Method for manufacturing optical waveguide element
By measuring and correcting the structural parameters of optical waveguides through a digital twin simulation, the method addresses fabrication deviations in ridge-type optical waveguides, improving yield and performance.
Patent Information
- Application Number
- JP2023522194
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-05-21
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2041-05-21
AI Technical Summary
Conventional ridge-type optical waveguide fabrication methods using direct bonding face challenges in achieving the target structure due to processing accuracy limits, leading to deviations from desired characteristics and low yield.
A method involving structural measurement, prediction of optical properties, and reprocessing (trimming) of the optical waveguide structure to align with target specifications, using techniques like direct bonding, thinning, and dry etching, with the aid of a digital twin simulation to correct manufacturing errors.
This approach significantly improves the yield and performance of optical waveguides by ensuring they meet the target characteristics, enhancing optical damage resistance and reliability.
Smart Images

Figure 0007560790000001 
Figure 0007560790000002 
Figure 0007560790000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing an optical waveguide element. [Background technology]
[0002] Conventionally, optical elements capable of generating and modulating coherent light in the ultraviolet, visible, near-infrared, and terahertz wavelength bands have been applied to a wide variety of fields, including wavelength conversion and optical modulation of optical signals in optical communication systems, optical measurement, and optical processing. Among these, optical elements that utilize nonlinear optical effects have been the subject of research and development due to their excellent properties in wavelength conversion and electro-optical effects.
[0003] Various types of materials have been developed as optical materials with nonlinear optical effects and electro-optical effects. Among them, oxide-based compound substrates, such as lithium niobate (LiNbO3:LN) and lithium tantalate (LiTaO3:LT), have been researched and developed as promising materials because they have high second-order nonlinear optical constants, high electro-optic constants, and are transparent in a wide wavelength range. Among LN and LT, periodically poled lithium niobate (PPLN) and periodically poled lithium tantalate (PPLT), which have a periodically poled structure formed by taking advantage of the property that they can be spontaneously polarized at room temperature, are widely used. The above optical materials have a periodically poled structure, which gives them high phase consistency and, as a result, high second-order nonlinear optical effects, and are therefore widely used. Optical devices using the high nonlinearity of PPLN and PPLT include second harmonic generation (SHG), difference frequency generation (DFC), and ferroelectric conversion (FCC). Wavelength conversion elements that utilize frequency generation (DFG) and sum frequency generation (SFG) are known.
[0004] The mainstream optical waveguide structures using PPLN have been diffusion-type optical waveguides called titanium diffusion optical waveguides and proton exchange optical waveguides. This is because LN is a difficult-to-process material, making it difficult to fabricate anything other than diffusion-type optical waveguides. However, this diffusion-type optical waveguide has issues in terms of optical damage resistance and long-term reliability because impurities are diffused to form the optical waveguide during fabrication, causing a refractive index difference. In the diffusion-type optical waveguide structure, when high-power light is incident on the optical waveguide, the crystal structure is damaged by the photorefractive effect, so there is a limit to the optical power that can be input to the optical waveguide.
[0005] As one of the methods to solve this problem, research and development is being conducted on ridge-type optical waveguides (see Non-Patent Document 1). In particular, the use of a direct bonding method to form a ridge-type optical waveguide makes it possible to input high-power light, and it is expected that this will lead to a wide range of applications, such as the generation of high-intensity optical modulation signals and laser processing technology. [Prior art documents] [Non-patent literature]
[0006] [Non-Patent Document 1] S. Kurimura, Y. Kato, M. Maruyama, Y. Usui, and H. Nakajima, “Quasi-Phase-Matched adhered ridge waveguide in LiNbO3,” Appl. Phys. Lett. 89(19), 191123(2006) Summary of the Invention
[0007] However, due to limitations in the processing accuracy of various processes in the direct bonding method for forming a ridge-type optical waveguide, the optical waveguide structure actually fabricated deviates from the target structure, and there is a problem that the targeted characteristics cannot be obtained.
[0008] The present disclosure has been made in consideration of such problems, and has as its object to provide a method for manufacturing an optical waveguide element in which the optical waveguide structure actually produced is the targeted structural target.
[0009] In order to achieve this object, a manufacturing method for an optical waveguide element according to one embodiment of the present invention includes measuring structural values of at least one of the height and width of a core of an optical waveguide formed on a substrate, predicting optical characteristics of the optical waveguide based on the measured structural values, determining a correction amount for at least one of the height and width of a core of the optical waveguide formed on the substrate, provided that the predicted optical characteristics do not match target optical characteristics, reprocessing at least one of the height and width of the core of the optical waveguide formed on the substrate in accordance with the determined correction amount, and chipping the substrate on which the optical waveguide is formed, provided that the predicted optical characteristics match the target optical characteristics. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a diagram showing a cross-sectional structure of a ridge-type optical waveguide. [Diagram 2] FIG. 2 is a diagram illustrating a conventional method for manufacturing a chip having a ridge-type optical waveguide. [Diagram 3] FIG. 3 is a diagram illustrating a method for manufacturing a chip having a ridge-type optical waveguide according to one embodiment of the present invention. [Figure 4] FIG. 4 is a diagram showing a schematic configuration of a computer for implementing a method for manufacturing a chip having a ridge-type optical waveguide according to one embodiment of this invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, the embodiments of the present invention will be described in detail with reference to the drawings. The same or similar reference symbols indicate the same or similar elements, and repeated explanations may be omitted. The materials and values in the following description are examples and are not intended to limit the technical scope of the present invention. The embodiments described below may be implemented using other materials and values within the scope of the present invention.
[0012] Hereinafter, a method for manufacturing an optical waveguide element according to an embodiment of the present invention will be described by taking as an example a ridge-type optical waveguide in which a core layer and an undercladding layer of a nonlinear optical material are directly bonded. The ridge-type optical waveguide included in the element may be, for example, a PPLN optical waveguide.
[0013] (Selection of nonlinear optical materials) The nonlinear optical material used in this embodiment may be any material that is transparent at a light wavelength of 400 nm to 2000 nm. The nonlinear optical material may be any material that has a nonlinear optical effect, and may be a second-order nonlinear optical effect or a third-order or higher nonlinear optical effect. Examples include lithium niobate (LiNbO3), lithium tantalate (LiTaO3), beta barium borate (β-BaB2O4:BBO), potassium titanyl phosphate (KTiOPO4:KTP), etc. The nonlinear optical material may be a material that has a nonlinear optical effect, and may be a material that has a second-order nonlinear optical effect or a third-order or higher nonlinear optical effect. Examples include lithium niobate (LiNbO3), lithium tantalate (LiTaO3), beta barium borate (β-BaB2O4:BBO), potassium titanyl phosphate (KTiOPO4:KTP), etc. In order to increase the nonlinear optical effect, the nonlinear optical material may have a periodic polarization inversion structure. When using a nonlinear optical material having a periodic polarization inversion structure, it is possible to appropriately select the optical waveguide processing conditions below the Curie temperature at which the periodic polarization inversion is not lost, and the optical waveguide structure that can achieve phase matching.
[0014] (Optical waveguide structure) FIG. 1 is a diagram showing the cross-sectional structure of a ridge-type optical waveguide. As shown in FIG. 1, the optical waveguide structure is composed of an undercladding layer 1, an overcladding layer 3, and a core layer 2, and light propagates inside the core layer 2. The undercladding layer 1 and the core layer 2 are directly bonded to each other, and therefore have high optical damage resistance, making it possible to input excitation light with a very high power density into the optical waveguide. There is no particular restriction on the refractive index of the overcladding layer 3, and the overcladding layer 3 may be air (air cladding) or may be formed by chemical vapor deposition (Chemical Vapor Deposition: CV). D) and Flame Hydrolysis Deposition (FHD) , glass deposited by a sputtering method, or the like, and any type may be used as long as it has an overcladding layer according to the optical waveguide structure design.
[0015] There is also no particular restriction on the core size, and it may be a relatively large core diameter (10 μm or more) that propagates light in multimode, or a small core diameter (10 μm or less) that propagates light in single mode. It may be an optical waveguide in which the core layer 2 is thinned by a smart cut method or the like to attempt to reduce the core size, and the core diameter may be very small (in nm units). There is also no particular restriction on the core shape, and it may be a square, rectangular, trapezoid, or any other shape that can be processed.
[0016] (Optical waveguide formation method) Next, a method for forming an optical waveguide will be described. First, a conventional method for manufacturing an optical waveguide element will be described as a comparative example with reference to Fig. 2, and then a method for manufacturing an optical waveguide element according to an embodiment of the present invention will be described with reference to Fig. 3.
[0017] As shown in FIG. 2, a conventional method for manufacturing an optical waveguide element includes step 1: direct bonding, step 2: thinning, step 3: optical waveguide formation, step 4: chip formation, and step 5: evaluation of optical properties.
[0018] In step 1, a substrate 10 of a nonlinear optical material that will become the undercladding layer 1 and a substrate 20 of a nonlinear optical material that will become the core layer 2 are directly bonded. The direct bonding in step 1 uses a direct bonding technique that does not use an adhesive, which leads to improved optical loss resistance when high-intensity light is used as input light. In step 1, by selecting the thermal expansion coefficients of the substrate 10 of the undercladding layer 1 and the substrate 20 of the core layer 2 that are as close as possible, it is possible to suppress substrate cracking in a heat treatment process in a later process. In the present disclosure, a substrate formed by directly bonding the substrate 10 and the substrate 20 is also referred to as a bonded substrate.
[0019] In step 2, the substrate 20 of the bonded substrate, which is made of a nonlinear optical material and which will become the core layer 2, is thinned. There are no particular limitations on the method for thinning the substrate, and examples of the method include a grinding and polishing process and a smart cut method.
[0020] In step 3, the substrate 20 is processed to form the core layer 2 of the optical waveguide 40. There are no particular limitations on the method for forming the optical waveguide, and possible methods include a dry etching process and cutting out the core layer 2 of the optical waveguide 40 with a dicing saw. In step 3, an overcladding layer 3 of the optical waveguide 40 is formed by a known method as necessary.
[0021] In step 4, the substrate having the fabricated optical waveguide 40 is chipped to produce an optical waveguide element. A method using a dicing saw is one possible method for chipping, but there is no particular limitation on the processing method. In addition, by optically polishing the end face after chipping or coating it with an anti-reflection film, it is possible to reduce the optical loss when light enters or exits the chip 50 as the optical waveguide element.
[0022] In step 5, the optical characteristics of the chip 50 having the fabricated optical waveguide 40 are evaluated. cormorant.
[0023] In the conventional manufacturing method of an optical waveguide element shown in FIG. 2, when the optical characteristics of optical waveguide 40 of chip 50, which is an optical waveguide element, are evaluated in step 5, many optical waveguides that do not satisfy the target optical characteristics are manufactured due to manufacturing errors, etc., and once chipped, it is difficult to reprocess them, so there is a limit to improving the yield.
[0024] 3, the manufacturing method of the optical waveguide element of this embodiment includes direct bonding in step 1, thinning in step 2, optical waveguide formation in step 3, chipping in step 4, and optical property evaluation in step 5, and further includes structure measurement in step 31, property prediction in step 32, correction amount determination in step 33, and reprocessing in step 343. The manufacturing method in FIG. 3 is a method incorporating a correction process for the optical waveguide structure.
[0025] Steps 1 and 2 are respectively the same steps as those described with reference to FIG.
[0026] In step 3, the substrate 20 is processed to form the core layer 2 of the optical waveguide 40. There are no particular limitations on the method for forming the optical waveguide, and possible methods include a dry etching process and cutting out the optical waveguide with a dicing saw. In step 3, the overcladding layer 3 is not formed. If the overcladding layer 3 of the optical waveguide 40 is necessary, it is formed after steps 31 and 32.
[0027] In step 31, the structure of the fabricated optical waveguide 40 is measured. As main measurement items, the distribution of the width W and height H of the core layer 2 of the optical waveguide 40 in the light propagation direction can be mentioned as candidates. This is because the effective refractive index of the optical waveguide 40 is determined by the product of these items, and these are the items that ultimately have the greatest influence on the effective refractive index distribution of the optical waveguide in the propagation direction of the optical waveguide 40. As a method for measuring the structure, the width W of the core layer 2 of the optical waveguide 40 can be measured by an optical microscope or a length measuring scanning electron microscope (SEM). In addition, the height H of the core layer 2 of the optical waveguide 40, that is, the film thickness distribution of the core layer 2 can be measured by a method using optical interference. The measurement of the height H of the core layer 2 of the optical waveguide 40 in step 31 may be performed after step 2 and before step 3. In this case, the film thickness distribution of the thinned substrate 20 before the optical waveguide is formed may be measured.
[0028] In step 32, the same structure (digital twin of the optical waveguide) is created on a simulator based on the actual measurement values of the structure obtained in step 31 (distribution of the width W and the height H of the core layer 2 of the optical waveguide 40), and the optical characteristics are simulated. The simulation method at this time can be determined according to the target physical quantity (e.g., optical loss, nonlinear optical effect). Representative simulation methods include the Beam Propagation Method (BPM) and the Finite Difference Time Domain (FDTD). In step 32, it is determined whether the optical characteristics predicted by the simulation are the target characteristics. If it is determined that the predicted optical characteristics are the target characteristics, the process proceeds to the chipping process in step 4, and if it is determined that the predicted optical characteristics are not the target characteristics due to a manufacturing error or the like, the process proceeds to a correction process (trimming process) in step 33 to step 34.
[0029] In step 33, the amount of change required for various structural parameters is calculated so that the optical characteristics of the structure (digital twin) on the simulator created in step 32 reach the target characteristics, and the amount of correction (trimming amount) is determined.
[0030] In step 34, a correction (trimming) process is performed on the actual structure based on the correction amount determined in step 33. In this process, at least one of the width W and thickness H of the core layer 2 of the optical waveguide 40 may be corrected. A possible method for the correction process is local structural modification using a local etching device.
[0031] In step 35, steps 31 to 34 are repeated until the optical waveguide structure exhibits the target characteristics. Through these steps, the structure of the core layer 2 of the finally obtained optical waveguide 40 satisfies the initial target setting values. If necessary, an overcladding layer 3 is deposited. In this embodiment, the optical waveguide 40 is a ridge-type optical waveguide including an undercladding layer 1, a core layer 2, and an overcladding layer 3.
[0032] Steps 4 and 5 are respectively the same steps as those described with reference to FIG.
[0033] The method for producing an optical waveguide element of this embodiment (steps 1 to 5 above) is expected to dramatically improve yields and characteristics compared to conventional methods for producing optical waveguide elements.
[0034] (Direct bonding method (process 1)) Direct bonding is a technique for firmly bonding substrates together without using adhesives. In direct bonding, the substrates are first surface-treated using chemicals, then the substrates are placed together and bonded by the attractive forces between the surfaces. The surface treatment conditions (temperature, type of chemicals, etc.) for each substrate can be optimized depending on the type and combination of substrates to be bonded. In addition, when bonding substrates together, it is desirable to perform the work in a clean atmosphere with as few microparticles as possible. In addition, the direct bonding process is performed at room temperature, but the bonding strength at this time is small, so that a heat treatment at a high temperature is performed afterwards to perform diffusion bonding and improve the bonding strength. The bonded substrates are free of microparticles or the like at the bonding surface, are void-free, and do not develop cracks at room temperature.
[0035] Direct bonding technology, which can firmly bond substrates together without using adhesives, has features such as high optical damage resistance, long-term reliability, and ease of device design. In addition, it has the advantage of being able to avoid the inclusion of impurities and absorption by adhesives when generating mid-infrared light using difference frequency generation, a type of nonlinear optical effect.
[0036] (Thinning method (Step 2)) Techniques for thinning the substrate 20 include a grinding / polishing process, a thinning process using smart cut, etc. In this embodiment, there is no particular limitation on the thinning method, and either thinning by grinding / polishing or thinning by smart cut may be used.
[0037] In the thinning process by grinding and polishing, a device with a controlled flatness of the grinding and polishing platen is used to perform grinding and polishing until the optical waveguide is present at the desired depth. By performing a polishing process after the grinding and polishing process, a mirror-like polished surface (optical end face) can be obtained. Finally, the parallelism of the substrate (the difference between the maximum and minimum heights of the substrate) is measured using an optical parallelism measuring device, and the parallelism of the substrate as a whole can be obtained.
[0038] The thinning process by Smart Cut mainly consists of two steps: an ion implantation step and a thin film peeling step. In the ion implantation step, helium or hydrogen ions are implanted into the substrate 20 that needs to be thinned to have a second-order nonlinear optical effect. The ions are implanted from the substrate surface with a controlled acceleration voltage and controlled dose, and are trapped at a certain depth from the surface. The ions used are preferably smaller than the atoms that make up the substrate, such as hydrogen or helium. In the substrate peeling step, the substrate into which the ions have been implanted is heat-treated to peel off the substrate at the damaged layer within the substrate. When the nonlinear optical material has a periodic polarization inversion structure, the heat treatment temperature in the substrate peeling step is set to be lower than the Curie temperature of the second-order nonlinear optical crystal in order to prevent the patterned polarization direction from being destroyed.
[0039] The core layer thinned by the above method has an in-plane thickness distribution due to its processing accuracy. In particular, the thinning process by grinding and polishing, which can produce a ridge-type optical waveguide 40 having a relatively large core layer 2 with high optical damage resistance, has a relatively large processing limit in suppressing the thickness distribution. Due to the thickness distribution caused by these processing accuracy limits, it is difficult to produce an optical waveguide having the final target structure.
[0040] (Method of forming core layer of optical waveguide (step 3)) The core layer 2 of the ridge-type optical waveguide 40 can be formed by a method using a dry etching process or a method using mechanical processing such as a dicing saw. In this embodiment, the method for forming the core layer 2 of the ridge-type optical waveguide 40 is not particularly limited, and the dry etching process can be used. The method may be a method using a guide rail, a method using a dicing saw, or any other forming method.
[0041] In the method using dry etching, a dry etching device is used to etch the surface of the substrate 20 that will become the core layer 2 (hereinafter referred to as the core substrate surface), thereby forming the core layer 2 of the optical waveguide 40. At this time, a pattern of the optical waveguide 40 is created on the core substrate surface by a normal photolithography process. The resist of the optical waveguide pattern is used as a mask, and dry etching is performed by a dry etching device to form the core layer 2 of the optical waveguide 40. With this method, distribution occurs in the optical waveguide width due to the following two causes.
[0042] The first cause is the fabrication error of the optical waveguide pattern created by the photolithography process. In this process, it is possible to suppress the optical waveguide width distribution by optimizing the photolithography conditions, but it is difficult to fabricate a resist pattern that is completely free of optical waveguide width distribution.
[0043] The second cause is the in-plane distribution of the amount of etching during dry etching. In the dry etching process, it is difficult to completely eliminate the in-plane distribution of the amount of etching that affects the width of the optical waveguide 40 that is finally formed. The reasons for this include, for example, in the case of a nonlinear optical substrate having a periodically poled structure, the etching rate differs slightly depending on the polarization direction, a temperature distribution occurs within the substrate surface during the process, and the etching rate differs depending on the substrate temperature, and the density of the plasma during dry etching does not necessarily have a uniform distribution within the surface.
[0044] In the method using mechanical processing, typically a dicing saw, a dicing blade used in a normal dicing process is used to form the core layer 2 of the optical waveguide 40. In this method, the precision of the structure of the optical waveguide 40 to be fabricated is determined mainly by the precision of the processing machine, in particular the positional precision of the stage that fixes the sample and the processing part. Therefore, there is a limit to the precision with which the core layer 2 of the optical waveguide 40 can be fabricated, and it is difficult to fabricate an optical waveguide having an optical waveguide width that is exactly as designed. Waveguides are difficult to fabricate.
[0045] For the above reasons, in the currently widely used processes for fabricating ridge-type optical waveguides, it is difficult to fabricate an optical waveguide that completely matches the initially set target structure, in particular the optical waveguide having the optical waveguide width.
[0046] (Reprocessing (trimming)) As explained with reference to Fig. 2, in the conventional method for manufacturing an optical waveguide element, after forming the element into a chip in step 4, the optical characteristics are evaluated in step 5. The "characteristics" in step 5 refer to index values that represent the function or performance of the optical waveguide, such as the second-order nonlinear optical constant or optical transmittance in the case of a nonlinear optical element.
[0047] In the conventional manufacturing method of optical waveguide elements, the target optical characteristic value is set, and the structure of the optical waveguide is designed to realize the target optical characteristic value. Then, the process moves to the optical waveguide processing step, aiming at the target structure. In the actual processing step, the structure of the optical waveguide 40 obtained deviates from the target structure. This is due to manufacturing errors in each step. In step 4, the optical waveguide 40 obtained through steps 1 to 3 is chipped by dicing or the like, optical end faces are formed, and a chip 50 having the optical waveguide 40 is completed. In step 5, the completed chip 50 is inspected, and the characteristics of the optical waveguide 40 are not known until it is inspected. In the conventional optical waveguide forming step, the characteristics of the optical waveguide are not known until it is inspected after being inspected, and even if it is found by inspection that a chip that does not satisfy the target characteristics has been manufactured, it is difficult to correct the structure after it has been manufactured, and there is a problem that a chip that does not have a structure having the target characteristics is manufactured.
[0048] In the manufacturing method of the optical waveguide element of this embodiment described with reference to Fig. 3, target optical characteristic values are also set, and the structure of the optical waveguide is designed to realize the target optical characteristic values. Then, the process moves to the processing step of the optical waveguide, aiming for the target structure. In the actual processing step, the structure of the optical waveguide 40 obtained deviates from the target structure. This is due to manufacturing errors in each process, and the manufacturing method up to this step is the same as the conventional manufacturing method of the optical waveguide element.
[0049] In this embodiment, based on structural information obtained by measuring various structural values such as the height H and width W of the core layer 2 of the fabricated optical waveguide 40, the same structure is formed on a simulator, and the optical characteristics are predicted using various simulation methods. At this time, the optical waveguide fabricated on the simulator is a digital twin of the actually fabricated optical waveguide 40, and it is possible to predict the characteristic values non-destructively on the simulator. A pass / fail judgment is made as to whether the characteristic values obtained on the simulator reach the initially set target values (judgment as to whether the initially set target values are reached). If the predicted characteristics pass, an overcladding layer 3 is formed as necessary, and then the process proceeds to chip formation.
[0050] If the predicted characteristics are not met, a correction step (trimming) is performed on the structure of the core layer 2. The amount of structural correction in the correction process is calculated on the simulator. The amount of correction is reflected in the structure on the simulator, and calculations are performed until the obtained optical characteristics exceed the pass standard. Then, based on the obtained amount of correction, the core layer 2 of the actual optical waveguide 40 is reworked (trimmed). Any method of reworking may be used as long as it has a processing accuracy that can realize reworking with the amount of correction obtained on the simulator, and in this embodiment, local etching, which performs dry etching locally, is listed as a candidate technology. After the reworking is completed, the structural value of the core layer 2 is measured again, the digital twin is reproduced on the simulator, and optical characteristics are predicted. By repeating the above correction steps (steps 31 to 34) until the predicted optical characteristics satisfy the set target value, it becomes possible to manufacture an optical waveguide 40 having the target characteristics. Note that, when the optical waveguide 40 has a rectangular cross section, the optical characteristics such as the effective refractive index (equivalent refractive index) and propagation characteristics of the optical waveguide 40 are basically determined by the width and height of the core layer, the refractive index of the core, and the refractive index of the cladding. In addition, the correction of the optical characteristics by correcting the width W of the core layer can also be performed by correcting the height of the core layer. Therefore, by correcting either or both of the width and height of the core layer of the optical waveguide, the optical characteristics of the optical waveguide can be corrected. Therefore, the amount of structural correction calculated on the simulator can indicate the amount of correction for either or both of the width W and height H of the core layer 2 of the optical waveguide 40 formed on the bonded substrate.
[0051] (Measurement of the height of the optical waveguide) In this embodiment, the distribution of height H (film thickness distribution) of core layer 2 of optical waveguide 40 is measured using optical interference. Specifically, light is incident on the surface of substrate 20 that will become core layer 2, and non-contact evaluation of the film thickness of the multilayer film can be performed by analyzing the reflection spectrum of light. The method of analyzing the film thickness using interference with reflected light is a widely used method, and the film thickness is measured using the optical interference method that is commonly used in this embodiment. The film thickness may be measured either by a method of measuring the entire substrate surface after step 2, which is prior to the formation of the optical waveguide in step 3, or by a method of measuring only core layer 2 of optical waveguide 40 in step 4, which is subsequent to the formation of the optical waveguide in step 3.
[0052] Furthermore, the film thickness measurement technique in this embodiment may be a technique other than that using optical interference, and any technique may be used as long as it is non-invasive to the optical waveguide structure.
[0053] (Measurement of the width of the optical waveguide) In this embodiment, the distribution of the width W of the core layer 2 of the optical waveguide 40 is measured by directly observing the core layer 2 of the optical waveguide 40. A specific observation method may be any method that is non-invasive to the optical waveguide structure, and representative examples include a method using an optical microscope and a method using an electron microscope such as a scanning electron microscope. In addition to the above methods, a method using a step gauge or a highly accurate measurement method using an atomic force microscope may also be used. In this case, there is no particular limit to the interval between measurement points when measuring the distribution of the width W of the core layer 2 of the optical waveguide, and the number of measurement points may be a number that can provide sufficient structural information in the structure trimming process and does not significantly reduce the throughput of the optical waveguide formation process.
[0054] (simulator) In the manufacturing method of the optical waveguide element of this embodiment, a simulator is used to simulate the same structure as the core layer 2 of the actually manufactured optical waveguide 40, the optical characteristics of the simulated structure are predicted, and an inspection is performed to determine whether the predicted optical characteristics meet the initial target characteristics to determine pass / fail. If the optical characteristics of the simulated structure do not meet the target values, in step 33, the simulator calculates to what extent the structure of the core layer 2 needs to be corrected to achieve the target optical characteristics. Then, in step 34, the structure of the core layer 2 of the actually manufactured optical waveguide 40 is corrected using the correction amount obtained in step 33.
[0055] In this embodiment, a local etching method capable of processing only a targeted range locally with high accuracy is used as the structural correction method, but any method capable of processing the structure of the core layer 2 of the optical waveguide 40 with high accuracy may be used. Then, for the processed structure, structural values such as the height H and width W of the core layer 2 of the optical waveguide 40 are measured in the same manner. Using the obtained processed structural values, a core structure of the optical waveguide that is a digital twin of the structure of the core layer 2 of the actual optical waveguide 40 is recreated on a simulator, optical characteristics are predicted, and an inspection is performed on the simulator to determine whether the predicted optical characteristics are the initial target characteristics or not, thereby making a pass / fail judgment. A series of steps including structure measurement in step 31, characteristic prediction in step 32, correction amount determination in step 33, reprocessing in step 34, structure measurement in step 31, and characteristic prediction in step 32 are repeated until the predicted optical characteristics become the initially set target characteristics, thereby making it possible to form an optical waveguide having the target characteristics.
[0056] FIG. 4 is a diagram showing a schematic configuration of a computer 100 constituting a simulator that can be used in the manufacturing method of the optical waveguide element of the present embodiment. The computer 100 has a processor 101, a memory 102, an input device 103, an output device 104, a communication device 105, and a storage 106. The processor 101 can be, for example, a central processing unit (CPU), a microprocessor implemented in an integrated circuit (IC), or a micro-processing unit (MPU), or other processors. The processor 101 can function as a measurement data processing unit 132 and a control data processing unit 133 by loading a program stored in the storage 106 into the memory 102 and executing it. The memory 102 can be, for example, a random access memory (RAM) or a read only memory (ROM). The input device 103 can be, for example, a keyboard, a mouse, a camera, or a sensor. The output device 104 can be, for example, a display device or a printer. The communication device 105 can be, for example, a wireless communication device or a wired communication device. The storage 106 may be, for example, a hard disk drive (HDD) or a solid state drive (SSD).
[0057] The computer 100 includes a measurement data processing unit 132 and a control data processing unit 133 that execute the functions of the simulator described above. The measurement data processing unit 132 executes the characteristic prediction of step 32 described with reference to Fig. 3, and the control data processing unit 133 executes the correction amount determination (trimming amount determination) of step 33 described with reference to Fig. 3.
[0058] In the feedforward system of Fig. 4, the solid lines indicate the flow of the object according to the process, the dashed lines indicate the measurement data obtained by the structure measurement in process 31, and the dashed lines indicate the correction amount (trimming amount) data for "control" in process 34.
[0059] The predicted value derived by the measurement data processing unit 132 is passed to the control data processing unit 133. Based on the predicted value, the control data processing unit 133 determines the correction amount (trimming amount) in the subsequent process 34. When the process 34 is performed, the control data processing unit 133 supplies correction amount data for the process 34 to be set in the manufacturing equipment according to the determined correction amount.
[0060] As described above, the method for manufacturing an optical waveguide element of this embodiment makes it possible to solve the problem in conventional methods for manufacturing optical waveguide elements that, due to the limitations of the processing accuracy of various processes, the actually manufactured optical waveguide structure deviates from the target structure, making it impossible to obtain the targeted characteristics. [Industrial Applicability]
[0061] According to the manufacturing method of the optical waveguide element of this embodiment, the optical characteristics of the optical waveguide are predicted based on the measured structural values of the optical waveguide structure formed on the substrate, and the optical waveguide structure is corrected. This is expected to dramatically improve the yield in the optical waveguide manufacturing process and the performance of the optical waveguide compared to conventional methods. [Explanation of symbols]
[0062] 1 Undercladding layer 2. Core layer 3 Overclad layer 10, 20 board 40 Optical waveguide 50 chips 100 calculator 101 Processor 102 Memory 103 Input Device 104 Output Device 105 Communication equipment 106 Storage 132 Measurement data processing section 133 Control data processing section
Claims
1. A method for manufacturing an optical waveguide element, comprising the steps of: Measuring at least one of a height distribution and a width distribution of a core layer of an optical waveguide formed on a substrate; predicting optical properties of a simulated digital twin of the optical waveguide based on the measured structural values; and determining a correction amount for at least one of a height and a width of the core layer of the optical waveguide formed on the substrate, on condition that the predicted optical characteristics are not equal to target optical characteristics, and locally reprocessing at least one of the height and the width of the core layer of the optical waveguide formed on the substrate according to the determined correction amount; forming the substrate on which the optical waveguide is formed into a chip under the condition that the predicted optical characteristics are the target optical characteristics; A manufacturing method comprising:
2. The method of claim 1 , wherein the structural value of at least one of the height distribution and width distribution of the optical waveguide is measured non-invasively for at least one of the height and width.
3. Determining a correction amount for at least one of the height and the width of the core layer of the optical waveguide formed on the substrate includes: Calculating at least one of the structural values of a height and a width of a core layer of the simulated digital twin of the optical waveguide, such that optical characteristics of the digital twin of the optical waveguide simulated based on the measured structural values of the optical waveguide become the target optical characteristics; determining a correction amount for at least one of a height and a width of the core layer of the optical waveguide formed on the substrate based on the calculated structural value of the digital twin of the optical waveguide and the measured structural value; The method of any one of claims 1 to 2, comprising:
4. reprocessing at least one of the height and the width of the core layer of the optical waveguide formed on the substrate according to the determined correction amount, The manufacturing method according to claim 3, further comprising locally reprocessing at least one of a height and a width of the core layer of the optical waveguide formed on the substrate based on the calculated structural values of the digital twin of the optical waveguide and the correction amount determined based on the measured structural values.
5. forming a bonded substrate by directly bonding a substrate that will become an undercladding layer and a substrate that will become the core layer; thinning a substrate that will become the core layer of the bonded substrate; forming the optical waveguide on the bonded substrate in which the substrate that will become the core layer has been thinned; Further equipped 4. The manufacturing method according to claim 1, wherein measuring a structural value of a distribution of heights of the core layer of the optical waveguide formed in the substrate includes measuring a distribution of a film thickness of a substrate that becomes the thinned core layer of the bonded substrate before the optical waveguide is formed in the bonded substrate.
Citation Information
Patent Citations
Phase matching and coupling length adjusting hethod
JP1981027105A
Manufacturing system
JP1988249328A
Semiconductor manufacturing system
JP1998163080A
Manufacture of optical waveguide type filter, and optical waveguide filter
JP1998307220A
Method of manufacturing optical waveguide, optical waveguide device using the method, and waveguide type optical multiplexer / Demultiplexer
JP2003232948A