Diamond wafer-based electronic components and manufacturing methods

Single-crystal diamond wafers address the inefficiencies in power inverter architectures by providing superior thermal and electrical conductivity, enhancing energy efficiency and range in electric vehicles through reduced thermal impedance and improved thermal management.

JP2024543304AInactive Publication Date: 2024-11-21DIAMOND FOUNDRY INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024518770
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-12-10
Filing Date
2022-11-21
Publication Date
2024-11-21
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing power inverter architectures in electric vehicles face challenges in thermal and electrical conductivity, leading to significant power dissipation and inefficiencies, with current materials failing to meet the requirements for high thermal conductivity and electrical isolation, resulting in reduced energy efficiency and increased system failure.

Method used

The use of single-crystal diamond (SCD) wafers for power semiconductor devices, which provide extreme thermal conductivity and electrical insulation, reducing the thermal impedance and enabling a new thermal-electrical path configuration that closely aligns the semiconductor junction temperature with the coolant temperature, thereby minimizing conduction losses.

Benefits of technology

This configuration significantly reduces thermal impedance, enhances energy efficiency by up to 10%, increases the driving range by 5.33%, and lowers costs, while maintaining high reliability and scalability for electric mobility applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543304000001_ABST
    Figure 2024543304000001_ABST
Patent Text Reader

Abstract

Disclosed are electronic components, intermediate stages of production, and methods of manufacture that include a stack having a metal substrate, a single crystal diamond (SCD) wafer, and a metal layer. A first sintered metal layer forms a bond between the substrate and the SCD wafer, and a second sintered metal layer forms a bond between the SCD wafer and the metal layer. The metal layer is thinner than the metal substrate.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Benefit of priority This international application claims the benefit of priority to U.S. Provisional Patent Application No. 63 / 288,066, filed December 10, 2021, the contents of which are incorporated herein by reference in their entirety.

[0002] Aspects of the present disclosure relate to substrates for semiconductor devices. In particular, aspects of the present disclosure relate to diamond substrates for semiconductor devices. [Background technology]

[0003] Improving Energy Efficiency in EV Power Electronics

[0004] The bulk of the power inverter architecture consists of converting the DC voltage from the battery into a three-phase AC format compatible with electric traction motors. Currently, power conversion ranges from 50kW to 250kW (peak 400kW) depending on the model. In the coming years, MW systems will emerge (trucking industry, naval transport, and more importantly aviation e-mobility). Each phase requires two power switches mounted in a so-called "half-bridge" topology. During operation, the three phases shift through an angle of 120 degrees, so that at any given time two switches are simultaneously closed (ON) and the other four open (OFF).

[0005] To evaluate the efficiency of an inverter, the conduction losses are calculated from the voltage difference when the switches are closed multiplied by the current through the switches, of course multiplied by 6 (3 x 2 = 6 switches). The level of power loss generated is considerable, and designers have always tried to reduce it to extend the driving range or reduce the battery size. When designing a power traction inverter, several other considerations also become part of the equation, such as wire bond stress and capacitance, gate driver performance, overall system size and cost. So far, the rule of thumb to reduce power losses has been to use more silicon surface area or better heat sinks. Both approaches have significant drawbacks. By using more silicon switches, the power conduction losses are reduced, and therefore the power dissipation, as the "on" state current is shared among more switches. However, switching losses increase accordingly, especially in insulated gate bipolar transistors (IGBTs). The drawbacks are the exponential surface mounts used, the increasing number of weak links in the power path such as wire bonds, the differences between the dies, the increasing physical distances that lead to harmful parasitic inductances, and the difficulty of perfectly synchronizing each die to its companion die, ultimately leading to unnecessary complexity and reduced efficiency for the effort deployed. Moreover, cost considerations make this approach problematic.

[0006] Meanwhile, cooling strategies have been the subject of experimentation and research and development for years. Designers felt that, rather than focusing solely on silicon improvements, lowering the operating temperature of the die might lead to power efficiency, cost savings, and improved reliability. That intuition is certainly correct, but the materials currently available to guarantee satisfactory results are much harder to come by.

[0007] Because the electrical and thermal paths in power silicon are identical and both are of significant size, it is extremely difficult to literally disconnect them in order to manage the thermal path to the liquid coolant, which must be electrically isolated for safety reasons, and the electrical path, which must be as short and robust as possible. The disconnection mechanism (the "dielectric") is achieved by the techniques and technologies shown in Figures 1A-1C, which have evolved very little over the past 40 years and have provided poor results despite their large-scale adoption.

[0008] FIG. 2 shows a general architecture of a power device. In general, the device includes a silicon die 201 attached to a copper layout 203 by an attachment 202, and thermally coupled to a coolant 206 through a substrate 204 and a dielectric material 205. Current flows primarily laterally in the copper layout 203, but primarily vertically from the die 201 through the attachment 202, layout 203, substrate 204, and dielectric 205. Such an architecture is characterized by relatively poor two-dimensional vector thermal conduction in the thermal path between the silicon die 201 and the coolant 206. For example, if the temperature of the coolant 206 is about 80°C, the temperature of the die 201 will typically be 175-200°C due to the thermal impedances in the thermal path. The general architecture of FIG. 2 can be broken down by a simplified thermal impedance (Rth) model shown in FIG. 3A and summarized in the table shown in FIG. 3B.

[0009] FIG. 3 shows that the thermal impedance (Rth) between the die 201 and the coolant 206 is distributed into three main categories. 1) Dielectric material 205 (Rth4): The dielectric material must have a wide range of performance and characteristics to ensure the highest thermal conductivity to achieve the automotive insulation requirements of about 4 kV for 1 minute, and therefore the thickness Rth of the material is determined. 2) Substrate and Mechatronics (Rth2, Rth6, Rth8): The substrate provides mechanical robustness and die mounting, as well as providing thermal continuity to the coolant through the inverter system (mechatronics) via the exposed surface. 3) Surface joints are the junctions of different elements attached together and can be classified into three main groups: a) Soldered or sintered diffusion (Rth1) provides the best thermal conductivity depending on the material used, interface thickness and thermal conductivity. b) Deposition coatings of ceramics onto metals (e.g., Al2O3 flame spray coatings) inducing a material-material interface with its own Rth (Rth3, Rth5) depending on the porosity and permeability. c) Pressure contact (Rth7) where two surfaces are pressed together creating a thermal path (and often an electrical path as well). This type of interface is highly dependent on the applied pressure, coplanarity, surface roughness and shape. Performance is usually poor and degrades over time.

[0010] Although counterintuitive, liquid to solid surface contact (Rth8) is part of this category, but can be more stable and of better quality / performance depending on the strategy employed. Laminar flow over a flat surface is less efficient since only a few molecules of the coolant surface in contact with the solid surface carry the calories to be extracted. The remaining liquid does not actively participate in cooling. Turbulent flow creates a larger surface contact area and more carriers, but requires special mechanisms to be implemented (i.e. thin fins) which leads to increased material usage and system volume. As stated above, the total bond Rth to the coolant is a conglomerate of material properties, technology, and surface area, rather than a single dimensional problem. There is considerable room for progress.

[0011] Advances in power inverters have been slow and incremental due to complex design and manufacturing exacerbated by custom subsystem requirements, advanced integration of high power electronics, material science, mechatronics, and thermal management. Power density is certainly a key indicator of modern power inverter performance, indicative of technology and efficiency. For reference, state-of-the-art designs show 33kW / L (Tesla Model 3 is 12L, 4.8kg, 400kW), and 36kW / L (Audi e-Tron is 5.5L, 8kg, 200kW).

[0012] Power semiconductors are fundamentally driven by two factors: thermal conductivity, which is the path for cooling, and electrical conductivity, which is the path for carrying high currents. While the electrical path has been researched for many years with more or less success, the thermal path has always been the main challenge.

[0013] In addition to the need for high thermal and electrical conductivity, power semiconductors carry high voltages and therefore need to be insulated from the rest of the environment. This is a safety requirement. Voltage isolation barriers (such as DBC substrates) typically have poor thermal conductivity. Common isolation barriers such as high thermal conductivity compounds exhibit thermal conductivity of 2-5 W / mK. State-of-the-art oxides such as aluminum oxide (Al2O3) exhibit thermal conductivity of 24-28 W / mK. More modern aluminum nitride (AlN) offers a realistic thermal conductivity of 150-180 W / mK. Therefore, for these materials, the thickness required to ensure electrical isolation creates a significant and undesirable thermal difference between the semiconductor junction temperature (Tj) and the cooling mechanism (usually liquid glycol).

[0014] Power semiconductors such as silicon insulated gate bipolar transistors (Si IGBTs) and silicon carbide metal oxide semiconductor field effect transistors (SiC MOSFETs) have the same electrical and thermal paths through the bottom surface, unlike other power dissipation devices such as MCUs, logic, memory, and DSP chips. The current most common solution to ensure electrical insulation and high current carrying capacity for Si IGBTs and SiC MOSFETs is the direct bonded copper (DBC) substrate. Unfortunately, it does not provide high heat transfer capacity.

[0015] It is within this context that aspects of the present disclosure arise. [Brief description of the drawings]

[0016] The teachings of the present disclosure can be readily understood by considering the following detailed description in conjunction with the accompanying drawings.

[0017] [Figure 1] 1A-1C are thermal profiles and side views of different wafer types showing the general impact of adding diamond to power electronics in prior art implementations. [Diagram 2] FIG. 1 is a cross-sectional view of a prior art electrical / thermal path in a power device. [Figure 3A] 1 is a thermal impedance Rth model representation of a prior art electrical / thermal path in a power device. [Figure 3B] 1 is a table containing relevant values ​​for calculation of thermal impedance for an exemplary prior art electrical / thermal path in a power device. [Figure 4A] 1 is a line graph illustrating normalized on-resistance (RdsON) versus temperature for a typical silicon carbide (SiC) power device. [Figure 4B] 1 is a line graph showing collector-emitter saturation voltage (VCE(sat)) versus temperature for a typical IGBT device. [Diagram 5]1 is a table of power conduction losses for a three-phase 250kW inverter system converted to a standard EV sedan range according to current power device standards. [Figure 6] FIG. 1 is a cross-sectional view of an improved thermal-electrical pathway power device according to an aspect of the present disclosure. [Figure 7] 1 is a thermal impedance (Rth) model representation of an improved electrical / thermal path power device according to an embodiment of the present disclosure. [Figure 8] 1 is a table containing relevant values ​​for calculation of thermal impedance for an exemplary improved electrical / thermal path power device. [Figure 9] FIG. 1 is a diagram of a metal-based substrate used in the fabrication of a single crystal diamond substrate for silicon transistors according to an aspect of the present disclosure. [Figure 10] FIG. 1 illustrates the alignment of a metal-based substrate on a metal-based substrate assembly during the fabrication of a single crystal diamond substrate for silicon transistors according to an aspect of the present disclosure. [Figure 11] FIG. 1 illustrates the placement of a first stencil and sinter paste on a metal-based substrate during the fabrication of a single crystal diamond substrate for silicon transistors according to an embodiment of the present disclosure. [Figure 12] FIG. 1 illustrates the addition of a single crystal diamond wafer on top of a sintering paste during the fabrication of a single crystal diamond substrate for silicon transistors according to an aspect of the present disclosure. [Figure 13] FIG. 13 illustrates the arrangement of a second stencil and a second sinter paste layer applied on top of a single crystal diamond wafer during the fabrication of a single crystal diamond substrate for silicon transistors according to an embodiment of the present disclosure. [Figure 14] FIG. 1 illustrates the placement of a thin metal layer on top of a second sinter paste layer of a single crystal diamond wafer during the fabrication of a single crystal diamond substrate for silicon transistors according to an embodiment of the present disclosure. [Figure 15] FIG. 1 illustrates sintering of an assembly stack using a sintering press during the fabrication of a single crystal diamond substrate for silicon transistors according to an aspect of the present disclosure. [Figure 16]FIG. 1 illustrates the sintering press and removal of the sintering dye leaving the completed SCD component during the fabrication of a single crystal diamond substrate for silicon transistors according to an embodiment of the present disclosure. [Figure 17] FIG. 1 illustrates the removal of an SCD component from a dam bar during the fabrication of a single crystal diamond substrate for silicon transistors according to an embodiment of the present disclosure. [Figure 18] 1A-1D illustrate etching of SCD components during fabrication of a device package according to an embodiment of the present disclosure. [Figure 19] 13A-13D illustrate removal of SCD components from dam bars and application of sinter paste during fabrication of a device package according to an embodiment of the present disclosure. [Figure 20] 1 illustrates sintering of metal bus bars to SCD components during fabrication of a device package according to an embodiment of the present disclosure. [Figure 21] 1 illustrates a silicon device sintered to an SCD component during fabrication of a device package according to an embodiment of the present disclosure. [Figure 22] 1 illustrates bond wires conductively coupling a silicon device to a metal bus bar during fabrication of a device package according to aspects of the present disclosure. [Figure 23] 1A-1C illustrate a potting die formed to fit the SCD components, bus bars, and silicon device assembly during fabrication of a device package according to an embodiment of the present disclosure. [Figure 24] A diagram showing the SCD component, bus bar, and silicon device assembly placed within a potting die and aligned via alignment pets within the potting die during fabrication of a device package according to an embodiment of the present disclosure. [Diagram 25] FIG. 1 illustrates a completed pot-shaped device package according to an aspect of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Although the following detailed description contains many specific details for purposes of explanation, those skilled in the art will appreciate that many variations and modifications to the following details are within the scope of the invention. Accordingly, the exemplary embodiments of the invention described below are set forth without any loss of generality to, and without imposing limitations on, the claimed invention. introduction overview

[0019] Power electronics in electric vehicles (EVs) are becoming increasingly heat dissipation limited, with available materials restricting the potential scope of electronics architectures. Thermal stresses induced in power semiconductor switches have presented a challenging problem for semiconductor and inverter companies. Engineers across the industry have been stuck using materials in electronics designs that do not truly meet the properties required for EV power electronics advancements, particularly materials that combine extreme thermal conductivity with extreme voltage insulation.

[0020] Single crystal diamond (SCD) is the most extreme material in several dimensions, each critical in its own right, due in particular to its combination of extreme thermal conductivity and extreme electrical insulation. SCD exhibits remarkable dielectric properties, including a low dielectric constant of 5.7, a loss tangent below 0.0001 at 35 GHz, and a high dielectric strength of 10 MV / cm. It is a material that is extremely thin, with a thickness of 20 μm (2×10 -5 This means that an SCD with 1.5 mm in diameter can insulate 20 kV and at the same time achieve a high thermal conductivity of 3,000 W / mK.

[0021] Diamond Foundry, Inc. of South San Francisco, Calif., has achieved production of wafer-sized single crystal diamonds covering the die sizes required by commercially relevant computer and power electronics chips. The power traction inverter dilemma

[0022] The Power Traction Inverter (PTI) in EVs is a critical element of electric mobility. Due to its level of complexity, electrical and thermal stress, and cost, the PTI has always been one of the weakest links in electric mobility implementation, with notable levels of failure in the early development of this emerging market, certainly creating a technical barrier to entry for OEM adoption. Driving conditions and driving style often induce significant electrical and thermal stresses on the inverter's active components and its surrounding elements which, if not properly addressed, will dramatically shorten their lifespan and ultimately lead to system failure.

[0023] Advances in power inverters have been slow and incremental due to complex design and manufacturing exacerbated by custom subsystem requirements, advanced integration of high power electronics, material science, mechatronics, and thermal management. Power density is certainly a key indicator of modern power inverter performance, indicative of technology and efficiency. For reference, state-of-the-art designs show 33kW / L (Tesla Model 3 is 12L, 4.8kg, 400kW), and 36kW / L (Audi e-Tron is 5.5L, 8kg, 200kW).

[0024] Power semiconductors are fundamentally driven by two factors: thermal conductivity, which is the path for cooling, and electrical conductivity, which is the path for carrying high currents. While the electrical path has been researched for many years with more or less success, the thermal path has always been the main challenge.

[0025] In addition to the need for high thermal and electrical conductivity, power semiconductors carry high voltages and therefore need to be electrically isolated from the rest of the environment. This is a safety requirement. Unfortunately, voltage isolation barriers (such as DBC substrates) typically have poor thermal conductivity. Common isolation barriers such as high thermal conductivity compounds exhibit 2-5 W / mK, state-of-the-art oxides such as aluminum oxide (Al2O3) exhibit 24-28 W / mK, and more modern aluminum nitride (AlN) realistically provides 150-180 W / mK, thus maintaining a significant undesirable thermal difference between the semiconductor junction temperature (Tj) and the cooling mechanism (usually liquid glycol) at the thickness required to ensure electrical isolation.

[0026] Power semiconductors such as silicon insulated gate bipolar transistors (Si IGBTs) and silicon carbide metal oxide semiconductor field effect transistors (SiC MOSFETs) have the same electrical and thermal paths through the bottom surface, unlike other power dissipation devices such as MCUs, logic, memory, and DSP chips. The current most common solution to ensure electrical insulation and high current carrying capacity for Si IGBTs and SiC MOSFETs is the direct bonded copper (DBC) substrate. Unfortunately, it does not provide high heat transfer capacity. Diamond-Based Power Electronics

[0027] Diamond and diamond-based solutions have always held a key position among power semiconductor developers due to their exceptional properties. They exhibit ultra-high thermal conductivity and an ultra-high band gap, properties that some call the "holy grail" for semiconductor applications. Unlike graphene (another allotrope of carbon), which is electrically conductive, diamond is an excellent insulator. Diamond Foundry now offers a practical, affordable solution to a very old problem: how to efficiently implement a cooling path to power semiconductors and ensure dielectric isolation at the same time.

[0028] The advantages of diamond have been well known for some time, so in fact this is neither surprising nor new. What is new and disruptive is that Diamond Foundry has achieved a) producing high quality single crystal diamond wafers for any chip die size, b) reducing the cost to the levels required for automotive power electronics, and c) new power electronics architectures that take full advantage of the capabilities of the new diamond wafers.

[0029] Previous work by our team and others has shown that diamond can reduce the peak temperatures of various semiconductors by as much as 20%, and that such reduction translates into a 10% increase in power efficiency during such periods.

[0030] SCD wafers are made of direct bonded copper ( DBC SCD wafers can be used in multiple ways, such as replacing ceramics (such as aluminum oxide (Al2O3), aluminum nitride (AlN), silicon nitride (Si3N4)) in silicon-based (SiC) substrates, replacing heat spreaders in novel discrete packages, and allowing for thinner semiconductor wafers. SCD wafers enable size, weight, and cost reductions in inverters based on any semiconductor technology, without having to "bet" on a new form of semiconductor gaining commercial traction. The Importance of Maintaining Lower Junction Temperatures

[0031] Thermal stresses induced in power semiconductor switches result in failures and reduced energy efficiency. As a general rule of thumb, the semiconductor life expectancy is halved for every 10°C increase in temperature, setting a trend towards silicon designs that can withstand higher temperatures, for example from 175°C to 200°C for silicon carbide power switches. ce(sat) Unlike IGBTs, which have a temperature coefficient, the RdsON of MOSFETs (including SiC) is a positive temperature dependent parameter (TDP), which means that the RdsON increases with temperature.

[0032] Figure 4A shows the normalized RdsON for a typical SiC device. A typical RdsON is specified to be 1 (e.g., 7 mOhm) at 25°C, so it increases by 45% (10.39 mOhm) at 150°C, 64% (11.64 mOhm) at 175°C, and 90% (12.87 mOhm) at 200°C. The increase in RdsON vs. Tj is split into a linear region (25-150°C) and an exponential region (150-200°C), which means that for the same current (400A), the power conduction loss is 1120W at 25°C, 1359W at 100°C, 1662W at 150°C, 1863W at 175°C, and 2060W at 200°C.

[0033] Figure 4B shows the V ce(sat) The conduction losses at 400A are established at 800W at 25°C, 920W at 125°C and 1000W at 150°C (no further data available). At the inverter frequency operation of EVs (e.g. 15kHz), the conduction losses represent about 60% of the cumulative conduction switching losses of the device. This is mainly due to the so-called "tail effect" of IGBTs, which is directly related to the surface area of ​​the silicon chip: the larger the surface area, the higher the switching losses. The total cumulative conduction and switching losses of the IGBTs are 1375W at 25°C, 1580W at 125°C and 1720W at 150°C. Despite the negligible efficiency advantage of SiC over IGBTs, it is noteworthy that even with the cost advantage of SiC vs IGBTs (about 5x), the trend towards SiC adoption seems irreversible, confirming that implementation costs are being compromised in favor of improved performance and range of EVs.

[0034] Since the on-board coolant temperature for EVs is typically set at 80°C, the challenge here is to get Tj as close as possible to the coolant, eliminating the unnecessary conduction losses induced by Tj in the exponential and part of the linear region of SiC, and allowing for a reduction in the die surface area of ​​the IGBT. Bipolar structures such as IGBTs are fairly resilient with respect to forward current, unless a temperature-dependent latch-up condition is triggered. Typically, 1000A / cm 2The current density up to 1000 MHz sets a limit, and IGBT manufacturers are typically allowed to stay within 80% to 90% of this limit over the temperature range. Mastering the IGBT junction temperature under latch-up conditions allows for a significant reduction in the active area of ​​the die size, which proportionately impacts the switching losses IGBTs have suffered since their inception. With proper application of thermal management solutions such as Diamond Foundry's solution, modern SiC and older IGBT technologies can become equivalent at one-fifth the cost in the e-mobility frequency switching range (10-20 kHz). Specific impacts on EV driving range

[0035] Figure 5 summarises the power conduction losses of a three-phase 250kW inverter system converted to a standard EV sedan range according to current standards. Losses with a current of 400A per phase (peak 565A) are investigated over a Tj range of 80°C (coolant) to 200°C.

[0036] The "Inverter Power Loss Saved" column shows the energy saved from the battery at various Tj, the range is calculated from the battery capacity accordingly. Assuming that the power switch Tj can be kept close to the coolant temperature (80°C), the total power loss savings can reach up to 2812W per battery charge, or 11.72 miles, or a range increase of 5.33%.

[0037] The study is conservative in that it does not take into account regenerative power savings, estimated at 15-20% of these figures. This includes the temperature dependence of power losses in the fast recovery diodes (FRDs) associated with IGBTs, the heat-dependent losses of the SiC MOSFET built-in diodes (which perform less well over temperature), and the reduction of associated circuitry such as gate drivers and ancillary components. A size reduction of such proportions opens the possibility for a directly integrated inverter motor to eliminate the power losses in cable lengths and terminals that take up yet another fraction of the battery capacity. Single Form Factor Architecture for EV Power Electronics

[0038] The combination of the incredible thermal conductivity, voltage insulation and wafer finish properties of single crystal diamond wafers now available from Diamond Foundry enables new device and system designs, as well as more efficient assembly processes, that the industry has not yet had a chance to pursue with GaN, SiC and IGBT silicon chips.

[0039] In particular, Diamond Foundry's SCD wafers will enable single form factor power inverters to exceed 1000kW / L (e.g., 400kW for a 0.4L system), improving system efficiency, reducing losses and system costs, leading to energy savings and extended range for electric mobility.

[0040] A new thermal management configuration according to an embodiment of the present disclosure is shown in FIG. 6. This configuration significantly reduces the number of thermal impedance elements from nine to four. In this configuration, a semiconductor die 601 is attached to a copper substrate 603 by silver attachments 602. The copper substrate 602 is diffusion bonded to a SCD wafer 607. The diffusion process used for attachment between a simplified number of elements that make up the thermal path is now scaled down to the nanometer scale, ensuring free thermal conduction from the semiconductor die 1 through the diamond tip 607 to the coolant 606. The use of the SCD wafer 607 allows for a more three-dimensional thermal conduction, as indicated by the dashed arrows.

[0041] One or more pressurized coolant jets 608 deliver coolant 606 to the exposed surface of the diamond wafer 607, providing a normal impingement flow that results in superior performance over laminar, turbulent, or turbulent "thin fin" solutions. The corresponding thermal impedance model shown in Figure 7, and the table shown in Figure 8 summarize these advantages.

[0042] Due to the significant reduction in total Rth (0.0155 compared to the state of the art value of about 0.11), the Tj of the silicon die is now closely related to the coolant temperature in the lockdown position, forming a Tj "clamp" of about 12°C above the coolant, allowing significant savings in conduction losses compared to the one described with reference to Figure 5, optimizing the mechanical geometry of the inverter design and reducing the required active silicon die surface.

[0043] Advanced materials and thermal management techniques in configurations such as those in Figure 6 dramatically reduce thermal impedance and shrink inverter size, paving the way for significantly increased EV range, lower costs, and extremely high reliability. Furthermore, the technology is scalable and adaptable to similar markets where high power efficiency and reliability are mission critical (i.e. power generation, charging stations, grid balancing, etc.). Fabrication of single crystal diamond substrates for silicon transistors

[0044] Single crystal diamond substrates for silicon devices may improve thermal conduction. Formation of a single crystal diamond substrate begins with a metal substrate 901 as shown in FIG. 9. The metal substrate 901 may be any suitable metal or metal alloy, such as copper, aluminum, silver, gold, nickel, iron, etc. As shown in the figure, the metal substrate may be included in a fabrication assembly with alignment holes 902 along a dam bar D that may be used to fabricate multiple copper substrates 901 at once. Notches 903 separate each metal substrate 901 for ease of separation. As an example, the metal substrate may be made of copper with a thickness of 0.590 mm to 1 mm, more preferably 0.6 mm thick.

[0045] 10, a metal substrate assembly 1001 may be attached to an assembly die 1002. The assembly die 1002 may include alignment pegs 1003. Each alignment peg 1003 may be configured to fit into an alignment hole 1004 in the metal substrate assembly 1001.

[0046] FIG. 11 shows that a first stencil 1102 can be added on top of the metal substrate 1101 to aid in the application of the first layer of sinter paste 1103. The sinter paste 1103 generally includes metal particles in a binder. By way of example and not limitation, the sinter paste 1103 may be a silver sinter paste. Alignment pegs 1104 assist in aligning the stencil with the metal substrate, using alignment holes also present in the stencil 1102. The first stencil 1102 ensures that the first layer of sinter paste 303 is properly positioned on the substrate 1101. The first layer of sinter paste 1103 may be 70-90 micrometers thick before sintering.

[0047] In FIG. 12, a single crystal diamond wafer (SCD) 1203 is added on top of the first layer of sinter paste 1103. A first stencil 1202 ensures that the SCD 1203 is properly aligned on top of the sinter paste and metal substrate 1201. The thickness of the SCD is between 50 and 1000 micrometers (5×10 5 m~1×10 -3 m), preferably 300 micrometers (3×10 -4 In one implementation, the SCD wafer is 18 millimeters long by 18 millimeters wide (1.8×10 -2 m×1.8×10 -2 m).

[0048] A second layer of sinter paste 1301 is then applied over the SCD layer using the first stencil to align the application, as shown in Figure 13. A second stencil 1302 is then placed over the first stencil and aligned using alignment pegs. The thickness of the second layer of sinter paste 1301 can be 70-90 micrometers.

[0049] A thin metal layout layer 1401 is applied over the second layer of sinter paste to create the SCD component assembly stack as shown in FIG. 14. The thin metal layout layer may be comprised of a thin layer of, for example, but not limited to, copper, gold, silver, or aluminum. A second template 1402 aligns the thin metal layout layer 1401 in the proper orientation over the second layer of sinter paste. The thickness of the thin metal layout layer is between 30 and 300 micrometers (3×10 -5 ~3×10 -4 m) thick, nominally 100 micrometers (1×10 4 The thickness is (mm).

[0050] As shown in FIG. 15, a sintered press insert 1501 is placed over the thin metal layout layer and the second stencil 1502. The sintered press insert 1501 includes protrusions configured to fit into holes in the second stencil 1502. The protrusions are configured to lie flat against the thin metal layout layer in the holes in the second stencil 1502. The sintered press insert 1501 also includes a cut out area to accommodate the second stencil 1502 when a force is applied to the sintered press insert and the protrusions are forced into the holes in the second stencil 1502.

[0051] The assembly stack is then sintered. Pressure 1503 is applied to the sinter press insert and assembly die 1505. While pressure 1503 is being applied, the entire assembly is heated 1504 at a pressure, temperature, and time sufficient to bond the sinter paste to the thin metal layout layer and the SCD layer, and to bond the metal substrate to the SCD layer. In one exemplary implementation, the pressure applied between the sinter press insert 1501 and the assembly die 1501 can be approximately 16 megapascals while a sinter press platter heated at 230 degrees Celsius heats the assembly for 6 minutes. After the application of pressure and heat, the sinter paste shall be bonded to the SCD layer, the metal substrate layer, and the thin metal layout layer. The final thickness of each sinter paste layer can be on the order of 6-10 micrometers.

[0052] Finally, the sinter press insert, stencil, and assembly die are removed leaving the completed SCD substrate component 1601, as shown in Figure 16. Dam bars with alignment holes can be used to fabricate multiple SCD substrate components at once.

[0053] 17 shows that after sintering and removing the assembly die, each SCD substrate component can be removed from the dam bar. Removal of the SCD substrate parts from the dam bar can be accomplished by any removal means, such as cutting or stamping. As shown, some implementations of the SCD substrate components can be made without a dam bar, and instead the assembly die 1704 includes a notch 1703 for aligning the copper substrate layer to the assembly die 1704. SCD Substrate Component Integrated Device Package:

[0054] The SCD substrate component can be further integrated into a silicon device package to improve cooling of the silicon device. As shown in FIG. 18, the SCD substrate component 1801 can be masked 1802 onto the thin metal layout layer with a patterned etch mask to bond the SCD substrate component to the semiconductor device. The etch mask can be any etch mask material known in the art, such as a photolithography mask, a mechanically applied mask, etc. The SCD substrate component 1801 with the patterned mask 1802 can then be etched. The etchant can be selective to the thin metal layout layer on the surface of the SCD substrate device, such as, for example, but not limited to, ferric chloride, nitric acid, hydrochloric acid, aluminum hydroxide, etc.

[0055] 19 shows that the etched SCD component device 1901 is removed from the dam bar and prepared for integration into a device package. Sinter paste 1902 may be spread over the area above the etched surface of the component device.

[0056] As shown in Figure 20, a metal bus bar 2002 is placed on the sinter paste on the etched surface of the SCD component device 2001. Sufficient pressure 2003 and heat 2004 are applied to the bus bar and SCD component assembly for a sufficient time to sinter the bus bar into the SCD component device using the sinter paste. For example, but not limited to, the bus bar and SCD component assembly may be subjected to approximately 16 megapascals of pressure via a heated vice or press at 230°C for 6 minutes to sinter the device. Once complete, the metal bus bar 2002 may be bonded to the etched surface of the SCD component device 2001.

[0057] Next, as shown in FIG. 21, one or more silicon devices 2102, such as, for example, but not limited to, MOSFETs, integrated gate bipolar transistors, resistors, diodes, or other types of transistors, may be sintered to the etched surface of the SCD component 2101. The silicon devices 2102 may be placed on a sintering paste, such as a silver sintering paste, that has been applied to the etched surface of the SCD component 2101. As shown, multiple silicon devices 2102 may be sintered to the surface of the SCD component at once with sufficient pressure and heat to bond the sintering paste to the etched surface of the silicon devices and SCD component. For example, but not limited to, a pressure of about 16 megapascals may be applied to the silicon devices and SCD component via a vice or press while being heated in an oven at 230° C. for 6 minutes to sinter the silicon devices to the SCD component.

[0058] 22, bond wires 2202 may then be formed to attach the silicon device 2203 to a portion of the SCD component 2201. The bond wires 2202 may be formed by any known method, such as, for example, but not limited to, ball bonding, wedge bonding, or compliant bonding.

[0059] A potting die can be fabricated to fit the SCD-substrate-component-integrated assembly, as shown in Figure 23. The potting die can include a number of alignment pins to properly position the SCD-substrate-component-integrated assembly in the potting die. The alignment pins can fit into screw holes or other alignment holes in the SCD components or bus bars.

[0060] The SCD substrate component integrated assembly 2402 is then placed into the potting die 2401 using alignment pins 2403 to ensure proper alignment, as shown in Figure 24. A potting compound solution is poured over the SCD substrate component integrated assembly and allowed to cure. The compound solution may be, for example, but not limited to, epoxy potting compound, silicone potting compound, urethane potting compound, polyacrylate potting compound, potting gel, etc.

[0061] Once the potting compound has cured, the SCD substrate component integrated device shown in Figure 25 can be removed from the potting die. The SCD substrate component integrated device is now complete and can be used in other devices. The SCD substrate allows for superior cooling of the integrated device because single crystal diamond provides excellent thermal conductivity and the small cross section created by sintering allows for even improved thermal coupling.

[0062] While the above is a complete description of the preferred embodiment of the present invention, various alternatives, modifications, and equivalents can be used. The scope of the invention should therefore not be determined with reference to the above description, but instead with reference to the appended claims, along with their full scope of equivalents. Any feature described herein, whether preferred or not, may be combined with any other feature described herein, whether preferred or not. In the following claims, the indefinite article "A" or "An" refers to a quantity of one or more items following the article, unless expressly stated otherwise. The appended claims are not to be construed as including means-plus-function limitations unless such limitations are expressly recited in a given claim using the phrase "means for."

Claims

1. 1. A method for manufacturing an electronic component, comprising: forming a stack having a metal substrate, a single crystal diamond (SCD) wafer, and a metal layer, a first layer of sintered metal paste between the substrate and the SCD wafer, and a second layer of sintered metal paste between the SCD wafer and the metal layer, the metal layer being thinner than the metal substrate; and applying heat and pressure to the stack for a time sufficient to sinter the first and second layers of metal sinter paste to bond the metal layer to the SCD wafer and the SCD wafer to the substrate.

2. The method of claim 1 , wherein the metal substrate is made of copper.

3. The method of claim 1 , wherein the metal layer is made of copper.

4. The method of claim 1 , wherein the metal substrate and the metal layer are both made of copper.

5. The method of claim 1 , wherein the first layer of metal sinter paste comprises a silver paste.

6. The method of claim 1 , wherein the second layer of metal sinter paste comprises silver paste.

7. The method of claim 1 , wherein the first and second layers of metal sinter paste both comprise silver sinter paste.

8. The method of claim 1 , wherein the metal substrate and the metal layer are both made of copper, and the first and second layers of metal sinter paste both comprise silver sinter paste.

9. An electronic component at an intermediate stage of manufacture, comprising:

1. An electronic component comprising: a stack having a metal substrate, a single crystal diamond (SCD) wafer, and a metal layer; a first layer of metal sinter paste between the substrate and the SCD wafer; and a second layer of metal sinter paste between the SCD wafer and the metal layer, the metal layer being thinner than the metal substrate.

10. The electronic component of claim 9 , wherein the substrate is made of copper.

11. The electronic component of claim 10, wherein the metal substrate has a thickness of about 0.5 mm to about 1 mm.

12. 10. The electronic component of claim 9, wherein the metal layer is made of copper.

13. The electronic component of claim 12, wherein the metal layer has a thickness of about 30 μm to about 300 μm.

14. 10. The electronic component of claim 9, wherein the metal substrate and the metal layer are both made of copper.

15. 10. The electronic component of claim 9, wherein the first layer of metal sinter paste comprises a silver sinter paste.

16. The electronic component of claim 15, wherein the first layer of metal sinter paste has a thickness of about 70 μm to about 90 μm.

17. 10. The electronic component of claim 9, wherein the second layer of metal sinter paste comprises a silver sinter paste.

18. 18. The electronic component of claim 17, wherein the second layer of metal sinter paste has a thickness of about 70 μm to about 90 μm.

19. 10. The electronic component of claim 9, wherein the first and second layers of metal sinter paste both comprise silver sinter paste.

20. 10. The electronic component of claim 9, wherein the metal substrate and the metal layer are both made of copper, and the first and second layers of metal sinter paste both comprise silver paste.

21. The electronic component of claim 9, wherein the SCD wafer has a thickness of about 50 μm to 1000 μm.

22. 22. The electronic component of claim 21, wherein said SCD wafer is approximately 18 mm long by approximately 18 mm wide.

23. a stack having a metal substrate, a single crystal diamond (SCD) wafer, and a metal layer, a first sintered metal layer forming a bond between the substrate and the SCD wafer, and a second sintered metal layer forming a bond between the SCD wafer and the metal layer, the metal layer being thinner than the metal substrate; Electronic components.

24. 24. The electronic component of claim 23, wherein the substrate is made of copper.

25. The electronic component of claim 24, wherein the metal substrate has a thickness of about 0.5 mm to about 1 mm.

26. 24. The electronic component of claim 23, wherein the metal layer is made of copper.

27. 27. The electronic component of claim 26, wherein the metal layer has a thickness of about 30 μm to about 300 μm.

28. 24. The electronic component of claim 23, wherein the metal substrate and the metal layer are both made of copper.

29. 25. The electronic component of claim 24, wherein the first sintered metal layer comprises silver.

30. 30. The electronic component of claim 29, wherein the first sintered metal layer has a thickness of about 6 μm to about 10 μm.

31. 24. The electronic component of claim 23, wherein the second sintered metal layer comprises silver.

32. 32. The electronic component of claim 31, wherein the second sintered metal layer has a thickness of about 6 μm to about 10 μm.

33. 24. The electronic component of claim 23, wherein the first and second sintered metal layers comprise silver.

34. 24. The electronic component of claim 23, wherein the metal substrate and the metal layer are both made of copper, and the first and second sintered metal layers both comprise silver.

35. The electronic component of claim 23, wherein the SCD wafer has a thickness of about 50 μm to 1000 μm.

36. 36. The electronic component of claim 35, wherein the SCD wafer is about 18 mm long by about 18 mm wide.