Lead isolation materials for perovskite devices

By integrating lead sequestration materials with lead-binding groups into perovskite devices, the issue of lead leakage is addressed, resulting in enhanced stability and safety through effective immobilization of lead ions.

JP2024543927AInactive Publication Date: 2024-11-26CUBIC PBUOY INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024531496
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-28
Filing Date
2022-11-28
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Perovskite photovoltaic devices face challenges due to lead leakage, which can lead to the release of harmful lead and metal ions, necessitating improved lead and metal ion isolation techniques and materials.

Method used

Incorporation of lead sequestration materials such as oxides, hydroxides, amines, amides, acetylacetones, acetylacetonates, carboxylates, carboxylic acids, aldehydes, esters, ethers, phosphines, phosphinates, phosphonic acids, and sulfates with lead-binding groups like phosphate, sulfide, and sulfate into the perovskite material to form a lead sequestration layer.

Benefits of technology

The lead sequestration materials effectively reduce lead and metal ion leakage, enhancing the stability and safety of perovskite photovoltaic devices by immobilizing lead ions, thereby improving their performance and environmental safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543927000001_ABST
    Figure 2024543927000001_ABST
Patent Text Reader

Abstract

The composition has a binding material and a lead-sequestering compound attached to the binding material, the lead-sequestering compound comprising one or more lead-binding groups selected from the group consisting of carboxylates, phosphates, sulfides, sulfates, and any combination thereof.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application claims priority to U.S. Provisional Patent Application No. 63 / 283,514, filed November 28, 2021, entitled "Lead Isolation Materials for Perovskite Devices," the contents of which are incorporated herein by reference in their entirety. [Background technology]

[0002] The use of photovoltaics (PV) to generate electricity from solar energy or solar radiation may offer many advantages, including, for example, power source, low or zero emissions, power generation independent of the power grid, durable physical structure (no moving parts), stable and reliable systems, modular construction, relatively quick installation, safe manufacture and use, and good public opinion and acceptance of use. Perovskite photovoltaics, as an emerging highly efficient and low-cost photovoltaic technology, face obstacles such as lead leakage. Summary of the Invention [Problem to be solved by the invention]

[0003] PV incorporates a layer of perovskite material as the photoactive layer that produces electricity when exposed to light. Some perovskite photovoltaic devices contain lead and other metal ions, which can be prone to leakage. Therefore, improved lead and metal ion isolation techniques and materials are desirable. [Means for solving the problem]

[0004] In certain embodiments, the perovskite material device comprises a lead sequestration compound comprising one or more lead binding groups selected from the group consisting of oxide, hydroxide, amine, amide, ammonium, acetylacetone, acetylacetonate, carboxylate, carboxylic acid, aldehyde, ester, ether, phosphine, phosphinate, phosphonate, phosphate, sulfide, sulfate, and any combination thereof.

[0005] In one embodiment, a method includes providing a substrate; depositing a precursor ink on the substrate comprising a lead isolation material, the lead isolation material comprising a lead isolation compound comprising one or more lead binding groups selected from the group consisting of oxide, hydroxide, amine, amide, ammonium, acetylacetone, acetylacetonate, carboxylate, carboxylate, aldehyde, ester, ether, phosphine, phosphinate, phosphonate, phosphate, sulfide, sulfate, and any combination thereof; and a binding material; and drying the lead isolation precursor ink to form a lead isolation material layer.

[0006] In one embodiment, a composition comprises a bonding material and a lead-sequestering compound attached to the bonding material, the lead-sequestering compound having one or more lead-binding groups selected from the group consisting of oxides, hydroxides, amines, amides, ammonium, acetylacetones, acetylacetonates, carboxylates, carboxylic acids, aldehydes, esters, ethers, phosphines, phosphinates, phosphonates, phosphates, sulfides, sulfates, and any combination thereof. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Diagram 2] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Diagram 3] 1A-1C are schematic diagrams illustrating examples of lead isolation mechanisms according to some embodiments of the present disclosure. [Figure 4] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Diagram 5] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Figure 6] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Figure 7]FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Figure 8] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Figure 9] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Figure 10A] FIG. 1 shows chemical structures of lead-sequestering ethylenediaminetetraacetic acid (EDTA) and EDTA derivatives according to some embodiments of the present disclosure. [Figure 10B] FIG. 1 shows chemical structures of lead-sequestering ethylenediaminetetraacetic acid (EDTA) and EDTA derivatives according to some embodiments of the present disclosure. [Figure 11A] FIG. 1 shows chemical structures of EDTA derivatives according to some embodiments of the present disclosure. [Figure 11B] FIG. 1 shows chemical structures of EDTA derivatives according to some embodiments of the present disclosure. [Figure 11C] FIG. 1 shows chemical structures of EDTA derivatives according to some embodiments of the present disclosure. [Figure 11D] FIG. 1 shows chemical structures of EDTA derivatives according to some embodiments of the present disclosure. [Figure 11E] FIG. 1 shows chemical structures of EDTA derivatives according to some embodiments of the present disclosure. [Figure 12A] FIG. 1 shows chemical structures of organophosphates according to some embodiments of the present disclosure. [Figure 12B] FIG. 1 shows chemical structures of organophosphates according to some embodiments of the present disclosure. [Figure 12C] FIG. 1 shows chemical structures of organophosphates according to some embodiments of the present disclosure. [Figure 12D] FIG. 1 shows chemical structures of organophosphates according to some embodiments of the present disclosure. [Figure 12E] FIG. 1 shows chemical structures of organophosphates according to some embodiments of the present disclosure. [Figure 12F]FIG. 1 shows chemical structures of organophosphates according to some embodiments of the present disclosure. [Figure 13A] FIG. 1 illustrates a lead organophosphate sequestration compound according to some embodiments of the present disclosure. [Figure 13B] FIG. 1 illustrates a lead organophosphate sequestration compound according to some embodiments of the present disclosure. [Figure 13C] FIG. 1 illustrates a lead organophosphate sequestration compound according to some embodiments of the present disclosure. [Figure 14A] FIG. 1 illustrates a lead organophosphate sequestration compound according to some embodiments of the present disclosure. [Figure 14B] FIG. 1 illustrates a lead organophosphate sequestration compound according to some embodiments of the present disclosure. [Figure 15A] FIG. 1 illustrates a lead organophosphate sequestration compound according to some embodiments of the present disclosure. [Figure 15B] FIG. 1 illustrates a lead organophosphate sequestration compound according to some embodiments of the present disclosure. [Figure 16A] FIG. 1 illustrates an organosulfate lead sequestration compound according to some embodiments of the present disclosure. [Figure 16B] FIG. 1 illustrates an organosulfate lead sequestration compound according to some embodiments of the present disclosure. [Figure 16C] FIG. 1 illustrates an organosulfate lead sequestration compound according to some embodiments of the present disclosure. [Figure 17A] FIG. 1 illustrates an organosulfate lead sequestration compound according to some embodiments of the present disclosure. [Figure 17B] FIG. 1 illustrates an organosulfate lead sequestration compound according to some embodiments of the present disclosure. [Figure 18A] FIG. 1 illustrates an organosulfate lead sequestration compound according to some embodiments of the present disclosure. [Figure 18B] FIG. 1 illustrates an organosulfate lead sequestration compound according to some embodiments of the present disclosure. [Figure 19A] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 19B]FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 19C] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 19D] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 19E] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 20] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 21A] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 21B] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 21C] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 21D] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 21E] FIG. 1 illustrates a lead sequestration compound attached to an inorganic material according to some embodiments of the present disclosure. [Figure 22A] FIG. 1 illustrates a lead sequestration compound attached to silica gel according to some embodiments of the present disclosure. [Figure 22B] FIG. 1 illustrates a lead sequestration compound attached to silica gel according to some embodiments of the present disclosure. [Figure 22C] FIG. 1 illustrates a lead sequestration compound attached to silica gel according to some embodiments of the present disclosure. [Figure 22D] FIG. 1 illustrates a lead sequestration compound attached to silica gel according to some embodiments of the present disclosure. [Figure 23A] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 23B]FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 24A] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 24B] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 24C] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 24D] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 24E] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 25A] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 25B] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 25C] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 26] FIG. 1 illustrates a lead sequestration compound attached to a polymer according to some embodiments of the present disclosure. [Figure 27] FIG. 1 illustrates the structure of a crosslinked porous resin (CPR) according to some embodiments of the present disclosure. [Figure 28] FIG. 1 shows a lead sequestration compound attached to a CPR according to some embodiments of the present disclosure. [Figure 29] FIG. 1 is a schematic diagram illustrating components of an example PV device according to some embodiments of the present disclosure. [Diagram 30] FIG. 1 is a schematic diagram illustrating components of an example apparatus according to some embodiments of the present disclosure. [Diagram 31] FIG. 1 shows X-ray diffraction patterns of perovskite materials according to some embodiments of the present disclosure. [Diagram 32]FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. [Diagram 33] FIG. 1 is a schematic diagram illustrating components of a photovoltaic device according to some embodiments of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] The features and advantages of the present disclosure will be readily apparent to those skilled in the art, and many modifications may be made by those skilled in the art that fall within the scope of the present invention.

[0009] The present disclosure generally relates to compositions, apparatus and methods of use of materials in photovoltaic cells in generating electrical energy from solar radiation, and some or all of the materials according to certain embodiments of the present disclosure may be advantageously used in any organic or other electronic device, some examples of which include, but are not limited to, batteries, field effect transistors (FETs), light emitting diodes (LEDs), nonlinear optical devices, transistors, ionizing radiation detectors, memristors, capacitors, rectifiers, and / or rectifying antennas.

[0010] In certain embodiments, the present disclosure may provide PV and other similar devices (e.g., batteries, hybrid PV cells, multi-junction PVs, FETs, LEDs, X-ray detectors, gamma ray detectors, photodiodes, CCDs, etc.). In some embodiments, such devices may have improved active materials, interfacial layers (IFLs), and / or one or more perovskite materials. The perovskite materials may be incorporated into one or more various aspects of the PV or other devices. Perovskite materials according to various embodiments are described in more detail below.

[0011] (Photovoltaic cells and other electronic devices) Some PV embodiments are described by reference to an exemplary depiction of a perovskite material device as shown in FIG. 1. An exemplary PV architecture according to an embodiment may be substantially in the form of substrate-anode-IFL-active layer-IFL-cathode. The active layer of some embodiments may be photoactive and / or include photoactive materials. Other layers and materials may be utilized in the cell as known in the art. Additionally, it should be noted that the use of the term "active layer" is not meant to explicitly or implicitly limit or define the properties of any other layers. For example, in an embodiment, either or both of the IFLs may be active, so long as they may be semiconducting. In particular, referring to FIG. 1, a generic PV cell 1000 is shown, illustrating the highly interfacial nature of some layers within the PV. The PV 1000 represents a generic architecture applicable to some PV devices, such as perovskite material PV embodiments. The PV cell 1000 includes transparent substrate layers 1010 and 1070, which may be glass (or a similar material transparent to solar radiation) allowing solar radiation to pass through the layers. The transparent layers of some embodiments are also referred to as superstrates or substrates, which may include any one or more of a variety of rigid or flexible materials, such as glass, polyethylene, polypropylene, polycarbonate, polyimide, PMMA, PET, PEN, Kapton, or quartz. In general, the term substrate is used to describe the material on which the device is deposited during fabrication. The photoactive (PAM) layer 1040 may be comprised of electron donors or p-type materials, and / or electron acceptors or n-type materials, and / or ambipolar semiconductor materials that exhibit both p-type and n-type material properties, and / or intrinsic semiconductors that exhibit neither n-type nor p-type material properties. In some embodiments, the photoactive layer 1040 may be a perovskite material as described herein. The active layer, i.e., PAM layer 1040 as shown in Figure 1, is sandwiched between two conductive electrode layers 1020 and 1060. In Figure 1, electrode layer 1020 may be a transparent conductor, such as tin-doped indium oxide (ITO material), or other materials described herein.In some embodiments, the second electrode 1060 may be transparent. The second electrode layer 1060 may be an aluminum material or other metal, or other conductive material such as carbon. Other materials known in the art may be used. The cell 1100 also includes an interfacial layer (IFL) 1030, as shown in the example of FIG. 1. The IFL may aid in charge separation. In other embodiments, the IFL 1030 may include a multi-layer IFL. For example, the perovskite material device may include zero, one, two, three, four, five, or more interfacial layers (such as the example device of FIG. 2, which includes four interfacial layers 2030, 2050, 2055, and 2070). There may also be an IFL 1050 adjacent to the second electrode 1060. In some embodiments, the IFL 1050 adjacent to the second electrode 1060 may additionally or instead have a multi-layer IFL. The IFL according to an embodiment may be semiconducting in nature and may be either intrinsic, ambipolar, p-type, or p-type. Alternatively, it may be dielectric in nature. In an embodiment, the IFL on the cathode side of the device (e.g., IFL 1050 shown in FIG. 1) may be p-type and the IFL on the anode side of the device (e.g., IFL 1030 shown in FIG. 1) may be n-type. However, in other embodiments, the cathode side IFL may be n-type and the anode side IFL may be p-type. The cell 1100 may be attached to electrical leads by the electrodes 1060 and 1020 and a discharge unit such as a battery, a motor, a capacitor, an electrical grid, or any other electrical load.

[0012] In various embodiments, the device has an interface layer between any two other layers and / or materials, if necessary. However, the device does not necessarily have to include an interface layer. For example, a perovskite material device may include zero, one, two, three, four, five, or more interface layers (such as the exemplary device of FIG. 2, which includes four interface layers 2030, 2050, 2055, and 2070). The interface layer may include any suitable material that improves charge transport and / or charge collection between two layers or materials. This may also help to inhibit or reduce the possibility of charge recombination after charge is transported from one of the materials adjacent to the interface layer. The interface layer may further homogenize the substrate physically and electrically, resulting in changes to the substrate's roughness, dielectric constant, adhesion, and creation or annihilation of defects (e.g., charge traps, surface states).Suitable interface materials include Ag, Al, Au, B, Bi, Ca, Cd, Ce, Co, Cu, Fe, Ga, Ge, H, In, Mg, Mn, Mo, Nb, Ni, Pt, Sb, Sc, Si, Sn, Ta, Ti, V, W, Y, Zn, Zr; carbides of any of the aforementioned metals (e.g., SiC, Fe3C, WC, VC, MoC, NbC); silicides of any of the aforementioned metals (e.g., Mg2Si, SrSi2, Sn2Si); indium tin oxide, aluminum doped zinc oxide (AZO), Any oxide of the foregoing metals (e.g., alumina, silica, titania, SnO2, ZnO, NiO, ZrO2, HfO2), including transparent conductive oxides ("TCOs") such as cadmium oxide (CdO) and fluorine-doped tin oxide (FTO); any sulfide of the foregoing metals (e.g., CdS, MoS2, SnS2); any nitride of the foregoing metals (e.g., GaN, Mg3N2, TiN, BN, Si3N4); any selenide of the foregoing metals (e.g., CdSe, FeS2 , ZnSe); tellurides of any of the above metals (e.g., CdTe, TiTe2, ZnTe); phosphides of any of the above metals (e.g., InP, GaP, GaInP); arsenides of any of the above metals (e.g., CoAs3, GaAs, InGaAs, NiAs); antimonides of any of the above metals (e.g., AlSb, GaSb, InSb); halides of any of the above metals (e.g., CuCl, CuI, BiI3); pseudohalides of any of the above metals (e.g., CuSCN, AuCN, Fe(SCN)2); carbonates of any of the above metals (e.g., CaCO3, Ce2(CO3)3); functionalized or non-functionalized alkylsilyl groups; graphite; graphene; fullerenes; carbon nanotubes; any of the mesoporous and / or interfacial materials discussed elsewhere herein; and combinations thereof (including, in certain embodiments, bilayers, trilayers, or multilayers of combined materials). In some embodiments, the interfacial layer may include a perovskite material. Additionally, the interfacial layer may include doped embodiments of any of the interfacial materials described herein (e.g., Y-doped ZnO, N-doped single-walled carbon nanotubes).The interfacial layer may also include a compound containing three of the above materials (e.g., CuTiO3, Zn2SnO4), or a compound containing four of the above materials (e.g., CoNiZnO). The aforementioned materials may exist in planar, mesoporous, or other nanostructured morphologies (e.g., rods, spheres, flowers, pyramids), or aerogel structures. U.S. Pat. No. 11,171,290, incorporated herein by reference, describes additional types of interfacial layers and suitable materials for the IFLs of the present disclosure.

[0013] Also, some perovskite material PV cells may have so-called "tandem" PV devices that include two or more perovskite photoactive layers. FIG. 2 shows an example of a tandem PV device that includes two photoactive materials 2040 and 2060. In some embodiments, both photoactive materials 2040 and 2060 in FIG. 2 may be perovskite materials. FIG. 2 shows a two-terminal tandem PV device 2000. That is, two photoactive materials are integrated into a single monolithic PV cell. In such a tandem PV cell, the interface layer between the two photoactive layers, such as IFLs 2050 and 2055 in FIG. 2, may include a multi-layer or composite IFL. In some embodiments, the layer sandwiched between the two photoactive layers of the tandem PV device may include an electrode layer. In some embodiments, the tandem PV device may be a four-terminal device, such as the device shown in FIG. 32. A four-terminal tandem PV device has two subcells that are electrically independent from each other but may be optically coupled.

[0014] A two-terminal tandem PV device may have the following layers, in order, from top to bottom or bottom to top: a first substrate, a first electrode, a first interfacial layer, a first perovskite material, a second interfacial layer, a second electrode, a third interfacial layer, a second perovskite material, a fourth interfacial layer, and a third electrode. In an embodiment, the first and third interfacial layers may be hole transporting interfacial layers and the second and fourth interfacial layers may be electron transporting interfacial layers. In other embodiments, the first and third interfacial layers may be electron transporting interfacial layers and the second and fourth interfacial layers may be hole transporting interfacial layers. In yet another embodiment, the first and fourth interfacial layers may be hole transporting interfacial layers and the second and third interfacial layers may be electron transporting interfacial layers. In other embodiments, the first and fourth interfacial layers may be electron transporting interfacial layers and the second and third interfacial layers may be hole transporting interfacial layers.

[0015] In a tandem PV device, the first and second perovskite materials may have different bandgaps. In some embodiments, the first perovskite material is formamidinium lead bromide (FAPbBr3) and the second perovskite material is formamidinium lead iodide (FAPbI3). In other embodiments, the first perovskite material may be methylammonium lead bromide (MAPbBr3) and the second perovskite material may be formamidinium lead iodide (FaPbI3). In other embodiments, the first perovskite material may be methylammonium lead bromide (MAPbBr3) and the second perovskite material may be methylammonium lead iodide (MAPbI3).

[0016] (Perovskite materials) The perovskite material may be incorporated into one or more aspects of a PV or other device. The perovskite material according to some embodiments has the general formula w M y X zwherein C comprises one or more cations (e.g., amines, ammonium, phosphonium, Group 1 metals, Group 2 metals, and / or other cations or cation-like compounds); M comprises one or more metals (e.g., including Be, Mg, Ca, Sr, Ba, Fe, Cd, Co, Ni, Cu, Ag, Au, Hg, Sn, Ge, Ga, Pb, In, Tl, Sb, Bi, Ti, Zn, Cd, Hg, and Zr); X comprises one or more anions; and w, y, and z represent real numbers between 1 and 20. In some embodiments, C may comprise one or more organic cations. In certain embodiments, each organic cation C may be larger than each metal M, and each anion X may be capable of binding to both the cation C and the metal M.

[0017] In certain embodiments, C is ammonium, having the general formula [NR4] + where the R groups can be the same or different. Suitable R groups include, but are not limited to, hydrogen, methyl, ethyl, propyl, butyl, pentyl groups or isomers thereof; any alkane, alkene, or alkyne C x H y , where x=1-20 and y=1-42; cyclic, branched, or linear; halogenated alkyl, C x H y X z, x=1-20, y=0-42, z=1-42, X=F, Cl, Br, or I; any aromatic group (e.g., phenyl, alkylphenyl, alkoxyphenyl, pyridine, naphthalene); cyclic complexes containing at least one N in the ring (e.g., pyridine, pyrrole, pyrrolidine, piperidine, tetrahydroquinoline); any sulfur-containing group (e.g., sulfoxide, thiol, alkylsulfide); any nitrogen-containing group (nitroxide, amine); any phosphorus-containing group (phosphate); any boron-containing group (e.g., boronic acid); any organic acid (e.g., acetic acid, propanoic acid); and their ester or amide derivatives; any amino acid including α, β, γ, and larger derivatives (e.g., glycine, cysteine, proline, glutamic acid, arginine, serine, histidine, 5-ammonium valerate); any silicon-containing group (e.g., siloxane); and any alkoxy or group -OC x H y , where x=0~20, y=1~42;

[0018] In certain embodiments, C is formamidinium, having the general formula [RNCRNR] + where the R groups can be the same or different. Suitable R groups include, but are not limited to, hydrogen, methyl, ethyl, propyl, butyl, pentyl groups or isomers thereof; any alkane, alkene, or alkyne C x H y , where x=1-20, y=1-42, cyclic, branched or linear; halogenated alkyl, C x H y X z, x=1-20, y=0-42, z=1-42, X=F, Cl, Br, or I; any aromatic group (e.g., phenyl, alkylphenyl, alkoxyphenyl, pyridine, naphthalene); cyclic complexes containing at least one N in the ring (e.g., imidazole, benzimidazole, pyrimidine, (azolidinylidenemethyl)pyrrolidine, triazole); any sulfur-containing group (e.g., sulfoxide, thiol, alkylsulfide); any nitrogen-containing group (nitroxide, amine); any phosphorus-containing group (phosphate); any boron-containing group (e.g., boronic acid); any organic acid (acetic acid, propanoic acid) and its ester or amide derivatives; any amino acid including α, β, γ and larger derivatives (e.g., glycine, cysteine, proline, glutamic acid, arginine, serine, histidine, 5-ammonium valerate); any silicon-containing group (e.g., siloxane); and any alkoxy or group -OC. x H y , where x=0~20, y=1~42;

[0019] [ka] Formula 1 contains the general formula [R2NCRNR2] as described above. + Formula 2 shows the structure of some example formamidinium cations that can function as the cation "C" in perovskite materials.

[0020] [ka] In certain embodiments, C is guanidinium, having the general formula [(RN)C=NR] + where the R groups can be the same or different groups. Suitable R groups include, but are not limited to, hydrogen, methyl, ethyl, propyl, butyl, pentyl groups or isomers thereof; any alkane, alkene, or alkyne C x H y, where, x=1-20, y=1-42, cyclic, branched or linear); alkyl halide, C x H y X z , x=1-20, y=0-42, z=1-42, X=F, Cl, Br, or I; any aromatic group (e.g., phenyl, alkylphenyl, alkoxyphenyl, pyridine, naphthalene); cyclic complexes in which at least one nitrogen is contained within the ring (e.g., octahydropyrimido[1,2-a]pyrimidine, pyrimido[1,2-a]pyrimidine, hexahydroimidazo[1,2-a]imidazole, hexahydropyrimidin-2-imine); any sulfur-containing group (e.g., sulfoxide, thiol, sulfur, any nitrogen-containing group (nitroxide, amine); any phosphorus-containing group (phosphate); any boron-containing group (e.g., boronic acid); any organic acid (acetic acid, propanoic acid) and its ester or amide derivatives; any amino acid including alpha, beta, gamma and larger derivatives (e.g., glycine, cysteine, proline, glutamic acid, arginine, serine, histidine, 5-ammonium valerate); any silicon-containing group (e.g., siloxane); and any alkoxy or group O-C. x H y , where x=0~20, y=1~42;

[0021] [ka] Formula 3 includes the general formula [(R2N)2C=NR2] as mentioned above. + Formula 4 shows the structure of some example guanidinium cations that can function as the cation "C" in perovskite materials.

[0022] [ka] TIFF2024543927000006.tif99170 In certain embodiments, C is an ethenetetramine cation, having the general formula [(R2N)2C=C(NR2)2] +where the R groups can be the same or different groups. Suitable R groups include, but are not limited to, hydrogen, methyl, ethyl, propyl, butyl, pentyl groups or isomers thereof; any alkane, alkene, or alkyne C x H y , where x=1-20 and y=1-42; cyclic, branched, or linear; halogenated alkyl, C x H y X z , x=1-20, y=0-42, z=1-42, X=F, Cl, Br, or I; any aromatic group (e.g., phenyl, alkylphenyl, alkoxyphenyl, pyridine, naphthalene); cyclic complexes in which at least one nitrogen is contained within the ring (e.g., 2-hexahydropyrimidin-2-ylidenehexahydropyrimidine, octahydropyrazino[2,3-b]pyrazine, pyrazino[2,3-b]pyrazine, quinoxalino[2,3-b]quinoxaline); any sulfur-containing group ( any nitrogen-containing group (nitroxide, amine); any phosphorus-containing group (phosphate); any boron-containing group (e.g., boronic acid); any organic acid (acetic acid, propanoic acid) and its ester or amide derivatives; any amino acid including alpha, beta, gamma and larger derivatives (e.g., glycine, cysteine, proline, glutamic acid, arginine, serine, histidine, 5 ammonium valerate); any silicon-containing group (e.g., siloxane); and any alkoxy or group OC. x H y , where x = 0 to 20 and y = 1 to 42;

[0023] [ka] Formula 5 is the general formula as mentioned above: [(R2N)2C=C(NR2)2] + Formula 6 shows the structure of some example ethenetetraamine ions that can function as the cation "C" in perovskite materials.

[0024] [ka] In certain embodiments, C is an imidazolium cation, having the general formula [CRNRCRNRCR] + where the R groups can be the same or different. Suitable R groups include, but are not limited to, hydrogen, methyl, ethyl, propyl, butyl, pentyl groups or isomers thereof; any alkane, alkene, or alkyne C x H y , where x=1-20 and y=1-42; cyclic, branched or linear; halogenated alkyl, C x H y X z , x=1-20, y=0-42, z=1-42, X=F, Cl, Br, or I; any aromatic group (e.g., phenyl, alkylphenyl, alkoxyphenyl, pyridine, naphthalene); cyclic complexes containing at least one nitrogen in the ring (e.g., 2-hexahydropyrimidin-2-ylidenehexahydropyrimidine, octahydropyrazino[2,3-b]pyrazine, pyrazino[2,3-b]pyrazine, quinoxalino[2,3-b]quinoxaline); any sulfur-containing group (e.g., sulfoxide, thiol, , alkyl sulfides); any nitrogen-containing group (nitroxides, amines); any phosphorus-containing group (phosphates); any boron-containing group (e.g., boronic acid); any organic acid (acetic acid, propanoic acid) and its ester or amide derivatives; any amino acid including alpha, beta, gamma and larger derivatives (e.g., glycine, cysteine, proline, glutamic acid, arginine, serine, histidine, 5-ammonium valerate); any silicon-containing group (e.g., siloxanes); and any alkoxy or group -OC. x H y , where x = 0 to 20 and y = 1 to 42;

[0025] [ka] In some embodiments, X may include one or more halides. In certain embodiments, X may additionally or alternatively include a Group 16 anion. In certain embodiments, the Group 16 anion may be an oxide, sulfide, selenide, or telluride. In certain embodiments, X may additionally or alternatively include one or more pseudohalides (e.g., cyanide, cyanate, isocyanate, fulminate, thiocyanate, isothiocyanate, azide, tetracarbonylcobaltate, carbamoyldicyanomethanide, dicyanonitrosomethanide, dicyanoamide, and tricyanomethanate).

[0026] For purposes of illustration, and without implying any limitation, formula C w M y X z Exemplary embodiments of perovskite materials having the formula: are described below. In one embodiment, the perovskite material may have the empirical formula: CMX3, where M comprises one of the metals and C comprises one or more of the cations, Group 1 metals, Group 2 metals, and / or other cations or cation-like compounds.

[0027] In another embodiment, the perovskite material may have an empirical formula C'M2X6, where C' comprises a cation having a 2+ charge, including one or more of the above cations, butanediammonium, Group 1 metals, Group 2 metals, and / or other cations or cation-like compounds.

[0028] In another embodiment, the perovskite material may have an empirical formula C'MX4, where C' comprises a cation having a 2+ charge, including one or more of the above cations, diammonium butane, Group 1 metals, Group 2 metals, and / or other cations or cation-like compounds. In such an embodiment, the perovskite material may have a 2D structure. In one embodiment, the perovskite material may have the empirical formula C3M2X9, where C includes one or more of the above cations, Group 1 metals, Group 2 metals, and / or other cations or cation-like compounds.

[0029] In one embodiment, the perovskite material may have the empirical formula CM2X7, where C includes one or more of the above cations, Group 1 metals, Group 2 metals, and / or other cations or cation-like compounds.

[0030] In one embodiment, the perovskite material may have the empirical formula C2MX4, where C includes one or more of the cations, group 1 metals, group 2 metals, and / or other cations or cation-like compounds. The perovskite material may also include mixed ion formulations, where C, M, or X includes two or more species. In some embodiments, the perovskite material may include two or more anions or three or more anions. In some embodiments, the perovskite material may include two or more cations or three or more cations. In certain embodiments, the perovskite material may include two or more metals or three or more metals.

[0031] In one example, the perovskite material in the active layer is CMX 3-y X' y (0≧y≧3), where C comprises one or more cations (e.g., amines, ammonium, Group 1 metals, Group 2 metals, formamidinium, guanidinium, ethenetetramine, phosphonium, imidazolium, and / or other cations or cation-like compounds); M comprises one or more metals (e.g., Be, Mg, Ca, Sr, Ba, Fe, Cd, Co, Ni, Cu, Ag, Au, Hg, Sn, Ge, Ga, Pb, In, Tl, Sb, Bi, Ti, Zn, Cd, Hg, and Zr); and X and X′ comprise one or more anions. In one embodiment, the perovskite material is CPbI 3-y Cl y In another example, the perovskite material in the active layer may comprise a compound represented by formula C1-x C' x In another example, the perovskite material in the active layer may have the formula CM 1-z M' z X3 (0≧z≧1), where M and M′ comprise one or more metals as described above. In one example, the perovskite material in the active layer may have the formula C 1-x C' x M 1-z M' z X 3-y X' y (0≧x≧1; 0≧y≧3; 0≧z≧1). C and C' comprise one or more cations as described above; M and M' comprise one or more metals as described above; and X and X' comprise one or more anions as described above.

[0032] For purposes of illustration, and without implying any limitation, an exemplary embodiment of a perovskite material is Cs 0.1 FA 0.9 Pb(I 0.9 Cl 0.1 )3;Rb 0.1 FA 0.9 Pb(I 0.9 Cl 0.1 )3, Cs 0.1 FA 0.9 PbI3;FAPb 0.5 Sn 0.5 I3;FA 0.83 Cs 0.17 Pb(I 0.6 Br 0.4 )3;FA 0.83 Cs 0.12 Rb 0.05 Pb(I 0.6 Br 0.4 )3 and FA 0.85 MA 0.15 Pb(I 0.85 Br 0.15 )3.

[0033] (Composite Perovskite Material Device Design) In certain embodiments, the present disclosure may provide hybrid designs of PV and other similar devices (e.g., batteries, hybrid PV cells, FETs, LEDs, nonlinear optical elements (NLOs), waveguides, etc.) that include one or more perovskite materials. For example, one or more perovskite materials may function as either or both of the first and second active materials of certain embodiments. More generally, certain embodiments of the present disclosure provide PV or other devices having an active layer that includes one or more perovskite materials. In such embodiments, perovskite materials (i.e., materials that include any one or more perovskite materials) may be used in active layers of various configurations. Furthermore, perovskite materials may function as any one or more components of the active layer, as described in more detail below. In certain embodiments, the same perovskite material may perform multiple such functions, while in other embodiments, multiple perovskite materials may be included in a device, with each perovskite material performing one or more such functions. In certain embodiments, regardless of the role the perovskite material plays, it may be prepared and / or present in the device in various states. For example, in some embodiments, it may be substantially solid. A solution or suspension may be coated or deposited within the device (e.g., onto another component of the device, such as a mesoporous, interfacial, charge transport, photoactive, or other layer, and / or electrode). The perovskite material in some embodiments may be formed in-situ on a surface of another component of the device (e.g., by deposition of an underlying layer as a thin film solid). Any other suitable means of forming a layer comprising the perovskite material may be used.

[0034] In general, a perovskite material device may have a first electrode, a second electrode, and an active layer comprising a perovskite material, with the active layer being at least partially disposed between the first electrode and the second electrode. In some embodiments, the first electrode may be one of the anode and the cathode, and the second electrode may be the other of the anode and the cathode. The active layer according to certain embodiments may include any one or more active layer components, including one or more of a charge transport material, a liquid electrolyte, a mesoporous material, a photoactive material (e.g., dye, silicon, cadmium telluride, cadmium sulfide, cadmium selenide, copper indium gallium selenide, gallium arsenide, germanium indium phosphide, semiconducting polymers, other photoactive materials), and an interface material. Any one or more of these active layer components may include one or more perovskite materials. In some embodiments, some or all of the active layer components may be disposed in whole or in part in a sublayer. For example, the active layer may include any one or more of an interfacial layer including an interfacial material, a mesoporous layer including a mesoporous material, and a charge transport layer including a charge transport material. Furthermore, in some embodiments, an interfacial layer may be included between any two or more other layers of the active layer and / or between an active layer member and an electrode. Reference to a layer may include the final arrangement (e.g., substantially separate portions of each material separately definable within the device) and / or reference to a layer may refer to the arrangement of the device during construction, regardless of the possibility of subsequent mixing of the materials in each layer. In some embodiments, the layers may include separate and substantially continuous materials (e.g., the layers may be in the form stylistically shown in FIG. 1).

[0035] In some embodiments, the perovskite material device may be a field effect transistor (FET). The FET perovskite material device may include a source electrode, a drain electrode, a gate electrode, a dielectric layer, and a semiconducting layer. In some embodiments, the semiconducting layer of the FET perovskite material device may be a perovskite material.

[0036] Perovskite material devices according to certain embodiments may include one or more substrates, if necessary. In certain embodiments, one or both of the first electrode and the second electrode may be coated or otherwise disposed on a substrate, with the electrodes disposed substantially between the substrate and the active layer. The materials of the components of the device (e.g., substrate, electrodes, active layer and / or active layer components) may be either rigid or flexible in whole or in part in various embodiments. In some embodiments, the electrodes may function as substrates, thereby eliminating the need for a separate substrate.

[0037] Furthermore, perovskite material devices according to certain embodiments may include an anti-reflective layer or coating (ARC) if required.

[0038] Some description of the various materials that may be included in a perovskite material device is provided in part with reference to FIG. 29. FIG. 29 is a schematic diagram of a tandem two-terminal perovskite material device 3900 according to an embodiment. In FIG. 29 and other figures of the present disclosure illustrating perovskite devices (e.g., FIGS. 1-2, 4-9, 31, and 32-33), various components of the device are shown as separate layers comprising continuous materials, but it should be understood that such figures are schematic. Thus, embodiments according thereto may have such separate layers, and / or substantially intermixed non-continuous layers, consistent with the use of "layer" discussed above. The device 3900 includes a first substrate 3901 and a second substrate 3913. A first electrode 3902 is disposed on an inner surface of the first substrate 3901, and a second electrode 3912 is disposed on an inner surface of the second substrate 3913. The active layer 3950 is sandwiched between two electrodes 3902 and 3912. The active layer 3950 includes a mesoporous layer 3904, first and second photoactive materials 3906 and 3908, a charge transport layer (CTL) 3910, and several interfacial layers. FIG. 29 further illustrates an example of a device 3900 according to an embodiment, where the sub-layers of the active layer 3950 are separated by interfacial layers, which are further disposed on each electrode 3902 and 3912. In particular, second, third, and fourth interfacial layers 3905, 3907, and 3909 are disposed between the mesoporous layer 3904, the first photoactive material 3906, the second photoactive material 3908, and the charge transport layer 3910, respectively. The first and fifth interfacial layers 3903 and 3911 are disposed between (i) the first electrode 3902 and the mesoporous layer 3904, and (ii) the charge transport layer 3910 and the second electrode 3912, respectively. Thus, the architecture of the exemplary device shown in FIG. 29 can be characterized as substrate-electrode-active layer-electrode-substrate. The structure of the active layer 3950 can be characterized as interfacial layer-mesoporous layer-interfacial layer-photoactive material-interfacial layer-photoactive material-interfacial layer-charge transport layer-interfacial layer. In some embodiments, no interfacial layers may be present. Alternatively, one or more interfacial layers may be included only between some but not all components of the active layer and / or components of the device.

[0039] Substrates, such as one or both of the first substrate 3901 and the second substrate 3913, may be flexible or rigid. If two substrates are included, at least one should be transparent or semi-transparent to electromagnetic (EM) radiation (e.g., UV, visible, or IR radiation, etc.). If one substrate is included, it may be transparent or semi-transparent as well, although this is not necessary as long as some portion of the device allows EM radiation to contact the active layer 3950. Suitable substrate materials include any one or more of glass, sapphire, magnesium oxide (MgO), mica, polymers (e.g., PEN, PET, PEG, polyolefins, polypropylene, polyethylene, polycarbonate, PMMA, polyamide, vinyl, Kapton), ceramic, carbon, composites (e.g., fiberglass, Kevlar, carbon fiber), fabrics (e.g., cotton, nylon, silk, wool), wood, drywall, tile (e.g., ceramic, composite, or clay), metal, steel, silver, gold, aluminum, magnesium, concrete, and combinations thereof.

[0040] As previously mentioned, an electrode (e.g., one of electrodes 3902 and 3912 in FIG. 29) may be either an anode or a cathode. In some embodiments, one electrode may function as a cathode and the other electrode as an anode. One or both of electrodes 3902 and 3912 may be coupled to leads, cables, wires, or other means that allow charge transport to and / or from device 3900 and / or device 118. The electrodes may be constructed of any conductive material, and at least one electrode should be transparent or semi-transparent to EM radiation and / or positioned such that EM radiation can contact at least a portion of active layer 3950. Suitable materials include any one or more of indium tin oxide or tin-doped indium oxide (ITO), fluorine-doped tin oxide (FTO), cadmium oxide (CdO), zinc indium tin oxide (ZITO), aluminum zinc oxide (AZO), aluminum (Al), gold (Au), silver (Ag), calcium (Ca), chromium (Cr), copper (Cu), magnesium (Mg), titanium (Ti), steel, carbon (and its allotropes), doped carbon (e.g., nitrogen-doped), nanoparticles in a core-shell configuration (e.g., silicon-carbon core-shell structures), and combinations thereof.

[0041] The mesoporous material (e.g., the material included in mesoporous layer 3904 of FIG. 29) may include any pore-containing material. In certain embodiments, the pores may have a diameter ranging from about 1 to about 100 nm. In other embodiments, the diameter of the pores may range from about 2 to about 50 nm. Suitable mesoporous materials include any interfacial material and / or mesoporous material described elsewhere herein, aluminum (Al), bismuth (Bi), cerium (Ce), hafnium (Hf), indium (In), molybdenum (Mo), niobium (Nb), nickel (Ni), silicon (Si), titanium (Ti), vanadium (V), zinc (Zn), zirconium (Zr), oxides of any one or more of the foregoing metals (e.g., alumina, ceria, titania, zinc oxide, zirconia, etc.), sulfides of any one or more of the foregoing metals, nitrides of any one or more of the foregoing metals, and any combination thereof. In some embodiments, any of the materials disclosed herein as IFLs may be mesoporous materials. In other embodiments, the device shown in Figure 29 may not include a mesoporous material layer, but may include only a non-mesoporous thin film, or "compact" IFL.

[0042] The photoactive material (e.g., first or second photoactive material 3906 or 3908 in FIG. 29) can be silicon (e.g., polycrystalline silicon, single crystal silicon, or amorphous silicon), cadmium telluride, cadmium sulfide, cadmium selenide, copper indium gallium selenide, copper indium selenide, copper zinc tin sulfide, gallium arsenide, germanium, germanium indium phosphide, indium phosphide, one or more semiconductor polymers (e.g., polythiophenes (e.g., poly(3-hexylthiophene) and its derivatives, or P3HT); polyheptadecanylcarbazole dithienylbenzothiadiazole, and The photoactive compounds may include any one or more of carbazole-based copolymers, such as carbazole-based copolymers and derivatives thereof (e.g., PCDTBT); other copolymers, such as polycyclopentadithiophene-benzothiadiazole and derivatives thereof (e.g., PCDTBT), polybenzodithiophenyl-thienothiophenediyl and derivatives thereof (e.g., PTB6, PTB7, PTB7-th, PCE-10); poly(triarylamine) compounds and derivatives thereof (e.g., PTAA); polyphenylenevinylene and derivatives thereof (e.g., MDMO-PPV, MEH-PPV), and combinations thereof.

[0043] In certain embodiments, the photoactive material may additionally or alternatively include a dye (e.g., N719, N3, other ruthenium-based dyes). In some embodiments, the dye (regardless of composition) may be coated onto another layer (e.g., the mesoporous layer and / or the interfacial layer). In some embodiments, the photoactive material may include one or more perovskite materials. The perovskite-containing photoactive material may be in solid form, or in some embodiments, may take the form of a dye containing suspension or solution that includes the perovskite material. Such a solution or suspension may be coated onto other device components in a similar manner as other dyes. In some embodiments, the solid perovskite-containing material may be deposited by any suitable means (e.g., vapor deposition, solution deposition, direct placement of solid material). Devices according to various embodiments may include one, two, three, or more photoactive compounds (e.g., one, two, three, or more perovskite materials, dyes, or combinations thereof). In certain embodiments including multiple dyes or other photoactive materials, each of the two or more dyes or other photoactive materials may be separated by one or more interfacial layers or may be at least partially intermixed.

[0044] In some embodiments, the photoactive material may comprise any photoactive material described herein, such as thin film semiconductors (e.g., CdTe, CZTS, CIGS), photoactive polymers, dye-sensitized photoactive materials, fullerenes, small molecule photoactive materials, and crystalline and polycrystalline semiconductor materials (e.g., silicon, GaAs, InP, Ge). In yet other embodiments, one or both of active layers 3906a and 3908a may include a light emitting diode (LED), a field effect transistor (FET), a thin film cell layer, or a combination thereof. In an embodiment, one of active layers 3906a and 3908a may comprise a photoactive material and the other may comprise an LED, a FET, a thin film cell layer, or a combination thereof.

[0045] As used herein, "charge transport material" refers to any solid, liquid, or other material that can collect and / or transport charge carriers (electrons or holes). The charge transport material (e.g., the charge transport material of charge transport layer 3910 of FIG. 29) may include a solid charge transport material (i.e., colloquially labeled solid electrolyte) or may include a liquid electrolyte and / or an ionic liquid. In a PV device according to an embodiment, the charge transport material may be capable of transporting charge carriers to an electrode. The charge carriers may include holes (whose transport makes the charge transport material just aptly labeled "hole transport material") and electrons. Depending on the placement of the charge transport material relative to either the cathode or anode in a PV or other device, the holes may be transported toward the anode and the electrons may be transported toward the cathode. Suitable examples of charge transport materials according to certain embodiments include perovskite materials; I- / I3-; Co complexes; polythiophenes (e.g., poly(3-hexylthiophene) and its derivatives, or P3HT); carbazole-based copolymers, such as polyheptadecanylcarbazole dithienylbenzothiadiazole and its derivatives (e.g., PCDTBT); other copolymers, such as polycyclopentadithiophene benzothiadiazole and its derivatives (e.g., PCDTBT), polybenzodithiophenyl-thienothiophenediyl and its derivatives (e.g., PTB6, PTB7, PTB7-th, PCE-10); poly(triarylamine) compounds and their derivatives (e.g., PTAA); spiro-OMeTAD; polyphenylenevinylene and its derivatives (e.g., MDMO-PPV, MEH-PPV); fullerenes and / or fullerene derivatives (e.g., C 60, PCBM); carbon nanotubes; graphite; graphene; carbon black; amorphous carbon; glassy carbon; carbon fiber; and combinations thereof. The charge transport material of some embodiments may be an n-type or p-type active, ambipolar, and / or intrinsic semiconductor material. The charge transport material may be disposed in proximity to one of the electrodes of the device. In some embodiments, it may be disposed adjacent to the electrode, while in other embodiments, an interfacial layer may be disposed between the charge transport material and the electrode (e.g., as shown by the fifth interfacial layer 3911 in FIG. 29). In certain embodiments, the type of charge transport material may be selected based on the electrode it is adjacent to. For example, if the charge transport material collects and / or transports holes, it may be disposed in proximity to the anode and holes may be transported to the anode. However, the charge transport material may instead be disposed in proximity to the cathode and selected or constructed to transport electrons to the cathode.

[0046] Further, in some embodiments, the perovskite material may have more than two active layers. As an example, Figure 31 is a schematic diagram illustrating an embodiment of a two-terminal perovskite material device 3900b that includes three active layers and is otherwise similar in structure to the perovskite material device 3900 shown in Figure 29. Figure 30 has active layers 3904b, 3906b, 3908b. In some embodiments, one or more of the active layers 3904b, 3906b, and 3908b may include any of the photoactive materials described with respect to Figure 29 above. Other layers shown in FIG. 30, such as layers 3901b, 3902b, 3903b, 3904b, 3905b (i.e., recombination layer), 3907b (i.e., recombination layer), 3909b, 3910b, 3911b, 3912b, and 3913, may be similar to the corresponding layers as described with respect to FIG. 29.

[0047] In an embodiment, the tandem PV device may be a four-terminal device, as shown in FIG. 32. The four-terminal device 2300 may include two subcells 2400 and 2500 that are electrically independent of each other. In an embodiment, the four-terminal device has two subcells 2400 and 2500 that are mechanically stacked on top of each other and optically coupled, so that light transmitted through the front subcell 2400 reaches the rear subcell 2500. The four-terminal PV device 2300 has a first substrate layer 2310, which may be glass (or a similar material transparent to solar radiation) through which solar radiation can be transmitted. The transparent layer in an embodiment may also be referred to as a superstrate or substrate, and may comprise any one or more of a variety of rigid or flexible materials as discussed above.

[0048] The first PAM layer 2350 of the front subcell 2400 may be comprised of an electron donor or p-type material, and / or an electron acceptor or n-type material, and / or an ambipolar semiconductor that exhibits both p-type and n-type material properties, and / or an intrinsic semiconductor that exhibits neither n-type nor p-type properties. In some embodiments, the photoactive layer 2350 may have any of the photoactive materials described above with respect to Figures 29-30. The active layer, or photoactive layer 2350 as shown in Figure 32, is sandwiched between two conductive electrode layers 2320 and 2370. As previously described, the active layer in some embodiments is not necessarily photoactive, but in the device shown in Figure 32, it is. In Figure 32, the electrode layers may be transparent conductors such as fluorine doped tin oxide (FTO material) or other materials described herein. In other embodiments, the second substrate 2390 and the second electrode 2370 may be transparent. The electrode layer 2370 may be a transparent conductor such as indium zinc oxide (IZO material) or other electrode materials described herein or known in the art. The front subcell 2400 also has interfacial layers (IFLs) 2330, 2340, 2350, 2355. The IFLs may comprise any suitable material as previously described. In some embodiments, 2330 may be a nitride, 2340 may be NiO, 2355 may be a fullerene, and / or 2360 may be SnO2. Although two IFLs are shown on either side of the photoactive layer 2350, the front subcell 2400 may have zero, one, two, three, four, five, or more interfacial layers on either side of the photoactive material layer 2350. The IFL according to some embodiments may be semiconducting in nature and may be intrinsic, ambipolar, p-type, n-type, or it may be dielectric in nature. In some embodiments, the IFLs on the cathode side of the device (e.g., IFLs 2355 and 2360 shown in FIG. 32) can be n-type and the IFLs on the anode side of the device (e.g., IFLs 2330 and 2340 shown in FIG. 32) can be p-type. However, in other embodiments, the cathode side IFL can be p-type and the anode side IFL can be n-type.The front subcell 2400 may be attached to electrical leads by electrodes 2320 and 2370 and a discharging unit such as a battery, a motor, a capacitor, an electrical grid, or any other electrical load.

[0049] The rear subcell 2500 of the PV device 2300 may have a similar or different architecture than the front subcell 2400. The rear subcell 2500 may include a second photoactive material, and in some embodiments, may include any of the photoactive materials described with respect to FIGS. 29-30. In one example, the rear subcell 2500 may have electrodes, IFLs, and other layers of the same or different architecture as the front subcell 2400. In some embodiments, one or both of the photoactive layers of the front subcell 2400 and the rear subcell 2500 may include any of the photoactive materials described with respect to FIGS. 29-30, or one may include a photoactive material and the other may include an LED, FET, thin film battery layer, or a combination thereof. The layers, such as the substrate, electrodes, and IFLs, of the front subcell 2400 and the rear subcell may be similar to the corresponding layers as described with respect to FIGS. 29-30 and may include any of the materials or configurations described as suitable for these corresponding layers.

[0050] A non-conductive layer 2380 may be disposed between and adjacent to the front subcell 2400 and the rear subcell 2500. As used herein, "non-conductive layer" means a layer that is electrically non-conductive and is not intended to define the thermal properties of the non-conductive layer, which may be thermally conductive or thermally insulating. In some embodiments, the non-conductive layer 2380 may include, but is not limited to, adhesives, epoxies, glass, laminates, waxes, polymers, resins, elastomers, thermosets, or any combination thereof. In some embodiments, the non-conductive layer 2380 may include polyvinyl acetate, polyolefins, polystyrene, polyglycols, polyorganic acids, natural rubbers, synthetic rubbers, polyesters, nylons, polyamides, polyaryls, polynucleic acids, polysaccharides, polyurethanes, acrylonitrile butadiene styrene, acrylics, acrylic polymers, acrylic resins, cross-linked porous resins, and any combination or derivative thereof. Examples of polymers suitable for certain embodiments include, but are not limited to, poly(ethylene-vinyl acetate) (EVA), high density polyethylene (HDPE), low density polyethylene (LDPE), polypropylene (PP), polystyrene (PS), polyethylene glycol (PEG / PEO), poly(methyl methacrylate) (PMMA), polyoxymethylene (POM), poly(acrylonitrile butadiene styrene) (ABS), polyphenylene sulfide (PPS), polytetrafluoroethylene (PTFE), polyvinyl chloride (PCC), polyvinyl chloride (PCF), polyvinyl chloride (PCT ... FE), polyvinylidene fluoride (PVDF), polyvinyl chloride (PVC), polyethylene terephthalate (PET), polylactic acid (PLA), polycarbonate (PC), polyether ether ketone (PEEK), polybutylene terephthalate (PBT), butylene rubber, polyisoprene, polyurethane (PU), polydimethylsiloxane (PDMS), urea formaldehyde resin, epoxy resin, phenol formaldehyde resin (PF), derivatives thereof, and any combination thereof. The configuration of the polymer backbone of the binding polymer may be isotactic, syndiotactic, or atactic. In one example, the non-conductive layer 2380 is transparent. In another example, the non-conductive layer 2380 is not transparent.

[0051] Additional more specific example embodiments of perovskite devices are further discussed with respect to another schematic drawing of an exemplary device. The schematic nature of these depictions of Figures 29-30 and 32 is likewise not intended to limit the types of devices that may be constructed according to any one or more of Figures 29-30 and 32 in an embodiment. That is, the architectures shown in Figures 29-30 and 32 may be adapted to provide BHJs, batteries, FETs, hybrid PV cells, series multi-cell PVs, parallel multi-cell PVs, and other similar devices of other embodiments of the present disclosure according to any suitable means, including both those explicitly discussed elsewhere in this application and other suitable means apparent to those of ordinary skill in the art having the benefit of this disclosure.

[0052] (Formation of perovskite material active layer) In certain embodiments, the perovskite material may be deposited onto a substrate layer as an active layer in a PV device, for example by blade coating, drop casting, spin casting, slot-die printing, screen printing, or inkjet printing, using the steps described below.

[0053] First, a lead halide precursor ink is formed. A quantity of lead halide may be collected in a clean, dry container in a controlled atmosphere environment (e.g., a controlled atmosphere box with a globe-containing porthole allows for material manipulation in an air-free environment). Suitable lead halides include, but are not limited to, lead (II) iodide, lead (II) bromide, lead (II) chloride, and lead (II) fluoride. The lead halide may include a single species of lead halide or may have a mixture of lead halides in precise ratios. In certain embodiments, the lead halide mixture may have any binary, ternary, or quaternary ratio of 0.001 to 100 mole % iodide, bromide, chloride, or fluoride. In one embodiment, the lead halide mixture may have lead (II) chloride and lead (II) iodide in a ratio of about 10:90 mol:mol. In other embodiments, the lead halide mixture may have lead(II) chloride and lead(II) iodide in a ratio of about 5:95, about 7.5:92.5, or about 15:85 mol:mol.

[0054] Alternatively, other lead salt precursors may be used in conjunction with or in place of the lead halide salt to form the precursor ink. Suitable precursor salts may have lead(II) or lead(IV) in any combination with the following anions: nitrate, nitrite, carboxylate, acetate, acetonylacetonate, formate, oxalate, sulfate, sulfite, thiosulfate, phosphate, tetrafluoroborate, hexafluorophosphate, tetra(perfluorophenyl)borate, hydride, oxide, peroxide, hydroxide, nitride, arsenate, arsenite, perchlorate, carbonate, bicarbonate, chromate, dichromate, iodate, bromate, chlorate, chlorite, hypochlorite, hypobromite, cyanide, cyanate, isocyanate, fulminate, thiocyanate, isothiocyanate, azide, tetracarbonylcobaltate, carbamoyldicyanomethanide, dicyanonitrosomethanide, dicyanamide, tricyanomethanate, amide, and permanganate.

[0055] The precursor ink may further comprise, as a salt of the aforementioned anions, a lead(II) salt or a lead(IV) salt with respect to the following metal ions Be, Mg, Ca, Sr, Ba, Fe, Cd, Co, Ni, Cu, Ag, Au, Hg, Sn, Ge, Ga, Pb, In, Tl, Sb, Bi, Ti, Zn, Cd, Hg, and Zr in a molar ratio of 0 to 100%.

[0056] A solvent may then be added to the container to dissolve the lead solids and form the lead halide precursor ink. Suitable solvents include, but are not limited to, dry N-cyclohexyl-2-pyrrolidone, alkyl-2-pyrrolidone, dimethylformamide, dialkylformamide, dimethylsulfoxide (DMSO), methanol, ethanol, propanol, butanol, tetrahydrofuran, formamide, tert-butylpyridine, pyridine, alkylpyridine, pyrrolidine, chlorobenzene, dichlorobenzene, dichloromethane, chloroform, alkylnitriles, arylnitriles, acetonitrile, alkoxyalcohols, alkoxyethanols, 2-methoxyethanol, glycols, propylene glycol, ethylene glycol, and combinations thereof. In one embodiment, the lead solids are dissolved in dry dimethylformamide (DMF). In some embodiments, the solvent may further include 2-methoxyethanol and acetonitrile. In certain embodiments, the 2-methoxyethanol and acetonitrile may be added in a volume ratio of about 25:75 to about 75:25, or at least 25:75. In certain embodiments, the solvent may have a ratio of 2-methoxyethanol and acetonitrile to DMF of about 1:100 to about 1:1, or about 1:100 to about 1:5, by volume. In certain embodiments, the solvent may have a ratio of 2-methoxyethanol and acetonitrile to DMF of at least about 1:100, by volume.

[0057] In an embodiment, the lead solids may be dissolved at a temperature of about 20° C. to about 150° C. In one embodiment, the lead halide solids are dissolved at about 85° C. The lead solids are dissolved long enough to form a solution, which may be carried out for a period of up to about 72 hours. The resulting solution forms the base of the lead halide precursor ink. In an embodiment, the lead halide precursor ink may have a lead halide concentration of between about 0.001 M and about 10 M, or about 1 M.

[0058] Optionally, certain additives may be added to the lead halide precursor ink to affect the crystallinity and stability of the final perovskite. In an embodiment, the lead halide precursor ink may further comprise an amino acid (e.g., 5-aminovaleric acid, histidine, glycine, lysine), an amino acid hydrohalide salt (e.g., 5-aminovaleric acid hydrochloride), an IFL surface modification (SAM) agent (discussed earlier herein), or a combination thereof. Suitable amino acids for the lead halide precursor ink include, but are not limited to, α-amino acids, β-amino acids, γ-amino acids, δ-amino acids, and any combination thereof. In an embodiment, formamidinium chloride may be added to the lead halide precursor ink. In other embodiments, halides of any cation discussed earlier herein may be used. In an embodiment, a combination of additives may be added to the lead halide precursor ink, including, for example, a combination of formamidinium chloride and 5-aminovaleric acid hydrochloride.

[0059] In some embodiments, additives including formamidinium chloride and / or 5-aminovaleric acid hydrochloride may be added to the lead halide precursor ink at various concentrations depending on the desired properties of the resulting perovskite material. In some embodiments, the additives may be added at a concentration of about 1 nM to about 1 M, about 1 μM to about 1 M, or about 1 μM to about 1 mM.

[0060] Optionally, in certain embodiments, water may be added to the lead halide precursor ink. For purposes of illustration and not to limit the present disclosure to any particular theory or mechanism, the presence of water affects perovskite thin film crystal growth. Under normal circumstances, water is absorbed as vapor from the air. However, by adding water directly to the lead halide precursor ink at a specific concentration, it is possible to control the crystallinity of the perovskite PV. Suitable water includes distilled water, deionized water, or any other water source that is substantially free of contaminants (including minerals). Based on optical IV sweeps, it has been found that the light-to-electrical power conversion efficiency of perovskite PV can be nearly tripled by the addition of water compared to a completely dry device.

[0061] Water may be added to the lead halide precursor ink in various concentrations depending on the desired properties of the resulting perovskite material, hi some embodiments, water may be added at a concentration of about 1 nL / mL to about 1 mL / mL, about 1 μL / mL to about 0.1 mL / mL, or about 1 μL / mL to about 20 μL / mL.

[0062] The lead halide precursor ink may then be deposited on a desired substrate. Suitable substrate layers may include any substrate layer previously identified in this disclosure. As previously described, the lead halide precursor ink may be deposited by various means, including, but not limited to, drop casting, spin coating, slot die printing, inkjet printing, gravure printing, screen printing, sputtering, PE-CVD, atomic layer deposition, thermal evaporation, spray coating, and any combination thereof. In certain embodiments, the lead halide precursor ink may be spin coated on the substrate at a speed of about 500 rpm to about 10,000 rpm for a time period of about 5 seconds to about 600 seconds. In one embodiment, the lead halide precursor ink may be spin coated on the substrate at about 3000 rpm for about 30 seconds. The lead halide precursor ink may be deposited on the substrate in an ambient atmosphere within a humidity range of about 0% relative humidity to about 50% relative humidity. The lead halide precursor ink may then be dried in a substantially water-free atmosphere, ie, less than 30% relative humidity, to form a thin film.

[0063] The thin film may then be thermally annealed at a temperature of about 20° C. to about 300° C. for up to about 24 hours. In one embodiment, the thin film may be thermally annealed at a temperature of about 50° C. for about 10 minutes. The perovskite material active layer may then be completed by a conversion process. In this process, the precursor film is immersed in or rinsed with a solution containing a solvent or mixture of solvents (e.g., DMF, isopropanol, methanol, ethanol, butanol, chloroform, chlorobenzene, dimethylsulfoxide, water) at a concentration between 0.001 M and 10 M and a salt (e.g., methylammonium iodide, formamidinium iodide, guanidinium iodide, 1,2,2-triaminovinylammonium iodide, 5-aminovaleric acid hydroiodide). Also, in certain embodiments, the thin film may be thermally post-annealed in the same manner as in the first line of this paragraph.

[0064] In an embodiment, a lead salt precursor may be deposited on a substrate to form a lead salt thin film. The substrate may have a temperature approximately equal to ambient temperature or a controlled temperature between 0° C. and 500° C. The lead salt precursor may be deposited by any of the methods previously described for the lead halide precursor ink. In certain embodiments, deposition of the lead salt precursor may include a sheet-to-sheet or roll-to-roll manufacturing method. Deposition of the lead salt precursor may be carried out in various atmospheres at ambient pressure, or at atmospheric or subambient pressure (e.g., 1 mTorr to 500 mTorr). Deposition atmospheres include ambient air, controlled humidity environments (e.g., 0 to 100 g H2O / m 3 The controlled humidity environment may comprise an environment in which the absolute humidity or % relative humidity is maintained at a fixed value, or an environment in which the absolute humidity or % relative humidity varies according to a predetermined set point or a predetermined function. In certain embodiments, deposition may be performed in a controlled humidity environment having a % relative humidity greater than or equal to 0% and less than or equal to 50%. In other embodiments, deposition may be performed in a controlled humidity environment having a % relative humidity greater than or equal to 0 gH2O / m 3 Gas, 20 gH2O / m 3 It may be carried out in a controlled humidity environment below 100° C. Unless otherwise stated, any annealing or deposition steps described herein may be carried out under the aforementioned conditions.

[0065] The lead salt precursor may be a liquid, gas, solid, or a combination of these states of matter, such as a solution, suspension, colloid, foam, gel, or aerosol. In some embodiments, the lead salt precursor may be a solution containing one or more solvents. For example, the lead salt precursor may contain one or more of N-cyclohexyl-2-pyrrolidone, alkyl-2-pyrrolidone, dimethylformamide, dialkylformamide, dimethylsulfoxide (DMSO), acetonitrile, methanol, ethanol, propanol, butanol, tetrahydrofuran, formamide, tert-butylpyridine, pyridine, alkylpyridine, pyrrolidine, chlorobenzene, dichlorobenzene, dichloromethane, chloroform, and combinations thereof. The lead salt precursor may have a single lead salt (e.g., lead(II) iodide, lead(II) thiocyanate), or any combination disclosed herein (e.g., PbI2+PbCl2; PbI2+Pb(SCN)2). The lead salt precursor may also contain one or more additives, such as amino acids (e.g., 5-aminovaleric hydroiodic acid), 1,8-diiodooctane, 1,8-dithiooctane, formamidinium halides, acetic acid, trifluoroacetic acid, methylammonium halides, or water. The lead salt precursor may be dried in a substantially water-free atmosphere, i.e., less than 30% relative humidity, to form a thin film. The lead salt thin film may then be thermally annealed under the same conditions and for the same time as described above for the lead halide precursor ink thin film. The annealing environment may have the same pressure and atmosphere as the lead salt deposition environment and conditions described above. In certain embodiments, the annealing process may be performed in a controlled humidity environment having a relative humidity % of 0% or more and 50% or less. In other embodiments, the annealing may be performed in a controlled humidity environment having a relative humidity % of 0 gH2O / m 3 Gas and 20gH2O / m 3 It may be carried out in a controlled humidity environment containing the following gases:

[0066] After the lead salt precursor is deposited, a second salt precursor (e.g., formamidinium iodide, formamidinium thiocyanate, guanidinium thiocyanate) may be deposited on the lead salt thin film. The lead salt thin film may have a temperature approximately equal to ambient temperature or may have a controlled temperature between 0°C and 500°C. In an embodiment, the second salt precursor may be deposited at ambient temperature or at an elevated temperature of about 25°C to 125°C. The second salt precursor may be deposited by any of the methods previously described for the lead halide precursor ink. The deposition of the second salt precursor may be carried out in the same environment and under the same conditions previously described for the first salt precursor.

[0067] In certain embodiments, the second salt precursor may be a solution containing one or more solvents (eg, one or more of the solvents described above for the first lead salt precursor).

[0068] After deposition of the lead salt precursor and the second salt precursor, the substrate may be annealed. Annealing the substrate may convert the lead salt precursor and the second salt precursor to a perovskite material (e.g., FAPbI3, GAPb(SCN)3, FASnI3). The annealing may be performed in the same environment as the lead salt deposition environment and under the same conditions as those described above. In certain embodiments, the annealing process may be performed in a controlled humidity environment having a relative humidity % of 0% or more and 50% or less. In other embodiments, the annealing may be performed in a controlled humidity environment having a relative humidity % of 0 gH2O / m 3 Gas: 20gH2O / m 3 It may be performed in a gas or less controlled humidity environment. In an embodiment, the annealing may be performed at a temperature between 50° C. and 300° C.

[0069] For example, in certain embodiments, FAPbI3 perovskite materials may be formed by the following process. First, a lead (II) halide precursor having a molar ratio of PbI2 to PbCl2 of about 90:10 dissolved in anhydrous DMF may be deposited on a substrate by spin coating or slot die printing. The lead halide precursor ink may be dried in a substantially water-free atmosphere, i.e., less than 30% relative humidity, for about 1 hour (±15 minutes) to form a thin film. The thin film may then be thermally annealed at a temperature of about 50°C (±10°C) for about 10 minutes. Next, a formamidinium iodide precursor comprising a 25 to 60 mg / mL concentration of formamidinium iodide dissolved in anhydrous isopropyl alcohol may be deposited on the lead halide thin film by spin coating or slot die printing. After the lead halide precursor and formamidinium iodide precursor are deposited, the substrate may be dried in a substantially water-free atmosphere, i.e., less than 30% relative humidity (about 4 to 7 gH2O / m 3 air) and annealed at between about 125 and 200° C. to form a formamidinium lead iodide (FAPbI3) perovskite material.

[0070] In another embodiment, the perovskite material may include C'CPbX3, where C' is one or more Group 1 metals (e.g., Li, Na, K, Rb, Cs). In certain embodiments, M' may be cesium (Cs). In yet another embodiment, the perovskite material may include C' v C w Pb y X z where C′ is one or more Group 1 metals and v, w, y, and z represent real numbers between 1 and 20. In certain embodiments, the perovskite material may be deposited as an active layer in a PV device onto a substrate layer by, for example, drop casting, spin casting, gravure coating, blade coating, reverse gravure coating, slot-die printing, screen printing, or inkjet printing.

[0071] First, a lead halide solution is formed. The lead halide solution may be prepared in any of the same manners and of similar composition as the lead halide precursor inks described above. Other lead salt precursors (such as those described above with respect to the lead halide precursor inks) may be used in conjunction with or in place of the lead halide salt to form the lead salt solution.

[0072] A Group 1 metal halide solution is then formed. A quantity of Group 1 metal halide may be mass collected in a clean, dry container under controlled atmosphere environment. Suitable Group 1 metal halides include, but are not limited to, cesium iodide, cesium bromide, cesium chloride, cesium fluoride, rubidium iodide, rubidium bromide, rubidium chloride, rubidium fluoride, lithium iodide, lithium bromide, lithium chloride, lithium fluoride, sodium iodide, sodium bromide, sodium chloride, sodium fluoride, potassium iodide, potassium bromide, potassium chloride, potassium fluoride. The Group 1 metal halide may comprise a single Group 1 metal halide or may have a mixture of Group 1 metal halides in precise ratios.

[0073] Alternatively, other Group 1 metal salt precursors may be used along with or in place of the Group 1 metal halide salt to form a Group 1 metal salt solution. Suitable precursor Group 1 metal salts may include any combination of Group 1 metals and the following anions: nitrate, nitrite, carboxylate, acetate, formate, oxalate, sulfate, sulfite, thiosulfate, phosphate, tetrafluoroborate, hexafluorophosphate, tetra(perfluorophenyl)borate, hydride, oxide, peroxide, hydroxide, nitride, arsenate, arsenite, perchlorate, carbonate, bicarbonate, chromate, dichromate, iodate, bromate, chlorate, chlorite, hypochlorite, hypobromite, cyanide, cyanate, isocyanate, fulminate, thiocyanate, isothiocyanate, azide, tetracarbonylcobaltate, carbamoyldicyanomethanide, dicyanonitrose, dicyanamide, tricyanomethanate, amide, and permanganate.

[0074] A solvent may then be added to the vessel to dissolve the Group 1 metal halide solids and form a Group 1 metal halide solution. Suitable solvents include, but are not limited to, dry N-cyclohexyl-2-pyrrolidone, alkyl-2-pyrrolidone, dimethylformamide (DMF), dialkylformamide, dimethylsulfoxide (DMSO), acetonitrile, methanol, ethanol, propanol, butanol, tetrahydrofuran, formamide, tert-butylpyridine, pyridine, alkylpyridine, pyrrolidine, chlorobenzene, dichlorobenzene, dichloromethane, chloroform, and combinations thereof. In an embodiment, the lead solids are dissolved in dry dimethylsulfoxide (DMSO). The Group 1 metal halide solids may be dissolved at a temperature between about 20° C. and about 150° C. In one embodiment, the Group 1 metal halide solids are dissolved at room temperature (i.e., about 25° C.). The Group 1 metal halide solids may be dissolved for as long as necessary to form a solution, which may be carried out for up to about 72 hours. The resulting solution forms a Group 1 metal halide solution. In some embodiments, the Group 1 metal halide solution may have a Group 1 metal halide concentration of between about 0.001 M and about 10 M, or about 1 M. In some embodiments, the Group 1 metal halide solution may further comprise an amino acid (e.g., 5-aminovaleric acid, histidine, glycine, lysine), an amino acid hydrohalide (e.g., 5-aminovaleric acid hydrochloride), an IFL surface modification (SAM) agent (discussed earlier in the specification), or a combination thereof.

[0075] The lead halide solution and the Group 1 metal halide solution are then mixed to form a thin film precursor ink. The lead halide solution and the Group 1 metal halide solution may be mixed in a ratio such that the resulting thin film precursor ink has a molar concentration of the Group 1 metal halide that is between 0% and 25% of the molar concentration of the lead halide. In certain embodiments, the thin film precursor ink may have a molar concentration of the Group 1 metal halide that is 1%, 5%, 10%, 15%, 20%, or 25% of the molar concentration of the lead halide. In some embodiments, the lead halide solution and the Group 1 metal halide solution may be agitated during or after mixing.

[0076] The thin film precursor ink may then be deposited on a desired substrate via any deposition means previously described. Suitable substrate layers may have any of the substrate layers previously identified in this disclosure. In certain embodiments, the thin film precursor ink may be spin coated onto the substrate at a speed of about 500 rpm to about 10,000 rpm for a time of about 5 seconds to about 600 seconds. In one embodiment, the thin film precursor ink may be spin coated onto the substrate at about 3000 rpm for about 30 seconds. The thin film precursor ink may be deposited onto the substrate in an ambient atmosphere in a humidity range of about 0% relative humidity to about 50% relative humidity. The thin film precursor ink may then be spin coated onto the substrate in a substantially water-free atmosphere, i.e., a relative humidity of less than 30% or 7 gH2O / m 3 The solution may be dried at less than 200° C. to form a thin film.

[0077] The thin film may then be thermally annealed at a temperature of about 20° C. to about 300° C. for a time period up to about 24 hours. In one embodiment, the thin film may be thermally annealed at a temperature of about 50° C. for about 10 minutes. The perovskite material active layer is then completed by a conversion process in which the precursor film is immersed or rinsed in a solvent or mixture of solvents (e.g., DMF, isopropyl alcohol, methanol, ethanol, butanol, chloroform, chlorobenzene, dimethyl sulfoxide, water) and a salt solution containing a salt (e.g., methylammonium iodide, formamidinium iodide, guanidinium iodide, 1,2,2-triaminovinylammonium iodide, 5-aminovaleric acid hydroiodide) at a concentration of 0.001 M to 10 M. Also, in certain embodiments, the perovskite material thin film may be thermally post-annealed in the same manner as in the first line of this paragraph.

[0078] In an embodiment, the salt solution may be prepared by collecting the salt in a clean, dry container in a controlled atmosphere environment. Suitable salts include, but are not limited to, methylammonium iodide, formamidinium iodide, guanidinium iodide, imidazolium iodide, ethenetetramine iodide, 1,2,2-triaminovinylammonium iodide, and 5-aminovaleric acid hydroiodide. Other suitable salts may include any organic cation previously described in the chapter entitled "Perovskite Materials". The salt may have a single species or may have a mixture of salts in the correct ratio. A solvent may then be added to the container to dissolve the salt solids and form a salt solution. Suitable solvents include those described in the previous paragraph and combinations thereof. In one embodiment, the formamidinium iodide salt solids are dissolved in isopropanol. The salt solids may be dissolved at a temperature between about 20° C. and about 150° C. In one embodiment, the salt solids are dissolved at room temperature (i.e., about 25° C.). The salt solids are dissolved for as long as necessary to form a solution, which may be for up to about 72 hours. The resulting solution forms a salt solution. In some embodiments, the salt solution may have a salt concentration of about 0.001 M to about 10 M. In some embodiments, the salt solution has a salt concentration of about 1 M.

[0079] For example, the process described above using lead(II) iodide solution, cesium iodide solution, and methylammonium iodide (MA) salt solution can be used to obtain cations of the general formula Cs i MA 1-i A perovskite material having PbI3, where i is equal to a number between 0 and 1, may be obtained. As another example, a lead(II) iodide solution, a rubidium iodide solution, and a formamidinium iodide (FA) salt solution may be used to obtain Rb i FA 1-i A perovskite material may be obtained having a chemical formula of PbI3, where i is equal to a number between 0 and 1. As another example, a lead(II) iodide solution, a cesium iodide solution, and a formamidinium iodide (FA) salt solution may be used to produce Cs i FA 1-iA perovskite material having the general formula of PbI3, where i is equal to a number between 0 and 1, may be obtained. As another example, a lead(II) iodide solution, a potassium iodide solution, and a formamidinium iodide (FA) salt solution may be used to obtain a perovskite material having the general formula of K i FA 1-i A perovskite material having PbI3, where i is equal to a number from 0 to 1, may be obtained. As another example, a lead(II) iodide solution, a sodium iodide solution, and a formamidinium iodide (FA) salt solution may be used to obtain a perovskite material having PbI3. i FA 1-i A perovskite material may be obtained having a general formula of PbI3, where i is equal to a number between 0 and 1. As another example, by using a lead(II) iodide-lead chloride mixture solution, a cesium iodide solution, and a formamidinium iodide (FA) solution, Cs i FA 1-i A perovskite material having the general formula PbI3 is obtained, where i is equal to a number between 0 and 1 and y represents a number between 0 and 3.

[0080] In certain embodiments, the lead halide solution may have a molar ratio of PbI2 to PbCl2 of 90:10. A cesium iodide (CsI) solution may be added to the lead halide solution to form a thin film precursor ink having 10 mol% CsI, as described above. This thin film precursor solution may be used to produce FAPbI3 perovskite material, as described above. Cesium ions may be added via the CsI solution, as described above, to incorporate chloride anions and cesium atoms into the FAPbI3 crystal lattice. This may result in a greater degree of lattice contraction compared to not adding chloride ions and adding cesium or rubidium ions, as described above. Table 1 below shows the lattice parameters of FAPbI3 perovskite materials containing 10 mol% rubidium and 10 mol% cesium with 20 mol% chloride (e.g., 10 mol% PbCl2), 10 mol% cesium, and 20 mol% chloride, where the mol% concentration represents the concentration of the additive relative to the lead atoms in the lead halide solution. As can be seen from Table 1, the FAPbI3 perovskite material with the addition of cesium and chloride has a smaller lattice constant than the other two perovskite material samples.

[0081] [Table 1] The data also show that FAPbI3 perovskite materials doped with rubidium, cesium and / or chloride have a Pm3-m cubic structure. FAPbI3 perovskites containing up to 10 mol% Rb and 10 mol% Cl, or 10 mol% Cs, or 10 mol% Cs and 10 mol% Cl have been observed to maintain the cubic Pm3-m cubic crystal structure. Figure 5 shows the X-ray diffraction patterns corresponding to each sample shown in Table 1. Tables 2-4 provide the X-ray diffraction peaks and intensities for the three perovskite materials shown in Table 1. Data was collected at ambient conditions on a Rigaku Miniflex 600 using a CuKα radiation source at a scan rate of 1.5 degrees 2θ / min.

[0082] [Table 2]

[0083] [Table 3]

[0084] [Table 4] Table 5 shows the geometrically expected X-ray diffraction patterns of a cubic Pm3-m material with a lattice constant of 6.3375 Å under Cu-Kα irradiation. As can be seen from the data, perovskite materials made with 10 mol% Rb and 10 mol% Cl, 10 mol% Cs, and 10% Cs and 10% Cl each have diffraction patterns that match the pattern expected for a cubic Pm3-m perovskite material.

[0085] [Table 5] (lead isolation material layer) As used herein, a "lead-sequestering material" refers to a material having at least one lead-sequestering compound that includes one or more lead-binding groups as a substituent (e.g., moiety or functional group) of the lead-sequestering compound. Examples of lead-binding groups suitable for certain embodiments of the present disclosure include, but are not limited to, oxides, hydroxides, amines, amides, ammonium, carboxylates, carboxylic acids, aldehydes, esters, ethers, phosphines, phosphinates, phosphonates, phosphates, sulfides, sulfates, and any combination thereof. FIG. 3 illustrates an example of a lead-sequestering mechanism. In the example illustrated in FIG. 3, a lead-sequestering compound that includes an acetylacetonate lead-binding group 3000 is attached to a particle 3100. As shown in FIG. 3, Pb 2+Lead ions can be sequestered due to strong ionic or coordinative-covalent interactions between the acetylacetonate groups 3000 and the acetylacetonate groups 3000. It is also believed that other Pb orbitals / p orbitals overlap, such as Pb orbitals overlapping with CC and C-O π bonds, can sufficiently bind and sequester Pb. Although only a few of the many potential advantages to the disclosed methods, compositions, and devices are mentioned herein, the disclosed lead sequestration materials can sequester free lead ions and reduce leakage of lead ions or other metal ions in perovskite devices.

[0086] In some embodiments, the perovskite material device may include a lead isolation material, either as a separate lead isolation layer or as part of one or more other device layers. Figure 4 is a schematic diagram of a perovskite material device 4000 according to some embodiments of the present disclosure. By way of example, Figure 4 shows an embodiment of a perovskite material device 4000 having a lead isolation material (LSM) layer 4010. The perovskite material device 4000 has a similar structure to the perovskite material device 1000 shown in Figure 1.

[0087] In one embodiment, the lead isolation material layer is deposited or placed on the front side of the perovskite material device. For example, in FIG. 4, the lead isolation material layer 4010 is deposited or placed on the surface of the first substrate 1010. In this example, the lead isolation material layer 4010 may be transparent. In one embodiment, the lead isolation material may be in the form of a solid composite or a solution ink that can be processed into a thin film or coating by thermal extrusion, blade coating, slot die coating, spin coating, nozzle spraying, and / or dip casting. In another embodiment, the lead isolation material layer is insoluble in water. In an embodiment, the lead isolation material layer 4010 may be a coating, a deposit, a film, a thin film, etc.

[0088] In one embodiment, the photoactive material layer may include a lead isolation material. FIG. 5 is a schematic diagram of a perovskite material device 5000 according to an embodiment. By way of example, FIG. 5 illustrates an embodiment of a perovskite material device 5000 having a PAM layer including a lead isolation material (LSM) 5040. The perovskite material device 5000 has a similar structure to the perovskite material device 1000 illustrated in FIG. 1. In one embodiment, the lead isolation material is mixed with the perovskite precursor (e.g., added to the precursor ink) prior to forming the perovskite material layer. In certain embodiments, the volume ratio of perovskite to lead isolation material in the perovskite material layer is between about 0.01 and about 50. One of ordinary skill in the art, given the benefit of this disclosure, will know how to determine a suitable volume ratio for a given perovskite material device. In another embodiment, the layer including the lead isolation material 5040 may be a composite of a PAM and one or more lead isolation materials.

[0089] In one embodiment, the lead isolation material layer is deposited or placed on the back surface of the perovskite material device adjacent to or as a component of the non-conductive layer. Figures 6-8 are schematic diagrams of perovskite material devices according to some embodiments. In the examples shown in Figures 6-8, the lead isolation material (LSM) is deposited or placed on the back surface of the perovskite material device adjacent to or as a component of the non-conductive layer. As an example, Figure 6 shows an embodiment of a perovskite material device 6000 having a non-conductive layer 6010 and a lead isolation material (LSM) layer 6020. In some embodiments, the non-conductive layer 6010 may be similar to the non-conductive layer 2380 described in paragraph

[0087] above. In the example shown in Figure 6, the lead isolation material (LSM) layer 6020 is deposited or placed between the second electrode layer 1060 and the non-conductive layer 6010. 7, a lead isolation material (LSM) layer 6020 is deposited or placed between the second substrate layer 1070 and the non-conductive layer 6010. In the example shown in FIG. 8, the lead isolation material may be mixed with the non-conductive layer to form a composite layer 8010.

[0090] FIG. 9 illustrates an exemplary perovskite device 9000 according to various embodiments. The device 9000 illustrates an embodiment including a first glass substrate 9010 and a second glass substrate 9080. In the example illustrated in FIG. 9, a first electrode (FTO) 9020 is disposed on the inner surface of the first substrate 9010, and a second electrode 9070 is disposed on the inner surface of the second substrate 9080. The second electrode 9070 may be a chromium-aluminum bilayer (Cr / Al), where a layer of chromium is coated with a layer of aluminum to form a bilayer. An active layer 9100 is sandwiched between the two electrodes 9020 and 9070. The active layer 9100 includes a photoactive material (e.g., MAPbI3, FAPbI3) 9040 and a charge transport layer (e.g., C 60 ) 9050. A laminate layer including a lead isolation material 9060 is adjacent to and in contact with the inner surface of the second electrode 9070.

[0091] In an embodiment, a lead isolation material layer may be present in a four terminal tandem PV device. Figure 33 is a schematic diagram of a four terminal tandem perovskite material device according to an embodiment. In the example shown in Figure 33, the LSM 6020 is deposited or placed on the back side of the front subcell 2400 (as shown), adjacent to or as a component of the non-conductive layer 2380. In certain embodiments, the LSM may be part of the rear subcell 2500, or there may be multiple LSMs across the two subcells.

[0092] In some embodiments, the lead isolation material layer may be an anti-reflective coating. In certain embodiments, the lead isolation material layer may have a refractive index (n) of about 1 to about 1.5. In some embodiments, the lead isolation material layer may have a refractive index (n) of about 1.2 to about 1.3. In one embodiment, for example, the lead isolation material layer may have a refractive index (n) of 1.25. In certain embodiments, the perovskite material device may have one or more additional anti-reflective coatings in addition to the lead isolation material.

[0093] In some embodiments, the lead isolation material layer may be an anti-fouling layer. In certain embodiments, surface contaminants such as oil, dirt, water, and animal waste tend not to adhere preferentially to the lead isolation material compared to substrate surfaces such as glass and polymers. In certain embodiments, the lead isolation material may be hydrophobic and / or oleophobic. In some embodiments, the perovskite material device may include one or more additional anti-fouling coatings in addition to the lead isolation material.

[0094] In certain embodiments, the lead isolation material layer may have a thickness of from about 1 nm to about 1 mm, from 10 nm to about 500 μm, or from 0.1 μm to about 200 μm.

[0095] (Lead isolation material) Lead sequestration materials suitable for certain embodiments of the present disclosure may have at least one lead sequestration compound that includes one or more lead-binding groups as a substituent (e.g., moiety or functional group) of the lead sequestration compound. In certain embodiments, the lead sequestration compound is Pb 2+ The lead-binding group may have a strong affinity for ions. Examples of lead-binding groups suitable for certain embodiments of the present disclosure include, but are not limited to, oxides, hydroxides, amines, amides, ammonium, carboxylates, carboxylic acids, aldehydes, esters, ethers, phosphines, phosphinates, phosphonates, carboxylates, phosphates, sulfides, sulfates, and any combinations thereof. Examples of lead-sequestering compounds suitable for certain embodiments of the present disclosure include, but are not limited to, EDTA, organophosphates, organosulfates, thiols, thioureas, carbamates, carbonates, aminos, formamidinos, and any derivatives or combinations thereof. In certain embodiments, the lead-sequestering compound may be a monomer or an organic small molecule. In certain embodiments, the lead-sequestering compound may be free of polymers or free of organic polymers.

[0096] In certain embodiments, the lead isolation material and / or lead isolation compound may be water insoluble. In some embodiments, the lead isolation material may have the lead isolation compound attached (e.g., bound) to a water insoluble binding material. In one embodiment, the lead isolation material may be in the form of a solid composite or solution ink that can be processed into a thin film or coating by thermal extrusion, blade coating, slot die coating, spin coating, nozzle spraying, and / or dip casting.

[0097] In some embodiments, the lead sequestration compound includes a carboxylate as a lead-binding group. Examples of lead sequestration compounds including a carboxylate lead-binding group include, but are not limited to, ethylenediaminetetraacetic acid (EDTA), EDTA derivatives, and any combination thereof. FIG. 10A shows the chemical structure of EDTA, and FIG. 10B shows the chemical formulas of some exemplary EDTA derivatives that may be used as lead sequestration compounds in certain embodiments. With reference to the EDTA derivative structure in FIG. 10B, in some embodiments, n may be an integer from 1 to 12, and R1, R2, R3, and R4 may each independently be H, Li, Na, K, or NH4. In one embodiment, two or more of R1, R2, R3, and R4 may be the same, or they may each be different. FIGS. 11A-11E show chemical structures of additional examples of EDTA derivatives suitable for certain embodiments.

[0098] In some embodiments, the lead sequestration compound includes phosphate as a lead-binding group. Examples of lead sequestration compounds that include phosphate lead-binding groups include organophosphates. Figures 12A-15B show structures and examples of organophosphates suitable for certain embodiments. Figure 12A shows a first chemical structure of an organophosphate that may be used as a lead sequestration compound, according to some embodiments. With reference to the organophosphate structure in Figure 12A, in some embodiments, n may be an integer from 1 to 12, and R1 and R2 are each independently H, Li, Na, K, NH4, -CH3, or -CH2(CH2). m1CH3, where m1 is an integer from 0 to 10, and R3 and R4 are each independently H, -(CH2) m2 -PO(OR1)(OR2), or -(CH2) m3 -COOR1, where m2 can be an integer from 1 to 6 and m3 can be an integer from 1 to 6. In some embodiments, R1 and R2 can be the same or different. In certain embodiments, R3 and R4 can be the same or different. Figures 12B-12F show various exemplary molecules having the organophosphate structure of Figure 12A.

[0099] FIG. 13A shows a second chemical structure of an organophosphate that may be used as a lead sequestration compound, according to an embodiment. In an embodiment, the organophosphate may be a phosphinate or a phosphonate. With reference to the organophosphate structure in FIG. 13A, R1 may be H, -CH3, -CH2(CH2), m1 CH3, or -CH2 (CH2) m2 m1 may be an integer from 0 to 10, m2 may be an integer from 0 to 10, and R2 may be H, -CH3, or -CH2(CH2). m3 m3 may be an integer from 0 to 10, and R3, R4, R5, and R6 may each independently be H, Li, Na, K, NH4, -CH3, or -CH2(CH2). m4 R3, R4, R5, and R6 may be the same or different. Figures 13B and 13C show various exemplary molecules having the organophosphate structure of Figure 13A.

[0100] 14A shows a third structure of an organophosphate that may be used as a lead sequestration compound according to an embodiment. With reference to FIG. 14A, n1 may be an integer from 0 to 6, n2 may be an integer from 0 to 6, n3 may be an integer from 0 to 6, n4 may be an integer from 0 to 6, and R1 may be H, Li, Na, K, NH4, -CH3, or -CH2(CH2). m1 where m1 may be an integer from 0 to 10, and R2 may be H, Li, Na, K, or -CH2(CH2) m2 R1, R2, R3, R4, or R5 may be the same or different. FIG. 14B shows an exemplary molecule having the organophosphate structure of FIG. 14A.

[0101] Figure 15A shows a fourth structure of an organophosphate that may be used as a lead sequestration compound, according to an embodiment. With reference to Figure 15A, n1, n2, n3, n4, n5, n6, and n7 may each independently be an integer from 0 to 6. R1, R2, R3, R4, R5, R6, R7, R8, R9, R 10 are each independently H, Li, Na, K, NH4, -CH3, or -CH2(CH2) m CH 3で and m may be an integer from 0 to 10. In some embodiments, R1, R2, R3, R4, R5, R6, R7, R8, R9, or R 10 Two or more of may be the same or different. Figure 15B shows an exemplary molecule having a fourth structure of an organophosphate.

[0102] In some embodiments, the lead sequestration compound includes sulfate as a lead binding group. Examples of lead sequestration compounds that include sulfate lead binding groups include organosulfates. Figures 16A-18B show structures and examples of organophosphates suitable for certain embodiments. Figure 16A shows a first structure of an organosulfate that may be used as a lead sequestration compound according to some embodiments. With reference to Figure 16A, n is an integer between 0 and 10, and R1 and R2 are H, Li, Na, K, or NH4. In certain embodiments, R1 and R2 may be the same or different. Figures 16B and 16C show examples of molecules having the organosulfate structure of Figure 16A.

[0103] Figure 17A shows a second structure of an organosulfate that may be used as a lead sequestration compound according to an embodiment. With reference to Figure 17A, n is an integer from 0 to 19, and R1 may be H, Li, Na, K, or NH4. Figure 17B shows an example of a molecule having the organosulfate structure of Figure 17A.

[0104] Figure 18A shows a third structure of an organosulfate that may be used as a lead sequestration compound according to an embodiment. With reference to Figure 18A, n is an integer from 0 to 19, and R1 is H, Li, Na, K, or NH4. Figure 18B shows an example of a molecule having the organosulfate structure of Figure 18A.

[0105] In some embodiments, the lead sequestration material further comprises a binding material. In some examples, one or more lead sequestration compounds (e.g., as shown in Figures 12A-18B) may be attached to the binding material to form a solid composite or solution ink. In some embodiments, the binding material may be an inorganic material. In some embodiments, the solid composite or solution ink with the lead sequestration compounds may be processed into a thin film by thermal extrusion, blade coating, slot die coating, spin coating, nozzle spraying, dip casting. In other examples, inorganic additives may be added to the solid composite or solution ink containing lead binding groups to improve film properties and / or enhance sequestration efficiency. Examples of inorganic additives suitable for certain embodiments of the present disclosure include, but are not limited to, phosphates and hydrophosphates, sulfates, carbonates, chromates and dichromates, sulfide salts, silicates, aluminosilicates, and any combination thereof, of Li, Na, K, NH4.

[0106] In an embodiment, the binding material to which the lead sequestration compound is attached is an inorganic material. In one embodiment, the inorganic material is functionalized with the lead sequestration compound to form a functionalized inorganic material. Examples of inorganic materials suitable for certain embodiments of the present disclosure include, but are not limited to, nanoparticles, microparticles, flat surfaces, structured surfaces, mesoporous materials, covalent organic frameworks, metal organic frameworks, aerogels, and any combination thereof. FIG. 19A shows an example of a lead sequestration compound attached to an inorganic particle. In the example shown in FIG. 19A, n can be an integer from 0 to 12, and z can be an integer from 1 to 10. 6 R may be an integer of -H, -NH, -N(CHCOOR), -NH(PO(OR), -N(CHPO(OR), -NHCHCHSH, -NH-C(=S)-NH, where R, R, and R are each independently H, Li, Na, K, NH, -CH, or -CH(CH). m19A and other similar figures of the present disclosure, z may represent the number of lead-sequestering compounds attached to the inorganic particle. In another embodiment, z may represent the molar concentration of the lead-sequestering compound attached to the inorganic particle. In such embodiments, z in FIG. 19A may be from about 0.01 to about 100 mmol / g, from about 0.1 to about 10 mmol / g, or from about 0.5 to about 2.0 mmol / g.

[0107] Examples of inorganic microparticles or nanoparticles suitable for certain embodiments include, but are not limited to, silica, silicate, zinc oxide, titania, vanadia, tantala, zirconia, hafnia, silicon nitride, boron nitride, and any combination thereof. In some embodiments, the size of the microparticles is about 1 to about 1,000 microns. In other embodiments, the size of the nanoparticles is about 1 to about 1,000 nm. In some embodiments, the shape of the microparticles or nanoparticles is spherical, ellipsoidal, rod-shaped, cubic, hexagonal, triangular, star-shaped, prismatic, plate-shaped, flower-shaped, or bar-shaped. In one embodiment, the microparticles and nanoparticles are non-porous, microporous (pore size up to 2 nm), mesoporous (pore size 2 to 50 nm), or macroporous (pore size 50 nm to 75 microns). Figure 19B shows an example of Figure 19A with lead sequestration compounds bound to SiO2 particles. In one embodiment, the SiO2 particles are microparticles. In another embodiment, the SiO2 particles are nanoparticles.

[0108] Another example of a lead sequestration compound attached to an inorganic particle is shown in Figure 20. In the example shown in Figure 20, n can be an integer from 0 to 4, m can be an integer from 0 to 6, and z can be an integer from 1 to 10. 6R may be H, -SH, -NH, -N(CHCOOR), -NH(PO(OR), -N(CHPO(OR), -NHCHCHSH, or -NH-C(=S)-NH, where R, R, and R are each independently H, Li, Na, K, NH, -CH, -CH(CH). m 20 may be CH3, where m may be an integer from 0 to 10. In another embodiment, z in Figure 20 may represent a molar concentration of about 0.01 to about 100 mmol / g, about 0.1 to about 10 mmol / g, or about 0.5 to about 2.0 mmol / g. The shape and size of the particles in Figure 20 are similar to those previously described.

[0109] FIG. 21A shows another example of a lead sequestration compound attached to an inorganic particle. With reference to FIG. 21A, n can be an integer from 0 to 4, m can be an integer from 0 to 6, and z can be an integer from 1 to 10. 6 R1 may be H, -SH, -NH2, -N(CH2COOR3)2, -NH(PO(OR4)2), -N(CH2PO(OR5)2), -NHCH2CH2SH, -NH-C(=S)-NH2. R 3-5 is H, Li, Na, K, NH4, -CH3, -CH2(CH2) m2 R2 may be the same as R1, or may be H, -SH, -NH2, -N(CH2COOR3)2, -NH(PO(OR4)2), -N(CH2PO(OR5)2), -NHCH2CH2SH, or -NH-C(=S)-NH2. R3, R4, and R5 are each independently H, Li, Na, K, NH4, -CH3, -CH2(CH2) m2 m may be CH3, where m2 may be an integer from 0 to 10. In another embodiment, z in Figure 21A may represent a molar concentration of about 0.01 to about 100 mmol / g, about 0.1 to about 10 mmol / g, or about 0.5 to about 2.0 mmol / g. The shape and size of the particles in Figure 21A are similar to those in Figure 19A.

[0110] 21B-21E show various examples of FIG. 21A with lead sequestration compounds attached to SiO2 particles, where z is between 1 and 10. 6 or z may represent a molar concentration of about 0.01 to about 100 mmol / g, about 0.1 to about 10 mmol / g, or about 0.5 to about 2.0 mmol / g. In one embodiment, the SiO2 particles are microparticles. In another embodiment, the SiO2 particles are nanoparticles.

[0111] 22A-22C show various examples of lead sequestration compounds that can be attached to silica gel to form functionalized silica gel. In the examples shown in FIG. 22A-22C, z ranges from 1 to 10. 6 In other embodiments, z in Figures 22A-22C may represent a molar concentration of about 0.01 to about 100 mmol / g, about 0.1 to about 10 mmol / g, or about 0.5 to about 2.0 mmol / g. The size and shape of the SiO2 particles are similar to the particles shown in Figure 19A. Figure 22D shows an example of a lead sequestration compound attached to a mesoporous silica gel.

[0112] In some embodiments, the lead sequestration compound may be attached (e.g., bonded) to a polymeric material. In some embodiments, the polymeric material is a polymer, a resin, an elastomer, or a thermoset. In some embodiments, the polymeric material may include polyvinyl acetate, polyolefin, polystyrene, polyglycol, polyorganic acid, natural rubber, synthetic rubber, polyester, nylon, polyamide, polyaryl, polynucleic acid, polysaccharide, polyurethane, acrylonitrile butadiene styrene, acrylic, acrylic polymer, acrylic resin, crosslinked porous resin, and any combination or derivative thereof. Examples of polymers suitable for certain embodiments include, but are not limited to, poly(ethylene-vinyl acetate) (EVA), high density polyethylene (HDPE), low density polyethylene (LDPE), polypropylene (PP), polystyrene (PS), polyethylene glycol (PEG / PEO), poly(methyl methacrylate) (PMMA), polyoxymethylene (POM), poly(acrylonitrile butadiene styrene) (ABS), polyphenylene sulfide (PPS), polytetrafluoroethylene (PTFE). , polyvinylidene difluoride (PVDF), polyvinyl chloride (PVC), poly(ethylene terephthalate) (PET), polylactic acid (PLA), polycarbonate (PC), polyether ether ketone (PEEK), polybutylene terephthalate (PBT), butylene rubber, polyisoprene, polyurethane (PU), polydimethylsiloxane (PDMS), urea formaldehyde resin, epoxy resin, phenol formaldehyde resin (PF), derivatives thereof, and any combination thereof. The configuration of the polymer backbone of the bound polymer may be isotactic, syndiotactic, or atactic. In certain embodiments, the functionalized inorganic material containing one or more lead-sequestering compounds may be incorporated into polymeric materials such as polymers, resins, elastomers, and thermosets to form composites. In certain embodiments, the lead-sequestering compounds may be covalently attached as a substituent or pendant group of the polymeric material.

[0113] 23A and 23B show examples of polyvinyl backbone (main chain) polymers suitable as the polymeric material in certain embodiments. In the example shown in FIG. 23A, n can be an integer from 1 to 20 or 1 to 6, and R can be H, -SH, -NH, -N(CHCOOR), -NH(PO(OR), -N(CHPO(OR), -NHCHCHSH, or -NH-C(=S)-NH, where R, R, and R are H, Li, Na, K, NH, -CH, or -CH(CH). m 23B, x and y may be, independently, integers from 1 to 20 or 1 to 6. R1 may be, independently, H, -SH, -NH2, -N(CH2COOR3)2, -NH(PO(OR4)2), -N(CH2PO(OR5)2), -NHCH2CH2SH, or -NH-C(=S)-NH2, where R3, R4, and R5 are, independently, H, Li, Na, K, NH4, -CH3, or -CH2(CH2) m R2 may be R1, H, -SH, -NH2, -N(CH2COOR3)2, -NH(PO(OR4)2), -N(CH2PO(OR5)2), -NHCH2CH2SH, or -NH-C(=S)-NH2, where R3, R4, and R5 are each independently H, Li, Na, K, NH4, -CH3, or -CH2(CH2). m It may be CH3, where m is an integer from 0 to 10.

[0114] Figures 24A-24E show various examples of lead sequestration compounds attached to polyvinyl backbone polymers. In the examples shown in Figures 24A-24C, n can be an integer from 1 to 20 or 1 to 6. In the examples shown in Figures 24D and 24E, x and y can independently be integers from 1 to 20 or 1 to 6, and z can be an integer from 1 to 10. 6In other embodiments, z in Figure 24E may represent a molar concentration of about 0.01 to about 100 mmol / g, about 0.1 to about 10 mmol / g, or about 0.5 to about 2.0 mmol / g.

[0115] FIG. 25A shows a first structure of a polystyrene derivative backbone polymer to which a lead sequestration compound can be attached. With reference to FIG. 25A, n can be an integer from 1 to 20 or 1 to 6, R1 can be -SO3R4 or -CH2-N(CH2COOR5)2, R2 can be -CH3 or -OCH3, R3 can be H or -CH3, R4 can be H, Li, Na, K, or NH4, and R5 can be H, Li, Na, K, or NH4. Furthermore, R1, R2 can be in ortho, meta, or para positions relative to the polymer chain. FIG. 25B and FIG. 25C show two examples of lead sequestration compounds attached to a polystyrene derivative backbone polymer. In these compounds, n can be an integer from 1 to 20 or 1 to 6.

[0116] FIG. 26 shows a second structure of a polystyrene derivative-backbone polymer to which lead binding groups can be attached. In the example shown in FIG. 26, x and y can be independently integers from 1 to 20 or 1 to 6. R1 can be -SO3R7 or -CH2-N(CH2COOR8)2, where R7 can be H, Li, Na, K or NH4. R8 can be H, Li, Na, K or NH4. R2 can be -CH3 or -OCH3. R3 can be -H or -CH3. R4 can be -SO3R9 or -CH2-N(CH2COOR 10 R9 may be H, Li, Na, K or NH4, and R 10 may be H, Li, Na, K or NH4. R5 may be -CH3 or -OCH3 and R6 may be H or -CH3. Additionally, R1, R2, R3, R4 may be in the ortho, meta or para positions relative to the polymer chain.

[0117] In an embodiment, the lead sequestration compound may be attached to a cross-linked polymer resin. FIG. 27 is a schematic diagram of a cross-linked porous resin (CPR) structure to which the lead sequestration compound may be attached. In the example shown in FIG. 27, R may be -SH, -NH2, -N(CH2COOR1)2, -NH(PO(OR2)2), -N(CH2PO(OR3)2), -NHCH2CH2SR4, -SO3R5, or -NH-C(=S)-NH2. Here, R1, R2, R3, R4, and R5 may each independently be H, Li, Na, K, or NH4. In one embodiment, the resin may be based on a polystyrene backbone cross-linked with divinylbenzene. In one example, the resin size is between 1 and 1,000 microns. In another example, the shape of the resin is spherical, elliptical, rod-shaped, cubic, hexagonal, triangular, star-shaped, prismatic, plate-shaped, bar-shaped, flower-shaped, and any combination thereof. The CPR may have a macroporous structure comprising a microporous cross-linked polymer, as shown in Figure 27. Figure 28 shows various examples of lead binding molecules attached to the CPR shown in Figure 27.

[0118] Numerous modifications, variations, and variations can be made to the described embodiments without departing from the scope of the invention as defined in the claims. The invention is not limited to the described embodiments, but is intended to have the full scope defined by the language of the claims and their equivalents.

Claims

1. 1. A perovskite material device comprising: A perovskite material device having a lead sequestration compound having one or more lead binding groups selected from the group consisting of carboxylate, phosphate, sulfide, sulfate, and any combination thereof.

2. 2. The perovskite material device of claim 1, wherein the lead sequestration compound is ethylenediaminetetraacetic acid (EDTA) or an EDTA derivative.

3. 2. The perovskite material device of claim 1 , wherein the lead sequestration compound is an organophosphate.

4. 2. The perovskite material device of claim 1 , wherein the lead sequestration compound is an organosulfate.

5. 13. The perovskite material device of claim 1 , wherein the lead sequestration compound is attached to a water insoluble binding material.

6. 6. The perovskite material device of claim 5, wherein the binding material is selected from the group consisting of nanoparticles, microparticles, flat surfaces, structured surfaces, mesoporous materials, covalent organic frameworks, metal organic frameworks, aerogels, and any combination thereof.

7. 6. The perovskite material device of claim 5, wherein the binder material and the lead sequestration compound form a solid composite material.

8. 6. The perovskite material device of claim 5, wherein the binder composition comprises silica, silicate, zinc oxide, titania, vanadia, tantala, zirconia, hafnia, silicon nitride, or boron nitride.

9. the binding material is a microparticle or nanoparticle; 6. The perovskite material device of claim 5, wherein the shape of the binder material is a sphere, an ellipsoid, a rod, a cube, a hexagon, a triangle, a star, a prism, a plate, or a bar.

10. 10. The perovskite material device of claim 9, wherein the microparticles have a size of about 1 to about 1,000 microns.

11. 10. The perovskite material device of claim 9, wherein the nanoparticles have a size of about 1 to about 1,000 nm.

12. 10. The perovskite material device of claim 1, wherein the lead sequestration compound is bound to a polymeric material selected from the group consisting of a polymer, a resin, an elastomer, a thermoset, and any combination thereof.

13. 13. The perovskite material device of claim 12, wherein the polymeric material is selected from the group consisting of polyolefins, polystyrenes, polyglycols, polyorganic acids, natural rubbers, synthetic rubbers, polyesters, nylons, polyamides, polyaryls, polynucleic acids, polysaccharides, polyurethanes, acrylonitrile butadiene styrene, acrylics, acrylic polymers, acrylic resins, crosslinked porous resins, and any combination thereof.

14. The composite material further comprises one or more inorganic additives, the inorganic additives being Li, Na, K, NH 4 8. The perovskite material device of claim 7, wherein the perovskite salt is selected from the group consisting of phosphates, hydrophosphates, sulfates, carbonates, chromates, and dichromates, sulfide salts, silicates, aluminosilicates, and any combination thereof.

15. 2. The perovskite material device of claim 1 , wherein the lead isolation material is an anti-reflective coating.

16. Providing a substrate; depositing a precursor ink on the substrate comprising a lead isolation material, the lead isolation material comprising: a lead-sequestering compound comprising one or more lead-binding groups selected from the group consisting of carboxylate, phosphate, sulfide, sulfate, and any combination thereof; A binding material; and drying the lead isolation precursor ink to form a lead isolation material layer; The method comprising:

17. 1. A composition comprising: A binding material; a lead-sequestering compound attached to the binding material, the lead-sequestering compound comprising one or more lead-binding groups selected from the group consisting of carboxylate, phosphate, sulfide, sulfate, and any combination thereof; having The composition, wherein the binding material is selected from the group consisting of nanoparticles, microparticles, flat surfaces, structured surfaces, mesoporous materials, covalent organic frameworks, metal organic frameworks, aerogels, and any combination thereof.

18. 18. The composition of claim 17, wherein the lead sequestering compound is ethylenediaminetetraacetic acid (EDTA) or an EDTA derivative.

19. 18. The composition of claim 17, wherein the lead sequestering compound is an organophosphate.

20. 18. The composition of claim 17, wherein the lead sequestering compound is an organosulfate.