Enamel superconductor
A thin film composite superconductor architecture with a ceramic insulating layer addresses the challenges of insulating high-temperature superconductors by ensuring high current density and thermal conductivity, while maintaining mechanical integrity and reducing volume, using methods like RF sputtering to apply the insulating layer at low temperatures.
Patent Information
- Application Number
- JP2024517147
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-20
- Filing Date
- 2022-09-17
- Publication Date
- 2024-10-16
AI Technical Summary
Existing insulating layers in high-temperature superconductors complicate the design, increase the volume occupied by the conductor-insulator system, reduce engineering current density, and fail to maintain mechanical integrity and thermal conductivity at cryogenic temperatures.
A thin film composite superconductor architecture with a metal substrate, buffer layer, superconducting layer, and ceramic insulating layer, where the insulating layer is applied at low temperatures using methods like RF sputtering, ensuring a compressive mismatch and high breakdown voltage, thermal conductivity, and mechanical strength.
The solution provides a robust insulating layer that maintains high engineering current density, withstands mechanical stresses, and efficiently dissipates heat, while minimizing volume and maintaining superconducting properties at cryogenic temperatures.
Smart Images

Figure 2024537684000001_ABST
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to and the benefit of U.S. Provisional Patent Application No. 63 / 245,967, filed September 20, 2021, and entitled "Enameled Superconductor," the entire contents of which are incorporated herein by reference. [Background technology]
[0002] FIELD OF THE DISCLOSURE
[0002] Embodiments of the subject matter disclosed herein relate generally to insulated superconductors, and more specifically to ceramic insulators, methods of applying ceramic insulation to high temperature superconductors, and structures and architectures of superconductors that use particular ceramic insulators.
[0003] Background information Electrical insulation plays an important role in the design and application of electromagnetic systems that utilize coated conductors, especially high temperature superconductors. High temperature superconductors (HTS) offer the possibility of developing superconducting components that operate at higher temperatures compared to conventional superconductors that operate at liquid helium temperatures (4.2K). Thus, superconductors that operate at higher temperatures allow the development of more economically operating superconducting components and products. YBa2Cu3O 7-x Thin film HTS materials made from YBCO (YBCO) are one of a group of oxide-based high temperature superconductors. After the initial discovery of YBCO superconductors, other superconductors were discovered with similar chemical composition but with Y replaced by other rare earth elements. This family of superconductors is often denoted as REBCO, where RE stands for rare earth and may include Y, La, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, or Lu. This material formed the basis of second generation or "2G" HTS wire technology, which provided a more cost-effective material for producing HTS tapes and wires.
[0004] Such HTS films are typically deposited as oriented REBCO thin films, which may include one or more buffer layers, on atomically oriented metal substrates. In the case of metal-organic chemical vapor deposition (MOCVD), organic ligands may comprise the gas-phase precursors that are delivered to the substrate for the deposition reaction. In the manufacture of high-temperature superconductors by chemical vapor deposition (CVD) or MOCVD, the process is carried out under vacuum conditions, whereby a stainless steel or Hastelloy substrate tape is heated to high temperatures, for example 800°C to 900°C, to deposit the gas-phase precursor material on the substrate tape, and the growth of the HTS film occurs. Following the deposition of the buffer layer and the superconducting layer, one or more stabilizing and / or insulating layers may be applied.
[0005] Various types of coated conductors used in electromagnetic systems contain some organic material for insulation. In some superconductors, epoxy (with or without glass fiber reinforcement) is used to epoxy coat the conductor and pot coils. For example, enameled superconductors used in magnets may be encapsulated or coated with an epoxy resin consisting of organic polyimide, or polyepoxide, or prepolymers and polymers containing epoxy groups, applied by dip or spray coating. The minimum thickness reported for these enamels is about 4 microns (um). Thus, for a thermal conductivity of 0.8 W / mk, a 4 um thick enamel will have a thermal conductivity of 5×10 -6 m 2 It will have a room temperature thermal resistance of 100 K / W.
[0006] In other cases, metals such as brass tape may be laminated to the coated conductor. Although brass is technically a conductor, it acts like an insulator because it has a relatively high resistance compared to superconductors. In some superconductor applications, coils may be wound without insulation to achieve high current densities. This approach results in a non-insulated coil with a time constant that is much higher than that of a fully insulated coil due to the lack of insulation resistance, resulting in very slow coil charge-discharge rates.
[0007] The application of insulators complicates the design of insulated superconductor architectures, and also reduces the engineering current density in the system, since it increases the volume occupied by the conductor-insulator system. For example, a typical coated conductor may be 100um thick, but the insulator can easily add 50um, thus increasing the cross-sectional area by 50%, thereby reducing the engineering current density.
[0008] In many applications, especially HTS, an insulating layer is required on the superconductor to prevent the transfer of electrical current between layers. For these reasons, new insulating superconductors, architectures, as well as systems and materials methodologies are needed. The insulating layer needs to be very thin (e.g., about 2um or less) while having sufficient mechanical properties to withstand the Lorentz forces, high thermal conductivity to dissipate any heat generated, and high dielectric breakdown strength to prevent the conduction of electrical current from layer to layer while maintaining low thermal resistance. Furthermore, the insulating layer must be applied at low temperatures to avoid degradation of the superconducting properties of the wire. Summary of the Invention
[0009] According to one embodiment, a metal substrate, a buffer layer, a superconducting layer, and a 10 -7 m 2 There are thin film composite superconductors having thermal resistances of less than K / W and ceramic insulating layers with breakdown voltages of over 20V.
[0010] According to another embodiment, there is a thin film composite superconductor article having a metallic substrate, a buffer layer, a superconducting layer, and a ceramic insulating layer having a compression mismatch with respect to the superconducting layer when cooled to a temperature of 77 K or less. The mismatch is determined by the ratio of the volumetric thermal expansion coefficient measured at room temperature of the ceramic insulating layer to the volumetric thermal expansion coefficient of the superconducting layer, and is substantially equal to or less than 0.75.
[0011] In a method embodiment, there is a method of forming a superconducting article that includes providing a metallic substrate, depositing a buffer layer on the substrate, depositing a superconducting layer on the buffer layer at a first temperature, and depositing a ceramic insulating layer on the superconducting layer at a second temperature such that a compressive mismatch to the superconducting layer is established upon cooling to a temperature substantially equal to or less than 77 K.
[0012] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate one or more embodiments and, together with the description, explain these embodiments. Unless otherwise indicated, elements in the drawings are not to scale. [Brief description of the drawings]
[0013] [Figure 1A] 1 illustrates an exemplary layered insulated superconductor. [Figure 1B] 1 illustrates an exemplary encapsulated insulated superconductor. [Figure 1C] 1 illustrates an exemplary multi-stack superconductor architecture as a pancake coil. [Diagram 2] A and B show exemplary filamentary and bundled insulated superconductors. [Diagram 3] 1 illustrates an embodiment of a reinforced insulated superconductor. [Figure 4] 1A-C show exemplary methods for producing insulated type I and type II high temperature superconductors (HTS) and low temperature superconductors (LTS). [Diagram 5] 1 illustrates an exemplary system for manufacturing an insulated superconductor. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] The following embodiments are described with reference to the accompanying drawings. The same reference numbers in different drawings identify the same or similar elements. The following detailed description is not intended to limit the invention. Instead, the scope of the invention is defined by the appended claims. Although the following embodiments may be described with particular reference to insulated high temperature superconductors (HTS), the disclosed insulation system and insulation process are also applicable to other superconductors (e.g., low temperature superconductors (LTS)) and other solid conductors or coated conductors. Furthermore, although a particular embodiment using amorphous boron nitride is described as a preferred embodiment, other inorganic ceramics may also be applicable to insulated superconductors.
[0015] Throughout this specification, reference to "one embodiment" or "an embodiment" means that a particular feature, structure, or characteristic described in connection with an embodiment is included in at least one embodiment of the disclosed subject matter. Thus, the phrases "in one embodiment" or "in an embodiment" appearing in various places throughout this specification do not necessarily refer to the same embodiment. Furthermore, the described features, structures, or characteristics may be combined in any suitable manner in one or more embodiments.
[0016] The embodiments disclosed herein include superconductors having a thin coating of an inorganic insulator that is applied as a final step in the superconductor manufacturing process. In a preferred embodiment, the insulator is a very thin coating (e.g., about 20 nm) of an amorphous ceramic such as boron nitride (BN). The coating is applied in a specific manner that allows for and enhances its compatibility with high temperature superconductors due to a unique combination of conditions described below. Insulating amorphous boron nitride has a dielectric breakdown voltage of about 20 V or greater, approximately 5×10 measured at 25° C. -9 m 2It is deposited as a thin coating of about 20 nm while providing a thermal resistance of less than 10 K / W and while maintaining high mechanical properties including high wear resistance. The process of application of amorphous boron nitride may be the deposition methods and conditions described below. At this thickness the breakdown voltage is about 20 V. If the application requires a higher breakdown voltage, the coating can be made thicker, for example 160 nm thick, the breakdown voltage increases to 140 V and the thermal resistance is 5×10 -8 m 2 Increase to K / W.
[0017] Superconducting tapes and wires can be coated accordingly and formed into product applications. For example, one or more superconducting wires or tapes can be wound into coils to make electromagnets and electromagnetic products, such as high-strength magnets in magnetic resonance imaging (MRI) and nuclear magnetic resonance (NMR) devices and systems, or rotating machine applications such as motors and generators, and many other applications. In addition, multi-tape and multi-wire systems can also be coated similarly, but with the insulating coating applied only to select portions or faces. For example, as described in more detail below, when multiple conductors are wound, adjacent windings must be insulated from each other to ensure that the current travels in a designed path while minimizing the overall conductor volume and cross-sectional area, leaving other sides that do not contact adjacent windings uncoated.
[0018] There are several properties required for an insulator to be suitable for superconductor applications. First, high dielectric breakdown strength and high electrical resistance ensure that a higher voltage drop across the insulator is tolerated. This is a challenge given that the thickness of the insulator is preferably minimized to enforce other needs of superconductor applications such as high thermal conductivity and smaller conductor cross-sectional area. A smaller cross-sectional area allows for higher engineering current densities, which in turn allows for higher magnetic fields.
[0019] It is also very important, especially for superconductors, that the thermal resistance of the insulator is very low, given the need to quickly dissipate the heat generated to prevent quenching, a phenomenon in which localized heat buildup in the conductor leads to high local electrical resistance, which then cascades to generate more heat. Therefore, the thermal resistance of the insulating material must be low, allowing it to dissipate heat quickly.
[0020] Mechanically, in addition to the minimum thickness of the insulation, uniformity of the insulation thickness, measured at each point around the conductor, is important so that any local variations in the breakdown strength are minimized to avoid the possibility of short circuits where gaps or excess thickness in the coating may exist. The advantage of a thin layer is that it essentially conforms to the superconductor surface allowing the coil to have a large contact area between the layers. This contact area allows the heat to be rapidly conducted away in the event of a quench.
[0021] The insulating coating must also withstand mechanical stresses that arise during winding of the conductor, inducing bending, stretching, and friction. This is a very important requirement, since the total stress experienced by the insulating coating is exacerbated by internal stresses resulting from the mismatch of the coefficients of thermal expansion (CTE) of the various layers in the architecture of the coated conductor. These forces are amplified when the wire is cooled to the operating temperature of the superconductor, below 77 K. When energized, high Lorentz forces are further added to the stress profile within the conductor, especially the superconductor. Thus, insulators for such applications must withstand stress magnitudes that are often greater than those of a typical copper winding. Furthermore, the thermo-mechanical performance of the insulator at very low temperatures is very important, so that the mechanical strength of the insulating coating is maintained at cryogenic temperatures (e.g., below 77 K) and through multiple thermal cycles.
[0022] The operating conditions of superconductors are very different from copper. Although the heat generated in copper coils by ohmic heating can reach temperatures of over 200C, superconductors also operate at temperatures below -196C and even below -268C. Such thermal conditions have a significant impact on the choice of materials. At low temperatures, most materials become brittle and break easily. Also, most polymer-based insulators, due to their high thermal expansion coefficient, contract significantly below their glass transition temperature and do not deform to relieve contraction stresses. The glass transition temperature of a polymer is the temperature below which the polymer becomes glassy, i.e., rigid and non-plastic. Importantly, especially for polymer enamels that usually have a lower initial (room temperature) thermal conductivity, the thermal conductivity decreases as the temperature decreases, making the polymer enamel less suitable for superconductor applications. On the other hand, inorganic ceramics are generally good insulators with good electrical resistivity and thermal properties, but it is a challenge to produce inorganic ceramics in a form that is suitable for very thin enamels for superconductors.
[0023] An example of an insulated coated superconductor tape 100 is shown in FIG. 1A. The superconductor may be a type I or type II high temperature superconductor (HTS) or low temperature superconductor (LTS) and may be fabricated as a single wire or tape or a cable consisting of multiple filaments or bundles of filaments, wires, or tapes. Type II superconductors are coated conductors that are typically a few mm wide and less than 1 mm thick, with an overall structure of rectangular cross section. In the type II HTS example of FIG. 1A, the tape has a thin film composite structure with a basic architecture including a metal substrate 110, a buffer layer 120, a superconducting layer 130, and a capping or stabilizing layer 140 followed by an insulating coating 150. In this example, for ease of illustration, the insulator 150 is shown as coating only the top surface, but in a preferred embodiment, the insulator 150 may encapsulate the entire structure (110-150 in this example).
[0024] Multiple deposition layers of those shown in Figure 1A or other layers may provide additional purposes to the basic architecture described herein. For example, Figure 1B shows another type II HTS in which a superconductor layer 130 is deposited on a metallic substrate tape 110. (The superconductor may be deposited on one or more buffer layers 130 that are first deposited on the substrate 110.) The superconductor thin film may then be covered with a layer of metallic silver 140, which may be encased in a copper layer 145. An insulating layer 150 is then deposited or applied such that the entire coated conductor architecture is encased in insulating material.
[0025] In other examples, the insulating layer 150 may be applied preferentially to certain sides or faces of the superconductor, such as the pancake coil 160 shown in FIG. 1C, which consists of a stack of multiple HTS tapes 100 sandwiched in intimate contact with and wrapped around a coil for magnet-related applications. In this case, the tape 100 is wrapped around like a roll of tape, with the side of one conductor 100 touching the other side of an adjacent conductor 100. Thus, the thin insulating layer 150 allows for a dense and compact superstructure, and the insulating coating 150 applied only to the faces between adjacent conductors in this example further minimizes the overall conductor volume.
[0026] 2A shows a first type superconductor in which the filaments of superconductor 130 are arranged in a bundle, e.g., individual honeycomb units each embedded in a matrix of silver 140, and an insulating layer 150 is applied to encapsulate the entire architecture, which is shown as circular but may also consist of linear shaped elements in bundles of various shapes. FIG. 2B shows an exemplary low temperature superconductor (LTS) in which the filaments of superconductor 130 are embedded in a matrix of copper 145, and an insulating layer 150 encapsulates the architecture. Filament bundles can also be fabricated with HTS wire by various techniques, and then the filament strands are twisted together to form the HTS bundled wire.
[0027] In certain applications, the superconductor wire or tape 100 may be reinforced to limit distortion caused by Lorentz or other forces by laminating the basic architecture (e.g., 110-140) with a metal tape 105, such as steel or brass, as shown in exemplary Figure 3. In this example, an insulating layer 150 is applied over the reinforcing tape 100 after the reinforcing tape 105 is affixed to the superconducting architecture 110-140 with solder 106 (as one example). In other approaches, the reinforcing tape 105 may be joined to the conductor by brazing or other types of metallurgical bonding methods.
[0028] Several insulating materials are used in their thin film form including HfO, MgO, SrTiO3, and others including boron nitride (BN), which is widely used in its cubic (c-BN) and hexagonal (h-BN) phases due to its properties including high thermal conductivity, resistance to thermal shock, and chemical inertness. The cubic phase material forms durable hard coatings and has improved chemical resistance at high temperatures. During the formation of c-BN, an intermediate material is formed, amorphous boron nitride (a-BN), which is transparent and insulating and therefore can be used as a dielectric in electronic devices.
[0029] 4A-4C show exemplary methods of fabricating insulated type 1 HTS 400, type 2 HTS 420, and LTS 430 superconductors, respectively. Typically, the final step common to the three types of superconductors involves depositing an insulating layer 150. The challenge is to deposit and grow a-BN at lower temperatures on substrates such as superconductors, which are very sensitive to heat. Traditionally, c-BN has been grown from borazine polymers at high temperatures using plasma-assisted CVD at temperatures of about 900C, which would be unsuitable for superconductors due to loss of lattice oxygen at high temperatures.
[0030] The superconductor 100 disclosed herein includes an insulating layer 150 of a-BN that is deposited or applied to the superconducting architecture at temperatures of about 200 C or less by utilizing less heat intensive processes including magnetron sputtering, RF sputtering, pulsed laser deposition (PLD), atomic layer deposition (ALD), plasma spray, binder spray, and electron beam evaporation.
[0031] In one example, the a-BN layer was deposited to a thickness of about 22 nm using RF sputtering, as shown in Figure 5. The resulting insulating layer had a dielectric constant (DC) of about 6.5 and a dielectric breakdown voltage (DBV) of about 9.1 MV / cm, with a dielectric constant of about 3 x 10 12 This resulted in properties including a high electrical resistivity (ER) of Ωcm. These parameters mean that at a thickness of about 22 nm, an a-BN layer would have a breakdown voltage of about 20 V. It is difficult to measure or estimate the thermal conductivity (TC) of a film with a thickness measured in nanometers. However, h-BN has a thermal conductivity as high as 400 W / mK in the c-axis at room temperature, and about 5 W / mK in the a- and b-axes at room temperature. Cubic phase BN has a structure similar to diamond and has a thermal conductivity of >700 W / mK. Thus, amorphous boron nitride exhibits a thermal conductivity of about 3 W / mK.
[0032] Thermal resistivity (TR) or R-value is defined as thickness divided by thermal conductivity (TC). For a 22 nm film, the dielectric breakdown strength (DBS) is approximately 20 V, and the thermal conductivity of 3 W / mK is 5.3×10, indicating little resistance to the flow of heat through the insulating layer (high thermal conductivity). -9 m 2 In comparison, if the insulating layer is an order of magnitude thicker, i.e., about 160 nm, the breakdown voltage increases to 140 V, while the thermal resistance (TR) is 5.3 × 10 -8 m 2 K / W. Thus, depending on the breakdown voltage required, the layer thickness can be adjusted to achieve effective heat transfer while still limiting the voltage.
[0033] In another example, a 68 nm layer of amorphous alumina is deposited on the superconductor. With a thermal conductivity of 1.73 W / mK and a dielectric breakdown strength of 300 V / μm, this film has a dielectric breakdown voltage of 20 V at room temperature and a dielectric constant of 3.9×10 -8 m 2 It will give a thermal resistance of 100 K / W.
[0034] The operating temperatures of superconductors are typically below 77 K for high temperature superconductors and below 4.2 K for low temperature superconductors. For example, the metallic components of the exemplary HTS superconductor 100, such as copper 140, silver 145, and Hastelloy C276 substrate 110, have coefficients of thermal expansion (CTE) (at room temperature) of 16.7×10 -6 , 19×10 -6 , and 11.3 × 10 -6 / °C. As temperature decreases, the CTE also decreases. For example, the CTE of copper is 16.7×10 at room temperature. -6 / ℃, 10×10 at 100K -6 / °C, 2 x 10 at 40K -6 / °C. Thus, because the volume fraction of the metal substrate 110 is significantly greater than the superconductor thin film 130, the superconductor 130 and insulating layer 150 are held in compression by the difference in the relative expansion rates of the metallic components. This is advantageous because to fracture, insulating materials must first overcome a compressive stress and then be subjected to a tensile stress.
[0035] Similarly, the large expansion of the metal in the conductor determines the contraction of the superconductor insulator. When a-BN is applied (e.g., at 200C) and then cooled to operating temperature, components with higher thermal expansion coefficients such as copper and Hastelloy contract more, resulting in a contraction of about 3×10 of this material. -6 The low CTE of 1000 .mu.m / °C induces compressive stress in the film, which is particularly useful in maintaining the integrity of the layers when the superconducting tape is wound into a coil.
[0036] For example, in the first type superconductor shown in FIG. 2A, the bulk superconductor 130 is a-BN (approximately 3×10 -6 / ℃) is approximately 14×10 -6 / °C, the conductor will tend to contract more than boron nitride when cooled to operating temperatures <77K, thus putting the insulation in compression, thereby protecting the outer coating from cracking. Similarly, composites used in structures such as that of Figure 2B also have a higher coefficient of expansion than boron nitride, thereby putting the outer surface in compression.
[0037] Recognizing that ceramic layers are much stronger when held in compression, especially in the case of superconductor insulators, a-BN films held in compression ensure that these films perform well mechanically, not just electrically and thermally.Thus, even at minimal thicknesses, a-BN insulators are able to withstand the harsh handling conditions and other processing stresses of superconductors, including windings.
[0038] As mentioned above, less heat-intensive processing techniques are required to successfully coat temperature-sensitive superconductors. In a preferred embodiment, the second type HTS tape 100 is fabricated using photoassisted metalorganic chemical vapor deposition (PAMOCVD) at a temperature of about 900C, followed by coating with an a-BN insulating layer deposited by RF sputtering at or near room temperature. FIG. 5 shows an exemplary system 500 for producing insulating superconductors by PAMOCVD combined with RF sputtering. In this example, simplified to show the major components, the MOCVD reactor 510 consists of a vacuum housing 512 that encloses the deposition system components including radiant lamps 514 and a hot block type susceptor 516 that supports and heats a translating substrate tape 110, typically stainless steel or Hastelloy. The reactor 510 is maintained at vacuum through an outlet port 518, and precursor reactant(s) 520 are introduced through a showerhead 522. For MOCVD, the precursor reactants 510 preferably consist of one or more organic ligands delivered as gas phase components, or in other embodiments may occur as solid phase components that are first evaporated prior to injection into the showerhead 522. The substrate tape 110 is heated to about 800-900 C via a susceptor 516, while radiant lamps 514 photoenhance the thin film growth of one or more buffer 120 layers and superconductor layer 130 on the substrate 110. As mentioned above, one or more additional layers (not shown), such as, for example, a stabilizing coating 140 (not shown), may also be deposited after the superconductor thin film 130.
[0039] A subsequent stage of the system 500 is a radio frequency sputtering (RFS) chamber 530 for depositing thin insulating (e.g., a-BN) material 150. RF sputtering has many advantages, including simple and cost-effective equipment, high growth rates while maintaining a high degree of control over deposition thickness, good adhesion with high uniformity, and good compatibility of superconductors due to low operating temperatures.
[0040] RF sputtering operates substantially at room temperature and low pressure and relies on alternating current (AC) power instead of direct current (DC) power, alternating at frequencies in the RF range (5-30 MHz). RF sputtering involves the sputtering of positive ions (e.g., Ar) from a sputtering gas 532 formed from a radio frequency discharge plasma. + ) is utilized to bombard a sputtering target 534 such that target atoms 536 are sputtered out and deposited on the surface of the grounded substrate. In a preferred embodiment, the sputtering target 534 may be comprised of solid hexagonal boron nitride (h-BN) to deposit an insulating layer 150 of a-BN. The grounded substrate in the HTS case is the product architecture provided from the PAMOCVD process 510, including the metal substrate 110, the buffer 120, and the superconducting thin film 130.
[0041] For clarity, Fig. 5 shows an example of these two coating-related operations (PAMOCVD and RFS), but note that other manufacturing steps are also required, as outlined in the exemplary Fig. 4, and which vary for each type of superconductor. Also, importantly, while Fig. 5 shows separate unit operations or batch mode manufacturing, the entire system 500 may be operated in a continuous or semi-continuous mode, whereby the initial substrate 110 is fed into the PAMOCVD chamber 510 via a reel-to-reel system that may then be transferred to another reel-to-reel system for the subsequent stage (e.g., 540, 530). Alternatively, a single reel-to-reel system may feed all stages of the system 500.
[0042] In a situation where a very thin film is applied to a relatively thick substrate (e.g., a 50 nm film on a 100 um thick superconducting tape, thickness ratio 2000), the stress in the film is given by:
number
[0043] High stresses such as these typically result in delamination of the coating, especially when the coated conductor is bent or formed into a coil. c and α f The stress is often lower than estimated because it decreases and becomes independent of temperature as it cools to operating temperatures (below -196C). Alternatively, stresses may be induced in the film during the formation of the coating, which further reduces damage due to high stresses.
[0044] Unexpectedly, given that the cryogenic thermal conductivity of preferred embodiments utilizing a-BN is an order of magnitude (or even two orders of magnitude, depending on the material) higher than at room temperature, very thin insulating coatings on HTS conductors provide advantageous performance characteristics, including low thermal resistance, which is one or two orders of magnitude lower than at room temperature.
[0045] Using this system and process, a thin film composite superconductor resulting from a metal substrate having a buffer layer and a superconducting layer deposited by MOCVD combined with the application by RFS of a thin (e.g., 22 nm) inorganic ceramic insulating layer at substantially room temperature (25 C) results in a robust superconductor architecture that, when cooled to temperatures below substantially 77 K, imparts a compressive mismatch between the superconducting 130 layer and the insulating 150 layer. The compressive mismatch is determined by the ratio of the volumetric thermal expansion coefficients measured at room temperature of the ceramic insulating 150 layer and the superconducting 130 layer, which in this example are 3×10, respectively. -6 / ℃ and 14×10 -6 / °C, which in turn produces a volumetric coefficient of thermal expansion (CTE) ratio of about 0.21. The total stress in the coating is the sum of the intrinsic stress (i.e., the stress imparted during the coating process) and the thermal expansion stress. The intrinsic stress can be compressive or tensile depending on the coating conditions. In order for the total stress in the coating to be negative, the conductor to coating CTE ratio is preferably less than about 0.75 to ensure that the coating is under compressive stress.
Claims
1. A thin film composite superconducting article, A metal substrate; A buffer layer; A superconducting layer; 10 at 25C -7 m 2 A ceramic insulation layer having a thermal resistance of less than K / W and a breakdown voltage of more than 20V. The thin film composite superconducting article comprises:
2. 2. The superconductor article of claim 1, wherein said ceramic insulating layer comprises an amorphous ceramic.
3. 3. The superconductor article of claim 2, wherein said amorphous ceramic is boron nitride.
4. 10. The superconducting article of claim 1, wherein the ceramic insulating layer is applied to the superconducting layer at a deposition temperature substantially equal to or less than 200C.
5. 2. The superconducting article according to claim 1, wherein the ceramic insulating layer has a thickness substantially equal to or less than 2 μm.
6. 2. The superconducting article of claim 1, wherein the superconducting layer is a high temperature superconductor.
7. A thin film composite superconducting article, A metal substrate; A buffer layer; A superconducting layer; a ceramic insulating layer having a compression mismatch with said superconducting layer when cooled to a temperature substantially equal to or less than 77K; Equipped with the mismatch is determined by a ratio of a volumetric thermal expansion coefficient measured at room temperature of the ceramic insulating layer to a volumetric thermal expansion coefficient of the superconducting layer; The ratio of the volumetric thermal expansion coefficients is substantially 0.75 or less; The thin film composite superconducting product.
8. 8. The superconductor article of claim 7, wherein said ceramic insulating layer comprises an amorphous ceramic.
9. 9. The superconductor article of claim 8, wherein the amorphous ceramic is boron nitride.
10. 8. The superconducting article of claim 7, wherein the ceramic insulating layer is applied to the superconducting layer at a deposition temperature substantially equal to or less than 200C.
11. 8. The superconducting article according to claim 7, wherein the ceramic insulating layer has a thickness substantially equal to or less than 2 μm.
12. 8. The superconducting article of claim 7, wherein the superconducting layer is a high temperature superconductor.
13. 1. A method of forming a superconducting article, comprising the steps of: Providing a metal substrate; depositing a buffer layer on the substrate; depositing a superconducting layer on the buffer layer at a first temperature; depositing a ceramic insulating layer over the superconducting layer at a second temperature such that a compressive mismatch to the superconducting layer is established upon cooling to a temperature substantially equal to or less than 77 K; The method comprising:
14. The method of claim 13 , wherein the ceramic insulating layer comprises an amorphous ceramic.
15. The method of claim 14, wherein the amorphous ceramic is boron nitride.
16. The method of claim 13 , wherein the ceramic insulating layer is deposited at a deposition temperature substantially equal to or less than 200° C.
17. 17. The method of claim 16, wherein the superconducting layer is deposited by MOCVD and the ceramic insulating layer is deposited by a different technique selected from the group of RF sputtering, magnetron sputtering, pulsed laser deposition, atomic layer deposition, or electron beam evaporation.
18. The method of claim 13, wherein the ceramic insulating layer has a thickness substantially equal to or less than 2 μm.
19. The method of claim 13 , wherein the superconducting layer is a high temperature superconductor.
20. The ceramic insulating layer is 10 -7 m 2 14. The method of claim 13, comprising a thermal resistance of less than K / W and a breakdown voltage of greater than 20V.
Citation Information
Patent Citations
Supercoductive thin film and its preparation
JP1989163058A
Thin-film magnetic head and magnetic recording device
JP1999016127A
Superconductor article and method of making and using same
JP2007524198A
Oxide superconductor and production method therefor
JP2013012321A
Superconducting thin film and a method for preparing the same
US5447908A