Compressed Natural Gas Combustion and Exhaust Systems
A dual-coated catalyst system with palladium-containing alumina and zeolite coatings addresses sulfur and thermal aging in natural gas engines by regenerating the first coating in a rich mode, ensuring efficient methane oxidation without temperature increase.
Patent Information
- Application Number
- JP2024529450
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-20
- Filing Date
- 2022-12-19
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2042-12-19
AI Technical Summary
Natural gas engines face challenges with catalyst deactivation due to sulfur, water, and thermal aging, which affect methane emissions and increase operational costs, especially in lean-burn conditions.
A dual-coated catalyst system with a palladium-containing alumina first coating for sulfur capture and a palladium-containing zeolite second coating, operating in lean and rich modes to regenerate the first coating, reducing sulfur deactivation without temperature increase.
The system effectively maintains catalyst performance by intermittently releasing sulfur from the first coating, reducing deactivation and maintaining high methane oxidation performance, while avoiding costly high-temperature regeneration.
Smart Images

Figure 2024542464000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to compressed natural gas combustion and exhaust systems, and more particularly to systems having improved sulfur tolerance. [Background technology]
[0002] Natural gas is of increasing interest as an alternative fuel for vehicles and stationary engines that traditionally use gasoline and diesel fuels. Natural gas is composed primarily of methane (typically 70-90%) with varying percentages of other hydrocarbons such as ethane, propane and butane (up to 20% in some deposits) and other gases. It can be produced commercially from oil or natural gas fields and is widely used as a combustion energy source for electricity generation, industrial cogeneration and home heating. It can also be used as a vehicle fuel.
[0003] Natural gas can be used as a transportation fuel in the form of compressed natural gas (CNG) and liquefied natural gas (LNG). CNG is carried in tanks pressurized to 3600 psi (about 248 bar) and has an energy density of about 35% of that of gasoline per unit volume. LNG has 2.5 times the energy density of CNG and is used mainly in heavy vehicles. LNG is cooled to liquid form at -162°C, resulting in a 600-fold reduction in volume, which means that LNG is easier to transport than CNG. Bio-LNG is a potential alternative to natural (fossil) gas and is produced from biogas, obtained by anaerobic digestion from organic matter such as landfill waste or manure.
[0004] Natural gas has many environmental advantages: it is a cleaner burning fuel that typically contains fewer impurities, has a higher energy per carbon (Bti) than traditional hydrocarbon fuels, resulting in lower carbon dioxide emissions (25% lower greenhouse gas emissions), and has lower PM and NO emissions compared to diesel and gasoline. xBiogas can reduce these emissions even further.
[0005] Further driving the adoption of natural gas includes its high abundance and lower cost compared to other fossil fuels.
[0006] Natural gas engines have significantly lower PM and NO emissions compared to large and small diesel engines. x NG engines emit less than 95% and 70%, respectively. However, the exhaust gases produced by NG engines often contain significant amounts of methane (so-called "methane slip"). Regulations limiting emissions from these engines currently include Euro VI and the US Environmental Protection Agency (EPA) Greenhouse Gas Act. These impose emission limits for methane, nitrogen oxide (NOx), and particulate matter (PM).
[0007] The two main operating modes used for methane-fueled engines are stoichiometric (λ=1) and lean-burn (λ≧1.3) conditions. Palladium-based catalysts are known as the most active type of catalyst for methane oxidation under both conditions. Regulated emission limits for both stoichiometric and lean-burn compressed natural gas engines can be met by applying either a palladium-rhodium three-way catalyst (TWC) or a platinum-palladium oxidation catalyst, respectively.
[0008] The development of this Pd-based catalyst technology depends on overcoming challenges related to cost and catalyst deactivation due to sulfur, water and heat aging.
[0009] Methane is the least reactive hydrocarbon, and high energy is required to break the primary C-H bond. The ignition temperature of alkanes generally decreases with increasing fuel-air ratio and with increasing hydrocarbon chain length, which correlates with C-H bond strength. It is known that Pd-based catalysts have a higher light-off temperature for methane conversion than other hydrocarbons ("light-off temperature" means the temperature at which the conversion rate reaches 50%).
[0010] When operated under stoichiometric conditions (λ=1), the TWC can be used as an effective and cost-effective aftertreatment system for combusting methane. -3 Most bimetallic Pd-Rh catalysts with high total platinum group metal (pgm) loadings exceeding 10 ...
[0011] NO x The reduction of NO and oxidation of methane are also more difficult under highly oxidizing conditions. In lean-burn CNG applications, Pd-Pt with high total pgm loadings (>200 gft-3) are required for methane combustion at lower temperatures. Unlike stoichiometric engines, NO is reduced in the presence of excess oxygen. x A reductant must also be injected into the exhaust stream so that NO can be reduced. This is usually in the form of ammonia (NH3), and thus lean-burn applications require a completely different catalytic system than the stoichiometric one, where efficient NO xReduction can be accomplished using CO or HC at slightly rich or stoichiometric conditions.
[0012] Methane emissions may increase during cold start and idle conditions due to non-reactivity (or insufficient reactivity) of methane at lower temperatures. To improve methane reactivity at lower temperatures, one option is to use higher pgm loadings, but this increases costs.
[0013] Natural gas catalysts, especially Pd-based catalysts, can suffer from poisoning by water (5-12%) and sulfur (<0.5 ppm SO2 in lubricating oil), especially under lean conditions, which results in a dramatic decrease in catalyst conversion over time. Water deactivation is significant due to the formation of hydroxyls, carbonates, formates and other intermediates on the catalyst surface. Activity is reversible and can be fully restored when the water is removed. However, this is impractical since methane combustion feeds always contain high levels of water due to the high content of H in methane.
[0014] H2O can be either an inhibitor or promoter, depending on the air-fuel ratio, i.e., λ. Under stoichiometric and reducing conditions (λ>1), H2O can act as a promoter for the oxidation of hydrocarbons through the steam reforming reaction in both CNG and gasoline engines. However, in lean-burn CNG operating at λ>1, H2O acts as an inhibitor of methane oxidation. It is important to understand the water inhibition effect and design catalysts that are more tolerant to the presence of H2O. This will allow improvements when trying to control methane emissions from lean-burn CNG.
[0015] Although sulfur levels in engine exhaust are very low, Pd-based catalysts are severely deactivated upon sulfur exposure due to the formation of stable sulfates. Regeneration of the catalyst to restore activity after sulfur poisoning is difficult and usually requires high temperatures, rich operation, or both. This is easily achievable under stoichiometric operation, but is more difficult under lean combustion. Lean-burning vehicles operate at much higher air-fuel ratios than stoichiometric vehicles and require injection of much higher concentrations of reductant to switch to rich operation. Thermal deactivation resulting from poor engine transient control and high levels of misfire events due to ignition systems destroys the catalyst and results in correspondingly high levels of exhaust emissions.
[0016] Palladium-containing catalysts deactivate under both lean and stoichiometric conditions, but sulfur poisoning has a more dramatic effect than heat aging in lean operation. Sulfur poisoning can be ameliorated by adding small amounts of Pt to the Pd catalyst. This is because sulfur inhibition due to the formation of palladium sulfate can be significantly reduced by the addition of Pt. However, the addition of Pt further increases costs.
[0017] It is therefore desirable to provide an improved system for natural gas combustion and exhaust gas treatment to reduce methane emissions by addressing catalyst deactivation due to sulfur, water, thermal aging, etc., without increasing the cost of the catalyst. It is an object of the present invention to address this problem and address the shortcomings associated with the prior art, or at least provide a commercially useful alternative thereto. Summary of the Invention
[0018] According to a first aspect, there is provided a compressed natural gas combustion and exhaust system, comprising: (i) a natural gas burning engine; (ii) an exhaust treatment system, the exhaust treatment system comprising an intake for receiving exhaust gases from the combustion engine, and a catalytic article disposed to receive and treat the exhaust gases, the catalytic article comprising: a substrate having at least a first and a second coating, the first coating comprising a palladium-containing alumina and / or a base metal-containing alumina and the second coating comprising a palladium-containing zeolite; The first coating is disposed in contact with the exhaust gas before the second coating, and the system comprises: (a) a lean first mode in which sulfur is captured on the first coating; (b) a second mode in which sulfur is richly emitted from the first coating.
[0019] In the following passages, different aspects / embodiments are defined in more detail. Each aspect / embodiment so defined can be combined with any other aspect / embodiment or aspects / embodiments, unless expressly indicated otherwise. In particular, any feature indicated as being preferred or advantageous can be combined with any other feature or features indicated as being preferred or advantageous.
[0020] The present invention relates to compressed natural gas combustion and exhaust systems.
[0021] A natural gas combustion engine is an engine used to combust natural gas. The natural gas combustion engine may be a mobile engine, generally meaning suitable for use in an automobile or other vehicle (e.g., off-road vehicle), where such systems may have changes in fuel supply and demand during operation depending on operator requirements such as acceleration. In mobile applications, the natural gas combustion may be configured to operate in a lean or stoichiometric configuration. In mobile applications, it is generally possible to operate the system temporarily in a rich mode. It is understood that although the engine is described as being "mobile", it may be used across a variety of different applications.
[0022] The exhaust treatment system is a system suitable for treating exhaust gases from a combustion engine. The exhaust treatment system comprises an inlet for receiving exhaust gases from the combustion engine and a catalytic article arranged to receive and treat the exhaust gases. The inlet may be a conduit or pipe configured to direct exhaust from the combustion engine to the catalytic article.
[0023] Catalytic articles are components suitable for use in exhaust gas systems. Typically, such articles are honeycomb monoliths, sometimes referred to as "bricks". They have a high surface area configuration suitable for contacting the gas to be treated with the catalytic material to effect conversion or transformation of the exhaust gas components. Other forms of catalytic articles are also known, including plate configurations, as well as wrapped metal catalytic substrates. The catalytic articles described herein are suitable for use in all of these known forms, but are particularly preferred in the form of honeycomb monoliths, as they offer a good balance between cost and simplicity of manufacture.
[0024] The catalytic article is for the treatment of exhaust from a natural gas combustion engine, i.e., the catalytic article is for catalytic treatment of exhaust gas from a natural gas combustion engine, converting or transforming components of the gas before it is released to the atmosphere to meet emission regulations. When natural gas is combusted, it produces both carbon dioxide and water, but the exhaust gas also contains amounts of additional methane (and other short chain hydrocarbons) that need to be catalytically removed before the exhaust is released to the atmosphere. The exhaust gas also typically contains significant amounts of water and sulfur that can accumulate and deactivate the catalyst.
[0025] The catalytic article comprises a substrate having at least a first and a second coating. Preferably, the first coating is provided as a washcoat on the substrate and / or the second coating is provided as a washcoat on the substrate. Preferably, both coatings are provided as washcoats on the substrate. Preferably, the substrate is a flow-through monolith.
[0026] The first coating comprises a palladium-containing alumina and / or a base metal-containing alumina. The first coating is effective to absorb or capture sulfur present in the exhaust gas received from the CNG engine under lean conditions (λ>1) and can be regenerated (i.e., sulfur is released therefrom) for a short period of time under rich conditions (λ<1). Advantageously, the release of sulfur from the first coating, and thus the regeneration of the first coating, can be chemically induced by reducing the oxygen concentration of the exhaust gas received by the catalytic article, and optionally also by injecting a hydrocarbon into the exhaust gas received by the catalytic article, as discussed with respect to the data shown in FIG. 2 of the present application. In other words, the rich condition of the rich second mode can be achieved by reducing the oxygen concentration of the exhaust gas received by the catalytic article, and optionally also by injecting a fuel or a hydrocarbon into the exhaust gas received by the catalytic article.
[0027] The alumina may be any type of alumina, such as alpha or gamma alumina. Additionally, the alumina may be doped as known in the art. For example, doping with Si or La in an amount of up to 15 wt%, such as 1-10 wt%, preferably about 5 wt%, can provide improved thermal stability. Preferably, the alumina in the first coating is gamma alumina. Preferably, the first coating has a thickness of 1-50 g / ft 3 , more preferably 5 to 40 g / ft 3 , and most preferably 10 to 30 g / ft 3 The washcoat loading is
[0028] The second coating includes a palladium-containing zeolite. Such palladium-containing zeolite exhibits excellent activity for treating exhaust gas from a CNG engine, despite the presence of water in the exhaust gas, but is susceptible to sulfur inhibition. Such palladium-containing catalysts have high stability when exposed to rich conditions during the rich second mode, and can withstand periodic exposure to high concentrations of sulfur, such as during the rich second mode. As shown by the data in FIG. 1 of the present application and described later herein, the presence of SO2 in the exhaust gas during the rich second mode temporarily reduces the activity of the palladium-containing zeolite. However, since the palladium-containing zeolite does not significantly store SO2 when exposed to SO2 for the short period of time that the system operates in the lean second mode, the activity of the palladium-containing zeolite is substantially restored when the lean first mode resumes. In other words, the palladium-containing zeolite is not destabilized by sulfur released from the first coating during intermittent operation of the system in the rich second mode. This is in contrast to other palladium-containing catalysts, such as palladium supported on alumina, as illustrated by the data in FIG. 1, which is discussed in more detail below.
[0029] Preferably, the zeolite has an SAR of ≧1200, preferably ≧1300, such as ≧1500 (e.g. ≧1700), more preferably ≧2000, such as ≧2200. Preferably, the second coating has an SAR of 1 to 50 g / ft 3 , more preferably 5 to 40 g / ft 3 , and most preferably 10 to 30 g / ft 3 The washcoat loading is
[0030] The first coating is positioned to contact the exhaust gas before the second coating, which allows the first coating to capture sulfur in the exhaust gas such that the exhaust gas received by the second coating during the first lean mode has a reduced sulfur content, thereby reducing deactivation of the palladium-containing zeolite of the second coating by sulfur during the first lean mode.
[0031] Preferably, the first coating is upstream of the second coating in a zoned configuration, which allows the first coating to contact the exhaust gases before the second coating.
[0032] Preferably, the substrate has an inlet end and an outlet end, and optionally, the first coating extends from the inlet end and the second coating extends from the outlet end, which allows the first coating to contact the exhaust gases before the second coating.
[0033] Preferably, the first coating extends over 20-80%, preferably 60-80%, of the axial length of the substrate, and / or the second coating extends over 20-80%, preferably 20-40%, of the axial length of the substrate, and / or the first and second coatings together substantially cover the substrate.
[0034] Preferably, the first coating and the second zone overlap by at least 10% of the axial length of the substrate. Preferably, the first coating and the second zone overlap by up to 25% of the axial length of the substrate.
[0035] Alternatively, the first coating may be disposed over the second coating in a layered configuration, allowing the first coating to contact the exhaust gases before the second coating.
[0036] The system is configured to selectively operate in (a) a lean first mode in which sulfur is captured on the first coating, and (b) a rich second mode in which sulfur is released from the first coating, During the lean first mode, the system operates under lean burn conditions, i.e., (λ>1), and During the rich second mode, the system operates under rich burn conditions, i.e., λ<1.
[0037] During the lean first mode, the first coating captures sulfur present in the exhaust gas such that the exhaust gas received by the second coating has a reduced sulfur content. This reduces the deactivation / poisoning of the palladium-containing zeolite catalyst present in the second coating, thereby maintaining its high oxidation performance during operation of the system in the lean first mode. To regenerate the catalyst, particularly the first coating of the catalyst, the system is periodically / intermittently operated in a rich second mode in which sulfur is released from the first coating.
[0038] During the rich second mode, the oxygen concentration in the exhaust gas received by the catalytic article can be reduced by injecting an inert gas, such as argon, for example. The system can include an injector upstream of the catalytic article configured to inject an inert gas, such as argon, into the exhaust gas during operation of the system in the rich second mode.
[0039] During the rich second mode, the concentration of hydrocarbons in the exhaust gas received by the catalytic article may be increased by injection of one or more hydrocarbons into the exhaust gas. For example, the system may include an injector upstream of the catalytic article configured to inject one or more hydrocarbons, such as propylene, into the exhaust gas during operation of the system in the rich second mode.
[0040] By reducing the oxygen concentration in the exhaust gas and optionally also increasing the hydrocarbon content, a rich condition can be achieved that releases sulfur from the first coating, thereby regenerating the first coating. In other words, operation of the system in the rich second mode can be achieved by reducing the concentration of oxygen in the exhaust gas received by the catalytic article, and optionally also by injection of one or more hydrocarbons. Advantageously, such chemically induced sulfur release does not require an increase in the temperature of the exhaust gas. In other words, the temperature of the exhaust gas can be maintained substantially the same between the lean first mode and the rich second mode. In contrast, typical techniques for the regeneration of known sulfur trap devices involve thermal release of stored sulfur, which requires a substantial temperature increase (i.e., several hundred degrees Celsius higher) from its operating temperature. This can be extremely difficult to apply due to the increased engine control required, the possibility of thermal deactivation of the catalytic article, and the possibility of thermal degradation of engine components such as the turbocharger.
[0041] As noted above, the temperature of the exhaust gases may remain substantially the same during the lean first mode and the rich second mode. For example, the temperature of the exhaust gases during the lean first mode may be within 20°C, preferably within 10°C, and more preferably within 5°C of the temperature of the exhaust gases during the second rich mode. The temperature of the exhaust gases during the lean first mode and the rich second mode may be less than 750°C, preferably less than 650°C, and most preferably between 500 and 600°C.
[0042] In an alternative, but less preferred, arrangement, the temperature of the exhaust gases may be increased during the rich second mode. During the first lean mode, the temperature of the exhaust gases may be less than 750° C. Preferably, during the rich second mode, the temperature of the exhaust gases does not exceed 850° C.
[0043] Preferably, during one cycle, the system is configured to operate in the second rich mode for less than 5 minutes, preferably less than 3 minutes, more preferably 1 minute or less, and to operate in the first lean mode for more than 10 minutes, preferably more than 30 minutes, preferably 60 minutes or more. In other words, the system may intermittently switch to operating in the second rich mode. By operating intermittently in the second rich mode, the first coating acting as a sulfur trap can be regenerated without destabilizing the performance of the palladium-containing zeolite of the second coating. In other words, the downstream second coating can withstand the rich conditions and high concentrations of sulfur experienced during the second rich mode during these short periods. Because the system allows for effective regeneration of the first coating over such short periods, the time between regeneration intervals (i.e., the time the system operates in the first lean mode) can be increased.
[0044] Preferably, the system further includes a sulfur trap downstream of the catalyst article to receive sulfur released from the first coating during the rich second mode. The sulfur trap can capture sulfur released from the first coating during the rich second mode, thereby reducing sulfur emissions from the system.
[0045] Optionally, the system includes a SO2 sensor downstream of the second coating, and a controller configured to switch the system to operate in a rich second mode when the sensor detects an exhaust stream SO2 level above a threshold. This is advantageous because by measuring the SO2 level in the exhaust gas downstream of the second coating, the SO2 sensor can monitor the SO2 absorption by the first coating and determine whether the first coating needs to be regenerated. For example, if the SO2 level in the exhaust gas increases significantly, this demonstrates that the sulfur in the exhaust gas is not being sufficiently captured / absorbed by the first coating, and as a result, the first coating needs to be regenerated by operating the system in a rich second mode. The SO2 sensor may be positioned downstream of the catalyst article.
[0046] According to a further aspect of the present invention, there is provided a method for treating exhaust gas from a natural gas burning engine, the method comprising: contacting the exhaust gas with a catalytic article of an exhaust treatment system; The catalytic article comprises: a substrate having at least a first and a second coating, the first coating comprising a palladium-containing alumina and / or a base metal-containing alumina and the second coating comprising a palladium-containing zeolite; a first coating is disposed in contact with the exhaust gas prior to the second coating; The method further includes operating the exhaust system in a lean first mode in which sulfur is trapped on the first coating, and intermittently operating the exhaust system in a rich second mode in which sulfur is released from the first coating.
[0047] Preferably, the method described in this aspect may be applied to the system described herein, and therefore all features described as being preferred for the system apply equally to the method aspect. [Brief description of the drawings]
[0048] The invention is further described with respect to the following non-limiting figures. [Figure 1] The top graph in FIG. 1 shows the methane conversion performance of the catalysts of Example 1 and Example 2 under simulated steady-state reactor conditions at 550° C., where a pulse of 50 ppm SO2 having a duration of 1 minute was introduced into the synthesis gas mixture flowing through the catalyst every hour. The middle graph in FIG. 1 shows the SO2 slip from the catalyst of Example 2, which is a palladium-containing zeolite, under simulated steady-state reactor conditions at 550° C., where a pulse of 50 ppm SO2 having a duration of 1 minute was introduced into the synthesis gas mixture flowing through the catalyst every hour. The bottom graph in FIG. 1 shows the SO2 slip from the catalyst of Example 1, which is palladium supported on alumina, under simulated steady-state reactor conditions at 550° C., where a pulse of 50 ppm SO2 having a duration of 1 minute was introduced into the synthesis gas mixture flowing through the catalyst every hour. [Diagram 2] 1 is a graph showing the release of stored sulfur from the catalyst of Example 2, palladium supported on alumina, upon reduction in oxygen concentration and injection of polypropylene into the syngas mixture flowing past the catalyst. [Diagram 3] 1 shows the methane and ethane conversion performance of the catalysts of Examples 1 and 2 under simulated steady-state reactor conditions at 550°C, where rich pulses having a duration of 1 minute occurred for durations of 1 minute at 4.5, 10.5 and 16.5 hours. The supply of NO gas to the syngas mixture was turned off at 7.5 hours and turned on again at 14 hours such that there was no NO in the syngas mixture from 7.5 to 14 hours. The top graph shows the methane and ethane conversion for the catalyst of Example 2, which is palladium supported on alumina, and the bottom graph shows the methane and ethane conversion for the catalyst of Example 1, which is a palladium-containing zeolite. EXAMPLES
[0049] The invention will now be further described with reference to the following non-limiting examples.
[0050] Example 1 The catalyst of Example 1 is a catalyst having a palladium-containing high siliceous (SAR>1500) zeolite having a palladium content of 2 to 3 wt %.
[0051] The catalyst of Example 1 was prepared by impregnating a powder sample of siliceous zeolite (SAR>1500) with a solution of palladium nitrate by conventional incipient wetness technique. After impregnation, the sample was dried at 80° C. for 5 hours and calcined in a static oven at 500° C. in air for 2 hours.
[0052] A washcoat containing preformed Pd-containing siliceous zeolite, alumina binder and silica binder was applied to a ceramic substrate, and then the washcoat was pulled down onto the substrate using a vacuum. The article was dried and calcined at about 500° C. for about 1 hour. The loading of Pd on the article was 120 g / ft 3 It was.
[0053] Example 2 The catalyst of Example 2 is a palladium supported on alumina catalyst, and has a palladium content of 3 wt %.
[0054] A washcoat containing palladium nitrate, gamma-alumina, an alumina binder, and citric acid was applied to a ceramic substrate and then the washcoat was pulled down onto the substrate using a vacuum. The article was dried and calcined at about 500°C for about 1 hour. The loading of Pd on the article was 120g / ft 3 It was.
[0055] The sulfur tolerance of the catalysts of Example 1 and Example 2 was tested by measuring their methane conversion under simulated steady-state reactor conditions at 550° C., where a pulse of 50 ppm SO2 having a duration of 1 minute was introduced hourly into the synthesis gas mixture flowing through the catalyst. The synthesis gas mixture was heated to a space velocity of 100,000 h -1The composition was 1000 ppm CH4, 25 ppm C2H6, 5 ppm C3H8, 1000 ppm CO, 500 ppm NO, 12% O2, 8% H2O, 7.2% CO2, balance N2. Data from the sulfur tolerance is shown in the top graph of Figure 1.
[0056] This test simulated the increase in sulfur that occurs during cyclic operation of the system of the present invention in the rich second mode due to sulfur release from the first coating, with the rich second mode being operated for 1 minute and the lean first mode being operated for 59 minutes in each cycle.
[0057] The catalyst of Example 1 has the same composition as the second coating of the invention (palladium-containing zeolite). Thus, this test compares the sulfur resistance of the second coating of the invention during cyclic operation of the system in the rich second mode (1 minute per cycle) with Example 2, which instead contains palladium supported on alumina.
[0058] In FIG. 1, the methane conversion performance of the catalyst of Example 1, which is a palladium-containing zeolite, is shown by a series of peaks that are all between 90 and 100%. The methane conversion performance of the catalyst of Example 2, which is palladium supported on alumina, is shown by a series of peaks that continuously decrease to less than 80%. As shown in FIG. 1, for the catalyst of Example 1, a sharp drop in performance occurred during each SO2 pulse due to the deactivation of the palladium-containing zeolite by sulfur in the exhaust gas, but the performance drop was quickly recovered upon removal of sulfur from the gas stream, and the performance stabilized at above 95% methane conversion after multiple cycles. In contrast, for the catalyst of Example 2 (palladium supported on alumina), the performance of the catalyst continuously decreased with each SO2 pulse and did not stabilize after multiple cycles. The contrasting behavior in performance recovery can be explained by monitoring the SO2 slip from the catalysts of Example 1 and Example 2 during the sulfur tolerance test, which is shown in the middle and bottom graphs of FIG. 1. As shown in the middle graph of Figure 1, palladium supported on alumina stored a significant amount of SO2 during the SO2 pulse. In contrast, as shown in the bottom graph of Figure 1, SO2 passes through the palladium-containing zeolite of Example 1 during the SO2 pulse, as evidenced by the greater SO2 slip. The palladium-containing zeolite of Example 1 does not store sulfur significantly during the SO2 pulse and is therefore not deactivated by sulfur over these short periods of high sulfur concentration.
[0059] 2 is a graph showing the chemically induced release of stored sulfur from the catalyst of Example 2 (palladium supported on alumina), which has the same composition as the first coating of the catalyst of the present invention. The catalyst of Example 2, which has 0.5 ppm SO2 and a composition of 1000 ppm CH4, 25 ppm C2H6, 5 ppm C3H8, 1000 ppm CO, 500 ppm NO, 12% O2, 8% H2O, 7.2% CO2, balance N2, was subjected to a space velocity of 100,000 h -1A synthesis gas mixture was run at a temperature of 550°C. The oxygen concentration of the gas mixture was reduced by periodically injecting propylene into the gas mixture in 1 min / h cycles. In other words, in each cycle, a lean gas mixture was fed to the catalyst for 59 min and a rich gas mixture was fed to the catalyst for 1 min.
[0060] Figure 2 shows that palladium supported on alumina effectively absorbs sulfur during lean operation and releases sulfur during periodic rich pulses. The concentration of sulfur released during each rich pulse increased with time (i.e., a greater amount of sulfur was released during the 15.5 hour rich pulse than during the 9.5 hour rich pulse). This is expected because the longer exposure of palladium supported on alumina to the gas mixture caused more sulfur to be absorbed thereon, which could then be released during the rich pulse.
[0061] Figure 2 demonstrates that periodic rich pulses can be created by simultaneously decreasing the oxygen concentration of the gas received by the catalyst and increasing the hydrocarbon concentration. In other words, Figure 2 demonstrates that the release of SO2 from palladium on alumina can be chemically induced, and thus the temperature of the exhaust gas can be maintained at 550°C during regeneration of the palladium on alumina.
[0062] Thus, FIG. 2 demonstrates that the composition of the first coating of the present invention, palladium supported on alumina, can absorb sulfur during lean operation without a substantial temperature increase, but instead can be regenerated by chemical induction. In other words, the data in FIG. 2 demonstrates that lowering the oxygen concentration and increasing the hydrocarbon concentration of the exhaust gas received by the catalyst during operation of the system of the present invention in a rich second mode releases sulfur from the first coating without the need to increase the temperature of the exhaust gas. This is advantageous because thermal release of stored sulfur typically requires a substantial temperature increase (i.e., several hundred degrees Celsius higher) from its operating temperature, which can be extremely difficult to apply in terms of engine control, potential thermal deactivation of the catalyst, and potential thermal degradation of components such as the turbocharger.
[0063] The effect of rich pulses on the catalysts of Example 1 and Example 2 was examined by measuring their methane and ethane conversions under simulated steady-state reactor conditions at 550 °C when a syngas mixture was flowed through the catalyst. The syngas mixture was heated to a space velocity of 100,000 h -1 The mixture contained 1000 ppm CH4, 25 ppm C2H6, 5 ppm C3H8, 1000 ppm CO, 500 ppm NO, 12% O2, 8% H2O, 7.2% CO2, and the balance N2. Rich pulses, in which the oxygen concentration in the synthesis mixture was reduced via injection of propylene, occurred for 1 minute at 4.5, 10.5, and 16.5 hours. The supply of NO gas to the synthesis gas mixture was turned off at 7.5 hours and turned back on at 14 hours, ensuring that no NO was present in the synthesis gas mixture from 7.5 to 14 hours. Data from this test are shown in Figure 3.
[0064] In FIG. 3, the ethane conversion for both Example 1 and Example 2 remains at 90-100%. The methane conversion for the catalyst of Example 1 (palladium-containing zeolite) starts at 100% and remains at 90-100% during lean operation, but shows a sharp decrease of about 20-25% during each rich pulse. The methane conversion for the catalyst of Example 2 (palladium-containing zeolite) shows a gradual decrease before and after each rich pulse. For both Example 1 and Example 2, the temperature of the exhaust gas at the inlet decreases from 700-710°C after 2 hours and then remains at about 560°C, and the temperature of the exhaust gas at the outlet decreases from 650°C after 2 hours and remains at about 570-580°C, and then increases sharply to about 610°C during the rich pulse.
[0065] As shown in FIG. 3, the conversion performed by the catalyst of Example 2, which is palladium supported on alumina, gradually decreases over time both before and after each rich pulse. This is expected to be due to water-induced catalyst deactivation. However, after the rich pulse, when NO was not present in the syngas mixture, the deactivation rate of the catalyst of Example 2 showed a sharp increase. This suggests that a significant change had occurred to the palladium of the catalyst and that the methane oxidation activity is dependent on the presence of NO in the feed. It was expected that the change to palladium of the catalyst of Example 2 was a reduction of PdO to metallic Pd, an assessment supported by visual observation of the color of the samples. In contrast, the graph in FIG. 3 demonstrates that the performance of the catalyst of Example 1, which is a palladium-containing zeolite, is extremely stable both before and after the rich pulse and is not affected by the presence of NO in the feed / removal of NO from the feed. Overall, these results suggest a much higher stability of the palladium-containing zeolite, regardless of the rich pulse, compared to palladium supported on alumina. It should be noted that this greater stability is particularly advantageous when such catalysts are used as the second coating of the present invention, since the system of the present invention can withstand rich conditions when operating in a rich second mode to regenerate the first catalytic coating.
[0066] As used herein, the singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise. Use of the term "comprising" is intended to be interpreted as including such features but not excluding other features, and is intended to include options of features that are necessarily limited to those recited. In other words, this term also includes the limitations "consisting essentially of" (intended to mean that certain additional components may be present provided they do not materially affect the essential properties of the recited feature) and "consisting of" (intended to mean that no other features may be included when the components are expressed as percentages by their proportions, such that they add up to 100%, taking into account any unavoidable impurities), unless the context clearly dictates otherwise.
[0067] Although terms such as "first", "second", and the like may be used herein to describe various elements, layers, and / or portions, it will be understood that the elements, layers, and / or portions should not be limited by these terms. These terms are used only to distinguish one element, layer, or portion from another or further element, layer, or portion. It will be understood that the term "on" is intended to mean "directly on", such that there is no intervening layer between one material that is said to be "on" another material. For ease of description to describe the relationship of one element or feature to another element or feature, spatially relative terms such as "under", "below", "beneath", "lower", "over", "above", "upper", and the like may be used herein. It will be understood that the spatially relative terms are intended to encompass different orientations of the device during use or operation in addition to the orientation depicted in the figures. For example, if a device described herein were inverted, elements described as being "below" or "below" other elements or features would then be oriented "above" or "above" the other elements or features. Thus, the exemplary term "below" can encompass both an orientation of above and below. The device may be otherwise oriented, and the spatially relative descriptors used herein would be interpreted accordingly.
[0068] The foregoing detailed description has been provided for purposes of explanation and illustration and is not intended to limit the scope of the appended claims. Many variations of the presently preferred embodiments described herein will be apparent to those of ordinary skill in the art and remain within the scope of the appended claims and their equivalents.
Claims
1. 1. A compressed natural gas combustion and exhaust system comprising: (i) a natural gas burning engine; (ii) an exhaust gas treatment system, the exhaust gas treatment system comprising an intake for receiving exhaust gases from the combustion engine, and a catalytic article positioned to receive and treat the exhaust gases, the catalytic article comprising: a substrate having at least a first and a second coating, the first coating comprising a palladium-containing alumina and / or a base metal-containing alumina and the second coating comprising a palladium-containing zeolite; the first coating is disposed to contact the exhaust gas prior to the second coating, and the system further comprises: (a) a lean first mode in which sulfur is trapped on the first coating; (b) a sulfur-rich second mode in which sulfur is released from said first coating.
2. The system of claim 1 , wherein during the rich second mode, the oxygen concentration in the exhaust gas received by the catalytic article is decreased.
3. 3. The system of claim 1 or 2, further comprising an injector upstream of the catalytic article, the injector configured to inject one or more hydrocarbons into the exhaust gas during operation of the system in the rich second mode.
4. A system according to any preceding claim, wherein the temperature of the exhaust gas remains substantially the same during the lean first mode and the rich second mode.
5. 2. The system of claim 1, wherein during the rich second mode, a temperature of the exhaust gas increases, and optionally, during the first lean mode, a temperature of the exhaust gas is less than 750°C, and during the rich second mode, a temperature of the exhaust gas increases to greater than 800°C.
6. The system of any one of claims 1 to 5, wherein the first coating is disposed upstream of the second coating in a zoned configuration.
7. 7. The system of claim 6, wherein the substrate comprises an inlet end and an outlet end, and optionally the first coating extends from the inlet end of the substrate and the second coating extends from the outlet end of the substrate.
8. 8. The system of claim 6 or 7, wherein the first coating extends over 20-80%, preferably 60-80%, of the axial length of the substrate, and / or the second coating extends over 20-80%, preferably 20-40%, of the axial length of the substrate, and / or the first and second coatings together substantially cover the substrate.
9. 9. The system of claim 6, 7, or 8, wherein the first coating and the second zone overlap by at least 10% of the axial length of the substrate.
10. The system of any one of claims 1 to 9, wherein the first coating is disposed on the second coating in a layered configuration.
11. The first coating is provided as a washcoat on the substrate and has a coating weight of 1 to 50 g / ft. 3 and / or the second coating is provided as a washcoat on the substrate and has a washcoat loading of 1 to 50 g / ft 3 The system of any one of claims 1 to 10, having a washcoat loading of
12. 12. The system of claim 1, further comprising a sulfur trap downstream of the catalytic article for receiving sulfur released from the first coating during the rich second mode.
13. SO downstream of the second coating 2 a sensor for detecting SO in the exhaust flow above a threshold value by said sensor; 2 A system according to any preceding claim, further comprising: a controller configured to switch the system to operate in the rich second mode when a level is detected.
14. The system of any one of claims 1 to 13, wherein the substrate is a flow-through substrate.
15. The system of any one of claims 1 to 14, wherein the zeolite has a SAR of at least 1500 and / or the alumina is gamma alumina.
16. 16. The system of any one of claims 1 to 15, wherein during one cycle, the system is configured to operate in the second rich mode for less than 5 minutes, preferably less than 3 minutes, more preferably 1 minute or less, and to operate in the first lean mode for more than 10 minutes, preferably more than 30 minutes, preferably 60 minutes or more.
17. 1. A method for treating exhaust gas from a natural gas burning engine, comprising: contacting the exhaust gas with a catalytic article of an emission treatment system; The catalyst article comprises: a substrate having at least a first and a second coating, the first coating comprising a palladium-containing alumina and / or a base metal-containing alumina and the second coating comprising a palladium-containing zeolite; the first coating is disposed in contact with the exhaust gas prior to the second coating; The method further includes operating the exhaust system in a lean first mode in which sulfur is trapped on the first coating, and intermittently operating the exhaust system in a rich second mode in which sulfur is released from the first coating.
Citation Information
Patent Citations
Exhaust gas post-treatment system for an internal combustion engine and method
DE102014226669A1
Exhaust emission controlling method
JP2003254117A
Oxidation catalysts for stoichiometric natural gas engines.
JP2019528160A
Exhaust gas purification catalyst
JP2020157262A
Catalyst material for methane purification
JP2021000588A