【0011】 本発明によれば、金属ボールが低合金鋼で作られる場合に、より優れた耐摩耗性と耐衝撃性を可能にし、それによって、使用される鋼の炭素質量分率を低減することを可能にします。
Smart Images

Figure 2024544443000001 
Figure 2024544443000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a ball-shaped metal product.
[0002] As a method for manufacturing ball-shaped metal products (hereinafter referred to as "balls") from low-alloy spheroidal graphite cast iron, a method is known in which the cast iron is melted, a steel bar is cast, rolled in a cross rolling mill, isothermal quenched, and then tempered at 280°C to 320°C (see Patent Document 1).
[0003] This known method has the disadvantage that it cannot ensure the hardness difference between the surface and the center of the sphere, which reduces the wear resistance and impact resistance. Another disadvantage is the more complex and expensive technology of heat treatment of the balls, which includes the need to have equipment for isothermal quenching in molten salt and tempering in a conveyor quenching and tempering device to ensure the required hardness of the balls.
[0004] From the point of view of technical essence, the closest solution to the proposed invention refers to a method for producing grinding balls, which includes heating a concussed billet and rolling a round billet of the corresponding size in a hot rolling mill. Then it is heated in an induction device, rolled into a ball shape in a cross rolling mill at 950 ° C ~ 1050 ° C, cooled to 840 ° C ~ 900 ° C in a cooling drum with additional air supply, and then quenched. Then, tempering with running water is performed in a tempering drum, the ball temperature is reduced to 125 ° C ~ 160 ° C, and the ball is self-tempered in a container (see Patent Document 2).
[0005] This method has the following disadvantages: Quenching is done at rolling temperatures above the GSE line (lower on the iron-carbon alloy diagram)1 and cooling to the quenching value, which results in the formation of large austenite grains and poor properties for subsequent phase transformations.
[0006] Furthermore, to ensure a group 3 to 5 hardness for ball 2 at unit production volume, it is necessary to use high carbon, high alloy steel (carbon mass fraction of 0.6% or more) as the billet material. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] Russian Patent Publication No. RU2082530 [Patent Document 2] Russian Patent Publication No. RU2596737 Summary of the Invention [Problem to be solved by the invention]
[0008] The present invention aims to solve the problems in the conventional technology described above.
[0009] The technical results provided by the present invention are higher hardness group properties of ball-shaped metal products, improved wear and impact resistance of such products at unit output when made from low-alloy steels, and the possibility of reducing the carbon mass fraction of the steel used in the process. [Means for solving the problem]
[0010] In order to achieve such technical results, the manufacturing method of the ball-shaped metal product according to the present invention (including heating, rolling, cooling, quenching and tempering of the ball) is characterized in that a round billet made to an appropriate size is heated in a medium frequency induction device, the billet is rolled into a ball at 950°C to 1070°C in a cross rolling mill, the ball is cooled to 620°C to 700°C in a cooling drum while being forced air cooled, the surface of the ball is heated to 850°C to 930°C in a high frequency induction device including a rotating conveying tube and multiple inductor parts, the ball is quenched to 125°C to 160°C in a quenching drum cooled with running water, and the ball is self-quenched in a container. Effect of the Invention
[0011] According to the invention, better wear and impact resistance is possible when the metal balls are made of low alloy steel, thereby making it possible to reduce the carbon mass fraction of the steel used. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The essence of the invention is as follows. In the proposed method, the balls are rolled and heated to 850°C-930°C in a high-frequency induction device, then cooled to 620°C-700°C, and then subjected to a thermal cycle. This allows the austenite grain size to be reduced and finely dispersed quenched martensite to be obtained before tempering the ball surface, thus increasing the hardness of the ball surface. Further low-temperature tempering helps to redistribute the carbon in the quenched martensite and form tempered martensite. It is a process that reduces internal stresses while maintaining the same level of high hardness and wear resistance. The combination of high surface hardness and a relatively ductile core improves the ball's impact resistance, i.e. its ability to resist shock loads.
[0013] The high frequency induction unit 3, which contains a rotating conveying tube made of heat-resistant dielectric material and arranged at an inclination angle to the horizontal, is used to move the balls being processed. The tube is arranged in several sections of the inductor. This solution ensures that the moving ball is heated evenly (axisymmetrically) on its surface up to the specified depth.
[0014] Thus, the proposed ball manufacturing method allows for better wear and impact resistance when the metal balls are made of low-alloy steel, thereby making it possible to reduce the carbon mass fraction of the steel used.
Claims
[Claim 1] A method for manufacturing a ball-shaped metal product, comprising the steps of: heating a round billet made to an appropriate size in a medium frequency induction device; rolling the round billet into a ball at 950°C to 1070°C in a cross rolling mill; cooling the ball to 620°C to 700°C in a cooling drum while forcibly cooling the ball; heating the surface of the ball to 850°C to 930°C in a high frequency induction device including a rotating conveying pipe and a plurality of inductor parts; quenching the ball to 125°C to 160°C in a quenching drum cooled with running water; and self-hardening the ball in a container.
Citation Information
Patent Citations
Induction hardening method, and steel parts
JP2002256336A
Heat treatment apparatus and heat-treatment method for steel ball
JP2008169430A
JPS4717657A
Method of making cast iron grinding balls
RU2082530C1
Method for production of steel grinding balls
RU2596737C1