Manufacturing method of carbon graphite products

The use of urea as a filler in a closed vessel with restricted air access addresses oxidation and simplifies the firing process, enhancing the quality and enabling mass production of carbon graphite products by creating a protective atmosphere.

JP2024541852AInactive Publication Date: 2024-11-13JOINT STOCK COMPANY ROSENERGOATOM +2
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2024522606
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-21
Filing Date
2021-12-08
Publication Date
2024-11-13
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing methods for manufacturing carbon graphite products face challenges such as oxidation and deformation during firing, especially for small-sized products, leading to cracking and fracture, and require complex hardware designs due to the use of inert or reducing atmospheres and high pressures, making mass production difficult.

Method used

A method involving the use of urea as a filler in a closed vessel with restricted air access, which decomposes to create a protective atmosphere of ammonia and carbon monoxide, preventing oxidation and simplifying the firing process by using conventional furnaces.

Benefits of technology

The method effectively prevents oxidation and coking of small carbon graphite products, improving their quality and enabling mass production without complex hardware, by using urea to create a protective atmosphere during firing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024541852000001
    Figure 2024541852000001
  • Figure 2024541852000002
    Figure 2024541852000002
  • Figure 2024541852000003
    Figure 2024541852000003
Patent Text Reader

Abstract

The present invention relates to a carbon product manufacturing, i.e., a calcination processing technology, which can be used in various technical fields for manufacturing electrodes, crucibles, heaters, and also for manufacturing materials for nuclear engineering, such as uranium graphite fuel elements. The method for manufacturing carbon graphite products includes the steps of placing a workpiece together with a filler in a container and calcining in an air atmosphere, in which urea is used as a filler in the container in an amount of 5-10 wt% of the workpiece, and the container is placed in a closed vessel with limited access to air, which is also filled with a carbon filler containing urea in an amount of 5-10 wt%. The problem of the present invention and the technical result achieved by using the present invention are to simplify the calcination process and to improve the quality of carbon graphite products, especially small products, by preventing oxidation and coking of the filler.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to the manufacture of carbon products, i.e. pyroprocessing technology, which can be used in various technical fields for the manufacture of electrodes, crucibles, heaters, as well as for the manufacture of materials for nuclear engineering, such as uranium graphite fuel elements. [Background technology]

[0002] The manufacturing process of carbon graphite products consists of several steps including sintering, which is a special step in the manufacturing of carbon graphite products.

[0003] The main process during the firing of a "green" workpiece is the formation of a cementing coke lattice from the binder, which involves the thermal destruction of the binder, the formation of semi-coke from it, and its subsequent transformation into coke.

[0004] Calcination determines the quality and performance characteristics of the carbon graphite product. The quality of the resulting carbon graphite product is highly dependent on the degree of oxidation during calcination.

[0005] Carbon graphite is known to be stable at relatively low temperatures (up to 400 °C) in oxidizing environments, but reacts relatively readily at higher temperatures. Depending on the environment, the temperature at which significant interactions with graphite begin can vary greatly.

[0006] For example, reactions with atmospheric oxygen begin at 400°C, and with carbon dioxide at 500°C (Levashova AI, Kravtsov AV Chemical Technology of Carbon Materials: Textbook. Tomsk: TPU Publishing House, 2008, p. 14).

[0007] Furthermore, during firing, the oxidized and non-oxidized portions of the carbon graphite workpiece will shrink to different amounts, inevitably leading to cracking and fracture.

[0008] Therefore, the firing temperature range of 400-600 ° C requires the most responsible approach to the selection of the gas environment.

[0009] To ensure the quality of the baking process, indirect heating through the wall is used, but in most cases this is insufficient.

[0010] This problem is solved by placing the carbon graphite workpieces in a packing material (filler), which partially prevents oxidation and deformation of the product, distributes the temperature field more uniformly throughout the heating chamber, reduces the temperature gradient, and influences the composition and pressure of the gas atmosphere in the furnace (Levashova AI, Kravtsov AV Chemical Technology of Carbon Materials: Textbook. Tomsk: TPU Publishing House, 2008, p. 72). Crushed metallurgical coke or a mixture of anthracite and river sand is used as the packing material.

[0011] A method for producing carbon graphite products is known in which the heat treatment is carried out in the phase transition region of the binder while periodically lowering the sintering temperature of the product (Russian Patent No. 2230380, IPC G21C 21 / 02 (2000.01), published on June 10, 2004).

[0012] Such firing requires heat treatment in an inert or reducing atmosphere, complicating the process hardware design.

[0013] Furthermore, a method for producing carbon graphite products is known, in which the product is sintered in a container by the pressure of released volatile gases (USSR Patent No. 865789, IPC C01B 31 / 04 (2000.01), published 23 September 1981).

[0014] The disadvantage of this method is that when the workpiece is pressed into the container and heat-treated, the release pressure of volatile gases reaches several tens of atmospheres. In addition, it is necessary to make dedicated containers individually, which makes it difficult to use for mass production of products.

[0015] The method for producing carbon graphite products that comes closest in terms of technical description and problem to be solved involves placing a workpiece of carbon graphite in a container with a carbon filler between the workpiece and the wall of the container, and then sintering the workpiece in a closed vessel under pressure such that volatile materials are released, thereby graphitizing the workpiece (GB Patent No. 759160, IPC C04B 35 / 532, published 17 October 1956).

[0016] This method is very effective for obtaining large products when the amount of air contained in the charge is not sufficient to cause significant oxidation on the surface of the workpiece being fired.

[0017] However, such firing of small workpieces in the presence of fillers leads to partial oxidation of the surface of the resulting product and coking of the fillers. Moreover, firing at high temperatures and pressures (tens of atmospheres) in a closed vessel complicates the hardware design of the process. [Prior art documents] [Patent documents]

[0018] [Patent Document 1] Russian Patent No. 2230380 [Patent Document 2] USSR Patent No. 865789 [Patent Document 3] British Patent No. 759160 Summary of the Invention [Problem to be solved by the invention]

[0019] The object of the present invention and the technical result achieved by using the present invention are to simplify the calcination process and to improve the quality of carbon graphite products, especially small products, by preventing oxidation of the products and coking of the fillers. [Means for solving the problem]

[0020] The above problem is solved by a method according to the present invention, namely a method for producing a carbon graphite product, comprising a step of placing a workpiece together with a filler in a container and sintering in an air atmosphere, characterized in that as the filler, urea is used in an amount of 5-10 wt % of the workpiece, the container is placed in a closed vessel with limited access to air, and the closed vessel is also filled with a carbon filler with urea in an amount of 5-10 wt %. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0021] In a specific embodiment of the present invention, graphlex or graphite is used as the material of the container for the workpiece, petroleum granular coke is used as the carbon filler, and the workpiece is heated to a temperature of 750 to 800°C and sintered.

[0022] To provide (create) a protective atmosphere during calcination, urea ((NH2)2CO) is added to the carbon charge and to the container containing the calcined sample.

[0023] When heated above 150°C, urea decomposes to produce ammonia and carbon dioxide. Carbon dioxide reacts with carbon at temperatures above 500°C to produce carbon monoxide:

[0024] С+СO2=2СO The carbon monoxide and ammonia produced act as a protective atmosphere to prevent oxidation of the calcined sample.

[0025] The proposed method for sintering carbon graphite workpieces was tested on "green" workpieces obtained by pressing a mixture of graphite powder and phenol formaldehyde resin. (Implementation of the method) Workpieces with dimensions of approximately 12.8 mm × 55 mm (d × l), made from a mixture of MPG-6 graphite powder (5–100 μm) and artificial graphite powder with particle size less than 100 μm and binder of SFP 011A phenol-formaldehyde resin in the amount of 18 wt%, were pressed at temperatures of 70–130 °C and pressures of 8–10 MPa.

[0026] According to the above technical solution, the pressed "green" workpiece was placed in a cylindrical container containing urea filler in an amount of 5-10 wt.% of the workpiece. The container was made of GMZ graphite and Graflex.

[0027] The container with the workpiece and urea charge was placed in a heat-resistant steel vessel with a lid restricting access to air, and in the vessel was covered with a carbon charge containing urea in an amount of 5–10 wt %.

[0028] Calcination was carried out in a standard calcination muffle furnace of the SNOL 6 / 10 type at a heating rate of 30-50°C / h until a temperature of 750°C was reached. Test sample No. 1 (see table) was calcined without the addition of urea.

[0029] The firing results of the carbon graphite product samples are shown in Table 1.

[0030] [Table 1]

[0031] The firing results in the table show that the mass of the samples was reduced by 6.9 to 10.2%. This mass reduction is mainly due to the thermal decomposition of the binder phenol formaldehyde resin SFP 011A, and less due to the partial oxidation of carbon.

[0032] Since the mass loss due to the thermal decomposition of the binder was almost the same for all samples, the degree of oxidation of the sample can be judged by the total mass loss of the fired sample (mass loss due to the thermal decomposition of the binder and loss due to the oxidation of carbon).

[0033] As can be seen from the test data described, the samples with the smallest mass loss were samples No. 3 to No. 5, which were fired with 5 to 10 wt% urea added to the container containing the fired sample and the carbon filler filled in the container, respectively. These samples showed no significant oxidation after firing and had a smooth and shiny surface.

[0034] The test data show that even if the urea content in the filling material for containers and vessels exceeds the upper limit of the above range, there is no noticeable change in the mass loss of the product (sample), but if it falls below the lower limit, the mass loss of the sample increases and, accordingly, the surface oxidation of the fired sample becomes noticeable.

[0035] The proposed method allows the heat treatment to be carried out in a conventional calcination muffle furnace without the use of inert or reducing gases and without the use of a complex assembly system for sealing the container with the calcined sample, thus significantly simplifying the production of carbon graphite products and improving their quality by preventing the oxidation of the product surface and the coking of the filler on the surface.

[0036] The proposed method for producing carbon-graphite workpieces is applicable for sintering "green" workpieces obtained by powder metallurgy and by impregnating graphite and other porous ceramic materials with various metal salt solutions.

[0037] The proposed method is particularly useful for the production of small products, which have strict requirements regarding the possibility of oxidation, the presence or absence of cracks, and the surface condition of the product.

Claims

1. 1. A method for producing a carbon graphite product, comprising: The workpiece is placed in a container together with a filler material and fired in an air atmosphere; As the filler, urea is used in an amount of 5 to 10 wt % of the workpiece; The container is disposed within an enclosed enclosure with limited access to air; The container is also filled with a carbon filler containing urea in an amount of 5-10 wt %. A method comprising:

2. The container for containing the workpiece is made of graphite or graphite.

2. The method of claim 1 .

3. Petroleum granular coke is used as the carbon filler.

2. The method of claim 1 .

4. The workpiece is heated and sintered at a temperature of 750 to 800° C.

2. The method of claim 1 .

Citation Information

Patent Citations

  • Carbonaceous brick for blast furnace excellent in alkali resistance and its production

    JP1996143361A

  • Production of carbon-containing refractory

    JP1996259309A

  • Method of producing carbide sintered compact and carbide sintered compact

    JP2003201178A

  • Firing device

    WO2015029306A1

  • Improvements in or relating to production of carbon masses

    GB759160A