Cylindrical battery with reduced resistance
The jelly-roll electrode assembly with a novel tab structure for the first electrode and a tabless structure for the second electrode addresses high resistance and short circuit issues in cylindrical batteries, improving safety and performance.
Patent Information
- Application Number
- JP2024533087
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-01
- Filing Date
- 2022-11-30
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-11-30
AI Technical Summary
Conventional cylindrical batteries face issues with high resistance and heat generation due to concentrated current flow in strip-shaped electrode tabs, leading to potential fires, especially in large-capacity cells, and existing tab structures or tabless designs suffer from short circuits and reduced capacity.
A jelly-roll electrode assembly with a novel tab structure for the first electrode, featuring uncoated portions and multiple tabs positioned to minimize resistance and prevent short circuits, combined with a tabless structure for the second electrode to enhance space utilization and stability.
The solution effectively reduces resistance, minimizes short circuits, and improves space utilization in cylindrical batteries, enhancing their safety and performance without compromising capacity.
Smart Images

Figure 2024543226000001_ABST
Abstract
Description
[Technical field]
[0001] This application claims the benefit of priority based on Korean Patent Application No. 10-2021-0169768 dated December 1, 2021, and all contents disclosed in the documents of said Korean patent application are incorporated herein by reference.
[0002] The present invention relates to a cylindrical battery including a jelly roll type electrode assembly, and more particularly to a cylindrical battery structure in which the positive electrode and the negative electrode have different tab and tabless structures, respectively. [Background technology]
[0003] Secondary batteries, which have high applicability across a range of products and electrical properties such as high energy density, are widely used not only in portable devices but also in electric vehicles (EVs) and hybrid electric vehicles (HEVs) that are driven by electrical sources.
[0004] These secondary batteries not only have the primary advantage of dramatically reducing the use of fossil fuels, but also have the advantage of not producing any by-products from energy use, so they are attracting attention as a new energy source that is environmentally friendly and improves energy efficiency.
[0005] Currently, the types of secondary batteries that are widely used include lithium ion batteries, lithium polymer batteries, nickel cadmium batteries, nickel metal hydride batteries, and nickel zinc batteries. The operating voltage of these unit secondary battery cells, i.e., unit battery cells 100, is about 2.5V to 4.5V. Therefore, when a higher output voltage is required, a battery pack may be configured by connecting a plurality of battery cells in series. Also, a battery pack may be configured by connecting a number of battery cells 100 in parallel according to the charge / discharge capacity required for the battery pack. Therefore, the number and electrical connection form of the battery cells included in the battery pack may be variously set according to the required output voltage and / or charge / discharge capacity.
[0006] Meanwhile, cylindrical, square, and pouch-type battery cells are known as types of unit secondary battery cells. In the case of a cylindrical battery cell, a separator, which is an insulator, is interposed between a positive electrode and a negative electrode, and the separator is wound to form a jelly-roll-type electrode assembly, which is then inserted into a battery can to form a battery. A strip-shaped electrode tab may be connected to each uncoated portion of the positive electrode and the negative electrode, and the electrode tab electrically connects the electrode assembly to an electrode terminal exposed to the outside. For reference, the positive electrode terminal is a cap plate of a sealing body that seals an opening of the battery can, and the negative electrode terminal is the battery can. However, according to a conventional cylindrical battery cell having such a structure, current is concentrated in the strip-shaped electrode tab connected to the positive electrode uncoated portion and / or the negative electrode uncoated portion, which causes problems such as high resistance, large heat generation, and poor current collection efficiency.
[0007] Resistance and heat generation are not major issues for small cylindrical battery cells with the 18650 form factor. However, if the internal resistance of a large-capacity cylindrical battery cell is high, a large amount of heat may be generated around the electrode tabs during fast charging, causing the cylindrical battery cell to catch fire.
[0008] There have been various attempts to solve this problem. Representative examples include increasing the number of electrode tabs to multiple to widen the current path, and arranging the electrode tabs toward the center of the electrode from the position before winding to shorten the current path. These methods can reduce electrical resistance because electrical resistance is inversely proportional to the area of the path through which the current flows and proportional to its length.
[0009] 3 is a cross-sectional view of a cylindrical battery including a jelly-roll type electrode assembly having a tab structure. In both the positive electrode 2 and the negative electrode 4, the current is connected to the battery can lid 63 or the battery can 6 only through the positive electrode tab 23 or the negative electrode tab 43 provided at one or more places on each of the positive electrode 2 and the negative electrode 4. In this case, the area of the current path is narrow and the resistance is high.
[0010] 1 and 2 show the state of the positive electrode and the negative electrode constituting a jelly roll type electrode assembly having a tab structure before being wound. Referring to these drawings, the positive electrode 2 is shorter than the negative electrode 4, and two positive electrode tabs 23 are located in the middle of the positive electrode 2. In contrast, the negative electrode 4 is wound radially outwardly relative to the positive electrode 2, and is longer than the positive electrode 2, so that the negative electrode tabs 43 can only be located at both ends due to the manufacturing process. As a result, the resistance of the positive electrode 2 can be significantly reduced by a method of reducing the length of the current path, but in particular, another method of reducing the resistance of the negative electrode 4 is urgently needed.
[0011] Yet another method devised to reduce resistance is a jelly roll battery with a tabless structure that does not use electrode tabs. FIG. 4 is a cross-sectional view of a cylindrical battery including a jelly roll type electrode assembly with a tabless structure. Referring to this, a positive electrode uncoated portion 21 that is not coated with an active material protrudes from one axial side of a positive electrode 2, and a negative electrode uncoated portion 41 that is not coated with an active material protrudes from the other axial side of a negative electrode 4. Each uncoated portion 21, 41 is welded to a current collector plate 5 and functions as an electrode tab as a whole. This increases the area of the current path, and the resistance can be significantly reduced. Here, each uncoated portion 21, 41 can be bent in a radial direction to form a flat surface in order to improve the welding characteristics with the current collector plate 5.
[0012] However, in the above-mentioned tabless structure, there is a high possibility that a short circuit will occur between the negative electrode and the positive electrode during the process of welding the uncoated portions 21, 41 to the current collector plate 5 or during the process of bending the uncoated portions 21, 41 to improve welding characteristics. In addition, the tabless structure requires an additional insulating layer 65 to insulate the positive current collector plate from the battery can, and an additional axial length of the battery can is required by the thickness of the positive uncoated portion 21 and the current collector plate 5, which results in a problem of reduced battery capacity.
[0013] Meanwhile, the thickness of the part of the jelly roll type electrode assembly where the tab is connected is thicker than the part where the tab is not connected. As a result, the radius of the jelly roll where the tab is located in the circumferential direction of the electrode assembly wound into a jelly roll is larger than the radius of the jelly roll where the tab is not located. Due to this difference in radius, when the cell is repeatedly charged and discharged, the part where the tab is located receives more pressure in the radial direction than the other parts, and deterioration such as collapse of the hollow part of the core or detachment of the attached layer occurs more quickly. Summary of the Invention [Problem to be solved by the invention]
[0014] The present invention has been devised in light of the background of the prior art as described above, and aims to provide a jelly-roll type electrode assembly capable of reducing the resistance of the second electrode, in which there is a limit to how much resistance can be reduced by simply improving the tab structure of both electrodes, and a cylindrical battery structure including the same.
[0015] Meanwhile, an object of the present invention is to provide an economical electrode assembly that improves space utilization and increases capacity by simplifying the structure and manufacturing process as much as possible, and a cylindrical battery structure including the same.
[0016] Yet another technical object of the present invention is to provide an electrode assembly that can minimize the possibility of a short circuit occurring between a first electrode and a second electrode without introducing excessive insulation treatment, and a cylindrical battery structure including the same.
[0017] The present invention also provides an electrode assembly that can minimize the phenomenon of cell deterioration caused by the thickness of the tabs when using one or more tabs to reduce resistance, and a cylindrical battery structure including the same.
[0018] Another object of the present invention is to provide a battery pack including the improved cylindrical battery cell, and a vehicle including the battery pack.
[0019] The technical object of the present invention is not limited to the above-mentioned objects, and other objects and advantages of the present invention not mentioned above can be understood from the following description and can be more clearly understood from the embodiments of the present invention. In addition, it is easy to understand that the objects and advantages of the present invention can be realized by the means and combinations thereof set forth in the claims. [Means for solving the problem]
[0020] In order to achieve the above object, the present invention provides a jelly roll type electrode assembly in which an electrode stack including a first electrode, a second electrode, and a separator is wound up, and the first and second electrodes are alternately stacked in both radial directions with a separator interposed therebetween, wherein the first electrode is provided with a first electrode uncoated portion that is not coated with an active material, a first electrode tab electrically connected to the first electrode uncoated portion protrudes from one axial direction of the electrode assembly, and a second electrode uncoated portion that is not coated with an active material is provided at an end of the other axial direction of the second electrode to serve as a tab.
[0021] The first electrode uncoated portion may be provided in a region corresponding to a region coated with an active material in the axial direction.
[0022] The first electrode uncoated portion may be provided in a form that further extends axially outward from an axial end portion of the region coated with the active material.
[0023] The first electrode uncoated portion may be provided over the entire length or over a part of the length.
[0024] The number of the first electrode uncoated portion and the first electrode tab may be one or more.
[0025] The plurality of first electrode tabs may overlap each other to form one electrically connected tab.
[0026] The one first electrode tab may be connected to the first electrode at a position avoiding both ends of the first electrode in a winding direction.
[0027] The two or more first electrode tabs may be connected to the first electrode at positions avoiding both ends and a center portion in a winding direction of the first electrode.
[0028] When only one first electrode tab is provided, in order to prevent an increase in resistance due to an increase in the current path, when the first electrode is divided along the width direction so as to be divided into three equal parts in the winding direction, the first electrode tab can be electrically connected to the first electrode at a position that avoids both regions at both ends in the winding direction.
[0029] When only two first electrode tabs are provided, in order to prevent an increase in resistance due to an increase in the current path, when the first electrode is divided along the width direction into four equal parts in the winding direction, one first electrode tab may be located in each of two central regions avoiding both end regions in the winding direction and electrically connected to the first electrode. When three or more first electrode tabs are provided, they may be arranged in a similar manner to reduce the current path.
[0030] Depending on the method of arranging the first electrode tabs, the plurality of first electrode tabs may be arranged at different radial positions in the radial direction.
[0031] In an electrode assembly in which the first electrode tabs are connected to regions corresponding to regions coated with an active material in an axial direction, the circumferential positions at which the first electrode tabs are arranged may be arranged so as not to overlap with each other.
[0032] In an electrode assembly in which the plurality of first electrode tabs are connected to a first electrode uncoated portion that extends further axially outward from an axial end of a region coated with an active material, the circumferential positions at which the plurality of first electrode tabs are disposed may be arranged to overlap each other.
[0033] The first electrode tab may be connected to the first electrode at an appropriate position such that the first electrode tabs are easily connected to each other when the electrode stack is wound.
[0034] The second electrode uncoated portion may be provided in a continuous shape from the other axial end portion of the second electrode in the winding direction, or may be provided in a notched shape that is discontinuous in the winding direction.
[0035] The second electrode uncoated portion may have an axially protruding height that increases continuously or intermittently.
[0036] The second electrode uncoated portion may be bent in the radial direction in order to improve the performance of welding to a current collector plate or the bottom surface of a battery can, which will be described later.
[0037] A current collecting plate may be coupled to the second electrode uncoated portion. For example, a current collecting plate may be coupled to a surface of the second electrode uncoated portion bent in the radial direction by welding.
[0038] The second electrode and the separation membrane may have an axial length greater than that of the first electrode.
[0039] An axial end portion of the first electrode may be positioned lower than an axial end portion of the second electrode.
[0040] A distance between one axial end of each of the first electrode and the second electrode may be shorter than a distance between the other axial end of the first electrode and a point where the uncoated portion of the second electrode begins.
[0041] The present invention also provides a cylindrical battery structure including the electrode assembly.
[0042] The cylindrical battery may include a cylindrical battery can having one axial side open. The electrode assembly may be accommodated in the battery can such that the second electrode uncoated portion faces a bottom surface of the battery can, and the second electrode uncoated portion may be electrically connected to the bottom surface of the battery can. The first electrode tab may be electrically connected to a battery can lid (cap) covering an upper portion of the battery can.
[0043] A beading portion may be provided on the side wall of the battery can between one axial end of the electrode assembly and the battery can lid, the beading portion including the side wall of the battery can radially inward.
[0044] An insulating layer may be provided at the first electrode tab portion to insulate the first electrode tab from the battery can and the second electrode.
[0045] The insulating layer may cover one axial side of the electrode assembly, and the first electrode may pass through the insulating layer to be connected to the battery can lid.
[0046] The insulating layer may be provided in a portion of the first electrode tab adjacent to the second electrode.
[0047] The above-mentioned problems can also be solved by a battery pack including the cylindrical battery cell, and a vehicle including the battery pack. These battery packs and vehicles are already known to those having ordinary skill in the art, and therefore will not be described in this specification. Effect of the Invention
[0048] The present invention provides a jelly roll type electrode assembly structure in which resistance is reduced by applying a tabless structure to the second electrode, where there is a limit to how much resistance can be reduced by improving the tab structure alone.
[0049] From another aspect, the present invention applies an improved tab structure to a first electrode, which can sufficiently reduce resistance through an improved tab structure. This prevents a decrease in space utilization and a complication of a manufacturing process that would occur if a tabless structure were applied, since the thickness of the first electrode uncoated portion and the current collector plate welded thereto would be increased and the first electrode uncoated portion and the current collector plate would have to be insulated from the battery can and the second electrode.
[0050] In the present invention, one or more tabs applied to reduce resistance are axially connected to a plain portion at an end of the tab that is outside the active material coating region. Therefore, even if the number of tabs is increased, the tabs are not interposed in the retention portion region coated with the active material, thereby preventing deterioration caused by uneven thickness of the tabs.
[0051] In the present invention, two or more tabs applied to reduce resistance are arranged in axially corresponding positions to each other in the circumferential direction when the tabs are connected to the plain portion provided at the end outside the active material coating region, which makes the assembly process, such as overlapping and welding the tabs and connecting the tabs to the lid, very convenient.
[0052] In the present invention, even if two or more tabs applied to reduce resistance are axially connected to uncoated portions provided in areas corresponding to active material coating areas, the tabs are arranged in positions that do not overlap with each other in the circumferential direction, thereby minimizing the phenomenon of deterioration caused by heterogeneous thicknesses of the tabs.
[0053] The present invention can also provide an electrode assembly structure with improved stability that can cut off a short circuit between the first electrode and the second electrode at both axial ends without the need for excessive insulation processing that would be required if the tabless structure is also applied to the first electrode.
[0054] The present invention can provide an improved cylindrical battery cell including the improved electrode assembly, a battery pack including the battery cell, and a vehicle including the battery pack.
[0055] In addition, the present invention can have a number of different effects, which will be described in each embodiment, or the description of effects that can be easily inferred by a person of ordinary skill in the art will be omitted. [Brief description of the drawings]
[0056] [Figure 1] 1 is a view showing an electrode stack in a state before being wound into a jelly roll to form an electrode assembly. [Diagram 2] FIG. 4 is a development view showing a state before a first electrode and a second electrode of a tab structure are wound up. [Diagram 3] FIG. 2 is a cross-sectional view of a cylindrical battery including an electrode assembly having a tab structure. [Figure 4] FIG. 2 is a cross-sectional view of a cylindrical battery including an electrode assembly having a tabless structure. [Diagram 5] 13 is a development view showing a state before a first electrode and a second electrode are wound according to an embodiment of the present invention, in which a continuous uncoated portion is provided at the other axial end of the second electrode. FIG. [Figure 6] 13 is a development view showing a state before a first electrode and a second electrode are wound according to an embodiment of the present invention, in which an uncoated portion having a discontinuous cutout shape is provided at the other axial end of the second electrode. FIG. [Figure 7] 1 is a cross-sectional view of an electrode assembly according to an embodiment of the present invention, in which a first electrode is connected to a second electrode and a non-coated portion is provided on a second electrode, the non-coated portion protruding and bent to the other side in the axial direction. [Figure 8] FIG. 7 shows an electrode assembly according to an embodiment of the present invention, in which a current collector plate is connected to the bent second electrode uncoated portion. [Figure 9] 2 is an enlarged cross-sectional view showing an electrode assembly according to an embodiment of the present invention, in which the axial length of a first electrode is shorter than the axial length of a second electrode. [Figure 10] FIG. 9 is an enlarged cross-sectional view showing an electrode assembly according to one embodiment of the present invention, in which the distance between one axial end of the active material-coated region of the first electrode and the second electrode is shorter than the distance between the other axial end. [Figure 11] 2 is a cross-sectional view of a cylindrical battery according to an embodiment of the present invention, in which one axial side of an electrode assembly is covered with an insulating layer. [Figure 12] FIG. 2 is a cross-sectional view of a cylindrical battery according to an embodiment of the present invention, in which only a portion of a first electrode tab is covered with an insulating layer. [Figure 15] FIG. 13 is a development view of another embodiment of the first electrode and the second electrode. [Figure 16] FIG. 13 is a development view of another embodiment of the first electrode and the second electrode. [Figure 17] FIG. 13 is a development view of another embodiment of the first electrode and the second electrode. [Figure 18] FIG. 18 is a perspective view of a jelly roll type electrode assembly including the first electrode and the second electrode of FIGS. 15 to 17 and wound up. [Figure 19] FIG. 19 is a side cross-sectional view of FIG. 18. [Figure 20] 11 is another embodiment of the second electrode. [Figure 21] 21 is an enlarged cross-sectional view of a laminated structure using the second electrode of FIG. 20. [Figure 22] 1 is a perspective view showing a battery pack including a cylindrical battery cell according to the present invention; [Figure 23] FIG. 23 is a perspective view showing a vehicle including the battery pack of FIG. 22. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0057] The above-mentioned objects, features and advantages will be described in detail below with reference to the accompanying drawings, so that a person having ordinary skill in the art to which the present invention pertains can easily implement the technical idea of the present invention. In describing the present invention, if a detailed description of a known technology according to the present invention is deemed to make the gist of the present invention unclear, the detailed description will be omitted. Hereinafter, a preferred embodiment according to the present invention will be described in detail with reference to the accompanying drawings. The same reference numerals in the drawings are used to indicate the same or similar components.
[0058] Although the terms "first", "second", etc. are used to describe various components, it is understood that these components are not limited by these terms. These terms are used merely to distinguish one component from another, and it is understood that a first component may also be a second component unless otherwise specified.
[0059] Unless otherwise specified to the contrary in the entire specification, each element may be singular or plural.
[0060] Hereinafter, when an arbitrary structure is arranged on the "top (or bottom)" of a component or "above (or below)" a component, it means that the arbitrary structure is not only arranged in contact with the upper surface (or lower surface) of the component, but also that other structures may be interposed between the component and the arbitrary structure arranged on (or below) the component.
[0061] In addition, when a component is described as being "coupled," "coupled," or "connected" to another component, it should be understood that the components may be directly coupled or connected to each other, but that there may be other components "intervening" between each component, or each component may be "coupled," "coupled," or "connected" via other components.
[0062] As used herein, singular expressions include plural expressions unless the context clearly indicates otherwise. In this application, the terms "comprise" or "include" should not be interpreted as including all of the multiple components or multiple steps described in the specification, and should be interpreted as including some of the components or steps that may not be included or may include additional components or steps.
[0063] Throughout the specification, "A and / or B" means A, B, or A and B, unless otherwise specified, and "C to D" means C or more and D or less, unless otherwise specified.
[0064] For ease of explanation, in this specification, the direction along the longitudinal direction of the winding shaft of the electrode assembly wound into a jelly roll is referred to as the axial direction (Y). The direction surrounding the winding shaft is referred to as the circumferential direction (X). The directions approaching the winding shaft or moving away from the winding shaft are referred to as the radial direction (Z). Of these, the direction approaching the winding shaft is referred to as the centripetal direction, and the direction moving away from the winding shaft is referred to as the centrifugal direction.
[0065] The present invention provides a jelly roll electrode assembly structure that can reduce resistance, increase space utilization, and prevent short circuits, and a cylindrical battery cell structure including the electrode assembly.
[0066] Hereinafter, preferred embodiments of the present invention will be described with reference to the accompanying drawings.
[0067] First, the structure and manufacturing method of a tab-type and tabless-type cylindrical battery will be described. Generally, a cylindrical battery is manufactured by incorporating an electrode assembly wound in a jelly roll shape inside a battery can.
[0068] FIG. 1 shows an electrode stack before being wound into a jelly roll to form an electrode assembly. Referring to this figure, the jelly roll type electrode assembly can be formed by winding up an electrode stack in which roll sheets of a first electrode 2, a separator 3, a second electrode 4, and a separator 3 are sequentially stacked. As a result, the jelly roll type electrode assembly has a circular pipe shape with a hollow portion formed in a winding shaft. That is, the longitudinal direction (X) of the electrode stack corresponds to the winding direction of the cylindrical electrode assembly, i.e., the circumferential direction, the width direction (Y) of the electrode stack corresponds to the axial direction of the electrode assembly, and the normal direction (Z) of the electrode stack corresponds to the radial direction (centripetal direction or centrifugal direction) of the electrode assembly.
[0069] The separator may be made of the same material and have the same shape regardless of the stacking position. The separator may be made of a material and have a structure that insulates the first electrode 2 and the second electrode 4 in the electrode stack from each other while allowing the electrolyte to pass therethrough, as described below, so as to prevent electrical short-circuiting between the two electrodes.
[0070] The separator includes a porous polymer substrate and porous coating layers disposed on both sides of the porous polymer substrate and including inorganic particles and a binder polymer.
[0071] The porous polymer substrate may be a polyolefin-based porous substrate.
[0072] The polyolefin porous substrate may be in the form of a film or a non-woven web. The porous structure allows smooth movement of the electrolyte between the positive and negative electrodes, and increases the electrolyte impregnation of the substrate itself, ensuring excellent ion conductivity, and preventing an increase in the internal resistance of the electrochemical device, thereby preventing a decrease in the performance of the electrochemical device.
[0073] The polyolefin porous substrate used in the present invention may be any planar porous substrate typically used in electrochemical devices, and its material and shape may be selected from a variety of options depending on the intended purpose.
[0074] The polyolefin porous substrate may be, but is not limited to, a film or non-woven web formed of high density polyethylene, low density polyethylene, linear low density polyethylene, ultra-high molecular weight polyethylene, polypropylene, or a mixture of two or more of these.
[0075] The polyolefin porous substrate may have a thickness of 8 to 30 μm, but this is merely an example, and a thickness outside the above range may be adopted in consideration of mechanical properties and high-rate charge / discharge characteristics of the battery.
[0076] The nonwoven sheet according to the present invention may be made of polyethylene (PE), polypropylene (PP), or a mixture of two or more of them. For example, the nonwoven sheet may be manufactured by fiber radiating. For example, the nonwoven sheet may be manufactured by using a melt blown method to radiate the fibers of the material at a temperature above the melting point, followed by blending and radiating.
[0077] The nonwoven fabric sheet may have an elongation ratio of 200 to 400%, more preferably 300 to 400%. If the elongation ratio is less than 200%, the probability of contact between the electrodes increases when the nail is penetrated, and if it is more than 400%, the surrounding area where the nail is penetrated is also elongated, the separation membrane becomes thin, and the barrier property is reduced.
[0078] The nonwoven fabric sheet has a plurality of pores having an average diameter of 0.1 to 10 μm formed therein. If the pore size is smaller than 0.1 μm, the lithium ions and / or the electrolyte do not move smoothly, and if the pore size is larger than 10 μm, it is difficult to achieve the effect of the present invention, which is to prevent contact between the positive electrode and the negative electrode by stretching the nonwoven fabric sheet when a nail is penetrated.
[0079] The nonwoven fabric sheet may have a porosity of 40 to 70%. If the porosity is less than 40%, it is difficult for lithium ions and / or electrolyte to move smoothly, and if the porosity is greater than 70%, it is difficult to achieve the effect of the present invention of preventing contact between the positive and negative electrodes by stretching the nonwoven fabric sheet when a nail is penetrated. The nonwoven fabric sheet manufactured in this manner may have an air permeability of 1 to 20 seconds / 100 mL.
[0080] In addition, the nonwoven fabric sheet may have a thickness of 10 to 20 μm, but this is merely an example and is not limited thereto. Depending on the permeability of the nonwoven fabric sheet, a nonwoven fabric sheet having a thickness outside the above range may also be adopted.
[0081] The nonwoven fabric sheet can be bonded to the separation membrane component placed under the nonwoven fabric sheet by lamination. The lamination can be performed at a temperature range of 100 to 150° C. If the lamination is performed at a temperature lower than 100° C., the lamination effect is not generated, and if the lamination is performed at a temperature higher than 150° C., part of the nonwoven fabric melts.
[0082] The separation membrane according to one embodiment of the present invention, laminated under the above-mentioned conditions, has improved resistance to nail penetration when compared to a separation membrane made of a conventional nonwoven fabric sheet and when compared to a separation membrane in which a layer containing inorganic particles is formed on at least one surface of a film or nonwoven fabric sheet.
[0083] The inorganic particles in the porous coating layer are bound to each other by the binder polymer while being in contact with each other, and thus interstitial volumes are formed between the inorganic particles. The interstitial volumes between the inorganic particles become vacant spaces and can form pores.
[0084] The inorganic particles used to form the porous coating layer are inorganic particles, i.e., the inorganic particles are within the operating voltage range of the electrochemical element (e.g., Li / Li + Inorganic particles that do not undergo oxidation and / or reduction reactions at a voltage of 0 to 5 V relative to the reference voltage can be further added and used. In particular, when inorganic particles having ion transfer ability are used, the ionic conductivity in the electrochemical element can be increased, thereby improving performance. In addition, when inorganic particles having a high dielectric constant are used as the inorganic particles, the inorganic particles can contribute to an increase in the degree of dissociation of the electrolyte salt, for example, lithium salt, in the liquid electrolyte, thereby improving the ionic conductivity of the electrolyte.
[0085] For the reasons mentioned above, the inorganic particles preferably include high dielectric constant inorganic particles having a dielectric constant of 5 or more, preferably 10 or more, inorganic particles having lithium ion transport ability, or a mixture thereof.
[0086] Non-limiting examples of inorganic particles having a dielectric constant of 5 or greater include BaTiO3, Pb(Zr,Ti)O3 (PZT), Pb 1-x La x Zr 1-y Ti y O3(PLZT), PB(Mg 1 / 3 Nb 2 / 3)O3-PbTiO3 (PMN-PT), hafnia (HfO2), SrTiO3, SnO2, CeO2, MgO, NiO, CaO, ZnO, ZrO2, Y2O3, Al2O3, TiO2, SiC, or mixtures thereof.
[0087] In particular, the aforementioned BaTiO3, Pb(Zr,Ti)O3 (PZT), and Pb 1-x La x Zr 1-y Ti y O3(PLZT), PB(Mg 1 / 3 Nb 2 / 3 Inorganic particles such as PMN-PT, PbTiO3, and hafnia (HfO2) not only exhibit high dielectric constant characteristics with a dielectric constant of 100 or more, but also have piezoelectricity in which, when tensioned or compressed by applying a certain pressure, electric charges are generated and a potential difference occurs between both surfaces, thereby preventing internal short circuits between the two electrodes due to external impact and improving the safety of the electrochemical device. In addition, when the above-mentioned high dielectric constant inorganic particles are mixed with inorganic particles having lithium ion transfer ability, these increasing effects can be doubled.
[0088] The inorganic particles having lithium ion transport ability are inorganic particles that contain lithium elements but do not store lithium but have the function of transporting lithium ions. The inorganic particles having lithium ion transport ability can transport and transport lithium ions due to a type of defect present inside the particle structure, thereby improving the lithium ion conductivity in the battery and thereby improving the battery performance. Non-limiting examples of the inorganic particles having lithium ion transport ability include lithium phosphate (Li3PO4), lithium titanium phosphate (Li x Ti y (PO4)3, 0 <x<2、0<y<3)、リチウムアルミニウムチタンホスフェート(Li x Al y Ti z(PO4)3, 0 < x < 2, 0 < y < 1, 0 < z < 3), (LiAlTiP) such as 14Li2O - 9Al2O3 - 38TiO2 - 39P2O5 x O y series glass (0 < x < 4, 0 < y < 13), lithium lanthanum titanate (Li x La y TiO3, 0 < x < 2, 0 < y < 3), Li 3.25 Ge 0.25 P 0.75 lithium germanium thiophosphate (Li x Ge y P z S w , 0 < x < 4, 0 < y < 1, 0 < z < 1, 0 < w < 5), lithium nitride (Li x N y , 0 < x < 4, 0 < y < 2), SiS2 series glass (Li x Si y S z , 0 < x < 3, 0 < y < 2, 0 < z < 4), P2S5 series glass (Li x P y S z , 0 < x < 3, 0 < y < 3, 0 < z < 7), or a mixture thereof, etc.
[0089] Although there is no limit to the size of the inorganic particles of the porous coating layer, for the formation of a coating layer with a uniform thickness and an appropriate porosity, it is preferably 0.001 to 10 μm. If it is less than 0.001 μm, the dispersibility of the inorganic particles may decrease. If it exceeds 10 μm, the thickness of the porous coating layer increases, the mechanical properties may decrease, and due to the size of the pores being too large, the probability of internal short - circuit occurring during battery charge and discharge increases.
[0090] Binder polymers forming the porous coating layer include polyvinylidene fluoride-co-hexafluoropropylene (PVdF), polyvinylidene fluoride-cotrichloroethylene, polymethylmethacrylate, polybutylacrylate, polyacrylonitrile, polyvinylpyrrolidone, polyvinylacetate, ethylene-vinyl acetate copolymer, polyethylene oxide, polyarylate, cellulose acetate, cellulose acetate butyrate, and cellulose acetate propionate. The binder polymer may be any one selected from the group consisting of cellulose acetate propionate, cyanoethyl pullulan, cyanoethyl polyvinyl alcohol, cyanoethyl cellulose, cyanoethyl sucrose, pullulan, and carboxyl methyl cellulose, or a mixture of two or more of these, but is not limited thereto.
[0091] The composition ratio of inorganic particles and binder polymer used in the porous coating layer is, for example, preferably in the range of 50:50 to 99:1, more preferably 70:30 to 95:5. If the content ratio of inorganic particles to binder polymer is less than 50:50, the content of binder polymer increases, and the improvement of thermal safety of the separator may be reduced. In addition, the size and porosity of the pores may decrease due to the reduction of the vacant space formed between the inorganic particles, which may ultimately cause a decrease in battery performance. If the content of inorganic particles exceeds 99 parts by weight, the content of binder polymer is too small, and the peel resistance of the porous coating layer may be weakened. The thickness of the porous coating layer is not particularly limited, but is preferably in the range of 0.01 to 20 μm. In addition, the size and porosity of the pores are not particularly limited, but the size of the pores is preferably in the range of 0.001 to 10 μm, and the porosity is preferably in the range of 10 to 90%. The size and porosity of the pores mainly depend on the size of the inorganic particles, and for example, when inorganic particles with a particle size of 1 μm or less are used, the pores formed are also approximately 1 μm or less. These pore structures are filled with the electrolyte that is injected later, and the electrolyte thus filled plays a role in transmitting ions. If the size and porosity of the pores are less than 0.001 μm and 10%, respectively, it can act as a resistance layer, and if the size and porosity of the pores are more than 10 μm and 90%, respectively, the mechanical properties can be deteriorated.
[0092] The porous coating layer can be formed by dissolving or dispersing a binder polymer in a dispersion medium, adding inorganic particles to obtain a slurry for forming a porous coating layer, and coating and drying the slurry on at least one surface of a substrate. The dispersion medium preferably has a solubility index similar to that of the binder polymer to be used and a low boiling point. This is for uniform mixing and easy removal of the dispersion medium thereafter. Non-limiting examples of the dispersion medium that can be used include acetone, tetrahydrofuran, methylene chloride, chloroform, dimethylformamide, N-methyl-2-pyrrolidone (NMP), cyclohexane, water, or a mixture thereof.
[0093] It is preferable to add inorganic particles to the dispersion liquid in which the binder polymer is dispersed in the dispersion medium, and then crush the inorganic particles. At this time, the crushing time is appropriately 1 to 20 hours, and the particle size of the crushed inorganic particles is preferably 0.001 to 10 μm as described above. As the crushing method, a conventional method can be used, and in particular, the ball mill method is preferable.
[0094] Then, the binder polymer dispersion liquid in which the inorganic particles are dispersed is coated on at least one surface of the porous polymer substrate under a humidity condition of 10 to 80%, and then dried. The dispersion liquid can be coated on the porous polymer substrate by a conventional coating method known in the art, and various methods such as dip coating, die coating, roll coating, comma coating, or a mixture thereof can be used.
[0095] The porous coating layer components may further include other additives such as a conductive agent in addition to the inorganic particles and the binder polymer described above.
[0096] The final separator according to the present invention may have a thickness of 1 to 100 μm or 5 to 50 μm. If the thickness is less than 1 μm, the separator may not fully function and mechanical properties may deteriorate, and if the thickness exceeds 100 μm, battery properties may deteriorate during high-rate charging and discharging. In addition, the separator may have a porosity of 40 to 60% and an air permeability of 150 to 300 sec / 100 mL.
[0097] According to an embodiment of the present invention, the porous polymer substrate may be made of polyethylene or polypropylene, and the inorganic particles in the porous coating layer may be made of Al oxide or Si oxide coating materials.
[0098] When using a separator according to an embodiment of the present invention, since the porous coating layers are provided on both sides of the porous polymer substrate, a uniform solid electrolyte interface layer can be formed to improve the impregnation performance of the electrolyte, and superior air permeability can be secured compared to a conventional single-sided inorganic coating separator. For example, it may be within 120s / 100cc. Even if inorganic porous coating layers are provided on both sides, the thickness can be the same as that of a conventional single-sided inorganic coating separator. For example, it may be within 15.0 μm.
[0099] In addition, when a separator according to an embodiment of the present invention is used, the safety of the separator is improved and heat resistance and compression resistance can be ensured. Specifically, heat resistance with thermal shrinkage of 5% or less based on 180°C can be ensured, and a puncture strength of 550gf or more can be ensured. When core deformation occurs during cycles of a battery using these separators, damage or puncture of the separator at the step can be prevented.
[0100] The first electrode 2 may be a positive electrode and the second electrode 4 may be a negative electrode, but the reverse may also be true, and so they are referred to herein as a first electrode and a second electrode, respectively.
[0101] The first electrode 2 can be wound more inward than the second electrode 4. As a result, the first electrode 2 can have a shorter radius from the winding axis than the second electrode 4, and therefore a shorter circumferential length along the winding direction. In this case, the first electrode 2 before winding can have a shorter length in the longitudinal direction than the second electrode 4 before winding.
[0102] 2 is an exploded view showing a state before the first and second electrodes having a tab structure are wound. Referring to this, each of the first and second electrodes 2 and 4 may be coated with an active material 22 or 42 on one or both sides. The active material 22 or 42 is coated on the surface of the first and second electrodes 2 and 4 and participates in an electrode reaction by storing or releasing ions.
[0103] In the present invention, the positive electrode active material coated on the positive electrode plate and the negative electrode active material coated on the negative electrode plate can be any active material known in the art.
[0104] The positive electrode active material is a layered compound such as lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2), or a compound substituted with one or more transition metals; 1+x Mn 2x Lithium manganese oxides (LiMnO2), such as LiMnO3, LiMn2O3, and LiMnO2; lithium copper oxide (Li2CuO2); vanadium oxides, such as LiV3O8, LiFe3O4, V2O5, and Cu2V2O7; and the chemical formula LiNi 1-x M xLithium nickel oxide with nickel site type represented by the formula LiMnO2 (where M=Co, Mn, Al, Cu, Fe, Mg, B or Ga, and x=0.01 to 0.3); 2-x M x Lithium intercalation materials include, but are not limited to, lithium manganese composite oxides represented as LiMnO2 (wherein M is Co, Ni, Fe, Cr, Zn, or Ta, and x is 0.01 to 0.1) or Li2Mn3MO8 (wherein M is Fe, Co, Ni, Cu, or Zn); LiMn2O4 in which part of the lithium in the chemical formula is replaced with an alkaline earth metal ion; disulfide compounds; Fe2(MoO4)3, or composite oxides formed by a combination of these.
[0105] The positive electrode current collector has a thickness of, for example, 3 to 500 μm. The positive electrode current collector is not particularly limited as long as it does not cause a chemical change in the battery and has conductivity, and for example, stainless steel, aluminum, nickel, titanium, plastic carbon, or aluminum or stainless steel surface-treated with carbon, nickel, titanium, silver, etc. can be used. The electrode current collector can be formed with fine irregularities on its surface to increase the adhesive strength of the positive electrode active material, and can be in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.
[0106] A conductive material can be further mixed into the positive electrode active material particles. These conductive materials are added, for example, in an amount of 1 to 50% by weight based on the total weight of the mixture containing the positive electrode active material. These conductive materials are not particularly limited as long as they do not cause chemical changes in the battery and have high conductivity, and examples of the conductive materials that can be used include graphite such as natural graphite and artificial graphite; carbon black such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, and summer black; conductive fibers such as carbon fibers and metal fibers; metal powders such as carbon fluoride, aluminum, and nickel powder; conductive whiskers such as zinc oxide and potassium titanate; conductive oxides such as titanium oxide; and conductive materials such as polyphenylene derivatives.
[0107] The negative electrode is fabricated by coating and drying negative electrode active material particles on a negative electrode current collector, and may further include components such as the conductive material, binder, and solvent described above, if necessary.
[0108] The negative electrode current collector has a thickness of, for example, 3 to 500 μm. The negative electrode current collector is not particularly limited as long as it does not cause a chemical change in the battery and has conductivity, and for example, copper, stainless steel, aluminum, nickel, titanium, plastic carbon, copper or stainless steel surface-treated with carbon, nickel, titanium, silver, aluminum-cadmium alloy, etc. can be used. In addition, like the positive electrode current collector, fine irregularities can be formed on the surface to strengthen the binding force of the negative electrode active material, and it can be used in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.
[0109] The negative electrode active material is, for example, carbon such as non-graphitizable carbon or graphite-based carbon; Li x Fe2O3(0≦x≦1), Li x WO2(0≦x≦1), Sn x Me 1-x Me'yO zMetal composite oxides of (Me: Mn, Fe, Pb, Ge; Me’: Al, B, P, Si, Group 1, Group 2, Group 3 elements of the periodic table, halogen; 0 < x ≤ 1; 1 ≤ y ≤ 3; 1 ≤ z ≤ 8); lithium metal; lithium alloy; silicon-based alloy; tin-based alloy; oxides such as SnO, SnO2, PbO, PbO2, Pb2O3, Pb3O4, Sb2O3, Sb2O4, Sb2O5, GeO, GeO2, Bi2O3, Bi2O4, Bi2O5; conductive polymers such as polyacetylene; Li-Co-Ni-based materials, etc. can be used.
[0110] The binder polymer usable in the electrode is a component that aids in binding between the electrode active material particles and the conductive material and between the electrode current collector, and is added in an amount of, for example, 1 to 50 wt % based on the total weight of the mixture including the electrode active material. Examples of these binder polymers include polyvinylidene fluoride-co-hexafluoropropylene (PVdF), polyvinylidene fluoride-co-trichloroethylene, polymethylmethacrylate, polybutylacrylate, polyacrylonitrile, polyvinylpyrrolidone, polyvinylacetate, ethylene-vinyl acetate copolymer, polyethylene oxide, polyarylate, cellulose acetate, cellulose acetate butyrate, and cellulose acetate propionate. The binder polymer may be any one selected from the group consisting of cellulose acetate propionate, cyanoethyl pullulan, cyanoethyl polyvinyl alcohol, cyanoethyl cellulose, cyanoethyl sucrose, pullulan, and carboxyl methyl cellulose, or a mixture of two or more of these, but is not limited thereto.
[0111] Non-limiting examples of the solvent used in the preparation of the electrode include acetone, tetrahydrofuran, methylene chloride, chloroform, dimethylformamide, N-methyl-2-pyrrolidone (NMP), cyclohexane, water, or a mixture thereof, etc. These solvents provide an appropriate level of viscosity so that a slurry coating layer can be formed at a desired level on the surface of the electrode current collector.
[0112] The negative electrode comprises a current collector; and a negative electrode active material layer located on at least one surface of the current collector and including a negative electrode active material, a binder polymer, and a conductive material, the negative electrode active material layer comprising a lower layer region in contact with the current collector, and an upper layer region in contact with the lower layer region and extending to a surface of the negative electrode active material layer, the lower layer region and the upper layer region each independently containing at least one of graphite and a silicon-based compound as the negative electrode active material.
[0113] The lower layer region may include natural graphite as a negative electrode active material, and the upper layer region may include artificial graphite as a negative electrode active material.
[0114] The lower layer region and the upper layer region may each independently further include a silicon-based compound as a negative electrode active material.
[0115] The silicon-based compound is SiO x (0≦x≦2) and SiC.
[0116] According to an embodiment of the present invention, the negative electrode may be manufactured by coating and drying a lower layer slurry containing a lower layer negative electrode active material on a current collector to form a lower layer region, and then coating and drying an upper layer slurry containing an upper layer negative electrode active material on the lower layer region to form an upper layer region.
[0117] In addition, according to an embodiment of the present invention, the negative electrode may include a step of preparing a lower layer slurry including a lower layer negative electrode active material and an upper layer slurry including an upper layer negative electrode active material; coating one surface of a negative electrode current collector with the lower layer slurry, and simultaneously or after a predetermined time, coating the upper layer slurry on the lower layer slurry; and and drying the coated lower layer slurry and upper layer slurry simultaneously to form an active material layer.
[0118] In the latter case, a mixed region (intermixing) in which different types of active materials are mixed with each other may be present at the contact portion between the lower layer region and the upper layer region of the negative electrode. This is because, when an active material layer is formed by simultaneously or successively coating a lower layer slurry containing a lower layer negative electrode active material and an upper layer slurry containing an upper layer negative electrode active material on a current collector and then drying them simultaneously, a certain mixed region is generated at the interface where the lower layer slurry and the upper layer slurry contact each other before drying, and then the mixed region is formed in the form of a layer while drying.
[0119] In the negative electrode active material layer according to an embodiment of the present invention, the weight ratio (or the ratio of the load amount per unit area) of the upper layer region to the lower layer region may be 20:80 to 50:50, specifically, 25:75 to 50:50.
[0120] The thicknesses of the lower and upper regions of the negative electrode active material layer of the present invention may not be completely equal to the thicknesses of the coated lower layer slurry and the coated upper layer slurry, but the thickness ratio of the lower and upper regions of the negative electrode active material layer of the present invention finally obtained as a result of the drying or selective rolling process may be equal to the thickness ratio of the coated lower layer slurry and the coated upper layer slurry.
[0121] The first slurry is coated, and the second slurry is coated on the first slurry at the same time or after a predetermined time interval, and according to an embodiment of the present invention, the predetermined time difference may be 0.6 seconds or less, or 0.02 seconds to 0.6 seconds, or 0.02 seconds to 0.06 seconds, or 0.02 seconds to 0.03 seconds. Since the time difference occurs when coating the first slurry and the second slurry as described above, due to the coating equipment, it is more preferable to coat the first slurry and the second slurry simultaneously. The method of coating the second slurry on the first slurry can use an apparatus such as a double slot die.
[0122] The step of forming the active material layer may further include a step of rolling the active material layer after the drying step, wherein the rolling may be performed by a method commonly used in the art, such as roll pressing, at a pressure of 1 to 20 MPa and a temperature of 15 to 30°C.
[0123] The step of simultaneously drying the coated lower layer slurry and upper layer slurry to form an active material layer may be carried out by a method commonly used in the art using a combination of a hot air dryer and an infrared dryer.
[0124] The weight % of the first binder polymer in the solid content of the lower layer slurry may be equal to or greater than the weight % of the second binder polymer in the solid content of the upper layer slurry. According to an embodiment of the present invention, the weight % of the first binder polymer in the solid content of the lower layer slurry may be 1.0 to 4.2 times, 1.5 to 3.6 times, or 1.5 to 3 times greater than the weight % of the second binder polymer in the solid content of the upper layer slurry.
[0125] In this case, when the weight percentage of the first binder in the coated lower layer slurry and the weight percentage of the second binder in the coated upper layer slurry satisfy these ranges, the amount of binder in the lower layer region is not too small, so detachment of the electrode layer does not occur, and the amount of binder in the upper layer region is not too large, so the resistance of the upper layer of the electrode is reduced, which is advantageous for fast charging performance.
[0126] The weight percentage of the first binder polymer in the solid content of the lower layer slurry may be 2 to 30 weight%, or 5 to 20 weight%, or 5 to 20 weight%, and the weight percentage of the second binder polymer in the solid content of the upper layer slurry may be 0.5 to 20 weight%, or 1 to 15 weight%, or 1 to 10 weight%, or 2 to 5 weight%.
[0127] The total ratio (wt %) of the first binder polymer and the second binder polymer to the total solid content of the lower layer slurry and the upper layer slurry may be 2 to 20 wt % or 5 to 15 wt %.
[0128] 2, the first electrode 2 and the second electrode 4 may have a first electrode uncoated portion 21 and a second electrode uncoated portion 41 that are not coated with the active materials 22 and 42, respectively. The first electrode uncoated portion 21 and the second electrode uncoated portion 41 may have a first electrode tab 23 and a second electrode tab 43 electrically connected to the first electrode uncoated portion 21 and the second electrode uncoated portion 41, respectively, in order to electrically connect the first electrode 2 and the second electrode 4 to the outside.
[0129] The first electrode tab 23 and the second electrode tab 43 may be provided one by one, or a plurality of them may be provided.
[0130] If the second electrode uncoated portion 41 and the second electrode tab 43 are only provided on both ends of the second electrode 4 due to a manufacturing process, the current path of the second electrode 4 becomes longer, and the resistance increases. This is even more true when the second electrode 4 is longer than the first electrode 2.
[0131] 3 is a cross-sectional view of a cylindrical battery including an electrode assembly having a tab structure. Referring to this figure, an electrode assembly 1 in which an electrode laminate is wound up in a jelly roll shape is housed in a battery can 6 having one axial side open.
[0132] A first electrode tab 23 connected to the first electrode uncoated portion 21 of the electrode assembly 1 is connected to a first electrode terminal 631 provided on a battery can lid 63, thereby electrically connecting the first electrode 2 to the battery can lid 63 and the outside. One axial side of the electrode assembly 1 from which the first electrode tab 23 protrudes may be covered with an insulating layer 65.
[0133] The second electrode tab 43 connected to the second electrode uncoated portion 41 of the electrode assembly 1 is connected to a bottom surface 62 of the battery can, thereby electrically connecting the second electrode to the battery can 6 and the outside.
[0134] The battery can lid 63 is connected to the first electrode 2, and the battery can 6 is connected to the second electrode 4, so that an insulating layer 65 is provided between the battery can lid 63 and the battery can 6 to prevent short circuit.
[0135] The side wall 61 of the battery can may be provided with beading portions 64 extending radially inwardly on the electrode assembly 1. By providing these beading portions 64, the electrode assembly 1 may be stably accommodated in the battery can 6 without any gaps above or below.
[0136] In the above tab structure, the only current paths between the first electrode 2 and the second electrode 4 are the first electrode tab 23 and the second electrode tab 43, so the resistance of this portion is very high, heat may be generated, and performance and durability may be poor. This is because electrical resistance is proportional to the length of the current path and inversely proportional to the area, so if the current path is narrow, it is not favorable for reducing resistance.
[0137] 4 is a cross-sectional view of a cylindrical battery including an electrode assembly having a tabless structure. Referring to this figure, the electrode laminate is formed by winding up an electrode assembly 1 in a jelly-roll shape and housing it in a battery can 6 that is open on one axial side.
[0138] A first electrode uncoated portion 21 and a second electrode uncoated portion 41 protrude from both axial sides of the electrode assembly 1, and the first electrode uncoated portion 21 and the second electrode uncoated portion 41 are respectively connected to a current collector plate 5. In this case, the first electrode uncoated portion 21 and the second electrode uncoated portion 41 may be bent in a radial direction to improve the bonding performance between the first electrode collector plate 51 and the second electrode collector plate 52.
[0139] The first electrode current collector 51 connected to the first electrode uncoated portion 21 is connected to a first electrode tab 23, and the first electrode tab 23 is connected to a battery can lid 63 via a first electrode terminal 631, thereby electrically connecting the first electrode to the outside.
[0140] The second electrode current collector 52 connected to the second electrode uncoated portion 41 is connected to a bottom surface 62 of the battery can, thereby electrically connecting the second electrode to the battery can 6 and the outside.
[0141] Since the battery can lid 63 is connected to the first electrode 2 and the battery can 6 is connected to the second electrode 4, an insulating layer 65 is provided between the battery can lid 63 and the battery can 6 to prevent a short circuit. In addition, in order to prevent the first electrode current collector 51 from shorting with the inner wall of the battery can 6, the top and side surfaces of the first electrode current collector 51 may be covered with the insulating layer 65.
[0142] The side wall 61 of the battery can may be provided with beading portions 64 extending radially inwardly on the electrode assembly 1. By providing these beading portions 64, the electrode assembly 1 may be stably accommodated in the battery can 6 without any vertical clearance.
[0143] In the case of the second electrode, the above-mentioned tabless structure is advantageous in reducing resistance by making a wide current path on the second electrode 4 side by making the current flow through the second electrode uncoated portion 41, the second electrode current collector plate 52, and the bottom surface 62 of the battery can. However, on the first electrode 2 side, the current flows through the first electrode tab 23 anyway, so it is not useful for reducing resistance, and instead the first electrode uncoated portion 21, the first electrode current collector plate 51, and the insulating layer 65 are added, and the battery can 6 must be longer vertically. This results in a shorter length of the electrode assembly 1 in a cylindrical battery cell of the same standard, resulting in a reduced capacity. In addition, when the first electrode uncoated portion 21 and the second electrode uncoated portion 41 are bent in the radial direction to improve the bonding performance with the current collector plate 5, they may cause a short circuit with the axial ends of the second electrode 4 and the first electrode 2, respectively, and are also weak in stability.
[0144] Meanwhile, a thermal runaway prevention mechanism (CID; Current Interrupt Device) and / or a vent structure may be applied to the cover 63. However, as described above, the structure in which the first electrode uncoated portion 21 is bent in the radial direction and the current collector plate 5 is welded thereon may prevent the internal pressure of the battery can 6 from acting completely on the CID, cover the vent structure, or affect battery performance.
[0145] For this reason, the present invention provides an improved electrode assembly structure that has the effect of reducing resistance and improving space utilization of a tabless structure on the second electrode side, and has the space utilization of a tab structure and stability against short circuits on the first electrode side, which sufficiently reduces resistance even without a tabless structure.
[0146] 5 and 6 are development views showing the state before being wound up of the first electrode and the second electrode according to each embodiment of the present invention, in which a continuous uncoated portion and a discontinuous uncoated portion are provided at the other axial end of the second electrode, respectively.
[0147] Referring to these drawings, both surfaces of a first electrode 2 and a second electrode 4 are coated with active materials 22, 42. A first electrode uncoated portion 21 is provided in a portion of the interior of the first electrode 2 (the portion in which the active material is applied in the axial direction (Y)) in the longitudinal direction (X), and a first electrode tab 23 connected to the first electrode uncoated portion 21 protrudes to one side in the width direction (axial direction after winding) of the first electrode 2. A second electrode uncoated portion 41 is provided and exposed at the other end of the second electrode 4 in the width direction.
[0148] The first electrode uncoated portion 21 and the first electrode tab 23 may be provided in a single number or in a plurality of numbers. When a plurality of first electrode tabs 23 are provided, the current path of the first electrode 2 becomes wider, and a resistance reducing effect may be obtained. As described below, the plurality of first electrode tabs 23 may be formed such that at least a portion of the area of the first electrode tabs 23 overlaps with each other and is electrically connected to form one tab after winding. This structure makes it easier to connect the first electrode tabs 23 to the cover 63.
[0149] The number of first electrode tabs 23 may be determined as the minimum number at which a resistance value measured in a path connected to the first electrode 2 can fall below a predetermined resistance value. For example, if a resistance value measured when two first electrode tabs 23 are used is below a predetermined resistance value, it is sufficient to use two first electrode tabs 23, and it is not necessary to use three or more first electrode tabs 23.
[0150] The first electrode uncoated portion 21 and the first electrode tab 23 may be provided at appropriate positions to minimize the current path of the first electrode 2. For example, when one each of the first electrode uncoated portion 21 and the first electrode tab 23 is provided, the first electrode uncoated portion 21 and the first electrode tab 23 may be provided at positions avoiding both regions at both ends in the longitudinal direction when the first electrode 2 is divided along the width direction so as to be divided into three equal parts in the longitudinal direction (winding direction). Also, for example, when the first electrode uncoated portion 21 and the first electrode tab 23 are provided at two locations each, the first electrode uncoated portion 21 and the first electrode tab 23 may be provided at two locations avoiding both regions at both ends in the longitudinal direction when the first electrode 2 is divided along the width direction so as to be divided into four equal parts in the longitudinal direction (winding direction). When the first electrode non-coating portions 21 and the first electrode tabs 23 are provided at three or more locations, they can be appropriately arranged by a method similar to that described above.
[0151] Although the number of first electrode tabs 23 is minimized, if the resistance value measured by appropriately selecting the position of the first electrode tab 23 is higher than a predetermined resistance value, the number of first electrode tabs 23 can be minimized by increasing the number of first electrode tabs 23 by one and appropriately selecting the position of the first electrode tab 23.
[0152] The second electrode uncoated portion 41 may be provided at the other end of the second electrode in the four width directions in a continuous form in the longitudinal direction as shown in Fig. 5, or may be provided in a form in which the second electrode is intermittently cut out in the longitudinal direction as shown in Fig. 6. The cutouts may be for bending the second electrode uncoated portion 41, which will be described later.
[0153] The first electrode 2 and the second electrode 4 as described above may be stacked and wound with the separator 3 interposed therebetween to form a jelly roll type electrode assembly.
[0154] FIG. 7 is a cross-sectional view of an electrode assembly according to one embodiment of the present invention in which a first electrode is connected to a first electrode and a second electrode is provided with an uncoated portion that protrudes and bends to the other axial direction, and FIG. 8 is an electrode assembly according to one embodiment of the present invention in which a collector plate is connected to the bent uncoated portion of the second electrode in FIG. 7.
[0155] Referring to FIG. 7, the second electrode uncoated portion 41 may protrude toward the other axial direction of the electrode assembly 1 compared to the first electrode 2 and the separator 3. The second electrode uncoated portion 41 may be bent in a radial direction. The radial direction is a concept including both the centrifugal direction and the centripetal direction. More preferably, according to the embodiment, the second electrode uncoated portion 41 may be bent in a centripetal direction. As a result, the second electrode uncoated portion 41 provides a flat surface on the other axial direction side, and can improve the bonding performance when bonding with the current collector plate 5 or the bottom surface 62 of the battery can described later. This can also further widen the current path to reduce resistance.
[0156] 8, the bent second electrode uncoated portion 41 may have a surface to which a current collector 5 is connected. When the electrode assembly 1 is housed in a battery can 6 (described later) and the second electrode uncoated portion 41 is electrically connected to a bottom surface 62 of the battery can 6, the presence of the current collector 5 may improve the stability of assembly and bonding.
[0157] Even in a wound state, the first electrode tab 23 protrudes toward one axial direction compared to the second electrode 4 and the separator 3. When a plurality of first electrode tabs 23 are provided, they may overlap with each other to form a single electrically connected tab, thereby widening the current path and reducing resistance.
[0158] 9 is an enlarged cross-sectional view showing an electrode assembly according to an embodiment of the present invention in which the axial length of the first electrode is shorter than that of the second electrode. Referring to this figure, in particular, when the second electrode uncoated portion 41 is bent, the second electrode 4 and the first electrode may short-circuit with each other. In a typical jelly roll electrode assembly, such short-circuits can be prevented by making the separator 3 protrude in both axial directions from the first electrode 2 and the second electrode 4, but in a table-less structure such as the second electrode 4 side according to the embodiment of the present invention, the second electrode uncoated portion 41 protrudes in the other axial direction compared to the separator 3, making it difficult to prevent such short-circuits.
[0159] In order to solve the above-mentioned short circuit problem, the first electrode 2 may be formed to have an axial length shorter than that of the second electrode 4. As a result, the other axial end of the first electrode 2 is positioned deeper within the separator 3, and the separator 3 insulates between the second electrode uncoated portion 41 and the first electrode 2, thereby reducing the possibility of a short circuit occurring.
[0160] Fig. 10 is an enlarged cross-sectional view showing an electrode assembly according to an embodiment of the present invention in which the distance between one axial end of the regions coated with the active material of the first electrode and the second electrode in Fig. 9 is shorter than the distance between the other axial end of the regions. Referring to this, the distance between one axial end of the first electrode 2 and one axial end of the second electrode 4 may be shorter than the distance between the other axial end of the first electrode 2 and a position where the second electrode uncoated portion 41 of the second electrode 4 begins.
[0161] This is because the first electrode 2 has a tab structure, which reduces the risk of short circuiting, unlike a tabless structure. The first electrode 2 is not bent or pressed separately, and the first electrode tab 23 is insulated, so the risk of short circuiting is significantly lower than when the second electrode uncoated portion 41 is bent. Therefore, in the area where the first electrode tab 23 protrudes, the distance between the axial ends of the first electrode 2 and the second electrode 4 can be narrowed, thereby improving space utilization and increasing capacity.
[0162] In addition, in order to improve space utilization, the first electrode 2 may be provided so that its one axial end is positioned alongside or more inward than the one axial end of the second electrode 4, that is, its height is the same as or lower than the height of the one axial end of the second electrode 4. This is because, unlike the other axial end of the first electrode 2 being positioned relatively more inward than the other axial end of the second electrode 4 on the other axial side having the second electrode uncoated portion 41 to avoid short circuiting with the second electrode 4, there is little need to provide the one axial end of the second electrode 4 lower or further inward away from the one axial end of the first electrode 2, but by not protruding the end of the first electrode 2 toward the one axial side in this manner, space utilization can be improved and capacity can be increased.
[0163] According to an embodiment of the present invention, an electrode assembly is manufactured by winding an electrode stack, in which a first electrode 2, a separator 3, a second electrode 4, and a separator 3 are sequentially stacked, around a winding shaft in a winding direction (longitudinal direction). The first electrode 2 is a positive electrode, and the second electrode 4 is a negative electrode. When the first electrode 2 is divided along a width direction so as to be divided into four equal parts in the longitudinal direction, first electrode uncoated portions 21 are provided in two regions, one of which is provided in each region, excluding both longitudinal end regions. A first electrode tab 23 is electrically connected to each of the first electrode uncoated portions 21. The first electrode tab 23 protrudes to one side in the width direction (axial direction). The second electrode 4 is longer than the first electrode 2. The second electrode 4 is provided with second electrode uncoated portions 41 that are intermittently cut out in the longitudinal direction (winding direction) along the other width direction end. the second electrode uncoated portion 41 is exposed to the other width direction side of the second electrode 4, a height of one width direction end of the first electrode 2 in the electrode stack is the same as a height of one width direction end of the second electrode, the other axial end of the second electrode 4 and a separator 3 extend and protrude relatively to the other axial direction side compared to the other axial end of the first electrode 2, the axial length of the first electrode 2 is shorter than the axial length of the second electrode 4 and its center is located higher than the center of the second electrode 4, and after being wound up, the first electrode tabs 23 protrude to one axial direction side of the electrode assembly 1 and overlap each other to form one tab, the second electrode uncoated portion 41 is bent in a centripetal direction to form a flat surface, and a current collector plate 5 may be welded to the flat surface formed by bending the second electrode uncoated portion 41.
[0164] The present invention also provides a cylindrical battery cell structure including the improved electrode assembly.
[0165] FIG. 11 is a cross-sectional view of a cylindrical battery according to an embodiment of the present invention in which one axial side of an electrode assembly is covered with an insulating layer, and FIG. 12 is a cross-sectional view of a cylindrical battery according to an embodiment of the present invention in which only a portion of a first electrode tab is covered with an insulating layer.
[0166] 11, a cylindrical battery according to an embodiment of the present invention includes a battery can 6 having one side open in the axial direction, and the electrode assembly 1 may be manufactured by being housed in the battery can 6 such that the second electrode uncoated portion 41 faces a bottom surface 62 of the battery can 6. The second electrode uncoated portion 41 is electrically connected to the bottom surface 62 of the battery can, and at this time, a current collector 5 may be interposed between the second electrode uncoated portion 41 and the bottom surface 62 of the battery can. At this time, the second electrode uncoated portion 41 may be directly connected to the bottom surface 62 of the battery can without the current collector 5, thereby improving space utilization and increasing capacity.
[0167] A beading portion 64 that includes the side wall 61 of the battery can 6 on its inside is provided on one axial side of the battery can 6 in which the electrode assembly 1 is housed, in order to fix the battery can 6 on the electrode assembly 1. A battery can lid is provided on the beading portion 64, and is fixed to the battery can 6 by a crimping method with an insulating layer 65 interposed therebetween, and covers the open portion of one axial side of the battery can 6.
[0168] The first electrode tab 23 may protrude to one axial side of the electrode assembly 1 and be connected to the battery can lid 63 via a first electrode terminal 631. The first electrode terminal 631 may be provided separately and electrically connected to the lid 63, or may be provided as a part of the lid 63, or the lid 63 itself may be the first electrode terminal 631.
[0169] A thermal runaway prevention mechanism (CID; Current Interrupt Device) and / or a vent structure may be applied to the cover 63. The cover 63 may be electrically connected to the first electrode terminal 631 through the thermal runaway prevention mechanism (CID; Current Interrupt Device) and / or the vent structure.
[0170] At this time, one axial side of the electrode assembly 1 may be covered with an insulating layer 65 so as to protrude the first electrode tab.
[0171] 12, the insulating layer 65 may be provided to cover the area between the battery can lid 63 and the battery can 6, as well as the area where the first electrode tab 23 may interfere with the second electrode 4, preferably to cover the boundary area where the first electrode tab 23 protrudes from the jelly roll portion of the electrode assembly 1. This improves space utilization and increases capacity compared to a method of covering one side of the electrode assembly 1 entirely as in FIG. 11.
[0172] In a cylindrical battery cell according to an embodiment of the present invention, an electrode assembly 1 according to an embodiment of the present invention is accommodated in an open battery can at the top, with a second electrode uncoated portion 41 facing downward, the second electrode uncoated portion 41 being electrically connected to a bottom surface 62 of the battery can 6, the first electrode tab being electrically connected to a battery can lid 63 covering an upper portion of the battery can 6 via a first electrode terminal 631 provided on the battery can lid 63, and a portion of the first electrode tab 23 that may cause a short circuit with the second electrode 4 and a portion between the lid 63 and the battery can 6 may be covered with an insulating layer 65.
[0173] FIG. 13 illustrates a structure in which the second electrode uncoated portion 41 of the electrode assembly 1 is bent and overlapped and directly welded to the bottom surface 62 of the battery can 6, and two first electrode tabs 23 protrude in the axial direction at different radial positions and welded to a first electrode terminal 631.
[0174] The bottom surface 62 of the battery can 6 may have a structure that is slightly recessed from the lower end of the side wall 61 of the battery can 6. When such a recessed portion is welded to the second electrode uncoated portion 41, the welding may be performed by irradiating a laser onto the bottom surface of the bottom surface 62, and the recessed structure of the bottom surface 62 prevents such a welded portion from coming into contact with the ground and being damaged.
[0175] The first electrode terminal 631 may have a vent 633 structure that weakens the rigidity, such as a notch groove. Referring to Fig. 13, in comparison with Fig. 4, it can be seen that the energy density is further increased by providing a portion of the electrode assembly 1 where the active material is applied up to just before the beading portion 64.
[0176] The insulating layer 65 crimped together with the lid 63 extends in the axial direction and covers the inner circumference around the beading portion. Furthermore, the inner circumference surface of the insulating layer 65 guides the electrode tabs 23 to gather radially inward, and ensures that the electrode tabs 23 do not come into contact with the side wall 61 of the battery can 6.
[0177] The cylindrical battery can 6 can be filled with an electrolyte for the battery reaction. + B - The salt may have the structure: + Li + , Na + , K + and combinations of these cations. - F - , Cl - , Br - , I - , NO3 - , N(CN)2 - , BF4 - , ClO4 - , AlO4 - , AlCl4 - , PF6 - , SbF6 - , AsF6 - , BF2C2O4 - , BC4O8 - , (CF3)2PF4 - , (CF3)3PF3 - , (CF3)4PF2 - , (CF3)5PF - , (CF3)6P - , CF3SO3 - , C4F9SO3 - , CF3CF2SO3 - , (CF3SO2)2N -, (FSO2)2N - , CF3CF2(CF3)2CO - , (CF3SO2)2CH - , (SF5)3C - , (CF3SO2)3C - , CF3(CF2)7SO3 - , CF3 - , CH3CO2 - , SCN - , and (CF3CF2SO2)2N - The anion comprises at least one anion selected from the group consisting of:
[0178] The electrolyte can be dissolved in an organic solvent, such as propylene carbonate (PC), ethylene carbonate (EC), diethyl carbonate (DEC), dimethyl carbonate (DMC), dipropyl carbonate (DPC), dimethyl sulfoxide, acetonitrile, dimethoxyethane, diethoxyethane, tetrahydrofuran, N-methyl-2-pyrrolidone (NMP), ethyl methyl carbonate (EMC), gamma-butyrolactone, or a mixture thereof.
[0179] FIG. 14 shows another embodiment of the electrode assembly 1. As shown in FIG. 5 and FIG. 6, when the electrode tab 23 is connected to the region where the active material is applied in the axial direction, the thick electrode tab 23 makes the radial thickness of the jelly roll in the circumferential region where the electrode tab 23 is arranged thicker than other parts. According to the embodiment, in order to minimize the thickness deviation, a structure in which the multiple electrode tabs 23 are arranged at different positions in the circumferential direction is illustrated. When the multiple electrode tabs 23 are arranged at different positions in the circumferential direction, it is preferable to arrange them at substantially equal intervals in the circumferential direction. For example, when three electrode tabs 23 are provided as shown in the figure, the angle between them may be within or outside 120 degrees.
[0180] Of course, the radial distances at which the electrode tabs 23 are located from the center of the electrode assembly 1 may also be different from one another, as shown in the figure. The selection of the positions of the electrode tabs 23 has already been described with reference to Figures 5 and 6. The radial intervals between the electrode tabs 23 may become gradually smaller from the center to the centrifugal side. For example, if the radii of the electrode tabs located from the most centripetal side to the most centrifugal side are r1, r2, r3, and r4, they may have a relationship such as (r2-r1)>(r3-r2)>(r4-r3).
[0181] The electrode tabs 23 may be elastically deformed in the centripetal direction and may overlap each other in part. They may be welded to the cover 63 all at once or sequentially.
[0182] 15 to 19 show another embodiment of the electrode assembly 1. Referring to Fig. 15, a first electrode 2 has a first electrode uncoated portion 21 on one axial side where active material 22 is not applied. A plurality of first electrode tabs 23 are fixed to and electrically connected to the first electrode uncoated portion 21.
[0183] The second electrode 4 has a second electrode uncoated portion 41 on the other axial side where the active material 42 is not applied. The axial extension length of the second electrode uncoated portion 41 increases gradually or stepwise from the center to the centrifugal direction. The second electrode uncoated portion 41 may be formed in the shape of a notched tab, and the base end of the notched tab may be bent to lie in the radial direction.
[0184] Certain sections on the most centripetal side and the most distal side may not have a notched tab. The section without the notched tab is not bent. One turn on the distal side can be removed during the manufacturing process to prevent the notched tab from being deformed in an unexpected situation.
[0185] The first electrode tab 23 does not extend in the width direction (Y) to the area where the first electrode active material 22 is applied. Therefore, even when the first electrode 2, the second electrode 4, and the separator 3 are wound to form the electrode assembly 1, the first electrode tab 23 is not interposed in the area where the active materials 22, 42 are tightly attached in the radial direction. Therefore, even if the radius of the jelly roll repeatedly expands and contracts during charging and discharging, there is no area where excessive pressure is applied, and deterioration caused by this can be prevented.
[0186] 15 illustrates an example in which the first electrode uncoated portion 21 is provided in a form that extends long in the longitudinal direction. In this structure, if the first electrode uncoated portion 21 is too long, the risk of a short circuit increases, and if the first electrode uncoated portion 21 is too short, it is disadvantageous in ensuring a bonding area with the first electrode tab 23.
[0187] 16 discloses a structure in which the height of first electrode uncoated region 21 is made higher only in the section where first electrode tab 23 is coupled, and first electrode uncoated region 21 is kept short in other areas. By reducing the height of first electrode uncoated region 21 in this manner, it is possible to prevent first electrode uncoated region 21 from protruding further outward than separator 3.
[0188] In addition, as shown in FIG. 17, by removing the section to which the first electrode tab 23 is coupled as well as the first electrode uncoated portion 21, it is possible to maximize the area of the first electrode 2 that contributes to the capacitance.
[0189] In this manner, according to the structure in which the plurality of first electrode tabs 23 are connected to the first electrode non-coating portion 21 protruding toward one side in the axial direction, the first electrode tabs 23 can be arranged at positions that coincide with one another in the circumferential direction, as shown in Figures 18 and 19. Since the first electrode tabs 23 in the jelly roll are arranged at positions outside the active material coating layer anyway, there is no need to arrange them in a dispersed manner in the circumferential direction.
[0190] On the contrary, when they are arranged at substantially the same position in the circumferential direction, the plate-like first electrode tabs 23 are arranged substantially parallel to each other as shown in the figure, and therefore these can be bent side by side. Therefore, compared to the case where a plurality of first electrode tabs 23 are arranged dispersedly along the circumferential direction, both welding to the lid 63 and handling after welding the lid 63 are easy. In particular, although they are spaced apart from each other in the radial direction, they are arranged on the same radial line, so that the effect of reducing the internal resistance is still achieved.
[0191] In particular, the position at which the first electrode tab 23 should be provided is such that the first electrode uncoated portion 21 protrudes to one side in the axial direction, and the first electrode uncoated portion 21 is provided higher in a predetermined section as shown in Figures 16 and 17, or the first electrode uncoated portion 21 is provided only in a predetermined section but the first electrode uncoated portion 21 in that section protrudes to one side in the axial direction, and the section is set wide in consideration of the winding deviation. Then, after first winding the electrode assembly 1, the first electrode tab 23 can be brought into contact with and connected to the first electrode uncoated portion 21 protruding in the axial direction, thereby accurately aligning the circumferential position of the first electrode tab 23.
[0192] Furthermore, since the first electrode tabs 23 are concentrated in the smallest area while maintaining an appropriate radial spacing, the insulating layer 65 can be formed to include only that area, which provides various advantages, such as ease of installation of the insulating layer 65 and the ability to firmly contact the first electrode tabs 23 with the first electrode uncoated portion 21 via the insulating layer 65.
[0193] This multiple first electrode tab 23 structure can minimize the area of the cover 63 that must be left open for welding to the first electrode tabs 23, regardless of the application of multiple first electrode tabs 23, and the position can be determined to be a portion extending radially from one circumferential position (area indicated by dashed double-dashed lines in Figures 18 and 19), so it is convenient to apply a CID or vent to the cover 63 while connecting multiple first electrode tabs 23 to the cover 63.
[0194] Fig. 20 is a development view of the second electrode 4 in which the second electrode uncoated portion 41 is further coated with an insulating coating layer 44. Fig. 21 is an enlarged view of the second electrode uncoated portion 41 coated with the insulating coating layer of Fig. 20 after being wound up and folded.
[0195] The insulating coating layer 44 reinforces the rigidity of the vicinity of the base end of the second electrode uncoated portion 41. As a result, when the second electrode uncoated portion 41 receives a force in the axial direction from the second electrode current collector plate 52 or the bottom surface 62 of the battery can 6 in order to weld the second electrode uncoated portion 41, the base end of the second electrode uncoated portion 41 is likely not to buckle.
[0196] When the base end of the second electrode uncoated portion 41 is reinforced with an insulating coating layer 44, even if the base end of the second electrode uncoated portion 41 buckles, the second electrode uncoated portion 41 and the first electrode 2 do not come into direct contact with each other but come into contact with each other via the insulating coating layer 44, thereby preventing a short circuit from occurring between the first electrode 2 and the second electrode 4.
[0197] The insulating coating layer 44 provides bending resistance in a process of bending the second electrode uncoated portion 41 in a radial direction. As a result, when the second electrode uncoated portion 41 is bent in a radial direction, the section coated with the insulating coating layer 44 is hardly deformed, and deformation occurs mainly in the section not coated with the insulating coating layer 44.
[0198] The insulating coating layer 44 covers a predetermined section from a boundary between the coating portion of the second electrode active material 42 and the second electrode uncoated portion 41 toward an end of the second electrode uncoated portion 41. The insulating coating layer 44 starts inside the axial end of the separator 3 and extends further outward in the axial direction than the separator 3.
[0199] When the insulating coating layer 44 covers the boundary region between the coated portion of the second electrode active material 42 and the second electrode uncoated portion 41, it also covers a small section of the end of the coated portion of the second electrode active material 42. The region where the greatest deformation occurs due to buckling may be the boundary region between the coated portion of the second electrode active material 42 and the second electrode uncoated portion 41. The insulating coating layer 44 covers the small section of the end of the coated portion of the second electrode active material 42 at these boundary regions, thereby greatly increasing the buckling resistance of the boundary region between the coated portion of the second electrode active material 42 and the second electrode uncoated portion 41.
[0200] The insulating coating layer 44 may be coated to a constant thickness or may vary in thickness in the axial direction. In FIG. 21, the insulating coating layer 44 has a structure in which the thickness of the insulating coating layer 44 gradually increases in a glide section (a section where the thickness becomes thinner) formed at the end of the negative active material.
[0201] The thickness of the insulating coating layer 44 may be thinner than the thickness of the negative electrode active material layer. Thus, as shown in the figure, the coating portion of the second electrode active material 42 may be in close contact with the separator 3 in the radial direction, but the insulating coating layer 44 may be spaced apart from the separator 3 to some extent or may be in contact with the separator 3 but not in close contact.
[0202] As a result, even if an external force is applied to second electrode uncoated portion 41 and the base end of second electrode uncoated portion 41 is deformed during the process of bending second electrode uncoated portion 41 and during the process of welding second electrode current collector plate 52 to second electrode uncoated portion 41, not only can the amount of deformation be suppressed but also the deformation of the base end of second electrode uncoated portion 41 does not immediately affect separator 3. In other words, second electrode uncoated portion 41 has a section that does not affect separator 3 and is allowed to deform, the section being the distance between insulating coating layer 44 and separator 3.
[0203] Furthermore, when the insulating coating layer 44 is spaced apart from the separator 3, the heat generated in the process of welding the second electrode uncoated portion 41 to the second electrode current collector plate 52 or the bottom surface 62 of the battery can 6 is prevented from being directly conducted to the separator 3 via the insulating coating layer 44, thereby protecting the separator 3 from the welding heat. Furthermore, the insulating coating layer 44 can further shorten the axial protruding height of the separator 3, and therefore the distance from the position where the welding heat is generated to the axial end of the separator 3 can be further increased, thereby further increasing the effect of protecting the separator 3 from the welding heat.
[0204] Since the electrode assembly 1 is wound into a cylindrical shape, the insulating coating region of the second electrode uncoated portion 41 coated with the insulating coating layer 44 also has a cylindrical curved surface. The cylindrical curved surface has bending resistance due to its shape. According to the embodiment, since the insulating coating region has a thicker cylindrical curved surface, the insulating coating region provides higher bending resistance when the region provided on the upper part of the cylindrical curved surface is bent in the radial direction. As a result, bending is induced in the portion of the second electrode uncoated portion 41 that is not insulating coated.
[0205] In this case, since the insulating coating region provides a higher bending resistance, the thickness of the insulating coating layer 44 is thinner than the thickness of the negative electrode active material layer, and the surface of the insulating coating layer 44 is separated from the separator 3 in the radial direction, so that the bending resistance can be sufficiently exerted even if it is not supported by the separator 3.
[0206] The front end of the insulating coating layer 44 is coated to maintain a slight gap (G) with the folding portion (F) of the second electrode uncoated portion 41. This has the effect of inducing the second electrode uncoated portion 41 to fold at the folding portion (F). In addition, since the second electrode uncoated portion 41 deforms with a slight gap (G) from the insulating coating layer 44, it is possible to prevent the insulating coating layer 44 from being damaged by the folding process of the uncoated portion.
[0207] In this manner, the second electrode uncoated portion 41 including the insulating coating layer 44 can prevent buckling even when pressure is applied in the axial direction.
[0208] Fig. 22 is a perspective view showing a battery pack including a cylindrical battery cell according to the present invention, and Fig. 23 is a perspective view showing a vehicle including the battery pack of Fig. 22. Referring to these figures, the electrode assembly and cylindrical battery cell (C) according to the present invention can be applied to a battery pack (P) including the electrode assembly and cylindrical battery cell (C) and a vehicle (V) including the battery pack (P). The implementation of the battery pack (P) and the vehicle (V) is already known to those skilled in the art, and will not be described separately in this specification.
[0209] It should be understood that the above-described embodiments are illustrative in all respects and are not limiting, and the scope of the present invention is defined by the following claims rather than the above detailed description. Any modifications and variations that can be achieved within the meaning and scope of the following claims, as well as equivalent concepts, should be construed as being included in the scope of the present invention.
[0210] Although the present invention has been described above with reference to the illustrative drawings, the present invention is not limited to the embodiments and drawings disclosed in this specification, and it is obvious that various modifications can be made by those skilled in the art within the scope of the technical concept of the present invention. Furthermore, even if the effects of the configuration of the present invention are not explicitly described and explained while describing the embodiments of the present invention, it is natural that the effects that can be predicted by the configuration should also be recognized. [Explanation of symbols]
[0211] 1 Electrode assembly 2 1st electrode 21 First electrode (positive electrode) uncoated portion 22 First electrode (positive electrode) active material 23 First electrode (positive electrode) tab 3 Separation membrane 4 Second electrode (negative electrode) 41 Second electrode (negative electrode) uncoated area 42 Second electrode (negative electrode) active material 43 Second electrode (negative electrode) tab 44 Insulating coating layer 5 Current collector plate 51 First electrode (positive electrode) current collector 52 Second electrode (negative electrode) current collector 6 Battery Can 61 Side wall 62 Bottom 63 Battery Can Lid 631 1st electrode terminal 633 Vent 64 Beading section 65 Insulating Layer C Battery Cell P Battery pack V Automobile
Claims
1. A jelly roll electrode assembly in which a first electrode, a separator, a second electrode, and a separator are sequentially stacked and wound in a winding direction around a winding shaft, a first electrode tab electrically connected to the first electrode; and a second electrode uncoated portion provided on a portion of the second electrode and not coated with an active material; Including, The first electrode tab protrudes toward one side in the axial direction relative to the first electrode, the second electrode uncoated portion is exposed at the other axial end of the second electrode and serves as a tab; Electrode assembly.
2. The first electrode tab is provided in one or more. The electrode assembly of claim 1 .
3. Two or more of the first electrode tabs overlap each other to form one electrically connected tab. The electrode assembly according to claim 2 .
4. One of the first electrode tabs is connected to the first electrode at a position avoiding both ends of the first electrode in the winding direction. The electrode assembly according to claim 2 .
5. The two or more first electrode tabs are connected to the first electrode at positions avoiding both ends and a center portion of the first electrode in a winding direction. The electrode assembly according to claim 2 .
6. the first electrode tab is in contact with a first electrode uncoated portion that is not coated with an active material; The electrode assembly of claim 1 .
7. The first electrode uncoated portion is provided in a region corresponding to a region coated with an active material in an axial direction. The electrode assembly according to claim 6.
8. The first electrode uncoated portion is provided in a form that further extends axially outward from an axial end portion of the region coated with the active material. The electrode assembly according to claim 6.
9. The first electrode uncoated portion is provided over the entire length or a part of the length. The electrode assembly of claim 8.
10. The length of the first electrode uncoated portion extending outward in the axial direction is longer in a predetermined section including a portion where the first electrode tab contacts than in other sections. The electrode assembly of claim 8.
11. The first electrode tab is provided in a plurality of pieces, the first electrode tabs are disposed at different radial positions in a radial direction; 9. The electrode assembly according to claim 7 or 8.
12. The first electrode tab is provided in a plurality of pieces, The first electrode tabs are arranged at circumferential positions that do not overlap with each other. The electrode assembly of claim 7.
13. The first electrode tab is provided in a plurality of pieces, The circumferential positions at which the first electrode tabs are disposed at least partially overlap each other. The electrode assembly of claim 8.
14. The axial length of the first electrode is shorter than the axial length of the region of the second electrode coated with the active material and the separator. The electrode assembly of claim 1 .
15. The height of one axial end of the first electrode is the same as the height of one axial end of the second electrode, or is lower than the height of one axial end of the second electrode. The electrode assembly of claim 1 .
16. an axial distance between one axial end of the first electrode and one axial end of the second electrode is shorter than an axial distance between the other axial end of the first electrode and a point where an uncoated portion of the second electrode begins; 16. The electrode assembly of claim 15.
17. The second electrode uncoated portion has a shape in which the second electrode uncoated portion is continuously or intermittently cut out in the winding direction. The electrode assembly of claim 1 .
18. The second electrode uncoated portion has a height that protrudes in an axial direction and increases continuously or intermittently. The electrode assembly of claim 1 .
19. The second electrode uncoated portion is bent in a radial direction. The electrode assembly of claim 1 .
20. A current collector plate is coupled to the bent surface of the second electrode uncoated portion.
20. The electrode assembly of claim 19.
21. The electrode assembly according to any one of claims 1 to 20, Cylindrical battery.
22. a battery can that accommodates the electrode assembly such that one axial side surface is open and the second electrode uncoated portion faces a bottom; a battery can lid for covering the open top of the battery can with the electrode assembly housed in the battery can; and an insulating layer insulating the first electrode tab from the battery can and the axial end of the second electrode; Including, the first electrode tab is electrically connected to the battery can lid, The second electrode uncoated portion is electrically connected to a bottom surface of the battery can.
22. The cylindrical battery of claim 21.
23. A beading portion is provided on a side wall of the battery can, protruding radially inward to fix the electrode assembly from above and below. the insulating layer is disposed between the beading portion and the electrode assembly; 23. The cylindrical battery of claim 22.
24. the insulating layer covers one axial side of the electrode assembly, and the first electrode tab penetrates the insulating layer and protrudes to one axial side.
23. The cylindrical battery of claim 22.
25. The insulating layer is provided at each boundary portion between the first electrode tab, the second electrode, and the battery can.
23. The cylindrical battery of claim 22.
Citation Information
Patent Citations
JP1990119348U
Battery
JP1997035701A
Secondary battery
JP2006012834A
Battery cell design and assembly method
JP2010534916A
spiral lithium battery
JP3015663U