Sensor device

A sensor device with a thin glass film and resin layer laminate maintains strain sensor sensitivity and impact resistance, addressing the issue of reduced sensitivity from thick protective materials.

JP7554734B2Active Publication Date: 2024-09-20NITTO DENKO CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021503491
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-03-06
Filing Date
2020-02-10
Publication Date
2024-09-20
Estimated Expiration
2040-02-10

AI Technical Summary

Technical Problem

The use of thick protective materials like tempered glass reduces the sensitivity of strain sensors in electronic devices, and there is a need for a protective material that does not easily damage the glass while maintaining sensor sensitivity.

Method used

A sensor device comprising an optical laminate with a thin glass film (20 μm to 150 μm) sandwiched between adhesive layers, which includes a resin layer for impact resistance and a strain detection unit, allowing the glass film to protect the resin layer and maintain sensor sensitivity.

Benefits of technology

The solution provides a sensor device with enhanced impact resistance and puncture resistance, while maintaining strain sensor sensitivity by using a thin glass film that does not impair detection sensitivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007554734000002
    Figure 0007554734000002
  • Figure 0007554734000001
    Figure 0007554734000001
Patent Text Reader

Abstract

Provided is a sensor device wherein the sensitivity of a distortion sensor is not impeded readily even if a glass material is being used as a protective material, and wherein the glass material does not become damaged readily. This sensor device comprises a distortion detection unit, and an optical layered body having a glass film, an adhesive layer, a resin layer, and a pressure-sensitive adhesive layer in this order, wherein the thickness of the glass film is 20 μm to 150 μm. In one embodiment, the distortion detection unit is disposed on the pressure-sensitive adhesive layer side of the optical layered body.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a sensor device. [Background technology]

[0002] In recent years, electronic devices equipped with touch panels have become widespread. As one such electronic device, an electronic device equipped with a strain sensor has been considered, and in this electronic device, the strain sensor detects the touch position.

[0003] Meanwhile, a protective material is often placed on the outermost surface (touch surface) of an electronic device to protect the device. A glass plate or a plastic plate is used as the protective material (for example, Patent Document 1). In particular, a glass plate is useful because of its excellent hardness and is widely used. In addition, tempered glass, which has a strength greater than that of ordinary glass, is sometimes used as the glass plate. However, tempered glass tends to be thick to ensure strength, and the use of a thick protective material poses a problem of reducing the sensitivity of the strain sensor. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2010-164938 A Summary of the Invention [Problem to be solved by the invention]

[0005] The present invention has been made to solve the above-mentioned problems in the conventional art, and its object is to provide a sensor device that uses glass material as a protective material while not impairing the sensitivity of the strain sensor and in which the glass material is not easily damaged. [Means for solving the problem]

[0006] The sensor device of the present invention includes an optical laminate having a glass film, an adhesive layer, a resin layer, and a pressure-sensitive adhesive layer in this order, and a strain detection unit, and the glass film has a thickness of 20 μm to 150 μm. In one embodiment, the strain detection unit is disposed on the pressure-sensitive adhesive layer side of the optical laminate. In one embodiment, the glass film and the resin layer are disposed without any layer other than the adhesive layer being present between the glass film and the resin layer. In one embodiment, the resin layer is a polarizing plate. In one embodiment, the resin layer has an elastic modulus at 23° C. of 1 GPa to 10 GPa. Effect of the Invention

[0007] According to the present invention, it is possible to provide a sensor device in which the sensitivity of the strain sensor is not easily impaired even when a glass material is used as a protective material, and the glass material is not easily damaged. [Brief description of the drawings]

[0008] [Figure 1] 1 is a schematic cross-sectional view of a sensor device according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] A. Overall configuration of the sensor device 1 is a schematic cross-sectional view of a sensor device according to one embodiment of the present invention. The sensor device 100 includes an optical laminate 10 including a glass film 11, an adhesive layer 12, a resin layer 13, and a pressure-sensitive adhesive layer 14 in this order, and a strain detection unit 20. The strain detection unit 20 is disposed on the pressure-sensitive adhesive layer 14 side of the optical laminate 10. The glass film 11 has a thickness of 20 μm to 150 μm. The glass film 11 and the resin layer 13 are preferably disposed directly via the adhesive layer 12 (i.e., without any layer other than the adhesive layer 12 being present between the glass film 11 and the resin layer 13).

[0010] The optical laminate 10 has high hardness because it includes the glass film 11. The optical laminate 10 can be arranged in an electronic device including the sensor device of the present invention so that the glass film 11 is the outermost surface. By using the optical laminate 10 including the glass film 11, the electronic device including the sensor device of the present invention can be effectively protected. In addition, the optical laminate 10 includes the resin layer 13 on one side of the glass film 11, so that the glass film 11 can be prevented from being broken, and is excellent in impact resistance and piercing resistance. In the present invention, the impact given to the surface of the glass film 11 can be effectively released to the resin layer 13 side, so that it is considered to have excellent impact resistance as described above. In addition, the glass film 11 has a function of protecting the resin layer 13. That is, in the present invention, the glass film 10 and the resin layer 13 protect each other. Therefore, it is possible to reduce the protective member, and a lightweight and thin optical laminate can be obtained.

[0011] Furthermore, in the present invention, since a thin glass film 11 can be employed, the detection sensitivity of the strain detection unit 20 is unlikely to be impaired. The strain detection unit 20 includes a strain sensor 21, which detects the amount of strain by reading a resistance value that changes when strain occurs in the strain detection unit 20. In reality, the amount of strain is detected when the strain detection unit 20 bends due to an external force applied from the glass film 11 side. In general, assuming that an external force is applied to the center of a two-point supported sample (glass film), the amount of strain is expressed as {(external force)×(distance between support points) 3} / {48 × (elastic modulus of sample) × (second moment of area)}, and the second moment of area is {(sample depth) × (sample thickness) 3} / 12, which is proportional to the cube of the thickness of the sample. That is, the amount of strain is inversely proportional to the cube of the thickness of the sample (glass film). In the present invention, a thin glass film can be used by combining it with a resin layer, and as a result, a sensor device in which the sensitivity of the strain detection unit is unlikely to be impaired can be provided.

[0012] Although not shown, the sensor device of the present invention may further include any other appropriate members as long as the effects of the present invention can be obtained. For example, a liquid crystal cell, a display member such as an organic light-emitting display, an optical film such as a polarizing plate, etc. may be disposed between the optical laminate and the strain detection unit.

[0013] B. Optical laminate As described above, the optical laminate includes a glass film, an adhesive layer, a resin layer, and a pressure-sensitive adhesive layer in this order. The optical laminate may further include other layers. Examples of the other layers include an anti-reflection layer, an anti-glare layer, an antistatic layer, and a conductive layer.

[0014] The thickness of the optical laminate is preferably 60 μm to 550 μm, and more preferably 100 μm to 300 μm.

[0015] B-1. Glass film Any appropriate glass film may be adopted. The glass film may be classified according to composition, for example, soda-lime glass, borate glass, aluminosilicate glass, quartz glass, etc. Also, according to alkali components, it may be non-alkali glass or low-alkali glass. The content of alkali metal components (e.g., Na2O, K2O, Li2O) in the glass is preferably 15% by weight or less, more preferably 10% by weight or less.

[0016] The thickness of the glass film is 20 μm to 150 μm, preferably 30 μm to 150 μm, and more preferably 50 μm to 100 μm. Within such a range, an optical laminate having excellent flexibility, in which the glass film is less likely to break, and excellent productivity can be obtained.

[0017] The glass film preferably has a light transmittance of 85% or more at a wavelength of 550 nm, and a refractive index of 1.4 to 1.65 at a wavelength of 550 nm.

[0018] The density of the glass film is preferably 2.3 g / cm 3 ~3.0g / cm 3 and more preferably 2.3 g / cm 3 ~2.7g / cm 3 With a glass film within the above range, a lightweight optical laminate can be obtained.

[0019] Any suitable method may be adopted as the method for forming the glass film. Typically, the glass film is produced by melting a mixture containing a main raw material such as silica or alumina, an antifoaming agent such as mirabilite or antimony oxide, and a reducing agent such as carbon at a temperature of 1400°C to 1600°C, forming it into a thin plate, and then cooling it. Examples of the method for forming the glass film include a slot downdraw method, a fusion method, and a float method. The glass film formed into a plate shape by these methods may be chemically polished with a solvent such as hydrofluoric acid as necessary to make it thinner or to increase its smoothness.

[0020] B-2.Adhesive layer In this specification, the adhesive layer refers to a layer that can bond substances by being interposed between the substances. Therefore, when the adherend attached to the adhesive layer is peeled off, the adhesive layer does not have practical adhesive strength. On the other hand, the pressure-sensitive adhesive layer refers to a substance that has adhesiveness at room temperature and adheres to the adherend with light pressure. Therefore, even when the adherend attached to the pressure-sensitive adhesive layer is peeled off, the pressure-sensitive adhesive maintains practical adhesive strength. In the present invention, both the glass film and the resin layer can be effectively protected by laminating the glass film and the resin layer via an adhesive.

[0021] The adhesive layer is formed from any suitable adhesive. Examples of the adhesive include polyester adhesives, polyurethane adhesives, polyvinyl alcohol adhesives, and epoxy adhesives. Among these, epoxy adhesives are preferred because they provide particularly good adhesion.

[0022] In one embodiment, a curing adhesive such as a thermosetting, photocuring, or moisture curing adhesive is used as the adhesive. When the adhesive is a thermosetting adhesive, the adhesive layer can exhibit peel resistance by being heated and cured (solidified). When the adhesive is a photocuring adhesive such as an ultraviolet curing adhesive, the adhesive layer can exhibit peel resistance by being irradiated with light such as ultraviolet light and cured. When the adhesive is a moisture curing adhesive, it can react with moisture in the air and cure, and therefore it can also be left to cure and exhibit peel resistance.

[0023] The adhesive may be, for example, a commercially available adhesive, or may be prepared as an adhesive solution (or dispersion) by dissolving or dispersing various curable resins in a solvent.

[0024] The thickness of the adhesive layer is preferably 0.1 μm to 30 μm, more preferably 0.5 μm to 20 μm, and further preferably 1 μm to 10 μm. Within such a range, an optical layered body having excellent flexibility and excellent puncture resistance can be obtained.

[0025] The elastic modulus of the adhesive layer at 23°C is preferably 0.5 GPa to 15 GPa, more preferably 0.8 GPa to 10 GPa, and further preferably 1 GPa to 5 GPa. Within such ranges, an optical laminate having excellent flexibility and excellent puncture resistance can be obtained. In this specification, the elastic modulus can be measured using an autograph under the following conditions. <Method for measuring elastic modulus> Measurement temperature: 23℃ Sample size: thickness 50μm, width 2cm, length 15cm Chuck distance: 10cm Tensile speed: 10mm / min

[0026] B-3.Resin layer Examples of the resin layer include a polarizing plate, a retardation plate, an isotropic film, a conductive film, etc. The resin film may have a single layer structure or a multilayer structure.

[0027] Any suitable material can be used as the material for forming the resin layer. Examples of the material for forming the resin layer include polyolefin resins, cyclic olefin resins, polycarbonate resins, cellulose resins, polyester resins, polyamide resins, polyimide resins, polyether resins, polystyrene resins, (meth)acrylic resins, (meth)acrylic urethane resins, polysulfone resins, acetate resins, epoxy resins, silicone resins, polyarylate resins, polysulfone resins, polyetherimide resins, epoxy resins, urethane resins, silicone resins, and polyvinyl alcohol (PVA) resins.

[0028] The thickness of the resin layer is preferably from 5 μm to 300 μm, more preferably from 30 μm to 250 μm, further preferably from 50 μm to 200 μm, and particularly preferably from 50 μm to 100 μm.

[0029] The elastic modulus of the resin layer at 23° C. is preferably 1 GPa to 10 GPa, more preferably 2 GPa to 7 GPa, and further preferably 2 GPa to 5 GPa. Within such ranges, an optical layered body having excellent impact resistance and puncture resistance can be obtained.

[0030] B-3-1. Polarizing plate In one embodiment, as described above, the resin layer is a polarizing plate. The polarizing plate includes a polarizer and a protective film disposed on at least one side of the polarizer. The thickness of the polarizing plate is preferably 5 μm to 300 μm, more preferably 10 μm to 250 μm, further preferably 25 μm to 200 μm, and particularly preferably 25 μm to 150 μm.

[0031] (Polarizer) The thickness of the polarizer is not particularly limited, and an appropriate thickness can be adopted depending on the purpose. The thickness is typically about 1 μm to 80 μm. In one embodiment, a thin polarizer is used, and the thickness of the polarizer is preferably 20 μm or less, more preferably 15 μm or less, further preferably 10 μm or less, and particularly preferably 6 μm or less. By using such a thin polarizer, a thin optical laminate can be obtained.

[0032] The polarizer preferably exhibits absorption dichroism at any wavelength of 380 nm to 780 nm. The single transmittance of the polarizer is preferably 40.0% or more, more preferably 41.0% or more, even more preferably 42.0% or more, and particularly preferably 43.0% or more. The degree of polarization of the polarizer is preferably 99.8% or more, more preferably 99.9% or more, and even more preferably 99.95% or more.

[0033] Preferably, the polarizer is an iodine-based polarizer. More specifically, the polarizer may be made of a polyvinyl alcohol-based resin (hereinafter, referred to as a "PVA-based resin") film containing iodine.

[0034] Any appropriate resin may be adopted as the PVA-based resin forming the PVA-based resin film. Examples include polyvinyl alcohol and ethylene-vinyl alcohol copolymer. Polyvinyl alcohol is obtained by saponifying polyvinyl acetate. Ethylene-vinyl alcohol copolymer is obtained by saponifying ethylene-vinyl acetate copolymer. The saponification degree of the PVA-based resin is usually 85 mol% to 100 mol%, preferably 95.0 mol% to 99.95 mol%, and more preferably 99.0 mol% to 99.93 mol%. The saponification degree can be determined in accordance with JIS K 6726-1994. By using a PVA-based resin having such a saponification degree, a polarizer having excellent durability can be obtained. If the saponification degree is too high, gelation may occur.

[0035] The average degree of polymerization of the PVA resin can be appropriately selected depending on the purpose. The average degree of polymerization is usually 1000 to 10000, preferably 1200 to 5000, and more preferably 1500 to 4500. The average degree of polymerization can be determined in accordance with JIS K 6726-1994.

[0036] Examples of the method for producing the polarizer include a method (I) of stretching and dyeing a PVA-based resin film alone, and a method (II) of stretching and dyeing a laminate (i) having a resin substrate and a polyvinyl alcohol-based resin layer. The method (I) is a well-known and commonly used method in the art, and therefore a detailed description thereof will be omitted. The production method (II) preferably includes a step of stretching and dyeing a laminate (i) having a resin substrate and a polyvinyl alcohol-based resin layer formed on one side of the resin substrate to produce a polarizer on the resin substrate. The laminate (i) can be formed by applying a coating liquid containing a polyvinyl alcohol-based resin onto a resin substrate and drying it. Alternatively, the laminate (i) may be formed by transferring a polyvinyl alcohol-based resin film onto a resin substrate. Details of the production method (II) are described in, for example, JP 2012-73580 A, which is incorporated herein by reference.

[0037] (Protective film) Any suitable resin film may be used as the protective film. Examples of materials for forming the protective film include polyester resins such as polyethylene terephthalate (PET), cellulose resins such as triacetyl cellulose (TAC), cycloolefin resins such as norbornene resins, olefin resins such as polyethylene and polypropylene, and (meth)acrylic resins. The term "(meth)acrylic resin" refers to acrylic resins and / or methacrylic resins.

[0038] In one embodiment, the (meth)acrylic resin has a glutarimide structure.The (meth)acrylic resin has a glutarimide structure (hereinafter also referred to as glutarimide resin) is described in, for example, JP2006-309033A, JP2006-317560A, JP2006-328329A, JP2006-328334A, JP2006-337491A, JP2006-337492A, JP2006-337493A, JP2006-337569A, JP2007-009182A, JP2009-161744A, and JP2010-284840A. These descriptions are incorporated herein by reference.

[0039] The protective film and the polarizer are laminated via any suitable adhesive layer. The resin substrate used in producing the polarizer can be peeled off before or after laminating the protective film and the polarizer.

[0040] The thickness of the protective film is preferably 4 μm to 250 μm, more preferably 5 μm to 150 μm, further preferably 10 μm to 100 μm, and particularly preferably 10 μm to 50 μm.

[0041] The elastic modulus of the protective film at 23° C. is preferably 1 GPa to 10 GPa, more preferably 2 GPa to 7 GPa, and further preferably 2 GPa to 5 GPa. Within such ranges, an optical laminate having excellent impact resistance and puncture resistance can be obtained.

[0042] B-4.Adhesive layer The pressure-sensitive adhesive layer is formed from any appropriate pressure-sensitive adhesive. For example, a pressure-sensitive adhesive having an acrylic polymer, a silicone polymer, a polyester, a polyurethane, a polyamide, a polyether, a fluorine-based polymer, a rubber-based polymer, or the like as a base polymer is used. An acrylic pressure-sensitive adhesive is preferably used. This is because an acrylic pressure-sensitive adhesive has excellent optical transparency, and exhibits adhesive properties such as appropriate wettability, cohesiveness, and adhesiveness, and can be excellent in weather resistance, heat resistance, and the like. In particular, an acrylic pressure-sensitive adhesive made of an acrylic polymer having 4 to 12 carbon atoms is preferred.

[0043] The thickness of the pressure-sensitive adhesive layer is preferably 1 μm to 100 μm, more preferably 3 μm to 80 μm, and further preferably 3 μm to 50 μm. Within such a range, an optical laminate having excellent flexibility, impact resistance, and puncture resistance can be obtained.

[0044] The pressure-sensitive adhesive layer has a modulus of elasticity at 23° C. of preferably 0.00001 GPa to 10 GPa, more preferably 0.001 GPa to 8 GPa, and further preferably 0.001 GPa to 5 GPa. Within such a range, an optical laminate having excellent flexibility, impact resistance, and puncture resistance can be obtained.

[0045] C. Strain detection unit The strain detection unit detects strain caused by an external force applied to a surface (the surface opposite to the strain detection unit) of the optical laminate laminated on the strain detection unit. As long as it has such a function, the strain detection unit may have any appropriate configuration.

[0046] In one embodiment, as shown in Fig. 1, the strain sensing unit 20 has at least one strain sensor 21. More specifically, the strain sensing unit 20 has a transparent substrate 22 and a strain sensor 21 arranged on at least one side of the transparent substrate 22. When the strain sensors 21 are arranged on both sides of the transparent substrate 23, it is preferable that the strain sensor 21 arranged on one side and the strain sensor 21 arranged on the other side face each other via the transparent substrate 23. On the transparent substrate 22, the strain sensor 21 is arranged in any appropriate form. For example, the strain sensor 21 is arranged in a grid pattern.

[0047] In one embodiment, the strain sensor includes a strain gauge formed of a transparent material. The strain gauge measures strain by detecting the change in resistance value that is specific to a metal material when the metal material is compressed / stretched. The strain gauge may be formed of a plurality of nanostructures, such as a nanomesh structure and a nanowire structure. A material with a low gauge factor is preferably used as a material constituting the strain gauge. The strain gauge factor is a characteristic specific to the material constituting the strain gauge, and represents the sensitivity of the material to strain. The amount of strain ε is expressed by the formula (resistance change amount / gauge resistance) / gauge factor, and the lower the gauge factor of a material, the higher the sensitivity to strain. Examples of materials constituting the strain gauge include Cu, Ni, Cr, and alloys thereof.

[0048] Although not shown, the strain sensing unit may include a detection and processing circuit connected to the strain sensor via wiring. The detection and processing circuit can correlate the change in resistance of the strain gauge with the magnitude of the external force applied to the surface of the optical stack based on a signal from the strain sensor that detects the change in resistance.

[0049] Details of the strain sensing unit are described, for example, in U.S. Patent Application Publication No. 2017 / 0075465, the entire disclosure of which is incorporated herein by reference. EXAMPLES

[0050] The present invention will be described in detail below with reference to examples, but the present invention is not limited to these examples. In the examples, "parts" and "%" are by weight unless otherwise specified.

[0051] [Production Example 1] (Preparation of adhesive) An ultraviolet-curing adhesive was prepared by mixing an epoxy resin (manufactured by Daicel Chemical Industries, Ltd., product name "Celloxide 2021P"), an epoxy resin (manufactured by Daicel Chemical Industries, Ltd., product name "EHPE3150"), an oxetane resin (manufactured by Toa Gosei Co., Ltd., product name "Aron Oxetane OXT-221"), an epoxy group terminal coupling agent (manufactured by Shin-Etsu Chemical Co., Ltd., product name "KBM-403"), and a polymerization initiator (manufactured by San-Apro Ltd., CPI101A, San-Apro Ltd.) in a ratio of 60:10:20:4:2.

[0052] [Example 1] A glass film (manufactured by Nippon Electric Glass Co., Ltd., product name "OA-10G", thickness: 50 μm) and a polyethylene terephthalate film (manufactured by Toray Industries, Inc., product name "Lumirror S10", thickness: 100 μm, elastic modulus: 4 GPa) were laminated via the adhesive prepared in Production Example 1. The obtained laminate was irradiated with ultraviolet light (accumulated light amount: 300 mJ / cm 2 ) was irradiated to obtain a laminate A composed of a glass film / adhesive layer (thickness: 1 μm, elastic modulus: 1 GPa) / resin layer (PET). A laminate B was obtained by laminating an adhesive film (manufactured by Nitto Denko Corporation, product name "LUCIACS CS9861UAS", adhesive layer thickness: 25 μm) on the resin layer (PET) side of the laminate A. Next, the film on the upper side of the liquid crystal panel of a smartphone (manufactured by Apple Inc., product name "i-phone X") was peeled off, and the laminate B was mounted on the liquid crystal panel via the adhesive layer. The elastic modulus was measured under the following conditions using an autograph (manufactured by Shimadzu Corporation, product name "AG-IS"). <Method for measuring elastic modulus> Measurement temperature: 23℃ Sample size: thickness 50μm, width 2cm, length 15cm Chuck distance: 10cm Tensile speed: 10mm / min

[0053] [Example 2] A sensor device was obtained in the same manner as in Example 1, except that the thickness of the glass film was 100 μm.

[0054] [Comparative Example 1] A sensor device was obtained in the same manner as in Example 1, except that the thickness of the glass film was 300 μm.

[0055] [Comparative Example 2] A sensor device was obtained in the same manner as in Example 1, except that the adhesive layer constituting the laminate A was a pressure-sensitive adhesive layer (manufactured by Nitto Denko Corporation, acrylic pressure-sensitive adhesive, product name "LUCIACS CS9861UAS", pressure-sensitive adhesive layer thickness: 25 μm).

[0056] <Evaluation> The sensor devices obtained in the examples and comparative examples were subjected to the following evaluations. The results are shown in Table 1. 1. Sensitivity The glass surface of the laminate B mounted on a smartphone was pressed with a finger, and if the display responded, it was marked as "O", and if there was a delayed response or no response, it was marked as "X". In order to make the display screen visible, a polarizing plate (manufactured by Nitto Denko Corporation, product name "NPF SEG1425DU") was simply placed over the viewing side (above the glass) to check. 2. Shock resistance When a 100g iron ball was dropped from a height of 50mm onto the glass surface of Laminate B mounted on a smartphone, if the glass film or display screen did not break, it was marked as "O", and if it did break, it was marked as "X".

[0057] [Table 1] [Explanation of symbols]

[0058] 10 Optical laminate 11 Glass film 12 Adhesive layer 13 Resin layer 20 Strain sensing unit 100 Sensor Device

Claims

1. An optical laminate having a glass film, an adhesive layer, a resin layer, and a pressure-sensitive adhesive layer in this order; and a strain detection unit that detects a strain caused by an external force applied to a surface of the optical laminate; The thickness of the glass film is 20 μm to 150 μm, The adhesive layer has an elastic modulus of 0.5 GPa to 15 GPa at 23°C. Sensor device.

2. The sensor device according to claim 1 , wherein the strain detection unit is disposed on the pressure-sensitive adhesive layer side of the optical laminate.

3. The sensor device according to claim 1 , wherein the glass film and the resin layer are disposed without any layer other than the adhesive layer being present between the glass film and the resin layer.

4. The sensor device according to claim 1 , wherein the resin layer is a polarizing plate.

5. The sensor device according to any one of claims 1 to 4, wherein the resin layer has an elastic modulus of 1 GPa to 10 GPa at 23°C.

Citation Information

Patent Citations

  • Touch screen panel

    JP2010164938A

  • Protective substrate for display unit

    JP2013037207A

  • Glass laminate, and protective material for display device

    JP2017024386A

  • Deformation detection sensor and electronic apparatus

    JP2017219392A

  • Strain gauge

    JP2018185346A