Ceramic Electronic Components
By incorporating carbon materials like carbon black in the conductive paste for internal electrodes, the electrical properties and high-temperature load reliability of ceramic electronic components are enhanced, addressing the challenges of miniaturization and capacity in multilayer ceramic capacitors.
Patent Information
- Application Number
- JP2022023333
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-11-29
- Filing Date
- 2022-02-17
- Publication Date
- 2024-09-18
- Estimated Expiration
- 2042-02-17
AI Technical Summary
Existing ceramic electronic components face challenges in achieving miniaturization, high capacity, and high reliability, particularly in the electrical properties and high-temperature load reliability of multilayer ceramic capacitors.
The use of a conductive paste containing a carbon material, such as carbon black, to form internal electrodes within the ceramic electronic components, ensuring the carbon material remains after sintering and at the interface between dielectric layers and internal electrodes, enhancing electrical properties and high-temperature load reliability.
This approach improves electrical characteristics and ensures excellent high-temperature load reliability by maintaining uniformity in dielectric composition and preventing the formation of coarse grains, while allowing for thinner internal electrodes and better heat dissipation.
Smart Images

Figure 0007553183000006 
Figure 0007553183000005 
Figure 0007553183000002
Abstract
Description
[Technical field]
[0001] The present disclosure relates to ceramic electronic components, such as multi-layered ceramic capacitors (MLCCs). [Background technology]
[0002] With the realization of more complex and higher performance electronic devices, there is a demand for smaller multilayer ceramic capacitors with higher capacitance. In addition, high reliability is also required for applications to electrical components. Development is being carried out in various fields to ensure the miniaturization, high capacitance, high reliability, etc., of such multilayer ceramic capacitors. For example, there is a demand for improving the characteristics of internal electrodes that form a laminated structure alternately with dielectric layers. Summary of the Invention [Problem to be solved by the invention]
[0003] One of the various objects of the present disclosure is to provide a ceramic electronic component that can have improved electrical properties.
[0004] Another of the various objects of the present disclosure is to provide a ceramic electronic component having excellent high-temperature load reliability. [Means for solving the problem]
[0005] One of the various solutions proposed by the present disclosure is to form an internal electrode from a conductive paste containing a carbon material, so that the carbon material is disposed inside the internal electrode after sintering and / or at the interface between the dielectric layer and the internal electrode.
[0006] For example, a ceramic electronic component according to one example includes a body including a dielectric layer and an internal electrode, and an external electrode disposed on the body, with a carbon material disposed within the internal electrode and / or a carbon material disposed at the interface between the dielectric layer and the internal electrode. Effect of the Invention
[0007] One of the various effects of the present disclosure is that it is possible to provide a ceramic electronic component that can improve electrical characteristics.
[0008] Another of the various effects of the present disclosure is that it is possible to provide a ceramic electronic component having excellent high-temperature load reliability. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a schematic perspective view of a ceramic electronic component according to an example. [Diagram 2] 2 is a cross-sectional view that shows a schematic cross section taken along line II' in FIG. 1. [Diagram 3] 2 is a cross-sectional view that shows a schematic cross section taken along line II-II' in FIG. 1. [Figure 4] FIG. 3 is a cross-sectional view showing a schematic example of a P region in FIG. 2. [Diagram 5] 3 is a cross-sectional view showing a schematic diagram of another example of the P region in FIG. 2. [Figure 6] 1 is a diagram illustrating the shapes of internal electrodes and dielectric layers after sintering when ceramic and carbon black are used as a co-material for forming internal electrodes; [Figure 7] 1 is a spectrum showing the components of carbon black by Raman analysis. [Figure 8] 1 is a photograph showing the shape of carbon black taken with a TEM (Transmission Electron Microscopy). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] The present disclosure will be described below with reference to the accompanying drawings. The shapes and sizes of elements in the drawings may be scaled (or highlighted or simplified) for a clearer description.
[0011] In the drawings, the first direction can be defined as the thickness direction, the second direction as the length direction, and the third direction as the width direction.
[0012] FIG. 1 is a schematic perspective view of a ceramic electronic component according to an example, FIG. 2 is a schematic cross-sectional view taken along line II' in FIG. 1, and FIG. 3 is a schematic cross-sectional view taken along line II-II' in FIG. 1.
[0013] Referring to the drawing, a ceramic electronic component 100 according to one example includes a body 110 including a dielectric layer 111 and internal electrodes 121 and 122 , as well as external electrodes 131 and 132 disposed on the body 110 .
[0014] The specific shape of the body 110 is not particularly limited, but may be a hexahedron or a similar shape. Due to shrinkage of the ceramic powder contained in the body 110 during firing and / or sintering, the body 110 may have a substantially hexahedral shape rather than a hexahedral shape having perfectly straight lines. The outer shape of the body 110 having corners, for example, the corners, may be rounded by a polishing process or the like.
[0015] The main body 110 may have a first surface 1 and a second surface 2 facing each other in the thickness direction, a third surface 3 and a fourth surface 4 connected to the first surface 1 and the second surface 2 and facing each other in the length direction, and a fifth surface 5 and a sixth surface 6 connected to the first surface 1 and the second surface 2 and also connected to the third surface 3 and the fourth surface 4 and facing each other in the width direction.
[0016] The body 110 may be formed by alternately stacking dielectric layers 111 and internal electrodes 121, 122. The dielectric layers 111 forming the body 110 are in a fired and / or sintered state, and the boundaries between adjacent dielectric layers 111 may be integrated to such an extent that they are difficult to see without using a scanning electron microscope (SEM).
[0017] The dielectric layer 111 may be formed by firing a ceramic green sheet containing ceramic powder, an organic solvent, and an organic binder. The ceramic powder may be a material having a high dielectric constant, such as a barium titanate (BaTiO3)-based material or a strontium titanate (SrTiO3)-based material, but is not limited thereto.
[0018] Although the thickness of the dielectric layer 111 does not need to be particularly limited, in general, when the dielectric layer 111 is formed thin, less than 0.6 μm, there is a risk of reliability decreasing, particularly when the dielectric layer 111 is 0.4 μm or less in thickness. On the other hand, in the present disclosure, excellent reliability can be ensured even when the dielectric layer 111 is 0.4 μm or less in thickness. Therefore, when the dielectric layer 111 is 0.4 μm or less in thickness, the effect of improving reliability according to the present disclosure can be more significant, and miniaturization and high capacity of ceramic electronic components can be more easily achieved.
[0019] The thickness of the dielectric layer 111 may refer to an average thickness of the dielectric layer 111 disposed between the internal electrodes 121 and 122. The average thickness of the dielectric layer 111 may be measured by scanning an image of a cross section of the body 110 in the length and thickness directions using a scanning electron microscope with a magnification of 10,000. More specifically, the thickness of one dielectric layer may be measured at 30 equally spaced points in the length direction in the scanned image to measure an average value. The 30 evenly spaced points may be designated as active parts Ac, which will be described later. Furthermore, if such an average measurement is extended to 10 dielectric layers 111 to measure the average value, the average thickness of the dielectric layer 111 may be further generalized.
[0020] The body 110 may include an active portion Ac in which a capacitance is formed including a plurality of first internal electrodes 121 and a plurality of second internal electrodes 122 arranged to face each other with the dielectric layer 111 therebetween. The active portion Ac is a portion that contributes to forming the capacitance of the capacitor, and may be formed by repeatedly stacking the plurality of first internal electrodes 121 and the plurality of second internal electrodes 122 with the dielectric layer 111 therebetween.
[0021] The body 110 may further include cover parts 112 and 113 disposed on the upper and lower sides of the active part Ac based on the thickness direction. The cover parts 112 and 113 may include a first cover part 112 disposed on the upper side of the active part Ac and a second cover part 113 disposed on the lower side of the active part Ac. The first cover part 112 and the second cover part 113 may be formed by stacking a single dielectric layer or two or more dielectric layers on the upper and lower surfaces of the active part Ac in the thickness direction, respectively, and may basically play a role in preventing damage to the internal electrodes due to physical or chemical stress. The cover parts 112 and 113 may not include an internal electrode and may include the same material as the dielectric layer 111. For example, the cover parts 112 and 113 may include a ceramic material, for example, the barium titanate-based material described above. Therefore, the boundary between the cover parts 112 and 113 and the adjacent dielectric layer 111 may be integrated to such an extent that it is difficult to confirm without using a scanning electron microscope. In this respect, the cover parts 112 and 113 may include the dielectric layer 111. For example, the cover parts 112 and 113 may be formed of a dielectric layer 111. There is no need to particularly limit the thickness of the cover parts 112 and 113. However, in order to more easily achieve miniaturization and high capacity of the ceramic electronic component, the thickness of the cover parts 112 and 113 may be 20 μm or less.
[0022] The body 110 may further include margin parts 114, 115 disposed on both sides of the active part Ac based on the width direction. The margin parts 114, 115 may include a first margin part 114 providing a fifth surface 5 of the body 110 and a second margin part 115 providing a sixth surface 6. The margin parts 114, 115 may refer to regions between both ends of the internal electrodes 121, 122 and the boundary surface of the body 110 in a cross section obtained by cutting the body 110 in the width-thickness direction. The margin parts 114, 115 may basically serve to prevent damage to the internal electrodes 121, 122 due to physical or chemical stress. The margin parts 114, 115 may include the same or different material as the dielectric layer 111. For example, the margin parts 114, 115 may be formed by applying a conductive paste to a ceramic green sheet except for a portion where the margin parts are to be formed to form an internal electrode. Alternatively, in order to suppress the steps caused by the internal electrodes 121, 122, after lamination, the internal electrodes 121, 122 can be cut to expose them, and then a single dielectric layer or two or more dielectric layers can be laminated on both sides in the width direction of the active portion Ac to form margin portions 114, 115.
[0023] The internal electrodes 121, 122 may be alternately stacked with the dielectric layer 111. The internal electrodes 121, 122 may include a plurality of first internal electrodes 121 and a plurality of second internal electrodes 122. The plurality of first internal electrodes 121 and the plurality of second internal electrodes 122 may be alternately arranged to face each other with the dielectric layer 111 therebetween, and may be exposed to the third surface 3 and the fourth surface 4 of the main body 110, respectively. For example, the plurality of first internal electrodes 121 may be separated from the fourth surface 4 and exposed through the third surface 3. Also, the plurality of second internal electrodes 122 may be separated from the third surface 3 and exposed through the fourth surface 4, respectively. The plurality of first internal electrodes 121 and the plurality of second internal electrodes 122 may be electrically separated from each other by the dielectric layer 111 arranged therebetween. The plurality of first internal electrodes 121 and the plurality of second internal electrodes 122 may be alternately stacked in the thickness direction, but are not limited thereto, and may also be alternately stacked in the width direction.
[0024] The internal electrodes 121 and 122 may be formed of a conductive paste including a conductive metal and a common material. For example, the conductive paste may be printed on the ceramic green sheet forming the dielectric layer 111 by a printing method such as a screen printing method or a gravure printing method, and the internal electrodes 121 and 122 may be printed as a result. The ceramic green sheets on which the internal electrodes 121 and 122 are printed are alternately stacked and fired and / or sintered to form the active part Ac of the body 110. The conductive metal may include nickel (Ni), copper (Cu), palladium (Pd), silver (Ag), gold (Au), platinum (Pt), tin (Sn), tungsten (W), titanium (Ti), and / or an alloy including the same, and may preferably include, but is not limited to, nickel (Ni). The common material may include, but is not limited to, a carbon material, for example, carbon black, graphite, and may preferably include, but is not limited to, carbon black.
[0025] On the other hand, since the sintering temperature of nickel (Ni) internal electrodes is about 600℃ lower than that of ceramic dielectrics, it is possible to consider using a ceramic co-material, which is the same material as the dielectric, as a sintering inhibitor to delay the sintering shrinkage of the internal electrodes. However, in this case, the ceramic co-material may cause non-uniformity in the dielectric composition, and it may be difficult to improve the electrical characteristics and reliability due to side effects that are difficult to control, such as the generation of coarse grains.
[0026] Meanwhile, the ceramic electronic component 100 according to an embodiment uses a non-ceramic carbon material, for example, carbon black, as a common material in the conductive paste for forming the internal electrodes 121 and 122. In this case, electrical properties can be improved and excellent reliability under high temperature load can be ensured. For example, it is possible to realize a level of connectivity of the internal electrodes equivalent to or higher than that of a ceramic common material. In addition, the use of a common material that is free from reaction with the dielectric can maintain the uniformity of the dielectric composition and suppress the generation of coarse grains. Therefore, it is possible to improve the level of electrical properties and reliability.
[0027] In addition, in the ceramic electronic component 100 according to an example, even after sintering, a carbon material, for example, carbon black, may be disposed and present inside the internal electrodes 121, 122 and / or at the interface between the dielectric layer 111 and the internal electrodes 121, 122. For example, the carbon material, for example, carbon black, may remain without being decomposed. Therefore, the coverage bridge characteristics of the defective parts of the connection of the internal electrodes 121, 122 may improve the level of electrical characteristics and reliability. This may be advantageous in realizing thinner internal electrodes 121, 122. In addition, the heat dissipation function via the carbon material may have the effect of reducing heat accumulation during high pressure operation.
[0028] Meanwhile, the carbon material, for example, carbon black, may have a substantially spherical shape. Having a substantially spherical shape includes not only a completely spherical shape but also a roughly spherical shape. The substantially spherical carbon material, for example, carbon black, may have various forms, such as hollow, core-shell, and filled. In this case, the above-mentioned effects can be more effectively achieved. Meanwhile, the shape may be within the conductive paste, but is not limited thereto, and the shape within the internal electrodes 121 and 122 after sintering or the shape at the interface with the dielectric layer 111 may be substantially the same.
[0029] Furthermore, the carbon material, for example, carbon black, may be smaller than the conductive particles, for example, nickel (Ni) particles. For example, the particle size may be 1 / 2 or less of the nickel (Ni) particles. For example, the particle size may be 0.05 μm or less. The particle size may be measured by photographing the shape of the carbon black in the conductive paste using a TEM or the like, or by polishing the body 110 to expose the internal electrodes 121 and 122 and then photographing them using a TEM or the like. When multiple carbon black particles are present, each particle size may be 0.05 μm or less. In this case, the above-mentioned effect can be more effectively achieved. Meanwhile, the particle size may be the particle size in the conductive paste, but is not limited thereto, and the particle size in the internal electrodes 121 and 122 after sintering or the particle size at the interface with the dielectric layer 111 is substantially the same.
[0030] Furthermore, the carbon material, for example, carbon black, can have electrical conductivity. In this case, the above-mentioned role of the sintering inhibitor can be performed more effectively. In this case, the above-mentioned effects can be realized more effectively. Meanwhile, such electrical conductivity can be obtained not only in the conductive paste, but also in the internal electrodes 121, 122 after sintering, or at the interface with the dielectric layer 111.
[0031] Although the thickness of the internal electrodes 121, 122 does not need to be particularly limited, in general, when the internal electrodes 121, 122 are formed thin, less than 0.6 μm, there is a risk of reliability decreasing, especially when the thickness of the internal electrodes 121, 122 is 0.4 μm or less. On the other hand, in the present disclosure, excellent reliability can be ensured even when the thickness of the internal electrodes 121, 122 is 0.4 μm or less. Therefore, when the thickness of the internal electrodes 121, 122 is 0.4 μm or less, the effect of improving reliability according to the present disclosure can be more remarkable, and miniaturization and high capacity of ceramic electronic components can be more easily achieved.
[0032] The thickness of the internal electrodes 121, 122 may refer to the average thickness of the internal electrodes 121, 122. The average thickness of the internal electrodes 121, 122 may be measured by scanning an image of a cross section of the body 110 in the length and thickness directions using a scanning electron microscope with a magnification of 10,000. More specifically, the thickness of one internal electrode may be measured at 30 equally spaced points in the length direction in the scanned image, and an average value may be measured. The 30 equally spaced points may be designated as active parts Ac. Furthermore, if such an average measurement is extended to 10 internal electrodes and an average value is measured, the average thickness of the internal electrodes may be further generalized.
[0033] The external electrodes 131 and 132 are disposed on the third surface 3 and the fourth surface 4 of the main body 110, and may extend partially to the first surface 1, the second surface 2, the fifth surface 5, and the sixth surface 6, respectively. The external electrodes 131 and 132 may include a first external electrode 131 and a second external electrode 132 connected to a plurality of first internal electrodes 121 and a plurality of second internal electrodes 122, respectively. The first external electrode 131 is disposed on the third surface 3 of the main body 110, and may extend partially to the first surface 1, the second surface 2, the fifth surface 5, and the sixth surface 6, respectively. The second external electrode 132 is disposed on the fourth surface 4 of the main body 110, and may extend partially to the first surface 1, the second surface 2, the fifth surface 5, and the sixth surface 6, respectively. However, the present invention is not limited thereto, and the number and shape of the external electrodes 131 and 132 may be changed according to the shape of the internal electrodes 121 and 122 and other purposes.
[0034] The external electrodes 131 and 132 may be formed using any material having electrical conductivity such as a metal, and a specific material may be determined in consideration of electrical characteristics, structural stability, etc., and may further have a multi-layer structure. For example, the external electrodes 131 and 132 may include first electrode layers 131a and 131b disposed on the main body 110, and second electrode layers 131b and 132b disposed on the first electrode layers 131a and 132a.
[0035] The first electrode layers 131a and 132a may be, for example, fired electrodes including conductive metal and glass. The first electrode layers 131a and 132a may be formed by dipping the body 110 into a paste including conductive metal and glass. Alternatively, the first electrode layers 131a and 132a may be formed by transferring a sheet including conductive metal and glass onto the body 110. The conductive metal included in the first electrode layers 131a and 132a may be a material having excellent electrical conductivity, but is not limited thereto. For example, the conductive metal may include copper (Cu), nickel (Ni), palladium (Pd), platinum (Pt), gold (Au), silver (Ag), lead (Pb), and / or an alloy including the same, and may preferably include copper (Cu) and / or nickel (Ni), but is not limited thereto.
[0036] The first electrode layers 131a and 132a may be, for example, resin-based electrodes containing conductive metal and resin. The first electrode layers 131a and 132a may be formed by applying and curing a paste containing conductive metal and resin. The conductive metal contained in the first electrode layers 131a and 132a may be, but is not limited to, a material having excellent electrical conductivity. For example, the conductive metal may include copper (Cu), nickel (Ni), palladium (Pd), platinum (Pt), gold (Au), silver (Ag), lead (Pb) and / or an alloy containing the same, and may preferably include, but is not limited to, copper (Cu) and / or nickel (Ni). The resin contained in the first electrode layers 131a and 132a may be, but is not limited to, an insulating resin. For example, the resin may include, but is not limited to, an epoxy resin.
[0037] The first electrode layers 131a and 132a may have a multi-layer structure in which the resin-based electrode is disposed on the fired electrode, but is not limited thereto, and various other electrode layers may be disposed.
[0038] The second electrode layers 131b and 132b can improve mounting characteristics. The type of the second electrode layers 131b and 132b is not particularly limited, and may be a plating layer containing nickel (Ni), tin (Sn), palladium (Pd) and / or an alloy containing these, and may be formed of a plurality of layers. The second electrode layers 131b and 132b may be, for example, a nickel (Ni) plating layer or a tin (Sn) plating layer, and may be in a form in which a nickel (Ni) plating layer and a tin (Sn) plating layer are sequentially formed on the first electrode layers 131a and 132a. The second electrode layers 131b and 132b may also include a plurality of nickel (Ni) plating layers and / or a plurality of tin (Sn) plating layers.
[0039] FIG. 4 is a cross-sectional view that illustrates an example of the P region in FIG.
[0040] Referring to the drawing, a plurality of first carbon materials a1 may be disposed in the first internal electrode 121. Also, a plurality of second carbon materials a2 may be disposed at an interface between the dielectric layer 111 and the first internal electrode 121. The dielectric layer 111 may be in contact with an upper surface and a lower surface of the first internal electrode 121, and a plurality of second carbon materials a2 may be disposed at interfaces between the upper surface and the lower surface of the dielectric layer 111 and the first internal electrode 121, respectively.
[0041] Each of the plurality of first carbon materials a1 may include the above-mentioned carbon black. The plurality of first carbon materials a1 may form a cluster channel. Here, the cluster channel may be a plurality of channels formed by arranging the plurality of first carbon materials a1 in the first internal electrode 121, and the plurality of channels may be connected to each other. For example, a plurality of carbon black particles may be arranged in various directions in the internal electrode to form a plurality of channels, and the plurality of channels may be connected to each other.
[0042] Each of the plurality of second carbon materials a2 may include the above-mentioned carbon black. The plurality of second carbon materials a2 may form a cluster channel. Here, the cluster channel may be formed by arranging the plurality of second carbon materials a2 in a line at the interface between the dielectric layer 111 and the first internal electrode. For example, the plurality of carbon black particles may be arranged in a line at the interface between the dielectric layer and the internal electrode to form a channel.
[0043] Meanwhile, the arrangement of the plurality of first carbon materials a1 and the plurality of second carbon materials a2 has been described using the first internal electrode 121, but the same content can be applied to the second internal electrode 122, and detailed description thereof will be omitted to avoid duplication.
[0044] FIG. 5 is a cross-sectional view that illustrates another example of the P region in FIG.
[0045] Referring to the drawing, a plurality of first carbon materials a1' may be disposed in the first internal electrode 121. Also, a plurality of second carbon materials a2 may be disposed at an interface between the dielectric layer 111 and the first internal electrode 121. The dielectric layer 111 may be in contact with an upper surface and a lower surface of the first internal electrode 121, and a plurality of second carbon materials a2 may be disposed at interfaces between the dielectric layer 111 and the upper surface and the lower surface of the first internal electrode 121, respectively.
[0046] Each of the plurality of first carbon materials a1' may include the above-mentioned carbon black. Such a plurality of first carbon materials a1' may form cluster spots. Here, the cluster spots may be formed by some of the plurality of first carbon materials a1' gathering together to form a plurality of spots in the first internal electrode 121, and the plurality of spots may be spaced apart from each other. The gathered first carbon materials a1' may or may not be in contact with each other. For example, carbon black particles may gather together to form a plurality of spots in the internal electrode, and these spots may be spaced apart from each other.
[0047] Each of the plurality of second carbon materials a2 may include the above-mentioned carbon black. The plurality of second carbon materials a2 may form a cluster channel. Here, the cluster channel may be formed by arranging the plurality of second carbon materials a2 in a line at the interface between the dielectric layer 111 and the first internal electrode 121. For example, the plurality of carbon black particles may be arranged in a line at the interface between the dielectric layer and the internal electrode to form a channel.
[0048] Each particle of the plurality of first carbon materials a1' disposed inside the first internal electrode 121 may have a larger diameter, etc. than each particle of the plurality of second carbon materials a2 disposed at the interface between the dielectric layer 111 and the first internal electrode 121, but is not limited to this.
[0049] Meanwhile, the arrangement of the plurality of first carbon materials a1' and the plurality of second carbon materials a2 has been described using the first internal electrode 121, but the same content can be applied to the second internal electrode 122, and detailed description thereof will be omitted to avoid duplication.
[0050] FIG. 6 shows schematic diagrams of the shapes of the internal electrodes and dielectric layers after sintering when ceramic and carbon black are used as co-materials for forming the internal electrodes.
[0051] Referring to the drawings, when a material including nickel (Ni) particles A and ceramic co-material b is used as a conductive paste material for forming the internal electrodes 121', 122' as in (a), coarse grains G' may be formed during the sintering process, and the coarse grains G' may be distributed at the interface between the internal electrodes 121', 122' after sintering, which may reduce the connectivity and smoothness of the internal electrodes 121', 122'. On the other hand, when a material including nickel (Ni) particles A and carbon black co-material a is used as a conductive paste material for forming the internal electrodes 121, 122 as in (b), it is possible to prevent the grains G from becoming coarse during the sintering process, and the grains G are uniformly distributed at the interface between the internal electrodes 121, 122 after sintering, which may increase the connectivity and smoothness of the internal electrodes 121, 122.
[0052] FIG. 7 is a spectrum showing the components of carbon black by Raman analysis.
[0053] In the figure, (a) shows the Raman spectrum of powdered carbon black, (b) shows the Raman spectrum of the powdered carbon black after sintering, and (c) shows the Raman spectrum of the electrode region of the internal electrode part inside the ceramic body.
[0054] Referring to the drawing, it can be seen from the Raman spectrum that a carbon material, for example, carbon black, is present inside the internal electrodes 121, 122 and / or at the interface between the dielectric layer 111 and the internal electrodes 121, 122.
[0055] FIG. 8 is a photograph showing the shape of carbon black taken with a TEM (Transmission Electron Microscopy).
[0056] Referring to the drawing, the carbon black in a powder sol state before being mixed into the conductive paste for forming the internal electrodes may be, but is not limited to, spherical fine conductive crystallized carbon black having a diameter of about 50 nm or less.
[0057] In the present disclosure, a multilayer ceramic capacitor has been described as an example of a ceramic electronic component, but the present disclosure is not limited thereto, and may also be applied to other types of ceramic electronic components, such as inductors, piezoelectric elements, varistors, thermistors, and the like.
[0058] In this disclosure, expressions such as side and side surface are used for convenience to mean a left / right direction or a surface in that direction based on the drawing, expressions such as upper side, upper part, and top surface are used for convenience to mean an upper direction or a surface in that direction based on the drawing, and expressions such as lower side, lower part, and bottom surface are used for convenience to mean a lower direction or a surface in that direction. Furthermore, being located on the side, upper side, upper part, lower part, or bottom part is used as a concept that includes not only a case where a target component is in direct contact with a reference component in the corresponding direction, but also a case where the target component is located in the corresponding direction but is not in direct contact with the reference component. However, this is a definition of the direction for convenience of explanation, and the scope of the claims is not particularly limited by the description of the direction, and the concepts of up / down can be changed at any time.
[0059] In the present disclosure, the term "connected" refers not only to being directly connected, but also to being indirectly connected via an adhesive layer or the like. Furthermore, the term "electrically connected" refers to both being physically connected and not being connected. Furthermore, the terms "first" and "second" are used to distinguish one component from another, and do not limit the order and / or importance of the corresponding components. In some cases, the first component may be named the second component, and similarly the second component may be named the first component, without departing from the scope of the right.
[0060] The expression "one example" used in the present disclosure does not mean the same embodiment as the other, but is provided to emphasize and explain the unique features that are different from each other. However, the above-mentioned one example does not exclude that it is realized in combination with the features of another example. For example, even if the matter described in a specific example is not described in another example, it can be understood as a description related to the other example, unless there is a description that is opposite or contradictory to the matter in the other example.
[0061] The terms used in this disclosure are merely used to describe an example and are not intended to limit the disclosure. In this case, the singular expression includes the plural expression unless the context clearly indicates otherwise.
Claims
1. a body including a dielectric layer and an internal electrode; an external electrode disposed on the body; A plurality of first carbon materials each including carbon black are disposed within the internal electrode; The carbon black is substantially spherical and interconnected, The plurality of first carbon materials form a cluster channel including a plurality of channels connected to each other.
2. a body including a dielectric layer and an internal electrode; an external electrode disposed on the body; A plurality of first carbon materials each including carbon black are disposed within the internal electrode; a plurality of second carbon materials each including carbon black are disposed at interfaces between the dielectric layers and the internal electrodes; each particle of the plurality of first carbon materials has a larger diameter than each particle of the plurality of second carbon materials; The plurality of first carbon materials form cluster spots including a plurality of spots spaced apart from each other by gathering a portion of the plurality of first carbon materials, The plurality of second carbon materials are arranged in a row at the interface to form cluster channels.
3. The ceramic electronic component according to claim 2 , wherein the carbon black has a substantially spherical shape.
4. The ceramic electronic component according to claim 1 , wherein the carbon black has electrical conductivity.
5. The ceramic electronic component according to claim 1 , wherein the carbon black has a particle size of 0.05 μm or less.
6. a plurality of second carbon materials each including carbon black are disposed at interfaces between the dielectric layers and the internal electrodes; The ceramic electronic component according to claim 1 , wherein the plurality of second carbon materials are arranged in a row at the interface to form a cluster channel.
7. The ceramic electronic component according to claim 1 , wherein the internal electrodes have a thickness of 0.4 μm or less.
8. The ceramic electronic component according to claim 1 , wherein the internal electrodes contain nickel (Ni).
9. a body including a dielectric layer and an internal electrode; an external electrode disposed on the body; a plurality of carbon materials including carbon black are disposed at the interfaces of the dielectric layers and the internal electrodes; The carbon black is substantially spherical and interconnected, The plurality of carbon materials are aligned in a row at the interface to form cluster channels.
10. the dielectric layer contacts the upper and lower surfaces of the internal electrodes; The ceramic electronic component according to claim 9 , wherein the plurality of carbon materials are disposed at an interface between the dielectric layer and the upper surface of the internal electrode and an interface between the dielectric layer and the lower surface of the internal electrode.
Citation Information
Patent Citations
Layered ceramic capacitor
JP2000150293A