Electrochemical system and method for manufacturing oxygen electrode of electrochemical system
A composite Ni-TiO material with specific composition improves the durability of oxygen electrodes in electrochemical systems by stabilizing active sites, addressing the deterioration issue in nickel-based electrodes.
Patent Information
- Application Number
- JP2020168019
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-10-02
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2040-10-02
AI Technical Summary
Nickel-based oxygen electrodes in electrochemical systems deteriorate easily during repeated oxygen generation or reduction.
Using a composite material of Ni and TiOx with a predetermined composition, specifically Ni-TiO with 1.99
The Ni-TiO composite material enhances the durability of the oxygen electrode, maintaining its activity and stability in electrochemical systems.
Smart Images

Figure 0007561419000001 
Figure 0007561419000002
Abstract
Description
[Technical field]
[0001] The present invention relates to an electrochemical system and a method for manufacturing an oxygen electrode of an electrochemical system. [Background technology]
[0002] Electrochemical systems such as alkaline water electrolysis devices and alkaline fuel cells include an oxygen electrode, which serves as a cathode electrode for reducing oxygen or an anode electrode for generating oxygen.
[0003] In an electrochemical system, the electrode material of the oxygen electrode is a very important factor in terms of electrolysis performance, durability, etc. As a conventional general oxygen electrode, for example, as described in Patent Document 1, a nickel-based material has been used. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 55-011132 Summary of the Invention [Problem to be solved by the invention]
[0005] However, an oxygen electrode made of a nickel-based material has a problem in that it easily deteriorates during repeated oxygen generation or oxygen reduction.
[0006] In order to solve such problems, an object of the present invention is to provide an electrochemical system equipped with an oxygen electrode having good durability. [Means for solving the problem]
[0007] As a result of extensive research, the present inventors have found that by using a composite material of Ni and TiOx with a specific composition, it is possible to provide an oxygen electrode for an electrochemical system having good durability.
[0008] The above problems are solved by the present invention specified as follows. (1) An electrochemical system having a cathode electrode and an anode electrode, wherein either one of the cathode electrode and the anode electrode is an oxygen electrode, the oxygen electrode is a composite material of Ni and TiO x and is composed of Ni-TiO x wherein in the formula, 1.99 < x ≤ 2.00 and it contains 0.9 to 1.0 at% of Ni, an electrochemical system. (2) The electrochemical system is an alkaline water electrolyzer, and the oxygen electrode is the anode electrode of the alkaline water electrolyzer, the electrochemical system according to (1). (3) The electrochemical system is an alkaline fuel cell, and the oxygen electrode is the air electrode of the alkaline fuel cell, the electrochemical system according to (1). (4) A method for manufacturing the oxygen electrode of the electrochemical system according to any one of (1) to (3), comprising adding a powder of nickel oxide to a powder of titanium oxide, mixing them, firing at 1330 to 1370 °C for 40 to 80 minutes, and then molding.
Advantages of the Invention
[0009] According to the present invention, an electrochemical system provided with an oxygen electrode having good durability can be provided.
Brief Description of the Drawings
[0010] [Figure 1] It is a schematic diagram of an alkaline water electrolyzer according to an embodiment of the present invention. [Diagram 2] It is a schematic diagram of an alkaline fuel cell according to an embodiment of the present invention.
Embodiments for Carrying Out the Invention
[0011] Next, embodiments for carrying out the present invention will be described in detail with reference to the drawings. It should be understood that the present invention is not limited to the following embodiments, and design changes, improvements, etc. can be appropriately made based on the ordinary knowledge of those skilled in the art without departing from the spirit of the present invention.
[0012] <Electrochemical system> The electrochemical system according to an embodiment of the present invention is an electrochemical system having a cathode electrode and an anode electrode, wherein either the cathode electrode or the anode electrode is an oxygen electrode, and the oxygen electrode is a composite material of Ni and TiO x and is composed of Ni-TiO x wherein 1.99 < x ≤ 2.00 and contains 0.9 to 1.0 at% of Ni. In the oxygen electrode, since "x" of TiO x is 1.99 < x ≤ 2.00, the physical properties approach those of so-called valve metal oxides or insulators, and the stability becomes good. Also, while the active sites of the catalyst are imparted to TiO x by Ni, Ni is covered with a stable material (TiO x ), so due to the advantageous relationship between the two, activity is observed while the durability of the electrochemical system is considered to be improved.
[0013] Examples of the electrochemical system include an alkaline water electrolyzer and an alkaline fuel cell, and specific embodiments thereof will be described in detail below.
[0014] <Alkaline water electrolyzer> FIG. 1 is a schematic diagram of an alkaline water electrolyzer 20 according to an embodiment of the present invention. The alkaline water electrolyzer 20 has an anode chamber 22 provided with an anode electrode 24, a cathode chamber 21 provided with a cathode electrode 23, and a diaphragm 25 that partitions the anode chamber 22 and the cathode chamber 21.
[0015] In the alkaline water electrolyzer 20, the following reactions occur as the cathode reaction, anode reaction, and electrolyzer reaction, respectively, as shown in the following reaction formulas. Cathode reaction: 2H2O + 2e -→ H2 + 2OH - Anode reaction: 2OH - → H2O → 1 / 2O2 + 2e - Electrolyzer reaction: H2O → H2 + 1 / 2O2
[0016] For the cathode electrode 23 and the diaphragm 25 of the alkaline water electrolyzer 20 according to the embodiment of the present invention, in the technical field related to the electrolysis device of alkaline water, those with known configurations can be used respectively. Specifically, for the cathode electrode 23, known materials can be used, for example, it can be composed of iron-based materials, nickel-based materials, etc. For the diaphragm 25, known materials can be used, for example, it can be composed of asbestos, polymer-reinforced asbestos, PTFE-bonded potassium titanate, PTFE-bonded zirconia, polysulfone-bonded polyantimonate / antimony oxide, sintered nickel, ceramics / nickel oxide-coated nickel, polysulfone, etc.
[0017] In the alkaline water electrolyzer 20 according to the embodiment of the present invention, as the alkaline water 26 to be electrolyzed, an aqueous sodium hydroxide solution, an aqueous potassium hydroxide solution, etc. can be used. In particular, an aqueous potassium hydroxide solution of 20 - 30 mass% can be used.
[0018] As the anode electrode 24 of the alkaline water electrolyzer 20 according to the embodiment of the present invention, as described above, a composite material of Ni and TiO x Ni - TiO x which is composed of, where 1.99 < x ≦ 2.00 and contains 0.9 - 1.0 at% of Ni, is used as the oxygen electrode of the electrochemical system according to the embodiment of the present invention. According to such a configuration, the durability of the oxygen electrode against the repetition of oxygen generation in the electrochemical system is improved.
[0019] <Alkaline fuel cell> 2 is a schematic diagram of an alkaline fuel cell 40 according to an embodiment of the present invention. The alkaline fuel cell 40 includes an anion exchange electrolyte membrane 41, and a cathode electrode 43 and an anode electrode 44 provided on each surface of the anion exchange electrolyte membrane 41.
[0020] In an alkaline fuel cell 40, the anode electrode 44 functions as a fuel electrode, and the cathode electrode 43 functions as an air electrode (oxygen electrode). An anion exchange electrolyte membrane 41, through which hydroxide ions can pass, is sandwiched between the anode electrode 44 and the cathode electrode 43 and used as an electrolyte. When hydrogen gas, which serves as a fuel, is supplied to the anode electrode 44, and oxygen gas and H2O are supplied to the cathode electrode 43, the cathode reaction and the anode reaction shown in the following reaction formula proceed at each electrode, resulting in a cell reaction. Hydroxide ions produced by the cathode reaction pass through the anion exchange electrolyte membrane 41 and move to the cathode electrode 43. At the cathode electrode 43, a reaction to produce water proceeds.
[0021] Cathodic reaction: 3 / 2O2 + 3H2O + 6e - → 6OH - Anode reaction: 3H2+ 6OH - → 6H2O + 6e - Battery reaction: H2+ 1 / 2O2 → H2O
[0022] The anion exchange electrolyte membrane 41 and the anode electrode 44 of the alkaline fuel cell 40 according to the embodiment of the present invention may each have a known configuration. Specifically, the anion exchange electrolyte membrane 41 may be made of a known material, such as an A201 membrane or A901 membrane manufactured by Tokuyama Corporation. The anode electrode 44 may be made of a known material, such as an iron-based material or a nickel-based material.
[0023] As described above, the cathode electrode 43 of the alkaline fuel cell 40 according to the embodiment of the present invention is made of Ni and TiO x Ni-TiO xIt is composed of, where 1.99 < x ≤ 2.00 and contains 0.9 to 1.0 at% of Ni, and the oxygen electrode of the electrochemical system according to the embodiment of the present invention is used. According to such a configuration, the durability of the oxygen electrode against the repetition of oxygen reduction in the electrochemical system is improved.
[0024] <Manufacturing Method of Oxygen Electrode of Electrochemical System> Next, the manufacturing method of the oxygen electrode of the electrochemical system according to the embodiment of the present invention will be described in detail. First, nickel oxide powder is added to titanium oxide powder. At this time, the charging ratio of titanium oxide to nickel oxide is titanium oxide: nickel oxide = 99.0 to 99.1 at%: 0.9 to 1.0 at%.
[0025] Next, the titanium oxide powder and the nickel oxide powder are mixed by a ball mill. Subsequently, firing is performed at 1330 to 1370 °C for 40 to 80 minutes. The firing is preferably carried out under oxygen-deficient conditions. After firing, it is molded into a rod shape or the like. Thereby, the oxygen electrode of the electrochemical system according to the embodiment of the present invention is obtained.
Example
[0026] The present invention will be described in more detail with reference to the following examples, but the present invention is not limited thereto.
[0027] (Example 1) First, nickel oxide powder was added to titanium oxide powder. At this time, the charging ratio of titanium oxide to nickel oxide was titanium oxide: nickel oxide = 99.0 at%: 1.0 at%. Next, the titanium oxide powder and the nickel oxide powder were mixed by a ball mill, and subsequently, firing was performed at 1350 °C for 60 minutes under an oxygen-deficient state. Also, the fired sample was molded into a rod shape to obtain an oxygen electrode.
[0028] Next, using the obtained oxygen electrode, SSV was carried out under the following conditions to evaluate the electrochemical characteristics related to the oxygen generation reaction. <SSV:Slow Scan Voltammetry> · Electrochemical system: three - electrode cell · Reference electrode: Reversible hydrogen electrode (RHE) · Counter electrode: glassy carbon plate · Working electrode: oxygen electrode prepared in Example 1 · Electrolyte: 7.0 M KOH · Voltage range: 1.2 - 2.0 V vs. RHE · Scanning rate: 5 mV / s -1
[0029] <TG analysis> For Example 1, before and after the above - mentioned electrochemical measurement, thermogravimetric differential thermal analysis (TG - DTA: ThermoGravimeter - Differential Thermal Analyzer) was performed on the oxygen electrode. Details of the apparatus and measurement conditions are shown below. · TG apparatus: Thermo plus EVO TG 8120 manufactured by Rigaku · Heating rate: 10.0 °C / min · Temperature range: 20 - 1000 °C As a result, it was found that the value of "x" in Ni - TiOx was 1.99 < x ≤ 2.00.
[0030] <XPS surface analysis> For Example 1, before and after the above - mentioned electrochemical measurement, surface analysis by X - ray photoelectron spectroscopy (XPS: X - ray Photoelectron Spectroscopy) was performed on the oxygen electrode using XPS QuanteraSXM manufactured by ULVAC - PHI, Inc. as an X - ray photoelectron spectrometer under the following conditions. · X - ray source: monochromatic Al (1486.6 eV) · Detection area: 100 μmφ · Detection depth: about 4 - 5 nm (take - off angle 45°) As a result, it was found that the doping amount of Ni was 0.9 - 1.0 at%.
[0031] <Deterioration test (durability evaluation test)> Regarding Example 1, a deterioration test was carried out on the oxygen electrode before and after the above-mentioned electrochemical measurement using the following device. Electrochemical system: Three-electrode cell Reference electrode: Reversible hydrogen electrode (RHE) Counter electrode: Glassy carbon plate Working electrode: the oxygen electrode prepared in Example 1 ·Electrolyte: 7.0M KOH Voltage range: 0~2.0V vs. RHE Scanning speed: 1Vs -1
[0032] The deterioration test was carried out by carrying out the above-mentioned SSV and then electrolysis using the following device, which was counted as one cycle. The current density was evaluated after a total of 5,000, 10,000, 15,000, and 20,000 cycles, and it was found that in Example 1, even with an increase in the number of cycles, the decrease in current density relative to voltage was suppressed, and the material had good durability. [Explanation of symbols]
[0033] 20. Alkaline water electrolysis equipment 21 Cathode chamber 22 Anode chamber 23 Cathode electrode 24 Anode electrode (oxygen electrode) 25 Diaphragm 26. Alkaline Water 40 Alkaline fuel cell 41 Anion-conducting electrolyte membrane 43 Cathode electrode (oxygen electrode) 44 Anode electrode
Claims
1. 1. An electrochemical system having a cathode electrode and an anode electrode, One of the cathode electrode and the anode electrode is an oxygen electrode, The oxygen electrode is made of Ni and TiO x A composite material with Ni-TiO x wherein in the formula, 1.99<x≦2.00, and the total content of all elements including Ni, Ti, and O is 0.9 to 1.0 at % Ni.
2. the electrochemical system is an alkaline water electrolysis apparatus; 2. The electrochemical system according to claim 1, wherein the oxygen electrode is an anode electrode of the alkaline water electrolysis device.
3. the electrochemical system is an alkaline fuel cell; 2. The electrochemical system of claim 1, wherein the oxygen electrode is an air electrode of the alkaline fuel cell.
4. The method for producing an oxygen electrode of an electrochemical system according to any one of claims 1 to 3, comprising the steps of: adding nickel oxide powder to titanium oxide powder, mixing the mixture, baking the mixture at 1330 to 1370°C for 40 to 80 minutes under oxygen-deficient conditions, and then molding the mixture to produce the oxygen electrode.
Citation Information
Patent Citations
Electrode for electrolysis of water
JP1980011132A
Electrochemical apparatus with insoluble electrode
JP1982149480A
Fuel electrode for solid oxide fuel cell and its manufacturing method
JP2005166481A
Electrode for photolytic water decomposition reaction using photocatalyst
JP2011131170A