Chemically recycled PET manufacturing method
By recovering and reintroducing ethylene glycol into the dicarboxylic acid-diol slurry, the process addresses the viscosity issues in chemically recycling PET, ensuring smooth polymerization and equivalent properties to virgin PET using existing manufacturing equipment.
Patent Information
- Application Number
- JP2024530437
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-25
- Filing Date
- 2022-11-18
- Publication Date
- 2024-10-31
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing chemical recycling methods for PET face challenges in incorporating BHET into the virgin PET manufacturing process, leading to unbalanced OH/COOH molar ratios and increased viscosity of the dicarboxylic acid-diol slurry, which hinders smooth production of chemically recycled PET.
A process that recovers residual ethylene glycol from the polymerization reactor and reintroduces it into the dicarboxylic acid-diol slurry to balance the OH/COOH molar ratio, ensuring fluidity and enabling smooth polymerization using existing PET manufacturing equipment.
The process allows for the production of chemically recycled PET with properties similar to virgin PET by maintaining fluidity and optimizing the dicarboxylic acid-diol slurry viscosity, facilitating efficient use of existing equipment.
Smart Images

Figure 2024540632000001 
Figure 2024540632000002 
Figure 2024540632000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing chemically recycled PET. [Background technology]
[0002] The consumption of plastic products is increasing year by year. In particular, polyethylene terephthalate (PET) is widely used as a raw material for bottle containers, films, fibers, etc., and the increase in the consumption of bottle containers is particularly notable. However, plastic products such as PET do not decompose in the environment after use, and the need for recycling has been continuously emphasized due to environmental issues, and efforts to increase the recovery and recycling rates of waste PET products are ongoing worldwide.
[0003] Recycling methods for PET products can be divided into physical recycling and chemical recycling. In physical recycling, waste PET products are washed, refined, classified, and crushed, and then refined and classified again to produce flakes from which impurities have been removed, followed by an extrusion-filtration process to produce recycled PET, which is then reused as a mixture with virgin PET to produce new products such as bottles, fibers, and films. However, PET produced by such mechanical recycling methods is difficult to apply to colored PET containing pigments, and cannot be used as a product for storing food such as beverages, so there are restrictions on its use when it contains recycled PET.
[0004] Recently, therefore, research has been conducted into chemical recycling methods in which waste PET is depolymerized to produce BHET (bis(2-hydroxyethyl)terephthalate), which is then used as a raw material to polymerize PET and produce recycled PET. As an example of the chemical recycling method for PET, China Patent Publication No. 103132175 proposes a method of depolymerizing polyester waste using a metal catalyst.
[0005] The demand for recycled PET using chemical recycling continues, but there are many difficulties in incorporating BHET into the virgin PET manufacturing process to produce recycled PET with physical properties similar to those of virgin PET, making related research and development necessary. Summary of the Invention [Problem to be solved by the invention]
[0006] The present invention provides a process for producing chemically recycled PET. Specifically, the present invention provides a process for smoothly producing chemically recycled PET by recycling ethylene glycol in the esterification reaction and ensuring the fluidity of the dicarboxylic acid-diol slurry during the production of chemically recycled PET. [Means for solving the problem]
[0007] One embodiment of the present invention includes the steps of: supplying a dicarboxylic acid compound and a diol compound to a mixing vessel to obtain a dicarboxylic acid-diol slurry; feeding the BHET powder into a melting drum to obtain molten BHET; feeding the dicarboxylic acid-diol slurry and the molten BHET into a polymerization reactor and inducing an esterification reaction; recovering residual ethylene glycol from the polymerization reactor top stream; supplying the residual ethylene glycol to the mixing vessel. Effect of the Invention
[0008] The process for producing chemically recycled PET according to one embodiment of the present invention has the advantages of being able to make maximum use of existing PET production facilities, recovering and recycling ethylene glycol during the process to ensure the fluidity of the dicarboxylic acid-diol slurry, and enabling smooth polymerization of chemically recycled PET. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] In this specification, when a part "comprises" a certain component, this does not mean excluding other components, but means that the part may further include other components, unless otherwise specified.
[0010] To manufacture chemically recycled PET (C-rPET), recycled BHET (bis(2-hydroxylethyl) terephthalate) obtained by depolymerization of PET is used, and it is economical to remodel the mass production line of an existing virgin PET manufacturing plant. However, the addition of BHET containing OH functional groups requires adjustment of the amount of raw material input in the virgin PET polymerization process. For example, the BHET is produced through esterification and condensation polymerization reactions with PTA (terephthalic acid) and EG (ethylene glycol), which are raw materials for PET polymerization, to produce C-rPET. When BHET is added to an existing PET manufacturing process, the OH functional groups contained in BHET cause the OH / COOH molar ratio in the raw material to become unbalanced. Therefore, in order to balance the OH / COOH molar ratio by adding BHET, the amount of ethylene glycol needs to be reduced, but if the amount of ethylene glycol is reduced, the viscosity of the dicarboxylic acid-diol slurry increases, which may cause a problem of difficult transport to the esterification reactor.
[0011] That is, the PET polymerization process may be performed in the order of ES (Esterification), PC (Polycondensation), and SSP (Solid-state Polymerization), which correspond to a liquid phase polymerization process. When BHET is added to produce chemically recycled PET, the viscosity of the dicarboxylic acid-diol slurry supplied for the esterification reaction increases, which may make it difficult to utilize existing PET production facilities.
[0012] In order to solve the problem of the decrease in fluidity of the dicarboxylic acid-diol slurry, the present inventors have found that the problem can be solved by recovering ethylene glycol from the product of the esterification reaction and adding it to the dicarboxylic acid-diol slurry to ensure the fluidity of the dicarboxylic acid-diol slurry.
[0013] The present invention will be described in detail below.
[0014] One embodiment of the present invention includes the steps of: supplying a dicarboxylic acid compound and a diol compound to a mixing vessel to obtain a dicarboxylic acid-diol slurry; feeding the BHET powder into a melting drum to obtain molten BHET; feeding the dicarboxylic acid-diol slurry and the molten BHET into a polymerization reactor and inducing an esterification reaction; recovering residual ethylene glycol from the polymerization reactor top stream; supplying the residual ethylene glycol to the mixing vessel.
[0015] According to one embodiment of the present invention, the dicarboxylic acid compound may include at least one selected from the group consisting of aromatic dicarboxylic acid compounds having 8 to 20 carbon atoms and aliphatic dicarboxylic acid compounds having 4 to 12 carbon atoms. The aromatic dicarboxylic acid compound may be at least one selected from the group consisting of terephthalic acid, isophthalic acid, naphthalenedicarboxylic acid, and diphenyldicarboxylic acid. The aliphatic dicarboxylic acid compound may be at least one selected from the group consisting of cyclohexanedicarboxylic acid, phthalic acid, sebacic acid, succinic acid, isodecylsuccinic acid, maleic acid, fumaric acid, adipic acid, glutaric acid, and azelaic acid. Specifically, the dicarboxylic acid compound may include at least one of terephthalic acid and isophthalic acid.
[0016] According to one embodiment of the present invention, the diol compound may include at least one selected from the group consisting of aromatic diol compounds having 8 to 40 carbon atoms and aliphatic diol compounds having 2 to 12 carbon atoms. The aromatic diol compound may include at least one selected from the group consisting of polyoxyethylene-(a)-2,2-bis(4-hydroxyphenyl)propane, polyoxypropylene-(b)-2,2-bis(4-hydroxyphenyl)propane, and polyoxypropylene-(c)-polyoxyethylene-(d)-2,2-bis(4-hydroxyphenyl)propane. Here, the (a), (b), (c), and (d) may mean the number of polyoxyethylene or polyoxypropylene units. The aliphatic diol compound may include at least one selected from the group consisting of ethylene glycol, diethylene glycol, triethylene glycol, propanediol, butanediol, pentanediol, hexanediol, neopentyl glycol, cyclohexanediol, and cyclohexanedimethanol. Specifically, the diol compound may include at least one of ethylene glycol and diethylene glycol.
[0017] The chemically recycled PET manufacturing process according to the present invention utilizes existing PET manufacturing equipment, so as in the existing PET manufacturing process, a dicarboxylic acid compound and ethylene glycol are mixed in a mixing vessel to obtain a dicarboxylic acid-diol slurry, which is then supplied to a polymerization reactor.
[0018] According to one embodiment of the present invention, the BHET powder is obtained by depolymerization of waste PET. Specifically, the BHET powder is a polymerization reaction product containing BHET, and the BHET content may be 25 mol% to 50 mol%. In the case of 100 mol% BHET, since no esterification reaction is required, it is not suitable for the chemically recycled PET manufacturing process of the present invention, which utilizes the existing PET manufacturing process, and is therefore not preferred.
[0019] The chemically recycled PET manufacturing process according to the present invention utilizes existing PET manufacturing equipment, and therefore esterification (ES) and polycondensation (PS) reactions are carried out sequentially as in the virgin PET manufacturing process. Since the esterification and polycondensation reactions are liquid phase polymerization processes, in order to make the most of the existing PET manufacturing equipment, it is necessary to liquefy the solid BHET powder before supplying it to the polymerization reactor. Therefore, the present invention adds a melting drum for melting the solid BHET powder, and supplies the molten BHET in liquid phase to the polymerization reactor.
[0020] According to one embodiment of the present invention, the melting drum may melt the BHET powder at a temperature range of 110° C. to 130° C. Specifically, the melting drum may melt the BHET powder at a temperature range of 110° C. to 125° C. Within this temperature range, the BHET powder may be supplied to the polymerization reactor in a molten state without any reaction.
[0021] According to one embodiment of the present invention, ethylene glycol can be recovered from the gas phase reactants of the esterification reaction in the polymerization reactor. Specifically, the top stream of the polymerization reactor can be transferred to a distiller to recover ethylene glycol. The residual ethylene glycol thus recovered can be fed to the mixing vessel. The residual ethylene glycol can reduce the viscosity of the high-viscosity dicarboxylic acid-diol slurry to allow it to flow to the polymerization reactor.
[0022] As described above, the amount of diol compound, i.e., ethylene glycol, in the mixing vessel is reduced to balance the OH / COOH molar ratio by adding BHET, and the viscosity of the dicarboxylic acid-diol slurry may be such that it is difficult to smoothly flow through the transfer pipes in existing PET manufacturing facilities. The process for producing chemically recycled PET according to the present invention can reduce the viscosity of the dicarboxylic acid-diol slurry to 20 poise or less and allow it to flow to the polymerization reactor without adjusting the ratio of the dicarboxylic acid compound and diol compound added by recycling the remaining ethylene glycol to the mixing vessel.
[0023] According to one embodiment of the present invention, the esterification reaction in the polymerization reactor may be carried out at a temperature range of 200° C. to 260° C. and a pressure range of 1 bar to 4 bar. That is, the esterification reaction in the production process of chemically recycled PET according to the present invention may be controlled under conditions of a lower temperature range and a higher pressure range than the esterification reaction conditions in the conventional production process of virgin PET, which are carried out at a temperature range of 250° C. to 300° C. and a pressure range of 1 bar to 2 bar.
[0024] According to one embodiment of the present invention, the esterification reaction and the polycondensation reaction may be carried out in the presence of a metal catalyst selected from the group consisting of titanium compounds, antimony compounds, germanium compounds, aluminum compounds, tin compounds, or mixtures thereof. The content of the catalyst may be 1 ppm to 500 ppm based on the central metal atom of the PET resin to be polymerized.
[0025] According to an embodiment of the present invention, a phosphorus-based stabilizer may be used in the esterification reaction and the polycondensation reaction. Specifically, a phosphorus-based stabilizer selected from the group consisting of phosphoric acid, trimethyl phosphate, triethyl phosphate, triphenyl phosphate, triethyl phosphonoacetate, or a mixture of two or more thereof may be added in the esterification reaction and the polycondensation reaction.
[0026] According to an embodiment of the present invention, the molar ratio of dicarboxylic acid to diol in the esterification reaction may be 1:1.05 to 1:3.0, specifically, 1:1.05 to 1:1.3.
[0027] According to an embodiment of the present invention, the polycondensation reaction may be carried out at a temperature ranging from 250° C. to 330° C., specifically, from 270° C. to 290° C. Also, the polycondensation reaction may be carried out under a pressure ranging from 0.1 torr to 5 torr, specifically, from 0.5 torr to 2 torr.
[0028] As described above, the process for producing chemically recycled PET according to the present invention may utilize residual ethylene glycol to produce chemically recycled PET using BHET using existing PET production facilities.
Claims
1. Supplying a dicarboxylic acid compound and a diol compound to a mixing vessel to obtain a dicarboxylic acid-diol slurry; feeding BHET powder into a melting drum to obtain molten BHET; feeding the dicarboxylic acid-diol slurry and the molten BHET into a polymerization reactor and inducing an esterification reaction; recovering residual ethylene glycol from the polymerization reactor top stream; and supplying the residual ethylene glycol to the mixing vessel.
2. The method for producing chemically recycled PET according to claim 1, wherein the melting drum melts the BHET powder at a temperature in the range of 110°C to 130°C.
3. 2. The method for producing chemically recycled PET according to claim 1, wherein the esterification reaction in the polymerization reactor is carried out at a temperature range of 200 to 260° C. and a pressure range of 1 to 4 bar.
Citation Information
Patent Citations
Continuous production of polyester
JP1985163918A
Method for producing polyester
JP2006016548A
Preparation method of polyester based polymer
KR1020140100754A