Precision multi-axis photolithography alignment correction using stressor films
Stressor films on the backside of wafers correct wafer curvature in multiple directions, addressing overlay errors and enhancing pattern printing accuracy in semiconductor manufacturing.
Patent Information
- Application Number
- JP2024529315
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-08-16
- Filing Date
- 2022-11-04
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-11-04
AI Technical Summary
Semiconductor manufacturing processes face challenges in maintaining wafer flatness due to induced stresses from multiple film layers, leading to overlay errors and non-uniformity of critical features, exacerbated by heating and clamping issues, particularly in advanced patterning and 3D device construction.
The application of stressor films on the backside of wafers to modify wafer geometry in multiple directions, using direct write laser patterning to correct curvature and alignment, allowing stepwise correction in orthogonal directions to improve overlay accuracy.
Enhances overlay alignment precision by correcting wafer curvature in multiple axes, reducing overlay errors and improving pattern printing accuracy on semiconductor wafers.
Smart Images

Figure 2024541404000001_ABST
Abstract
Description
[Technical field]
[0001] Incorporation by Reference This disclosure claims the benefit of U.S. Provisional Patent Application No. 63 / 281,431, filed November 19, 2021, entitled "Precision Multi-Axis Photolithography Alignment Correction Using Stressor Film," and U.S. Non-Provisional Patent Application No. 17 / 888,553, filed August 16, 2022, entitled "Precision Multi-Axis Photolithography Alignment Correction Using Stressor Film," which are incorporated by reference in their entireties herein.
[0002] The present disclosure relates to semiconductor manufacturing, and more particularly to wafer curvature, bow and overall wafer shape. [Background technology]
[0003] The background description provided herein is intended to generally present the context of the present disclosure. The inventors' work to the extent described in this Background section and aspects of the description that would not otherwise be admitted as prior art at the time of filing are not expressly or implicitly admitted as prior art to the present disclosure.
[0004] Semiconductor manufacturing involves several different steps and processes. One typical manufacturing process is known as photolithography (also called microlithography). Photolithography uses radiation, such as ultraviolet or visible light, to create fine patterns in semiconductor device designs. Semiconductor manufacturing techniques, including photolithography, etching, film deposition, surface cleaning, metallization, etc., can be used to construct a variety of semiconductor devices, such as diodes, transistors, and integrated circuits.
[0005] An exposure system (also called an exposure tool) is used to implement photolithography techniques. An exposure system typically includes an illumination system, a reticle (also called a photomask) or a spatial light modulator (SLM) that creates the circuit pattern, a projection system, and a wafer alignment stage that aligns a semiconductor wafer covered with a photosensitive resist. The illumination system illuminates an area of the reticle or SLM with a (preferably) rectangular slot illumination field. The projection system projects an image of the illuminated area of the reticle pattern onto the wafer. For accurate projection, it is important to expose the wafer to the light pattern, which is relatively flat or planar, preferably with a height deviation of less than 10 microns. Summary of the Invention
[0006] Aspects of the present disclosure provide a method for improving overlay alignment of patterning by correcting wafer shape. For example, the method may include receiving a wafer having a work surface with at least partially fabricated semiconductor devices and a back surface opposite the work surface. The method may also include forming a first stressor film on the back surface. The first stressor film may modify the overlay alignment of the work surface in a first direction across the work surface of the wafer and may not include overlay alignment in a second direction across the work surface of the wafer. The second direction is different from the first direction. The method may also include forming one or more first semiconductor structures on the work surface of the wafer. The first semiconductor structures are aligned in the first direction.
[0007] In one embodiment, the second direction may be rotated at least 15 degrees relative to the first direction. For example, the second direction may be rotated 45 degrees relative to the first direction. As another example, the second direction may be orthogonal to the first direction.
[0008] In one embodiment, the method may further include forming a second stressor film on the backside after forming the first semiconductor structure on the working surface of the wafer, the second stressor film modifying an overlay alignment of the working surface in a second direction across the working surface of the wafer, and forming one or more second semiconductor structures on the working surface of the wafer, the second semiconductor structures being aligned in the second direction. In another embodiment, the method may further include forming a second stressor film on the backside after forming the first semiconductor structure on the working surface of the wafer, the second stressor film modifying an overlay alignment of the working surface in a second direction across the working surface of the wafer, and modifying the first semiconductor structure on the working surface of the wafer, the modified first semiconductor structure being aligned in the second direction. In yet another embodiment, the method may further include forming a second stressor film on the backside prior to forming the first semiconductor structure on the working surface of the wafer, the second stressor film modifying an overlay alignment of the working surface in a second direction across the working surface of the wafer, and modifying the first semiconductor structure on the working surface of the wafer after forming the first semiconductor structure on the working surface of the wafer, the modified first semiconductor structure being aligned in the second direction. For example, the first stressor film and the second stressor film are formed in a lithography-etch-lithography-etch (LELE) process or a lithography-freeze-lithography-etch (LEFE) process.
[0009] In one embodiment, the first stressor film may be patterned based on a measurement of the curvature of the wafer in a first direction. For example, the first stressor film may be patterned using direct write patterning.
[0010] Aspects of the present disclosure also provide another method of improving patterning overlay alignment by correcting wafer shape. For example, the method may include receiving a wafer having a work surface with at least partially fabricated semiconductor devices and a back surface opposite the work surface. The method may also include forming a stressor film on the back surface. The stressor film may modify the overlay alignment of the work surface in a first and second direction across the work surface of the wafer. The method may also include forming one or more semiconductor structures on the work surface of the wafer. The semiconductor structures are aligned in the first and second directions.
[0011] In one embodiment, the stressor film may be patterned based on a curvature measurement of the wafer in a first direction and a curvature measurement of the wafer in a second direction. In another embodiment, the stressor film may be patterned based on α times the curvature measurement of the wafer in a first direction and (1-α) times the curvature measurement of the wafer in a second direction, where 0≦α≦1. For example, α is 1 / 2.
[0012] It should be noted that this summary section does not specify all embodiments and / or inherently novel aspects of the present disclosure or claimed invention. Rather, this summary provides only a preliminary discussion of various embodiments and corresponding points of novelty over the prior art. For additional details and / or possible perspectives of the present disclosure and embodiments, the reader is directed to the Detailed Description section and corresponding figures of the present disclosure, which are further described below. [Brief description of the drawings]
[0013] Various embodiments of the present disclosure, proposed by way of example, will now be described in detail with reference to the following figures, in which like reference numerals refer to like elements, and in which:
[0014] [Figure 1] FIG. 2 shows an alignment tree that is prepared before the photomask is generated. [Figure 2A]FIG. 1 illustrates an example of an overlay patterning error. [Figure 2B] FIG. 1 illustrates an example of an overlay patterning error. [Figure 2C] FIG. 1 illustrates an example of an overlay patterning error. [Figure 2D] FIG. 1 illustrates an example of an overlay patterning error. [Figure 3A] FIG. 1 illustrates the alignment of two layers without wafer stress compensation. [Figure 3B] FIG. 13 illustrates the alignment of two layers when wafer stress compensation in the X direction is performed, according to some embodiments of the present disclosure. [Figure 3C] FIG. 3C illustrates further alignment of the layers shown in FIG. 3B when wafer stress compensation in the Y direction is performed according to some embodiments of the present disclosure. [Figure 4] 1 is a flowchart illustrating an example method for improving patterning overlay alignment by correcting wafer shape in two directions, according to some embodiments of the present disclosure. [Figure 5A] 1A-1C illustrate correction of overlay alignment of a work surface of a wafer in a first direction according to some embodiments of the present disclosure. [Figure 5B] 1A-1C illustrate correction of overlay alignment of a work surface of a wafer in a first direction according to some embodiments of the present disclosure. [Figure 5C] 1A-1C illustrate correction of overlay alignment of a work surface of a wafer in a first direction according to some embodiments of the present disclosure. [Figure 5D] 1A-1C illustrate correction of overlay alignment of a work surface of a wafer in a first direction according to some embodiments of the present disclosure. [Figure 6A] 5A-5D in a second direction according to some embodiments of the present disclosure. FIG. [Figure 6B]5A-5D in a second direction according to some embodiments of the present disclosure. FIG. [Figure 6C] 5A-5D in a second direction according to some embodiments of the present disclosure. FIG. [Figure 6D] 5A-5D in a second direction according to some embodiments of the present disclosure. FIG. [Figure 7A] FIG. 1 illustrates a Lithography-Etch-Lithography-Etch (LELE) process used in accordance with some embodiments of the present disclosure. [Figure 7B] FIG. 1 illustrates a Lithography-Etch-Lithography-Etch (LELE) process used in accordance with some embodiments of the present disclosure. [Figure 7C] FIG. 1 illustrates a Lithography-Etch-Lithography-Etch (LELE) process used in accordance with some embodiments of the present disclosure. [Figure 7D] FIG. 1 illustrates a Lithography-Etch-Lithography-Etch (LELE) process used in accordance with some embodiments of the present disclosure. [Figure 8A] FIG. 1 illustrates a lithography-freeze-lithography-etch (LFLE) process used in accordance with some embodiments of the present disclosure. [Figure 8B] FIG. 1 illustrates a lithography-freeze-lithography-etch (LFLE) process used in accordance with some embodiments of the present disclosure. [Figure 8C] FIG. 1 illustrates a lithography-freeze-lithography-etch (LFLE) process used in accordance with some embodiments of the present disclosure. [Figure 8D] FIG. 1 illustrates a lithography-freeze-lithography-etch (LFLE) process used in accordance with some embodiments of the present disclosure. [Figure 9A]FIG. 13 illustrates correction of wafer bow and curvature in only the X-direction according to some embodiments of the present disclosure. [Figure 9B] FIG. 13 illustrates correction of wafer bow and curvature in only the X-direction according to some embodiments of the present disclosure. [Figure 9C] FIG. 13 illustrates correction of wafer bow and curvature in only the X-direction according to some embodiments of the present disclosure. [Figure 10A] FIG. 13 illustrates correction of wafer bow and curvature in only the Y direction according to some embodiments of the present disclosure. [Figure 10B] FIG. 13 illustrates correction of wafer bow and curvature in only the Y direction according to some embodiments of the present disclosure. [Figure 10C] FIG. 13 illustrates correction of wafer bow and curvature in only the Y direction according to some embodiments of the present disclosure. [Figure 11] 1 is a flowchart illustrating an exemplary method for improving patterning overlay alignment by correcting wafer shape in a single axis, according to some embodiments of the present disclosure. [Figure 12A] FIG. 13 illustrates an example of average X-correction and Y-correction results, according to some embodiments of the present disclosure. [Figure 12B] FIG. 13 illustrates an example of average X-correction and Y-correction results, according to some embodiments of the present disclosure. [Figure 12C] FIG. 13 illustrates an example of average X-correction and Y-correction results, according to some embodiments of the present disclosure. [Figure 12D] FIG. 13 illustrates an example of average X-correction and Y-correction results, according to some embodiments of the present disclosure. [Figure 13] 1 is a flowchart illustrating an exemplary method for improving patterning overlay alignment by correcting wafer shape, according to some embodiments of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] Current semiconductor manufacturing developments incorporate techniques such as advanced patterning and 3D device structures to reduce feature sizes and increase device density. However, the implementation of such techniques brings new challenges for proper microfabrication. These new manufacturing methods involve creating multiple layers of films of various materials on the wafer surface. However, each layer adds more stress to the wafer's surface. As layers of films build up, the induced stress distorts the flat wafer. This distortion has been shown to reduce the size uniformity of critical features across the wafer's surface.
[0016] This distortion also causes overlay errors and problems. Various manufacturing process steps can cause the substrate to expand and / or contract, resulting in a warped or curved substrate. For example, the substrate during exposure is locally heated by the energy transferred to the substrate from the exposure beam. The substrate is also heated during the annealing process. This heating causes the substrate to expand. If the substrate expansion is not controlled, the expansion will exceed the overlay error requirements. Furthermore, if the clamping force between the substrate and the substrate chuck is insufficient to prevent the substrate from expanding, the substrate may slip on the substrate chuck, resulting in a larger expansion of the substrate and a larger overlay error. Slippage may be more pronounced in some processes, such as extreme ultraviolet (EUV) systems, because the environment surrounding the substrate during exposure is a vacuum. Thus, vacuum clamping is not always possible and weaker electrostatic clamps must be used instead of vacuum clamps.
[0017] Other manufacturing processes may also cause the substrate to expand and contract. For example, a deposited film may cause the substrate to shrink. Furthermore, various annealing or doping processes may cause a significant amount of bowing in a given substrate. Annealing processes may especially cause overlay problems. As a result of these various manufacturing processes, the substrate may become non-uniform or non-flat. For example, the backside of the substrate may have z-height variations (i.e., vertical height variations), with some areas being higher and some areas being lower. Such bowing z-height variations may be on the order of about 1 micron to about 100 microns. This variation is quite large, since the semiconductor devices or structures exposed by the various exposure tools are exposed on the scale of tens to hundreds of nanometers. Thus, bowing variations of thousands to 10,000 nanometers may dramatically reduce yields.
[0018] FIG. 1 shows an alignment tree 100 prepared before a photomask is generated. In the alignment tree 100, layer L7 is aligned using the alignment marks of layer L1, and layers L11 and L12 are aligned using the alignment marks of layer L7. Layer L7 is directly aligned to layer L1, and layers L11 and L12 are indirectly aligned to layer L1. Layers L1, L7, L11, and L12 may be transistors, fins, metal layers, masks, or any other sacrificial or final structures on a wafer formed during microfabrication. Walkout of successive layers may occur. During the microfabrication process, it is inevitable that stress is induced on each layer, so that successive layers may gradually shift relative to each other and the first layer.
[0019] Microfabrication generates stresses on the wafer due to deposition, removal, annealing, etching, etc. of various materials. Due to process stresses on the wafer, some of the possible wafer curvatures are Zernike polynomials, including vertical tiling, horizontal tilt, oblique astigmatism, defocus, etc. Figures 2A-2D show an example of an overlay patterning error. There are various patterns of wafer curvature and curvature. This example shows oblique astigmatism, resulting in layer L11 being misaligned to various degrees in both the X and Y directions (the dashed lines show where layer L11 is desired to be located, and the solid lines show where L11 is actually located due to the wafer curvature).
[0020] For partially processed substrates, conventional techniques used to address substrate bowing and non-uniform curvature focus on chucking techniques, where the substrate is chucked (or clamped / sucked) to a substrate holder to flatten the curvature. However, if the curvature is relatively significant, it may be very difficult or impossible to accurately flatten the substrate with chucking alone. It is therefore desirable to have a substrate bow correction technique that corrects the substrate bow to improve overlay before it is sent or returned to the scanner for further exposure.
[0021] The techniques described herein include methods to improve overlay alignment of patterning by correcting wafer shape or correcting wafer curvature and radius to print patterns on the wafer more accurately. The techniques described herein include alignment or correction in a single axis or direction followed by secondary alignment or correction in another axis or direction. Such stepwise multi-axis correction can achieve higher accuracy compared to correcting curvature in all directions at once. Thus, the techniques described herein provide alignment correction in different directions in a stepwise or continuous manner. Some techniques provide correction in one direction and no correction in another direction (typically orthogonal).
[0022] The techniques disclosed herein use a stressor film on the backside of the wafer. In some embodiments, a direct-write laser process is used exclusively to modify the stress values to create the optimal wafer shape using a wafer shape correction tool. Such a stress correction tool is configured to modify the wafer shape (wafer bow, wafer curvature) to improve overlay. One technique is to deposit one or more stressor films on the backside of the wafer. The one or more stressor films may have different initial internal stresses. The stressor films can be patterned and etched to selectively increase or decrease stress at given point locations across the backside, thereby modifying the wafer shape and thereby improving the overlay value. The patterning can be performed using direct-write laser exposure. An advantage of direct-write patterning is that the intensity at each coordinate location on the wafer can be controlled by software and laser based on the wafer shape signature or wafer bow measurement to create the patterning. Thus, it is easily possible to vary the exposure pattern from wafer to wafer. Of course, mask-based exposure is also envisioned. As an option, a given stressor film described herein can be removed in selective areas of the backside. The stressor films described herein can be reset and either kept in place or removed. The stressor films described herein can be a single layer or N layers. The stressor films described herein can be modified between the X and Y directions or can be multi-axis photolithography alignment corrections.
[0023] FIG. 3A shows the alignment of layer L2 with respect to layer L1 without wafer stress compensation. Note that there is a misalignment in both the X and Y directions. This is a problem to be solved. FIG. 3B shows the alignment of layer L2 with respect to layer L1 first with wafer stress compensation in the X direction according to the present disclosure. Note that in the X direction, layer L2 is correctly aligned with layer L1, but in the Y direction there is still a misalignment with layer L1. FIG. 3C shows the alignment of layer L2 with respect to layer L1 further with wafer stress compensation in the Y direction according to the present disclosure. Note that layer L2 is also aligned with layer L1 in the Y direction. The X and Y directions run across the working surface of the wafer and are orthogonal to each other. Thus, wafer stress is compensated and layer L2 is aligned with respect to layer L1 in two steps.
[0024] The techniques disclosed herein use backside film stress modification and novel lithographic integration.
[0025] FIG. 4 is a flow chart illustrating an exemplary method 400 for improving overlay alignment of patterning by correcting wafer shape in two different axes according to some embodiments of the present disclosure. For example, the method 400 can correct the wafer curvature and bow in two or more independent directions to print patterns on the wafer more accurately. Thus, two masks can be used. Nevertheless, with a wafer shape correction tool, an additional masking layer can be integrated with the backside stressor film. In one embodiment, the two or more independent directions can include an X direction and a Y direction. In another embodiment, the two or more independent directions can include a first direction and a second direction that is rotated at least 15 degrees, e.g., 45 degrees, relative to the first direction.
[0026] Typically, one or more stressor films may be deposited on the backside of the wafer, which is opposite the working surface where the active devices are located. A photoresist film may then be deposited and patterned on the backside. Patterning may be done with a photomask and a scanner, but patterning is preferably performed using direct-write laser exposure. Direct-write is preferred because the exposure pattern can be modified or tailored to each individual wafer. For example, the shape of each wafer may be measured to generate a wafer curvature measurement. The wafer curvature measurement may be, for example, a map of relative z-height variation across the wafer or other overlay misalignment measurement. After the photoresist formed on the backside is patterned and developed, one or more stressor films may be etched. This modifies the internal stress of the wafer, resulting in a modification of the wafer shape, for example improving the overlay or flattening the wafer. The stressor film may have an initial internal stress, which may be tensile or compressive. By selectively removing material from each coordinate location, the internal stress of the wafer is modified accordingly.
[0027] To induce / modify stress, further backside film correction techniques are introduced, for example, an epoxy film, whose internal stress changes as a response to the pattern of light corresponding to each specific location of the epoxy film. Thus, stress modification can be performed without the need for etching. Thus, a stressor film as described herein refers to any film formed on the backside of a wafer and treated to induce stress modification to the wafer. This may include depositing one (or more) stressor films (e.g., silicon oxide or silicon nitride films), coating the stressor film with a photoresist layer, exposing (e.g., direct writing), developing the photoresist layer, etching the stressor film, and removing the photoresist layer. At this point, patterning of the working surface of the wafer can proceed. The techniques described herein have found distinct advantages over incremental overlay correction. One finding is that correcting alignment in one direction at a time can achieve higher accuracy compared to correcting curvature in all directions at once. Thus, the techniques described herein provide alignment correction in different directions in a stepped or continuous manner, and some techniques provide correction in one direction but not in another (typically orthogonal) direction.
[0028] Method 400 begins at step S410, where a wafer is received having a back surface and a working surface opposite the back surface. The working surface may have at least partially fabricated devices and measurements of wafer curvature of the wafer may be made as a result of one or more microfabrication steps on the working surface. For example, as shown in Figures 5A and 5B, layers L1 and L7 are formed on the working surface of the wafer. It is desirable to add layer L11 at an indicated location (shown by the dashed line), where layer L11 is spaced apart from layers L1 and L7 or aligned independently of the alignment of layers L1 and L7.
[0029] In step S420, a first stressor film 510, shown in Figures 5A and 5B, is deposited and formed on the backside of the wafer. In one embodiment, the first stressor film 510 is used to correct the overlay alignment of the working surface of the wafer in a first direction (e.g., X direction) across the working surface of the wafer, and no stress correction is performed in the Y direction. Thus, the first stressor film 510 targets the overlay alignment correction in one direction (e.g., X direction) and not in another direction (e.g., Y direction). For example, a wafer with layers L1 and L7 formed on the working surface can be measured to determine the curvature measurement of the wafer in the X direction, and the first stressor film 510 can have its internal stress in the X direction corrected based on the curvature measurement in the X direction. In one embodiment, the first stressor film 510 is coated with a photoresist layer, the photoresist layer is patterned and developed according to the curvature measurement in the X direction, and the first stressor film 510 is etched by dry or wet etching to remove the photoresist layer, whereby the internal stress of the first stressor film 510 is modified according to the curvature measurement in the X direction of the wafer, and as a result, the wafer is considered to be near flat or flat in the X direction. In another embodiment, the first stressor film 510 may be responsive to heat such that its internal stress is changed by the applied heat, and heat in a pattern corresponding to the curvature measurement in the X direction may be applied to the first stressor film 510. In some other embodiments, the first stressor film 510 may be responsive to light of a first wavelength such that its internal stress is changed by exposure to light of the first wavelength, and light of a first wavelength in a pattern corresponding to the curvature measurement in the X direction may be generated to expose the first stressor film 510. The first stressor film 510 thus formed is used to correct overlay alignment in a first direction (i.e., the X direction) and does not include substantial or significant overlay alignment in a second direction (e.g., the Y direction) that is different from the first direction or perpendicular to the first direction.
[0030] Next, a photoresist layer L11x may be formed on the working surface of the wafer and aligned in the X direction with respect to layer L1. The photoresist layer L11x may be patterned, exposed, and developed in a lithography process to form a hard mask L11x as shown in FIG. 5C and FIG. 5D, and the wafer may be etched accordingly. Note that the hard mask L11x is formed and placed between layers L1, and no alignment correction in the Y direction is performed. Thus, the hard mask L11x covers a portion of layer L7. This may be acceptable depending on the etching selectivity and patterning purpose. The hard mask L11x is aligned in the X direction, i.e., does not overlap layer L1.
[0031] In step S430, the second stressor film 610 shown in Figures 6A and 6B is deposited and formed on the backside of the wafer. In one embodiment, the second stressor film 610 is used to correct the overlay alignment of the working surface of the wafer in a second direction (e.g., Y direction) across the working surface of the wafer, and no stress correction is performed in the X direction. Thus, the second stressor film 610 targets the overlay alignment correction in one direction (e.g., Y direction) and not in another direction (e.g., X direction). For example, measuring a wafer with layers L1 and L7 formed on the working surface and the first stressor film 510 formed on the backside can reveal the curvature measurement of the wafer in the Y direction, and the second stressor film 610 can have its internal stress in the Y direction corrected based on the curvature measurement in the Y direction. In one embodiment, the second stressor film 610 is coated with a photoresist layer, the photoresist layer is patterned and developed according to the Y-direction curvature measurements, and the second stressor film 610 is etched by dry or wet etching to remove the photoresist layer, whereby the internal stress of the second stressor film 610 is modified according to the Y-direction curvature measurements of the wafer, and the wafer is considered near flat or flat in the Y-direction. In another embodiment, the second stressor film 610 may be heat-responsive such that its internal stress is changed by applied heat or may be heat-responsive to a second wavelength of light such that its internal stress is changed by exposure to the second wavelength of light, and heat in a pattern corresponding to the Y-direction curvature measurements is applied to the second stressor film 610, or light in a pattern corresponding to the Y-direction curvature measurements is generated to expose the second stressor film 610. The second stressor film 610 thus formed is used to correct the overlay alignment in a second direction (i.e., the Y direction) and does not include any substantial or significant overlay alignment in a first direction (e.g., the X direction) that is different from or perpendicular to the second direction.
[0032] Next, a photoresist layer L11y may be formed on the working surface of the wafer and aligned in the Y direction with respect to layer L7. The photoresist layer L11y may be patterned, exposed, and developed in a lithography process to form a hard mask L11 as shown in Figures 6C and 6D, and the wafer may be etched accordingly. Note that the hard mask L11 is formed and disposed between layers L1 and L7, is aligned in the X and Y directions, and does not overlap layers L1 and L7.
[0033] In one embodiment, the first stressor film 510 can be removed in selective areas of the backside of the wafer before the second stressor film 610 is formed. Stress memorization can also be used here. In some embodiments, even if the first stressor film 510 is removed, the semiconductor lattice still has a memory effect because the stress of the first stressor film 510 is transferred to the silicon lattice of the wafer.
[0034] In some embodiments, the second stressor film 610 and the first stressor film 510 can be formed in a double patterning lithography process. For example, in a lithography-etch-lithography-etch (LELE) process, as shown in FIG. 7A, the second stressor film 610 and the first stressor film 510 are formed on the backside of the wafer 710, and a first resist layer 720 is coated on the first stressor film 510 and patterned according to the curvature measurement in the X direction. As shown in FIG. 7B, the first stressor film 510 is etched. As shown in FIG. 7C, the first resist layer 720 is stripped, and a second resist layer 730 is coated on the second stressor film 610 and patterned according to the curvature measurement in the Y direction. As shown in FIG. 7D, the second stressor film 610 is etched, and the second resist layer 730 is stripped. In the LELE process, two lithography steps and two etching steps are performed. As another example, in the lithography-freeze-lithography-etch (LFLE) process, as shown in FIG. 8A, a first resist layer 720 is coated on the second stressor film 610 and patterned according to the curvature measurement in the X direction, and as shown in FIG. 8B, the patterned first resist layer 720 is frozen by chemical processing. As shown in FIG. 8C, a second resist layer 730 is coated on the second stressor film 610 and patterned according to the curvature measurement in the Y direction. As shown in FIG. 8D, the second stressor film 610 is etched to modify its internal stress according to the curvature measurement in the X direction and the Y direction, and the first resist layer 720 and the second resist layer 730 are stripped. In the LFLE process, two lithography steps and only one etching step are performed. The first stressor film 510 and the second stressor film 610 may be formed in a lithography-curing-lithography-etching (LCLE) process, in which the patterned first resist layer 720 is baked instead of frozen in a chemical process.
[0035] In step S440, one or more semiconductor devices (e.g., layer L11) may be formed on the work surface of the wafer, and the semiconductor devices may be aligned in the X and Y directions because the wafer curvature in the first and second directions of the wafer has been corrected and the wafer is considered near-flat or flat in the X and Y directions.
[0036] The embodiments described herein also include corrections in a single axis or direction at a time. Some embodiments include alignment corrections in only one direction if sufficient for the desired microfabrication application. For example, in some microfabrication processes, there may be certain features that only have alignment dependency in the X direction or alignment dependency in the Y direction. Such features may be isolated on the X mask and Y mask, respectively, eliminating the need for a cut mask approach. An example with vias 900 is shown in FIG. 9A. In this figure, layer L2 with vias arranged in the Y direction is formed on layer L1 with metal signal lines. The critical vias in the X direction of layer L2 may be on hard mask L2x, as shown in FIGS. 9B and 9C. Another example with vias 1000 is shown in FIG. 10A. In this figure, layer L2 with vias arranged in the X direction is formed on layer L1 with metal signal lines. The critical vias in the Y direction of layer L2 may be on hard mask L2y, as shown in FIGS. 10B and 10C.
[0037] FIG. 11 is a flow chart illustrating an example method 1100 for improving overlay alignment of patterning by correcting wafer shape in a single axis, according to some embodiments of the present disclosure. For example, the method 1100 can correct the bow and curvature of the wafer in a single axis, as described according to FIGS. 9A-9C and 10A-10C. The method 1100 starts with step S410, followed by step S420, in which a first stressor film 510 is formed and patterned on the backside of the wafer to correct the overlay alignment of the work surface of the wafer in a first direction (e.g., X-direction). In step S1130, one or more first semiconductor devices (e.g., vias 900 or layer L2x) can be formed on the work surface of the wafer. Since the wafer bow in the first direction of the wafer is corrected and the wafer is considered to be near or flat in the X-direction, the first semiconductor devices can be aligned in the X-direction. The method 1100 may then perform step S430, in which a second stressor film 610 is formed and patterned on the backside of the wafer to correct the overlay alignment of the work surface of the wafer in a second direction (e.g., the Y direction). In step S1150, one or more second semiconductor devices (e.g., via 1000 or layer L2y) may be formed on the work surface of the wafer. Because the wafer curvature in the second direction of the wafer has been corrected and the wafer is considered near flat or flat in the Y direction, the second semiconductor devices may be aligned in the Y direction.
[0038] Some embodiments may include average X and Y corrections. The layers may be L1 to Ln, where n is between 1 and 300. For example, an alignment tree is prepared as follows: L1→L7→L11, with layers L1 and L7 already patterned. Ideally, the wafer shape for hard mask L11x is L1, while the wafer shape for hard mask L11y is L7. In one embodiment, the wafer shape is L11=αL1+(1-α)L7, where 0≦α≦1. For example, α=½ and L11=(L1+L7) / 2. As an advantage, this process is less costly due to less processing (one stressor film). Figures 12A-12D show an example result. Note that layer L11 is aligned within layers L1 and L7, but not as precisely as in the case of stepwise correction and placement. This alignment correction is still better than without the use of a stressor film.
[0039] FIG. 13 is a flow chart illustrating an exemplary method 1300 for improving overlay alignment of patterning by correcting wafer shape, according to some embodiments of the present disclosure. For example, the method 1300 may include an average X and Y correction of the wafer curvature and curvature, as described in accordance with FIGS. 12A-12D. The method 1300 begins with step S410. In step S1320, a stressor film is deposited and formed on the backside of the wafer. In one embodiment, the stressor film is used to correct the overlay alignment of the wafer's working surface in the average of a first and second direction (e.g., X and Y directions) across the working surface of the wafer. For example, measuring a wafer with layers L1 and L7 formed on the working surface can reveal the wafer's X and Y curvature measurements, and the stressor film can have its X and Y internal stresses corrected based on the X and Y curvature measurements. For example, the stressor film may have its internal stresses in the X and Y directions modified based on α times the curvature measurement in the X direction and (1-α) times the curvature measurement in the Y direction, where 0≦α≦1, e.g., α=½. Method 1300 may also include step S440, in which one or more semiconductor devices (e.g., layer L11) may be formed on a work surface of a wafer. The wafer curvature in the first and second directions of the wafer may be modified such that the wafer is flatter in the X and Y directions than a wafer without a stressor film formed on its backside, such that the semiconductor devices may be aligned in the X and Y directions.
[0040] In another exemplary embodiment, in the example of A, H, Z, another way to approach the Zx Zy problem is to preemptively match the shapes of A and H. Assuming H has a relatively large overlay budget, it would be easy to apply a wafer shape correction tool to manipulate the wafer shape to match A. Then, when Z should be layered, there is a best Zx→A and Zy→H overlay. Even if the overlay budget of H is not large, a co-optimization can be done to match A while staying within the budget, which makes the wafer tool correction in Z easier. In the above flow, A and H are interchangeable. If A is more flexible, feedback from previous lots can be used to preemptively make A's shape similar to H.
[0041] The precision multi-axis disclosed herein is partly realized by performing photolithography exposures. Exposing at the limit of resolution of a given photolithography system often makes it easy to print features as lines during exposure. Thus, by performing multiple exposures, lines can be printed in different directions. Of course, lithography exposures are quite different from stress correction, but here, the stress correction can be improved by splitting the directional stress correction into components. For example, correction and application in the X direction is followed by correction and application in the Y direction. Some transistor designs may have a 45 degree feature shift, so a third alignment correction may be performed as well as a fourth alignment correction and a fifth alignment correction, etc. Thus, by splitting the backside alignment correction into component directions, improved precision and accuracy of aligned patterning is realized.
[0042] In the above description, specific details have been described, such as the specific geometry of the processing system and a description of the various components and processes used. However, it should be understood that the technology described herein can be implemented in other embodiments that differ from these specific details, and such details are for the purpose of explanation, not limitation. The embodiments disclosed herein have been described with reference to the accompanying drawings. Similarly, for the purpose of explanation, specific numerical values, materials, and configurations have been shown to provide a sufficient understanding. However, the embodiments can be implemented without such specific details. Components having substantially the same functional structure are indicated by similar reference numerals, and redundant descriptions may be omitted.
[0043] It should be understood that the order of description of the various steps described herein has been presented for clarity of description. In general, these steps may be performed in any suitable order. Moreover, although each of the various features, techniques, configurations, etc. described herein may be described in separate parts of the disclosure, it is understood that each concept may be performed independently of each other or in combination with each other. Thus, the disclosure may be implemented and viewed in a variety of ways.
[0044] To aid in understanding various embodiments, various techniques have been described as multiple separate operations. The order of description should not be construed to imply that these operations are necessarily order dependent. In fact, these operations need not be performed in the order presented. The described operations may be performed in a different order than in the described embodiments. In additional embodiments, various additional operations may be performed and / or described operations may be omitted.
[0045] As used herein, "substrate" or "target substrate" generally refers to an object to be processed according to the present disclosure. The substrate may include any material portion or structure of a device, particularly a semiconductor device or other electronic device, such as a base substrate structure, such as a semiconductor wafer, a reticle, or a layer (such as a thin film) on or overlaid on the base substrate structure. Thus, the substrate is not limited to any particular base structure, lower layer, or upper layer, patterned or unpatterned, but is contemplated to include any such layer or base structure, and any combination of layers and / or base structures. While the above description may refer to a particular type of substrate, this is for illustrative purposes only.
[0046] Those skilled in the art will also understand that various modifications may be made to the operation of the above-described techniques that achieve the same purpose of the present disclosure. Such modifications are intended to be included within the scope of the present disclosure. Thus, the above description of the embodiments of the present disclosure is not intended to be limiting. Rather, any limitations to the embodiments of the present disclosure are presented in the following claims.
Claims
1. receiving a wafer having a work surface having at least partially fabricated semiconductor devices thereon and a back surface opposite the work surface; forming a first stressor film on the backside, the first stressor film modifying an overlay alignment of the working surface in a first direction across the working surface of the wafer and not including an overlay alignment in a second direction across the working surface of the wafer, the second direction being different from the first direction; forming one or more first semiconductor structures on the work surface of the wafer, the first semiconductor structures being aligned in the first direction; The method includes:
2. The method of claim 1 , wherein the second orientation is rotated at least 15 degrees relative to the first orientation.
3. The method of claim 2 , wherein the second direction is rotated 45 degrees relative to the first direction.
4. The method of claim 2 , wherein the second direction is orthogonal to the first direction.
5. forming a second stressor film on the backside surface of the wafer after forming the first semiconductor structure on the work surface of the wafer, the second stressor film modifying an overlay alignment of the work surface in the second direction across the work surface of the wafer; forming one or more second semiconductor structures on the work surface of the wafer, the second semiconductor structures being aligned in the second direction; The method of claim 1 further comprising:
6. 6. The method of claim 5, wherein the first stressor film and the second stressor film are formed by a lithography-etch-lithography-etch (LELE) process or a lithography-freeze-lithography-etch (LFLE) process.
7. forming a second stressor film on the backside surface of the wafer after forming the first semiconductor structure on the work surface of the wafer, the second stressor film modifying an overlay alignment of the work surface in the second direction across the work surface of the wafer; modifying the first semiconductor structure on the work surface of the wafer, the modified first semiconductor structure being aligned in the second direction; The method of claim 1 further comprising:
8. The method of claim 7 , wherein the first stressor film and the second stressor film are formed by a LELE process or a LFLE process.
9. forming a second stressor film on the backside surface prior to forming the first semiconductor structure on the work surface of the wafer, the second stressor film modifying an overlay alignment of the work surface in the second direction across the work surface of the wafer; after forming the first semiconductor structure on the work surface of the wafer, modifying the first semiconductor structure on the work surface of the wafer, the modified first semiconductor structure being aligned in the second direction; The method of claim 1 further comprising:
10. 10. The method of claim 9, wherein the first stressor film and the second stressor film are formed by a lithography-etch-lithography-etch (LELE) process or a lithography-freeze-lithography-etch (LFLE) process.
11. The method of claim 1 , wherein the first stressor film is patterned based on a curvature measurement of the wafer in the first direction.
12. The method of claim 1 , wherein the first stressor film is patterned using direct write patterning.
13. receiving a wafer having a work surface having at least partially fabricated semiconductor devices thereon and a back surface opposite the work surface; forming a stressor film on the backside surface, the stressor film extending across the working surface of the wafer to modify an overlay alignment of the working surface in first and second directions; forming one or more semiconductor structures on the work surface of the wafer, the semiconductor structures being aligned in the first and second directions; The method includes:
14. 14. The method of claim 13, wherein the stressor film is patterned based on curvature measurements of the wafer in the first and second directions.
15. 15. The method of claim 14, wherein the stressor film is patterned based on α times the curvature measurement of the wafer in the first direction and (1-α) times the curvature measurement of the wafer in the second direction, where 0≦α≦1.
16. The method of claim 15, wherein α is ½.
17. The method of claim 13 , wherein the stressor film is patterned using direct write patterning.
18. The method of claim 13 , wherein the second orientation is rotated at least 15 degrees relative to the first orientation.
19. 20. The method of claim 18, wherein the second orientation is rotated 45 degrees relative to the first orientation.
20. The method of claim 18 , wherein the second direction is orthogonal to the first direction.
Citation Information
Patent Citations
Manufacture of semiconductor integrated circuit device
JP1990047821A
Mask for lithography and method for forming pattern using the same
JP1999015138A
Substrate for exposure, exposure method and aligner
JP2000082648A
Improvement of alignment target contrast in lithography double patterning method
JP2010226105A
Semiconductor device and manufacturing method of the same
JP2013157498A