Sodium Vaporizer and Method of Using Sodium Vaporizer

The vaporizer system with a movable crucible and adjustable surface area exposure addresses the instability of sodium vapor output, ensuring stable vaporization for accurate detector calibration in sodium-cooled reactors.

JP7559048B2Active Publication Date: 2024-10-01TERRAPOWER LLC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2022506811
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-08-23
Filing Date
2020-07-21
Publication Date
2024-10-01
Estimated Expiration
2040-07-21

AI Technical Summary

Technical Problem

Existing sodium vaporizers struggle to produce a stable vapor output across a wide range of sodium vapor concentrations due to the formation of oxide films on the molten sodium surface, leading to unstable vaporization at both high and low concentrations, which complicates the calibration of sodium ionization detectors in sodium-cooled nuclear reactors.

Method used

A vaporizer system with a movable crucible and adjustable surface area exposure to heated inert gas, allowing for controlled vapor concentration levels by selectively positioning the molten material within a guide tube, combined with temperature regulation to maintain stable vaporization output.

Benefits of technology

The system achieves stable vaporization output across varying sodium vapor concentrations, enabling accurate calibration of ionization detectors and reducing aerosol formation, thereby enhancing diagnostic operations in sodium-cooled nuclear reactors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007559048000001
    Figure 0007559048000001
  • Figure 0007559048000002
    Figure 0007559048000002
  • Figure 0007559048000003
    Figure 0007559048000003
Patent Text Reader

Abstract

The vaporizer includes an outer tube configured to receive a heated gas flow and an inner tube disposed at least partially within the outer tube. The inner tube is spaced apart from the outer tube, and the heated gas flow is routed through an annular space therebetween. The vaporizer also includes a crucible disposed at least partially within the inner tube. The crucible is movable within the outer tube and retractable relative to the inner tube. The crucible is configured to hold the molten metal such that a surface area of ​​the molten metal exposed to the heated gas flow is adjustable based on the position of the crucible relative to the inner tube. A heater is configured to vaporize the molten material, and the vapor mixes with the heated gas flow.
Need to check novelty before this filing date? Find Prior Art

Description

Detailed Description of the Invention

[0001] (CROSS REFERENCE TO RELATED APPLICATIONS) This application was filed as a PCT international patent application on July 21, 2020, and claims priority to and the benefit of U.S. Provisional Application No. 62 / 891,244, filed August 23, 2019, the entirety of which is incorporated herein by reference.

[0002] [Introduction] Sodium-cooled nuclear reactors may use sodium ionization detectors in safety systems to detect leaks and / or diagnose system performance in removing alkali metal vapor. The sodium ionization detector produces an electrical signal proportional to the concentration of sodium vapor in the inert gas. Therefore, quantitative measurement of sodium vapor concentration requires calibration of the sodium ionization detector so that the relationship between signal and concentration is known.

[0003] To calibrate a sodium ionization detector, heated inert gas is passed through a vaporizer containing sodium. The sodium is heated and the resulting vapor is carried in the inert gas through a detector which generates an ion current between a filament and a collector. The vapor is then trapped downstream of the detector and its contents are elementally analyzed to determine the total amount of sodium trapped during the calibration run. The vaporizer must produce a steady vapor output so that the time averaged vapor concentration in the inert gas can be known with low variance and the corresponding average detector signal can be measured. The vaporizer temperature is incremented to produce a larger or smaller signal (e.g., ion current) and new runs are run to obtain a series of data points for a calibration curve.

[0004] It is desirable for the vapor source to produce a stable vapor output during the calibration run and over a range of sodium vapor concentration levels. This is because a particular concentration in the gas (which corresponds to the mass of sodium collected over and averaged over the duration of the calibration run) will correlate with a single average signal value at the sodium ionization detector. However, it can be difficult to generate a stable vapor stream for both high and low sodium vapor concentration levels. Sodium can form an oxide film / layer on its molten surface, which inhibits the vaporization of sodium into the inert gas. By increasing the temperature of the sodium, the sodium oxide dissolves slowly (e.g., over many hours), while an unstable vapor output is generated during the dissolution process. However, significantly increasing the temperature of the molten sodium (e.g., 250°C to 350°C) can rapidly dissolve the oxide layer and result in a stable vapor output. However, this stability occurs only for flows with high sodium vapor concentration; flows with low sodium vapor concentration remain unstable. The reason for this is that high vapor output concentrations are always produced at high temperatures, and it is difficult to dilute the output with higher flows of inert gas, since the detector needs to be calibrated at a set (e.g., constant) flow rate for a given diagnostic operation. Therefore, an improved vaporizer is desired.

[0005] [Sodium vaporizer and method] A vaporizer and vaporization method are described herein for holding a charge of molten material at a high enough temperature to rapidly melt oxides and produce a stable vaporization output. This vapor output can be mixed with a flow of heated inert gas for use in calibrating ionization detectors. The molten material is held in a movable crucible within a guide tube in which the surface area of ​​the molten material exposed to the inert gas is adjustable and the concentration of vapor within the inert gas can be varied. Thus, a stable vaporization output is produced for a wide range of vapor concentrations (e.g., both higher and lower concentration levels).

[0006] These and various other features, as well as advantages characterizing the vaporizers and methods described herein, will become apparent from a reading of the following detailed description and a study of the associated drawings. Additional features will be set forth in the following description, and in part will be obvious from the description, or may be learned by the practice of the technology. The advantages and features of the technology will be realized and attained by the structure particularly set forth in this description and claims as well as the appended drawings.

[0007] It is to be understood that both the foregoing introduction and the following detailed description are exemplary and explanatory and are intended to provide further explanation of the invention as claimed.

[0008] [Brief description of the drawings] The following drawings, which form part of this application, are illustrative of the described technology and are not intended in any way to limit the scope of the claimed technology, which is to be determined by the claims appended hereto.

[0009] FIG. 1 is a schematic diagram of an exemplary vaporizer system.

[0010] FIG. 2 is an exploded perspective view of an exemplary vaporizer of the system shown in FIG.

[0011] FIG. 3 is a cross-sectional view of the carburetor in the advanced position.

[0012] FIG. 4 is a cross-sectional view of the carburetor in the retracted position.

[0013] FIG. 5 is a perspective view of an exemplary elongated boat in the vaporizer shown in FIGS.

[0014] FIG. 6 is a flow chart illustrating an exemplary method for vaporizing molten metal.

[0015] [Detailed Description] The present disclosure describes a vaporizer and method for producing a variable concentration stream of vaporized material. The vaporizer includes a crucible that holds a charge of molten material. The crucible is slidably disposed at least partially within an inner chamber / guide tube and is configured to selectively extend and retract therefrom. An outer chamber surrounds both the crucible and the inner chamber and receives a flow of heated inert gas. The inert gas passes over an exposed surface area of ​​the molten material and mixes with the vapor. The mixture of inert gas and vaporized material may be used for calibrating ionization detectors (e.g., sodium ionization detectors in sodium fast reactor plants), physical vapor deposition processes, or any other process / method required or desired.

[0016] As the molten material retreats into the inner chamber, the inner chamber shields the molten material from the inert gas flowing in the outer chamber. The surface area of ​​the molten material in the outer chamber can be selectively adjusted to control the vapor output into the inert gas and, therefore, its concentration. By being able to control the vapor output of the molten material into the inert gas, the vaporizer can heat the molten material to a temperature suitable to produce a stable vaporization output over a range of concentrations between high vapor concentration levels (e.g., a larger area of ​​surface area of ​​the molten material) and low vapor concentration levels (e.g., a smaller area of ​​surface area of ​​the molten material).

[0017] FIG. 1 is a schematic diagram of an exemplary vaporizer system 100. The vaporizer system 100 includes a vaporizer 102 configured to hold a charge of molten material for vaporization and to allow a heated inert gas to pass over the charge to mix with the vapor. A gas supply 104 is fluidly connected to the vaporizer 102. The gas supply 104 generates a flow 106 of heated inert gas, such as, but not limited to, argon or nitrogen, for collecting at least a portion of the vapor generated in the vaporizer 102. After the vapor mixes with the heated inert gas, the mixture 108 is conveyed downstream from the vaporizer 102 to a calibration system 110. The calibration system 110 includes a detector 112 configured to generate an ionic current between an anode and a cathode and record a current signal. Additionally, the calibration system 110 includes a gas scrubber / trap 114 configured to collect and analyze the vapor in the mixture 108. Additionally, the calibration system 110 may generate a calibration curve based on the measured data points over multiple calibration runs (eg, steady flows having various vapor concentration levels of the mixture 108).

[0018] The vaporizer 102 includes a gas manifold 116 that connects to the gas supply 104 and receives a flow of heated inert gas 106. The gas manifold 116 is connected to an outer chamber 118 that receives the heated inert gas and holds a charge of molten material therein. A clamshell heater 120 at least partially surrounds the outer chamber 118 and allows the molten material to be heated as required or desired. The heater 120 is illustrated as transparent in FIG. 1 so that the internal components can be viewed. Downstream of the outer chamber 118 is a sintered metal filter 122 that is configured to remove any entrained droplets or aerosols in the vapor mixture 108 before entering the calibration system 110. The filter 122 may be located at least partially within the heater 120. A gas thermocouple 124 is connected to the gas manifold 116 to measure the temperature of the flow of heated inert gas 106. The thermocouple 124 may be communicatively connected to the calibration system 110 to provide temperature data of the heated gas for the calibration process. Additionally, the molten substance thermocouple 126 is connected to the charge of molten substance to measure the temperature of the molten substance. The thermocouple 126 may be communicatively connected to the calibration system 110 to provide temperature data of the molten substance for the calibration process. For example, the thermocouples 124, 126 are used such that the temperature of the gas can be substantially matched to the temperature of the molten substance and the formation of aerosols is reduced or prevented.

[0019] In this example, the heater 120 is a clamshell heater that surrounds the outer chamber 118 and the filter 122, but does not surround the gas manifold 116. This configuration allows the heater 120 to heat the molten material to a required or desired temperature and maintain the filter 122 at a similar temperature to reduce or prevent aerosol generation that is undesirable for detector calibration, and to produce a steady vapor output. In other examples, the heater 120 may include any other heater that enables the vaporizer 102 to function as described herein. For example, the heater 120 may extend to partially surround other components, such as the gas manifold 116. This configuration allows the heater 120 to maintain a uniform temperature of the molten material and other vaporizer components to reduce or prevent aerosol generation, and to reduce the need for the filter 122.

[0020] Additionally or alternatively, the heater 120 may include multiple heaters such that the vaporizer 102 may have one or multiple heating zones. In one embodiment, the heater 120 may have a first heater (e.g., a clamshell heater) surrounding the outer chamber 118 and a second heater (not shown) configured to heat the gas manifold 116. In this example, the second heater may heat the molten substance disposed within the gas manifold 116 to a temperature approximately equal to the temperature of the first heater 120. In another example, the second heater may heat the molten substance to a temperature higher than the temperature of the first heater 120 or lower than the temperature of the first heater 120. At least in part, the heating of the gas manifold 116 may prevent cooling of the molten substance disposed therein. This allows mechanical adjustment of the vaporizer 102 to adjust the vapor output. In another example, the steam output can be thermally regulated in addition to or as an alternative to mechanical regulation by heating the molten material in various heating zones.

[0021] Vaporizer 102 also includes a moving mechanism 128 configured to control the position of the charge of molten material within outer chamber 118. Moving mechanism 128 is connected to an actuator 129 configured to generate a linear movement M. Actuator 129 may include any type of system or device that generates linear movement as described herein, such as an electric motor, a solenoid, manual, etc. Moving mechanism 128 allows the surface area of ​​the molten material to be selectively controlled to cause a steady flow of mixture 108 having various vapor concentration levels as described herein.

[0022] 2 is an exploded perspective view of the vaporizer 102 in the vaporizer system 100 (shown in FIG. 1). As described above with reference to FIG. 1, the vaporizer 102 includes a gas manifold 116, an outer chamber 118, a heater 120, a filter 122, thermocouples 124, 126, and a moving mechanism 128. Additionally, the vaporizer 102 includes an inner chamber 130 disposed at least partially within and spaced apart from the outer chamber 118. In this example, both the outer chamber 118 and the inner chamber 130 are substantially tubular shaped components, such that the outer tube 118 has a diameter larger than a diameter of the inner tube 130, and both tubes are substantially concentric with each other.

[0023] An elongated boat 132 is at least partially disposed within the inner chamber 130. The elongated boat 132 is configured to hold a charge of molten material and allow a heated inert gas to pass over a surface of the molten material. In this example, the boat 132 is an open vessel, which in some examples may be a crucible, as needed or desired. In this example, the heater 120 at least partially surrounds the boat 132 to cause vaporization of the molten material. The boat 132 is connected to a movement mechanism 128 such that the boat 132 may move into and out of the inner chamber 130 while remaining contained within the outer chamber 118. The inner chamber 130 serves as a guide tube and cover for the boat 132 within the vaporizer 102.

[0024] In this example, the gas manifold 116 can be a four-way connector, such as a union cross fitting. One of the openings can include a reducer 134 so that the manifold 116 can be fluidly connected to the gas supply 104 (shown in FIG. 1 ). The opposite opening can include a reducer 136 configured to support the gas thermocouple 124 and allow the thermocouple 124 to measure the temperature of the heated inert gas flowing through the manifold 116. One end of the outer chamber 118 can be connected to another opening 138 so that a flow of heated gas can be delivered into the outer chamber 118. The opposite opening can include a fitting 140 used to support the inner chamber 130 that extends through the manifold 116. For example, the fitting 140 can be a bore-through fitting that allows the inner chamber 130 to slide through. Additionally, the transfer mechanism 128 includes a reducing union fitting 152 that connects to a nut on the aft end of the internal chamber 130 and swages to the transfer mechanism 128. The fitting 152 may be used to allow the boat 132 to be completely removed from within the internal chamber 130. It should be understood that other arrangements and layouts of the components of the manifold 116 may be used as needed or desired.

[0025] 3 is a cross-sectional view of the vaporizer 102 in an extended position. Certain components have been described above and will not necessarily be described further. Additionally, the heater 120 (shown in FIGS. 1 and 2) is not shown for clarity. The outer chamber 118 has an inlet 142 and an opposing outlet 144 defining a longitudinal axis 146 therebetween. The inlet 142 is connected to an opening 138 of the gas manifold 116 such that heated inert gas may flow therethrough.

[0026] The internal chamber 130 has a first end 148 and an opposite second end 150 and extends along a longitudinal axis 146. The first end 148 of the internal chamber 130 is supported at one or more locations proximate a fitting 140 opposite the opening 138 of the gas manifold 116, the fitting 140 receiving the external chamber 118. The internal chamber 130 thus cantilevers through the gas manifold 116 via the fitting 140 and partially extends into the external chamber 118 to form the cantilevered second end 150. Additionally, in this example, a reducer 152 is disposed at the first end 148 of the internal chamber 130 adjacent the fitting 140. The second end 150 of the internal chamber 130 is disposed within the external chamber 118 closer to the inlet 142. The reducer 152 forms a seal against the interior of the vaporizer 100. The reducer 152 allows the movement mechanism 128 to extend into the interior chamber 130 and connect to the elongated boat 132. For example, the reducer 152 may include a Teflon ferrule, which allows the movement mechanism 128 to slide against the Teflon ferrule. The fitting 140 also forms a seal around the interior chamber 130 in the gas manifold 116, such that the interior chamber 130 may extend outward.

[0027] An elongated boat 132 is slidably disposed within the interior chamber 130 proximate the second end 150. The boat 132 has a proximal end 154 that connects to the translation mechanism 128 and an opposite distal end 156 configured to move along the longitudinal axis 146 relative to the second end 150 of the interior chamber 130. As shown in FIG. 3, the boat 132 is in a fully advanced position. In the advanced position, the boat 132 is still disposed completely within the outer chamber 118, with the distal end 156 extending a distance D from the second end 150 of the interior chamber 130. Although the fully advanced position of the distal end 156 is shown in FIG. 3, it should be understood that the distal end 156 may be extended via the translation mechanism 128 to any position less than the fully advanced position, as needed or desired.

[0028] During operation, a flow of heated inert gas 106 is delivered from the gas manifold 116 toward the outlet 144 into the outer chamber 118. More specifically, the inert gas 106 is delivered at the inlet 142 of the outer chamber 118 into the annular space between the inner chamber 130 and the outer chamber 118. The inert gas 106 can then travel through the annular space to the second end 150 of the inner chamber 130, where it can pass over the boat 132 and the molten material disposed therein. The flow of inert gas mixes with vapor released from the molten material to produce a mixture 108 that is discharged from the outlet 144 of the outer chamber 118 and used for calibration measurements.

[0029] In this example, the distance D that the boat 132 extends from the inner chamber 130 defines the surface area of ​​the molten material that will produce vapor that mixes with the inert gas as the inert gas passes through it. In this manner, the surface area of ​​the molten material can be easily adjusted within the vaporizer 102, and as a result, the vapor concentration in the discharged mixture 108 can be easily controlled. Furthermore, this movement of the boat 132 allows the heater to maintain a temperature of the molten material that produces stable vaporization (e.g., reduced oxide layer formation on the material), while still allowing the vapor concentration in the mixture 108 to be controlled as needed or desired.

[0030] FIG. 4 is a cross-sectional view of the vaporizer 102 in a retracted position. Certain components have been described above and will not necessarily be described further. Additionally, the heater 120 (shown in FIGS. 1 and 2) is not shown for clarity. In the fully retracted position, a flow of heated inert gas 106 may still be routed through the vaporizer 102 as described above. However, the boat 132 has been retracted such that the tip 156 is located adjacent the second end 150 of the inner chamber 130 and the molten material is disposed entirely within the inner chamber 130. This position of the boat 132 shields the molten material from the heated inert gas 106 such that the inert gas no longer passes directly over the molten material and steam mixing with the gas is reduced or prevented.

[0031] It should be understood that a fully advanced ( FIG. 3 ) and a fully retracted ( FIG. 4 ) position of the boat 132 are shown and described. The boat 132 may be placed in any intermediate position as needed or desired. The intermediate positions allow the surface area of ​​the molten material in direct contact with the flow of heated inert gas 106 to be adjusted and allow the steam output to mix with the inert gas to be controlled because the gas does not pass directly over the molten material retracted into the inner chamber 130.

[0032] The movement mechanism 128 may be used to determine the position of the boat 132 relative to the internal chamber 130. The movement mechanism 128 may include a linkage 158 extending through the first end 148 of the internal chamber 130 via a reducer 152. One end of the linkage 158 connects to the proximal end 154 of the boat 132 to drive the movement of the boat 132 to a desired or required distance D (shown in FIG. 3). The other end of the linkage 158 connects to a coupler 160 such that the linkage 158 may be attached to an actuator 129 (shown in FIG. 1) which drives the linear movement M along the longitudinal axis 146. In this manner, the position of the movement mechanism 128 determines the position of the boat 132. The coupler 160 also allows for the attachment of a molten material thermocouple 126. In this example, the linkage 158 is an elongated tube concentric with both of the chambers 118 , 130 so that the junction of the thermocouple 126 can extend to the boat 132 .

[0033] FIG. 5 is a perspective view of elongated boat 132 of vaporizer 102 (shown in FIGS. 1-4 ). Inner chamber 130 is shown transparent in FIG. 5 to show boat 132 partially disposed therein. As shown in FIG. 5 , boat 132 is in a partially advanced (or partially retracted) position. In that position, tip 156 of boat 132 is located a distance D from second end 150 of inner chamber 130. As a result, a portion of the molten material disposed within boat 132 is shielded within inner chamber 130.

[0034] In this example, the boat 132 is substantially semicircular in cross-sectional shape to hold the molten material in the vaporizer and provide a surface area exposed to the heated inert gas. The second end 150 of the inner chamber 130 is partially surrounded by an end cap 162 to further shield the molten material in the inner chamber 130 from the flow of the heated inert gas. While the structure of the inner chamber 130 and the boat 132 limits the vapor from within the inner chamber 130 from mixing with the inert gas outside the inner chamber 130, the end cap 162 does not completely seal the second end 150 of the inner chamber 130, and at least a portion of the inert gas and / or vapor may pass through the second end 150. In this example, the end cap 162 is semicircular in shape, so that the end cap 162 may be used to prevent the boat 132 from rotating around its longitudinal axis (e.g., the sidewall of the boat 132 that engages the end cap 162) during operation. In addition, the junction of the thermocouple 126 extends through the base end 154 of the boat 132 so that the molten material contained therein can be measured. The thermocouple 126 is located at the bottom of the boat 132 and may be covered by the molten material during operation. Therefore, a sheathed thermocouple 126 may be used so that the thermocouple wires and junctions are protected from the liquid metal.

[0035] Additionally, the internal chamber 130 has at least one hole 164 defined therein. The hole 164 is defined between the ends of the internal chamber 130. In one example, the hole 164 is formed on the internal chamber 130 such that when the vaporizer is assembled, the hole 164 is located proximate to the fitting 140 on the gas manifold 116 (shown in FIG. 2). This location allows a portion of the heated inert gas to flow through the internal chamber 130 and exit from the second end 150. The flow of gas through the internal chamber 130 is less than the flow of gas through the outer chamber, and the flow of gas through the internal chamber 130 is used to reduce or prevent vapor from condensing from the molten material at the first end 148 of the internal chamber 130 (shown in FIG. 3). The first end of the internal chamber 130 may not be located within the heater 120 (shown in FIG. 1). In some examples, when the boat 132 is in a fully retracted position (shown in FIG. 4), at least a portion of the boat 132 may cover the holes 164 to reduce the flow of heated inert gas through the inner chamber 130.

[0036] In this example, as the boat 132 retracts toward the gas manifold and at least partially out of the heater, the temperature of the molten material may decrease when the boat 132 is in the retracted position. This change in temperature of the molten material may increase the formation of aerosols. However, a calibration curve can still be determined and any aerosols that are generated can be removed in a filter. In other examples, the heater may be configured to maintain the temperature of the molten material at any position of the boat 132 (e.g., even when the heater surrounds at least a portion of the gas manifold), thereby controlling the vapor output at a constant temperature and reducing or preventing the formation of aerosols.

[0037] During operation of the vaporizer, the position of the boat 132 relative to the inner chamber 130 determines the surface area of ​​the molten material exposed to the flow of heated inert gas, and therefore the vapor output of the vaporizer. Thus, decreasing the surface area of ​​the molten material decreases the vapor output of the vaporizer, while increasing the surface area of ​​the molten material increases the vapor output of the vaporizer. In the example described herein, it is the boat 132 that moves relative to the inner chamber 130. In other embodiments, the boat 132 remains stationary, while the inner chamber 130 can move relative to the boat 132 to adjust the surface area of ​​the molten material exposed to the flow of heated inert gas.

[0038] The vaporizers described herein can be used to vaporize any type of molten material as needed or desired. In one embodiment, the molten material can be an alkali metal, such as sodium. In another example, other alkali metals, such as cesium or a mixture of sodium and cesium, can be placed in the vaporizer. In another embodiment, potassium or rubidium can be vaporized.

[0039] FIG. 6 is a flow chart illustrating an exemplary method 200 for vaporizing molten metal. The method 200 begins with a charge of molten metal held in a crucible being heated to generate a vapor output (operation 202). The crucible is at least partially disposed within the inner chamber. Additionally, a heated inert gas is flowed into an inlet of an outer chamber (operation 204). The inlet chamber is at least partially disposed within the outer chamber. A flow of heated inert gas is then routed between the inner chamber and the outer chamber (operation 206). Downstream of the inner chamber, a flow of heated inert gas is passed over a surface area of ​​the molten metal contained within the crucible (operation 208). As the heated inert gas passes over the surface area of ​​the molten metal, at least a portion of the vapor output mixes with the heated inert gas and is carried further downstream. The crucible can be selectively moved relative to the inner chamber (operation 210) to adjust the surface area of ​​the molten metal exposed to the flow of heated inert gas to alter the vapor output of the molten metal.

[0040] In some examples, method 200 may further include filtering the mixture of steam output and heated inert gas to remove entrained droplets or aerosols (Operation 212). The heating operation (Operation 202) may further include directing the molten metal to dissolve oxides in the molten metal (Operation 214). Also, the molten metal and the inert gas may be heated to approximately equal temperatures to reduce the formation of aerosols. In one embodiment, the molten metal in method 200 may be sodium. Method 200 may further include calibrating a sodium ionization detector via the steam output (Operation 216).

[0041] In one embodiment, the crucible may be actively wetted before vaporizing the molten metal. Otherwise, the molten metal has a tendency to bead up in the unwetted areas, and as a result, the molten metal may not spread evenly within the crucible. To wet the crucible, a strip of metal (e.g., sodium) may be placed in the crucible and heated. The molten metal may then be mechanically stirred so that the crucible is wetted in all places. In some examples, the heat generated for this initial wetting may be from a clamshell heater. In other examples, a separate localized heater may be used for the initial wetting, and then the crucible is placed into the vaporizer.

[0042] Notwithstanding the scope of the appended claims, and in addition to the examples described above, further examples are disclosed in the following numbered items: 1. An outer tube configured to receive a flow of heated gas; an inner tube disposed at least partially within and spaced from the outer tube, the heated gas flow being routed through an annular space between the outer tube and the inner tube; a crucible disposed at least partially within the inner tube, the crucible being movable within the outer tube toward and away from the inner tube and configured to hold the molten metal such that a surface area of ​​the molten metal exposed to the flow of heated gas is adjustable based on a position of the crucible relative to the inner tube; a heater configured to vaporize the molten material, the vapor mixing with the heated gas flow; A vaporizer comprising:

[0043] 2. The vaporizer of claim 1, wherein when the crucible is retracted into the inner tube, the molten metal is not directly exposed to the heated gas stream.

[0044] 3. The vaporizer of any preceding item, wherein the heater comprises a clamshell heater at least partially surrounding the outer tube.

[0045] 4. The vaporizer of any preceding item, further comprising a sintered metal filter downstream of the outer tube configured to remove entrained droplets or aerosols in the mixture of vapor and heated gas.

[0046] 5. The vaporizer of any preceding item, further comprising a moving mechanism configured to control a position of the crucible relative to the inner tube.

[0047] 6. The vaporizer of item 5, wherein the moving mechanism includes a thermocouple configured to measure a temperature of the molten metal.

[0048] 7. The vaporizer of any preceding item, further comprising a thermocouple disposed upstream of the outer tube and configured to measure a temperature of the heated gas stream.

[0049] 8. An outer chamber having an inlet and an outlet, the outer chamber having a major axis defined between the inlet and the outlet; an inner chamber disposed at least partially within the outer chamber, the inner chamber having an end disposed proximate the inlet of the outer chamber; an elongated boat disposed at least partially within the interior chamber, the elongated boat having a distal end configured to advance and retract along the longitudinal axis relative to the end of the interior chamber; a heater at least partially surrounding the elongated boat; A vaporizer comprising:

[0050] 9. The outer chamber includes an outer tube and the inner chamber includes an inner tube; Item 9. The vaporizer of item 8, wherein the inner tube is concentric with the outer tube.

[0051] 10. Further comprising a filter connected to the outlet of the outer chamber; 10. The vaporizer of claim 8 or 9, wherein the filter is disposed at least partially within the heater.

[0052] 11. The vaporizer according to any one of items 8 to 10, further comprising a moving mechanism connected to a base end of the elongated boat.

[0053] 12. The vaporizer of item 11, wherein the displacement mechanism extends at least partially through the second end of the internal chamber.

[0054] 13. The vaporizer of any one of items 8 to 12, wherein the end of the internal channel is at least partially enclosed.

[0055] 14. The vaporizer according to any one of items 8 to 13, further comprising a gas manifold connected to the inlet of the outer chamber.

[0056] 15. Heating a charge of molten metal held in a crucible to produce a vapor output, wherein said crucible is at least partially disposed within an interior chamber; flowing the heated inert gas into an inlet of an outer chamber, wherein the inner chamber is at least partially disposed within the outer chamber; passing a flow of the heated inert gas between the inner chamber and the outer chamber; passing a flow of the heated inert gas over a surface area of ​​the molten metal, where at least a portion of the steam output mixes with the heated inert gas as it passes over the surface area; and selectively moving the crucible relative to the internal chamber to adjust the surface area of ​​the molten metal exposed to the flow of heated inert gas and vary the vapor output of the molten material; A method for vaporizing molten metal, comprising:

[0057] 16. The method of claim 15, further comprising filtering the mixture of steam output and heated inert gas to remove entrained droplets or aerosols.

[0058] 17. The method of claim 15 or 16, wherein heating the charge of molten metal in the crucible includes dissolving oxides in the molten metal.

[0059] 18. The method according to any one of items 15 to 17, wherein the molten metal and the inert gas are heated to approximately equal temperatures.

[0060] 19. The method according to any one of items 15 to 18, wherein the molten metal contains sodium.

[0061] 20. The method of any one of items 15 to 19, further comprising the step of calibrating a sodium ionization detector via the vapor output.

[0062] It is to be understood that the present disclosure is not limited to the specific structures, process steps, or materials disclosed herein, but extends to equivalents thereof, as would be recognized by one of ordinary skill in the art. It is also to be understood that the terminology used herein is used only for the purpose of describing specific examples, and is not intended to be limiting. It is to be noted that, as used herein, the singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise.

[0063] It will be apparent that the systems and methods described herein are well adapted to achieve the objects and advantages mentioned, as well as those inherent therein. Those skilled in the art will recognize that the methods and systems herein may be embodied in many forms and are therefore not limited by the illustrative examples and embodiments set forth above. In this regard, any number of the features of the various examples described herein may be combined into a single example, and alternative examples having fewer or more than all of the features described herein are possible.

[0064] Although various examples have been described for purposes of this disclosure, various changes and modifications may be made within the scope contemplated by this disclosure. Numerous other changes may be made that will be readily suggested to those skilled in the art and are encompassed by the spirit of this disclosure. [Brief description of the drawings]

[0065] [Figure 1] FIG. 1 is a schematic diagram of an exemplary vaporizer system. [Diagram 2] FIG. 2 is an exploded perspective view of an exemplary vaporizer for the system shown in FIG. 1. [Diagram 3] FIG. 2 is a cross-sectional view of the carburetor in an advanced position. [Figure 4] FIG. 2 is a cross-sectional view of the carburetor in a retracted position. [Diagram 5] FIG. 5 is a perspective view of an exemplary elongated boat in the vaporizer shown in FIGS. 1-4. [Figure 6] 1 is a flow chart illustrating an exemplary method for vaporizing molten metal.

Claims

1. an outer tube configured to receive a flow of heated gas; an inner tube disposed at least partially within and spaced from the outer tube, the heated gas flow being routed through an annular space between the outer tube and the inner tube; a crucible disposed at least partially within the inner tube, the crucible being movable within the outer tube toward and away from the inner tube and configured to hold the molten metal such that a surface area of ​​the molten metal exposed to the flow of heated gas is adjustable based on a position of the crucible relative to the inner tube; a heater configured to vaporize the molten metal, the molten metal vapor mixing with the heated gas flow; A vaporizer comprising:

2. 2. The vaporizer of claim 1, wherein the molten metal is not directly exposed to the heated gas flow when the crucible is retracted into the inner tube.

3. The vaporizer of any one of claims 1 to 2, wherein the heater comprises a clamshell heater that at least partially surrounds the outer tube.

4. The vaporizer of any one of claims 1 to 3, further comprising a sintered metal filter downstream of the outer tube configured to remove entrained droplets or aerosols in the mixture of vapor and heated gas.

5. The vaporizer of any one of claims 1 to 4, further comprising a moving mechanism configured to control a position of the crucible relative to the inner tube.

6. The vaporizer of claim 5 , wherein the moving mechanism includes a thermocouple configured to measure a temperature of the molten metal.

7. The vaporizer of any one of claims 1 to 6, further comprising a thermocouple disposed upstream of the outer tube and configured to measure a temperature of the heated gas flow.

8. an outer chamber having an inlet and an outlet, a major axis of the outer chamber being defined between the inlet and the outlet; an inner chamber disposed at least partially within the outer chamber, the inner chamber having an end disposed proximate the inlet of the outer chamber; an elongated boat disposed at least partially within the internal chamber, the elongated boat having a tip configured to move along the longitudinal axis from and to the end of the internal chamber; a heater at least partially surrounding the elongated boat; A vaporizer comprising:

9. the outer chamber includes an outer tube and the inner chamber includes an inner tube; 9. The carburetor of claim 8, wherein the inner tube is concentric with the outer tube.

10. a filter connected to the outlet of the outer chamber; 10. The vaporizer of claim 8 or 9, wherein the filter is disposed at least partially within the heater.

11. The vaporizer of any one of claims 8 to 10, further comprising a moving mechanism connected to a proximal end of the elongated boat.

12. The vaporizer of claim 11 , wherein the displacement mechanism extends at least partially through the second end of the internal chamber.

13. The vaporizer of any one of claims 8 to 12, wherein the end of the internal chamber is at least partially closed by an end cap.

14. The vaporizer of any one of claims 8 to 13, further comprising a gas manifold connected to the inlet of the outer chamber.

15. heating a charge of molten metal held in a crucible to produce a vapor output, the crucible being at least partially disposed within the interior chamber; flowing the heated inert gas into an inlet of an outer chamber, wherein the inner chamber is at least partially disposed within the outer chamber; passing a flow of the heated inert gas between the inner chamber and the outer chamber; passing a flow of the heated inert gas over a surface area of ​​the molten metal, where at least a portion of the steam output mixes with the heated inert gas as it passes over the surface area; and selectively moving the crucible relative to the internal chamber to adjust the surface area of ​​the molten metal exposed to the flow of heated inert gas and vary the vapor output of the molten metal; A method for vaporizing molten metal, comprising:

16. 16. The method of claim 15, further comprising filtering the mixture of steam output and heated inert gas to remove entrained droplets or aerosols.

17. 17. The method of claim 15 or 16, wherein heating the charge of molten metal in the crucible comprises melting oxides within the molten metal.

18. A method according to any one of claims 15 to 17, wherein the molten metal and the inert gas are heated to approximately equal temperatures.

19. The method of any one of claims 15 to 18, wherein the molten metal comprises sodium.

20. The method of any one of claims 15 to 19, further comprising the step of calibrating a sodium ionization detector via the vapor output.

Citation Information

Patent Citations

  • High dust sampling device

    JP1986024640U

  • JP1987182434U

  • Quantitative analytical method for micro amount of substance in gas, analyzer for quantitative analysis therefor, and sampling method and device therefor

    JP2006047232A

  • Matrix modifier and method for modifying a matrix to improve analysis of metal constituents during graphite furnace atomic absorption spectroscopy

    US4806489A