Air pocket structures for promoting total internal reflection in waveguide

By applying a cap layer with optical gas cavities to a waveguide, the challenge of maximizing projected light transmission and minimizing ambient light reflection is addressed, enhancing image clarity and brightness in virtual reality devices.

JP2024169435AActive Publication Date: 2024-12-05MAGIC LEAP INC
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2024139589
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2018-12-21
Filing Date
2024-08-21
Publication Date
2024-12-05
Estimated Expiration
2039-12-20

AI Technical Summary

Technical Problem

Existing virtual reality viewing devices face challenges in maximizing the transmission of projected light while minimizing ambient light reflection, leading to reduced image clarity and brightness.

Method used

A cap layer of selective transparent material is applied to a waveguide of high refractive index transparent material, forming a cavity filled with optical gas to enhance light absorption and reduce ambient light reflection.

Benefits of technology

The solution improves light transmission and reduces reflections, resulting in sharper and brighter images by maximizing the refractive index difference and minimizing ambient light interference.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024169435000001_ABST
    Figure 2024169435000001_ABST
Patent Text Reader

Abstract

To provide favorable air pocket structures for promoting total internal reflection in a waveguide.SOLUTION: Recesses are formed on a front side and a rear side of a waveguide. A solid porogen material is spun onto the front side and the rear side and fills the recesses. First front and rear cap layers are then formed on raised formations of the waveguide and on the solid porogen material. The entire structure is then heated and the solid porogen material decomposes into a porogen gas. The first front and rear cap layers are porous to allow the porogen gas to escape and to allow air to enter into the recesses. The air maximizes a difference in refractive indices between a high-index transparent material of the waveguide and the air to promote reflection in the waveguide from interfaces between the waveguide and the air.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] (CROSS REFERENCE TO RELATED APPLICATIONS) This application claims priority to U.S. Provisional Patent Application No. 62 / 783,778, filed December 21, 2018, the entirety of which is incorporated herein by reference in its entirety.

[0002] The present invention relates generally to optical systems and methods for manufacturing optical systems. [Background technology]

[0003] Modern computing and display technology has encouraged the development of so-called "virtual reality" viewing devices. Such viewing devices typically have a frame that is mountable on a user's head, and frequently contain two waveguides, one in front of each eye of the viewer. The waveguides are transparent so that ambient light from an object can transmit through the waveguides, making the object visible to the user. Each waveguide also serves to transmit projected light from a projector to a respective eye of the user. The projected light forms an image on the retina of the eye. The retina of the eye thus receives the ambient light and the projected light. The user sees the real object and the image produced by the projected light simultaneously.

[0004] The projected light typically enters the waveguide on the edge of the waveguide, then reflects within the waveguide, and then exits the waveguide through the waveguide pupil towards the user's eye. Total internal reflection (TIR) ​​is the ideal situation where there is no loss of projected light out of the waveguide, and 100 percent of the projected light reaches the user's eye. Summary of the Invention [Means for solving the problem]

[0005] The present invention provides a method of manufacturing an optical system that includes adhering a cap layer of a selectively transparent material to a waveguide of a high refractive index transparent material having a front side and a rear side, such that when an ambient light source is located at the front side of the waveguide, a cavity is defined between the cap layer and the waveguide with an optical gas in the cavity, such that a beam of ambient light transmits through the selectively transparent material of the cap layer, through the cavity holding an optical gas, and through the high refractive index transparent material of the waveguide.

[0006] The present invention also provides an optical system including a waveguide of a high refractive index transparent material having a front side and a rear side, a cap layer of a selectively transparent material affixed to the waveguide, a cavity being defined between the cap layer and the waveguide, and an optical gas in the cavity such that when an ambient light source is located at the front side of the waveguide, a beam of ambient light is transmitted through the selectively transparent material of the cap layer, through the cavity holding the optical gas, and through the high refractive index transparent material of the waveguide. The present specification also provides, for example, the following items: (Item 1) 1. A method of manufacturing an optical system, comprising the steps of: affixing a cap layer of a selectively transparent material to a waveguide of a high refractive index transparent material having a front side and a rear side, wherein a cavity is defined between the cap layer and the waveguide with an optical gas in the cavity such that when an ambient light source is located at the front side of the waveguide, a beam of ambient light is transmitted through the selectively transparent material of the cap layer, through the cavity holding an optical gas, and through the high refractive index transparent material of the waveguide, with an optical gas in the cavity; A method comprising: (Item 2) 2. The method of claim 1, wherein the cap layer is a front cap layer located between the ambient light source and a front side of the waveguide, and the beam of ambient light is transmitted sequentially through a selective transparent material of the front cap layer, through the cavity holding the optical gas, and into a high refractive index transparent material of the waveguide. (Item 3) 3. The method of claim 2, wherein the selected transparent material of the front cap layer is an anti-reflective material that increases absorption of the ambient light by the front surface of the waveguide and reduces reflection of the ambient light by the front surface of the waveguide. (Item 4) 4. The method of claim 3, wherein the high refractive index material is one of high refractive index glass, high refractive index lithium niobate, lithium tantalate, and silicon carbide. (Item 5) 4. The method of claim 3, wherein the high refractive index material has a refractive index of at least 1.74. (Item 6) 2. The method of claim 1, wherein the optical gas has a refractive index of less than 1.3. (Item 7) 2. The method according to claim 1, wherein the optical gas is air with a refractive index of 1. (Item 8) forming a stack including the waveguide, a solid porogen material, and the cap layer; replacing said porogen material with said optical gas; The method of claim 1, further comprising: (Item 9) The porogen material is heating the porogen material to a decomposition temperature at which the porogen material is converted into a sacrificial gas; removing the sacrificial gas from the cavity; and 9. The method according to item 8, wherein the ion exchange resin is removed by carrying out the steps of: (Item 10) 10. The method of claim 9, wherein the selected material of the cap layer is porous and the sacrificial gas outgases through the selected material of the cap layer. (Item 11) 10. The method according to claim 9, wherein the porogen material decomposes at a decomposition temperature of 120°C to 230°C. (Item 12) Item 11. The method of item 10, wherein the cap layer is made of SiOx having a thickness of at least 12 nm, where x is a variable. (Item 13) Item 10. The method of item 1, wherein a plurality of cavities are defined between the cap layer and the waveguide, and an optical gas is in each respective cavity. (Item 14) forming a front side of the waveguide having a plurality of recesses and a plurality of raised formations, each raised formation being located between two of the recesses; supporting the first portions of the cap layer with the ridge formations, with the second portions of the cap layer located between the first portions of the cap layer and across the recesses, such that respective ones of the cavities are defined by respective ones of the second portions of the cap layer and respective ones of the recesses at the front side of the waveguide; Item 14. The method of item 13, further comprising: (Item 15) Item 15. The method of item 14, wherein each recess has a depth and a width, the width being less than 300 microns. (Item 16) Item 15. The method according to item 14, wherein the recess is imprinted on the front side. (Item 17) forming a conformal layer on a front side of the waveguide, the conformal layer being made of a transparent material; 15. The method of claim 14, further comprising: (Item 18) the cap layer is a front cap layer located between the ambient light source and the front side of the waveguide, and the cavity is a front cavity between the front cap layer and the front side of the waveguide; affixing a rear cap layer of selectively transparent material to the waveguide, such that when an ambient light source is located at a front side of the waveguide, a rear cavity is defined between the rear cap layer and the rear of the waveguide with an optical gas present in the rear cavity such that a beam of ambient light is transmitted through the high index transparent material of the waveguide, through the rear cavity holding the optical gas, and through the selectively transparent material of the rear cap layer. The method of claim 1, further comprising: (Item 19) the cap layer is a first cap layer and the selectively transparent material is a first selectively transparent material; bonding a second cap layer of a second selected transparent material to the first cap layer. The method of claim 1, further comprising: (Item 20) 20. The method of claim 19, wherein the second cap layer is harder than the first cap layer. (Item 21) 20. The method of claim 19, wherein at least one of the selected transparent materials of the cap layer is an anti-reflective material that increases absorption of the ambient light by the front surface of the waveguide and reduces reflection of the ambient light by the front surface of the waveguide. (Item 22) Forming a stack of cap layers having refractive indices that vary in magnitude 22. The method of claim 21, further comprising: (Item 23) 23. The method of claim 22, wherein the cap layer is made of SiOx having a refractive index of 1.45 and TiOx having a refractive index of 2.2 to 2.3, where x is a variable. (Item 24) 1. An optical system comprising: a waveguide of a high refractive index transparent material having a front side and a rear side; a cap layer of a selectively transparent material affixed to the waveguide, a cavity being defined between the cap layer and the waveguide; an optical gas in the cavity, the optical gas in the cavity being such that when an ambient light source is located at a front side of the waveguide, the beam of ambient light transmits through a selective transparent material of the cap layer, through the cavity holding the optical gas, and through a high refractive index transparent material of the waveguide; An optical system comprising: [Brief description of the drawings]

[0007] The invention will further be described, by way of example only, with reference to the accompanying drawings in which:

[0008] [Figure 1A] FIG. 1A is a cross-sectional side view of a waveguide of high refractive index transparent material.

[0009] [Figure 1B] FIG. 1B is a view similar to FIG. 1A after the waveguide has been patterned to have multiple recesses and raised formations on the front and rear sides.

[0010] [Figure 1C] FIG. 1C is a view similar to FIG. 1B after the recesses have been filled with solid porogen material in a spin-on process.

[0011] [Figure 1D] FIG. 1D is a view similar to FIG. 1C after a first front cap layer has been formed on the front side and a first rear cap layer has been formed on the rear side.

[0012] [Figure 1E] FIG. 1E is a view similar to FIG. 1D after the structure has been heated to remove the solid porogen material and replace it with air.

[0013] [Figure 1F] FIG. 1F is a view similar to FIG. 1E after additional cap layers have been formed over the first front and first back cap layers to complete the fabrication of the optical system.

[0014] [Figure 1G] FIG. 1G is a view similar to FIG. 1F of the optical system, illustrating its function.

[0015] [Figure 1H] FIG. 1H is a cross-sectional side view of an optical system in accordance with an alternative embodiment of the invention in which the patterned layer is formed from a photoresist material.

[0016] [Diagram 2]FIG. 2 is a cross-sectional side view of an optical system according to an alternative embodiment of the invention having nanostructures to aid in the absorption of ambient light.

[0017] [Diagram 3] FIG. 3 is a cross-sectional side view similar to FIG. 1F with nanostructures having variable feature heights or variable duty cycles.

[0018] [Figure 4] FIG. 4 is a cross-sectional side view similar to FIG. 2 having nanostructures with variable feature height or variable duty cycle.

[0019] [Diagram 5] FIG. 5 is a cross-sectional side view of an optical system having air pockets in different layers.

[0020] [Figure 6A] FIG. 6A is a scanning electron microscope (SEM) image with a single coating.

[0021] [Figure 6B] FIG. 6B is an SEM image of an air pocket covered by a multi-layer coating.

[0022] [Figure 7A] FIG. 7A is a cross-sectional side view of an air pocket that has been covered with a silicon oxide layer and then spin-coated with an optical polymer.

[0023] [Figure 7B] FIG. 7B is a similar view to FIG. 7A at a lower magnification level.

[0024] [Figure 8] FIG. 8 is a 0° transmission graph from an experimental measurement.

[0025] [Figure 9] FIG. 9 is the model used for simulation purposes.

[0026] [Figure 10A] FIG. 10A is a side view of a waveguide without any coating for the simulation.

[0027] [Figure 10B] FIG. 10B is a side view of a waveguide with an optical polymer coating for the simulation.

[0028] [Figure 10C] FIG. 10C is a side view of a waveguide with an air pocket for the simulation.

[0029] [Figure 10D] FIG. 10D is a side view of a waveguide with polymer instead of an air gap for the simulation.

[0030] [Figure 11] FIG. 11 is a graph showing transmission data from the simulation.

[0031] [Figure 12] FIG. 12 is a graph showing user side diffraction efficiency from a simulation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0032] An optical system and a method for making the optical system are described. Recesses are formed on the front and rear sides of a waveguide. Solid porogen material is spun on the front and rear sides, filling the recesses. First front and rear cap layers are then formed on the ridge formations of the waveguide and the solid porogen material. The entire structure is then heated, and the solid porogen material decomposes into porogen gas. The first front and rear cap layers are porous, allowing the porogen gas to escape and air to enter the recesses. The air maximizes the refractive index difference between the high index transparent material of the waveguide and the air, encouraging reflections within the waveguide from the interface between the waveguide and the air. Second front and rear cap layers are formed on the first front and rear cap layers, respectively, and additional front and rear cap layers are then formed on the second front and rear cap layers. The cap layer has a refractive index that aids in the absorption of ambient light through the cap layer and into the waveguide.

[0033] 1A-1F illustrate a method of manufacturing an optical system according to one embodiment of the present invention.

[0034] FIG. 1A illustrates a waveguide 20, which serves as a primary substrate for subsequent processing. The waveguide 20 is made from a high index transparent material. Generally, the refractive index of the waveguide 20 is believed to be at least 1.5. In this embodiment, the waveguide 20 is made from a high index glass, which has a refractive index of 1.73. In another embodiment, the waveguide may be made from lithium niobate, lithium tantalate, or silicon carbide, which have a refractive index above 2.0. A high index transparent material is preferred, as it maximizes the field of view in the final product.

[0035] The waveguide 20 has front and back sides 22 and 24. The front and back sides 22 and 24 are spaced from each other by a thickness 26 of less than 3 mm. The front and back sides 22 and 24 each have a width 28 of 50-70 mm and a depth into the paper of 50-70 mm. The front and back sides 22 and 24 are planar surfaces that are mutually parallel planes. The material of the waveguide 20 is sufficiently soft to allow the front and back sides 22 and 24 to be formed at room temperature of 22° C. or at a moderately elevated temperature of 50° C. without the formation of microcracks or optical distortions in the material of the waveguide 20.

[0036] FIG. 1B illustrates the waveguide 20 after the front and rear sides 22 and 24 have been molded. The front side 22 is molded to have a plurality of recesses 30 and a plurality of raised formations 32, each of which is located between two of the recesses 30. The sidewalls 34 of the recesses 30 form the sidewalls of the raised formations 32. The raised formations 32 have outer surfaces 36 that are in the same plane. The recesses 30 have groove surfaces 38 that are in the same plane and parallel to the plane of the outer surface 36. Each recess 30 has a width 40 that is between 10 nm and 500 nm. The rear side 24 is molded to have a plurality of recesses 44 and a plurality of raised formations 46, each of which is located between two of the recesses 44. The sidewalls 48 of the recesses 44 form the sidewalls of the raised formations 46. The raised formations 46 have coplanar outer surfaces 50. The recesses 44 have coplanar groove surfaces 52 that are parallel to the plane of the outer surfaces 50. Each recess 44 has a width 54 that is between 10 nm and 500 nm.

[0037] The front and rear sides 22 and 24 are formed simultaneously with a tool that imprints the recesses 30 and 44 and the raised formations 32 and 46. The tool has a front portion and a rear portion made of hardened metal. The front portion has a shape that is complementary to the profile created in the front side 22 and the rear portion has a shape that is complementary to the shape created in the rear side 24. The waveguide 20 is inserted between the front and rear portions and an actuator moves the front and rear portions towards each other while a surface of the portion is used to apply pressure on the front and rear sides 22 and 24 of the waveguide 20. The waveguide 20 is then removed from the tool. The front and rear sides 22 and 24 are then etched. The etching process removes microscopic artifacts from the groove surfaces 38 and 52 and flattens the groove surfaces 38 and 52.

[0038] A thickness 58 of the waveguide 20 as measured between the outer surfaces 36 and 50 exceeds the thickness 26 of the substrate of FIG. 1A, and a thickness 60 as measured between the groove surfaces 38 and 52 is less than the thickness 26. The waveguide 20 has a thickness between 200 microns and 1 nm. Each recess 30 or 44 has a depth 62 between 10 nm and 500 nm.

[0039] 1C illustrates the waveguide 20 after a porogen (sacrificial) material has been deposited. The porogen material may be spin coated on the front side 22 and rear side 24 of the waveguide 20. The porogen material fills the recesses 30 and 44. The porogen material forms a plurality of isolated porogen portions 64 in the recesses 30 on the front side 22 and a plurality of isolated porogen portions 66 in the recesses 44 on the rear side 24. Each porogen portion 64 fills an individual recess 30 until an outer surface 68 of the porogen portion 64 is flush with the outer surface 36 of the ridge feature 32. The porogen portions 66 fill the recesses 44 until an outer surface 70 of the porogen portion 66 is flush with the outer surface 50 of the ridge feature 46.

[0040] Figure ID illustrates the structure of Figure 1C after a first front cap layer 74 and a first back cap layer 76 have been formed. The cap layers 74 and 76 may be formed, for example, in a chemical vapor deposition process.

[0041] The first front cap layer 74 is made from a selected solid transparent material. The first front cap layer 74 is formed directly on the outer surface 36 of the ridge formation 32 and the outer surface 68 of the porogen portion 64. The first front cap layer 74 also adheres to the outer surface 36 of the ridge formation 32 and is therefore secured to the waveguide 20.

[0042] The first front cap layer 74 is shown as final fabricated and is made from a relatively strong solid material. However, during its manufacture, the first front cap layer 74 is initially a thin, unstable film. Such a thin film is brittle and would collapse without the support provided by the solid material of the porogen portion 64. The first front cap layer 74 grows thicker and eventually becomes more stable as it becomes thick enough that it no longer relies on the support provided by the porogen portion 64 for its structural integrity. The first front cap layer 74 has a plurality of first portions 80 formed on the ridge formations 32 and a plurality of second portions 82 formed on the porogen portion 64.

[0043] Similarly, the first rear cap layer 76 relies on the solid material of the porogen portions 66 for support during its initial processing, but does not require the support of the porogen portions 66 after it is finally processed and acquires a thickness suitable for supporting itself without requiring the porogen portions 66. The first rear cap layer 76 has a plurality of first portions 84 formed on the ridge formations 46 and a plurality of second portions 86 formed on the porogen portions 66.

[0044] Figure 1E illustrates the structure of Figure 1D after porogen portions 64 and 66 have been removed and exited from respective cavities 88 and 90. Each cavity 88 and 90 has the same dimensions as the respective porogen portion being removed. Each cavity 88 and 90 is filled with an optical gas in the form of air.

[0045] The solid porogen material of the porogen portions 64 and 66 is a thermally decomposable material or mixture of materials that can be decomposed at a temperature that does not cause damage to the waveguide 20, the first front cap layer 74, or the first rear cap layer 76. The entire structure of FIG. 1D is heated to a decomposition temperature that converts the solid porogen material into porogen gas. The materials of the first front cap layer 74 and the first rear cap layer 76 are sufficiently porous to allow the porogen gas to permeate through the first front cap layer 74 and the first rear cap layer 76 so that the porogen gas exits the cavities 88 and 90, and air to permeate through the first front cap layer 74 and the first rear cap layer 76 into the cavities 88 and 90. For example, propylene carbonate (PPC) can be decomposed in an inert atmosphere or in air without leaving any obvious residue behind. Generally, the decomposition temperature is believed to be between 120° C. and 230° C. If a decomposition temperature of 200°C-300°C is used, the porogen moieties 64 and 66 can be displaced by air within a short amount of time. If the decomposition temperature needs to be lowered, adding additives or extending the firing time may be possible. A decomposition temperature of 120°C-160°C is possible with a suitable combination of materials, film thickness, and firing time. The firing temperature and temperature ramp rate need to be carefully controlled so that no significant residue is left behind and the release rate of the porogen gas is controlled to not cause damage such as ruptures, loosening, and cracking to the first front cap layer 74 and the first back cap layer 76.

[0046] When the cavities 88 and 90 are finally formed, the first portion 80 of the first front cap layer 74 and the first rear cap layer 76 are secured to and supported by the ridge formations 32 and 46. Each one of the cavities 88 is defined on three sides by a surface of a respective one of the recesses 30 and on a fourth side by one of the second portions 82 of the first front cap layer 74. Similarly, each one of the cavities 90 is defined on three sides by a surface of the recess 44 and on a fourth side by one of the second portions 86 of the first rear cap layer 76. It should be noted that the second portions 82 and 86 of the first front cap layer 74 and the first rear cap layer 76 are no longer supported by the porogen portions 64 and 66. However, the first front cap layer 74 and the first rear cap layer 76 are still supported by the ridge formations 32 and 46, and provided that the widths 40 and 54 of the cavities 88 and 90, respectively, are less than 500 nm, the structural integrity of the first front cap layer 74 and the first rear cap layer 76 can be preserved during and after outgassing of the solid porogen material.

[0047] 1F illustrates the structure of FIG. 1E after a second front cap layer 94 has been formed on the first front cap layer 74, and a further front cap layer 96 has been formed, in turn, on the second front cap layer 94. The second front cap layer 94 provides additional strength to the first front cap layer 74. For better adhesion, an adhesion promoter such as Valmat® or TranSpin® can be used between the first and second front cap layers 74 and 94, and between the second front cap layer 94 and the further front cap layer 96.

[0048] The second front cap layer 94 and the further front cap layer 96 are made of different selected transparent materials. One or more of the materials of the first, second and further front cap layers 74, 94 and 96 are selected to have refractive indices that promote light absorption and reduce light reflection. In a practical embodiment, the first front cap layer 74 is made of SiOx having a refractive index of 1.45, the second front cap layer 94 is made of TiOx having a refractive index of 2.2-2.3, the third front cap layer is made of SiOx and the fourth front cap layer is made of TiOx (where "x" is a variable).

[0049] FIG 1F also illustrates the structure of FIG 1E after a second rear cap layer 98 has been formed on the first rear cap layer 76, and a further rear cap layer 100 has been formed, in turn, on the second rear cap layer 98. The second rear cap layer 98 provides additional strength to the first rear cap layer 76. For better adhesion, an adhesion promoter such as Valmat® or TranSpin® can be used between the first and second rear cap layers 76 and 98, and between the second rear cap layer 98 and the further rear cap layer 100.

[0050] The second rear cap layer 98 and the further rear cap layer 100 are made of different selected transparent materials. One or more of the materials of the first, second and further rear cap layers 76, 98 and 100 are selected to have refractive indices that promote light absorption and reduce light reflection. In a practical embodiment, the first rear cap layer 76 is made of SiOx having a refractive index of 1.45, the second rear cap layer 98 is made of TiOx having a refractive index of 2.2-2.3, the third rear cap layer is made of SiOx, and the fourth front rear layer is made of TiOx (where "x" is a variable).

[0051] FIG. 1G further shows an ambient light source 102 and a projector 106. The ambient light source 102 may be, for example, an object that reflects ambient light. The ambient light is represented by beams 104A and 104B. Each beam 104A and 104B transmits through ambient air and then passes sequentially through front cap layers 96, 94, and 74, through the waveguide 20, and through rear cap layers 76, 98, and 100. The refractive index between adjacent cap layers is minimized to minimize reflection of the ambient light and to aid in absorption of the ambient light into the waveguide 20. Beam 104A also passes through air in one of the recesses 44 in the rear side 24 of the waveguide 20. Beam 104B passes through air in one of the recesses 30 in the front side 22 of the waveguide 20.

[0052] The projector 106 generates a projection light, represented by beam 104C. The beam 104C is inserted into the waveguide 20. The beam 104C may be inserted, for example, through the rear cap layers 100, 98, and 76, whose refractive indices are selected to promote the absorption of the beam 104C and limit its reflection. The beam 104C is directed into one of the recesses 30 in the front side 22. The difference between the refractive index of the waveguide 20 and the refractive index of the air in the recess 30 is maximized, promoting the reflection of the beam 104C and limiting the transmission of the beam 104C into the air in the recess 30. Air may have a refractive index of 1 and the waveguide 20 may have a refractive index of at least 1.74. The refractive indices therefore differ from each other by at least 0.74. In another embodiment, another optical gas may be used instead of air, provided that such optical gas has a refractive index less than 1.3. Ideally, the refractive index between the material of the waveguide 20 and the optical gas should be at least 0.50. The beam 104C, reflected from the air in one of the recesses 30, then transmits to one of the recesses 44 at the rear side 24 of the waveguide 20. The beam 104C reflects from the interface between the air in the recess 44 towards another of the recesses 30 at the front side 22 of the waveguide 20. An alternative structure can be a direct imprint pattern using a Si-containing resist over a spin-coated paraben material that is then evaporated. The Si-containing resist can be plasma treated to form a SiOx polymer structure.

[0053] The air interface reflection significantly improves optical image quality by: 1) improving the overall transmission of world light through the "transparent" eyepiece, making world-side objects sharper and brighter; 2) maintaining the refractive index difference between the groove-to-grating height of the relief structure, allowing for high diffraction efficiency of the grating, forming a functional waveguide relief structure; 3) reducing persistence of image artifacts from reflection of light exiting the eyepiece and reflecting back off different lenses or stacked waveguide interfaces; and 4) reducing extraneous light from diffraction into the user's eyebox, altering optical artifacts such as producing rainbow artifacts that would otherwise be much more intense without the nano-features and film stack architecture.

[0054] 1A-1G illustrate an example of producing an anti-reflective cap structure. Anti-reflective properties can also be produced using alternative methods. FIG. 1H illustrates an optical system in which front and rear patterning layers 120 and 122 are formed on the front and rear sides of the waveguide 20. The layers 120 and 122 are made of polymer or photoresist materials that may be patterned using conventional photolithography techniques or are suitable for patterning using photolithography. No additional etching steps are required. The layers are then coated with front and rear conformal layers 124 and 126, respectively. The conformal layers are made of inorganic SiOx and are formed using chemical vapor deposition. The conformal layers 124 and 126 define recesses 30 and 44, which are covered with front and rear cap layers 74 and 76.

[0055] Figure 2 illustrates an alternative structure in which nanopatterning 110 is performed on the exterior surface instead of multiple cap layers as illustrated in Figure IF. The nanopatterning 110 reduces ambient light reflection and aids in ambient light absorption. Figure 2 has reference numbers similar to those used in Figure IF, with like reference numbers indicating like or similar components.

[0056] Figures 3 and 4 are similar to Figures 1F and 2. The optical systems illustrated in Figures 3 and 4 have a waveguide with a variable height or "duty cycle." Porogen material can be formed into such structures in a spin-coating operation as described above.

[0057] Figure 5 illustrates a further optical system having different layers of different three-dimensional nanostructure stacks. The three-dimensional nanostructure stacks can be designed differently for different waveguiding purposes. The material composition, thickness, and nanopatterning with various spatial and geometric configurations per cap layer can be different or the same between layers.

[0058] FIG. 6A illustrates a scanning electron microscope (SEM) image of an air pocket covered with a single layer of SiOx over an etched lattice in high refractive index glass. FIG. 6B shows an air pocket SEM image covered with a multilayer coating. The multilayer coating alternates between SiOx and TiOx with different thicknesses per layer. The composition and thickness of the layers on the lattice are, from bottom to top, 20 nm porous SiOx, 15 nm TiOx, 65 nm SiOx, 34 nm TiOx, 18 nm SiOx, 59 nm TiOx, 97 nm SiOx. The multilayer coating on top of the air pocket structure can be applied by chemical and / or physical vapor deposition, or spin coating, or a combination of different coating techniques.

[0059] 7A and 7B show a sample with an air pocket that was first covered with a SiOx layer and then spin-coated with an optical polymer (Teflon AF1600 from Chemours Company) with a refractive index of 1.31. The air pocket reduced the effective refractive index of the nanostructured grating area, resulting in a gradual refractive index change from the bulk substrate, to the surface grating area, to the SiOx cap layer, to the spin-coated optical polymer layer, and finally to air. This kind of gradual refractive index change is beneficial for anti-reflection purposes and can significantly improve the transmission of ambient light.

[0060] Figure 8 is a 0° transmission graph from an experimental measurement showing that transmission is significantly increased by the combination of the air pockets and coatings of Figures 7 A and 7 B. The nanostructured substrate here is a high refractive index lithium niobate substrate that has been etched to form a surface grating.

[0061] FIG. 9 illustrates the model used for the purpose of simulating the reflection properties. FIG. 10A-10D show four different anti-reflection coating stacking configurations simulated in the structure of FIG. 9. FIG. 10A is a side view of a waveguide without any coating for the simulation. FIG. 10B is a side view of a waveguide with an optical polymer coating for the simulation. FIG. 10C is a side view of a waveguide with an air pocket for the simulation. FIG. 10D is a side view of a waveguide with a polymer instead of an air gap for the simulation. FIG. 11 is a graph illustrating transmission data based on the simulation. FIG. 12 shows the user-side diffraction efficiency from a simulation using high-index lithium niobate for the waveguide. With regard to the simulated transmission data, it can be seen that a directly spun-on low-index optical polymer (AF2400 from Chemours Company, refractive index 1.29) has a similar effect on improving transmission compared to the configuration with an air pocket. However, in terms of single bounce diffraction efficiency, the air pocket configuration is significantly better than configurations with only a spun-on low refractive index polymer, or stacks with PPC filling the grooves of the grating. Simulations show that the diffraction efficiency is significantly higher than the situation where a low refractive index material fills the grooves, but is still lower than the situation where no anti-reflection coating is applied. To further increase the efficiency, the geometry of the grating needs to be modified accordingly.

[0062] While certain exemplary embodiments have been described and shown in the accompanying drawings, it is to be understood that such embodiments are illustrative only and are not limiting of the invention, and that the invention is not limited to the specific construction and arrangements shown and described, since modifications may occur to those skilled in the art.

Claims

1. 1. A method of manufacturing an optical system, comprising the steps of: forming a waveguide of a high index transparent material having a front side and a rear side, such that the front side of the waveguide has a plurality of recesses and a plurality of raised formations, each raised formation being located between two of the recesses; adhering a cap layer of selectively transparent material to the waveguide, wherein a plurality of cavities are defined between the cap layer and the waveguide with a gas in each respective cavity such that when an ambient light source is located at a front side of the waveguide, a beam of ambient light is transmitted through the selectively transparent material of the cap layer, through the cavities holding the gas, and through the high index transparent material of the waveguide; supporting first portions of the cap layer with the ridge formations, with second portions of the cap layer located between the first portions of the cap layer and across the recesses, such that respective ones of the cavities are defined by respective ones of the second portions of the cap layer and respective ones of the recesses at the front side of the waveguide; A method comprising:

2. 2. The method of claim 1, wherein the cap layer is a front cap layer located between the ambient light source and a front side of the waveguide, and the beam of ambient light is transmitted sequentially through a selective transparent material of the front cap layer, through the cavity holding the gas, and into a high index transparent material of the waveguide.

3. The method of claim 2 , wherein the selected transparent material of the front cap layer is an anti-reflective material that increases absorption of the ambient light by the front surface of the waveguide and reduces reflection of the ambient light by the front surface of the waveguide.

4. The method of claim 3 , wherein the high refractive index transparent material is one of high refractive index glass, high refractive index lithium niobate, lithium tantalate, and silicon carbide.

5. The method of claim 3 , wherein the high refractive index transparent material has a refractive index of at least 1.

74.

6. The method of claim 1 , wherein the gas has a refractive index less than 1.

3.

7. The method of claim 1 , wherein the gas is air with a refractive index of 1. forming a stack including the waveguide, a solid porogen material, and the cap layer; replacing said solid porogen material with said gas; The method of claim 1 further comprising:

9. The solid porogen material, heating the solid porogen material to a decomposition temperature at which the solid porogen material is converted into a sacrificial gas; removing the sacrificial gas from the cavity; and The method of claim 8 , wherein the surface is removed by 10. The method of claim 9, wherein the selected material of the cap layer is porous and the sacrificial gas outgasses through the selected material of the cap layer.

11. The method of claim 9, wherein the solid porogen material decomposes at a decomposition temperature of 120°C to 230°C.

12. The method of claim 10 , wherein the cap layer is made of SiO x having a thickness of at least 12 nm, where x is a variable.

13. The method of claim 1 , wherein each recess has a depth and a width, the width being less than 300 microns.

14. The method of claim 1 , wherein the recess is imprinted on the front side.

15. conformally depositing a transparent layer on a front side of said waveguide; The method of claim 1 further comprising:

16. the cap layer is a front cap layer located between the ambient light source and the front side of the waveguide, and the cavity is a front cavity between the front cap layer and the front side of the waveguide; affixing a rear cap layer of a selectively transparent material to the waveguide, the rear cavity being defined between the rear cap layer and the rear face of the waveguide with a gas present in the rear cavity such that when an ambient light source is located at a front side of the waveguide, a beam of ambient light is transmitted through the high index transparent material of the waveguide, through the rear cavity holding the gas, and through the selectively transparent material of the rear cap layer; The method of claim 1 further comprising:

17. the cap layer is a first cap layer and the selectively transparent material is a first selectively transparent material; bonding a second cap layer of a second selected transparent material to the first cap layer. The method of claim 1 further comprising:

18. The method of claim 17 , wherein the second cap layer is harder than the first cap layer.

19. 20. The method of claim 17, wherein at least one of the selective transparent materials of the cap layer is an anti-reflective material that increases absorption of the ambient light by the front surface of the waveguide and reduces reflection of the ambient light by the front surface of the waveguide.

20. Forming a stack of cap layers having refractive indices that vary in magnitude 20. The method of claim 19, further comprising:

21. The method of claim 20, wherein the cap layer is made of SiOx having a refractive index of 1.45 and TiOx having a refractive index of 2.2-2.3, where x is a variable.

22. 1. An optical system comprising: a waveguide of a high refractive index transparent material having a front side and a rear side, the front side of the waveguide having a plurality of recesses and a plurality of raised formations, each raised formation located between two of the recesses; a cap layer of selectively transparent material affixed to the waveguide, a plurality of cavities being defined between the cap layer and the waveguide, the cap layer comprising a first portion supported using the ridge formations and a second portion located between the first portion of the cap layer and across the recesses, such that respective ones of the cavities are defined by respective ones of the second portion of the cap layer and respective ones of the recesses at a front side of the waveguide; a gas in each individual cavity, the gas in the cavity being such that when an ambient light source is located at the front side of the waveguide, a beam of ambient light is transmitted through the selective transparent material of the cap layer, through the cavity holding the gas, and through the high refractive index transparent material of the waveguide; An optical system comprising:

Citation Information

Patent Citations

  • Optical modulator and its manufacturing method, optical information processor equipped with the optical modulator, image forming apparatus equipped with the optical modulator, and image projection / display unit equipped with the optical modulator

    JP2002214550A

  • Optical article having heat resistant antireflective coating with optimized thickness ratio of low refractive index layer and high refractive index layer

    JP2009541808A

  • Dual-layer light guide for illuminating displays

    JP2010526341A

  • Display device and wearable device

    JP2016126134A

  • Compact head-mounted display system protected by ultra-fine structure

    JP2017535825A