RADIATION-EMITTING COMPONENT AND METHOD OF MANUFACTURING A RADIATION-EMITTING COMPONENT - Patent application
By directly applying a conversion element with a crosslinked polyorganosiloxane matrix to semiconductor chips, thermal barriers are eliminated, enhancing efficiency and reducing costs in radiation emitting components, particularly in high brightness applications.
Patent Information
- Application Number
- JP2024527272
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-26
- Filing Date
- 2022-11-24
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing radiation emitting components face challenges with thermal barriers due to the use of adhesives between semiconductor chips and conversion elements, leading to reduced efficiency and increased costs, especially in high brightness applications.
The conversion element is directly applied to the semiconductor chip without an adhesive, using a three-dimensionally crosslinked polyorganosiloxane matrix material with embedded phosphor particles, ensuring good thermal conduction and eliminating optical barriers.
This approach enhances thermal dissipation, reduces manufacturing complexity and costs, and improves efficiency by allowing high current densities and temperatures, while maintaining high color rendering index and brightness levels.
Smart Images

Figure 2024541308000001_ABST
Abstract
Description
[Technical field]
[0001] A radiation-emitting component and a method for making a radiation-emitting component are disclosed.
[0002] The problem of at least one embodiment is to provide a radiation-emitting component with improved properties. The problem of at least one further embodiment is to provide a method for manufacturing a radiation-emitting component with improved properties. These problems are solved by a component according to claim 1 and a method according to claim 16. Further configurations and further developments of the component and the method are the subject of the dependent claims.
[0003] A radiation-emitting component is disclosed. The radiation-emitting component has a semiconductor chip that, during operation, emits electromagnetic radiation in a first wavelength range from a radiation exit surface. The electromagnetic radiation in the first wavelength range thus forms the emission spectrum of the semiconductor chip and is also referred to as primary radiation. The radiation exit surface is also referred to as the radiation emission surface.
[0004] For example, the semiconductor chip is a light-emitting diode chip or a laser diode chip. Thus, the component can be a light-emitting diode (LED) or a laser. Preferably, the semiconductor chip has an epitaxially grown semiconductor layer sequence with an active region suitable for generating electromagnetic radiation. For example, the active region has a pn junction, a double heterostructure, a single quantum well or a multiple quantum well structure.
[0005] During operation, the semiconductor chip may emit electromagnetic radiation, for example, from the ultraviolet and / or visible spectral range, in particular the blue spectral range, so that the wavelength of the primary radiation is, for example, in the range of 400 nm to 500 nm.
[0006] According to at least one embodiment, the radiation-emitting component further comprises a conversion element on the cover side of the semiconductor chip comprising the radiation exit surface, the conversion element comprising a matrix material and phosphor particles embedded therein, for converting electromagnetic radiation of a first wavelength range into electromagnetic radiation of a second wavelength range. The cover side of the semiconductor chip is understood as the side facing outward from the bottom side of the semiconductor chip, extending parallel to the main extension direction of the semiconductor chip. In addition to the radiation exit surface, the cover side may comprise areas of electrical connections, saw marks and / or dark, i.e. non-emitting, edge areas.
[0007] The term "phosphor particles" is understood here and below to mean particulate wavelength-converting material, i.e. material that is set to absorb and emit electromagnetic radiation. In particular, phosphor particles absorb electromagnetic radiation that has a maximum wavelength different from the electromagnetic radiation emitted by the phosphor particles.
[0008] For example, a phosphor particle may absorb radiation with a wavelength maximum at a shorter wavelength than the emission maximum, and therefore emit radiation with an emission maximum that is red-shifted. In this case, pure scattering or pure absorption is not considered wavelength conversion.
[0009] According to at least one embodiment, the conversion element has a support surface equal to or smaller than the cover surface of the semiconductor chip. The conversion element therefore completely covers the cover surface of the semiconductor chip or only partially covers it. In the case of only partial coverage, i.e. partial coating of the cover surface of the semiconductor chip with the conversion element, certain areas, such as bond pads, edge areas and / or areas in contact with the semiconductor chip, such as saw marks, can be left specifically free of conversion elements.
[0010] According to at least one embodiment, the support surface is in full direct contact with the cover surface of the semiconductor chip. In other words, the support surface of the conversion element fits snugly against the cover surface of the semiconductor chip, regardless of the surface properties of the cover surface of the semiconductor chip. This means that the conversion element is fixed to the cover surface of the semiconductor chip without adhesive and thus has a common interface with the semiconductor chip.
[0011] According to at least one embodiment, a radiation emitting component is disclosed that includes a semiconductor chip that, in operation, emits electromagnetic radiation in a first wavelength range from a radiation exit surface and a conversion element in a cover surface of the semiconductor chip that includes the radiation exit surface, the conversion element including a matrix material and phosphor particles embedded therein, converting electromagnetic radiation in the first wavelength range into electromagnetic radiation in a second wavelength range, the conversion element having a support surface equal to or smaller than said cover surface of the semiconductor chip, said support surface being in full direct contact with said cover surface of said semiconductor chip.
[0012] The inventors have realized that arranging the conversion element directly, i.e. without adhesive, on the cover surface of the semiconductor chip allows for good thermal conduction of the conversion element. Conventionally, conversion platelets are used that have to be glued to the semiconductor chip, typically made of silicon. However, silicon has a low thermal conductivity, which results in a thermal barrier between the conversion plate and the semiconductor chip, which increases with increasing layer thickness. In the components described here, such a thermal barrier can be dispensed with, since the conversion element is arranged directly on the semiconductor chip. This means that the components can also be operated at high currents, for example in applications requiring high brightness levels, such as headlights or stage lighting. Current densities up to 1A / mm 2 Even in so-called high current applications, exceeding 100 .mu.m, the heat generated in the conversion element can be easily dissipated from this to the semiconductor chip.
[0013] The absence of an adhesive layer also has an advantageous effect on the manufacture of the components: for example, if a conventional prefabricated conversion platelet is placed on a previously applied adhesive layer, the adhesive material will be extruded and / or the reflector, e.g. silicon filled with titanium dioxide, will penetrate into the adhesive-free cavities below the edges of the platelet. Such phenomena lead to a decrease in brightness, meaning that the adhesive layer represents an optical barrier, which can be avoided by using the conversion element in the case described here. And finally, the omission of the adhesive layer simplifies and reduces the cost of the component manufacturing process, since no adhesive process is required and also fewer processes of binning, i.e. sorting the components according to their chromaticity coordinates, are required.
[0014] Furthermore, the conversion elements can be applied only to partial areas of the semiconductor chip, i.e. only defined areas of the cover side of the semiconductor chip can be coated with the conversion elements. As a result, the conversion elements are provided with only radiation emitting and radiation reflecting surfaces and no (dark) light traps, which increases the efficiency of the component. Such partial coating allows, for example, that edge areas (mesa edges) of the cover side of the semiconductor chip, approximately 10 μm to 12 μm wide, can be free of conversion elements. Areas for electrical contacts can also be left free of conversion elements and / or the radiation exit surface can only be partially coated with the conversion elements.
[0015] The components described herein are equally suitable for cold white applications, e.g. 5700K or 6500K, for warm white applications, e.g. 3200K, and for applications in which a color rendering index Ra of 80 or more, in particular 90 or more, is desired. Due to such a high color rendering index, there is a relatively high red part of the emission spectrum, and typical red emitters are particularly sensitive to high operating currents and temperatures due to their large Stokes shift and strong thermal quenching. Such high current densities and / or high operating temperatures can be achieved with the components described herein, since the conversion elements described herein are in particular in direct contact with the semiconductor chip, which allows good dissipation of the generated heat. This is a significant improvement compared to conventional conversion chips, e.g. with silicon as matrix material, since silicon has a low thermal stability and low thermal conductivity, which means that such conversion platelets can be used at current densities of 1A / mm2 up to 150°C. 2 This means that it is suitable for less than
[0016] According to at least one embodiment, the support surface of the conversion element is equal to or smaller than the radiation exit surface.
[0017] According to at least one embodiment, the semiconductor chip has a side surface, which is not provided with conversion elements. Here and below, a side surface of the semiconductor chip is to be understood as a region that runs approximately perpendicular to the main extension direction of the semiconductor chip and connects the cover surface to the bottom surface of the semiconductor chip. In particular, the side surface does not include a radiation exit surface. Thus, a loss of efficiency through the side surface of the chip can be avoided.
[0018] According to at least one embodiment, the conversion elements have a side surface with an average roughness of less than 2 μm, in particular less than 1 μm, and / or without saw marks. In particular, the side surface of the conversion element extends approximately perpendicularly to the support surface of the conversion element. The side surface of the conversion element therefore has a particularly smooth surface. The smooth side surface of the conversion element may reduce radiation from the side. Furthermore, the smooth surface of the conversion element ensures that particles, in particular phosphor particles, embedded in the matrix material of the conversion element do not damage elements adjacent to the conversion element. This is advantageous compared to conventionally used conversion platelets that are singulated by cutting or sawing and have a rather rough surface on the side surface.
[0019] According to at least one embodiment, the conversion element has side surfaces with rounded corners, so that two intersecting side surfaces form a rounded corner with a radius, rather than a clearly defined corner, e.g., without a 90° angle, such a radius being in the range of 0.04 mm to 0.1 mm, in particular 0.05 mm to 0.06 mm.
[0020] According to at least one embodiment, the conversion element has a cross-sectional area that tapers from the support surface towards the side of the conversion element facing away from the semiconductor chip. Such a conical shape can result in a particular light guide, in particular a reduction in the radiation emission area and an increase in brightness, i.e. a focusing of the emitted radiation.
[0021] According to at least one embodiment, the conversion element has a cross-sectional area that tapers from the side of the conversion element facing away from the semiconductor chip towards the support surface. Such a conical shape can result in a particular light guide, in particular an expansion of the emitted radiation.
[0022] According to at least one embodiment, the conversion element has a thickness of 150 μm or less, in particular 100 μm or less. In particular, the thickness can be 35 μm or less, for example 25 μm or less. The exact thickness can be adjusted to the size of the phosphor particles and the desired degree of conversion. For example, for a cold white emission a thickness of less than 25 μm can be used, whereas for an orange tone a thickness of the order of 80 μm to 90 μm can be selected. This allows the conversion element to be particularly thin, which for example reduces the lateral emission and ensures a good thermal coupling of the conversion element with the semiconductor chip. The thickness of the conversion element described here is particularly thin compared to conventionally used conversion platelets, which are produced on a glass plate or film and are only attached to the semiconductor chip after completion by an adhesive layer.
[0023] According to at least one embodiment, the thickness of the transduction element is 10 μm or more.
[0024] According to at least one embodiment, the conversion element has a solids content of 45% by volume or more, in particular 50% by volume or more. According to one embodiment, the solids content is formed by solid particles, which are phosphor particles up to 100%. This means that the solids content of the matrix material is high, which has a positive effect on the temperature, radiation and chemical resistance of the conversion element. In addition to phosphor particles, the solids content can be composed of microparticles / fillers and / or nanoparticles / fillers. In other words, the phosphor particles can be partially replaced by non-converting microparticles or nanoparticles, for example, so that the chromaticity coordinates can be adjusted and / or controlled while maintaining the same thickness of the conversion layer. For example, the conversion element can be heated to temperatures up to 220 ° C and up to 6 W / mm 2 It has been stable for a long time.
[0025] According to at least one embodiment, the matrix material has an organic content of less than 40% by weight, in particular less than 20% by weight. A low organic content contributes in particular to the long-term stability of the conversion element and thus the component.
[0026] According to at least one embodiment, the matrix material has a Shore D hardness of more than 50. This means that the conversion elements, for example the side of the conversion elements facing away from the semiconductor chip, can be easily reworked, such as by grinding (ground or polish). Modifications of the conversion elements, for example on the side of the conversion elements facing away from the semiconductor chip, are also conceivable. For example, the conversion elements can be suitably provided with further layers, small platelets or structuring. Furthermore, the conversion elements have a high mechanical stability due to their high hardness, which is advantageous, for example, when already applied conversion elements have to be separated from one another by sawing.
[0027] According to a further embodiment, the matrix material comprises a three-dimensional crosslinked polyorganosiloxane. Such a polyorganosiloxane is obtained from a precursor material having a curing temperature that does not damage the semiconductor chip and bonds or adheres well to it. Such a curing temperature is, for example, 220°C or less. Thus, to produce the conversion element, the precursor material of the matrix material can be applied directly to the semiconductor chip and cured there. In particular, this improves the thermal bonding between the conversion element and the semiconductor chip and increases the efficiency compared to conventional components. Furthermore, the three-dimensional crosslinked polyorganosiloxane can be formed without cracks or pores after curing, especially when the solid content is 45% by volume or more. The three-dimensional crosslinked polyorganosiloxane also has excellent thermal conductivity, especially when the organic content is low, for example less than 40% by weight.
[0028] Furthermore, the three-dimensional crosslinked polyorganosiloxane can be filled with a high proportion of phosphor particles, especially more than 45% by volume, which allows the conversion element to have high temperature, radiation and chemical resistance. After its curing, the three-dimensional crosslinked polyorganosiloxane has sufficient hardness to allow further mechanical processing and / or modification of the conversion element. The thickness of the conversion element can also be precisely adjusted, for example by grinding, which allows in particular to set the precise chromaticity coordinates of the converted radiation.
[0029] According to at least one embodiment, the three-dimensional crosslinked polyorganosiloxane has the following repeating units.
Number
[0030] In this general formula, a + b + c = 1, 0.65 ≦ a ≦ 1, 0 ≦ b + c ≦ 0.35, 0 ≦ b < 0.35, 0 ≦ c < 0.35. Further, R is independently selected from methyl, phenyl, and combinations thereof. T 1 and T 2 are independently selected from methyl, methoxy, and combinations thereof.... represents a connection point to a further repeating unit.
[0031] The three-dimensional crosslinked polyorganosiloxane also enables the embedding of various phosphor particles. According to at least one embodiment, the phosphor particles are selected from the following group. 0 < x ≦ 0.1 and 0 ≦ y ≦ 1, (RE 1-x Ce X ) 3 (Al 1-Y A’ Y ) 5 O 12 , 0 < x ≦ 0.1 and 0 ≦ y ≦ 2, (RE 1-x Ce X ) 3 (Al 5-2y Mg Y Si y )O 12 , 0 < x ≦ 0.1 and 0 ≦ y ≦ 0.5, (RE 1-x Ce x ) 3 Al 5-y Si y O 12-y N y , 0 < x ≦ 0.1, (RE 1-x Ce x ) 2 CaMg 2 Si 3 O 12 :Ce3+ , When 0 < x ≤ 0.1, (AE 1-x Eu X ) 2 Si 5 N 8 , When 0 < x ≤ 0.1, (AE 1-x Eu X )AlSiN 3 , When 0 < x ≤ 0.1, (AE 1-x Eu x ) 2 Al 2 Si 2 N 6 , When 0 < x ≤ 0.1, (Sr 1-x Eu x )LiAl 3 N 4 , When 0 < x ≤ 0.1, (AE 1-x Eu x ) 3 Ga 3 N 5 , When 0 < x ≤ 0.1, (AE 1-x Eu x )Si 2 O 2 N 2 , When 0 < 0.2 ≤ x ≤ 2.2 and 0 < y ≤ 0.1, (AE x Eu y )Si 12-2x-3y Al 2x+3y O y N 16-y , When 0 < x ≤ 0.1, (AE 1-x Eu x ) 2 SiO 4 , When 0 < x ≤ 0.1, (AE 1-x Eu x ) 3 Si 2 O 5 , When x ≤ 0.2 and 0 < y ≤ 1 - X, K 2 (Si 1-x-y Ti y Mn x )F 6 , 0 <x≦0.2で、(AE 1-x EU x ) 5 (PO 4 ) 3 Cl, 0 <x≦0.2で、(AE 1-x EU x )Al 10 O 17 , and any combination thereof, where RE is at least one of Y, Lu, Tb, Gd, AE is at least one of Mg, Ca, Sr, Ba, and A' is at least one of Sc and Ga, whereby the phosphor particles can optionally include one or more halogens.
[0032] Thus, three-dimensionally crosslinked polyorganosiloxanes offer the same flexibility in terms of chromaticity coordinate selection as conventional silicone matrices, and compared to converter ceramics and converters in which phosphor particles are embedded in glass, but offer improved optical and thermal performance, and heat resistance, compared to conventional silicone matrices.
[0033] According to at least one embodiment, the three-dimensional crosslinked polyorganosiloxane is produced from a precursor material that comprises an alkoxy-functionalized, particularly methoxy-functionalized, polyorganosiloxane resin. The three-dimensional crosslinked polyorganosiloxane thus produced has a low organic content, less than 40% by weight, particularly less than 20% by weight.
[0034] According to at least one embodiment, the precursor material has the following repeating units:
number
[0035] In this general formula, a+b+c=1, 0.65≦a≦1, 0≦b+c≦0.35, 0≦b<0.35, and 0≦c<0.35. Furthermore, R is independently selected from methyl, phenyl, and combinations thereof. 1 and T2 are independently selected from methyl, methoxy, and combinations thereof. ... represent points of attachment to additional repeat units.
[0036] According to at least one embodiment, the transduction element further comprises a filling material, which may be selected from the following group: - Oxides, e.g. SiO 2 , especially nano-SiO 2 and micro SiO 2 , ZrO 2 , TiO 2 , Al 2 O 3 and ZnO, nitrides such as AlN, Si 3 N 4 , BN and GaN, - Carbon-based filling materials, such as carbon nanotubes, graphene and its derivatives, heteropolyacids, such as 12-tungstophosphoric acid (H 3 P 12 WO 40 ) and 12-tungstosilicic acid (H 4 SiW 12 O 40 ), - organometallic components, such as alkoxides of silicon, titanium, zirconium, aluminium and / or hafnium; - organic molecules such as adhesion promoters, defoamers, thickeners, diluents, and plasticizers; - organic and inorganic polymers, such as poly(dimethylsiloxane), poly(methylphenylsiloxane), poly(diphenylsiloxane), and polysilsesquioxanes (PSQ); and combinations thereof can be selected. The above inorganic nanoparticles can be provided with a coating material on their surface to achieve good compatibility with the precursor material for producing the matrix material of the conversion element.
[0037] According to at least one embodiment, the component has connections for electrical contact, which are present on the side of the semiconductor chip facing away from the radiation exit face. This means that the connections are present on the non-emitting side of the semiconductor chip and can be soldered or glued there in an electrically conductive manner. Such semiconductor chips, also called flip chips, can be easily combined with the conversion elements described herein.
[0038] According to at least one embodiment, the component has connections for electrical contact, which are present on the side of the semiconductor chip facing the radiation-emitting surface. Such a semiconductor chip is in particular insulatively bonded or soldered to a base, such as a substrate, and can be easily combined with the conversion elements described herein.
[0039] According to at least one embodiment, the component comprises connections for electrical contact, the connections being present on the side of the semiconductor chip facing away from the radiation exit surface and on the side of the semiconductor chip facing the radiation exit surface. The connections are therefore arranged on different sides of the semiconductor chip. For example, bond pads are arranged on the side of the semiconductor chip facing away from the radiation exit surface and conductive soldering or bonding is arranged on the side of the semiconductor chip facing away from the radiation exit surface. Such semiconductor chips can also be combined with the conversion elements described herein.
[0040] The possibility of combining the conversion elements described here with semiconductor chips of different types is based, inter alia, on the fact that the conversion elements can be applied as partial coatings and thus dark areas, in particular edge areas and / or areas in contact with the semiconductor chip, can be left without conversion elements.
[0041] Further disclosed is a method for manufacturing the component. The method is particularly suitable for manufacturing the components described herein. Thus, all features mentioned in relation to the component also apply to the method and vice versa.
[0042] According to at least one embodiment, in this method, at least one semiconductor chip is provided, which emits electromagnetic radiation in a first wavelength range from the radiation exit surface during operation. It should be understood that by at least one semiconductor chip, the method can be used to provide not only a single semiconductor chip with a conversion element, but also multiple semiconductor chips at the same time. If multiple semiconductor chips are provided with conversion elements at the same time, the semiconductor chips can also be connected to each other and singulated after applying the conversion elements. Thus, this method allows multi-chip coating.
[0043] According to at least one embodiment, the method further includes depositing a precursor material embedded with phosphor particles that convert electromagnetic radiation in a first wavelength range to electromagnetic radiation in a second wavelength range, the deposition occurring directly on at least one region of a cover surface of the semiconductor chip that includes a radiation exit surface.
[0044] Precursor materials are materials that react through a chemical reaction initiated by an external influence to form the desired material present in the finished component. The external influence may include, for example, an increase in temperature or irradiation. Precursor materials may be, for example, alkoxy-functionalized, and in particular methoxy-functionalized, polyorganosiloxane resins. Such precursor materials may react to form three-dimensional crosslinked polyorganosiloxanes.
[0045] Direct deposition means that the precursor material is directly in contact with the cover surface of the semiconductor chip, has a common interface with the semiconductor chip, and fits closely to the cover surface of the semiconductor chip. Thus, an adhesive layer can be omitted. This is made possible, among other things, by ensuring that the precursor material has a certain adhesion and that the precursor material is fixed to the desired area of the semiconductor chip.
[0046] "On at least a portion of the cover surface" shall mean that the entire cover surface of the semiconductor chip is coated with the precursor or that only a partial coating is performed, with no precursor remaining on any particular area of the cover surface of the semiconductor chip.
[0047] According to at least one embodiment, the precursor material is deposited by a method selected from doctor blading, spraying, and printing. According to at least one embodiment, the precursor material embedded with phosphor particles is deposited in the form of a homogeneous mixture, which may also contain further filler substances. Possible filler substances and phosphor particles have already been mentioned in connection with the component and also apply to the method.
[0048] According to at least one embodiment, the method further comprises curing the precursor material to form a conversion element comprising a matrix material (5) and phosphor particles (1) embedded therein, the conversion element having a support surface equal to or smaller than the cover surface of the semiconductor chip, the support surface being in full direct contact with the cover surface of the semiconductor chip. Thus, during the curing process, a matrix material is formed from the precursor material, in which the phosphor particles are embedded, and which is substantially or completely free of pores and cracks. The conversion element is then fixed to the area of the cover surface of the semiconductor chip where the precursor material was previously deposited.
[0049] According to at least one embodiment, a method for manufacturing a radiation-emitting component is disclosed, the method including the following method steps. - providing at least one semiconductor chip that, in operation, emits electromagnetic radiation in a first wavelength range from a radiation exit face; - depositing a precursor material embedded with phosphor particles and adapted to convert electromagnetic radiation in a first wavelength range into electromagnetic radiation in a second wavelength range directly onto at least one area of a cover surface of the semiconductor chip, the area including the radiation exit surface; and - hardening the precursor material to form a conversion element comprising a matrix material and phosphor particles embedded therein, the conversion element having a support surface equal to or smaller than a cover surface of the semiconductor chip, the support surface being in full direct contact with the cover surface of the semiconductor chip.
[0050] The method is particularly simple and cost-effective to implement, since no adhesive layer is required between the semiconductor chip and the conversion element. Thus, no gluing step is necessary. Furthermore, the manufactured component is free of adhesive layers that represent a thermal and / or optical barrier between the conversion element and the semiconductor chip. Furthermore, the precursor material can be specifically deposited on the emission and / or reflection areas of the semiconductor chip, which allows mapping the shape of the active area and, for example, dark edge areas that are free of conversion elements. This reduces efficiency losses. Further advantages of components manufactured using the method described here have already been shown for the components and apply analogously to components manufactured using the method.
[0051] According to at least one embodiment, the curing is performed at a temperature of 220° C. or less. This means that a temperature is used for curing that will not damage temperature sensitive light emitting materials such as semiconductor chips, nitride phosphors, etc. According to one embodiment, the curing is performed for a period of 5 hours or less, particularly 2 hours or less.
[0052] According to at least one embodiment, a plurality of semiconductor chips are provided, which are singulated after deposition and hardening of the precursor material. Thus, by this method, a multi-chip coating can be realized. Furthermore, singulation results in a semiconductor chip on which the conversion elements are arranged, which has a smooth side surface. After singulation, the side surface of the conversion elements has a roughness of less than 2 μm, in particular less than 1 μm. Due to the hardness of the matrix material, the conversion elements can be easily separated mechanically, for example by sawing. Alternatively, if the precursor material is deposited such that the support surface of the conversion elements is smaller than the cover surface of the semiconductor chip, no separation or singulation of the conversion elements is necessary at all. In this case, only the semiconductor chips are singulated. This variant also presents conversion elements which are already provided with a smooth side surface as a result of the manufacturing process. If only the semiconductor chips have to be singulated, this likewise leads to cost advantages, since sawing of the conversion elements and the associated wear are avoided. Furthermore, due to the very smooth side surface of the conversion elements, components with particularly good optical performance can be provided.
[0053] According to at least one embodiment, the thickness and shape of the conversion element are adjusted during deposition and / or curing of the precursor material. For example, the precursor material can be applied to at least some areas of the cover surface of the semiconductor chip, where it is pre-cured at a first temperature and mechanically brought to the desired thickness, for example by grinding, in this state. The material can then be fully cured at a second temperature, in particular a temperature higher than the first temperature, to form the matrix material.
[0054] Alternatively or additionally, the precursor material can be structured during deposition. This can be done, for example, using lithographic processes. For example, before the deposition of the precursor material, a photoresist layer can be applied to the cover side of the semiconductor chip and structured by exposure to light. The resulting structure, i.e. the cover side of the semiconductor chip, can then be filled with precursor material in areas free of the photoresist layer and pre-cured. Full curing can take place via further steps, such as chemically removing the structured photoresist layer. Such methods can in particular be used to generate conical shapes and / or rounded corners of the conversion elements, as already explained above. For example, the structured photoresist layer forms a mask, and the resulting conversion elements can have a cross-sectional area that widens in the direction away from the semiconductor chip. According to another example, conversion elements can be generated by a so-called LDI (laser direct imaging) process, with a cross-sectional area that tapers in the direction away from the semiconductor chip.
[0055] According to at least one embodiment, the precursor material is crosslinked three-dimensionally during curing. In particular, when an alkoxy-functionalized polyorganosiloxane resin is used as the precursor material, during curing, a low three-dimensional SiO 2 structure with a weight ratio of organic residues of less than 40%, in particular less than 20% is obtained. 2 A network is formed in which solid particles are embedded, up to 100% of which are phosphor particles. The solids content of the conversion elements is, for example, at least 45% by volume, in particular at least 50% by volume.
[0056] Further advantageous and further embodiments of the components and methods can be taken from the exemplary embodiments described below in conjunction with the drawings. [Brief description of the drawings]
[0057] [Figure 1] 1 illustrates a schematic cross-sectional view of a transduction element according to an exemplary embodiment; [Diagram 2] 1 illustrates a schematic cross-sectional view of a component in accordance with an exemplary embodiment; [Diagram 3] 1A-1C show schematic cross-sectional views of a component according to an exemplary embodiment, and FIG. 1D shows a top view of the component according to an exemplary embodiment. [Figure 4] 1A-1C show schematic cross-sectional views of a component according to an exemplary embodiment, and FIG. 1D shows a top view of the component according to an exemplary embodiment. [Diagram 5] 1 illustrates a schematic cross-sectional view of a component in accordance with an exemplary embodiment; [Figure 6] 1 illustrates a schematic cross-sectional view of a component in accordance with an exemplary embodiment; [Figure 7] 1 shows an optical microscope image of a transduction element according to an example embodiment. [Figure 8] 1 shows an optical microscope image of a transduction element according to an example embodiment. [Figure 9] 1A-C show schematic cross-sectional views of components according to various exemplary embodiments. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0058] In the exemplary embodiments and figures, identical, similar or similarly acting elements may each be given the same reference numerals. The depicted elements and their relative sizes are not to scale. Rather, individual elements, such as layers, elements, components, regions, etc., may be depicted with exaggerated sizes for better depiction and / or understanding.
[0059] To manufacture a component according to an exemplary embodiment, a semiconductor chip 10, in particular a LED chip or a plurality of semiconductor chips in the form of a chip wafer, is provided. A precursor material with embedded phosphor particles 1 or a homogeneous mixture comprising a precursor material with embedded phosphor particles 1 is deposited directly on the cover surface 12 of the one or more semiconductor chips 10.
[0060] The precursor material is a methoxy-functionalized polyorganosiloxane resin having the following repeating units:
Number
[0061] The mixture is deposited by doctor blade, printing or spraying directly onto areas of the cover surface 12 of one or more semiconductor chips 10 (partial coating) or onto the entire cover surface 12. For example, in the case of partial coating, the areas of the semiconductor chip 10 where the conversion elements 20 are not provided are protected by a photoresist, which is removed again after the precursor material has been deposited and pre-cured.
[0062] After depositing the precursor material or a mixture containing the precursor material, the precursor material is cured to form a three-dimensional crosslinked polyorganosiloxane as the matrix material 5. The curing is carried out at a temperature of 220° C. or less. The three-dimensional crosslinked polyorganosiloxane has the following repeating units:
number
[0063] In this general formula, a+b+c=1, 0.65≦a≦1, 0≦b+c≦0.35, 0≦b<0.35, and 0≦c<0.35. Furthermore, R is independently selected from methyl, phenyl, and combinations thereof. 1 and T 2 are independently selected from methyl, methoxy, and combinations thereof. ... represent points of attachment to additional repeat units.
[0064] The thickness of the conversion element 20 thus produced is between 10 μm and 150 μm depending on the desired chromaticity coordinates.
[0065] 1 shows a cross-section of an exemplary embodiment of a transduction element 20 manufactured as described above. For better visualization of the details, the transduction element 20 is shown here without the semiconductor chip 10 to which it is directly applied.
[0066] The conversion element 20 comprises a matrix material 5 in which phosphor particles 1 are embedded. Also shown in Fig. 1a is a support surface 21 which is in direct contact with a cover surface 12 (not shown here) of the semiconductor chip 10. The conversion element 20 in Fig. 1a has side surfaces 25 in parallel planes which are perpendicular to the support surface 21.
[0067] Figures 1b and 1c show two alternative shapes of the conversion element 20. In contrast to Figure 1a, the cross-sectional area 26 of the conversion element is also shown here, which in Figure 1b tapers from the support surface 21 towards the opposite side of the support surface 21 (the side facing away from the semiconductor chip 10). Such a conical shape makes it possible, for example, to concentrate radiation during operation of the component 100. In Figure 1c, the conversion element 20 is also conical in shape, but the cross-sectional area 26 of the conversion element 20 increases with increasing distance from the support surface 21. Such a shape makes it possible, for example, to spread out radiation during operation of the component 100.
[0068] 2 shows a schematic cross-sectional area of an exemplary embodiment of a component 100 including a conversion element 20 according to FIG. 1. In each case, a semiconductor chip 10 is shown, on whose cover surface 12 the support surface 21 of the conversion element 20 is applied in direct contact and fits snugly without adhesive. This ensures good thermal conduction between the conversion element 20 and the semiconductor chip 10. The cover surface 12 also includes the radiation exit surface 11 of the semiconductor chip 10, but may be larger than this. FIG. 2a shows a component 100 with a conversion element 20 according to FIG. 1a, FIG. 2b shows a component 100 with a conversion element 20 according to FIG. 1b and FIG. 2c shows a component 100 with a conversion element 20 according to FIG. 1c. Also shown is a side surface 15 of the semiconductor chip 10 on which the conversion element 20 is not provided.
[0069] Figures 3a-c and 4a-c are schematic cross-sectional views of a component 100 in each case in which a transduction element 20 is applied as a partial coating to a semiconductor chip 10. For clarity, not all reference numbers shown in figures 1 and 2 are shown here, but they apply analogously to figures 3 and 4. Figures 3d and 4d respectively show the component 100 in a top view.
[0070] Figures 3a and 4a show the conversion element 20 of figure 1a, figures 3b and 4b show the conversion element 20 of figure 1b and figures 3c and 4c show the conversion element 20 of figure 1c of the semiconductor chip 10. In each case the conversion element 20 is applied to the semiconductor chip 10 as a partial coating. According to the top view of figure 3d, the area of the electrical connections 40 (bond pads or bond bars) and the saw marks 41 is free of the conversion element 20. The conversion element 20 covers the radiation exit surface 11 and the dark edge areas (mesa edges) 42 of the cover side of the semiconductor chip 10 and is shown hatched for clarity.
[0071] In Fig. 4, the conversion elements 20 extend only up to the radiation exit surface 11 and are shown as hatched layers in Figs. 4a-4c for illustrative purposes. Fig. 4d shows this arrangement of the conversion elements 20 again in a top view of the component 100, where the conversion elements 20 are shown as hatched layers.
[0072] Figure 5 shows a further variant of the component 100, where the conversion element 20 extends only over a partial area of the radiation exit surface 11, which is again shown as an additional layer in Figures 5a to 5c for illustrative purposes. The conversion element of Figure 1a is arranged on the semiconductor chip 10 of Figure 5a, the conversion element of Figure 1b is arranged on the semiconductor chip 10 of Figure 5b and the conversion element of Figure 1c is arranged on the semiconductor chip 10 of Figure 5c.
[0073] Another difference with the component 100 of the previous figures is that in Fig. 5 a potting 30 is shown laterally surrounding both the semiconductor chip 10 and the conversion element 20. The potting 30 can have various shapes and filling heights. The potting 30 can be flush with the conversion element 20, as shown in Fig. 5a, or can protrude beyond the conversion element 20 (Figs. 5b and 5c). Furthermore, the potting 30 can have parallel sided sidewalls (Fig. 5a) or sidewalls that are inclined towards the conversion element 20 (Figs. 5b and 5c). The potting can be made of, for example, silicone or epoxy resin, and can optionally be made of, for example, TiO 2 In further configurations, the nanoparticles can be filled with, for example, TiO 2 In addition, other filler materials may be included.
[0074] 6 shows a schematic cross-section of a semiconductor chip wafer as a number of successive semiconductor chips 10 to which conversion elements 20 have already been applied. After singulation, a number of components 100 are thus obtained by multi-chip coating.
[0075] Figure 7 shows a top view of the conversion element 20 under an optical microscope. It can be seen that the conversion element 20 is not provided in the area of the electrical connections 40 (bond bars) and the sawtooth 41. The conversion element 20 therefore only covers the radiation exit surface 11. The size of the conversion element 20 is approximately 1 mm 2 In this image, the transduction elements 20 have been fabricated by multi-chip coating, as the underlying semiconductor chip 10 has not yet been singulated. The corners of the transduction elements 20 are rounded, and the sides 25 of the transduction elements 20 appear straight and intact, i.e., no chips are visible.
[0076] Figure 8 shows the conversion elements 20 corresponding to Figure 7, still seen obliquely, before the singulation of the semiconductor chips 10, i.e. after multichip coating. They have the shape as described with reference to Figure 1b and are approximately 1 mm 2In addition to the rounded corners, the smooth, clearly structured and flawless side surfaces 25 of the conversion element can also be seen here. The thickness of the conversion element in this case is 25-30 μm. To apply the cold white color, garnet phosphor particles 1 are embedded.
[0077] FIG. 9 shows schematic cross-sectional views of a component 100 with different types of semiconductor chips 10, which can be combined with the conversion element 20 described here. In each of FIGS. 9a-c, the conversion element 20 according to FIG. 1a is applied to the semiconductor chip 10. However, any combination of the conversion element 20 described here with the various semiconductor chip types is also possible. In FIGS. 9a-c, the semiconductor chips 10 are each provided with electrical connections 40, both of which can be present on the side of the semiconductor chip 10 facing outward from the cover side 12 (flip-chip design, FIG. 9a). In this case, the cover side 12 can be completely covered by the conversion element 20, although partial coating is also contemplated. The electrical connections 40 can also be present on the cover side 12 and on the side of the semiconductor chip 10 facing outward from the cover side 12 (FIG. 9b) and also both on the cover side 12 of the semiconductor chip (FIG. 9c).
[0078] Exemplary embodiment 1: Component 100 with LED flip chip 10 having conversion element 20 for cool white applications Using alkoxy-functionalized polyorganosiloxane resin as a precursor material, nano-SiO 2 , optionally micro-SiO 2, and phosphor particles 1 containing one or more yellow-emitting garnet phosphors for producing a cold white emission, is sprayed over the entire cover surface 12 of an LED semiconductor chip 10 in flip-chip design (i.e. all electrical connections 40 for electrical contacts are present on the side of the semiconductor chip 10 facing outwards from the conversion element 20) or an LED semiconductor chip wafer in flip-chip design and cured for several hours at up to 150 ° C. The layer thickness of the conversion element 20 obtained for this chromaticity coordinate is 10-100 μm depending on the exact composition and particle size of the phosphor particles 1. Deposition of the homogeneous mixture is also possible by doctor blading or printing.
[0079] If the conversion elements 20 are not provided in the areas of the cover surface 12, they can also be partially removed there. Alternatively, these areas can be protected by a photoresist, which is also removed after the homogeneous mixture has been deposited and the conversion elements 20 have been formed. The conversion elements 20 can be subsequently surface-coated, for example with an optical coating, such as an anti-reflection coating (AR) or a coating for improving the color over angle (COA). Depending on the desired properties, the surface of the conversion elements 20 facing outwards from the semiconductor chip 10 can be rough or smooth, and the thickness of the conversion elements 20 can be readjusted.
[0080] Exemplary embodiment 2: Component 100 with an LED semiconductor chip 10 with electrical connections 40 on the cover side 12 and on the side of the semiconductor chip 10 facing outwards from the cover side 12 and a conversion element 20 on the cover side 12 for cool white applications All areas of the cover surface 12 of the semiconductor chip 10 that are to be kept free of the conversion elements 20, such as bond pads / bars as electrical connections 40 for electrical connections on the cover surface 12 of the semiconductor chip 10, and optionally saw marks 41 and optionally dark non-emissive areas on the cover surface 12 of the semiconductor chip 10, are protected by photoresist. Next, alkoxy-functionalized polyorganosiloxane resin as a precursor material, nano-SiO 2 , optionally micro-SiO2 A homogeneous mixture containing phosphor particles 1, which contain one or more yellow-emitting garnet phosphors for producing a cold white emission, is deposited by doctor blading or printing on the cover side 12 of the LED semiconductor chip 10 or LED semiconductor chip wafer and cured at up to 120°C for 1 hour. After removing the photoresist, the resulting conversion element 20 can be post-cured again at an elevated temperature, for example 220°C. The layer thickness of this chromaticity coordinate conversion element is 10-100 μm depending on the exact composition and particle size of the phosphor particles 1. The homogeneous mixture can also be atomized by spraying.
[0081] Alternatively, it is also conceivable to combine a complete coating of the cover surface 12 with a homogeneous mixture with a subsequent partial removal of the transduction element 20 .
[0082] The conversion element 20 can be subsequently surface coated, for example with an optical coating, such as an anti-reflection coating (AR) or a coating for improving color over angle (COA). Depending on the desired properties, the surface of the conversion element 20 facing away from the semiconductor chip 10 can be rough or smooth, and the thickness of the conversion element 20 can be readjusted.
[0083] Exemplary embodiment 3: component 100 with an LED semiconductor chip 10 with electrical connections 40 on the cover side 12 and on the side of the semiconductor chip 10 facing outwards from the cover side 12 and a conversion element 20 on the cover side 12 for orange (amber) applications This component is manufactured similarly to the exemplary embodiment 2, but with an amber phosphor mixture (green and red emitting phosphor particles 1). The layer thickness of the conversion layer of this color coordinate is 30-150 μm depending on the exact composition and particle size of the phosphor particles.
[0084] The conversion elements 20 can be subsequently surface coated, for example with an optical coating, such as an anti-reflection coating (AR). Depending on the desired properties, the surface of the conversion elements 20 facing away from the semiconductor chip 10 can be rough or smooth, and the thickness of the conversion elements 20 can be readjusted.
[0085] Exemplary embodiment 4: Component 100 with LED semiconductor chip 10 with electrical connections 40 only on the cover side 12 with conversion element 20 for warm white applications The component is manufactured in the same way as in the exemplary embodiment 3, but with a different type of chip with respect to the electrical connections 40 and a warm white phosphor mixture containing one or more different green- and red-emitting phosphor particles 1. The layer thickness of the conversion element 20 for this chromaticity coordinate is between 20 and 120 μm depending on the exact composition and particle size of the phosphor particles 1.
[0086] The conversion element 20 can be subsequently surface coated, for example with an optical coating, such as an anti-reflection coating (AR) or a coating for improving color over angle (COA). Depending on the desired properties, the surface of the conversion element 20 facing away from the semiconductor chip 10 can be rough or smooth, and the thickness of the conversion element 20 can be readjusted.
[0087] Subsequent surface coatings may also be multiple coatings, ie, multiple identical or different coatings may be applied to the transduction element 20 .
[0088] The features and example embodiments described in connection with the figures can be combined with each other according to further example embodiments, even if not all combinations are explicitly described. Furthermore, the example embodiments described in connection with the figures can alternatively or additionally have further features, such as those described in the summary section.
[0089] The present invention is not limited by the description based on the exemplary embodiments, but rather, any novel feature and any combination of features, including in particular any combination of features in the claims, is included in the present invention even if the feature or combination itself is not explicitly recited in the claims or in the exemplary embodiments.
[0090] This patent application claims priority from German patent application No. 102021131112.8, the disclosure of which is incorporated herein by reference. [Explanation of symbols]
[0091] 1. Phosphor particles 5. Matrix Material 10. Semiconductor Chips 11 Radiation exit plane 12 Cover surface 15 Side of a semiconductor chip 20 Conversion Factors 21 Support surface 25 Aspects of conversion factors 26 Cross-sectional area of transformation elements 30 Potting 40 Connection 41 Saw marks 42 Boundary Region 100 Components
Claims
1. A radiation-emitting component (100), comprising: a semiconductor chip (10) that, in operation, emits electromagnetic radiation in a first wavelength range from a radiation exit surface (11); a conversion element (20) on a cover surface (12) of the semiconductor chip (10) comprising the radiation exit surface (11), the conversion element (20) comprising a matrix material (5) and phosphor particles (1) embedded therein, the conversion element (20) converting electromagnetic radiation in the first wavelength range into electromagnetic radiation in a second wavelength range, the conversion element (20) has a support surface (21) equal to or smaller than the cover surface (12) of the semiconductor chip (10), the support surface (21) being in full direct contact with the cover surface (12) of the semiconductor chip (10); the conversion element (20) has a cross-sectional area (26) that tapers from the support surface (21) towards a side of the conversion element (20) that faces away from the semiconductor chip (10), or the conversion element (20) has a cross-sectional area (26) that tapers from a side of the conversion element (20) that faces away from the semiconductor chip (10) towards the support surface (21); and / or The conversion element (20) is a radiation-emitting component (100) having side surfaces (25) with rounded corners.
2. The radiation emitting component (100) of claim 1, wherein the support surface (21) is equal to or smaller than the radiation exit surface (11).
3. 3. The radiation-emitting component (100) according to claim 1 or 2, wherein the semiconductor chip (10) has a side surface (15), the side surface (15) being free of the conversion element (20).
4. The radiation emitting component (100) according to any one of the preceding claims, wherein the conversion element (20) has a side surface (25) with an average roughness of less than 2 μm and / or without saw marks.
5. Radiation-emitting component according to any one of the preceding claims, wherein the conversion element (20) is applied only to a partial area of the semiconductor chip (10).
6. The radiation emitting component (100) according to any one of claims 1 to 5, wherein an edge region of the cover surface (12) of the semiconductor chip (10) is free of the conversion elements (20), and the width of the edge region is selected from the range of 10 μm to 12 μm.
7. Radiation-emitting component (100) according to any one of the preceding claims, wherein the conversion element (20) has a thickness of less than or equal to 150 μm and / or greater than or equal to 10 μm.
8. The radiation-emitting component (100) according to any one of the preceding claims, wherein the conversion element (20) has a solids content of 45% by volume or more.
9. The radiation-emitting component (100) according to any one of the preceding claims, wherein the matrix material (5) has an organic content of less than 40% by weight.
10. The radiation emitting component (100) according to any one of the preceding claims, wherein the matrix material (5) has a hardness >50 Shore D.
11. The radiation-emitting component (100) according to any one of the preceding claims, wherein the matrix material (5) is a three-dimensionally crosslinked polyorganosiloxane.
12. The radiation-emitting component (100) of claim 11, wherein the three-dimensional crosslinked polyorganosiloxane is prepared from a precursor material comprising an alkoxy-functionalized polyorganosiloxane resin.
13. The radiation emitting component (100) according to any one of claims 1 to 12, further comprising a connection (40) for electrical contact, said connection (40) being present on the side of the semiconductor chip (10) facing away from the radiation exit surface (11).
14. The radiation emitting component (100) according to any one of the preceding claims, further comprising a connection (40) for electrical contact, said connection (40) being present on the side of the semiconductor chip (10) facing towards the radiation exit surface (11).
15. The radiation emitting component (100) according to any one of claims 1 to 12, further comprising connection portions (40) for electrical contact, said connection portions (40) being present on the side of the semiconductor chip (10) facing away from the radiation exit surface (11) and on the side of the semiconductor chip (10) facing towards the radiation exit surface (11).
16. A method of manufacturing a radiation-emitting component (100), comprising the steps of: - providing at least a semiconductor chip (10) which, in operation, emits electromagnetic radiation in a first wavelength range from a radiation exit surface (11); - depositing a precursor material, embedded with phosphor particles (1) and converting said first wavelength range of electromagnetic radiation into a second wavelength range, directly onto at least one area of the cover surface (12) of said semiconductor chip (10), including said radiation exit surface (11), - hardening said precursor material to form a conversion element (20) comprising a matrix material (5) and said phosphor particles (1) embedded therein, said conversion element (20) having a support surface (21) equal to or smaller than said cover surface (12) of said semiconductor chip (10), said support surface (21) being in full direct contact with said cover surface (12) of said semiconductor chip (10), the precursor material is structured during deposition, and the conversion element (20) has a cross-sectional area (26) that tapers from the support surface (21) in a direction towards a side of the conversion element (20) that faces away from the semiconductor chip (10), or the conversion element (20) has a cross-sectional area (26) that tapers from a side of the conversion element (20) that faces away from the semiconductor chip (10) in a direction towards the support surface (21), and / or The method, wherein the transduction element (20) has sides (25) with rounded corners.
17. 17. The method of claim 16, wherein the curing is carried out at a temperature of 220°C or less.
18. 18. The method of claim 16 or 17, wherein a plurality of semiconductor chips (20) are provided and singulated after said depositing and said curing of said precursor material.
19. The method according to any one of claims 16 to 18, wherein the thickness and shape of the conversion element (20) are adjusted during the deposition and / or the curing of the precursor material.
20. The method of any one of claims 16 to 19, wherein the precursor material is crosslinked in three dimensions during curing.
Citation Information
Patent Citations
Semiconductor light-emitting device and light-emitting module
JP2013247269A
Methods for manufacturing optoelectronic devices and optoelectronic devices
JP2013526047A
Method of manufacturing light emitting device
JP2015195294A
Manufacturing method of optoelectronic component and optoelectronic component
JP2020184641A
Segmented LED array architecture with reduced phosphor emitting surface area
JP2021507530A