Semiconductor device and method for manufacturing the same

By forming a doped polysilicon film on the trench sidewalls and using a two-layer polysilicon structure, the semiconductor device addresses the issues of thinning and electric field concentration, maintaining consistent capacitance and voltage withstand in trench capacitors.

JP7561541B2Active Publication Date: 2024-10-04LAPIS SEMICON CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2020141463
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-08-25
Publication Date
2024-10-04
Estimated Expiration
2040-08-25

AI Technical Summary

Technical Problem

The formation of fine irregularities on the sidewalls of trenches in semiconductor substrates during dry etching leads to thinning of the capacitive insulating film and concentration of the electric field, resulting in decreased withstand voltage and fluctuating capacitance of trench capacitors, especially as trench dimensions become smaller and aspect ratios increase.

Method used

A semiconductor device is designed with a polysilicon film doped with impurities formed on the inner wall of the trench to cover acute-angled portions, and a capacitive insulating film is formed on this polysilicon film, preventing thinning and electric field concentration, while using a two-layer polysilicon structure to maintain consistent capacitance characteristics.

Benefits of technology

The solution suppresses the decrease in withstand voltage and fluctuation of capacitance in trench capacitors, ensuring stable operation regardless of applied voltage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007561541000001
    Figure 0007561541000001
  • Figure 0007561541000002
    Figure 0007561541000002
  • Figure 0007561541000003
    Figure 0007561541000003
Patent Text Reader

Abstract

To provide a semiconductor device in which the decrease in withstanding voltage of a capacitance insulating film can be suppressed and the variation in capacitance of a trench capacitor depending on the applied voltage can be suppressed.SOLUTION: A semiconductor device includes a semiconductor substrate, a semiconductor film covering an inner wall surface of a trench formed extending from one surface of the semiconductor substrate to the inside, formed extending from the inner wall surface to the one surface of the semiconductor substrate continuously, and doped with impurities, a counter electrode including a first part provided at a position facing the semiconductor substrate with the semiconductor film interposed therebetween and extending to the one surface of the semiconductor substrate, and a second part extending to fill the trench continuing from the first part, and an insulating film insulating between the semiconductor film and the counter electrode.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a semiconductor device and a method for manufacturing the semiconductor device. [Background technology]

[0002] With the improvement of semiconductor manufacturing technology, the density is increasing by mounting more and more high-performance elements per unit area (unit information projection area) in a circuit. For capacitor elements used in semiconductor memories, etc., a method is known in which a groove shape (trench) is formed in a semiconductor substrate to form a three-dimensional structure to increase the surface area and increase the capacitance density per unit area (for example, Patent Document 1 and Patent Document 2). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2009-141307 A [Patent Document 2] JP 2005-142549 A Summary of the Invention [Problem to be solved by the invention]

[0004] Dry etching is generally used to form trenches in semiconductor substrates. In dry etching, efforts are made to make the sidewalls of the trench as smooth as possible. However, the surface of the sidewalls is not necessarily completely smooth, and minute irregularities that can be recognized as surface roughness may occur.

[0005] When a capacitive insulating film constituting a trench capacitor is formed directly on the sidewall of a trench having such fine unevenness, the film formation characteristics of the insulating film cause the capacitive insulating film to become thinner at the acute-angled portions of the fine unevenness structure. The thinning causes a decrease in the breakdown voltage of the capacitive insulating film. Furthermore, when a voltage is applied to the opposing electrode during device operation, an electric field concentrates at the acute-angled portions of the fine unevenness structure. This concentration of the electric field also causes a problem of a decrease in the breakdown voltage of the capacitive insulating film.

[0006] In addition, when a trench capacitor is formed directly in a low impurity concentration region of a semiconductor substrate as in the above-mentioned conventional technology, a characteristic that the capacitance varies depending on the voltage applied to the opposing electrode (so-called CV characteristic of a MOS capacitor) occurs. In order to prevent such a characteristic from occurring, a high impurity concentration region is formed around the formation region of the trench capacitor by ion implantation or the like, or a high impurity concentration region is formed near the surface of the sidewall and bottom of the trench by oblique rotation ion implantation. However, when these countermeasures are used, there is a problem that it becomes difficult to implement as the aspect ratio of the trench increases due to the progress of miniaturization of the trench capacitor, narrowing the opening width, and deepening the depth.

[0007] The present invention has been made in consideration of the above problems, and aims to provide a semiconductor device that can suppress a decrease in the breakdown voltage of a capacitive insulating film and suppress fluctuations in the capacitance of a trench capacitor according to an applied voltage. [Means for solving the problem]

[0008] The semiconductor device of the present invention is characterized by comprising: a semiconductor substrate; a semiconductor film doped with impurities, the semiconductor film covering an inner wall surface of a trench formed to extend inward from one surface of the semiconductor substrate and extending continuously from the inner wall surface into the first surface of the semiconductor substrate; a counter electrode provided at a position facing the semiconductor substrate across the semiconductor film, the counter electrode having a first portion extending into the first surface of the semiconductor substrate and a second portion extending continuously from the first portion so as to fill the trench; and an insulating film insulating the semiconductor film from the counter electrode.

[0009] Furthermore, a method for manufacturing a semiconductor device according to the present invention is characterized by including the steps of: forming a trench extending inward from one surface of a semiconductor substrate by dry etching; forming an impurity-doped semiconductor film so as to cover an inner wall surface of the trench and extend continuously from the inner wall surface onto the first surface of the semiconductor substrate; forming an insulating film on a surface of the semiconductor film; and forming a counter electrode on the insulating film, the counter electrode having a first portion extending onto the first surface of the semiconductor substrate and a second portion extending continuously from the first portion so as to fill the trench. Effect of the Invention

[0010] According to the semiconductor device of the present invention, it is possible to suppress a decrease in the breakdown voltage of the capacitive insulating film and to suppress a variation in the capacitance of the trench capacitor according to an applied voltage. [Brief description of the drawings]

[0011] [Figure 1] 1 is a cross-sectional view showing a structure of a semiconductor device according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is an enlarged view of the area enclosed by the dashed line in FIG. [Diagram 3] 3 is a flowchart showing a manufacturing procedure of the semiconductor device according to the first embodiment. [Figure 4] FIG. 11 is a cross-sectional view showing a structure of a trench capacitor according to a second embodiment of the present invention. [Diagram 5] 10 is a cross-sectional view showing a part of the surface of the trench capacitor in a process of forming a capacitive insulating film according to Example 2 of the present invention. [Figure 6] 11 is a cross-sectional view showing a part of the surface of the trench capacitor according to Example 2 of the present invention after thermal annealing treatment. FIG. [Figure 7] 10 is a flowchart showing a manufacturing procedure of a semiconductor device according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Preferred embodiments of the present invention will now be described in detail. In the following description of each embodiment and in the accompanying drawings, the same reference numerals are used to designate substantially the same or equivalent parts. EXAMPLES

[0013] 1 is a cross-sectional view showing a configuration of a semiconductor device 100 according to a first embodiment of the present invention. The semiconductor device 100 includes a semiconductor substrate 10 and a counter electrode 11. A trench capacitor TC is formed in the semiconductor substrate 10.

[0014] The semiconductor substrate 10 is made of, for example, a silicon (Si) substrate. A polysilicon film 12 and a capacitive insulating film 13 are formed on a surface of the semiconductor substrate 10 that constitutes an element mounting region (hereinafter referred to as the first surface).

[0015] A groove-shaped recess (hereinafter referred to as trench T1) extending inward is formed on one surface of the semiconductor substrate 10. The trench T1, together with a polysilicon film 12 and a capacitive insulating film 13 formed on the surface, constitutes a trench capacitor TC.

[0016] The trench T1 is formed by performing trench processing on the semiconductor substrate 10 by dry etching. A fine uneven portion is formed on the surface of the sidewall of the trench T1. The uneven portion is made of an irregular uneven structure that is recognized as surface roughness and has an acute angle shape. In the following description, such a fine uneven portion is referred to as a fine uneven portion.

[0017] The counter electrode 11 is made of polysilicon (Poly-Si). The counter electrode 11 is formed to face the semiconductor substrate 10 via the capacitive insulating film 13 and the polysilicon film 12. The counter electrode 11 has a flat portion (first portion) formed to extend on one surface of the semiconductor substrate 10, and a portion (second portion) extending continuously from the flat portion toward the inside of the semiconductor substrate 10 to fill the trenches of the semiconductor substrate 10.

[0018] The polysilicon film 12 is a semiconductor film formed to cover the inner surface (particularly the sidewall surface) of the trench T1 and extend to one surface of the semiconductor substrate 10. In this embodiment, the polysilicon film 12 is composed of a polysilicon film made of polysilicon doped with impurities (doped Poly-Si). The polysilicon film 12 is formed by depositing polysilicon on the surface of the semiconductor substrate 10 including the inner wall of the trench T1 using the LP-CVD method (i.e., low-pressure CVD method). In this embodiment, the polysilicon film 12 is formed as a polysilicon film doped with impurities (doped polysilicon film) by introducing impurities for increasing conductivity into the source gas during the deposition of the polysilicon film by the LP-CVD method.

[0019] The capacitive insulating film 13 is an insulating film provided between the counter electrode 11 and the polysilicon film 12. The capacitive insulating film 13 is formed on the surface of the polysilicon film 12, and is formed so as to cover the inner surface of the trench T1 and extend onto one surface of the semiconductor substrate 10. The capacitive insulating film 13 is made of an insulating film such as a silicon nitride (SiN) film, and is formed by depositing SiN directly on the surface of the polysilicon film 12 by, for example, the LP-CVD method.

[0020] A contact CT1 is provided on one surface of the semiconductor substrate 10. The contact CT1 is a substrate-side contact to which a voltage is applied, and is connected to the semiconductor substrate 10 via a polysilicon film 12.

[0021] A contact CT2 is provided on the surface of the flat plate portion of the counter electrode 11 (the surface opposite to the surface facing the semiconductor substrate 10). The contact CT2 is a contact on the electrode side to which a voltage is applied, and is connected to the counter electrode 11. The contacts CT1 and CT2 are made of a conductor such as tungsten.

[0022] Fig. 2 is an enlarged view of a portion A1 enclosed by a dashed line in Fig. 1. Here, hatching of the semiconductor substrate 10 is omitted.

[0023] As described above, a fine unevenness is formed on the sidewall of the trench T1 formed by dry etching. The fine unevenness includes, for example, as shown in Fig. 2, a portion (referred to as a recessed shape CS) recessed toward the semiconductor substrate 10 and a pointed portion (referred to as a pointed shape PS) on the sidewall surface of the trench T1. In this embodiment, the recessed shape CS has a certain size larger than the film thickness of the polysilicon film 12 and the capacitive insulating film 13. The tip shape PS has a size smaller than the film thickness of the polysilicon film 12.

[0024] Due to the film formation characteristics of LP-CVD, the polysilicon film 12 is formed so as to cover the sidewall surface of the trench T1 along the uneven shape of the fine unevenness. For example, in the recess shape CS, the polysilicon film 12 is formed along the uneven shape, and the capacitive insulating film 13 is further formed thereon. On the other hand, in the pointed shape PS, the polysilicon film 12 is formed so as to fill the pointed recess recessed toward the semiconductor substrate 10. This smoothes the surface of the sidewall portion of the trench T1.

[0025] Next, a method for manufacturing the semiconductor device 100 of this embodiment will be described with reference to the flow chart of FIG.

[0026] First, a trench is formed by dry etching the semiconductor substrate 10 (STEP 101), thereby forming a trench T1.

[0027] Next, polysilicon is formed on the surface of the semiconductor substrate 10 including the inner wall of the trench by LP-CVD while doping with impurities (STEP 102). This forms a polysilicon film 12 which is a polysilicon film doped with impurities.

[0028] Next, a silicon nitride film (SiN) is formed on the surface of the polysilicon film 12 by LP-CVD (STEP 103). At this time, patterning is performed so that a part of the polysilicon film 12 is exposed on the wafer surface at the position where the contact CT1 is to be formed, and then the silicon nitride film is formed. As a result, the capacitive insulating film 13 is formed.

[0029] Next, a polysilicon layer is formed on the surface of the capacitive insulating film 13 so as to fill the inside of the trench T1 and extend over one surface of the semiconductor substrate 10. This forms the counter electrode 11 made of polysilicon (STEP 104).

[0030] Next, contact holes are formed in the surface of the polysilicon film 12 exposed on the wafer surface and in the surface of the counter electrode 11, and the contact holes are filled with a conductor such as tungsten, thereby forming contacts CT1 and CT2 (STEP 105).

[0031] Through the steps described above, the semiconductor device 100 of this embodiment is manufactured.

[0032] In the semiconductor device 100 of this embodiment, a polysilicon film 12 is formed on the surface of the sidewall portion of the trench T1, and a capacitive insulating film 13 is further formed thereon. Therefore, in the semiconductor device 100 of this embodiment, the withstand voltage of the capacitive insulating film 13 in the trench capacitor TC is higher than in the case where a similar polysilicon film is not formed.

[0033] If a polysilicon film is not formed and a capacitive insulating film is formed directly on the sidewall surface of the trench, the capacitive insulating film is partially thinned at the acute-angled portion of the fine unevenness on the sidewall surface of the trench (for example, near the tip of the bent portion of the recess shape CS shown in FIG. 2). Furthermore, when a voltage is applied to the opposing electrode via a contact, an electric field is concentrated at the acute-angled portion of the fine unevenness. If a polysilicon film is not formed as in this embodiment, the partial thinning of the capacitive insulating film and the electric field concentration at the acute-angled portion when a voltage is applied reduce the breakdown voltage of the capacitive insulating film.

[0034] In contrast to this, in the semiconductor device 100 of this embodiment, the polysilicon film 12 is formed so as to cover the acute-angled portions of the concave shape CS of the fine concave-convex portion of the trench T1. In addition, since the peak shape PS of the fine concave-convex portion is smaller than the film thickness of the polysilicon film 12, it is embedded in the polysilicon film 12 and smoothed.

[0035] The capacitive insulating film 13 is formed on the surface of the polysilicon film 12, and is not formed directly on the sidewall surface of the trench T1. Therefore, the capacitive insulating film 13 is not partially thinned, and electric field concentration does not occur when a voltage is applied.

[0036] In this embodiment, the capacitive insulating film 13 is formed on the surface of the impurity-doped polysilicon film 12. If, unlike this embodiment, a non-doped polysilicon film were used instead of the polysilicon film 12, a characteristic would occur in which the capacitance of the trench capacitor varies depending on the value of the applied voltage when a voltage is applied to the opposing electrode 11 (the so-called CV characteristic of a MOS capacitor).

[0037] However, in the semiconductor device 100 of this embodiment, since the impurity-doped polysilicon film 12 is used instead of the non-doped polysilicon film, the trench capacitor TC operates as a MOS capacitor in charge accumulation mode regardless of the applied voltage when a voltage is applied to the opposing electrode 11. That is, in the trench capacitor TC of this embodiment, a roughly constant capacitance characteristic is obtained regardless of the voltage applied to the opposing electrode 11.

[0038] As described above, according to the semiconductor device 100 of this embodiment, there is no decrease in the breakdown voltage of the capacitive insulating film 13 due to thinning of the capacitive insulating film 13 or electric field concentration during voltage application. Furthermore, according to the semiconductor device 100 of this embodiment, there is no variation in the capacitance of the trench capacitor TC according to the applied voltage.

[0039] Therefore, according to the semiconductor device 100 of this embodiment, it is possible to suppress a decrease in the breakdown voltage of the capacitive insulating film and to suppress a variation in the capacitance of the trench capacitor according to the applied voltage. EXAMPLES

[0040] Next, a description will be given of a second embodiment of the present invention. Fig. 4 is a cross-sectional view showing the configuration of a semiconductor device 200 according to the second embodiment of the present invention.

[0041] In the semiconductor device 200 of this embodiment, the polysilicon film 14 is formed by sequentially forming a first polysilicon film doped with impurities and a second non-doped polysilicon film on the surface of the semiconductor substrate 10 including the sidewall of the trench T1, and then performing a thermal annealing process to cause the impurities in the first polysilicon film to diffuse into the second polysilicon film in a solid phase. Therefore, the polysilicon film 14 of this embodiment is formed thicker (for example, about twice as thick) than the polysilicon film 12 of the first embodiment.

[0042] FIG. 5 is an enlarged cross-sectional view of a portion (a portion A1 surrounded by a dashed line in FIG. 4) of the trench T1 before the thermal annealing treatment is performed.

[0043] A first polysilicon film 15 doped with impurities is formed on the surface of the semiconductor substrate 10 inside the trench. Furthermore, a second polysilicon film 16, which is a non-doped polysilicon film, is formed on the surface of the first polysilicon film 15, and a capacitive insulating film 13 is formed on the surface of the second polysilicon film 16.

[0044] FIG. 6 is an enlarged cross-sectional view showing a part (a part A1 surrounded by a dashed line in FIG. 4) of the trench T1 after the thermal annealing treatment.

[0045] 5, the thermal annealing process causes the impurities in the first polysilicon film 15 to diffuse into the second polysilicon film 16 in a solid phase, and the entire film having a two-layer structure of non-doped polysilicon / doped polysilicon is converted into doped polysilicon. As a result, as shown in FIG 6, a polysilicon film 14 doped with impurities is formed on the surface of the semiconductor substrate 10 to a thickness equivalent to two layers, and a capacitive insulating film 13 is formed on the surface of the polysilicon film 14.

[0046] Next, a method for manufacturing the semiconductor device 200 of this embodiment will be described with reference to the flow chart of FIG.

[0047] First, a trench is formed by dry etching the semiconductor substrate 10 (STEP 201), thereby forming a trench T1.

[0048] Next, polysilicon is formed on the surface of the semiconductor substrate 10 including the inner wall of the trench by LP-CVD while doping with impurities (STEP 202). This forms a first polysilicon film 15, which is a polysilicon film doped with impurities.

[0049] Next, polysilicon is further formed on the surface of the first polysilicon film 15 by LP-CVD (STEP 203). At this time, unlike STEP 202, no impurities are introduced. As a result, a second polysilicon film 16, which is a non-doped polysilicon film, is formed.

[0050] Next, a silicon nitride film (SiN) is formed on the surface of the second polysilicon film 16 by LP-CVD (STEP 204), thereby forming the capacitive insulating film 13.

[0051] Next, a thermal annealing process is performed on the semiconductor substrate 10 on which the impurity-doped first polysilicon film 15, the non-doped second polysilicon film 16, and the capacitive insulating film 13 are sequentially formed on the surface (STEP 205). As a result, the impurities in the first polysilicon film 15 are solid-phase diffused into the second polysilicon film 16, and both the first polysilicon film 15 and the second polysilicon film 16 become polysilicon films doped with impurities. That is, the entire film having a two-layer structure of non-doped polysilicon and doped polysilicon (polysilicon doped with impurities) becomes doped polysilicon to become the polysilicon film 14.

[0052] Next, a polysilicon layer is formed on the surface of the capacitive insulating film 13 so as to fill the inside of the trench T1 and extend over one surface of the semiconductor substrate 10. This forms the counter electrode 11 made of polysilicon (STEP 206).

[0053] Next, contact holes are formed in the surface of the polysilicon film 14 exposed on the wafer surface and in the surface of the counter electrode 11, and the contact holes are filled with a conductor such as tungsten, thereby forming contacts CT1 and CT2 (STEP 207).

[0054] Through the above-described steps, the semiconductor device 200 of this embodiment is manufactured.

[0055] In this embodiment, a first polysilicon film 15 doped with impurities and a second non-doped polysilicon film 16 are formed in sequence, and the capacitive insulating film 13 is formed on the surface of the non-doped polysilicon film 16. Then, a thermal annealing process is performed so that the entire two-layer polysilicon film becomes a polysilicon film doped with impurities. That is, at the stage of forming the capacitive insulating film 13, the underlying surface is the second polysilicon film 16, which is a non-doped polysilicon film.

[0056] Unlike the present embodiment, if the capacitive insulating film is directly formed on the surface of the polysilicon film doped with impurities, the film formation characteristics of the capacitive insulating film may be locally affected at the locations where the impurity atoms are exposed on the surface of the polysilicon film, which may result in a deterioration in the film quality of the capacitive insulating film and a decrease in the breakdown voltage.

[0057] However, according to the manufacturing method of this embodiment, when the capacitive insulating film 13 is formed, the surface of the base is the undoped second polysilicon film 16, so that no impurity atoms are present on the surface of the base. This makes it possible to avoid degradation of the film quality of the capacitive insulating film 13 due to the influence of the impurity atoms.

[0058] In this embodiment, the non-doped second polysilicon film 16 is changed into the impurity-doped polysilicon film 14 by thermal annealing. If the thermal annealing is not performed and the capacitive insulating film 13 is left in the state formed on the non-doped polysilicon film, a characteristic that the capacitance varies with the voltage when a voltage is applied to the counter electrode 11 (the so-called CV characteristic of a MOS capacitor) occurs.

[0059] However, in the semiconductor device 200 of this embodiment, the non-doped second polysilicon film 16 is changed into the polysilicon film 14 doped with impurities by thermal annealing. Therefore, when a voltage is applied to the counter electrode 11, the trench capacitor TC operates as a MOS capacitor on the charge storage side regardless of the applied voltage. That is, in the trench capacitor TC of this embodiment, a roughly constant capacitance characteristic is obtained regardless of the voltage applied to the counter electrode 11.

[0060] The present invention is not limited to the above-described embodiments. For example, in each of the above-described embodiments, the counter electrode 11 is formed using polysilicon. However, the present invention is not limited to this, and the counter electrode 11 may be formed using a conductive layer made of a material having conductivity other than polysilicon.

[0061] In the above embodiments, a polysilicon film is used as the semiconductor film for covering the acute-angled portion of the concave-convex structure of the trench. However, the present invention is not limited to this, and a semiconductor film other than a polysilicon film may be used.

[0062] In the above embodiment, the trench is formed by dry etching, but the specific method of dry etching is not particularly limited. For example, the trench may be formed by using the Bosch etching technique. [Explanation of symbols]

[0063] 100, 200 Semiconductor device 10. Semiconductor Substrate 11 Counter electrode 12, 14 Polysilicon film 13 Capacitive insulating film 15 First polysilicon film 16 Second polysilicon film

Claims

1. A semiconductor substrate; a semiconductor film doped with an impurity, the semiconductor film covering an inner wall surface of a trench formed to extend inward from one surface of the semiconductor substrate and extending continuously from the inner wall surface to the one surface of the semiconductor substrate; a counter electrode provided at a position facing the semiconductor substrate across the semiconductor film, the counter electrode having a first portion extending onto the first surface of the semiconductor substrate and a second portion extending continuously from the first portion so as to fill the trench; an insulating film that insulates the semiconductor film from the counter electrode; having a first recess having a surface on which the semiconductor film, the counter electrode and the insulating film are formed, and a second recess having a second semiconductor film formed therein,

2. 2. The semiconductor device according to claim 1, wherein the semiconductor film is a polysilicon film formed by using a low pressure CVD method.

3. 3. The semiconductor device according to claim 1, wherein the semiconductor film is formed by subjecting a first polysilicon film doped with impurities and a second non-doped polysilicon film formed in sequence on the inner wall surface of the trench to thermal annealing.

4. 4. The semiconductor device according to claim 1, wherein the trench is formed by dry etching.

5. In the first recess of the trench, the semiconductor film is formed along a shape of the recess, the insulating film is formed on the semiconductor film, and the counter electrode is formed to fill the recess; 5. The semiconductor device according to claim 1, wherein the semiconductor film is formed in the second recess of the trench so as to fill the recess.

6. forming a trench extending inwardly from one surface of a semiconductor substrate by dry etching; forming a semiconductor film doped with an impurity so as to cover an inner wall surface of the trench and extend continuously from the inner wall surface onto the first surface of the semiconductor substrate; forming an insulating film on a surface of the semiconductor film; forming a counter electrode on the insulating film, the counter electrode having a first portion extending on the first surface of the semiconductor substrate and a second portion extending continuously from the first portion so as to fill the trench; Including, a first recess having a surface on which the semiconductor film, the counter electrode, and the insulating film are formed, and a second recess having a second semiconductor film formed therein.

7. 7. The method for manufacturing a semiconductor device according to claim 6, further comprising the step of performing a thermal annealing process after the step of forming the insulating film.

8. The step of forming the semiconductor film includes: A first step of forming a first polysilicon film doped with impurities; a second step of forming a non-doped second polysilicon film on a surface of the first polysilicon film; 8. The method for manufacturing a semiconductor device according to claim 7, further comprising:

9. In the first recess of the trench, the semiconductor film is formed along a shape of the recess, the insulating film is formed on the semiconductor film, and the counter electrode is formed to fill the recess; 9. The method for manufacturing a semiconductor device according to claim 6, wherein the semiconductor film is formed in the second recess of the trench so as to fill the recess.

Citation Information

Patent Citations

  • Semiconductor memory

    JP1988158869A

  • Manufacture of semiconductor device

    JP1991147327A

  • Mis type semiconductor storage device

    JP1993175448A

  • Semiconductor memory and manufacture thereof

    JP1994021387A

  • Capacitor and its manufacture

    JP1994029465A