Sclerotic composition
The curable composition with isocyanate and active hydrogen compounds, combined with solid, hollow, and scaly particles, addresses stringiness and sagging issues, enhancing workability and film properties.
Patent Information
- Application Number
- JP2020165478
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-09-30
- Publication Date
- 2024-09-26
- Estimated Expiration
- 2040-09-30
AI Technical Summary
Two-component curable compositions with inorganic fillers face issues such as stringiness during application, which impede workability, particularly in rising parts of buildings.
A curable composition comprising a first liquid with an isocyanate group-containing compound and a second liquid with an active hydrogen-containing compound, incorporating specific fillers like solid, hollow, and scaly particles to enhance workability and film properties.
The composition improves workability by reducing stringiness and sagging, while maintaining excellent coating film properties, including strength and elongation.
Smart Images

Figure 0007556734000001
Abstract
Description
[Technical field]
[0001] The present invention relates to novel curable compositions. [Background technology]
[0002] Conventionally, as a two-liquid type curable composition, one consisting of a first liquid having an isocyanate group-containing compound and a second liquid having an active hydrogen-containing compound is known. Such a curable composition can exhibit excellent physical properties such as strength, extensibility, and durability, and is therefore applied to, for example, surface coating materials for buildings, civil engineering structures, and the like. In particular, it is preferably used as a coating waterproofing material that enhances waterproofing on the rooftops and verandas of buildings. Such coating waterproofing materials are generally often applied with trowels, spatulas, rollers, brushes, and the like, and good workability is required. In particular, in the rising parts of buildings, etc., it is necessary to ensure the hardness, strength, elongation, etc. of the coating film in addition to workability.
[0003] To address such problems, for example, Patent Document 1 (JP Patent Publication 2008-222792 A) discloses a urethane resin composition obtained by mixing a first component containing a specific urethane prepolymer obtained by reacting polyisocyanate with N-hydroxyalkyloxazolidine with a second component containing water, and describes that sufficient coating hardness, strength, elongation, etc. can be ensured. It also describes that the incorporation of an inorganic filler provides viscosity, making it applicable to rising portions. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2008-222792 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, when the inorganic filler is blended to provide viscosity while maintaining the coating film properties, problems such as stringiness may occur during application, impeding workability.
[0006] The present invention has been made in consideration of such problems, and an object of the present invention is to provide a curable composition comprising a first liquid containing an isocyanate group-containing compound and a second liquid containing an active hydrogen-containing compound, which has excellent workability and sufficient coating film properties. [Means for solving the problem]
[0007] Means for Solving the Problems The present inventors conducted intensive research to solve the above problems, and came up with the idea of including a specific filler in a curable composition consisting of a first liquid having an isocyanate group-containing compound and a second liquid having an active hydrogen-containing compound, thereby completing the present invention.
[0008] That is, the present invention has the following features. 1. A curable composition comprising a first liquid having an isocyanate group-containing compound and a second liquid having an active hydrogen-containing compound, The first liquid and / or the second liquid contain a filler, The filler includes solid particles, hollow particles, and scaly particles. fruit, the solid particles are one or more selected from heavy calcium carbonate, light calcium carbonate, calcium oxide, magnesium carbonate, barium sulfate, magnesium sulfate, diatomaceous earth, zeolite, silica gel, and resin particles; The solid particles include precipitated calcium carbonate, The scaly particles are one or more selected from muscovite, biotite, phlogopite, synthetic mica, talc, hydrous kaolin clay, and calcined kaolin clay. A curable composition comprising: 2. The curable composition according to 1, wherein the filler contains 3% by weight or more and 50% by weight or less of scale-like particles. 3. The curable composition according to 1 or 2, wherein the filler contains hollow particles in an amount of 0.01% by weight or more and 10% by weight or less. 4. The curable composition according to any one of 1. to 3., wherein the hollow particles have a median diameter of 10 to 80 μm. Effect of the Invention
[0009] In a curable composition consisting of a first liquid having an isocyanate group-containing compound and a second liquid having an active hydrogen-containing compound, by blending a specific filler into the first liquid and / or the second liquid, excellent workability and excellent coating film properties can be obtained. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, an embodiment of the present invention will be described.
[0011] The curable composition of the present invention comprises a first liquid having an isocyanate group-containing compound and a second liquid having an active hydrogen-containing compound. When distributed, the first liquid and the second liquid of such a curable composition are packaged separately, and are mixed together when used (applied).
[0012] (1st liquid) The isocyanate group-containing compound in the first liquid is a compound that is reactive with the active hydrogen-containing compound in the second liquid. As the isocyanate group-containing compound, a compound having two or more isocyanate groups in one molecule can be used. Specifically, for example, 4,4-diphenylmethane diisocyanate (pure-MDI), polymeric MDI, xylylene diisocyanate (XDI), tolylene diisocyanate (TDI), hexamethylene diisocyanate (HMDI), isophorone diisocyanate (IPDI), hydrogenated XDI, hydrogenated MDI, etc., or derivatives thereof by allophanation, biuretization, dimerization (uretidione formation), trimerization (isocyanurate formation), adductization, carbodiimide formation, etc. can be mentioned. In addition, isocyanate group-terminated prepolymers obtained by the reaction of isocyanate with polyol can also be used. As the isocyanate group-containing compound, one or more of these can be used. Among these, the present invention is suitable for the first liquid containing at least an isocyanate group-terminated prepolymer. The isocyanate group content (NCO group content) in the isocyanate group-terminated urethane prepolymer is preferably 1 to 10% by weight (more preferably 2 to 5% by weight).
[0013] (2nd liquid) Examples of the active hydrogen-containing compound in the second liquid include hydroxyl group-containing compounds and amino group-containing compounds. Of these, various polyols can be used as the hydroxyl group-containing compound. Examples of polyols include polyester polyols, polyether polyols, polycarbonate polyols, polycaprolactone polyester polyols, polybutadiene polyols, castor oil polyols, low molecular weight diols, trimethylolpropane, glycerin, sorbitol, mannitol, and dulcitol. These can be used alone or in combination of two or more.
[0014] Examples of the amino group-containing compound include compounds having two or more primary or secondary amino groups in one molecule. Examples of such amino group-containing compounds include aliphatic polyamines, alicyclic polyamines, aromatic polyamines, heterocyclic amines, aliphatic polyamidoamines, alicyclic polyamidoamines, aromatic polyamidoamines, etc. These can be used alone or in combination. Of these, the present invention is suitable for the second liquid containing at least an aromatic polyamine. Examples of aromatic polyamines include diethyltoluenediamine, 4,4'-methylene-bis(2-alkylaniline), 4,4'-methylene-bis(2,6-dialkylaniline), 1,3,5-alkyl-2,4-diaminobenzene, methylthiotoluenediamine, tetraalkyldiaminodiphenylmethane, t-butyltoluenediamine, etc.
[0015] The amount of the active hydrogen-containing compound is preferably within a range such that the equivalent ratio (NCO equivalents / active hydrogen equivalents) between the isocyanate groups in the first liquid and the active hydrogens (hydroxyl groups, amino groups, etc.) in the second liquid is 0.5 to 3 (more preferably 1.1 to 2.5).
[0016] (Filler) The present invention is characterized in that the first liquid and / or the second liquid contains a filler. The curable composition may be embodied in such a manner that both the first liquid and the second liquid contain a filler, or in such a manner that either the first liquid or the second liquid contains a filler. In the present invention, a preferred embodiment is one in which at least the second liquid contains a filler. The present invention is characterized in that such a filler contains solid particles, hollow particles, and scaly particles. This provides excellent coating workability and sufficient coating film properties.
[0017] In the present invention, the strength of the coating film can be increased by including solid particles. Note that the solid particles in the present invention refer to particles that do not have a hollow portion, and are different from the hollow particles described below. In addition, the solid particles are recognized as having a granular shape, and are different from the scaly particles described below.
[0018] The average particle diameter of the solid particles is preferably 0.001 to 50 μm (more preferably 0.005 to 30 μm). When this range is satisfied, the above-mentioned effects can be sufficiently obtained. As such solid particles, either inorganic particles or organic particles can be used. As solid inorganic particles, for example, heavy calcium carbonate, light calcium carbonate (also called "synthetic or precipitated calcium carbonate"), calcium oxide, magnesium carbonate, barium sulfate, magnesium sulfate, diatomaceous earth, zeolite, silica gel, etc. can be mentioned, and as solid organic particles, various resin particles, etc. can be mentioned, and these can also be used with some surface treatment. In addition, these can be used alone or in combination of two or more kinds. In the present invention, the average particle diameter can be measured by a laser diffraction type particle size distribution measuring device, etc.
[0019] In the present invention, it is preferable to contain solid inorganic particles, and particularly preferable to contain light calcium carbonate, and it is particularly preferable to contain surface-treated light calcium carbonate that has been surface-treated with a resin acid (rosin acid) or an organic acid as the light calcium carbonate. The average particle size of the light calcium carbonate is preferably 0.001 to 0.5 μm (more preferably 0.005 to 0.3 μm). By containing such light calcium carbonate, it is possible to impart appropriate viscosity (thixotropy, etc.) to the cured composition, which has excellent coating workability and allows finishing without causing sagging during coating.
[0020] In the present invention, light calcium carbonate and heavy calcium carbonate can be used in combination. The average particle size of the heavy calcium carbonate is preferably 0.1 to 50 μm (more preferably 0.5 to 30 μm). The mixing ratio of the light calcium carbonate and the heavy calcium carbonate is preferably 100:0 to 10:90 (more preferably 80:20 to 20:80, and further preferably 70:30 to 30:70) by weight. When the ratio is within such a range, the dispersibility and mixability of the filler in the curable composition are excellent, and the above-mentioned effects can be further enhanced.
[0021] The content of the solid particles in the filler is preferably 50% by weight or more and 97% by weight or less (more preferably 55% by weight or more and 95% by weight or less, and even more preferably 60% by weight or more and 90% by weight or less). When this range is satisfied, the above-mentioned effects can be fully exhibited.
[0022] The filler of the present invention is characterized by the use of hollow particles and scaly particles in combination with the solid particles. By using hollow particles and scaly particles in combination, stringiness during application can be effectively suppressed, and the paint workability can be further improved. In addition, sufficient viscosity (high viscosity) can be obtained even after application (low shear rate region), so that even when applied to rising parts, it is possible to finish without sagging. Furthermore, the strength of the paint film can be further improved.
[0023] The hollow particles in the present invention refer to particles having a hollow portion, and are different from the solid particles and the scaly particles described below. The hollow particles of the present invention are preferably a mixture of particles of various sizes, and the median diameter of the particle size distribution is preferably 10 to 80 μm (more preferably 20 to 70 μm, and even more preferably 30 to 60 μm). When such a range is satisfied, the hollow particles larger than the median diameter and the hollow particles smaller than the median diameter can be contained in a well-balanced manner. This enhances the effect of suppressing stringiness during application, further improving the coating workability, and obtaining a uniform finish. In addition, the tensile strength, tear strength, elongation, etc. of the formed coating film can be improved. Here, the median diameter means a diameter at which the larger side and the smaller side are equal when the particles are divided into two from a certain particle diameter, and can be measured by a laser diffraction type particle size distribution measuring device or the like.
[0024] The hollow particles preferably have a minimum diameter of 1 μm or more (more preferably 2 μm or more, and even more preferably 3 μm or more) and a maximum diameter of 120 μm or less (more preferably 100 μm or less, and even more preferably 90 μm or less). Furthermore, the true density of the hollow particles is preferably 0.05 to 0.9 g / cm. 3 (More preferably 0.1 to 0.8 g / cm 3 When this range is satisfied, the above-mentioned effects can be further enhanced.
[0025] As such hollow particles, either inorganic particles or organic particles can be used. Examples of hollow inorganic particles include glass balloons, silase balloons, silica balloons, carbon balloons, alumina balloons, zirconia balloons, and ceramic balloons, while examples of hollow organic particles include various resin balloons, and these may also be used after some surface treatment. These may be used alone or in combination of two or more. In the present invention, it is preferable to include hollow inorganic particles, and among these, it is preferable to use glass balloons.
[0026] The content of the hollow particles in the filler is preferably 0.01% by weight to 10% by weight (more preferably 0.05% by weight to 5% by weight, and even more preferably 0.1% by weight to 3% by weight). When this range is satisfied, the above-mentioned effects can be fully exhibited.
[0027] The scaly particles in the present invention refer to particles having a scaly (also called thin or flake-like) shape, and are different from the solid particles and hollow particles. The average particle size of the scaly particles is preferably 0.001 to 10 μm (more preferably 0.005 μm to 5 μm). The aspect ratio (average particle size / average thickness) is preferably 1 to 100 (more preferably 2 to 80). When such a range is satisfied, the above-mentioned effects can be sufficiently obtained. The above-mentioned average particle size can be measured by a laser diffraction type particle size distribution measuring device or the like. The above-mentioned thickness can be measured by a microscope or the like.
[0028] As such scaly particles, both inorganic particles and organic particles can be used. Examples of scaly inorganic particles include scaly particles of metals and oxides, scaly minerals, and scaly glass. Specifically, examples of scaly particles of metals and oxides include metals such as aluminum, silver, gold, platinum, nickel, chromium, zinc, indium, titanium, and copper, alloys containing these metals, and oxides of these metals. Examples of scaly minerals include micas such as muscovite, black mica, phlogopite, and synthetic mica, aluminum silicates such as talc, hydrous kaolin clay, and calcined kaolin clay, and examples of scaly organic particles include various resin flakes, and these may also be surface-treated. These may be used alone or in combination.
[0029] In the present invention, it is preferable to contain scaly inorganic particles, and more preferably, micas such as muscovite, biotite, phlogopite, synthetic mica, talc, hydrous kaolin clay, calcined kaolin clay, etc., and particularly preferably, hydrous kaolin clay. The average particle size of the hydrous kaolin clay is preferably 0.01 to 5 μm (more preferably 0.05 to 3 μm, and even more preferably 0.05 to 1 μm). When such a range is satisfied, the above-mentioned effects can be further enhanced.
[0030] The content of the above-mentioned scale-like particles in the filler is preferably 3% by weight or more and 50% by weight or less (more preferably 5% by weight or more and 45% by weight or less, and even more preferably 8% by weight or more and 40% by weight or less). When such a range is satisfied, the above-mentioned effects can be sufficiently exhibited.
[0031] The amount of the filler to be blended is preferably 10 to 500 parts by weight (more preferably 30 to 400 parts by weight) per 100 parts by weight of the isocyanate group-containing compound (solid content) in Liquid 1. When the amount is within this range, the effects of the present invention can be sufficiently obtained.
[0032] The second liquid preferably further contains a plasticizer. This adjusts the viscosity of the curable composition, ensures stable workability, and also effectively acts in terms of coating film strength. Examples of plasticizers include phthalates such as dioctyl phthalate, diisononyl phthalate, dibutyl phthalate, and butyl benzyl phthalate; and aliphatic carboxylates such as dioctyl adipate, diisodecyl succinate, dibutyl sebacate, and butyl oleate. These can be used alone or in combination of two or more.
[0033] The blending amount of the plasticizer is preferably 10 to 200 parts by weight (more preferably 30 to 100 parts by weight) per 100 parts by weight of the isocyanate group-containing compound (solid content) in Liquid 1. When the blending amount is within such a range, the effects of the present invention can be sufficiently obtained.
[0034] In addition to the components described above, the first liquid and the second liquid may contain, for example, color pigments, aggregates, dispersants, defoamers, deterioration inhibitors, diluents, thickeners, wetting agents, antifreeze agents, film-forming aids, catalysts, preservatives, antifungal agents, anti-algae agents, antibacterial agents, ultraviolet absorbers, light stabilizers, antioxidants, etc.
[0035] (Curable composition) The curable composition of the present invention is obtained by mixing the first liquid and the second liquid, and the mixing ratio of the first liquid to the second liquid may be within a range in which the equivalent ratio (NCO equivalent number / active hydrogen equivalent number) between the isocyanate group in the first liquid and the active hydrogen (hydroxyl group, amino group, etc.) in the second liquid is preferably 0.5 to 3 (more preferably 1.1 to 2.5). Such a range is suitable in terms of strength, extensibility, durability, etc.
[0036] The specific mixing ratio (weight ratio) of the first liquid and the second liquid can be appropriately set depending on the composition of the first liquid and the second liquid, but is preferably 50 to 500 parts by weight (more preferably 100 to 300 parts by weight) of the second liquid per 100 parts by weight of the first component. Within such a range, the effects of the present invention can be sufficiently obtained. EXAMPLES
[0037] The following examples will clarify the features of the present invention.
[0038] The following raw materials were used: Isocyanate-terminated urethane prepolymer (NCO%: 3% by weight) Active hydrogen compounds 1 [aromatic polyamines (diethyltoluenediamine)] Active hydrogen compounds 2 [Polyol compounds (polyoxypropylene glycol)] Solid particle 1 [light calcium carbonate (surface treated with rosin resin), average particle size 0.1 μm] Solid particles 2 [heavy calcium carbonate, average particle size 2.5 μm] Hollow particle 1 [glass balloon, median diameter 45 μm (minimum diameter 3 μm, maximum diameter 85 μm), true density 0.37 g / cm3 ] Hollow particle 2 [glass balloon, median diameter 65 μm (minimum diameter 5 μm, maximum diameter 120 μm), true density 0.15 g / cm 3 ] ·Scaly particles [hydrous kaolin clay, average particle size 0.2μm] Pigment [Titanium dioxide] Plasticizer [Diisononyl phthalate]
[0039] (Examples 1 to 5, Comparative Examples 1 to 3) Curable compositions were prepared by mixing the first and second liquids at the mixing ratio shown in Table 1. The equivalent ratio of the isocyanate groups in the first liquid to the active hydrogen groups in the second liquid was NCO / active hydrogen = 1.5, and the mixing was performed at room temperature (23°C, 50% RH environment). Each curable composition was evaluated as follows. The results are shown in Table 1.
[0040] <Painting workability evaluation> A slate board (300 mm x 300 mm) coated with a waterproofing primer was placed vertically, and the curable composition was applied with a trowel in an amount of 2.6 kg / m. 2 The workability at this time was evaluated. Painting workability rating: 1 Dripping during painting was visually evaluated. The evaluation criteria were a four-level rating system, with "A" being no dripping and "D" being significant dripping (A>B>C>D: poor). Painting workability rating 2 The stringiness when the iron was removed during painting was visually evaluated. The evaluation criteria were a four-level rating system, with "A" being no stringiness and "D" being significant stringiness (A>B>C>D: poor).
[0041] <Paint film strength evaluation> The tensile strength and tear strength were measured according to the test method specified in JIS A6021:2011 "Architectural coating waterproof materials." Tensile strength The evaluation standard is 3.0N / mm 2 The above are marked with "◎" 2.3N / mm 2 More than 3.0N / mm2 Less than 2.3N / mm is marked as "○" 2 Anything less than this was marked as "X". Tear strength The evaluation criteria were as follows: 14.0 N / mm or more was marked "◯", and less than 14.0 N / mm was marked "X".
[0042] [Table 1]
Claims
1. A curable composition comprising a first liquid having an isocyanate group-containing compound and a second liquid having an active hydrogen-containing compound, wherein the first liquid and / or the second liquid contains a filler, and the filler contains solid particles, hollow particles, and scaly particles, the solid particles are one or more selected from heavy calcium carbonate, light calcium carbonate, calcium oxide, magnesium carbonate, barium sulfate, magnesium sulfate, diatomaceous earth, zeolite, silica gel, and resin particles; The solid particles include precipitated calcium carbonate, The curable composition, wherein the scaly particles are one or more selected from the group consisting of muscovite, biotite, phlogopite, synthetic mica, talc, hydrous kaolin clay, and calcined kaolin clay.
2. 2. The curable composition according to claim 1, wherein the filler contains 3% by weight or more and 50% by weight or less of scale-like particles.
3. 3. The curable composition according to claim 1, wherein the filler contains hollow particles in an amount of 0.01% by weight or more and 10% by weight or less.
4. 4. The curable composition according to claim 1, wherein the hollow particles have a median diameter of 10 to 80 μm.
Citation Information
Patent Citations
Two-pack type curable composition
JP2004182997A
Composition for buildings, and its method of application
JP2005016291A
Film forming method
JP2006095358A
Two-pack type room temperature-curing urethane coating waterproof material composition
JP2008184554A
Two-component urethane resin composition
JP2008222792A