Axial reforming tube

JP2024521983A5Active Publication Date: 2024-11-06PARALLOY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2023562242
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-04-07
Filing Date
2022-04-06
Publication Date
2024-11-06
Estimated Expiration
2042-04-06

AI Technical Summary

Technical Problem

Existing axial reformer tubes for steam methane reforming have limitations in maximizing heat transfer efficiency and internal surface area while minimizing pressure drop, primarily due to their smooth inner surfaces which hinder optimal gas flow and heat exchange.

Method used

The inner surface of the axial reformer tubes is engineered with a roughened pattern of circumferential grooves and ridges, featuring an arithmetic mean roughness of 12.5 μm to 500 μm, promoting turbulent swirling flow and enhancing heat transfer without significant pressure loss.

Benefits of technology

This design significantly improves heat transfer coefficients by approximately 10% and maintains low pressure drop, thereby increasing the efficiency of the steam methane reforming process.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

In the axial reforming tube of the present invention, at least a portion of the inner surface of the reforming tube has a rough surface portion having an arithmetic mean roughness Ra of 12.5 μm or more and 500 μm or less, the axial reforming tube extends along its axial length, and the rough surface portion has a circumferential groove pattern.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to axial reforming tubes, and more particularly, but not exclusively, to axial reforming tubes for steam methane reforming. [Background technology]

[0002] Steam methane reforming is a widely used process in the production of hydrogen from natural gas. For example, steam and methane are heated to 700-1000°C and 3-40 bar and passed over a nickel catalyst to produce hydrogen, carbon monoxide, and some carbon dioxide in the highly endothermic steam methane reforming reaction ("chemical formula 1" below). Carbon monoxide and water react over the catalyst to produce carbon dioxide and more hydrogen via the moderately exothermic water gas shift reaction ("chemical formula 2" below). The carbon dioxide is then absorbed by pressure swing absorption, leaving essentially pure hydrogen.

[0003] [ka] [ka]

[0004] Steam methane reforming is typically carried out in axial reforming tubes (also called reformer tubes, reformer tubes, axial reforming tubes, reforming catalyst tubes, or reformers). Axial reforming tubes are also used in other reforming processes, such as the production of ammonia and methanol.

[0005] In use, reformer tubes for steam methane reforming are typically oriented vertically in a furnace (a refractory-lined box). Axial reformer tubes made of alloy steel are commonly used to withstand the pressures and temperatures required for reforming and to allow for rapid heat transfer from an external heat source through the walls of the reformer tube to the gas flowing along the reformer tube. An exemplary material used to manufacture axial reformer tubes is Paralloy's H39WM, a heat-resistant austenitic stainless steel containing 0.4% carbon, 25% chromium, 35% nickel, and 1% niobium.

[0006] To increase the strength of the axial reforming tubes while increasing the ratio of internal surface area to volume for heat transfer between the inner surface of the reforming tube and the gas flowing along the reforming tube, the axial reforming tubes are typically long compared to their inner diameter. For example, a reforming tube with an inner diameter of 10 cm may have a length of 13 m.

[0007] In use, gas flows generally axially along the axial reforming tubes. The steam methane reforming reaction takes place where the reagent gas passes over a catalyst, around which the gas flows along the reforming tubes. Gas also flows along the inner surface of the reforming tubes.

[0008] The catalyst typically has a high surface area to volume ratio and is advantageously configured to provide a relatively low pressure drop for gas flowing through the catalyst bed.

[0009] Axial reforming tubes are typically manufactured by spin casting, and the inner surface of the reforming tube is formed by a smooth boring process, for example to obtain an Ra roughness (arithmetic mean roughness) of 3.2 μm to 1.6 μm, which corresponds to an Rt roughness of 13 μm to 6.3 μm, where Rt is the range of roughness data points collected. It is conventionally believed that a smooth boring process is desirable for the inner surface of the reforming tube to reduce the resistance to gas flow along the inner surface of the reforming tube, thereby reducing the pressure drop along the reforming tube and maximizing the yield of reformed gas product. Summary of the Invention

[0010] According to the present disclosure there is provided an axial reforming tube and reforming system as set out in the accompanying claims.

[0011] According to a first aspect, there is provided an axial reforming tube, at least a part of the inner surface of which has a roughened surface portion having an arithmetic mean roughness of the surface of between 12.5 μm and 500 μm, the axial reforming tube extending along its axial length, the roughened surface portion having a circumferential groove pattern.

[0012] According to a second aspect, there is provided a reforming system comprising an axial reforming tube according to the first aspect.

[0013] The inner surface of the rough surface portion may have an arithmetic mean roughness of at least 25 μm. The inner surface of the rough surface portion may have an arithmetic mean roughness of at least 50 μm. The inner surface of the rough surface portion may have an arithmetic mean roughness of at least 100 μm.

[0014] The axial offset of the circumferential groove from the circumferential direction of the inner surface of the axial reforming tube may be 10 degrees or less.

[0015] The axial offset of the circumferential groove from the circumferential direction of the inner surface of the axial reforming tube may be 5 degrees or less.

[0016] The circumferential groove pattern may be formed as one or more spiral grooves.

[0017] The circumferential groove side surfaces may be inclined at a side angle between 0 and 50 degrees relative to a plane perpendicular to the axial length. The circumferential groove side surfaces may be inclined at a side angle between 0 and 30 degrees relative to a plane perpendicular to the axial length. The side angle may be at least 10 degrees. The side angle may be no greater than 25 degrees.

[0018] The axial length of the bottom of the circumferential groove may be 50% or more and 200% or less of the depth of the circumferential groove.

[0019] Adjacent circumferential grooves may be separated from each other by a top surface portion (crown portion), and the axial length of the top surface portion may be 50% or more and 100% or less of the depth of the circumferential groove.

[0020] Adjacent circumferential grooves may be separated from each other by a top surface portion, and a sharp edge may be formed between the top surface portion and a side surface of the circumferential groove, and the sharp edge may have an average radius of curvature of 20 μm or less.

[0021] The roughened surface may extend along the entire length of the axial reforming tube.

[0022] The axial reforming tube may comprise a smooth surface portion having an arithmetic mean roughness of 3.2 μm or less and bonded to the rough surface portion.

[0023] The rough surface portion may be bonded between two of the smooth surface portions.

[0024] The axial reforming tube may have a length of at least 700mm.

[0025] The inner diameter of the axial reforming tube may be less than or equal to 350 mm.

[0026] The axial reforming tube may have a length of at least 700mm and an inner diameter of the axial reforming tube may be between 95mm and 280mm.

[0027] The axial reforming tube may have a length of at least 2 metres. The inner diameter of the axial reforming tube may be between 95mm and 250mm.

[0028] The reforming system may further comprise a catalyst bed packed into at least a portion of the axial reforming tube, a heater for heating the at least a portion of the axial reforming tube, a pump for pumping gas through the catalyst bed, and a control system for monitoring and controlling operation of the reforming system. [Brief description of the drawings]

[0029] The embodiments are further described with reference to the accompanying drawings in which:

[0030] [Figure 1A] 1 shows an axial reformer tube. [Figure 1B] 1B shows a cross-sectional view of a portion of the axial reforming tube of FIG. 1A. [Figure 1C] 4 shows a photograph of a portion of the inside of an axial reforming tube. [Figure 1D] FIG. 2 shows a portion of the inside of an axial reforming tube. [Diagram 2] 4 illustrates an exemplary gas flow across the inner surface of an axial reforming tube. [Diagram 3] 1 shows another axial reformer tube. [Figure 4] 1 shows a reforming system. [Figure 5A] The heat transfer coefficients in three axial reforming tubes with different inner surface roughness are shown. [Figure 5B] The pressure drop in three axial reforming tubes with different inner surface roughness is shown. [Figure 6] 1 is a graph of experimental results showing heat transfer coefficient for different values ​​of inner surface roughness. [Figure 7A] 1 shows simulated plots of gas temperature along the center plane of two different axial reforming tubes. [Figure 7B] 1 shows simulated plots of gas temperature along the center plane of two different axial reforming tubes. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0031] Like reference numbers refer to like elements throughout the specification.

[0032] FIG. 1A shows an axial reforming tube 100 for use with a generally axial gas flow F (although for purposes of illustration, the catalyst is not shown), and FIG. 1B shows an expanded view of region B shown in FIG. 1A.

[0033] The axial reforming tube 100 has an axial length that is much longer than its inner diameter. The axial reforming tube may be hollow cylindrical. In use, the gas flow F will pass around the catalyst within the reforming tube, but is generally axial along the length of the reforming tube 100, as shown by line AA in FIG. 1A.

[0034] The inner surface 110 of the tube wall of the axial reforming tube 100 has an Ra roughness of at least 12.5 μm, where Ra roughness is the arithmetic mean roughness of the surface (e.g., an Rt roughness of at least 50 μm). Such roughness of the inner surface of the axial reforming tube changes the flow of gas along the inner surface of the axial reforming tube compared to a smooth inner surface. This results in turbulence, which prevents the formation of boundary layers and laminar flow along the inner surface of the tube wall. The turbulence enhances the heat transfer from the tube wall to the gas flowing in the reforming tube. By providing the inner surface 110 of the tube wall with an Ra roughness of at least 12.5 μm, the heat transfer can be significantly improved, and by providing the inner surface 110 of the tube wall with an Ra roughness of at least 25 μm, the heat transfer can be improved by about 10%. In these cases, the pressure drop (pressure loss) of the gas flowing along the reforming tube is only slightly affected. Such an improvement in the heat transfer rate can improve the efficiency of the steam methane reforming reaction. The inventors have determined that the benefits of improved heat transfer due to the surface roughness discussed above outweigh the effects of increased aerodynamic drag due to induced turbulence along the inner surface of the tube wall.

[0035] The inner surface 110 of the tube wall has an Ra roughness of 500 μm or less (e.g., an Rt roughness of 2000 μm or less). Limiting the Ra roughness to 500 μm or less promotes mixing of the turbulent flow generated by the rough surface features with the gas flow away from the inner surface, for example, to enhance heat transfer from the tube wall rather than leaving separate turbulent flow within the depth of the rough surface features (e.g., at the bottom of the grooves 112).

[0036] As shown in Figures 1B, 1C, and 1D, the roughness of the inner surface of the tube wall is formed as a pattern of grooves (circumferential grooves) 112 and ridges 114 extending in a generally circumferential direction. Figure 1D shows the inner surface of a portion of the axial reforming tube 100 (extending from the end 102 of the reforming tube) viewed radially outward from the central axis of the reforming tube (line AA in Figure 1A). The grooves 112 may extend around the inner surface of the reforming tube with an axial offset (angular offset from the radial direction) φ of 10 degrees or less, or 5 degrees or less, from the circumferential direction (perpendicular to the axial direction). A small axial offset (angular offset from the radial direction) φ of the extension direction of the grooves 112 from the circumferential direction promotes the formation of a turbulent swirling flow 182 within the grooves 112, as shown in Figure 2. This maintains a generally perpendicular gas flow across each groove 112 rather than sweeping the gas out of the grooves, preventing the formation of turbulent swirling flows within the grooves 112 .

[0037] 1C, for example, the roughness of the inner surface 110 of the reforming tube 100 may be provided by one or more helical grooves 112 cut (e.g., by cutting) into the inner surface 110 of the reforming tube 100. The helical grooves 112 may be cut to provide roughness to the inner surface 110 of the reforming tube 100 while reducing manufacturing complexity.

[0038] Alternatively, the grooves 112 may extend circumferentially (perpendicular to the axial length of the reformer tube 100). For example, the grooves 112 may be cut into a flat strip of material (e.g., steel) where the grooves 112 are cut perpendicular to the length of the strip before the strip is rolled across its width and the ends are sealed (e.g., by welding) to form the reformer tube 100.

[0039] 2 shows a model of gas 180 flowing axially along the axial reforming tube 100 and over the inner surface 110 of the reforming tube 100. Within the grooves 112, turbulent swirl 182 of the gas flow is created, which increases the rate at which heat is extracted from the tube wall compared to a smooth inner surface.

[0040] The depth d of the pattern of the grooves 112 and the ridges 114 is equal to the amplitude of the roughness of the inner surface 110, and is specified by, for example, an Rt roughness of 50 μm to 2000 μm (for example, an Ra roughness of 12.5 μm to 500 μm). The axial length L1 of the top surface (crown) of the ridges 114 may be 50% to 100% of the groove depth d. The axial length L2 of the bottom of the groove 112 may be 50% to 200% of the groove depth d. Providing the bottom of the groove 112 with an axial length L2 of 50% to 200% of the groove depth d promotes the formation of the turbulent swirling flow 182 in the groove 112. If the bottom of the groove 112 is narrower than this range, the size and formation of the turbulent swirling flow 182 in the groove 112 may be limited. If the base of the groove 112 is wider than this range, laminar flow may extend into the groove 112, thereby reducing the formation of turbulent swirling flow 182.

[0041] The sides 116A, 116B of the pattern of grooves 112 and ridges 114 generally face toward opposite ends of the reformer tube 100. The sides 116A, 116B may have a perpendicular that is substantially parallel to the axial length of the reformer tube 100, i.e., a side angle θ of substantially 0 degrees. 1 ,θ 2 (e.g., where the sides of the spiral groove are angled by only the pitch of the spiral groove). Alternatively, as shown in FIGS. 1B, 1C, and 2, the side angles θ of the sides 116A, 116B of the pattern of grooves 112 and ridges 114 may be 1 ,θ 2 For example, each of the side surfaces 116A and 116B has a side angle θ of 50 degrees or less (preferably 30 degrees or less). 1 ,θ 2 The thread angle (θ) is set to 100 degrees or less (preferably 60 degrees or less). 1 +θ 2 For example, the sides 116A and 116B each have a side angle θ greater than 0 degrees. 1 ,θ 2 (e.g., 50 degrees or less, or 30 degrees or less) with respect to a plane perpendicular to the length direction of the reforming tube 100. In FIG. 2, the depth d is 200 μm, and the side angle θ 1 ,θ2 are 15 degrees each. Side angles θ of at least 10 degrees 1 ,θ 2 Angling the sides 116A, 116B by an angle θ of 50 degrees or less (preferably 30 degrees or less) on the sides 116A, 116B of the groove 112 promotes the generation of turbulent swirling flow 182 near the top of the groove 112 (i.e., closer to the center of the reformer tube 100) rather than deeper in the groove 112. This enhances the interaction between the turbulent swirling flow 182 and the adjacent generally axial gas flow F, improving heat transfer from the tube wall and the gas flow F away from the tube wall. 1 ,θ 2 The angle of just above promotes the creation of turbulent swirling flow 182 within the grooves 112 while reducing laminar flow through the grooves 112, thereby promoting heat transfer from the tube wall to the main gas flow F.

[0042] The edges 118A, 118B of the top surface of the ridges 114 may be sharp. The sharpness of the edges 118A, 118B promotes turbulence in the gas flowing over the edges 118A, 118B, thereby disrupting the laminar flow and generating turbulent swirling flow 182 within the grooves 112. The sharp edges 118A, 118B may have a mean radius of curvature of less than 20 μm.

[0043] The roughness of the inner surface 110 of the axial reforming tube 100 also increases the inside surface area of ​​the reforming tube 100 compared to a smoothly bored tube, thereby increasing the surface area available for heat transfer to the gas flow F within the reforming tube 100, thereby enhancing the rate of heat transfer from the tube wall to the gas flow F.

[0044] The axial reforming tube 100 in FIG. 1A is shown as a single section having a roughened surface (eg, a pattern of grooves and ridges, such as a helical thread) extending along the entire length of the inner surface of the reforming tube 100.

[0045] Alternatively, as shown in FIG. 3, a part of the reforming tube 100' may be formed as a rough surface portion 100B' having a roughness pattern, and other parts of the reforming tube 100' may be formed as smooth surface portions 100A' and 100C' having smooth inner surfaces. For example, as shown in FIG. 3, a rough surface portion 100B' may be provided between two smooth surface portions 110A' and 110C'. Each part of the reforming tube 100' (e.g., the smooth surface portions 110A' and 110C' and the rough surface portion 100B') may have a length of several meters (e.g., at least 2 meters). For example, the reforming tube 100' may have a rough surface portion having an inner surface Ra roughness of 12.5 μm to 500 μm, and one or two smooth surface portions having a smooth inner surface (Ra roughness of 3.2 μm or less). The roughened surface may be provided in all or only a portion of the reforming tube 100' that is filled with the catalyst bed CAT (FIG. 4), thereby enhancing heat transfer from the tube wall to the gas flow F generally along the reforming tube 100' through the catalyst. Also, the smooth surface may be provided in one or more areas where no catalyst is present or in areas of the catalyst bed where enhanced heat transfer is not required. Enhanced heat transfer in the roughened surface of the reforming tube 100' may improve reaction performance. The area where the heat transfer is enhanced may be aligned with the portion of the axial reforming tube where the most endothermic reactions occur (e.g., a particular portion of the catalyst bed). The smooth surface provided in other portions of the axial reforming tube 100 may reduce the aerodynamic resistance to the gas flow F through the axial reforming tube 100, reducing manufacturing complexity and associated costs.

[0046] The axial reforming tube is many times longer than its inner diameter. The axial reforming tube may have a length of several meters. For example, the length of the axial reforming tube may be at least 700 mm, at least 2 m, or at least 5 m. Furthermore, the length of the axial reforming tube may be 8 m or more and 13 m or less. The axial reforming tube may have an inner diameter much smaller than 1 meter. For example, the inner diameter of the axial reforming tube may be 350 mm or less, 95 mm or more and 280 mm or less, 95 mm or more and 250 mm or less, or 95 mm or more and 175 mm or less. The wall thickness of the axial reforming tube may be 8 mm or more and 15 mm or less.

[0047] In general, the axial reformer tube 100 may be formed by welding together a series of tubular sections from one end to the other. A reformer tube having a section with a rough inner surface and another section with a smooth inner surface may be formed by welding together correspondingly formed tubular sections.

[0048] The axial reforming tube 100 may form part of a reforming system RS, in which the reforming tube 100 is provided with a heater and a catalyst bed CAT is packed in the reforming tube 100, as shown in FIG. 4. A number of axial reforming tubes 100 may be coupled in parallel to each other to receive a reagent flow RF. Said heater may be a furnace H through which the reforming tube 100 extends (also alternative heaters may be provided, such as, for example, a ribbon heater wrapped around each reforming tube). A flow straightener FS may be provided upstream of the catalyst bed CAT to reduce turbulence in the reagent flow F to the catalyst. A control system CS is provided to monitor the gas flow and temperature in various parts of the reforming system, for example before the reagents enter the catalyst and after they leave the catalyst at one or more positions over the length of the packed catalyst. It is noted that the control system CS may, for example, monitor each reforming tube 100, although by way of example only a monitor M is shown on one reforming tube. A pump P is provided for pumping the reagents through the catalyst, for example in the downstream stream of the cooled product gas after the endothermic reaction.

[0049] 5A and 5B show exemplary experimental data measuring the heat transfer coefficient and pressure drop for three axial reforming tubes (tubes 1 to 3 described below) 100 having different inner surface Ra roughness values. [Tube 1] Reformer tube with inner surface roughness Ra of 3.2 μm [Tube 2] Reformer tube with inner surface roughness Ra of 25 μm [Tube 3] Reformer tube with inner surface roughness Ra of 375 μm

[0050] In the test setup, air was drawn into the axial reforming tubes 100 through a flow straightener FS and through a packed bed of catalyst (roughened spheres with a diameter of 16 mm and a porosity of 0.56) (catalyst bed CAT) by a pump P. The outside of each axial reforming tube 100 was heated by a ribbon heater wrapped around the reforming tube. Each axial reforming tube was tested twice and the corresponding data was collected as shown in the figure.

[0051] FIG. 5A shows the heat transfer coefficient for each reforming tube (tubes 1-3), and FIG. 5B shows the pressure drop in each reforming tube (tubes 1-3). Tube 1 has a smooth inner surface and serves as the control tube for comparison purposes. The heat transfer coefficients measured for tubes 2 and 3 were approximately 10% higher than that of tube 1.

[0052] Tube 1 offers the lowest resistance to gas flow F adjacent to the inner surface of the axial reforming tube 100. Tubes 2 and 3 also offer a higher pressure drop than tube 1, which means that there is an increased resistance to gas flow adjacent to the inner surface of the axial reforming tube.

[0053] Table 1 below shows further exemplary experimental data on heat transfer coefficient and pressure drop measurements for several axial reforming tubes with different Rt roughness (and different Ra roughness) values. Several values ​​of Rt roughness from smooth to 2500 μm (for Ra roughness, e.g., smooth to about 625 μm) were used. Also, catalyst beds consisting of spherical or cylindrical catalyst were used. Figure 6 shows the heat transfer coefficient for the prototype axial reforming tubes of Table 1.

[0054] [Table 1]

[0055] Up to an Rt roughness of 1500 μm or 2000 μm on the inner surface of the axial reforming tube (e.g., up to an Ra roughness of about 375 μm or about 500 μm), the heat transfer coefficient increases. The overall pressure drop increases very little. Above an Rt roughness of 2000 μm, the manufacture of deeper grooves becomes complicated, and as a result, the heat transfer coefficient does not improve substantially.

[0056] Figure 7A shows a simulated plot of gas temperature along the central plane of an axial reforming tube with a smooth inner surface (e.g., Rt roughness of 25 μm or less), and Figure 7B shows a simulated plot of gas temperature along the central plane of an axial reforming tube with an Rt roughness of 2000 μm (e.g., Ra roughness of 500 μm). In both cases, the same cylindrical catalyst bed is used. Figure 7B shows how providing a 2000 μm Rt roughness on part of the inner surface of the axial reforming tube improves the heat transfer rate through the tube wall.

[0057] The figures provided in this application are schematic and not to scale.

[0058] Throughout the description and claims of this specification, the terms "comprise," "have," and "include," as well as their related terms, mean "including, but not limited to," and are not intended to exclude other parts, appendants, elements, integers, or steps. Throughout the description and claims of this specification, the singular encompasses the plural, unless the context requires otherwise. In particular, when the indefinite article is used, the specification should be understood as contemplating the plural as well as the singular, unless the context requires otherwise.

[0059] It should be understood that features, integers, properties, compounds, chemical moieties or groups described in connection with a particular aspect, embodiment or example of the invention are applicable to any other aspect, embodiment or example described herein, unless inconsistent therewith. All features disclosed herein (including the accompanying claims, abstract and drawings) and / or all steps of any method or process so disclosed may be combined in any combination, except combinations in which at least some of such features and / or steps are mutually exclusive. The invention is not limited to the details of the foregoing embodiments. The invention extends to any novel or any novel combination of features disclosed herein (including the accompanying claims, abstract and drawings) and / or any novel or any novel combination of steps of any method or process.

[0060] Attention is directed to all articles and documents related to this application that have been filed contemporaneously with or prior to this application and that are open to public inspection herewith, and the contents of all such articles and documents are incorporated herein by reference.

Claims

1. At least a part of the inner surface of the axial reforming tube has a rough surface portion having an arithmetic mean roughness of 12.5 μm or more and 500 μm or less; the axial reforming tube extends along an axial length, the roughened surface having a pattern of grooves; the deviation of the groove from the circumferential direction of the inner surface of the axial reforming tube is 10 degrees or less; Axial reforming tube.

2. At least a portion of the axial reforming tube is a rough surface portion having an inner surface with an arithmetic mean roughness of at least 25 μm. The axial reforming tube of claim 1.

3. the deviation of the groove from the circumferential direction of the inner surface of the axial reforming tube is 5 degrees or less; The axial reforming tube of claim 1.

4. The groove pattern is formed as one or more spiral grooves. The axial reforming tube of claim 1.

5. the groove sides are inclined at a side angle between 0 and 50 degrees relative to a perpendicular to the axial length; The axial reforming tube of claim 1.

6. The sides of the groove are inclined with respect to a perpendicular to the axial length by a side angle between 0 and 30 degrees.

6. The axial reforming tube of claim 5.

7. The side angle is at least 10 degrees.

6. The axial reforming tube of claim 5.

8. The side angle is 25 degrees or less.

6. The axial reforming tube of claim 5.

9. The axial length of the bottom of the groove is 50% or more and 200% or less of the depth of the groove. The axial reforming tube of claim 1.

10. The grooves are separated from each other by a top surface portion, and the axial length of the top surface portion is 50% or more and 100% or less of the depth of the groove. The axial reforming tube of claim 1.

11. The grooves are separated from each other by a top surface portion, and a sharp edge is formed between the top surface portion and a side surface of the groove, and the sharp edge has an average radius of curvature of 20 μm or less. The axial reforming tube of claim 1.

12. The rough surface portion extends over the entire length of the axial reforming tube. The axial reforming tube of claim 1.

13. The axial reforming tube has an arithmetic mean roughness of 3.2 μm or less and a smooth surface portion bonded to the rough surface portion. The axial reforming tube of claim 1.

14. The rough surface portion is bonded between two of the smooth surface portions.

14. The axial reforming tube of claim 13.

15. The axial reforming tube has a length of at least 700 mm. The axial reforming tube of claim 1.

16. The inner diameter of the axial reforming tube is 350 mm or less. The axial reforming tube of claim 1.

17. The axial reforming tube has a length of at least 2 meters, and the inner diameter of the axial reforming tube is equal to or greater than 95 mm and equal to or less than 280 mm. The axial reforming tube of claim 1.

18. The axial reforming tube has a length of at least 2 meters, and the inner diameter of the axial reforming tube is equal to or greater than 95 mm and equal to or less than 250 mm. The axial reforming tube of claim 1.

19. A reforming system comprising an axial reforming tube according to any one of claims 1 to 18.

20. a catalyst bed packed within at least a portion of the axial reforming tube; a heater for heating at least the portion of the axial reforming tube; a pump for pumping a gas through the catalyst bed; and a control system for monitoring and controlling the operation of the reforming system.

20. The reforming system of claim 19.