Raw material liquid concentration system and concentration device

The membrane distillation system with a hydrophobic porous membrane and polymer coating addresses the limitations of existing methods by ensuring efficient concentration of heat-sensitive substances without denaturation and wetting, achieving high recovery rates.

JP7555456B2Active Publication Date: 2024-09-24ASAHI KASEI KOGYO KABUSHIKI KAISHA
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023106069
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-10-11
Filing Date
2023-06-28
Publication Date
2024-09-24
Estimated Expiration
2040-10-09

AI Technical Summary

Technical Problem

Existing methods for concentrating raw material liquids, such as ultrafiltration and reverse osmosis, face issues like reduced recovery rates due to solute adhesion and pressure limitations, while membrane distillation suffers from wetting and low vapor permeation, especially when handling heat-sensitive substances.

Method used

A membrane distillation system using a porous membrane with high hydrophobicity and specific pore characteristics, combined with a hydrophobic polymer coating, to prevent wetting and enable efficient concentration at room temperature, maintaining solute integrity.

Benefits of technology

The system effectively concentrates heat-sensitive substances like peptides and proteins without denaturation, achieving high recovery rates and preventing membrane wetting, even at room temperature.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555456000008
    Figure 0007555456000008
  • Figure 0007555456000007
    Figure 0007555456000007
  • Figure 0007555456000006
    Figure 0007555456000006
Patent Text Reader

Abstract

To provide a raw material liquid concentration system in medicine production process which suppresses wetting of a membrane for membrane distillation, and has treatment speed that can be industrially achieved even at normal temperature.SOLUTION: There is provided a raw material liquid concentration system for a medicine production process using a membrane distillation method for bringing a raw material liquid containing a solvent and a solute into contact with cooling water through a membrane for membrane distillation, passing the solvent in the raw material liquid through the membrane for membrane distillation in a vapor state, and moving the solvent to the side of the cooling water, wherein a porous membrane having a water contact angle of the surface of 90° or more, an average pore diameter of 0.02 μm or more and 0.5 μm or less, and porosity of 60% or more and 90% or less is used as the membrane for membrane distillation.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a raw material liquid concentrating system and a concentrating device, and more particularly to a raw material liquid concentrating system and a concentrating device that can efficiently concentrate a raw material liquid by separating a part of a solvent from the raw material liquid containing a pharmaceutical substance and an intermediate by a membrane distillation method to concentrate the raw material liquid while suppressing deterioration or reduction of components in the raw material liquid. [Background technology]

[0002] There are many industrial cases where a raw material liquid that requires concentration contains both water and an organic solvent as solvents. Substances with amino acid sequences, such as peptides and proteins, are widely used as diagnostic and testing agents and pharmaceuticals. Because they are very expensive, it is important to recover them in high yields without denaturing them during the manufacturing process. Ultrafiltration membranes are commonly used as a method for stably and efficiently extracting and purifying proteins. Ultrafiltration membranes are a technology for separating components by sieving, and because this separation method does not involve temperature changes, it is possible to reduce energy load. For example, proteins with molecular weights of several thousand to several million can often be fractionated and purified using ultrafiltration membranes. When using ultrafiltration membranes, components with sizes equal to or larger than the membrane's molecular weight cutoff are retained in the raw liquid, but the solvent water passes through the membrane. Therefore, ultrafiltration membranes are effective for concentrating solutions containing proteins (e.g., Patent Document 1). Also known is the reverse osmosis (RO) method, which uses a membrane that allows the solvent to permeate at the molecular level. The RO method is a method in which the raw liquid is pressurized to a predetermined pressure higher than the osmotic pressure of the raw liquid and then supplied to an RO membrane module, and the solvent (typically water) in the raw liquid is removed by permeating through the RO membrane, thereby concentrating the raw liquid (for example, Patent Document 2).

[0003] Another method for concentrating a raw liquid is known as a membrane distillation (MD) method, which separates a solvent in a raw liquid by utilizing a vapor pressure difference between liquids. As one method of membrane distillation, a direct contact MD (DCMD) method is well known, in which the raw liquid is brought into contact with cooling water having a lower temperature than the raw liquid through a membrane, and the vapor that does not contain the effective substance in the raw liquid is transferred from the raw liquid to the cooling water, thereby concentrating the raw liquid (for example, Patent Document 3). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] International Publication No. 2013 / 170977 [Patent Document 2] Japanese Patent Application Publication No. 11-75759 [Patent Document 3] International Publication No. 2016 / 006670 Summary of the Invention [Problem to be solved by the invention]

[0005] However, the ultrafiltration membrane described in Patent Document 1 requires pressurization of the raw liquid, which causes the solutes contained in the raw liquid to adhere to the membrane surface, resulting in a problem of reduced recovery. In addition, in the case of medium-sized molecule drugs that have been developed recently, some have molecular weights smaller than the molecular cutoff of the ultrafiltration membrane, and some of them permeate the ultrafiltration membrane, resulting in a reduced recovery rate. The RO method of Patent Document 2 requires pressurization of the feed liquid, which causes the solutes contained in the feed liquid to adhere to the RO membrane surface, resulting in a decrease in recovery rate. In addition, in the RO method, the osmotic pressure of the solvent in the concentrated feed liquid does not exceed the pressure of the high-pressure pump used for pressurization, so the concentration rate of the feed liquid by the RO method is limited by the capacity of the pump.

[0006] On the other hand, according to the membrane distillation method of Patent Document 3, when the membrane distillation membrane is wetted, the raw material liquid flows into the cooling water side, making it impossible to concentrate. In addition, since a porous membrane with a small pore size is selected as the membrane distillation membrane, the amount of vapor permeation is small, which is an issue. Furthermore, in order to increase the amount of vapor permeation, it is necessary to increase the temperature of the raw material liquid. In this case, the raw material liquid is generally heated to 60°C or higher, and there are few reports of the application of the membrane distillation method to the concentration of raw material liquid containing solutes such as enzymes and peptides that are likely to be denatured by heat. The present invention aims to provide a system and an apparatus for concentrating raw material liquid in a pharmaceutical manufacturing process, which suppresses wetting of the membrane distillation membrane, which is a problem in the membrane distillation method, and has an industrially feasible processing speed even at room temperature. [Means for solving the problem]

[0007] The present invention has been made to achieve the above object. In other words, the inventors discovered that when concentrating a raw material liquid by membrane distillation, by using a porous membrane that is highly water permeable and highly hydrophobic as the membrane for membrane distillation, wetting of the membrane distillation membrane by the raw material liquid can be suppressed and vapor can be efficiently extracted even at room temperature, thereby enabling efficient concentration while preventing denaturation of the active ingredients in the raw material liquid, and thus completed the present invention. That is, the present invention is as follows.

[0008] A raw material liquid concentration system using a membrane distillation method in which a raw material liquid containing a solvent and a solute is contacted with cooling water via a membrane distillation membrane, and the solvent in the raw material liquid is passed through the membrane distillation membrane in a vapor state and transferred to the cooling water side, As the membrane for membrane distillation, a porous membrane is used having a surface water contact angle of 90° or more, an average pore size in the range of 0.02 μm to 0.5 μm, and a porosity of 60% to 90%. A raw material liquid concentration system for pharmaceutical manufacturing processes. Aspect 2: The raw material liquid concentration system according to aspect 1, wherein a hydrophobic polymer is attached to at least a portion of the membrane distillation membrane. Aspect 3: The raw material liquid concentration system according to aspect 2, wherein the amount of the hydrophobic polymer adhered has a distribution in the thickness direction of the membrane distillation membrane, and the amount of the hydrophobic polymer adhered on the surface layer of at least one side of the membrane distillation membrane is greater than the amount of the hydrophobic polymer adhered inside. Aspect 4: The raw material liquid concentrating system according to aspect 3, wherein the amount of the hydrophobic polymer attached decreases from the surface layer on one side of the membrane distillation membrane to the surface layer on the opposite side. Aspect 5: The opposite surface to which the hydrophobic polymer is less adhered is hydrophilically treated, and the hydrophilically treated surface is brought into contact with cooling water, and the side having a large amount of hydrophobic polymer attached thereto is not subjected to hydrophilization treatment, and the side is brought into contact with the raw material liquid; 5. The feedstock liquid concentrating system according to claim 4. Aspect 6: The raw material liquid concentrating system according to any one of aspects 2 to 5, wherein the hydrophobic polymer is a polymer having a fluorine atom-containing group in a side chain and has at least one side chain selected from a (per)fluoroalkyl group, a (per)fluoropolyether group, an alkylsilyl group, and a fluorosilyl group. <<Aspect 7>> The raw material liquid concentration system according to any one of Aspects 1 to 6, wherein the material of the membrane distillation membrane comprises at least one resin selected from the group consisting of polysulfone, polyethersulfone, polyethylene, polypropylene, polyvinylidene fluoride, polytetrafluoroethylene, ethylene-tetrafluoroethylene copolymer, and polychlorotrifluoroethylene. Aspect 8: The raw material liquid concentrating system according to any one of aspects 1 to 7, wherein the solvent includes at least one selected from the group consisting of water, acetonitrile, methanol, ethanol, and isopropanol. Aspect 9: The raw material liquid concentrating system according to any one of aspects 1 to 8, wherein the solute is at least one selected from the group consisting of amino acids, peptides, proteins, sugars, vaccines, nucleic acids, antibiotics, antibody-drug conjugates (ADCs), and vitamins. Aspect 10: The raw material liquid concentrating system according to any one of aspects 1 to 9, wherein the solute has a number average molecular weight of 100 to 50,000. Aspect 11: The raw material liquid concentrating system according to any one of aspects 1 to 10, wherein the temperature of the raw material liquid is adjusted to a range of 5°C or higher and 50°C or lower. A concentrating apparatus for concentrating a raw material liquid by a membrane distillation method, comprising: As the membrane for membrane distillation, a membrane having a water contact angle of 90° or more on the membrane surface, an average pore size in the range of 0.02 μm to 0.5 μm, and a porosity of 60 to 90% is used. Concentrator. Aspect 13: A concentrating device according to aspect 13, wherein a hydrophobic polymer is attached to at least a portion of the membrane distillation membrane. Aspect 14: The concentrating apparatus of aspect 13, wherein the amount of the hydrophobic polymer adhered has a distribution in the thickness direction of the membrane distillation membrane, and the amount of the hydrophobic polymer adhered on the surface layer of at least one side of the membrane distillation membrane is greater than the amount of the hydrophobic polymer adhered inside. Effect of the Invention

[0009] The concentration system of the present invention can concentrate a raw liquid containing a solute having an amino acid sequence, for example, by a membrane distillation process at near room temperature, without causing wetting and while substantially maintaining the solute composition of the raw liquid. If the concentration system of the present invention is applied to the concentration of raw material liquid containing useful components used for medical purposes in the manufacturing process of pharmaceuticals, etc., the useful components, which are sensitive to heat and pressure, can be concentrated with a high recovery rate without denaturing them. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a conceptual diagram for explaining an example of an embodiment of a membrane module applied to a raw material liquid concentration system of the present invention. [Diagram 2] FIG. 1 is a conceptual diagram for explaining an example of an embodiment of a raw material liquid concentrating system of the present invention. [Diagram 3]FIG. 2 is a conceptual diagram for explaining one example of an embodiment regarding adhesion of a membrane and a hydrophobic polymer to be applied to the raw material liquid concentrating system of the present invention. [Figure 4] FIG. 2 is a conceptual diagram for explaining one example of an embodiment relating to a membrane and hydrophilization applied to the raw material liquid concentrating system of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Preferred embodiments of the present invention will now be described in detail by way of non-limiting examples. <Raw material liquid concentration system> The raw material liquid concentrating system of the present invention will be described with reference to the drawings. FIG. 1 shows an example of a membrane module for membrane distillation that is preferably used when concentrating a raw material liquid by membrane distillation in the concentration system of the present invention. The membrane distillation membrane module (100) of Fig. 1 includes a housing (10) containing a plurality of hollow fiber membrane distillation membranes (20), both ends of which are bonded and fixed with an adhesive resin (30). Both ends of the membrane distillation membranes (20) are open and not closed. The side of the housing (10) has a first housing side pipe (11) for introducing cooling water (CW) and a second housing side pipe (12) for discharging the cooling water (CW), which enable the cooling water (CW) to circulate in the external space of the membrane distillation membrane (20). At both ends of the axial direction of the housing (10) (left-right direction in Figure 1), there are a left opening for introducing the raw liquid (a) and a right opening for discharging the raw liquid (a), which allow the raw liquid (a) to flow through the hollow portion of the membrane distillation membrane (20). The interior of the membrane distillation membrane module (100) is divided by the membrane distillation membrane (20) into a space on the hollow side of the membrane distillation membrane (20) and a space on the external space side of the membrane distillation membrane (20). These two spaces are fluidically isolated from each other except that a specific solvent can pass between them through the outer wall of the membrane distillation membrane (20).

[0012] The membrane distillation membrane (20) is, for example, a hollow fiber, and its outer wall must be highly hydrophobic and porous, but must not allow liquid to penetrate inside, and must allow only gas to pass through the outer wall. In addition, since high vapor permeability is required even at room temperature, the membrane must have a high porosity and an appropriate average pore size. In the present invention, As the membrane for membrane distillation, a porous membrane is used in which the water contact angle of the membrane surface is 90° or more, the average pore size is in the range of 0.02 μm to 0.5 μm, and the porosity is 60% to 90%.

[0013] To concentrate the raw liquid by the membrane distillation method, the raw liquid (a) is passed through one side of the membrane distillation membrane (20) (in FIG. 1, the hollow space of the hollow fiber membrane distillation membrane), while cooling water (CW) with a lower temperature than the raw liquid (a) is passed through the other side (in FIG. 1, the external space side of the hollow fiber membrane distillation membrane). Then, the pores communicating with both spaces inside the membrane wall come into contact with the raw liquid (a) and the cooling water (CW) through the membrane wall. As a result, the steam generated from the raw liquid (a) with a high vapor pressure passes through the membrane wall and moves to the cooling water (CW) with a low vapor pressure, where it is cooled and liquefied, thereby concentrating the raw liquid (a).

[0014] FIG. 2 shows an example of a concentration system of the present invention. In the concentration system of Fig. 2, a means (piping system) for circulating the raw liquid (a) is provided at both axial ends of the membrane module (100) for membrane distillation shown in Fig. 1. The piping system for circulating the raw liquid (a) includes a raw liquid storage tank (200), a pump (P) for circulating the raw liquid (a), a flowmeter (FM) for indicating the circulation flow rate, a flow rate regulator (not shown) for adjusting the circulation flow rate, a temperature regulator (TC) for maintaining the temperature of the raw liquid (a) at a set temperature, and a pressure gauge (PG) for indicating the liquid pressure when the raw liquid (a) is supplied to the membrane module (100) for membrane distillation. The raw liquid storage tank (200) is provided with a liquid level gauge (LG), and the concentration rate can be estimated from the degree of drop in the liquid level.

[0015] Meanwhile, the housing side pipe of the membrane module (100) for membrane distillation is provided with a means (piping system) for circulating cooling water (CW). This piping system is equipped with a cooling water storage tank (300), a pump (P) for circulating the cooling water (CW), a flowmeter (FM) indicating the circulation flow rate, a flow rate regulator (not shown) for adjusting the circulation flow rate, and a temperature regulator (TC) for maintaining the temperature of the cooling water (CW) at a set temperature. The solvent moves from the raw material liquid (a) to the cooling water (CW) by the membrane distillation, and the volume of the cooling water (CW) increases over time. Therefore, the storage amount of the cooling water storage tank (300) increases as the membrane distillation continues. At this time, if the cooling water (CW) can be disposed of, an overflow port can be provided in the cooling water storage tank (300) to maintain the storage amount of the cooling water (CW) at a constant volume.

[0016] In a raw material liquid concentration system for manufacturing pharmaceuticals, etc., raw material liquid (a) containing substances that can be decomposed by heating, such as peptides and proteins, must be handled, and therefore raw material liquid (a) must be kept at a low temperature (for example, below 50°C). In addition, as a solvent (b) for raw material liquid (a), a liquid with low surface tension, such as acetonitrile, methanol, ethanol, isopropanol, etc., is used. For these reasons, membranes for membrane distillation are required to have strong hydrophobicity so that they do not get wet even with liquids of low surface tension, and high vapor permeability so that the vapor of the solvent (b) can be efficiently extracted from the raw liquid (a) at room temperature. Therefore, the membrane for membrane distillation used in the present invention must be highly hydrophobic and have a water contact angle of 90° or more. It is also necessary to ensure high vapor permeability, and it is required to be a porous membrane with an average pore size in the range of 0.02 μm to 0.5 μm and a porosity of 60% to 90%. These requirements will be described later.

[0017] <<Each element of the raw material liquid concentration system>> The above is an overview of the concentration of the raw material liquid by the raw material liquid concentration system of the present invention. Next, each element constituting the raw material liquid concentration system of the present invention will be described in detail below. <Raw material liquid (a)> The raw liquid (a) is a fluid containing a solute and a solvent (b) and is intended to be concentrated by the system of the present invention. This raw liquid (a) may be an emulsion, so long as it is a fluid. Examples of the raw material liquid (a) applicable to the present invention include solutions or dispersions containing pharmaceuticals, pharmaceutical raw materials, pharmaceutical substances, pharmaceutical intermediates, etc. (hereinafter, these are collectively referred to as "pharmaceutical substances, etc."); food; seawater; produced water discharged from gas fields, oil fields, etc. In the raw liquid concentrating system of the present invention, a concentrated liquid (c) is obtained from the solvent removed while the composition of the raw liquid a is maintained almost unchanged. Therefore, when the raw liquid concentrating system of the present invention is applied to the concentration of a solution or dispersion containing a pharmaceutical substance or the like as a solute, it becomes possible to concentrate the solution or dispersion while maintaining its medical efficacy.

[0018] [Solute of raw material solution a] As the pharmaceutical substance, for example, it is preferable that the solute is a useful substance selected from the group consisting of amino acids, peptides, proteins, sugars, vaccines, nucleic acids, antibiotics, antibody-drug conjugates (ADCs), and vitamins, and that this solute is dissolved or dispersed in a suitable solvent.

[0019] An amino acid is a compound having an amino acid backbone consisting of a carboxyl group, an amino group, and a moiety connecting them. In this specification, the term "amino acid" encompasses essential amino acids, non-essential amino acids, and non-natural amino acids. Examples of essential amino acids include tryptophan, lysine, methionine, phenylalanine, threonine, valine, leucine, isoleucine, etc. Examples of non-essential amino acids include arginine, glycine, alanine, serine, tyrosine, cysteine, asparagine, glutamine, proline, aspartic acid, glutamic acid, etc.

[0020] An unnatural amino acid refers to any artificial compound that does not exist in nature and has an amino acid backbone in the molecule. However, examples of unnatural amino acids as pharmaceutical substances include those obtained by binding a desired labeling compound to the amino acid backbone. Examples of labeling compounds include dyes, fluorescent substances, luminescent substances, enzyme substrates, coenzymes, antigenic substances, and protein-binding substances. Examples of unnatural amino acids that are preferred as pharmaceutical ingredients include labeled amino acids and functionalized amino acids. A labeled amino acid is a non-natural amino acid having an amino acid backbone bound to a labeling compound, and specific examples thereof include amino acids having an amino acid backbone containing an aromatic ring in the side chain bound to a labeling compound. Examples of functionalized amino acids include photoresponsive amino acids, photoswitch amino acids, fluorescent probe amino acids, and fluorescently labeled amino acids.

[0021] A peptide refers to a compound in which 2 to less than 70 amino acid residues are bound, and may be linear or cyclic. Examples of peptides include L-alanyl-L-glutamine, β-alanyl-L-histidine cyclosporine, and glutathione. A protein generally refers to a compound in which amino acid residues are bound, and which has a longer chain length than a peptide. As used herein, the protein is preferably applied as, for example, a protein drug. Examples of protein preparations include interferon α, interferon β, interleukins 1 to 12, growth hormone, erythropoietin, insulin, granulocyte-colony stimulating factor (G-CSF), tissue plasminogen activator (TPA), natriuretic peptides, blood coagulation factor VIII, somatomedin, glucagon, growth hormone-releasing factor, serum albumin, and calcitonin.

[0022] Examples of sugars include monosaccharides, disaccharides, sugar chains (excluding disaccharides), and sugar chain derivatives. Examples of monosaccharides include glucose, fructose, galactose, mannose, ribose, deoxyribose, etc. Examples of disaccharides include maltose, sucrose, lactose, etc. The term "sugar chain" as used herein refers to a concept excluding disaccharides, and examples thereof include glucose, galactose, mannose, fucose, xylose, glucuronic acid, iduronic acid, etc. Examples of sugar chain derivatives include saccharide derivatives such as N-acetylglucosamine, N-acetylgalactosamine, and N-acetylneuraminic acid.

[0023] Vaccines include, for example, hepatitis A vaccine, hepatitis B vaccine, and hepatitis C vaccine; Examples of nucleic acids include oligonucleotides, RNA, aptamers, decoys, etc. Antibiotics include, for example, streptomycin and vancomycin; Each of them can be mentioned.

[0024] Examples of vitamins include vitamin A, vitamin B, vitamin C, etc., and include their derivatives, salts, etc. Examples of vitamin B include vitamin B6, vitamin B12, etc.

[0025] The number average molecular weight of the solute contained in the raw material liquid may be about 100 to 75,000, preferably about 100 to 50,000, more preferably about 100 to 10,000, and is particularly preferably a low molecular weight compound having a number average molecular weight of 100 to 6,000. If the molecular weight of the solute is excessively small, it may pass through the membrane for membrane distillation, whereas if the molecular weight is excessively large, it may cause adhesion of the solute to the membrane surface, which is undesirable.

[0026] [Solvent (b) in raw material solution (a)] The solvent (b) in the raw material liquid (a) can be any inorganic or organic solvent as long as it is liquid and can dissolve or disperse the solute in the raw material liquid (a). The solvent is preferably water, acetonitrile, methanol, ethanol, or isopropanol, and one or more selected from these may be appropriately selected and used. The solvent may be, for example, a mixture containing two or more selected from water, acetonitrile, methanol, and isopropanol.

[0027] <Concentrate (c)> The concentrated liquid (c) obtained by concentrating the raw liquid (a) is obtained by preserving the solutes in the raw liquid (a) almost as they are and preferentially separating the solvent (b). In the raw liquid concentration system of the present invention, the amount of the solvent (b) separated from the raw liquid (a) can be arbitrarily controlled.

[0028] <Membrane for membrane distillation> As the membrane for membrane distillation used in the present invention, it is preferable to use a porous membrane. A porous membrane has pores that are interconnected through the thickness of the membrane from one surface to the other. The pores may be voids in a network of the membrane material (e.g., a polymer) and may be branched or continuous. The pores may be permeable to vapor but not liquid.

[0029] The membrane distillation membrane used in the present invention has a water contact angle on at least one surface of 90° or more, preferably greater than 90°, more preferably 110° or more, and even more preferably 120° or more, from the viewpoint of avoiding wetting of the membrane. There is no upper limit to the water contact angle of the membrane in relation to the effects of the present invention, but in reality it may be 150° or less. The water contact angle in this specification is a value measured by the sessile drop method in accordance with JIS R 3257. Specifically, 2 μL of pure water is dropped onto the surface of the measurement object, and the angle formed between the measurement object and the droplet is quantified by analyzing a projected image. In the membrane distillation membrane used in the present invention, it is preferable that substantially the entire area of ​​one side surface exhibits a water contact angle in the above range. The shape of the membrane for membrane distillation used in the present invention will be described later. When the membrane is in the form of a hollow fiber, it is preferable that the outer surface of the hollow fiber exhibits a water contact angle in the above range.

[0030] The average pore size of the membrane for membrane distillation is in the range of 0.02 μm to 0.5 μm, preferably in the range of 0.03 μm to 0.3 μm. When the average pore size is 0.02 μm or more, the vapor permeation resistance is not too large, and the concentration rate of the raw material liquid a is increased. When the average pore size is 0.5 μm or less, the effect of suppressing wetting of the membrane is good. The average pore size is a value measured by the half-dry method in accordance with ASTM: F316-86. From the viewpoint of achieving both vapor permeability and wetting suppression, the narrower the pore size distribution of the membrane, the more preferable. Specifically, the pore size distribution, which is the ratio of the maximum pore size to the average pore size, is preferably within the range of 1.2 to 2.5, more preferably within the range of 1.2 to 2.0. The maximum pore size is a value measured using a bubble point method.

[0031] The porosity of the membrane distillation membrane is in the range of 60% or more and 90% or less from the viewpoint of achieving both high vapor permeability and long-term durability. In order to obtain high vapor permeability, the porosity of the membrane distillation membrane is 60% or more, preferably 70% or more. In order to maintain the strength of the membrane itself well and to prevent problems such as breakage during long-term use, the porosity of the membrane distillation membrane is 90% or less, preferably 85% or less. The surface opening ratio of the membrane for membrane distillation is preferably 15% or more, more preferably 18% or more, and even more preferably 20% or more for each surface from the viewpoint of obtaining an efficient concentration rate, and is preferably 60% or less, more preferably 55% or less, and even more preferably 50% or less from the viewpoint of maintaining the strength of the membrane itself well and making it difficult for problems such as breakage to occur during long-term use. The above surface opening ratio is a value obtained by detecting holes using image analysis software in an image of the membrane surface observed by a scanning electron microscope (SEM).

[0032] Examples of materials constituting the membrane for membrane distillation include materials containing at least one resin selected from the group consisting of polysulfone, polyethersulfone, polyethylene, polypropylene, polyvinylidene fluoride, polytetrafluoroethylene, ethylene-tetrafluoroethylene copolymer, and polychlorotrifluoroethylene. From the viewpoint of being able to manufacture a membrane excellent in hydrophobicity, mechanical durability, and thermal durability with high membrane formability, polyvinylidene fluoride, ethylene-tetrafluoroethylene copolymer, or polychlorotrifluoroethylene are preferred.

[0033] In one embodiment of the present invention, a hydrophobic polymer may be attached to at least a part of the membrane for membrane distillation in order to improve hydrophobicity. The hydrophobic polymer can form a hydrophobic coating on at least one surface of the membrane for membrane distillation or inside the membrane to impart water repellency to the membrane or improve the water repellency of the membrane. The hydrophobic polymer can be applied to the membrane for membrane distillation in a solution state dissolved in a suitable solvent such as water or a fluorine-based solvent, and then the solvent is evaporated to adhere to the surface or the inside, or both, of the membrane. The application of the hydrophobic polymer solution may be performed by a suitable method such as spraying or immersion. In this specification, the term "hydrophobic polymer" refers to a polymer that has low affinity for water, and may be, for example, a polymer having a hydrophobic structure. Examples of the hydrophobic structure include a non-polar group or a low polarity group, a non-polar skeleton or a low polarity skeleton, etc. Examples of the non-polar group or the low polarity group include a hydrocarbon group, a fluorine-containing group, etc., and examples of the non-polar skeleton or the low polarity skeleton include a hydrocarbon main chain, a siloxane main chain, etc.

[0034] Examples of hydrophobic polymers include polymers having siloxane bonds and fluorine atom-containing polymers. More specific examples include the following: (A) Polymers having siloxane bonds, such as dimethyl silicone gel, methylphenyl silicone gel, reactive modified silicone gels having organic functional groups (amino groups, fluoroalkyl groups, etc.), silicone-based polymers that react with silane coupling agents to form crosslinked structures, and polymer gels that are crosslinked products of these. (a) A fluorine atom-containing polymer is a polymer having a fluorine atom-containing group in a side chain, where the fluorine atom-containing group is a (per)fluoroalkyl group, a (per)fluoropolyether group, an alkylsilyl group, a fluorosilyl group, or the like. In particular, the hydrophobic polymer is preferably a polymer of a (meth)acrylate monomer and / or a vinyl monomer having a (per)fluoroalkyl group and / or a (per)fluoropolyether group having 1 to 12 carbon atoms.

[0035] The hydrophobic polymer may be attached to the entire pores of the membrane distillation membrane, but from the viewpoint of preventing the intrusion of liquid into the pores and ensuring vapor permeability, it is preferable that the amount of hydrophobic polymer attached has a distribution in the thickness direction of the membrane distillation membrane, with a large amount of polymer attached to the surface layer of the membrane that comes into contact with the liquid and a small amount attached inside the thickness direction of the membrane so that the pore structure is maintained. From this viewpoint, it is preferable that the amount of hydrophobic polymer attached on the surface layer of at least one side of the membrane distillation membrane is greater than the amount attached inside, and it is more preferable that the amount of hydrophobic polymer attached decreases from the surface layer of one side of the membrane distillation membrane to the surface layer of the opposite side. The "surface layer of the membrane" here refers to the part of the membrane that comes into contact with the liquid and its vicinity. Quantitatively, it refers to a range of about 10 μm from the outermost part of the membrane toward the inside in the thickness direction. On the other hand, the "inside of the membrane" refers to the part of the membrane that does not come into contact with the liquid and through which only vapor passes, and refers to the part other than the surface layer of the membrane. In the present invention, the ratio of the amount of hydrophobic polymer attached on the surface layer (inner surface and / or outer surface) of the membrane distillation membrane to the amount of hydrophobic polymer attached in the interior (center) is preferably 1.2 times or more, more preferably 2.0 times or more, and particularly preferably 3.0 times or more. When comparing the amount of hydrophobic polymer attached to the surface and inside of a membrane distillation membrane by analysis using an appropriate surface analysis device described below, the measured values ​​of the following regions of the membrane distillation membrane are used for comparison. Surface layer of membrane distillation membrane: The area from the surface of the membrane distillation membrane to a depth of 10 μm Inside the membrane distillation membrane: The area within ±5% of the membrane thickness, centered at a depth of 1 / 2 the membrane thickness from the surface of the membrane distillation membrane

[0036] Figure 3 shows an example of the distribution of hydrophobic polymers when the membrane for membrane distillation is in the form of a hollow fiber. Figure 3(a) shows the distribution of hydrophobic polymers in a cross section perpendicular to the longitudinal direction of the hollow fiber, and Figure 3(b) shows the distribution of hydrophobic polymers in a cross section in the longitudinal direction of the hollow fiber. In Figures 3(a) and (b), the darker the gray, the higher the concentration of hydrophobic polymers present. 3(a) and (b), in the case of this hollow fiber membrane for membrane distillation, a large amount of hydrophobic polymer is attached near the inner surface of the hollow fiber membrane, and the amount of hydrophobic polymer near the outer surface is small. In this case, it is preferable to pass the raw material liquid (a) through the hollow part in contact with the inner surface where the amount of hydrophobic polymer attached is large, from the viewpoint of preventing wetting of the membrane. The distribution of the hydrophobic polymer may be high near the outer surface of the hollow fiber and low near the inner surface. In this case, it is preferable to pass the raw material liquid (a) through the outer space of the hollow fiber in contact with the outer surface where the amount of the hydrophobic polymer attached is high.

[0037] The amount of hydrophobic polymer attached to a membrane distillation membrane can be determined directly as a mass by extracting the membrane distillation membrane having the hydrophobic polymer attached thereto with a good solvent for the hydrophobic polymer, and then removing the solvent from the extract. In addition, a suitable surface analysis device is used to analyze the membrane distillation membrane to which the hydrophobic polymer is attached, and the amount of attachment can be determined from the signal intensity ratio between the constituent material of the membrane distillation membrane and the hydrophobic polymer. Since the surface analysis device can analyze any part of the membrane distillation membrane, the distribution of attached hydrophobic polymer can be known by comparing the signal intensity ratio for each part of the membrane. Examples of surface analysis equipment in this case include an IR (infrared spectrum absorption) device, an XPS (X-ray photoelectron spectroscopy) device, and a TOF-SIMS (time-of-flight secondary ion spectroscopy) device.

[0038] To attach a hydrophobic polymer to a membrane for membrane distillation, a coating solution in which the hydrophobic polymer is dissolved in a suitable solvent can be applied to the membrane and dried. To obtain a desired hydrophobic polymer distribution, various methods can be used to appropriately adjust the coating site, the volatility (boiling point) of the solvent in the coating solution, the concentration of the hydrophobic polymer in the coating solution, and the drying conditions after coating. For example, when coating is performed by the immersion method, the lower the volatility (higher the boiling point) of the solvent in the coating solution and the milder the drying conditions after coating, the more the coating solution containing the hydrophobic polymer can move toward the membrane surface during the drying process, and therefore the more distribution can be generated in the thickness direction of the membrane.

[0039] When the hydrophobic polymer is attached in a distribution that decreases from the surface layer on one side of the membrane distillation membrane to the surface layer on the opposite side, the surface on which the amount of attached hydrophobic polymer is less may be subjected to a hydrophilization treatment. The surface on which the hydrophobic polymer is less attached has low hydrophobicity and high affinity with highly hydrophilic solvents, whereas the surface on which the hydrophobic polymer is more attached has high hydrophobicity and low affinity with highly hydrophilic solvents. By utilizing this, only the surface on which the hydrophobic polymer is less attached can be made hydrophilic by wetting it with a highly hydrophilic solvent. For example, when a membrane for membrane distillation in which the amount of attached hydrophobic polymer decreases from the surface layer on one side to the surface layer on the other side is immersed in, for example, ethanol, only the part with a small amount of attached hydrophobic polymer becomes wet with ethanol (21), as shown in Figure 4. When the membrane for membrane distillation in this state is used for concentration by membrane distillation, the distance in the thickness direction of the membrane through which the vapor passes is substantially shortened, and the amount of vapor passing per unit time can be increased. When using such a hydrophilically treated membrane for membrane distillation, it is preferable to bring the hydrophilically treated surface into contact with cooling water and the opposite surface having a larger amount of hydrophobic polymer attached thereto into contact with the raw material liquid (a).

[0040] [Membrane distillation membrane shapes and sizes] The shape of the membrane for membrane distillation may be any shape, such as flat membrane, hollow fiber membrane, tubular type, etc. When a flat membrane is used, the shape of the membrane module may be selected from spiral type, pleated type, laminated type, etc. The membrane is sealed in a bag shape and a spacer or the like is appropriately inserted so that the raw material liquid and the cooling liquid are not mixed and a flow path is secured. The thickness of the membrane for membrane distillation of the present invention is preferably 10 μm to 1,000 μm, more preferably 20 μm to 500 μm, from the viewpoint of achieving both vapor permeability and mechanical strength of the membrane. If the membrane thickness is 1,000 μm or less, high vapor permeability can be obtained, while if the membrane thickness is 10 μm or more, the membrane can be used without being deformed. When the membrane for membrane distillation is a hollow fiber membrane, the outer diameter is 300 μm or more and 5,000 μm or less, preferably 350 μm or more and 4,000 μm or less, and the inner diameter of the hollow fiber membrane is, for example, 200 μm or more and 4,000 μm or less, preferably 250 μm or more and 3,000 μm or less.

[0041] <Membrane distillation module> In the present invention, when the membrane distillation membrane is in the form of a hollow fiber, a membrane bundle in which a plurality of hollow fiber membrane distillation membranes are bundled together may be used in the form of a membrane distillation membrane module packed in an appropriate module. The shape of the module may be a cylinder, a polygonal prism, or another polyhedron, and there is no limitation on the shape. Preferably, the hollow fiber membrane bundle is housed in a cylindrical or polygonal prism housing so that the longitudinal direction of the hollow fibers coincides with the axial direction of the housing, and both ends of the hollow fiber bundle are fixed to the inside of the housing with an appropriate adhesive resin. In this case, it is preferable that the hollow fiber bundle is fixed liquid-tightly with the adhesive resin so that the flow paths inside and outside the hollow fiber membranes are not mixed.

[0042] The adhesive resin is desired to have high mechanical strength and heat resistance at 100° C. Examples of the adhesive resin include thermosetting epoxy resins and thermosetting urethane resins. From the viewpoint of heat resistance, epoxy resins are preferable. From the viewpoint of handling, urethane resins are preferable. The adhesive fixing method may be in accordance with a known adhesive method for producing a membrane module for membrane distillation. The configuration of the housing is selected from the viewpoints of chemical resistance, which is the property that various performances are not deteriorated by the solutes and solvents contained in the raw material liquid (a) and the cooling water (CW), as well as pressure resistance, heat resistance, impact resistance, weather resistance, etc. For example, resin, metal, etc. can be used. From the above viewpoints, it is preferable to select from synthetic resins such as polypropylene, polysulfone, polyethersulfone, polyvinylidene fluoride, ABS resin, fiber reinforced plastic, polyvinyl chloride resin, etc., and metals such as stainless steel, brass, titanium, etc.

[0043] (Component retention of the raw material liquid concentration system of the present invention) According to the above-described feedstock liquid concentrating system of the present invention, a highly concentrated product in which the composition of solutes contained in the feedstock liquid is substantially maintained can be efficiently obtained. Therefore, the source liquid concentrating system of the present invention is suitable for use in, for example, medical manufacturing processes. The analysis of the solutes in the obtained concentrate may be appropriately selected depending on the types of components contained in the raw material liquid and the concentrate, and may be performed by various known analytical methods such as ICP-MS (inductively coupled plasma mass spectrometry), nuclear magnetic resonance spectroscopy (NMR), gas chromatography / mass spectrometry (GC / MS), colorimetry, fluorescence, and high performance liquid chromatography (HPLC).

[0044] <Concentration device of the present invention> The concentrating device of the present invention includes the membrane for membrane distillation of the present invention as described above. Therefore, the concentrating device of the present invention has the following features: A concentrating apparatus for concentrating a raw material liquid by a membrane distillation method, comprising: The membrane used for membrane distillation has a water contact angle of 90° or more on the membrane surface, an average pore size in the range of 0.02 μm to 0.5 μm, and a porosity of 60% to 90%. A hydrophobic polymer may be attached to at least a portion of the membrane distillation membrane, and the amount of hydrophobic polymer attached may be distributed in the thickness direction of the membrane distillation membrane, and the amount of hydrophobic polymer attached on the surface layer of at least one side of the membrane distillation membrane may be greater than the amount of polymer attached inside. For other aspects of the concentrating device of the present invention, reference may be made to the description of the concentrating system of the present invention. EXAMPLES

[0045] The configuration and effects of the present invention will be further described below with reference to examples, but the present invention is not limited to the following examples in any way.

[0046] <<Physical properties of hollow fiber membranes for membrane distillation>> In this example, various physical properties of the hollow fiber membrane for membrane distillation were determined by the various measuring methods described below.

[0047] [Water contact angle on the outer surface of hollow fiber membrane] The water contact angle of the hollow fiber membrane for membrane distillation was measured by the sessile drop method in accordance with JIS R 3257. A 2μL droplet of pure water was dropped onto the outer surface of the hollow fiber membrane sample under the conditions of 23℃ and 50% relative humidity, and the contact angle was calculated by image analysis to determine the angle formed between the droplet and the outer surface of the hollow fiber membrane. The measurement was performed five times, and the number average value was used as the water contact angle.

[0048] [Outer diameter, inner diameter, and membrane thickness of hollow fiber membrane] The outer and inner diameters of the hollow fiber membrane distillation membrane were determined by microscopic observation. Specifically, the hollow fiber membrane was thinly cut with a razor or the like in a direction perpendicular to the longitudinal direction, a microscopic image of the cross section was obtained, and the outer and inner diameters of the cross section were measured. The membrane thickness of the hollow fiber membrane was calculated by the following formula (1):

number

[0049] [Average pore size of hollow fiber membrane] The average pore size of the hollow fiber membrane for membrane distillation was measured by the method for measuring the average pore size (also known as the half-dry method) described in ASTM: F316-86. The measurement was performed on a hollow fiber membrane approximately 10 cm long, using ethanol as the liquid, under standard measurement conditions of 25°C and a pressure rise rate of 0.01 atm / sec. The average pore size was calculated by the following formula (2): Average pore diameter [μm]=2,860×(s[dyne / cm]) / (p[Pa]) ···(2) {In the above formula, s is the surface tension of the liquid used, and p is the half-dry air pressure.} Here, the surface tension s of the liquid ethanol used at 25°C is 21.97 dyne / cm, so 2,860 × s = 62,834 is used, and equation (2) is transformed into the following equation (3). The value of the half-dry air pressure p is then substituted into equation (3) to determine the average pore diameter of the hollow fiber membrane. Average pore diameter [μm]=62,834 / (p[Pa]) ···(3)

[0050] [Maximum pore size of hollow fiber membrane] The maximum pore size of the hollow fiber membrane for membrane distillation was measured by the bubble point method using ethanol as an immersion liquid. One end of an 8 cm long hollow fiber membrane was blocked, and the other end was connected to a nitrogen gas supply line via a pressure gauge. In this state, nitrogen gas was supplied to replace the inside of the line with nitrogen, and then the hollow fiber membrane was immersed in ethanol. At this time, the hollow fiber membrane was immersed in ethanol under a very slight nitrogen pressure to prevent ethanol from flowing back into the line. With the hollow fiber membrane immersed in ethanol, the nitrogen gas pressure was slowly increased until the pressure P (kg / cm) at which nitrogen gas bubbles began to stably emerge from the hollow fiber membrane was reached. 2 This P was calculated using the following formula (4): d=C1γ / P (4) {In formula (4), d is the maximum pore diameter of the hollow fiber, C1 is a constant, γ is the surface tension of the immersion liquid, and P is the pressure.} The maximum pore diameter d of the hollow fiber membrane was calculated by substituting the above formula into the formula (4). In this case, the value of C1γ when ethanol was used as the immersion liquid was set to 0.632 (kg / cm), and the maximum pore diameter d (μm) was calculated.

[0051] [Porosity of hollow fiber membrane] The porosity of the hollow fiber membrane for membrane distillation was calculated from the mass of the hollow fiber membrane and the density (true density) of the material constituting the hollow fiber membrane. That is, the hollow fiber membrane is cut to a certain length, its mass is measured, and the mass is calculated by the following formula (5):

number

[0052] [Amount of hydrophobic polymer attached] (1) IR and ATR spectroscopy The amount of hydrophobic polymer attached to hollow fiber membranes for membrane distillation was compared by IR spectrum analysis and ATR (attenuated total reflection, internal reflection) method using a ZnSe crystal as a prism. The measurement was performed using a PerkinElmer Spectrum One, and the pressing pressure of the crystal was set to a pressure contour value of about 30. From the obtained IR spectrum, the ratio of the peak intensity derived from the hydrophobic polymer to the peak intensity derived from the constituent material of the hollow fiber membrane was calculated to calculate the amount of hydrophobic polymer attached to the membrane surface. The hollow fiber membrane samples were cut from the module. The samples for analyzing the outer surface of the hollow fiber membrane were cut at 1 cm intervals in a cross section perpendicular to the longitudinal direction, and the samples for analyzing the inner surface were cut in the longitudinal direction. In the examples, the material constituting the hollow fiber membrane was polyvinylidene fluoride resin (PVDF), and an acrylate polymer having a perfluoroalkyl group in the side chain was used as the hydrophobic polymer. -1 ν(C=O) and 1,180cm -1 The peak intensity ratio of (ν(CF) + ν(CO)) near the surface, ν(C=O) / (ν(CF) + ν(CO)), was calculated and used as an index of the amount of hydrophobic polymer attached. This peak intensity ratio was measured for each site of the hollow fiber membrane, and when the minimum value was taken as 1.0, sites showing a value of 1.2 or more were judged to have a large amount of hydrophobic polymer attached.

[0053] (2)TOF-SIMS analysis The amount of hydrophobic polymer attached to the hollow fiber membrane for membrane distillation was compared by observing the cross section of the hollow fiber membrane by TOF-SIMS in addition to the above-mentioned IR and ATR methods. As the observation sample, a hollow fiber membrane sliced ​​into thin pieces was used. The equipment used was a nano-TOF manufactured by ULVAC-PHI, Inc., and the primary ions were Bi3 ++The conditions were: acceleration voltage 30 kV, current 0.1 nA (DC), analysis area 350 μm × 350 μm, integration time 120 min, detection ions negative ions, and neutralization was performed with an electron gun. Mapping was performed for the hollow fiber membrane constituent material and the hydrophobic polymer by m / z with characteristically strong intensity, and the abundance ratio of the hydrophobic polymer in each part was determined by comparing the obtained intensity ratios. In the TOF-SIMS under the above conditions, an accumulation time of 30 minutes is sufficient, but in this example, the analysis was performed with an accumulation time of 120 minutes. In the examples, the hollow fiber membrane was made of polyvinylidene fluoride (PVDF) resin, and the hydrophobic polymer was an acrylate polymer having a perfluoroalkyl group in the side chain. Therefore, the intensity ratio of PVDF at m / z=67, where the intensity is particularly strong, and perfluorinated acrylate polymer at m / z=293, where the intensity is particularly strong, were calculated. Here, when the intensity ratio is 2.0 times or more, it can be determined that there is a significant difference in the abundance rate of the hydrophobic polymer.

[0054] Example 1 (1) Preparation of membrane distillation modules and measurement of the physical properties of membrane distillation membranes In Example 1, a hollow fiber porous membrane was used as the membrane distillation membrane (20), and the raw material liquid (a) was concentrated by membrane distillation without a hydrophobic polymer attached thereto. This membrane distillation membrane (20) was packed in a membrane distillation membrane module (100) having the configuration shown in FIG. 1 and used. As the membrane for membrane distillation (20), a porous hollow fiber membrane made of PVDF having an inner diameter of 0.7 mm, an outer diameter of 1.3 mm, an average pore size of 0.21 μm and a maximum pore size of 0.29 μm as determined in accordance with ASTM-F316-86, and a porosity of 72%, was cut into a length of 15 cm and used. The water contact angle of this porous hollow fiber membrane was measured by the above-mentioned method and was found to be 92°. A plurality of the above-mentioned membrane distillation membranes (20) were bundled together to form a membrane bundle, which was then housed in a housing (10). The membrane bundle of the membrane distillation membranes (20) was then adhered and fixed in the housing (10) by centrifugal adhesion using a thermosetting epoxy resin as the adhesive resin (30). By the above operations, the effective length (the length of the part not buried in the adhesive resin (30)) was 10 cm, and the total membrane area of ​​the inner surface of the membrane for membrane distillation (20) was 200 cm. 2 Two membrane distillation membrane modules (100) containing the hollow fiber membrane distillation membrane bundles were produced. One of the obtained membrane distillation modules was disassembled and used to measure the physical properties of the hollow fiber membrane. The measurement results are shown in Table 1. The remaining membrane module for membrane distillation was used for concentrating the raw material liquid (a).

[0055] (2) Implementation of membrane distillation Using the membrane module for membrane distillation (100) prepared above, a membrane distillation apparatus having the configuration shown in FIG. 2 was prepared, and membrane distillation was performed. As a simulant liquid of raw material liquid (a) containing pharmaceutical substances, etc., a solution having the following composition was used. Solvent (b): A mixed solvent of water and acetonitrile. The mixing ratio of water and acetonitrile was varied, and the concentration operation was carried out at each ratio. Solutes: Dipeptide 1,000 ppm, and NaCl 1,000 ppm Liquid volume: 0.5L NaCl was added to the feed solution a as a means of checking if the membrane for membrane distillation was wetting. The raw material liquid a was filled into the raw material liquid storage tank (200). The raw material liquid a was circulated at a flow rate of 600 ml / min by using a pump so as to pass through the inside of the hollow fiber membrane of the membrane distillation membrane module (100). At this time, the temperature of the drug raw material liquid a was adjusted by using a temperature controller (TC) so as to be maintained at 30° C. at the inlet side of the membrane distillation membrane module (100).

[0056] On the other hand, a cooling water storage tank (300) was provided to hold about 2 L of cooling water (CW), and the cooling water was pumped at a flow rate of 600 ml / min to the outside of the hollow fiber membrane of the membrane module for membrane distillation (100). At this time, the temperature of the cooling water (CW) was adjusted using a temperature controller (TC) so that it was maintained at 10°C. In addition, the conductivity of the cooling water (CW) leaving the membrane module for membrane distillation (100) was constantly measured. If the conductivity of the cooling water (CW) rose to 500 μS / cm or more, it was considered that NaCl added to the raw material liquid (a) had been mixed into the cooling water (CW). Therefore, in this case, it was determined that the membrane for membrane distillation had been wetted.

[0057] When the volume of the raw liquid (a) measured from the level gauge (LG) installed in the raw liquid storage tank (200) reached 100 ml, it was determined that the concentration rate had reached 5 times, and the concentration was terminated. In Example 1, the raw material liquid (a) containing water and acetonitrile at a mixing ratio of 95:5 (volume ratio) was concentrated 5 times in 39 hours. The conductivity of the cooling water (CW) was always 5 μS / cm or less, and no wetting of the membrane for membrane distillation occurred. However, when the mixture ratio of water and acetonitrile was 90:10 (volume ratio), the conductivity of the cooling water (CW) exceeded 500 μS / cm within 8 hours of operation, the membrane distillation membrane became wet, and wetting of the membrane occurred.

[0058] Example 2 (1) Preparation of membrane distillation modules and measurement of the physical properties of membrane distillation membranes In Example 2, the raw material liquid (a) was concentrated by membrane distillation in a state where a hydrophobic polymer was attached to the hollow fiber porous membrane used in Example 1. The hydrophobic polymer used was a fluororesin-based water repellent "DP02H" manufactured by AGC Seimi Chemical Co., Ltd. This "DP02H" is a solution containing an acrylate polymer having a perfluoroalkyl group in the side chain. Two membrane modules were produced by the same manufacturing method as in Example 1. These modules were completely immersed once in "DP02H" manufactured by AGC Seimi Chemical Co., Ltd., and then pulled out, and then dried by flowing dry air at a flow rate of 20 L / min on the inside and outside of the hollow fiber membrane to adhere the hydrophobic polymer to the hollow fiber membrane, thereby obtaining a membrane module for membrane distillation (100). Of the two obtained membrane distillation modules (100), one was disassembled and subjected to measurements of the physical properties of the hollow fiber membrane (IR, ATR, and TOF-SIMS analysis). Each physical property was measured using the central part in the longitudinal direction of the hollow fiber membrane. The water contact angle of the porous hollow fiber membrane after the hydrophobic polymer was attached was measured by the above-mentioned method and was found to be 120°. The measurement results are shown in Table 1. The remaining membrane module for membrane distillation was used for concentrating the raw material liquid (a).

[0059] (2) Implementation of membrane distillation A membrane distillation apparatus having the configuration shown in FIG. 2 was prepared in the same manner as in Example 1, except that the membrane module for membrane distillation (100) prepared above was used, and membrane distillation was performed. When the membrane module of Example 2 was used, the raw material liquid (a) with a mixture ratio of water and acetonitrile of 95:5 (volume ratio) was concentrated 5 times in 39 hours. The conductivity of the cooling water (CW) was always 5 μS / cm or less, and wetting of the membrane distillation membrane did not occur. Furthermore, the raw material liquid (a) with a mixture ratio of water and acetonitrile of 90:10 (volume ratio) was concentrated 5 times in 32 hours. However, when the mixture ratio of water and acetonitrile was 50:50 (volume ratio), the conductivity of the cooling water (CW) exceeded 500 μS / cm within 3 hours of operation, the membrane for membrane distillation became wet, and membrane wetting occurred.

[0060] Example 3 (1) Preparation of membrane distillation modules and measurement of the physical properties of membrane distillation membranes In Example 3, a hollow fiber-shaped porous membrane to which a hydrophobic polymer was attached was used as the membrane distillation membrane (20). The hollow fiber porous membrane used was a PVDF porous hollow fiber membrane with an inner diameter of 0.7 mm, an outer diameter of 1.3 mm, an average pore size of 0.05 μm and a maximum pore size of 0.12 μm as determined in accordance with ASTM-F316-86, and a porosity of 70%, cut into a length of 15 cm. The hydrophobic polymer used was a fluororesin-based water repellent agent "DP02H" manufactured by AGC Seimi Chemical Co., Ltd. Using the above hollow fiber porous membrane, two membrane modules were produced by the same manufacturing method as in Example 1. Using these modules, the modules were immersed in "DP02H" manufactured by AGC Seimi Chemical Co., Ltd., pulled out, and dried by the same method as in Example 2 to attach a hydrophobic polymer to the hollow fiber membrane, thereby obtaining a membrane module (100) for membrane distillation. Of the two obtained membrane distillation modules (100), one was disassembled and subjected to measurements of the physical properties of the hollow fiber membrane (IR, ATR, and TOF-SIMS analysis). Each physical property was measured using the central part in the longitudinal direction of the hollow fiber membrane. The water contact angle of the porous hollow fiber membrane after the hydrophobic polymer was attached was measured by the above-mentioned method and was found to be 120°. The measurement results are shown in Table 1. The remaining membrane module for membrane distillation was used for concentrating the raw material liquid (a).

[0061] (2) Implementation of membrane distillation A membrane distillation apparatus having the configuration shown in FIG. 2 was prepared in the same manner as in Example 1, except that the membrane module for membrane distillation (100) prepared above was used, and membrane distillation was performed. When the membrane module of Example 3 was used, the raw material liquid (a) with a mixing ratio of water and acetonitrile of 95:5 (volume ratio) was concentrated 5 times in 48 hours. The raw material liquid (a) with a mixing ratio of water and acetonitrile of 90:10 (volume ratio) was also concentrated 5 times in 41 hours. Furthermore, when the mixing ratio of water and acetonitrile was 50:50 (volume ratio), it was concentrated 5 times in 36 hours. In addition, the conductivity of the cooling water (CW) was always 5 μS / cm or less in all concentrations, and wetting of the membrane for membrane distillation did not occur.

[0062] Example 4 (1) Preparation of membrane distillation modules and measurement of the physical properties of membrane distillation membranes In Example 4, a hollow fiber porous membrane to which a hydrophobic polymer was attached was used as the membrane distillation membrane (20). The hollow fiber porous membrane used was a PVDF porous hollow fiber membrane with an inner diameter of 0.7 mm, an outer diameter of 1.3 mm, an average pore size of 0.45 μm determined in accordance with ASTM-F316-86, a maximum pore size of 0.80 μm, and a porosity of 71%, cut into a length of 15 cm. The hydrophobic polymer used was a fluororesin-based water repellent agent "DP02H" manufactured by AGC Seimi Chemical Co., Ltd. Using the above hollow fiber porous membrane, two membrane modules were produced by the same manufacturing method as in Example 1. Using these modules, the modules were immersed in "DP02H" manufactured by AGC Seimi Chemical Co., Ltd., pulled out, and dried by the same method as in Example 2 to attach a hydrophobic polymer to the hollow fiber membrane, thereby obtaining a membrane module (100) for membrane distillation. Of the two obtained membrane distillation modules (100), one was disassembled and subjected to measurements of the physical properties of the hollow fiber membrane (IR, ATR, and TOF-SIMS analysis). Each physical property was measured using the central part in the longitudinal direction of the hollow fiber membrane. The water contact angle of the porous hollow fiber membrane after the hydrophobic polymer was attached was measured by the above-mentioned method and was found to be 120°. The measurement results are shown in Table 1. The remaining membrane module for membrane distillation was used for concentrating the raw material liquid (a).

[0063] (2) Implementation of membrane distillation A membrane distillation apparatus having the configuration shown in FIG. 2 was prepared in the same manner as in Example 1, except that the membrane module for membrane distillation (100) prepared above was used, and membrane distillation was performed. When the membrane module of Example 2 was used, the raw liquid (a) with a mixture ratio of water and acetonitrile of 95:5 (volume ratio) was concentrated 5 times in 24 hours. Also, the raw liquid (a) with a mixture ratio of water and acetonitrile of 90:10 (volume ratio) was concentrated 5 times in 18 hours. In these cases, the conductivity of the cooling water (CW) was always 5 μS / cm or less, and wetting of the membrane distillation membrane did not occur. However, when the mixture ratio of water and acetonitrile was 50:50 (volume ratio), the conductivity of the cooling water (CW) exceeded 500 μS / cm within 2 hours of operation, the membrane distillation membrane became wet, and membrane wetting occurred.

[0064] Example 5 (1) Preparation of membrane distillation modules and measurement of the physical properties of membrane distillation membranes In Example 3, the raw material liquid (a) was concentrated by membrane distillation in a state in which a hydrophobic polymer was attached to the hollow fiber porous membrane used in Example 1 by a method different from that used in Example 2. As the hydrophobic polymer, Fluorocarbon resin water repellent "FS-392B" (polymer concentration 0.15 mass%) manufactured by Fluorotechnology Co., Ltd. was used, and the concentrate in which the polymer concentration was increased to 0.5 mass% by removing the low boiling point solvent was subjected to the hydrophobic polymer attachment operation. Two membrane modules were produced by the same method as in Example 1. These membrane modules were completely immersed once in Fluorotechnology's "FS-392B" concentrate, and then pulled out, and dried by flowing dry air at a flow rate of 200 ml / min only on the inside of the hollow fiber membrane. This immersion and completion operation was repeated a total of two times to attach the hydrophobic polymer to the hollow fiber membrane, thereby obtaining a membrane module (100) for membrane distillation. Of the two membrane distillation modules obtained, one was disassembled and used to measure the physical properties of the hollow fiber membrane. The water contact angle of the porous hollow fiber membrane after the hydrophobic polymer was attached was measured by the above-mentioned method and was found to be 130°. The measurement results are shown in Table 1. The remaining membrane module for membrane distillation was used for concentrating the raw material liquid (a).

[0065] (2) Implementation of membrane distillation A membrane distillation apparatus having the configuration shown in FIG. 2 was prepared in the same manner as in Example 1, except that the membrane module for membrane distillation (100) prepared above was used, and membrane distillation was performed. When the membrane module of Example 3 was used, the raw material liquid (a) with a mixture ratio of water and acetonitrile of 95:5 (volume ratio) was concentrated 5 times in 41 hours. In addition, the conductivity of the cooling water (CW) was always 5 μS / cm or less, and wetting of the membrane for membrane distillation did not occur. Even with the raw material liquid (a) in which the mixture ratio of water and acetonitrile was 90:10 (volume ratio), it was possible to concentrate it 5 times in 33 hours. Even with the mixture ratio of water and acetonitrile being 50:50 (volume ratio), it was possible to concentrate it 5 times in 24 hours, and the conductivity of the generated water was always 5 μS / cm or less. Furthermore, when the raw material liquid (a) was concentrated using a mixed solvent containing water and isopropanol in a volume ratio of 50:50 as the solvent (b), it was possible to concentrate it five-fold in 20 hours, and the conductivity of the cooling water (CW) was always below 5 μS / cm.

[0066] Example 6 A membrane module prepared in the same manner as in Example 5 was immersed in ethanol for 5 minutes. Then, the outside of the hollow fiber membrane in the membrane module was washed with running water for 10 minutes. By this operation, the inside of the hollow fiber membrane was not wetted with ethanol, but only the outside was wetted and became hydrophilic. A membrane distillation apparatus having the configuration shown in FIG. 2 was prepared in the same manner as in Example 1, except that the membrane module in this state was used, and the raw material liquid (a) was concentrated using a mixed solvent containing water and isopropanol in a volume ratio of 50:50. As a result, the time required to concentrate the raw material solution (a) by 5 times was shortened to 14 hours. In addition, the electrical conductivity of the cooling water (CW) was always below 5μS / cm. It is believed that by making part of the hollow fiber membrane hydrophilic, part of the membrane for membrane distillation contains water, reducing the effective thickness of the membrane, and shortening the distance that the solvent (b), which becomes vapor during membrane distillation, travels in the thickness direction of the membrane.

[0067] Comparative Example 1 In Comparative Example 1, a polyacrylonitrile hollow fiber membrane having an inner diameter of 0.7 mm, an outer diameter of 1.2 mm, an average pore size of 0.01 μm, a maximum pore size of 0.03 μm, and a porosity of 68%, cut into a length of 15 cm, was used as the membrane distillation membrane (20). The water contact angle of this porous hollow fiber membrane was measured by the above-mentioned method and was found to be 84°. Two membrane modules (100) for membrane distillation were produced in the same manner as in Example 1, except that the above-mentioned porous hollow fiber membrane was used. One of the obtained membrane distillation modules was disassembled and used to measure the physical properties of the hollow fiber membrane. The measurement results are shown in Table 1. The remaining membrane module for membrane distillation was used for concentrating the raw material liquid (a). A membrane distillation apparatus having the configuration shown in FIG. 2 was produced in the same manner as in Example 1, except that the obtained membrane module for membrane distillation (100) was used, and membrane distillation of a raw material liquid (a) using a mixed solvent containing water and acetonitrile in a volume ratio of 95:5 was performed. However, even after 50 hours of operation, the concentration did not reach five times the original concentration.

[0068] Comparative Example 2 A PVDF hollow fiber membrane with an inner diameter of 0.7 mm, an outer diameter of 1.3 mm, an average pore size of 0.12 μm, a maximum pore size of 0.60 μm, and a porosity of 69%, cut into a length of 15 cm, was used as the membrane distillation membrane (20). The water contact angle of this porous hollow fiber membrane was measured by the above-mentioned method and was found to be 92°. Two membrane modules (100) for membrane distillation were produced in the same manner as in Example 1, except that the above-mentioned porous hollow fiber membrane was used. One of the obtained membrane distillation modules was disassembled and used to measure the physical properties of the hollow fiber membrane. The measurement results are shown in Table 1. The remaining membrane module for membrane distillation was used for concentrating the raw material liquid (a). A membrane distillation apparatus having the configuration shown in FIG. 2 was prepared in the same manner as in Example 1, except that the above-mentioned membrane module for membrane distillation (100) was used, and membrane distillation of a raw material liquid (a) using a mixed solvent containing water and acetonitrile in a volume ratio of 95:5 was performed. However, after 13 hours of operation, the conductivity of the cooling water (CW) exceeded 500 μS / cm, causing membrane wetting and making it impossible to concentrate any further.

[0069] [Table 1]

[0070] [Table 2]

[0071] The abbreviations in Table 1 have the following meanings: <Hollow fiber membrane constituent materials> PVDF: Polyvinylidene fluoride PAN: Polyacrylonitrile <Hydrophobic polymer> DP02H: AGC Seimi Chemical Co., Ltd., fluororesin-based water repellent "DP02H" FS-392B: Fluoropolymer water repellent "FS-392B" manufactured by Fluoro Technology Co., Ltd. <Solvent (b)> AcCN: Acrylonitrile IPA: Isopropanol [Explanation of symbols]

[0072] 10. Housing 11 First housing side tube 12 Second housing side tube 20 Membrane for membrane distillation 30 Adhesive resin 100 Membrane distillation membrane module 200 Raw material liquid storage tank 300 Cooling Water Storage Tank a Raw material liquid b. Solvent c Concentrate CW cooling water FM flow meter LG liquid level gauge P-Pump PG Pressure Gauge TC temperature controller

Claims

1. A raw material liquid concentration system using a membrane distillation method in which a raw material liquid containing a solvent and a solute is contacted with cooling water via a membrane distillation membrane, and the solvent in the raw material liquid is passed through the membrane distillation membrane in a vapor state and transferred to the cooling water side, the solvent is selected from a mixture of water and one or more selected from acetonitrile, methanol, ethanol, and isopropanol; The membrane for membrane distillation is The water contact angle of the surface is 90° or more, The average pore size is in the range of 0.02 μm or more and 0.5 μm or less, and The porosity is 60% or more and 90% or less.

1. A porous membrane comprising: A hydrophobic polymer selected from a polymer having a siloxane bond and a fluorine atom-containing polymer is attached to at least a portion of the membrane for membrane distillation, The amount of the hydrophobic polymer attached has a distribution in the thickness direction of the membrane distillation membrane, and the amount of the hydrophobic polymer attached on the surface layer of at least one side of the membrane distillation membrane is greater than the amount of the hydrophobic polymer attached inside the membrane, When the membrane distillation membrane was subjected to TOF-SIMS analysis, The ratio of the m / z intensity derived from the hydrophobic polymer to the m / z intensity derived from the material of the membrane distillation membrane at the center of the thickness direction of the membrane distillation membrane, A ratio of an intensity ratio between an m / z intensity derived from the hydrophobic polymer and an m / z intensity derived from the material of the membrane distillation membrane in a surface layer of at least one side of the membrane distillation membrane. is 2.0 times or more, A raw material liquid concentration system for pharmaceutical manufacturing processes.

2. A raw material liquid concentration system using a membrane distillation method in which a raw material liquid containing a solvent and a solute is contacted with cooling water via a membrane distillation membrane, and the solvent in the raw material liquid is passed through the membrane distillation membrane in a vapor state and transferred to the cooling water side, The solvent is selected from a mixture of water and one or more selected from acetonitrile, methanol, ethanol, and isopropanol, provided that when the solvent is a mixture of water and acetonitrile, the proportion of acetonitrile in the solvent is 10% by volume or less; The membrane for membrane distillation is The water contact angle of the surface is 90° or more, The average pore size is in the range of 0.02 μm or more and 0.5 μm or less, and The porosity is 60% or more and 90% or less.

1. A porous membrane comprising: A hydrophobic polymer selected from a polymer having a siloxane bond and a fluorine atom-containing polymer is attached to at least a portion of the membrane for membrane distillation, The amount of the hydrophobic polymer attached has a distribution in the thickness direction of the membrane distillation membrane, and the amount of the hydrophobic polymer attached on the surface layer of at least one side of the membrane distillation membrane is greater than the amount of the hydrophobic polymer attached inside the membrane distillation membrane. A raw material liquid concentration system for pharmaceutical manufacturing processes.

3. When the IR spectrum analysis of the membrane distillation membrane was performed by the ATR method, The peak intensity ratio of the peak intensity originating from the hydrophobic polymer on one side of the membrane distillation membrane to the peak intensity originating from the material of the membrane distillation membrane, A ratio of a peak intensity ratio between a peak intensity attributable to the hydrophobic polymer on the opposite surface of the membrane distillation membrane and a peak intensity attributable to the material of the membrane distillation membrane. is less than 1.2 times; The raw material liquid concentrating system according to claim 2 .

4. The raw material liquid concentrating system according to any one of claims 1 to 3, wherein the solvent is selected from the group consisting of a mixture of water and acetonitrile and a mixture of water and isopropanol.

5. The raw material liquid concentrating system according to any one of claims 1 to 4, wherein the amount of the hydrophobic polymer attached decreases from a surface layer on one side of the membrane distillation membrane to a surface layer on the opposite side.

6. the opposite surface having a smaller amount of the hydrophobic polymer attached thereto is subjected to a hydrophilic treatment, the hydrophilic treated surface is brought into contact with cooling water, and the side having a large amount of hydrophobic polymer attached thereto is not subjected to hydrophilization treatment, and the side is brought into contact with the raw material liquid; The raw material liquid concentrating system according to claim 5 .

7. The raw material liquid concentrating system according to any one of claims 1 to 6, wherein the hydrophobic polymer is a polymer having a fluorine atom-containing group in a side chain, and has at least one side chain selected from a (per)fluoroalkyl group, a (per)fluoropolyether group, an alkylsilyl group, and a fluorosilyl group.

8. The raw material liquid concentrating system according to any one of claims 1 to 7, wherein the solute is at least one selected from the group consisting of amino acids, peptides, proteins, sugars, vaccines, nucleic acids, antibiotics, antibody-drug conjugates (ADCs), and vitamins.

9. The raw material liquid concentrating system according to any one of claims 1 to 8, wherein the solute has a number average molecular weight of 100 to 50,000.

10. The raw material liquid concentrating system according to any one of claims 1 to 9, wherein the temperature of the raw material liquid is adjusted to a range of 5°C or higher and 50°C or lower.

11. A concentrating apparatus for concentrating a raw material liquid by a membrane distillation method, comprising: The raw material liquid contains a solvent and a solute, the solvent is selected from a mixture of water and one or more selected from acetonitrile, methanol, ethanol, and isopropanol; The membrane for membrane distillation is The water contact angle of the film surface is 90° or more, The average pore size is in the range of 0.02 μm or more and 0.5 μm or less, and The porosity is 60-90% 1. A porous membrane comprising: A hydrophobic polymer selected from a polymer having a siloxane bond and a fluorine atom-containing polymer is attached to at least a portion of the membrane for membrane distillation, The amount of the hydrophobic polymer attached has a distribution in the thickness direction of the membrane distillation membrane, and the amount of the hydrophobic polymer attached on the surface layer of at least one side of the membrane distillation membrane is greater than the amount of the hydrophobic polymer attached inside the membrane, When the membrane distillation membrane was subjected to TOF-SIMS analysis, The ratio of the m / z intensity derived from the hydrophobic polymer to the m / z intensity derived from the material of the membrane distillation membrane at the center of the thickness direction of the membrane distillation membrane, A ratio of an intensity ratio between an m / z intensity derived from the hydrophobic polymer and an m / z intensity derived from the material of the membrane distillation membrane in a surface layer of at least one side of the membrane distillation membrane. is 2.0 times or more, Concentrator.

12. A concentrating apparatus for concentrating a raw material liquid by a membrane distillation method, comprising: The raw material liquid contains a solvent and a solute, The solvent is selected from a mixture of water and one or more selected from acetonitrile, methanol, ethanol, and isopropanol, provided that when the solvent is a mixture of water and acetonitrile, the proportion of acetonitrile in the solvent is 10% by volume or less; The membrane for membrane distillation is The water contact angle of the film surface is 90° or more, The average pore size is in the range of 0.02 μm or more and 0.5 μm or less, and The porosity is 60-90% 1. A porous membrane comprising: A hydrophobic polymer selected from a polymer having a siloxane bond and a fluorine atom-containing polymer is attached to at least a portion of the membrane for membrane distillation, The amount of the hydrophobic polymer attached has a distribution in the thickness direction of the membrane distillation membrane, and the amount of the hydrophobic polymer attached on the surface layer of at least one side of the membrane distillation membrane is greater than the amount of the hydrophobic polymer attached inside the membrane, When the IR spectrum analysis of the membrane distillation membrane was performed by the ATR method, The peak intensity ratio of the peak intensity originating from the hydrophobic polymer on one side of the membrane distillation membrane to the peak intensity originating from the material of the membrane distillation membrane, A ratio of a peak intensity ratio between a peak intensity attributable to the hydrophobic polymer on the opposite surface of the membrane distillation membrane and a peak intensity attributable to the material of the membrane distillation membrane. is less than 1.2 times; Concentrator.

Citation Information

Patent Citations

  • Production of powdery seasoning

    JP1999075759A

  • Porous membrane for membrane distillation, module for membrane distillation, and membrane distillation type water production system

    JP2011200770A

  • Amphiphilic block copolymers; compositions, membranes, and separation modules thereof; and methods of making the same

    JP2017514956A

  • Composite membrane with support comprising poly(phenylene ether) and amphiphilic polymer, method of manufacture, and separation module thereof

    JP2017514957A

  • Porous asymmetric polyphenylene ether membranes and related separation modules and methods

    JP2017515662A