and 24 sensor elements (E1-5) to (E1-25) were placed in each sensor chamber. A 5V constant voltage power supply and a 300Ω fixed resistor were connected in series to the ends of the lead wires taken out of the sensor chamber for each of the sensor elements (E1-5) to (E1-25), and a voltmeter was connected to measure the voltage across both terminals of the sensor element. In this way, odor sensors 13 to 33, each having 24 sensor elements (E1-5) to (E1-25), were constructed.
[0215] <Preparation of test samples> 0.01 g of ethanol, 0.05 g of d-limonene, and 0.02 g of ethyl acetate were introduced into an aluminum laminate gas bag (AA-10, GL Sciences) using a microsyringe, followed by 10 L of nitrogen gas. The gas bag was left at 40°C for 3 hours and then at room temperature for 9 hours to produce various organic solvent gases (1x). Furthermore, these gases were diluted with nitrogen gas at the following dilution ratios. Dilution ratios: 1.5x, 2x, 2.5x, 3x, 3.5x, 4x, 4.5x, 5x, 6x, 7x, 8x, 9x, 10x, 11x, 12x, 13x, 14x, 15x, 16x, 17x.
[0216] <Examples 1-9 to 1-26 and Comparative Examples 2 to 4> [Measurement of various organic solvent gases] For each of the odor sensors 13 to 33 installed in the laboratory (temperature 23°C, humidity 40%), the temperature inside the target sample receiving section was adjusted to 30°C using an aluminum block thermostatic bath. Then, one type of organic solvent gas with each dilution ratio that had been adjusted in advance as an odorant (sample) was placed into the inlet of the odor sensor. Then, nitrogen was flowed from the nitrogen gas cylinder for gas supply into the target sample receiving section at a flow rate of 1 L / min by the mass flow controller for 15 seconds, and discharged to the outside via the sensor chamber. Then, the nitrogen gas was directly flowed from the nitrogen gas cylinder into the sensor chamber at a flow rate of 1 L / min by the mass flow controller for 60 seconds without passing through the target sample receiving section, and discharged to the outside as it is. This operation removed the odorant attached to the sensor element. From the start of the introduction of the organic solvent gas to the completion of the removal of the odorant, the measured values of the voltmeter connected to the sensor element were recorded in the computer at a sampling rate of 100 Hz. In this way, the time change in the voltage value of each of the 24 sensor elements in the odor sensor was measured. This odor measurement procedure was repeated 16 times for each odor sensor.
[0217] [Measurement of the dilution ratio of the detection limit] For each sensor element, the maximum value ΔV of the difference between the output voltage V0 before the introduction of the sample and the voltage V during the introduction of the sample was calculated. The output voltage at this time was Vmax. The measurement period was set to include the voltage region before the introduction of the sample and the maximum voltage region during the introduction of the sample. In addition, the measurement value at a certain point in time was the arithmetic average value of the voltage data for 0.1 s before and after the point in time. The time region for taking the average value can also be 10 times the inverse of the sampling rate (Hz) (i.e., 10 points of data are obtained). In addition, the ratio of the standard deviation of the 10 points of data at the time of measurement to the output voltage V0 before the introduction of the sample and ΔV (how many times the standard deviation ΔV corresponds to) was taken. When the average of 16 times of this ratio was 3 times or more, it was determined that the sensor element was able to detect the sample at the dilution ratio used, and the measurement using the sample with the dilution ratio changed until the sensor element could no longer detect the sample was repeated to obtain the dilution ratio of the detection limit. In addition, the same measurement was performed for each sample prepared.
[0218] [Evaluation of repeatability] FIG. 13 is a graph for explaining the operation for obtaining Tz, with the vertical axis indicating voltage value and the horizontal axis indicating time. In FIG. 13, X indicates the change in the measured voltage value, and T0 indicates the time when the introduction of the specimen into the target sample receiving section was started. Hereinafter, the evaluation method and results of repeatability will be explained with reference to FIG. 13. Measurements were performed on sensor elements E1-5 to E1-25 using a sample diluted 1.5 times with ethanol, and the obtained voltage values were plotted against time. The obtained plot was subjected to the following processes 1 to 5 to obtain Tz. 1. Calculate T1. T1 is the time when nitrogen gas starts to flow from the nitrogen gas cylinder for cleaning after the sample is introduced into the sensor chamber. 2. On a graph obtained based on the plot (for example, the graph shown in FIG. 13), a line L1 is drawn that passes through the time (T0) when the sample introduction began and touches the vertical axis at a value higher than the voltage value V0. 3. As shown in "Operation A" in Figure 13, the set line L1 is asymptotically moved from the bottom of graph X until it touches the baseline (the line that passes through voltage value V0 and is parallel to the horizontal axis). Draw a vertical line from L1 obtained in 4.3, determine the point of intersection with the plot on graph X, and determine the time (T2) corresponding to the intersection point on the plot where a line segment can be drawn such that the distance between L1 and the plot is 10% of Vmax. 5.Let Tz be the difference between T2 and T1.
[0219] As can be seen from the above, T2 indicates the timing when the output voltage V rises and then falls to a value close to V0, specifically 10% of Vmax, when a measurement is performed using the sensor element, that is, the timing when it becomes possible to perform another measurement using the sensor element. Also, Tz indicates the time from T1 to T2, that is, the time when the output voltage V falls after reaching the maximum value Vmax and becomes possible to perform the next measurement. The timing when the output voltage V starts to fall can be considered to indicate the timing when the sample starts to be removed from the target sample receiving section. Therefore, Tz can also be expressed as indicating the time from when the sample starts to be removed from the target sample receiving section to when the next measurement can be performed. From the above, it can be said that the smaller Tz is, the shorter the time it is possible for the sensor element to perform the next measurement after performing one measurement. Therefore, it can be said that the smaller Tz is, the easier it is for the sensor element to remove the odor substance to be measured. In other words, it can be said that it is easier to perform a larger number of repeated measurements within a certain period of time. Note that when repeated measurements are performed, T1, T2, and Tz are defined for each measurement. In addition, if the length, diameter, and volume of the piping and sensor chamber are different between odor sensors, the timing of gas switching and the timing of gas hitting the sensor element may differ, which may affect the results. Therefore, the above-mentioned Tz measurement was performed using odor sensors configured under the same conditions except for the sensor element.
[0220] [Table 3]
[0221] Comparison of Examples 1-9 and Comparative Example 2 As shown in Table 3, although the composition of the odorant receiving layer was the same, R1-SiO 3 / 2Although there is no significant difference in Tz between Example 1-9 having an odorant-permeable layer containing a composition having a structure represented by the formula (1) and Comparative Example 2 not having the odorant-permeable layer, the Example group shows a higher dilution ratio of each organic solvent gas. Therefore, it can be said that the sensor element corresponding to Example 1-9 having the configuration according to the present invention has achieved improved measurement accuracy and improved responsiveness. The sensor elements according to Examples 1-10 to 1-26 also showed a similar tendency.
[0222] Comparison of Examples 1-9 and Comparative Example 3 As shown in Table 3, the odorant receiving layer had the same composition, but the odorant permeation layer was made of R1-SiO 3 / 2 In Example 1-9 having the above composition and Comparative Example 3 having the other composition, the Example group shows better results in terms of both the dilution ratio of each organic solvent gas and Tz. Therefore, it can be said that the sensor element according to Example 1-9 having the configuration according to the present invention can achieve improved measurement accuracy and improved responsiveness. In addition, the sensor elements according to Examples 1-10 to 1-26 also showed the same tendency as the sensor element according to Example 1-9.
[0223] Comparison of Examples 1-9 and Comparative Example 2 As shown in Table 3, although the composition of the odorant receiving layer was the same, R1-SiO 3 / 2 Although there is no significant difference in Tz between Example 1-26 having an odorant permeable layer containing a composition having a structure represented by the formula (1) and Comparative Example 4 not having such a layer, Example 1-26 shows a higher dilution ratio of each organic solvent gas. Therefore, it can be said that the sensor element corresponding to Example 1-26 having the configuration according to the present invention has improved measurement accuracy and improved responsiveness. [Industrial Applicability]
[0224] The present invention is useful as an odor identification sensor for medical use, gas detection, agriculture, and other industrial and daily uses. For example, farmers can use the odor identification sensor to determine the maturity of fragrant crops and manage the optimal harvest timing. In addition, the odor identification sensor can be used to digitize the odors of products such as food and cosmetics, helping to improve the efficiency of product development and stabilize quality. [Explanation of symbols]
[0225] 10, 10a Estimation device 11 Measurement value acquisition unit (acquisition unit) 12 Change pattern analysis section (analysis section) 16 Estimation part 30 Odor Sensor 31A Multiple sensor elements (sensor element group) 31, 31b, 31c Sensor element 32 Constant voltage power supply (power supply) 33 Voltmeter (measuring instrument) 100, 100a Odor measuring device 313A, 313C 1st metal wiring 313B, 313D 2nd metal wiring 315, 315c, 315d Odorant receptor layer 317 Odor-permeable layer 50 Target sample receiving section 51 Adjustment section 60 Sensor Chamber 80 Gas supply section 91, 92, 93, 94 Body 501 1st mouth 502 2nd mouth 503 Sample inlet
Claims
1. An odorant receiving layer comprising a resin composition comprising a resin (A) and a filler (B); A first metal wiring in contact with at least a portion of the odorant receiving layer, and a second metal wiring spaced apart from the first metal wiring and in contact with at least a portion of the odorant receiving layer; an odorant permeable layer that covers at least a portion of the odorant receiving layer on the side opposite to the side in contact with the first metal wiring and the second metal wiring; Equipped with The odorant permeable layer is R1-SiO 3/2 and R2-SiO 1 The composition includes at least one of the structures represented by R1 is a hydrocarbon group having 1 to 18 carbon atoms. A sensor element for an odor measuring device.
2. 2. The sensor element for an odor measuring device according to claim 1, wherein the odorant permeable layer is a thin film having a thickness of 0.1 μm or more and 50 μm or less.
3. The odorant receiving layer is made of R-SiO 3/2 The sensor element for use in an odor measuring device according to claim 1 , which does not contain a composition having a structure represented by the formula:
4. 2. The sensor element for an odor measuring device according to claim 1, wherein the odorant receiving layer is a thin film having a thickness of 1 μm or more and 50 μm or less.
5. 2. The sensor element for an odor measuring device according to claim 1, wherein the filler (B) is a conductive carbon material.
6. 2. The sensor element for use in an odor measuring device according to claim 1, wherein R1 includes one or more functional groups selected from the group consisting of an aliphatic hydrocarbon group and an aromatic group.
7. 2. The sensor element for an odor measuring device according to claim 1, wherein R2 includes one or more functional groups selected from the group consisting of a hydrogen atom, an amide group, a methyl group, an alkyl group having 1 to 12 carbon atoms, an aralkyl group having 1 to 12 carbon atoms, an amino group, a hydroxyl group, a carboxyl group, a fluoromethyl group, a polyester group, and a polyether group.
8. The content of the filler (B) is 10 to 50% by weight, when the total amount of the resin (A) and the filler (B) is 100% by weight. A sensor element for use in an odor measuring device according to claim 1.
9. A sensor element according to any one of claims 1 to 6, Odor measuring device.
Citation Information
Patent Citations
Return electrode monitor apparatus
JP1983103445A
Carbon dioxide gas sensor
JP2000235012A
Resin composition for forming odor substance receptive layer, sensor element using the same, odor sensor, and odor measurement device
JP2022045329A
An encased polymer nanofiber-based electronic nose
US20160195488A1
Gas detection system
WO2022196708A1
Cited By
Resin composition for forming odorant-accepting layer, sensor element using same, odor sensor, and odor measuring device