Tear-off Label

The breakable label design with a conductor layer and fracture portions concentrates electron density to generate sparks, effectively increasing the total length of cuts in adhered films, ensuring reliable steam release during microwave processing.

JP7557412B2Active Publication Date: 2024-09-27FUJI SEAL INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021060665
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-31
Publication Date
2024-09-27
Estimated Expiration
2041-03-31

AI Technical Summary

Technical Problem

Existing breakable labels fail to effectively increase the total length of cuts in adhered films during microwave irradiation, limiting the reliable release of vapor generated within the film.

Method used

A breakable label design featuring a main body layer with a conductor layer having edges, constrictions, and fracture portions, where the fracture portions are spaced apart and extend linearly, concentrating electron density to generate sparks and increase the total length of cuts in the adhered film.

Benefits of technology

The design ensures that the adhered film is cut along the shape of the broken portion, enhancing steam evacuation performance by increasing the total length of cuts and maintaining integrity during microwave irradiation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007557412000004
    Figure 0007557412000004
  • Figure 0007557412000009
    Figure 0007557412000009
  • Figure 0007557412000008
    Figure 0007557412000008
Patent Text Reader

Abstract

To reliably make cuts by microwave irradiation on a coating film along the shape of a breaking part and make the total length where there are cuts longer.SOLUTION: A label 10 for fracture comprises a body layer 11 and an adhesive layer 12. The body layer 11 includes a base layer 100 and a conductor layer 110. The conductor layer 110 has a first edge part 111, a second edge part 112, multiple constricted parts 120, and multiple breaking parts 130. Each of the multiple constricted parts 120 is sandwiched between the first edge part 111 and the second edge part 112. In each of the multiple constricted parts 120, the distance between the first edge part 111 and second edge part 112 is narrow. At least one of the multiple breaking parts 130 is provided in each of at least some of the constricted parts 120 among the multiple constricted parts 120. Each of the multiple breaking parts 130 divides the constricted parts 120 that are provided with the breaking parts among the at least some of the constricted parts 120 in the length direction.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a breakable label. [Background technology]

[0002] A prior document disclosing the configuration of a microwave-tearable label is Japanese Patent No. 5621127 (Patent Document 1). The tearable label described in Patent Document 1 is attached to an adhesive film of a packaging body. The tearable label has a label base material on which a conductive layer is laminated, and an adhesive layer provided on the back surface of the label base material. The label base material has a substantially bow-tie shape in plan. A slit portion is formed by cutting the entire layer of the label in the thickness direction within the range where the adhesive layer is provided. The slit portion has a linear shape with ends in plan. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5621127 Summary of the Invention [Problem to be solved by the invention]

[0004] In the tearable label described in Patent Document 1, the applied film is reliably cut along the shape of the slit portion by microwave irradiation, while there is room for increasing the total length of the cut. By increasing the total length of the cut, steam generated in the applied film can be reliably released to the outside.

[0005] The present invention has been made to solve the above-mentioned problems, and aims to provide a tear-off label that can ensure that a cut is made in the attached film along the shape of the tear portion by microwave irradiation, while also lengthening the total length of the cut. [Means for solving the problem]

[0006] The breakable label according to the present invention is attached to an adhesive film of a package for microwave processing. The breakable label includes a main layer and an adhesive layer. The adhesive layer is laminated on one side of the main layer. The main layer includes a base layer and an electrical conductor layer laminated together in a lamination direction with the adhesive layer. The electrical conductor layer has a first edge, a second edge, a plurality of constricted portions, and a plurality of breakable portions. When viewed from the lamination direction, the first edge extends along a length direction perpendicular to the lamination direction. When viewed from the lamination direction, the second edge extends along the length direction while being spaced apart from the first edge in a width direction perpendicular to the length direction. Each of the plurality of constricted portions is sandwiched between the first edge and the second edge. In each of the plurality of constricted portions, the gap between the first edge and the second edge is narrow. Each of the plurality of breakable portions penetrates the electrical conductor layer in the lamination direction. At least one of the plurality of break portions is provided in each of at least a portion of the plurality of constricted portions. Each of the plurality of break portions divides the constricted portion in which it is provided, among the at least a portion of the constricted portions, in the longitudinal direction.

[0007] In one embodiment of the present invention, each of the plurality of breakage portions extends linearly in the width direction.

[0008] In one form of the present invention, in each of at least some of the constrictions, the first edge has one curved portion that is convexly curved toward the second edge, and the second edge has another curved portion that is convexly curved toward the first edge.

[0009] In one embodiment of the present invention, in each of the at least some of the constricted portions, a direction connecting one curved portion and the other curved portion at the shortest distance is parallel to the width direction. Effect of the Invention

[0010] According to the present invention, it is possible to reliably form a cut in the coated film along the shape of the breaking portion by microwave irradiation, while increasing the total length of the cut. [Brief description of the drawings]

[0011] [Figure 1] 1 is a perspective view showing a configuration of a package for microwave treatment according to one embodiment of the present invention; [Diagram 2] 1 is a plan view showing a configuration of a tear-off label according to an embodiment of the present invention. [Diagram 3] 3 is a cross-sectional view of the tear-off label shown in FIG. 2, taken along the line III-III. [Figure 4] FIG. 11 is a plan view showing a tear-off label according to a first modified example of an embodiment of the present invention. [Diagram 5] FIG. 11 is a plan view showing a breakable label according to a second modified example of an embodiment of the present invention. [Figure 6] FIG. 13 is a plan view showing a breakable label according to a third modified example of an embodiment of the present invention. [Figure 7] FIG. 13 is a plan view showing a breakable label according to a fourth modified example of an embodiment of the present invention. [Figure 8] FIG. 13 is a plan view showing a tear-off label according to a fifth modified example of an embodiment of the present invention. [Figure 9] FIG. 13 is a plan view showing a tear-off label according to a sixth modified example of an embodiment of the present invention. [Figure 10] FIG. 13 is a plan view showing a tear-off label according to a seventh modified example of an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] A tear-off label according to an embodiment of the present invention will be described below with reference to the drawings. In the following description of the embodiment, the same or corresponding parts in the drawings are given the same reference numerals, and the description thereof will not be repeated. In the drawings, the length direction of the tear-off label is the X-axis direction, the width direction of the tear-off label is the Y-axis direction, and the thickness direction of the tear-off label is the Z-axis direction.

[0013] Fig. 1 is a perspective view showing the configuration of a package for microwave treatment according to one embodiment of the present invention. Fig. 2 is a plan view showing the configuration of a breakable label according to one embodiment of the present invention. Fig. 3 is a cross-sectional view of the breakable label of Fig. 2 as seen from the direction of the arrows along line III-III.

[0014] As shown in Fig. 1, a package 1 for microwave treatment according to one embodiment of the present invention includes a container 2, an adhesive film 3, and a breakable label 10. As shown in Fig. 2 and Fig. 3, the breakable label 10 according to one embodiment of the present invention includes a main body layer 11 and an adhesive layer 12.

[0015] As shown in Fig. 1, a package for microwave treatment 1 is a package that contains a packaged object (not shown), such as a food for use in a microwave oven, to be treated by microwave irradiation. The packaged object is heated by irradiating the package for microwave treatment 1 with microwaves.

[0016] The container 2 contains the packaged item. The container 2 is formed of a synthetic resin such as polypropylene (PP). The cladding film 3 seals the opening at the top of the container 2, and the container 2 and the cladding film 3 seal the packaged item.

[0017] The cladding film 3 is a single resin film or a laminated film in which multiple resin films are laminated together. The cladding film 3 is preferably a resin film that does not have heat shrinkability, but may be a resin film such as a heat shrinkable film or a self-stretchable film. The thickness of the cladding film 3 is, for example, 30 μm or more and 90 μm or less, and is 50 μm in this embodiment.

[0018] The break label 10 is attached to the outside of the covering film 3 of the package for microwave treatment 1. In the present embodiment, one break label 10 is attached to the covering film 3, but the number of break labels 10 attached to the covering film 3 is not limited to one, and may be multiple.

[0019] 2, the length 10W of the tear-away label 10 in the X-axis direction is, for example, 20 mm or more and 60 mm or less, and is 45 mm in this embodiment. The width 10L of the tear-away label 10 in the Y-axis direction is, for example, 10 mm or more and 40 mm or less, and is 20 mm in this embodiment.

[0020] As shown in Fig. 3, the main body layer 11 includes a base material layer 100 and a conductor layer 110 laminated together in the lamination direction with the adhesive layer 12. As shown in Fig. 2, in this embodiment, the base material layer 100 and the conductor layer 110 of the main body layer 11 have the same outer shape as each other when viewed from the lamination direction (Z-axis direction) of the main body layer 11 and the adhesive layer 12.

[0021] The main body layer 11 is not limited to a two-layer structure of the base material layer 100 and the conductive layer 110, and may have a light-shielding layer on the outermost surface opposite to the cladding film 3, taking into consideration the amount of sparks generated in the tear-off label 10 when irradiated with microwaves. Also, a resin laminate layer such as polyethylene terephthalate (PET) may be provided on the outermost surface opposite to the cladding film 3, taking into consideration the aesthetic appearance of the package 1 for microwave processing after microwave irradiation.

[0022] 3, the adhesive layer 12 is laminated on one side of the main body layer 11. Specifically, in this embodiment, the adhesive layer 12 is laminated adjacent to the conductor layer 110 and on the opposite side to the base layer 100 in the lamination direction (Z-axis direction) of the main body layer 11 and the adhesive layer 12. The adhesive layer 12 is laminated over the entire surface of one side of the conductor layer 110 in the lamination direction of the conductor layer 110.

[0023] The adhesive layer 12 preferably has an adhesiveness that allows it to stick to the adherend film 3 at room temperature and that adhesiveness lasts for a long time. Examples of materials constituting the adhesive layer 12 include acrylic resins, rubber resins, silicone resins, and urethane resins. The thickness of the adhesive layer 12 in the Z-axis direction is, for example, 10 μm or more and 30 μm or less.

[0024] 2 and 3, the base layer 100 in the main body layer 11 has a film shape. The thickness of the base layer 100 in the Z-axis direction is, for example, not less than 10 μm and not more than 100 μm.

[0025] The base layer 100 is, for example, a resin film such as PP or PET. The base layer 100 may be a resin film, synthetic paper, or a multi-layer film formed by laminating a plurality of layers made of different materials.

[0026] The conductive layer 110 has a film shape. The thickness (Z-axis direction) of the conductive layer 110 is, for example, a lower limit of 0.005 μm or more, preferably 0.01 μm or more, more preferably 0.015 μm or more, and even more preferably 0.04 μm or more, and an upper limit of 30 μm or less, preferably 20 μm or less, more preferably 10 μm or less, and even more preferably 1 μm or less, and most preferably 0.08 μm or less.

[0027] The conductive layer 110 is, for example, a metal such as aluminum, nickel, or chromium, an alloy, or a metal oxide. The conductive layer 110 may be provided on the base layer 100 by vapor deposition, or may be formed by adhering a foil-like conductive layer 110 to the base layer 100. The conductive layer 110 may be provided on the base layer 100 by applying ink containing a material constituting the conductive layer 110 onto the base layer 100 and curing it.

[0028] 2 and 3, the conductor layer 110 has a first edge portion 111, a second edge portion 112, a plurality of constricted portions 120, and a plurality of broken portions 130. In the present embodiment, the conductor layer 110 has two constricted portions 120 and two broken portions 130.

[0029] 2, the first edge portion 111 extends along a length direction (X-axis direction) perpendicular to the stacking direction when viewed from the stacking direction (Z-axis direction). Specifically, the first edge portion 111 extends in the X-axis direction while meandering in accordance with the multiple constricted portions 120.

[0030] When viewed from the stacking direction (Z-axis direction), the second edge portion 112 extends along the length direction (X-axis direction) while being spaced apart from the first edge portion 111 in the width direction (Y-axis direction) perpendicular to the length direction. Specifically, the second edge portion 112 extends in the X-axis direction while meandering in accordance with the multiple constricted portions 120 while being spaced apart from the first edge portion 111 in the Y-axis direction.

[0031] Each of the multiple constricted portions 120 is sandwiched between a first edge portion 111 and a second edge portion 112. In each of the multiple constricted portions 120, the distance between the first edge portion 111 and the second edge portion 112 is narrow. In this embodiment, the multiple constricted portions 120 are portions of the break label 10 including the conductor layer 110 that are narrowed in width in the Y-axis direction. In the break label 10 of one embodiment of the present invention, the base material layer 100 also has multiple constricted portions 120, but it is sufficient that at least the conductor layer 110 has multiple constricted portions 120.

[0032] The width 120L of each of the plurality of constricted portions 120 in the Y-axis direction is, for example, 4 mm or more and 20 mm or less, and is 8 mm in this embodiment. In this embodiment, each of the plurality of constricted portions 120 has a shape that is line-symmetrical with respect to a virtual central axis that passes through the center position of the width 10L in the Y-axis direction and extends in the X-axis direction, but is not limited to this shape, and may have a shape that is asymmetric with respect to the virtual central axis. For example, one of the first edge portion 111 and the second edge portion 112 may extend in the X-axis direction while meandering, and the other of the first edge portion 111 and the second edge portion 112 may extend parallel to the X-axis direction. In addition, each of the plurality of constricted portions 120 may have a shape different from each other.

[0033] In this embodiment, in each of the multiple constricted portions 120, the first edge portion 111 has one curved portion 111a curved in a convex shape toward the second edge portion 112 side, and the second edge portion 112 has the other curved portion 112a curved in a convex shape toward the first edge portion 111 side. Note that in all of the constricted portions 120, each of the first edge portion 111 and the second edge portion 112 does not necessarily have to have a curved portion, and it is sufficient that in the constricted portion 120 in which the break portion 130 is provided, each of the first edge portion 111 and the second edge portion 112 has a curved portion.

[0034] If each of the first edge 111 and the second edge 112 is bent, sparks may occur at the bent corners of each of the first edge 111 and the second edge 112 when microwaves are applied. By each of the first edge 111 and the second edge 112 being curved, it is possible to suppress sparks from occurring at the curved parts of each of the first edge 111 and the second edge 112 when microwaves are applied. Like the shape of each of the first edge 111 and the second edge 112, all corners of the outer shape of the tear-away label 10 in the XY plane have a curved shape.

[0035] As described later, in at least some of the constricted portions 120 in which the plurality of breakage portions 130 are provided, the direction connecting one curved portion 111a and the other curved portion 112a at the shortest distance is parallel to the width direction (Y-axis direction). In this embodiment, in each of the two constricted portions 120, the direction connecting one curved portion 111a and the other curved portion 112a at the shortest distance is parallel to the Y-axis direction.

[0036] As shown in FIG. 2 and FIG. 3, the plurality of breaks 130 penetrate the conductive layer 110 in the stacking direction (Z-axis direction). In this embodiment, the plurality of breaks 130 are provided in the conductive layer 110, but they may penetrate not only the conductive layer 110 but also at least one of the base layer 100 and the adhesive layer 12 on the same line in the Z-axis direction. For example, when the conductive layer 110 is provided on the base layer 100 by vapor deposition, the plurality of breaks 130 are provided by forming a defective portion of the conductive layer 110 by masking a part of the base layer 100. In this embodiment, the breaks 130 are slit holes, but are not limited to slit holes and may be cracks that inhibit the flow of electrons in the conductive layer 110 when microwaves are irradiated. The cracks can be formed by embossing, for example.

[0037] In this embodiment, as shown in FIG. 2, the plurality of break portions 130 are provided in one-to-one correspondence with at least some of the plurality of constricted portions 120. Two break portions 130 are provided for each of the two constricted portions 120. Note that there may be a constricted portion 120 in which no break portion 130 is provided. Also, there may be a constricted portion 120 in which a plurality of break portions 130 are provided. That is, at least one of the plurality of break portions 130 is provided in each of at least some of the constricted portions 120 in the plurality of constricted portions 120. Note that there may be a break portion provided in a portion other than the constricted portion 120.

[0038] Each of the multiple breakage parts 130 extends linearly in the width direction (Y-axis direction). The width 130W of each of the multiple breakage parts 130 in the X-axis direction is, for example, 1.0 mm or less, preferably 0.5 mm or less, and more preferably 0.2 mm or less. The length 130L of each of the multiple breakage parts 130 in the Y-axis direction is, for example, 2 mm or more and 6 mm or less, and is 4 mm in this embodiment.

[0039] Each of the multiple break portions 130 divides the constricted portion 120 in which the break portion 130 is provided in the length direction (X-axis direction) while being spaced apart from each of the first edge portion 111 and the second edge portion 112. Specifically, the vertical width 130L of the break portion 130 is narrower than the width 120L of the constricted portion 120, and the break portion 130 is spaced apart from each of the first edge portion 111 and the second edge portion 112. In this way, the break portion 130 divides the portion of the constricted portion 120 in the X-axis direction excluding both ends in the Y-axis direction.

[0040] In this embodiment, each of the multiple break portions 130 is a slit hole and is therefore spaced apart from each of the first edge portion 111 and the second edge portion 112, but this configuration is not limited thereto, and when each of the multiple break portions 130 is a crack, at least some of the multiple break portions 130 may be provided continuously from one curved portion 111a to the other curved portion 112a, thereby vertically cutting through the conductor layer 110. In this case, since the base layer 100 is not divided by a crack, the integrity of the break label 10 can be maintained even if the conductor layer 110 is completely divided by a crack.

[0041] The break portion 130 in the Y-axis direction is, for example, 2 mm away from each of the first edge portion 111 and the second edge portion 112. Specifically, as shown in Fig. 2, the dimension of each of the distance L2 between the first edge portion 111 and the break portion 130 and the distance L2 between the second edge portion 112 and the break portion 130 in the constricted portion 120 is 2 mm. The dimension of the distance L2 is preferably 0.1 mm or more and 2 mm or less.

[0042] In the plurality of breakages 130, the dimension of the distance L1 between adjacent breakages 130 in the length direction (X-axis direction) is 1 / 9 or more and 5 / 9 or less of the dimension of the length 10W of the conductive layer 110 in the length direction (X-axis direction). In this embodiment, the dimension of the distance L1 between adjacent breakages 130 in the X-axis direction is approximately 1 / 3 of the dimension of the length 10W of the conductive layer 110 in the X-axis direction. Since the dimension of the distance L1 is 1 / 9 or more and 5 / 9 or less of the dimension of the length 10W, the conductive layer 110 that serves as an electron supply source is secured between adjacent breakages 130 and on both outsides of the breakages 130, and a sufficient amount of electrons can be collected at the breakages 130 during microwave irradiation to generate sparks. As a result, the deposition film 3 can be effectively melted by heat generated by the sparks.

[0043] Hereinafter, the action of the breakable label 10 according to one embodiment of the present invention when irradiated with microwaves will be described.

[0044] When the tear-away label 10 is exposed to microwaves, eddy currents are generated in the conductive layer 110. The generated eddy currents are concentrated at positions along the constricted portion 120 and the broken portion 130 due to the so-called edge runaway phenomenon, which is concentrated at the severed tip of the conductive layer 110.

[0045] 2, since the width 120L of the constricted portion 120 is narrower than the width 10L of the tear-away label 10 in the Y-axis direction, the density of electrons is high in the constricted portion 120. Therefore, high-density electrons are concentrated in the position between the first edge portion 111 and the tearing portion 130 and in the position between the second edge portion 112 and the tearing portion 130 in the constricted portion 120.

[0046] In the conductive layer 110 at the position between the first edge 111 and the break portion 130 and at the position between the second edge 112 and the break portion 130 in the constricted portion 120, concentrated high-density electrons cannot flow because the electron flow path area is narrow, and as a result, discharge occurs between the end faces of the conductive layer 110 facing each other via the break portion 130 in the X-axis direction, generating a spark. The heat generated by this spark is transferred from the tear label 10 to the covering film 3, melting the portion of the covering film 3 along the break portion 130. The covering film 3 melts to form a cut, and steam generated from the packaged item heated by microwaves is discharged from the inside of the microwave processing package 1 to the outside through the cut in the covering film 3.

[0047] Even if the fracture portion 130 is a crack, a spark occurs due to discharge between the end faces of the conductive layers 110 facing each other in the X-axis direction through the fracture portion 130, which is a crack, just as in the case of the present embodiment where the fracture portion 130 is a slit hole.

[0048] In this embodiment, the breakable label 10 has multiple constricted portions 120 with breakable portions 130, so that the total length of the cuts in the adhesive film 3 can be increased, and as a result, steam generated within the adhesive film 3 can be reliably released to the outside. This gives the breakable label 10 a high steam release performance compared to a so-called substantially bow-tie type breakable label that has only one constricted portion with a breakable portion 130.

[0049] The cut formed in the cling film 3 is not limited to be for the purpose of discharging steam from inside the package for microwave treatment 1, but may also be used as an opening for opening the cling film 3.

[0050] Furthermore, if the width 120L of the constricted portion 120 is narrowed even slightly from the width 10L of the breakable label 10 in the Y-axis direction, electrons will be more likely to concentrate in the constricted portion 120, making the effect of causing sparks by microwave irradiation greater than that of a rectangular breakable label.

[0051] In the tear-away label 10 according to one embodiment of the present invention, by having a plurality of constricted portions 120 each having a tear portion 130, high-density electrons can be concentrated at the constricted portions 120 during microwave irradiation to generate sparks at the tear portion 130, thereby making it possible to ensure that the adherend film 3 is cut along the shape of the tear portion 130 while increasing the total length over which the cut is made.

[0052] In one embodiment of the present invention, the tear label 10 has tear portion 130 extending linearly in the width direction (Y-axis direction), which allows sparks to be generated uniformly along the entire length of tear portion 130 in the Y-axis direction. This allows the total length of the tear to be increased while ensuring that the adhesive film 3 cuts along the shape of tear portion 130.

[0053] In a break-away label 10 according to one embodiment of the present invention, in the constricted portion 120, the first edge 111 has one curved portion 111a that is convexly curved toward the second edge 112, and the second edge 112 has the other curved portion 112a that is convexly curved toward the first edge 111, thereby making it possible to prevent sparks from occurring at the one curved portion 111a and the other curved portion 112a when microwaves are irradiated.

[0054] In the tear-away label 10 according to one embodiment of the present invention, the shortest direction connecting one curved portion 111a and the other curved portion 112a in the constricted portion 120 is parallel to the width direction (Y-axis direction), so that the gap between the first edge portion 111 and the second edge portion 112 can be narrowed around the tearing portion 130 compared to a case where the shortest connecting direction is not parallel to the Y-axis direction, and therefore electrons can be concentrated at the tearing portion 130 during microwave irradiation to generate sparks. As a result, the deposition film 3 can be effectively melted by the heat generated by the sparks.

[0055] The following describes modified examples of the breakable label according to an embodiment of the present invention. The breakable labels according to the following modified examples have different configurations of the first edge, second edge, constricted portion, and breakable portion from the breakable label 10 according to an embodiment of the present invention, so that the configurations that are similar to those of the breakable label 10 according to an embodiment of the present invention will not be described repeatedly.

[0056] Fig. 4 is a plan view showing a tear-away label according to a first modified example of an embodiment of the present invention. As shown in Fig. 4, in a tear-away label 10A according to a first modified example of an embodiment of the present invention, the dimension of the distance L1 between adjacent tearing portions 130 is approximately 1 / 9 the dimension of the length 10W of the tear-away label 10.

[0057] Even if the dimension of the distance L1 between adjacent breaking portions 130 is reduced to approximately one-ninth the dimension of the length 10W of the tear-away label 10, the conductive layer 110 serving as an electron supply source is secured between adjacent breaking portions 130, and a sufficient amount of electrons can be gathered at the breaking portions 130 during microwave irradiation to generate sparks. As a result, the deposition film 3 can be effectively melted by the heat generated by the sparks.

[0058] In the tear-tooth label 10A according to a first modified example of an embodiment of the present invention, each of the two constricted portions 120 has a shape that is line-symmetrical with respect to an imaginary central axis that passes through the center position of the width 10L in the Y-axis direction and extends in the X-axis direction. The two constricted portions 120 have a shape that is line-symmetrical with respect to an imaginary central axis that passes through the center position of the tear-tooth label 10 in the X-axis direction and extends in the Y-axis direction.

[0059] As shown in FIG. 4, the angle between the constriction center line B passing through the center of the constriction portion 120 and extending in the Y-axis direction and the portion of the first edge portion 111 located between the constriction portions 120 is A1. The angle between the constriction center line B and the portion of the first edge portion 111 located outside the constriction portions 120 is A2. In this modified example, since A2>A1, the distance between the adjacent constriction portions 120 in the X-axis direction is shorter than one-third of the dimension of the length 10W of the tear-to-break label 10. As a result, the dimension of the distance L1 between the adjacent tear-to-break portions 130 is also shorter than one-third of the dimension of the length 10W of the tear-to-break label 10. The angle A1 and the angle A2 are not limited to the relationship A2>A1, and may satisfy the relationship A2=A1 as in this embodiment.

[0060] The breakage portion 130 is not limited to being provided on the constriction center line B, but may be provided within a range of ±5 mm in the X-axis direction centered on the constriction center line B. By providing the breakage portion 130 within this range, high-density electrons can be concentrated on the constriction portion 120 during microwave irradiation, causing sparks to be generated at the breakage portion 130.

[0061] Fig. 5 is a plan view showing a breakable label according to a second modified example of an embodiment of the present invention. As shown in Fig. 5, in a breakable label 10B according to a second modified example of an embodiment of the present invention, a maximum width 13L in the Y-axis direction between the breakable portions 130 is narrower than a width 10L at both ends in the X-axis direction, and is wider than a width 120L in the Y-axis direction of the constricted portion 120.

[0062] Fig. 6 is a plan view showing a break label according to a third modified example of an embodiment of the present invention. As shown in Fig. 6, in a break label 10C according to a third modified example of an embodiment of the present invention, each of a first edge 111 and a second edge 112 extends parallel to the X-axis direction within a range of length L3 at both ends of the break label 10C in the X-axis direction.

[0063] Fig. 7 is a plan view showing a break label according to a fourth modified example of an embodiment of the present invention. As shown in Fig. 7, in a break label 10D according to a fourth modified example of an embodiment of the present invention, the first edge 111 and the second edge 112 each extend parallel to the X-axis direction within a range of length L4 between the constricted portions 120.

[0064] Fig. 8 is a plan view showing a break label according to a fifth modified example of an embodiment of the present invention. As shown in Fig. 8, in a break label 10E according to a fifth modified example of an embodiment of the present invention, the second edge 112 extends parallel to the X-axis direction.

[0065] 9 is a plan view showing a tear-away label according to a sixth modified example of an embodiment of the present invention. As shown in FIG. 9, in a tear-away label 10F according to a sixth modified example of an embodiment of the present invention, one curved portion 111a and the other curved portion 112a are positioned so as to be shifted from each other in the X-axis direction. The tearing portion 130 extends in a direction that connects the one curved portion 111a and the other curved portion 112a in the shortest possible direction, and is positioned obliquely with respect to the Y-axis direction. In this modified example, the length of the tearing portion 130 can be increased, so that the total length in which the cut is made can be increased.

[0066] Fig. 10 is a plan view showing a break label according to a seventh modified example of an embodiment of the present invention. As shown in Fig. 10, a break label 10G according to a seventh modified example of an embodiment of the present invention is provided with three constricted portions 120. One break portion 130 is provided in each of the three constricted portions 120.

[0067] It should be noted that the above-mentioned embodiments disclosed herein are illustrative in all respects and are not intended to be a basis for restrictive interpretation. Therefore, the technical scope of the present disclosure should not be interpreted solely by the above-mentioned embodiments. Furthermore, all modifications within the meaning and scope equivalent to the claims are included. In the above-mentioned description of the embodiments, configurations that can be combined may be combined with each other. [Explanation of symbols]

[0068] 1 microwave treatment packaging body, 2 container, 3 adhesive film, 10, 10A, 10B, 10C, 10D, 10E, 10F, 10G tearable label, 11 main body layer, 12 adhesive layer, 100 base material layer, 110 conductor layer, 111 first edge portion, 111a one curved portion, 112 second edge portion, 112a the other curved portion, 120 constricted portion, 130 tearable portion.

Claims

1. A tear-off label attached to an adhesive film of a package for microwave treatment, comprising: A main body layer; an adhesive layer laminated on one side of the main body layer, the main body layer includes a base material layer and a conductor layer laminated together in a lamination direction with the adhesive layer, The conductive layer is A first edge portion extending along a length direction perpendicular to the stacking direction when viewed from the stacking direction; A second edge portion extending along the longitudinal direction while being spaced apart from the first edge portion in a width direction perpendicular to the longitudinal direction when viewed from the stacking direction; a plurality of constricted portions sandwiched between the first edge portion and the second edge portion, and a distance between the first edge portion and the second edge portion is narrowed; a plurality of breakage portions penetrating the conductive layers in the stacking direction; At least one of the plurality of breakable portions is provided in each of at least some of the plurality of constricted portions, A tear-away label, wherein each of the plurality of tear portions divides a constricted portion among the at least some of the constricted portions in the longitudinal direction.

2. The tearable label according to claim 1 , wherein each of the plurality of tear portions extends linearly in the width direction.

3. A tear-away label as described in claim 1 or claim 2, wherein in each of at least some of the constricted portions, the first edge portion has one curved portion that is convexly curved toward the second edge portion, and the second edge portion has another curved portion that is convexly curved toward the first edge portion.

4. The breakable label according to claim 3 , wherein in each of the at least some of the constricted portions, a direction connecting the one curved portion and the other curved portion at the shortest distance is parallel to the width direction.

Citation Information

Patent Citations

  • Surface working method for photoreceptor

    JP1981021127A

  • Tack label and package for unsealing product package for microwave treatment

    JP1990148974U

  • Sheet-like lid material for microwave processed package and microwave processed package

    JP2009234626A

  • Label for fracture by microwave and package for microwave treatment