Pressure reducing devices, housings, battery cells, batteries and power consuming devices

A pressure reducing device with a controlled thickness-to-hardness ratio in its fragile region addresses safety concerns by timely pressure release during thermal runaway, enhancing battery cell safety and longevity.

JP2024543399AActive Publication Date: 2024-11-21CONTEMPORARY AMPEREX TECHNOLOGY (HONG KONG) LIMITED
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024527514
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2022-06-02
Publication Date
2024-11-21
Estimated Expiration
2042-06-02

AI Technical Summary

Technical Problem

Existing battery technologies face challenges in ensuring safety by effectively managing pressure during thermal runaway without compromising the service life of the battery cell.

Method used

A pressure reducing device with a weakened region that has a specific thickness-to-hardness ratio (5HBW/mm ≦ A/a ≦ 10000 HBW/mm) is implemented, ensuring the fragile region ruptures timely during thermal runaway while maintaining strength during normal use.

Benefits of technology

The solution extends the battery cell's service life and reduces the risk of fire or explosion by timely pressure release during thermal events.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543399000001_ABST
    Figure 2024543399000001_ABST
Patent Text Reader

Abstract

The embodiments of the present application provide a pressure reducing device, a housing, a battery cell, a battery, and a power consuming device, which belong to the technical field of batteries. The pressure reducing device is used in a battery cell, and a weak area for bursting when the battery cell releases pressure is partially formed in the pressure reducing device, the thickness of the weak area is a, the hardness of the weak area is A, and the ratio of the hardness of the weak area to the thickness of the weak area is set within a reasonable range, so that the weak area has sufficient strength during the normal use of the battery cell, and the pressure reducing device is not likely to burst at the position of the weak area, which not only can extend the service life of the battery cell, but also can timely reduce the pressure through the weak area when the battery cell experiences thermal runaway, which can reduce the risk of the battery cell catching fire or exploding, and improve the safety of the battery cell.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present application relates to the technical field of batteries, and in particular to pressure reducing devices, housings, battery cells, batteries and power consuming devices. [Background technology]

[0002] 2. Description of the Related Art With the development of new energy technology, batteries are being used more and more widely, for example in mobile phones, notebook computers, electric bicycles, electric cars, electric airplanes, electric propulsion boats, electric toy cars, electric toy boats, electric toy airplanes, and power tools.

[0003] A battery cell is an energy storage device that generally outputs electrical energy through a chemical reaction between an electrode assembly and an electrolyte. In the development of battery technology, in addition to improving the performance of battery cells, safety issues also need to be considered. Therefore, how to improve the safety of battery cells is an issue that needs to be resolved as soon as possible in battery technology. Summary of the Invention

[0004] The embodiments of the present application provide a pressure reducing device, a housing, a battery cell, a battery, and a power consuming device that can effectively solve the safety issues of the battery cell.

[0005] In a first aspect, an embodiment of the present application provides a pressure reducing device for use with a battery cell, in which a weak area is partially formed to rupture when the battery cell releases pressure, the thickness of the weak area being a, the hardness of the weak area being A, and satisfying 5 HBW / mm≦A / a≦10,000 HBW / mm.

[0006] In the above technical solution, not only the influence of the thickness of the weak area on the performance of the pressure relief device is considered, but also the influence of the hardness of the weak area on the performance of the pressure relief device is considered. By setting the ratio of the hardness of the weak area to the thickness of the weak area within a reasonable range, the weak area has sufficient strength during the normal use process of the battery cell, the pressure relief device is less likely to rupture at the position of the weak area, and not only can the service life of the battery cell be extended, but also when the battery cell undergoes thermal runaway, the pressure relief device can be depressurized in a timely manner by the weak area, reducing the risk of ignition and explosion of the battery cell and enhancing the safety of the battery cell.

[0007] In some embodiments, 190 HBW / mm ≤ A / a ≤ 4000 HBW / mm. In this way, while ensuring that the performance of the pressure relief device is better and the weak area has sufficient strength during the normal use process of the battery cell, it also ensures that when the battery cell undergoes thermal runaway, the weak area ruptures and depressurizes in a timely manner. On the premise of ensuring the safety of the battery cell, the service life of the battery cell is extended.

[0008] In some embodiments, 8 HBW ≤ A ≤ 200 HBW.

[0009] In some embodiments, 0.02 mm ≤ a ≤ 1.6 mm.

[0010] In some embodiments, the pressure relief device includes a non-weak area connected to the periphery of the weak area, the thickness of the non-weak area is b, and a < b is satisfied. By setting the thickness of the weak area to be smaller than that of the non-weak area, it is ensured that the weak area is more likely to rupture than the non-weak area, and when the battery cell undergoes thermal runaway, the pressure relief device ruptures and depressurizes at the position of the weak area.

[0011] In some embodiments, 0.05 ≤ a / b ≤ 0.95. By setting the ratio of the thickness of the weak area to the thickness of the non-weak area between 0.05 and 0.95, not only can the probability of the weak area rupturing during the normal use process of the battery cell be reduced, but also the probability of accidents such as ignition and explosion occurring when the battery cell undergoes thermal runaway can be reduced.

[0012] In some embodiments, 0.12 ≦ a / b ≦ 0.8.

[0013] In some embodiments, the hardness of the non-fragile region is B, satisfying B < A. The fact that the hardness of the fragile region is greater than that of the non-fragile region corresponds to increasing the hardness of the fragile region and enhancing the strength of the fragile region, reducing the risk of the fragile region rupturing during the normal use process of the battery cell.

[0014] In some embodiments, A / B ≦ 3. The larger the ratio of the hardness of the fragile region to that of the non-fragile region, the more difficult it is for the fragile region to rupture. If the ratio is too large, there may be a situation where the fragile region cannot rupture in a timely manner to relieve pressure when the battery cell undergoes thermal runaway. Therefore, by setting the ratio of the hardness of the fragile region to that of the non-fragile region to 3 or less, it is ensured that the fragile region can rupture in a timely manner to relieve pressure when the battery cell undergoes thermal runaway, enhancing the safety of the battery cell.

[0015] In some embodiments, the non-fragile region and the fragile region are directly connected. The structure is simple and easy to mold.

[0016] In some embodiments, the pressure relief device is provided with a concave groove, a connection region is formed at the position where the concave groove of the pressure relief device is provided, the non-fragile region is connected around the connection region, and the fragile region is partially formed in the connection region. In this way, the connection region is thinner than the fragile region, and it is easier to form the fragile region in the connection region.

[0017] In some embodiments, the fragile region and the non-fragile region are integrally formed. This reduces the molding difficulty of the pressure relief device, has good economic efficiency, and the fragile region and the non-fragile region have good integrity, and the strength of the fragile region can be enhanced.

[0018] In some embodiments, the pressure reducing device includes a pressure reducing portion, the fragile region extends along the edge of the pressure reducing portion, and the pressure reducing portion is configured to open with the fragile region as a boundary. In this way, the pressure reducing area of the pressure reducing device becomes larger and the pressure reducing efficiency is improved. In some embodiments, a pressure reducing groove is provided in the pressure reducing device, and a fragile region is formed at the position where the pressure reducing groove of the pressure reducing device is provided. By providing a pressure reducing groove in the pressure reducing device to form a fragile region, the forming method of the fragile region is simple.

[0019] In some embodiments, an antioxidant layer is formed on the surface layer of the pressure reducing device, and the antioxidant layer is distributed along the groove wall surface of the pressure reducing groove in the region where the pressure reducing groove is provided. The antioxidant layer exerts a protective effect on the pressure reducing device and reduces the risk of the pressure reducing device being oxidized. Since the antioxidant layer is distributed along the groove wall surface of the pressure reducing groove in the region where the pressure reducing groove is provided, the antioxidant layer exerts a good protective effect on the region where the pressure reducing groove of the pressure reducing device is provided, and the risk that the pressure reducing device is oxidized in the region where the pressure reducing groove is provided and the strength of the fragile region becomes low can be reduced.

[0020] In some embodiments, the pressure reducing device includes a non-fragile region connected to the periphery of the fragile region. The thickness of the antioxidant layer in the fragile region is set to d, and the thickness of the antioxidant layer in the non-fragile region is set to e, satisfying d < e. The influence of the antioxidant layer on the fragile region is reduced, and it is ensured that the fragile region can rupture in a timely manner and reduce pressure when the battery cell undergoes thermal runaway.

[0021] In some embodiments, the pressure reducing device includes a plurality of walls, and the plurality of walls together define an accommodation space for accommodating the electrode assembly of the battery cell, and a fragile region is formed on at least one wall. The pressure reducing device can provide an accommodation space for the electrode assembly, whereby the pressure reducing device not only has an accommodation function for accommodating the battery cell but also has a pressure reducing function.

[0022] In some embodiments, the plurality of walls includes a bottom wall and a plurality of side walls, the plurality of side walls being arranged around the periphery of the bottom wall, the plurality of side walls together with the bottom wall defining a surrounding storage space, an opening being formed at one end of the pressure reducing device facing the bottom wall, a weakened area being formed in the bottom wall, and / or a weakened area being formed in at least one of the side walls.

[0023] In some embodiments, the pressure reducing device is a plate-like structure. The structure of the pressure reducing device is simple and easy to mold and manufacture.

[0024] In a second aspect, an embodiment of the present application provides a housing including a pressure reducing device provided according to any one of the embodiments of the first aspect.

[0025] In a third aspect, an embodiment of the present application provides a battery cell including an electrode assembly contained within a housing, and the housing provided according to any one of the embodiments of the second aspect.

[0026] In a fourth aspect, embodiments of the present application provide a battery including a housing and a battery cell provided according to any one of the embodiments of the third aspect housed within the housing.

[0027] In a fifth aspect, embodiments of the present application provide a power consumer device including a battery provided according to any one of the embodiments of the fourth aspect.

[0028] In order to more clearly explain the technical solutions of the embodiments of the present application, the drawings that need to be used in the embodiments are briefly described below. It should be understood that the following drawings only illustrate some embodiments of the present application, and should not be regarded as limiting the scope, and those skilled in the art can further obtain other related drawings based on these drawings without creative efforts. [Brief description of the drawings]

[0029] [Figure 1] 1 is a structural schematic diagram of a vehicle provided according to some embodiments of the present application. [Diagram 2] FIG. 2 is an exploded view of a battery provided in accordance with some embodiments of the present application. [Diagram 3] FIG. 2 is an exploded view of a battery cell provided in accordance with some embodiments of the present application. [Figure 4] FIG. 2 is a top view of a pressure reducing device provided in accordance with some embodiments of the present application. [Diagram 5] 5 is a cross-sectional view of the pressure reducing device shown in FIG. 4 taken along line AA. [Figure 6] FIG. 2 is a top view of a pressure reducing device provided in accordance with some alternative embodiments of the present application. [Figure 7] 7 is a cross-sectional view of the pressure reducing device shown in FIG. 6 taken along the line BB. [Figure 8] 13 is a top view of a pressure reducing device provided in accordance with yet further embodiments of the present application. FIG. [Figure 9] 9 is a cross-sectional view taken along line CC of the pressure reducing device shown in FIG. 8. [Figure 10] 1 is a top view of a pressure reducing device provided in accordance with still further embodiments of the present application. [Figure 11] FIG. 2 is a top view of a pressure reducing device provided in accordance with another embodiment of the present application. [Figure 12] 6 is a partial enlarged view of a portion D of the pressure reducing device shown in FIG. 5. [Figure 13] 8 is a partial enlarged view of a portion E of the pressure reducing device shown in FIG. 7. [Figure 14] 10 is a partial enlarged view of a portion F of the pressure reducing device shown in FIG. 9. [Figure 15] FIG. 2 is an axonometric view of a pressure reduction device provided in accordance with some embodiments of the present application. [Figure 16] FIG. 16 is a cross-sectional view of the pressure reducing device shown in FIG. [Figure 17] FIG. 13 is an axonometric view of a pressure reducing device provided in accordance with still further embodiments of the present application. [Figure 18] 1 is a structural schematic diagram of a housing provided according to some embodiments of the present application. [Figure 19] 1 is a structural schematic diagram of a housing provided according to some other embodiments of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0030] In order to clarify the objectives, technical solutions and advantages of the embodiments of the present application, the technical solutions in the embodiments of the present application are described below with reference to the drawings in the embodiments of the present application. It is clear that the described embodiments are only a part of the embodiments of the present application, and are not all of the embodiments. All other embodiments obtained based on the embodiments of the present application without the need for creative efforts by those skilled in the art are within the scope of protection of the present application.

[0031] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as commonly understood by those skilled in the art. The terms used in this application are only for describing specific embodiments and are not intended to limit this application. The terms "comprise", "have" and any variations thereof in this application's specification, claims and the above description of the drawings are intended to cover non-exclusive "comprise". The terms "first", "second", etc. in this application's specification, claims and the above description of the drawings are intended to distinguish different objects and are not intended to describe a specific order or a main-subordinate relationship.

[0032] When referring to an "embodiment" in this application, it means that a particular feature, structure, or characteristic described in connection with the embodiment may be included in at least one embodiment of this application. The appearances of this phrase in various places in the specification do not necessarily all refer to the same embodiment, nor are they mutually exclusive independent or alternative embodiments of other embodiments.

[0033] In the description of this application, unless otherwise specified or limited, the terms "attach," "connect," "join," and "couple" should be understood in a broad sense, and may refer to, for example, a fixed connection, a detachable connection, or an integral connection, a direct connection, an indirect connection via an intermediate medium, or internal communication between two elements. A person skilled in the art can understand the specific meaning of the above terms in the present application according to the specific circumstances.

[0034] The term "and / or" in this application merely describes the relationship between related objects and indicates that three relationships may exist, for example, A and / or B can represent three cases: A alone, A and B in combination, and B alone. Also, the character " / " in this application generally indicates that the related objects before and after it are in an "or" relationship.

[0035] In the embodiments of the present application, the same reference numerals represent the same elements, and for the sake of brevity, detailed descriptions of the same elements in different embodiments will be omitted. It should be understood that the dimensions of each element in the embodiments of the present application, such as thickness, length, width, etc., and the dimensions of the entire integrated device, such as thickness, length, width, etc., shown in the drawings, are merely illustrative and do not impose any limitations on the present application.

[0036] As used herein, "plurality" means two or more (including two).

[0037] In the present application, the battery cell may include a lithium ion secondary battery, a lithium ion primary battery, a lithium sulfur battery, a sodium lithium ion battery, a sodium ion battery, or a magnesium ion battery, etc., but the embodiment of the present application is not limited thereto. The battery cell may have a cylindrical shape, a flat shape, a rectangular shape, or other shapes, but the embodiment of the present application is not limited thereto. Battery cells are generally divided into three types, namely, cylindrical battery cells, rectangular battery cells, and soft-pack battery cells, according to packaging methods, but the embodiment of the present application is not limited thereto.

[0038] The battery referred to in the embodiments of the present application refers to a single physical module that includes one or more battery cells to provide higher voltage and capacity. For example, the battery referred to in the present application may include a battery module or a battery pack. The battery generally includes a housing for packaging one or more battery cells. The housing can prevent liquids or other foreign objects from affecting the charging or discharging of the battery cells.

[0039] The battery cell mainly operates by the movement of metal ions between the positive and negative plates. The positive plate includes a positive current collector and a positive active material layer, the positive active material layer is applied to the surface of the positive current collector, the positive current collector not coated with the positive active material layer protrudes from the positive current collector coated with the positive active material layer, and the positive current collector not coated with the positive active material layer is a positive tab. Taking a lithium ion battery as an example, the material of the positive current collector may be aluminum, and the positive active material may be lithium cobalt oxide, lithium iron phosphate, ternary lithium, or lithium manganate, etc. The negative plate includes a negative current collector and a negative active material layer, the negative active material layer is applied to the surface of the negative current collector, the negative current collector not coated with the negative active material layer protrudes from the negative current collector coated with the negative active material layer, and the negative current collector not coated with the negative active material layer is a negative tab. The material of the negative electrode current collector may be copper, and the negative electrode active material may be carbon or silicon, etc. In order to ensure that a large current flows without melting, the positive electrode tabs are multiple and stacked, and the negative electrode tabs are multiple and stacked. The material of the separator may be PP (polypropylene) or PE (polyethylene), etc. In addition, the electrode assembly may have a wound type structure or a stacked type structure, and the embodiment of the present application is not limited thereto.

[0040] In the development of battery technology, various design factors must be simultaneously considered, such as performance parameters such as energy density, cycle life, discharge capacity, and charge / discharge ratio, and battery safety must also be taken into account.

[0041] In order to ensure the safety of the battery cell, a pressure reducing device can be provided in the battery cell, and a weak area is formed in the pressure reducing device. When the battery cell experiences thermal runaway, the weak area releases the pressure inside the battery cell, thereby improving the safety of the battery cell.

[0042] The inventors have noticed that, in order to ensure that the pressure reducing device can timely reduce the pressure when the battery cell goes into thermal runaway, the thickness of the weak area can be set small, but in the normal use process of the battery cell, the weak area is easily burst in a vibration environment or due to the long-term change in the internal pressure of the battery cell, which shortens the service life of the battery cell. In order to ensure that the battery cell has a long service life, the thickness of the weak area can be set large, but it is easy to occur that the weak area cannot timely reduce the pressure when the battery cell goes into thermal runaway, which makes it easy to cause accidents such as the battery cell catching fire or exploding, and the safety of the battery cell is low.

[0043] In view of this, an embodiment of the present application provides a pressure reducing device in which the ratio of the hardness of the weakened area to the thickness of the weakened area is set to 5 HBW / mm to 10,000 HBW / mm.

[0044] In such a pressure reducing device, not only is the effect of the thickness of the weak area on the performance of the pressure reducing device taken into consideration, but also the effect of the hardness of the weak area on the performance of the pressure reducing device is taken into consideration, and the ratio of the hardness of the weak area to the thickness of the weak area is set within a reasonable range, so that the weak area has sufficient strength during the normal use of the battery cell, and the pressure reducing device is less likely to burst at the position of the weak area, not only can the service life of the battery cell be extended, but also the pressure reducing device can timely reduce pressure through the weak area when the battery cell experiences thermal runaway, reducing the risk of fire or explosion of the battery cell and improving the safety of the battery cell.

[0045] The pressure reducing device described in the embodiments of the present application is applied to a battery cell, a battery, and a power consuming device using a battery.

[0046] The power consumption devices may be vehicles, mobile phones, portable devices, notebook computers, ships, spacecraft, electric toys, power tools, etc. The vehicles may be gasoline-powered automobiles, gas-powered automobiles, or new energy automobiles, the new energy automobiles may be secondary battery-powered electric automobiles, hybrid electric automobiles, extended-range electric automobiles, etc., the spacecraft include airplanes, rockets, space shuttles, spacecraft, etc., the electric toys include game consoles, electric car toys, electric propulsion ship toys, electric plane toys, and other stationary or mobile electric toys, and the power tools include electric drills, electric grinders, electric wrenches, electric drivers, electric hammers, electric impact drills, metal cutting power tools such as concrete vibrators and electric planers, polishing power tools, mounting power tools, and railroad power tools. In the embodiments of the present application, there are no particular limitations on the power consumption devices.

[0047] In the following embodiment, for ease of explanation, a case will be described in which the power consuming device is a vehicle.

[0048] 1, which is a structural schematic diagram of a vehicle 1000 provided according to some embodiments of the present application. A battery 100 is provided inside the vehicle 1000, and the battery 100 may be provided at the bottom, front or rear of the vehicle 1000. The battery 100 can be used to power the vehicle 1000, for example, the battery 100 can be an operating power source for the vehicle 1000.

[0049] The vehicle 1000 may further include a controller 200 and a motor 300, where the controller 200 is used to control the battery 100 to power the motor 300, for example, to meet the operating power needs of the vehicle 1000 during starting, navigation, and driving.

[0050] In some embodiments of the present application, the battery 100 can be used not only as an operating power source for the vehicle 1000, but also as a driving power source for the vehicle 1000, providing driving power to the vehicle 1000 in place of, or in place of, gasoline or natural gas.

[0051] 2, which is an exploded view of a battery 100 provided in accordance with some embodiments of the present application. The battery 100 includes a battery cell 10 and a housing 20, where the battery cell 10 is housed within the housing 20.

[0052] The housing 20 is a member that houses the battery cells 10, and the housing 20 provides a housing space for the battery cells 10. The housing 20 can adopt various structures. In some embodiments, the housing 20 can include a first part 201 and a second part 202, and the first part 201 and the second part 202 are covered with each other to define a housing space for housing the battery cells 10. The first part 201 and the second part 202 can have various shapes, such as a rectangular parallelepiped or a cylindrical body. The first part 201 can be a hollow structure with one side open, and the second part 202 can also be a hollow structure with one side open, and when the open side of the second part 202 is covered with the open side of the first part 201, the housing 20 having the housing space is formed. The first part 201 may be a hollow structure with one side open, and the second part 202 may be a plate-like structure, and when the second part 202 is covered by the open side of the first part 201, a housing 20 having an accommodation space is formed. The first part 201 and the second part 202 may be sealed by a sealing element, and the sealing element may be a seal ring, a sealant, etc.

[0053] In the battery 100, the battery cell 10 may be one or more. If there are more than one battery cell 10, the battery cells 10 may be connected in series, parallel, or series-parallel, and series-parallel connection means that the battery cells 10 are connected in series or parallel. The battery modules may be first connected in series, parallel, or series-parallel to form a battery module, and the battery modules may be further connected in series, parallel, or series-parallel to form a whole and housed in the housing 20. All the battery cells 10 may be directly connected in series, parallel, or series-parallel, and then the whole consisting of all the battery cells 10 may be housed in the housing 20.

[0054] In some embodiments, the battery 100 may further include a bus bar member through which electrical connection is established between the multiple battery cells 10, thereby realizing a series connection, a parallel connection, or a series-parallel connection of the multiple battery cells 10. The bus bar member may be a metal conductor such as, for example, copper, iron, aluminum, stainless steel, or an aluminum alloy.

[0055] 3, which is an exploded view of a battery cell 10 provided according to some embodiments of the present application. The battery cell 10 can include a housing 1 and an electrode assembly 2.

[0056] The housing 1 is a member for accommodating the electrode assembly 2. The housing 1 may have various shapes, for example, a cylindrical body or a rectangular parallelepiped. The housing 1 may include a case 11 and an end cap 12.

[0057] Case 11 may be a hollow structure with an opening at one end, or case 11 may be a hollow structure with openings at both opposing ends. Case 11 may be made of various materials, such as copper, iron, aluminum, steel, and aluminum alloys.

[0058] The end cap 12 is a member that closes the opening of the case 11 so as to separate the internal environment of the battery cell 10 from the external environment. The end cap 12 and the case 11 together define a sealed space for accommodating the electrode assembly 2, the electrolyte, and other components. The end cap 12 can be connected to the case 11 by welding or sewing so as to close the opening of the case 11. The shape of the end cap 12 can be adapted to the shape of the housing 1, for example, the case 11 is a rectangular parallelepiped structure and the end cap 12 is a rectangular plate-like structure that fits the housing 1, or further, for example, the case 11 is a cylindrical body and the end cap 12 is a circular plate-like structure that fits the case 11. The material of the end cap 12 may be various materials, for example, copper, iron, aluminum, steel, aluminum alloy, etc.

[0059] The battery cell 10 may have one or two end caps 12. In an embodiment in which the case 11 has a hollow structure with openings formed at both ends, two end caps 12 may be provided correspondingly, with the two end caps 12 closing the two openings of the case 11, respectively, and the two end caps 12 defining a sealed space together with the case 11. In an embodiment in which the case 11 has a hollow structure with an opening formed at one end, one end cap 12 may be provided correspondingly, with the end cap 12 closing the opening at one end of the case 11, and the one end cap 12 defining a sealed space together with the case 11.

[0060] The electrode assembly 2 is a member where an electrochemical reaction occurs in the battery cell 10. The electrode assembly 2 may include a positive electrode plate, a negative electrode plate, and a separator. The electrode assembly 2 may have a wound structure formed by winding up a positive electrode plate, a separator, and a negative electrode plate, or may have a laminated structure formed by stacking and distributing a positive electrode plate, a separator, and a negative electrode plate. The electrode assembly 2 has a positive electrode tab 21 and a negative electrode tab 22, and the positive electrode tab 21 may be a portion of the positive electrode plate where a positive electrode active material layer is not applied, and the negative electrode tab 22 may be a portion of the negative electrode plate where a negative electrode active material layer is not applied.

[0061] The battery cell 10 may further include an electrode terminal, which is provided on the end cap 12 and is used to electrically connect to a tab of the electrode assembly 2 so as to output electrical energy of the battery cell 10. The electrode terminal may be directly connected to the tab, for example, the electrode terminal is directly welded to the tab. The electrode terminal may be indirectly connected to the tab, for example, the electrode terminal is indirectly connected to the tab via a current collecting member. The current collecting member may be a metal conductor such as copper, iron, aluminum, steel, or an aluminum alloy.

[0062] As shown in FIG. 3, for example, the case 11 has a hollow structure with an opening formed at one end. Two electrode terminals can be provided on the end cap 12, and the two electrode terminals are a positive electrode terminal 121 and a negative electrode terminal 122, respectively. The positive electrode terminal 121 is electrically connected to the positive electrode tab 21, and the negative electrode terminal 122 is electrically connected to the negative electrode tab 22.

[0063] The battery cell 10 may be provided with a pressure reducing device 13 (not shown in FIG. 3), which is a member that releases pressure inside the battery cell 10. When the pressure or temperature inside the battery cell 10 reaches a threshold value, the pressure reducing device 13 releases the pressure inside the battery cell 10. The specific structure of the pressure reducing device 13 will be described in detail below with reference to the drawings.

[0064] 4 and 5, Fig. 4 is a top view of a pressure reducing device 13 provided by some embodiments of the present application, and Fig. 5 is an AA cross-sectional view of the pressure reducing device 13 shown in Fig. 4. The embodiments of the present application provide a pressure reducing device 13 for use in a battery cell 10, in which a weakened area 131 is partially formed in the pressure reducing device 13, the weakened area 131 is used to burst when the battery cell 10 releases pressure, the thickness of the weakened area 131 is a, and the hardness of the weakened area 131 is A, satisfying 5HBW / mm≦A / a≦10000HBW / mm.

[0065] The pressure reducing device 13 may be the end cap 12 itself, or may be the case 11 itself. The pressure reducing device 13 may be an independent member provided on the case 11 and / or the end cap 12, for example, the pressure reducing device 13 is a rupture disc provided on the end cap 12 and / or the case 11. The pressure reducing device 13 may be made of a metallic material such as copper, iron, aluminum, steel, or an aluminum alloy, or may be made of a non-metallic material such as plastic.

[0066] The weak area 131 is a part that is weaker than other areas in the pressure reducing device 13, and in the pressure reducing device 13, the weak area 131 is more likely to rupture than other areas. When the internal pressure of the battery cell 10 reaches the pressure reducing pressure and needs to be released, the weak area 131 can rupture so as to discharge the exhaust inside the battery cell 10 and achieve the purpose of releasing the internal pressure of the battery cell 10. The thickness of the weak area 131 may be uniform or not uniform. If the thickness of the weak area 131 is uniform, the thickness measured at any position of the weak area 131 is the thickness of the weak area 131, and if the thickness of the weak area 131 is not uniform, the thickness measured at the thinnest position of the weak area 131 is the thickness of the weak area 131, i.e., a is the minimum thickness of the weak area 131.

[0067] The weakened region 131 may have various shapes, such as a rectangle, a circle, an ellipse, a ring, a U-shape, a C-shape, an H-shape, etc. When the weakened region 131 is ring-shaped, the weakened region 131 is an occluded structure extending along an occlusion locus in which both ends of the head and tail are connected, and the ring shape may be a rectangular ring, a circular ring, etc.

[0068] The hardness of the weak area 131 is Brinell hardness, and the unit is HBW. The measurement method of the Brinell hardness can be performed by referring to the measurement principle in GB / T 23.1-2018. In the actual measurement process, the hardness of the weak area 131 can be obtained by measuring any surface in the thickness direction Z of the weak area 131. Taking the end cap 12 of the battery cell 10 as the pressure reducing device 13 as an example, the hardness of the weak area 131 can be measured on the outer surface of the weak area 131, or the hardness of the weak area 131 can be measured on the inner surface of the weak area 131. In the battery cell 10, along the thickness direction Z of the weak area 131, the inner surface of the weak area 131 is the surface of the weak area 131 facing the inside of the battery cell 10, and the outer surface of the weak area 131 is the surface of the weak area 131 facing the outside of the battery cell 10.

[0069] A / a may be any value between 5HBW / mm and 10,000HBW / mm, for example, 5HBW / mm, 50HBW / mm, 100HBW / mm, 190HBW / mm, 500HBW / mm, 1000HBW / mm, 4000HBW / mm, 8000HBW / mm, 10,000HBW / mm, etc.

[0070] In order to test the effect of the ratio of the hardness of the weakened area 131 to the thickness of the weakened area 131 on the performance of the pressure reducing device 13, several groups of battery cells 10 were tested, and the test results are shown in Table 1.

[0071] [Table 1]

[0072] When A / a>10000HBW / mm, the weak area 131 is thin and has a high hardness, which makes the weak area 131 very thin and fragile and easy to burst, and the weak area 131 will burst within the normal usage cycle of the battery cell 10, shortening the service life of the battery cell 10. When A / a<5HBW / mm, the weak area 131 is thick and has a low hardness, and when the battery cell 10 experiences thermal runaway, the weak area 131 will first deform and then stretch, failing to burst in a timely manner and decompress.

[0073] When 5 HBW / mm≦A / a≦10,000 HBW / mm, the weak area 131 will not burst within the normal usage cycle of the battery cell 10, and when the battery cell 10 experiences thermal runaway, the weak area 131 can burst in a timely manner to reduce pressure.

[0074] It can be seen from this that by setting the ratio of the hardness of the weak area 131 to the thickness of the weak area 131 within a reasonable range, the weak area 131 has sufficient strength during the normal use of the battery cell 10, and the pressure reducing device 13 is less likely to burst at the position of the weak area 131, which not only extends the service life of the battery cell 10 but also allows the pressure reducing device 13 to timely reduce pressure through the weak area 131 when the battery cell 10 experiences thermal runaway, thereby reducing the risk of fire or explosion of the battery cell 10 and improving the safety of the battery cell 10.

[0075] In some embodiments, 190 HBW / mm ≤ A / a ≤ 4000 HBW / mm.

[0076] Exemplarily, A / a may be, for example, 190 HBW / mm, 500 HBW / mm, 1000 HBW / mm, 4000 HBW / mm, etc.

[0077] In this embodiment, by setting A / a to be 190 HBW / mm to 4000 HBW / mm, the performance of the pressure relief device 13 is more excellent, and it is ensured that when the battery cell 10 undergoes thermal runaway, the fragile area 131 ruptures in a timely manner to relieve pressure, and at the same time, it is ensured that the fragile area 131 has sufficient strength during the normal use process of the battery cell 10. On the premise of ensuring the safety of the battery cell 10, the service life of the battery cell 10 is extended.

[0078] In some embodiments, 8 HBW ≤ A ≤ 200 HBW.

[0079] A may be any value between 8 HBW / mm and 200 HBW / mm, for example, 8 HBW, 10 HBW, 15 HBW, 19 HBW, 50 HBW, 100 HBW, 200 HBW, etc.

[0080] In some embodiments, 0.02 mm ≤ a ≤ 1.6 mm.

[0081] a may be any value between 0.02 mm and 1.6 mm, for example, 0.02 mm, 0.025 mm, 0.05 mm, 0.1 mm, 0.15 mm, 0.2 mm, 1.6 mm, etc.

[0082] In some embodiments, continuing to refer to FIG. 4, the pressure relief device 13 includes a non-fragile area 132. The non-fragile area 132 is connected to the periphery of the fragile area 131. The thickness of the non-fragile area 132 is b, and a < b is satisfied.

[0083] The non-weakened region 132 is less likely to rupture than the weak region 131, and when the battery cell 10 experiences thermal runaway and the internal pressure reaches a reduced pressure, the weak region 131 ruptures and reduces the pressure, but the non-weakened region 132 does not rupture. The thickness of the non-weakened region 132 may or may not be uniform. If the thickness of the non-weakened region 132 is uniform, the thickness measured at any position of the non-weakened region 132 is the thickness of the non-weakened region 132, and if the thickness of the non-weakened region 132 is not uniform, the thickness measured at the thinnest position of the non-weakened region 132 is the thickness of the weak region 131, i.e., b is the minimum thickness of the non-weakened region 132.

[0084] The non-weakened area 132 and the weak area 131 may be directly connected or indirectly connected.

[0085] In this embodiment, the thickness of the weak area 131 is set to be smaller than the thickness of the non-weakened area 132, so that the weak area 131 is more likely to rupture than the non-weakened area 132, and it is ensured that the pressure reducing device 13 ruptures at the position of the weak area 131 to reduce pressure when the battery cell 10 experiences thermal runaway.

[0086] In other embodiments, the weakened area 131 may be made more susceptible to rupture than the non-weakened area 132 by other means, for example, the thicknesses of the weakened area 131 and the non-weakened area 132 are equal, but the materials of the weakened area 131 and the non-weakened area 132 are not the same, and the material of the weakened area 131 is more susceptible to rupture than the material of the non-weakened area 132, such that when the battery cell 10 experiences thermal runaway, the weakened area 131 ruptures but the non-weakened area 132 does not rupture.

[0087] In some embodiments, 0.05≦a / b≦0.95.

[0088] a / b may be any value between 0.05 and 0.95, for example, 0.05, 0.12, 0.2, 0.8, 0.95, etc.

[0089] If the ratio of the thickness of the fragile region 131 to the thickness of the non-fragile region 132 is too small, there may be a situation where the strength of the fragile region 131 is insufficient. If the ratio of the thickness of the fragile region 131 to the thickness of the non-fragile region 132 is too large, when the battery cell 10 undergoes thermal runaway, a situation may occur where the fragile region 131 cannot easily rupture, and there is a possibility that pressure cannot be reduced in a timely manner, resulting in accidents such as ignition and explosion of the battery cell 10.

[0090] Therefore, by setting the ratio of the thickness of the fragile region 131 to the thickness of the non-fragile region 132 between 0.05 and 0.95, not only can the probability of the fragile region 131 rupturing during the normal use process of the battery cell 10 be reduced, but also the probability of accidents such as ignition and explosion occurring when the battery cell 10 undergoes thermal runaway can be reduced.

[0091] In some embodiments, 0.12 ≦ a / b ≦ 0.8.

[0092] In this embodiment, by setting a / b between 0.12 and 0.8, the performance of the pressure relief device 13 is better, ensuring that the fragile region 131 ruptures and reduces pressure in a timely manner when the battery cell 10 undergoes thermal runaway, and at the same time ensuring that the fragile region 131 has sufficient strength during the normal use process of the battery cell 10.

[0093] In some embodiments, the hardness of the non-fragile region 132 is B, and B < A is satisfied.

[0094] The hardness of the non-fragile region 132 is also the Brinell hardness. The hardness of the non-fragile region 132 can be obtained by measuring on any surface in the thickness direction Z of the non-fragile region 132. Taking the case where the end cap 12 of the battery cell 10 is used as the pressure relief device 13 as an example, the hardness of the non-fragile region 132 may be measured on the outer surface of the non-fragile region 132, or the hardness of the non-fragile region 132 may be measured on the inner surface of the non-fragile region 132. Along the thickness direction Z of the non-fragile region 132, the inner surface of the non-fragile region 132 is the surface facing the inside of the battery cell 10 of the non-fragile region 132, and the outer surface of the non-fragile region 132 is the surface facing the outside of the battery cell 10 of the non-fragile region 132.

[0095] In this embodiment, the fact that the hardness of the fragile region 131 is greater than the hardness of the non-fragile region 132 is equivalent to increasing the hardness of the fragile region 131 and enhancing the strength of the fragile region 131, reducing the risk of the fragile region 131 rupturing during the normal use process of the battery cell 10.

[0096] In some embodiments, A / B ≤ 3.

[0097] Since B < A, it can be understood that 1 < A / B ≤ 3. Exemplarily, A / B may be 1.1, 1.5, 2, 2.5, 3, etc.

[0098] The larger the ratio of the hardness of the fragile region 131 to the hardness of the non-fragile region 132, the less likely the fragile region 131 is to rupture. If the ratio between the two is too large, there may be a situation where the fragile region 131 cannot rupture in a timely manner to relieve pressure when the battery cell 10 undergoes thermal runaway.

[0099] Therefore, by setting the ratio of the hardness of the fragile region 131 to the hardness of the non-fragile region 132 to be 3 or less, it is ensured that the fragile region 131 can rupture in a timely manner to relieve pressure when the battery cell 10 undergoes thermal runaway, enhancing the safety of the battery cell 10.

[0100] In some embodiments, continuing to refer to FIGS. 4 and 5, the non-fragile region 132 and the fragile region 131 are directly connected.

[0101] As shown in FIG. 4, taking the case where the pressure relief device 13 is a rectangular plate and the fragile region 131 is rectangular as an example, the non-fragile region 132 is the portion of the pressure relief device 13 provided to surround the periphery of the fragile region 131.

[0102] In this embodiment, the non-fragile region 132 and the fragile region 131 are directly connected, with a simple structure and being easy to mold.

[0103] 6 and 7, in some embodiments, Fig. 6 is a top view of a pressure reducing device 13 provided according to some other embodiments of the present application, and Fig. 7 is a BB cross-sectional view of the pressure reducing device 13 shown in Fig. 6. A recessed groove 133 is provided in the pressure reducing device 13, a connection region 134 is formed at the position where the recessed groove 133 is provided in the pressure reducing device 13, the non-weakened region 132 is connected around the connection region 134, and a weakened region 131 is partially formed in the connection region 134.

[0104] The recessed groove 133 may have various shapes, such as a rectangle, a circle, an oval, etc. The recessed groove 133 may be formed by various means, such as a stamping or milling process, and the embodiment of the present application is not particularly limited thereto.

[0105] In this embodiment, it is understood that the non-weakened region 132 and the weak region 131 are indirectly connected, and the portion of the connection region 134 other than the weak region 131 connects the weak region 131 and the non-weakened region 132. Taking the case where the recessed groove 133 and the weak region 131 are both rectangular as an example, the non-weakened region 132 is a portion of the pressure reducing device 13 that is provided around the periphery of the connection region 134, and the portion of the connection region 134 that is provided around the periphery of the weak region 131 connects the weak region 131 and the non-weakened region 132.

[0106] In this embodiment, since the connection area 134 is thinner than the non-weakened area 132, it is easier to mold the weak area 131 in the connection area 134, and the weak area 131 will not be too thick, and the thickness requirement of the weak area 131 is met.

[0107] In some embodiments, the weakened area 131 and the non-weakened area 132 are integrally formed.

[0108] It should be noted that the weakened area 131 and the non-weakened area 132 can be integrally molded regardless of whether the weakened area 131 and the non-weakened area 132 are directly or indirectly connected to each other.

[0109] In this embodiment, the weak area 131 and the non-weakened area 132 are an integrally molded structure, which reduces the difficulty of molding the pressure reducing device 13 and has good economic efficiency, and the weak area 131 and the non-weakened area 132 have good integrity, which can increase the strength of the weak area 131.

[0110] 8 to 11, in which Fig. 8 is a top view of the pressure reducing device 13 provided according to still other embodiments of the present application, Fig. 9 is a CC cross-sectional view of the pressure reducing device 13 shown in Fig. 8, Fig. 10 is a top view of the pressure reducing device 13 provided according to still other embodiments of the present application, and Fig. 11 is a top view of the pressure reducing device 13 provided according to another embodiment of the present application. The pressure reducing device 13 includes a pressure reducing portion 135, and the weakened region 131 extends along an edge of the pressure reducing portion 135, and the pressure reducing portion 135 is configured to open with the weakened region 131 as a boundary.

[0111] The pressure reduction portion 135 is a region of the pressure reduction device 13 that is defined by the weakened region 131. The pressure reduction portion 135 defined by the weakened region 131 may be one, for example, as shown in Fig. 8, the weakened region 131 is ring-shaped, or for example, as shown in Fig. 10, the weakened region 131 is C-shaped, and the pressure reduction portion 135 defined by the weakened region 131 may be multiple, for example, as shown in Fig. 11, the weakened region 131 is H-shaped, and the weakened region 131 defines two pressure reduction portions 135.

[0112] As shown in FIG. 11, in an embodiment in which the weakened area 131 is H-shaped, the weakened area 131 may include a first weakened segment 1311, a second weakened segment 1312, and a third weakened segment 1313, where the first weakened segment 1311 and the third weakened segment 1313 are arranged opposite each other, the second weakened segment 1312 is connected between the first weakened segment 1311 and the third weakened segment 1313, and the first weakened segment 1311, the second weakened segment 1312, and the third weakened segment 1313 together form an H shape. In other embodiments, the weakened region 131 may include a fourth weakened segment located between the first weakened segment 1311 and the third weakened segment 1313 and distributed so as to intersect with the second weakened segment 1312, such that an initial rupture location of the weakened region 131 is formed at the intersection of the fourth weakened segment and the second weakened segment 1312.

[0113] The weak region 131 may be an occluded structure extending along an occluded trajectory with both ends of the head and tail connected, for example, as shown in FIG. 8, the weak region 131 is ring-shaped, or the weak region 131 may be a non-occluded structure extending along an non-occluded trajectory with both ends of the head and tail spaced apart, for example, as shown in FIG. 10, the weak region is C-shaped.

[0114] When the battery cell 10 experiences thermal runaway, the weak area 131 bursts, and the pressure reducing portion 135 can open with the weak area 131 as a boundary to release the pressure inside the battery cell 10. If the weak area 131 has a closed structure, the weak area 131 can open to separate, and if the weak area 131 has a non-closed structure, the weak area 131 can open to invert outward.

[0115] For example, as shown in Figures 8 and 9, the weak area 131 and the non-weakened area 132 are directly connected, the non-weakened area 132 is connected to the outer edge of the weak area 131, and the pressure reduction section 135 is connected to the inner edge of the weak area 131.

[0116] For example, as shown in Figures 10 and 11, a recessed groove 133 is provided in the pressure reducing device 13, a connection area 134 is formed at the position where the recessed groove 133 of the pressure reducing device 13 is provided, the non-weakened area 132 is connected around the connection area 134, and a weak area 131 is partially formed in the connection area 134, thereby realizing an indirect connection between the weak area 131 and the non-weakened area 132.

[0117] In this embodiment, the pressure reducing section 135 increases the pressure reducing area of ​​the pressure reducing device 13 and improves the pressure reducing efficiency.

[0118] In some embodiments, with continued reference to Figures 4-11, the pressure reducing device 13 is provided with a pressure reducing groove 136, and a weakened area 131 is formed at the location of the pressure reducing device 13 where the pressure reducing groove 136 is provided.

[0119] After the pressure reducing device 13 is provided with the pressure reducing groove 136, the remaining part of the pressure reducing device 13 except for the position of the pressure reducing groove 136 is the weakened area 131. By providing the pressure reducing groove 136 in the pressure reducing device 13, it is possible to realize that the thickness of the non-weakened area 132 of the pressure reducing device 13 is greater than the thickness of the weakened area 131. As shown in Figures 4, 5, 8 and 9, when the pressure reducing device 13 is not provided with the recessed groove 133 but is provided with the pressure reducing groove 136, it is possible to realize the integral molding of the weakened area 131 and the non-weakened area 132. As shown in Figures 6, 7, 10 and 11, when the pressure reducing device 13 is provided with the recessed groove 133 and the pressure reducing groove 136, the pressure reducing groove 136 can be provided on the groove bottom surface of the recessed groove 133 (the surface of the connection area 134). During molding, a recessed groove 133 is machined in the decompression device 13, and then a decompression groove 136 is machined on the bottom surface of the recessed groove 133, thereby making it possible to integrally mold the weakened area 131 and the non-weakened area 132.

[0120] The decompression groove 136 may have various shapes, such as a rectangle, a circle, an ellipse, a ring, a U-shape, a C-shape, an H-shape, and the like. The shape of the decompression groove 136 is the same as the shape of the weakened area 131. For example, when the decompression groove 136 is rectangular, the weakened area 131 is also rectangular; for example, when the decompression groove 136 is C-shaped, the weakened area 131 is also C-shaped; for example, when the decompression groove 136 is H-shaped, the weakened area 131 is also H-shaped. The decompression groove 136 can be formed by various means, such as punching and milling, and the embodiment of the present application is not particularly limited thereto. After the decompression groove 136 is formed by punching, it can be realized that the hardness of the weakened area 131 is greater than the hardness of the non-weakened area 132.

[0121] As shown in Figures 5, 7 and 9, the pressure reducing device 13 has a first surface 137 and a second surface 138 that are provided opposite to each other along the thickness direction Z of the non-weakened region 132, and the distance between the first surface 137 and the second surface 138 is the thickness of the non-weakened region 132. As shown in Figures 5 and 9, the pressure reducing device 13 is provided with a pressure reducing groove 136, but in an embodiment in which the recessed groove 133 is not provided, the pressure reducing groove 136 may be provided on one of the first surface 137 and the second surface 138, or the pressure reducing groove 136 may be provided on both the first surface 137 and the second surface 138. 7, in an embodiment in which the pressure reducing device 13 is provided with the pressure reducing groove 136 and also with the recessed groove 133, the recessed groove 133 may be provided on one of the first surface 137 and the second surface 138, and then the pressure reducing groove 136 may be provided on the groove bottom surface of the recessed groove 133, or the recessed groove 133 may be provided on both the first surface 137 and the second surface 138, and then the pressure reducing groove 136 may be provided on the groove bottom surface of the recessed groove 133. Taking the case in which the pressure reducing device 13 is an end cap 12 of a battery cell 10 as an example, the first surface 137 may be a surface of the end cap 12 facing the inside of the battery cell 10, and the second surface 138 may be a surface of the end cap 12 facing the outside of the battery cell 10.

[0122] In this embodiment, the weakened area 131 is formed by providing the decompression groove 136 in the decompression device 13, and the method for forming the weakened area 131 is simple.

[0123] 12 to 14, in some embodiments, Fig. 12 is a partial enlarged view of a portion D of the pressure reducing device 13 shown in Fig. 5, Fig. 13 is a partial enlarged view of a portion E of the pressure reducing device 13 shown in Fig. 7, and Fig. 14 is a partial enlarged view of a portion F of the pressure reducing device 13 shown in Fig. 9. An oxidation prevention layer 139 is formed on the surface layer of the pressure reducing device 13, and the oxidation prevention layer 139 is distributed along the groove wall surface of the pressure reducing groove 136 in the region where the pressure reducing groove 136 is provided.

[0124] The portion of the oxidation prevention layer 139 located in the weakened region 131 defines a pressure reduction groove 136. The groove wall surface of the pressure reduction groove 136 includes a groove side surface and a groove bottom surface, and both the groove side surface and the groove bottom surface are part of the outer surface of the oxidation prevention layer 139. The oxidation prevention layer 139 may be a metal plating layer located on the surface of the pressure reduction device 13. For example, the main body portion of the pressure reduction device 13 is a steel layer, and the oxidation prevention layer 139 is a nickel layer plated on the surface of the main body portion. When measuring the hardness of the weakened region 131, the hardness of the portion of the main body portion located in the weakened region 131 is measured as a reference. When measuring the hardness of the non-weakened region 132, the hardness of the portion of the main body portion located in the non-weakened region 132 is measured as a reference.

[0125] The anti-oxidation layer 139 exerts a protective effect on the pressure reduction device 13, and reduces the risk of oxidation of the pressure reduction device 13. Since the anti-oxidation layer 139 is distributed along the groove wall surface of the pressure reduction groove 136 in the region where the pressure reduction groove 136 is provided, the anti-oxidation layer 139 exerts a good protective effect on the region of the pressure reduction device 13 where the pressure reduction groove 136 is provided, and can reduce the risk that the pressure reduction device 13 will be oxidized in the region where the pressure reduction groove 136 is provided, and the strength of the fragile region 131 will be reduced.

[0126] In some embodiments, continuing to refer to FIGS. 12 to 14, the pressure relief device 13 includes a non-fragile region 132, the non-fragile region 132 is connected around the fragile region 131, the thickness of the antioxidant layer 139 in the fragile region 131 is d, the thickness of the antioxidant layer 139 in the non-fragile region 132 is e, and d < e is satisfied.

[0127] The non-fragile region 132 and the fragile region 131 may be directly connected or indirectly connected.

[0128] In this embodiment, because d < e, the influence of the antioxidant layer 139 on the fragile region 131 is reduced, ensuring that the fragile region 131 can rupture in a timely manner and decompress when the battery cell 10 undergoes thermal runaway.

[0129] In some embodiments, referring to FIGS. 15 and 16, FIG. 15 is an axonometric view of the pressure relief device 13 provided by some embodiments of the present application, and FIG. 16 is a cross-sectional view of the pressure relief device 13 shown in FIG. 15. The pressure relief device 13 includes a plurality of walls, and the plurality of walls together define an accommodation space 140 for accommodating the electrode assembly 2 of the battery cell 10, and a fragile region 131 is formed on at least one wall.

[0130] The pressure relief device 13 may have various shapes, such as a cylinder or a cuboid. Exemplarily, in FIGS. 15 and 16, the pressure relief device 13 is a cuboid. In the pressure relief device 13, a fragile region 131 may be formed on one wall, or a fragile region 131 may be formed on a plurality of walls. For the wall on which the fragile region 131 is formed, when the fragile region 131 and the non-fragile region 132 are directly connected, the other regions of this wall except the fragile region 131 are non-fragile regions 132.

[0131] Taking the case where the pressure reducing device 13 is a rectangular parallelepiped as an example, the pressure reducing device 13 may have six walls, five of which constitute the case 11 of the housing 1, and the remaining wall is an end cap 12 of the housing 1, and the case 11 and the end cap 12 together constitute the pressure reducing device 13. The pressure reducing device 13 may have five walls, and the five walls constitute the case 11 of the housing 1, and the case 11 is constituted by the pressure reducing device 13.

[0132] The pressure reducing device 13 can provide an accommodating space 140 for the electrode assembly 2, so that the pressure reducing device 13 not only has an accommodating function for accommodating the battery cell 10, but also has a pressure reducing function.

[0133] 15 and 16 , in some embodiments, the walls include a bottom wall 141 and a plurality of side walls 142, the plurality of side walls 142 are provided around the periphery of the bottom wall 141, the plurality of side walls 142 together with the bottom wall 141 define the containing space 140, and an opening is formed at one end of the pressure reducing device 13 opposite the bottom wall 141. A weakened area 131 is formed in the bottom wall 141 and / or at least one of the side walls 142 is formed with a weakened area 131.

[0134] The number of side walls 142 in the pressure reducing device 13 may be three, four, five or more. Exemplarily, the pressure reducing device 13 is a rectangular parallelepiped, and there are a total of five walls in the pressure reducing device 13, one wall being the bottom wall 141 and four walls being the side walls 142. In FIG. 16 , the weakened area 131 is formed in the bottom wall 141.

[0135] In this embodiment, a weakened area 131 may be formed in the bottom wall 141 so as to reduce pressure from the bottom wall 141. A weakened area 131 may be formed in at least one side wall 142 so as to reduce pressure from the side wall 142. When the weakened areas 131 are formed in a plurality of side walls 142, the decompression device 13 can reduce pressure from a plurality of directions, and even if the weakened area 131 in one side wall 142 is blocked, the decompression device 13 can reduce pressure through the weakened area 131 in the other side wall 142. Of course, the weakened area 131 may be formed in both the bottom wall 141 and at least one side wall 142 so as to increase the efficiency of the decompression device 13.

[0136] In some embodiments, refer to Fig. 17, which is an axonometric view of a pressure reducing device 13 provided according to still other embodiments of the present application. The pressure reducing device 13 is a plate-like structure.

[0137] The plate-shaped pressure reducing device 13 can be an end cap 12 of the housing 1 so as to close the opening of the case 11. The pressure reducing device 13 may be a plate-shaped member, such as a rupture disk, attached to the end cap 12 and / or the case 11. The pressure reducing device 13 may have various shapes, such as a circular or rectangular shape. Exemplarily, in FIG. 17, the pressure reducing device 13 is a rectangular plate-shaped structure.

[0138] In this embodiment, the pressure reducing device 13 has a plate-like structure, and the structure of the pressure reducing device 13 is simple and easy to form and manufacture.

[0139] 18 and 19, Fig. 18 is a structural schematic diagram of a housing 1 provided according to some embodiments of the present application, and Fig. 19 is a structural schematic diagram of a housing 1 provided according to other some embodiments of the present application. The embodiment of the present application provides a housing 1 including a pressure reducing device 13 provided according to any one of the above embodiments.

[0140] In some embodiments, the pressure reducing device 13 is a case 11 of the housing 1, as shown in FIG 18. In other embodiments, the pressure reducing device 13 is an end cap 12 of the housing 1, as shown in FIG 19.

[0141] An embodiment of the present application provides a battery cell 10 including an electrode assembly 2 housed in a housing 1 and the housing 1 provided by any one of the above embodiments.

[0142] An embodiment of the present application provides a battery 100 including a housing 20 and the battery cell 10 provided by any one of the above embodiments housed in the housing 20.

[0143] An embodiment of the present application provides an electric power consuming device including the battery 100 provided by any one of the above embodiments.

[0144] Also, as shown in FIG. 19, an embodiment of the present application further provides a rectangular housing 1 including a case 11 and an end cap 12. The end cap 12 closes an opening of the case 11. The end cap 12 includes a fragile region 131 and a non-fragile region 132 directly connected to the fragile region 131. The non-fragile region 132 is connected around the fragile region 131. The thickness of the fragile region 131 is a, the hardness of the fragile region 131 is A, the thickness of the non-fragile region 132 is b, the hardness of the non-fragile region 132 is B, and a < b, B < A, and 5 HBW / mm ≤ A / a ≤ 10000 HBW / mm are satisfied. By setting the ratio of the hardness of the fragile region 131 to the thickness of the fragile region 131 within a reasonable range, the fragile region 131 has sufficient strength during the normal use process of the battery cell 10, the pressure relief device 13 is not easily ruptured at the position of the fragile region 131, not only can the service life of the battery cell 10 be extended, but also when the battery cell 10 undergoes thermal runaway, the pressure relief device 13 can be timely depressurized by the fragile region 131, reducing the risk of ignition and explosion of the battery cell 10 and enhancing the safety of the battery cell 10.

[0145] It should be noted that unless there is a conflict, the embodiments and features in the embodiments according to the present application can be combined with each other.

[0146] The above embodiments are only intended to illustrate the technical solutions of the present application, and are not intended to limit the present application. Those skilled in the art may make various modifications and variations to the present application. All modifications, equivalent replacements, improvements, etc. made within the spirit and principle of the present application shall be included within the protection scope of the present application. [Explanation of symbols]

[0147] 1. Housing 11 Cases 12 End cap 121 Positive electrode terminal 122 Negative electrode terminal 13 Pressure reducing device 131 Vulnerable areas 1311 First Weak Segment 1312 Second Weak Segment 1313 Third Weak Segment 132 Non-vulnerable area 133 Groove 134 Connection Area 135 Pressure reduction section 136 Pressure reduction groove 137 First Surface 138 Second Surface 139 Antioxidant layer 140 Storage Space 141 Bottom wall 142 Side wall 2 electrode assembly 21 Positive tab 22 Negative tab 10 Battery Cells 20. Cabinet 201 First Part 202 Second Part 100 batteries 200 Controller 300 Motor 1000 vehicles Z thickness direction

Claims

1. A pressure reducing device for a battery cell, the battery cell being partially formed with a weak area for bursting when pressure is released, comprising: A pressure reducing device in which the thickness of the weakened region is a, the hardness of the weakened region is A, and 5HBW / mm≦A / a≦10,000HBW / mm is satisfied.

2. 2. The pressure reducing device according to claim 1, wherein 190 HBW / mm≦A / a≦4000 HBW / mm.

3. 3. The pressure reducing device according to claim 1, wherein 8HBW≦A≦200HBW.

4. The pressure reducing device according to any one of claims 1 to 3, wherein 0.02 mm≦a≦1.6 mm.

5. The pressure reducing device according to any one of claims 1 to 4, further comprising a non-weakened region connected to a periphery of the weakened region, the non-weakened region having a thickness b, and a<b being satisfied.

6. 6. The pressure reducing device according to claim 5, wherein 0.05≦a / b≦0.

95.

7. 7. The pressure reducing device according to claim 6, wherein 0.12≦a / b≦0.

8.

8. The pressure reducing device according to any one of claims 5 to 7, wherein the hardness of the non-weakened region is B, and B<A is satisfied.

9. 9. The pressure reducing device according to claim 8, wherein A / B≦3.

10. The pressure reducing device according to any one of claims 5 to 9, wherein the non-weakened area and the weakened area are directly connected.

11. A pressure reducing device as described in any one of claims 5 to 9, wherein a recessed groove is provided in the pressure reducing device, a connection area is formed at the position where the recessed groove is provided in the pressure reducing device, the non-weakened area is connected around the connection area, and the weak area is partially formed in the connection area.

12. The pressure reducing device according to any one of claims 5 to 11, wherein the weakened area and the non-weakened area are integrally formed.

13. The pressure reduction device according to any one of claims 1 to 12, wherein the pressure reduction device includes a pressure reduction portion, the weakened area extends along an edge of the pressure reduction portion, and the pressure reduction portion is configured to open with the weakened area as a boundary.

14. The pressure reducing device according to any one of claims 1 to 13, wherein a pressure reducing groove is provided in the pressure reducing device, and the weakened area is formed at a position where the pressure reducing groove is provided in the pressure reducing device.

15. 15. The pressure reducing device according to claim 14, wherein an anti-oxidation layer is formed on a surface layer of the pressure reducing device, the anti-oxidation layer being distributed along a groove wall surface of the pressure reducing groove in a region where the pressure reducing groove is provided.

16. The pressure reducing device of claim 15, further comprising a non-weakened region connected to a periphery of the weak region, wherein the thickness of the oxidation prevention layer in the weak region is d, and the thickness of the oxidation prevention layer in the non-weakened region is e, where d<e.

17. The pressure reducing device according to any one of claims 1 to 16, comprising a plurality of walls, the plurality of walls being together surrounding each other to define an accommodation space for accommodating the electrode assembly of the battery cell, and the weakened area being formed in at least one of the walls.

18. The plurality of walls include a bottom wall and a plurality of side walls, the plurality of side walls are provided to surround the periphery of the bottom wall, the plurality of side walls surround the periphery of the bottom wall to define the accommodation space, and an opening is formed at one end of the pressure reducing device facing the bottom wall, 18. The pressure reducing device of claim 17, wherein the bottom wall is formed with the weakened area and / or at least one of the side walls is formed with the weakened area.

19. The pressure reducing device according to any one of claims 1 to 16, wherein the pressure reducing device has a plate-like structure.

20. A housing comprising a pressure reducing device according to any one of the preceding claims.

21. A housing according to claim 20; an electrode assembly contained within the housing; Including a battery cell.

22. A housing and The battery cell of claim 21 housed within the housing; Including batteries.

23. 23. A power consumer device comprising the battery of claim 22.

Citation Information

Patent Citations

  • Hermetic seal type liquid active material battery

    JP1988086245A

  • Manufacture of nonaqueous liquid active material battery

    JP1989024357A

  • Negative electrode collector for alkaline battery and alkaline battery

    JP2008226565A

  • Battery container with cruciform discharge vent and cover

    JP2009538506A

  • Sealing plate, manufacturing method of sealing plate and sealed battery

    JP2016157570A