Wound iron core, method for manufacturing wound iron core, and device for manufacturing wound iron core
By forming grooves on grain-oriented electrical steel sheets at bending areas and applying magnetic domain control strain, wound iron cores achieve reduced iron loss and improved performance without strain relief annealing.
Patent Information
- Application Number
- JP2020067557
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-04-03
- Publication Date
- 2024-10-07
- Estimated Expiration
- 2040-04-03
Smart Images

Figure 0007562280000001 
Figure 0007562280000002 
Figure 0007562280000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a wound iron core, a method for manufacturing a wound iron core, and an apparatus for manufacturing a wound iron core. [Background technology]
[0002] There are two types of iron cores for transformers: stacked cores and wound cores. Of these, wound cores are generally manufactured by stacking grain-oriented electromagnetic steel sheets in layers, winding them into a doughnut shape (wound shape), and then pressurizing the wound body to form it into a roughly rectangular shape. This forming process introduces mechanical processing strain (plastic deformation strain) into the entire grain-oriented electromagnetic steel sheet, and since this processing strain is a factor that significantly deteriorates the iron loss of the grain-oriented electromagnetic steel sheet, it is necessary to perform stress relief annealing.
[0003] The grain-oriented magnetic steel sheet used for the iron core is a grain-oriented magnetic steel sheet in which the axis of easy magnetization is aligned in one direction. Among such grain-oriented magnetic steel sheets, there is a so-called distortion-imparting magnetic domain control material, which is obtained by periodically irradiating the surface of the grain-oriented magnetic steel sheet with a laser in a direction intersecting the rolling direction and performing localized rapid heating (and rapid cooling from rapid heating to room temperature) to introduce a plurality of fine distortions (distortion for magnetic domain control) and subdivide the 180° magnetic domains from the closure magnetic domains generated at the site as the starting point, thereby reducing the iron loss (see, for example, Patent Document 1). However, when a grain-oriented magnetic steel sheet, which is a distortion-imparting magnetic domain control material to which such distortion for magnetic domain control is imparted, is used for a wound iron core, the distortions (including the distortions that are the starting points for magnetic domain control and processing distortions) disappear by performing the above-mentioned distortion relief annealing process, and as a result, the magnetic domain control effect also disappears, and the wound iron core does not have low iron loss. Therefore, the distortion-imparting type magnetic domain control material is generally used only for stacked cores, which do not require the pressure forming or annealing processes.
[0004] In addition, there are also so-called groove-formed magnetic domain control materials, which have a magnetic domain control effect that reduces the iron loss by forming grooves periodically on the surface of the grain-oriented electrical steel sheet in a direction intersecting with the rolling direction, and by using the same effect as the closure magnetic domain, the magnetic domain control effect is subdivided by 180° to reduce the iron loss (see, for example, Patent Document 2). Such groove-formed magnetic domain control materials can be used as materials for wound iron cores because the magnetic domain control effect does not disappear even when they are subjected to strain relief annealing. However, the groove-formed magnetic domain control material has a disadvantage that the iron loss improvement effect (magnetic domain control effect) is smaller than that of the strain-imparting magnetic domain control material. In addition, mechanical processing by a tooth press and chemical processing by etching are used as methods for forming grooves, but these methods have problems such as the need for large-scale machinery and wear of the tooth press compared to non-contact methods of irradiating lasers or electron beams that impart strain for magnetic domain control, and the etching method has problems in terms of cost and production capacity, such as the need for waste liquid treatment and masks. As a groove formation method, groove processing methods that irradiate with a laser, electron beam, etc. have the advantage of being non-contact. However, these groove processing methods using a laser, electron beam, etc. require greater power than methods that impart distortion for magnetic domain control, and therefore, when attempting to process grooves over the entire surface of a grain-oriented electromagnetic steel sheet, there are problems such as increased production capacity and costs.
[0005] In recent years, a method for manufacturing a wound core has become known in which steel sheets are individually folded (in very small numbers, such as one or two sheets) and cut, and these individually folded steel sheets are stacked in multiple layers to form a wound core into a rectangular shape (a wound core manufacturing method called "Unicore"; hereinafter, also referred to as the Unicore manufacturing method). By using this method, the curvature R of the folded portion can be made extremely small, and the value of the curvature R measured on the inside of the steel sheet can be made 3 mm or less, making it possible to limit the range of the processing strain introduced into the steel sheet due to the folding process to only the vicinity of the small folded portion, which is specified so that the curvature R is 3 mm or less. The lower limit of the curvature R is not particularly limited, but depends on the capacity of the folding device, and in reality, it is often about 1 mm. When manufacturing a wound core using this method, since bending is performed locally, processing distortion occurs only in the area near the corners created by the bending, so that the core loss deterioration of the entire wound core can be reduced, and therefore, there is an advantage that distortion-imparting type magnetic domain control material with extremely low core loss can be used as the material for the wound core.
[0006] In other words, as can be seen from the above, distortion-imparting type magnetic domain control materials have the disadvantage that, when used in wound cores, iron loss is not reduced due to the disappearance of distortion associated with the distortion relief annealing process. However, they have the advantage of being more effective in improving iron loss and being less expensive than groove-forming type magnetic domain control materials. Therefore, if wound cores are manufactured using distortion-imparting type magnetic domain control materials using the Unicore method, which can eliminate the distortion relief annealing process, it is possible to eliminate the disadvantages of distortion-imparting type magnetic domain control materials and make full use of their advantages. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] JP 2003-347128 A [Patent Document 2] International Publication No. 2011 / 125672 Summary of the Invention [Problem to be solved by the invention]
[0008] However, even when wound cores are manufactured using a strain-imparting type magnetic domain control material (grained electrical steel sheet with strain-imparting type magnetic domain control) by the Unicore manufacturing method, processing strain (plastic deformation strain) still remains in the corners and their vicinity when bending, causing deterioration in iron loss in such areas. Therefore, there is a demand for improvement in the deterioration in iron loss due to processing strain that remains in the corners and their vicinity when bending.
[0009] The present invention has been made in consideration of the above-mentioned circumstances, and has an object to provide a wound iron core that can be manufactured from a distortion-imparting type magnetic domain control material without a distortion relief annealing process, and that can suppress iron loss deterioration due to processing distortion in the bent portions, a manufacturing method for the wound iron core, and an apparatus for manufacturing the wound iron core. [Means for solving the problem]
[0010] In order to achieve the above-mentioned object, the present invention provides a wound iron core formed by individually bending grain-oriented electromagnetic steel sheets, the grains having on their surfaces magnetic domain control distortion extending in a width direction intersecting the rolling direction, and assembling them into a wound shape, in which grooves extending in the width direction are formed on the surfaces of the grain-oriented electromagnetic steel sheets in the regions that become the bent parts in the bending process and in the vicinity thereof.
[0011] The wound core of the present invention having the above-mentioned configuration is a wound core formed from grain-oriented electromagnetic steel sheets in which iron loss has been improved by imparting magnetic domain control distortion to the surface of the steel sheet to form closure domains, and is formed by stacking each grain-oriented electromagnetic steel sheet, which has been individually folded, in layers and assembling them into a wound shape (manufactured by the Unicore method which does not involve strain relief annealing), and in which a plurality of grooves extending in a direction intersecting the rolling direction of the steel sheet are formed in and near the sites which become the bends in the bending of each grain-oriented electromagnetic steel sheet.
[0012] When bending a grain-oriented electrical steel sheet locally, processing distortion occurs within a range of several mm to several tens of mm from the vicinity of the bent portion. This processing distortion is a factor that deteriorates the iron loss of the grain-oriented electrical steel sheet, and when a grain-oriented electrical steel sheet in which closure magnetic domains are formed with periodic magnetic domain control distortions (multiple magnetic domain control distortions at a predetermined interval from each other) as the starting point and magnetic domain control is performed is used, there is a problem that the iron loss improvement amount is offset. Therefore, the present inventors have focused on the fact that processing distortion occurs near the bent portion due to tension generated mainly in the bending direction from the bent portion as the starting point, and have found that when grooves are periodically formed (multiple grooves are formed at a predetermined interval from each other) in a range of several mm to several tens of mm from the said portion as the center, the iron loss of the entire iron core is improved by several percent. It is estimated that this is because the formation of the grooves relieves stress and relieves the effect of the processing distortion. In addition, since the periodic groove formation has a magnetic domain control effect, it is also considered that this contributes to the improvement of iron loss.
[0013] Methods for forming the grooves include, for example, etching, mechanical pressing, electron beams, lasers, etc. However, etching requires waste liquid treatment, mechanical pressing has a limited life span of the tooth profile, and electron beams require a vacuum chamber, which increases the size and cost of the equipment, so it is preferable to form the grooves by laser processing, which allows non-contact processing in the atmosphere. Furthermore, such grooves formed in and / or near the folded portions of each grain-oriented electrical steel sheet are provided instead of or in addition to distortion for magnetic domain control.
[0014] The present invention also provides a method for manufacturing a wound iron core, comprising: a distortion imparting step of irradiating a surface of a grain-oriented electromagnetic steel sheet with a beam to impart a magnetic domain control distortion extending in a width direction intersecting a rolling direction of the grain-oriented electromagnetic steel sheet; a groove forming step of irradiating the surface of the grain-oriented electromagnetic steel sheet with a beam to form grooves extending in the width direction of the grain-oriented electromagnetic steel sheet; a folding step of individually bending the grain-oriented electromagnetic steel sheets in which the magnetic domain control distortion has been imparted and the grooves have been formed; and an assembling step of assembling the folded grain-oriented electromagnetic steel sheets into a wound shape to form a wound iron core, wherein the distortion imparting step imparts the magnetic domain control distortion in areas of the surface of the grain-oriented electromagnetic steel sheet other than sites that will become bent portions in the bending process and their vicinity, and the groove forming step forms the grooves in sites that will become bent portions in the bending process and their vicinity, on the surface of the grain-oriented electromagnetic steel sheet.
[0015] The present invention also provides a wound iron core manufacturing device comprising: a beam irradiation unit that irradiates a surface of a grain-oriented electromagnetic steel sheet with a beam to impart magnetic domain control strain extending in a width direction intersecting the rolling direction of the grain-oriented electromagnetic steel sheet and forms grooves extending in the width direction of the grain-oriented electromagnetic steel sheet by irradiating the surface of the grain-oriented electromagnetic steel sheet with a beam; a folding processing unit that individually folds the grain-oriented electromagnetic steel sheet in which the magnetic domain control strain has been imparted and the grooves have been formed; and an assembly unit that assembles the folded electromagnetic steel sheets into a wound shape to form a wound iron core, wherein the beam irradiation unit imparts the magnetic domain control strain to areas of the surface of the grain-oriented electromagnetic steel sheet other than sites that will become bent parts in the bending process and their vicinity, and forms the grooves in sites that will become bent parts in the bending process and their vicinity, of the surface of the grain-oriented electromagnetic steel sheet.
[0016] The manufacturing method and device for the wound iron core configured as described above employs a Unicore manufacturing method in which magnetic steel sheets that have not been subjected to magnetic domain control are prepared, and this magnetic steel sheet is irradiated with a beam such as a laser or electron beam to impart distortion for magnetic domain control that serves as the starting point of closure domains, thereby performing magnetic domain control, and each grain-oriented magnetic steel sheet is bent, stacked in layers, and assembled into a wound shape to form the wound iron core.
[0017] In the manufacturing method and manufacturing apparatus having the above configuration, the same beam irradiation device may be used to switch between providing grooves to the surface of the grain-oriented electrical steel sheet and providing distortion for magnetic domain control by changing the irradiation conditions of the beam. Here, examples of the beam irradiated by the beam irradiation device include a laser and an electron beam.
[0018] In addition, in the present invention, a grain-oriented electrical steel sheet having a surface that is irradiated with a beam to impart distortion for magnetic domain control extending in the width direction intersecting the rolling direction may be obtained separately, and grooves may be formed in the grain-oriented electrical steel sheet having distortion for magnetic domain control imparted thereto. Effect of the Invention
[0019] The wound iron core of the present invention is formed by assembling individually bent grain-oriented electromagnetic steel sheets into a doughnut shape (wound shape), so it can be manufactured using a distortion-inducing magnetic domain control material without a distortion relief annealing process.In addition, grooves extending in the width direction of the grain-oriented electromagnetic steel sheet are formed in and near the portions that become the bends in the bending process of the grain-oriented electromagnetic steel sheet, so that iron loss deterioration due to processing distortion in the bent portions can be suppressed. [Brief description of the drawings]
[0020] [Figure 1] FIG. 2 is a perspective view of a wound iron core according to one embodiment of the present invention, including an enlarged layer cross section including linear grooves in the folded portions of each grain-oriented electromagnetic steel sheet that constitutes the wound iron core. [Diagram 2] FIG. 2 is a diagram showing how the iron loss of the wound iron core of the present invention changes when the iron loss of the comparative example is taken as 100. [Diagram 3] 1 is a cross-sectional view showing a form of a groove around a bent portion when a grain-oriented electromagnetic steel sheet constituting a wound iron core according to an embodiment of the present invention is bent. FIG. [Figure 4] FIG. 13 is a diagram showing the relationship between the groove formation range and the iron loss ratio for various groove intervals (laser irradiation pitches). [Diagram 5] 1 is a schematic perspective view of a method and an apparatus for manufacturing a wound iron core according to an embodiment of the present invention; [Figure 6] 1A and 1B are schematic diagrams showing a laser irradiation mode in a wound iron core manufacturing method and manufacturing apparatus according to one embodiment of the present invention, in which (a) shows a laser irradiation apparatus and its scanning direction, and (b) shows a focused beam shape. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS A wound core, a method for manufacturing a wound core, and an apparatus for manufacturing a wound core according to an embodiment of the present invention will be described below with reference to the drawings. FIG. 1 shows a wound core 10 according to an embodiment of the present invention. This wound core 10 has a substantially rectangular parallelepiped shape having a hollow portion 15, and its corners R are locally folded by using the Unicore manufacturing method. The wound core 10 is formed from a plurality of grain-oriented electromagnetic steel sheets 40, in which a plurality of magnetic domain control strains 20 extending linearly or with a curvature in a direction intersecting with the rolling direction (longitudinal direction) D of the grain-oriented electromagnetic steel sheets 40 are applied to the surface of the grain-oriented electromagnetic steel sheets 40, thereby subdividing the magnetic domains by 180° from the closure domains, thereby improving iron loss. The wound core 10 is formed by stacking grain-oriented electromagnetic steel sheets 40 (in this embodiment, the thickness and width are the same) that have been individually folded in layers and assembling them into a doughnut shape (wound shape) (see also FIG. 5). Since the bending process is performed locally, processing strain (plastic deformation strain) occurs only in the vicinity of the bent portion, which reduces deterioration in iron loss of the entire wound iron core 10. Therefore, the grain-oriented electrical steel sheet 40 according to the present embodiment does not need to be subjected to strain relief annealing before or after lamination.
[0022] In addition, the magnetic domain control strain 20 is specifically introduced on the surface of the grain-oriented electromagnetic steel sheet 40 at a predetermined interval Pl (e.g., 4 mm). Closure domains are generated starting from this magnetic domain control strain 20, and the 180° magnetic domains in the longitudinal direction D of the grain-oriented electromagnetic steel sheet 40 are subdivided, resulting in an improvement in iron loss of approximately 10% compared to before the introduction of the magnetic domain control strain 20.
[0023] In addition, in this embodiment, at the corners (i.e., the four corners of the wound iron core 10) when the grain-oriented electromagnetic steel sheet 40 is bent, a plurality of grooves 25 extending linearly or with a curved shape in a direction intersecting the rolling direction D of the grain-oriented electromagnetic steel sheet 40 are formed at predetermined intervals in the bends where the grain-oriented electromagnetic steel sheet is bent and in the area nearby.
[0024] These grooves 25 are formed at intervals Pl of 2 mm to 10 mm on both sides of a portion (top edge; bent portion) R1 where the grain-oriented electromagnetic steel sheet 40 is bent at the corner R, over a range (groove formation range) X of 1 mm to 50 mm along the rolling direction D of the grain-oriented electromagnetic steel sheet 40, when the grain-oriented electromagnetic steel sheet 40 is bent. For example, within the groove formation range X of 25 mm on both sides of the bent portion R1 at the corner R, the grooves 25 can be formed at intervals of 4 mm by laser processing, and the depth of the grooves 25 can be set to 25 μm on average. In FIG. 1, the grooves 25 formed in the bend R1 and the surrounding area (i.e., corresponding to the groove formation range X) are shown by solid lines, and a plurality of magnetic domain control distortions 20 formed over the entire surface of the other grain-oriented electrical steel sheet 40 are shown by some dashed lines.
[0025] Furthermore, the wound iron core 10 according to this embodiment becomes a transformer by, for example, winding a primary winding and a secondary winding (not shown) so that they penetrate the hollow portion 15, and when a current is passed through the primary winding or the secondary winding, a magnetic circuit of magnetic flux circulating around the hollow portion 15, i.e., a closed magnetic circuit, is formed. Furthermore, the grain-oriented electrical steel sheet 40 according to this embodiment has an easy magnetization axis of the crystal grains (body-centered cubic) aligned in the rolling direction D. <100> The grain-oriented electromagnetic steel sheet 40 is an electromagnetic steel sheet in which the direction of magnetization (direction) is nearly uniform, and has a structure in which multiple magnetic domains whose magnetization is oriented in the rolling direction D are arranged with magnetic walls in between. Such grain-oriented electromagnetic steel sheet 40 is suitable as an iron core material for transformers in which magnetic lines of force are oriented in a constant direction. Here, the grain-oriented electromagnetic steel sheet 40 is assembled in the wound iron core 10 so that the axis of easy magnetization of the grain-oriented electromagnetic steel sheet 40 corresponds to the circumferential direction of the wound iron core 10 (the direction in which the magnetic field flows around the hollow portion 15).
[0026] Fig. 2 is a diagram showing the iron loss of the wound core 10 according to the present embodiment when the iron loss of the comparative example is taken as 100. The wound core of the comparative example is imparted with the same magnetic domain control strain 20 as the wound core 10 of the present embodiment, but no groove 25 is formed in the bent portion R1 or in the area nearby when bending. As shown in Fig. 2, the wound core 10 of the present invention achieves an iron loss reduction of about 2% compared to the wound core of the comparative example.
[0027] Fig. 3 is a cross-sectional view showing a formation form of grooves 25 around a bent portion R1 when grain-oriented electromagnetic steel sheet 40 constituting wound iron core 10 according to the present embodiment shown in Fig. 1 is bent, and shows the formation interval Pl of grooves 25, the bent portion R1 at corner R of grain-oriented electromagnetic steel sheet 40, and the groove formation range X. In this example, groove 25 is formed directly above bent portion R1 at corner R of grain-oriented electromagnetic steel sheet 40, and another groove 25 is formed at an interval Pl0 of 1 mm from this bent portion R1.
[0028] Fig. 4 shows the relationship between the groove formation range X (mm) and the iron loss ratio for various intervals Pl (laser irradiation pitch) of the grooves 25. Fig. 4 shows the results of comparing the iron loss of wound cores produced by varying the interval Pl of the grooves 25 from 1 mm to 12 mm and the groove formation range X up to a maximum of 70 mm. The iron loss ratio in Fig. 4 is a relative value of the iron loss when the iron loss value of a wound core without grooves 25 is set to 100.
[0029] As can be seen from FIG. 4, when P1=1 mm, the wider the groove formation range X, the greater the iron loss. This is because the effect of reducing the iron loss improvement effect due to the change from the domain control distortion to the groove formation was greater than the effect of reducing the processing distortion caused by the bending process, and the iron loss of the entire groove formation range X increased. In addition, when Pl=2 mm, the iron loss was below 100, and when Pl=4 mm and Pl=6 mm, the iron loss was reduced by up to 2% when the groove formation range X was about 20 mm to 40 mm. On the other hand, as Pl increases, the iron loss reduction effect decreases, but the iron loss tends to decrease up to Pl=10 mm, and when Pl exceeds 10 mm, the iron loss is equivalent to that when the groove 25 is not formed. This is thought to be because when the groove interval Pl increases, the stress applied to reduce the processing distortion caused by the bending process becomes insufficient. In addition, even when Pl=10 mm or less, the iron loss increases when the groove formation range X exceeds 50 mm. This is thought to be because the effect of improving iron loss by imparting the magnetic domain control strain 20 became smaller, and the effect of the processing strain caused by the bending process became relatively larger, causing the iron loss to deteriorate.
[0030] Therefore, it is preferable that the grooves 25 are formed with a groove spacing Pl of 2 mm to 10 mm in a range of 1 mm to 50 mm in the rolling direction D of the grain-oriented electrical steel sheet 40, which can be considered to be in the vicinity of the bend R1 at the corner R created by the bending process of the grain-oriented electrical steel sheet 40.
[0031] FIG. 5 shows a schematic diagram of a method and an apparatus for manufacturing a wound iron core according to one embodiment of the present invention. First, with reference to FIG. 5, a manufacturing apparatus for a wound iron core according to this embodiment will be described. As shown in FIG. 5, the wound iron core manufacturing apparatus of this embodiment receives a supply of grain-oriented electromagnetic steel sheet 40 from a steel sheet supply unit 50 holding a hoop material 40a formed by winding grain-oriented electromagnetic steel sheet 40, by unwinding the grain-oriented electromagnetic steel sheet 40 at a conveying speed V1 (e.g., 30 m / s).
[0032] A beam 90 is irradiated from a beam irradiation unit 52 onto the surface of the grain-oriented electromagnetic steel sheet 40 supplied from a steel sheet supply unit 50, to impart a plurality of magnetic domain control strains 20 at predetermined intervals Pl, extending in a width direction W of the grain-oriented electromagnetic steel sheet 40 that intersects with the rolling direction D of the grain-oriented electromagnetic steel sheet 40. The type of beam irradiated from the beam irradiation unit 52 is not particularly limited. A laser is preferable because a high-energy light source is easily available at low cost, but an electron beam or the like can also be used in the same manner as the laser.
[0033] The grain-oriented electrical steel sheet 40, which has been given the domain-controlling strain 20 by the bending section 54 and has been subjected to magnetic domain control, is cut to an appropriate size and is then bent individually in small batches, such as one by one, for bending (i.e., using the Unicore method). In the grain-oriented electrical steel sheet 40 thus obtained, the curvature of the bent portion R1 at the corner R generated by the bending process is extremely small, and therefore the processing strain given to the grain-oriented electrical steel sheet 40 by the bending process is extremely small. The folded grain-oriented electromagnetic steel sheets 40 are stacked in layers and assembled into a wound shape by an assembly unit 56 (not shown), thereby manufacturing the wound core 10.
[0034] The control unit 58 is connected to the steel plate supply unit 50, the beam irradiation unit 52, the bending unit 54 and the assembly unit 56 directly or via a network or the like, either wired or wirelessly (some parts are omitted from the illustration). The control unit 58 calculates, based on a signal S1 from the bending unit 54, at which part of the (e.g., long) directional electrical steel sheet 40 supplied from the steel sheet supply unit 50 the position of the bend R1 during bending processing at the bending unit 54 is located. Then, the control unit 58 outputs a signal S2 to the beam irradiation unit 52, thereby synchronizing the operation of the beam irradiation unit 52 with the operation of the steel plate supply unit 50, and controls the operation of the beam irradiation unit 52 so that beam irradiation can be performed based on the portion on the directional electromagnetic steel sheet 40 supplied from the steel plate supply unit 50 that will become the bending portion R1 during the bending process.
[0035] For example, by controlling the control unit 58, the beam irradiation conditions (beam power, focusing shape and irradiation speed) of the beam irradiation unit 52 can be set to conditions for irradiating a beam with a relatively low power density, so that magnetic domain control distortion 20 is imparted to the entire area of the surface of the directional electromagnetic steel sheet 40, while on the other hand, in the area that will become the bend R1 in the bending process and the area nearby, the beam irradiation conditions of the beam irradiation unit 52 can be set to conditions for irradiating a beam with a higher power density, so that grooves 25 can be formed (by overwriting) on top of the imparted magnetic domain control distortion 20.
[0036] In addition, under the control of the control unit 58, for areas other than the area that will become the bend R1 in the bending process and its vicinity, the beam irradiation conditions of the beam irradiation unit 52 may be changed to conditions for irradiating a beam with a relatively low power density, thereby imparting distortion 20 for magnetic domain control, while for the area that will become the bend R1 in the bending process and its vicinity, the beam irradiation conditions of the beam irradiation unit 52 may be changed to conditions for irradiating a beam with a higher power density, thereby switching the beam so as to form groove 25.
[0037] Next, a method for manufacturing the wound iron core according to this embodiment will be described with reference to FIG. The hoop material 40a is a roll of a long grain-oriented electromagnetic steel sheet 40 that has not been subjected to magnetic domain control by imparting distortion for magnetic domain control. The hoop material 40a unwound from the steel sheet supply unit 50 is transported toward the beam irradiation unit 52 at a controlled constant speed V1. A beam such as a laser beam is irradiated from the beam irradiation device 52A onto the grain-oriented electromagnetic steel sheet 40, and the beam is scanned in the width direction W of the grain-oriented electromagnetic steel sheet 40, thereby forming distortion 20 for magnetic domain control extending in the width direction W on the surface of the grain-oriented electromagnetic steel sheet 40 (distortion imparting step). It is preferable to impart magnetic domain control strain 20 extending in a width direction W intersecting with the rolling direction D of the grain-oriented magnetic steel sheet 40 only to areas of the surface of the grain-oriented magnetic steel sheet 40 other than the portion that will become the bent portion R1 during bending and its vicinity; however, magnetic domain control strain may be imparted to the entire grain-oriented magnetic steel sheet 40, and then grooves 25 may be formed by overwriting in the groove forming step described below.
[0038] In addition to imparting the distortion 20 for magnetic domain control described above, the beam irradiation section 52 also forms grooves 25 extending in a width direction W intersecting the rolling direction D of the grain-oriented electromagnetic steel sheet 40 in the area of the surface of the grain-oriented electromagnetic steel sheet 40 that will become the bent portion R1 during the bending process and in the area nearby (groove formation step).
[0039] Furthermore, the bending section 54 individually bends the grain-oriented electromagnetic steel sheets 40, to which the magnetic domain control strain 20 has been imparted in the strain imparting step and the grooves 25 have been formed in the groove forming step, one by one, for example, in small batches (i.e., using the Unicore method) (bending step). In the grain-oriented electromagnetic steel sheet 40 thus obtained, the curvature of the bend R1 caused by the bending process is extremely small, and therefore the processing strain imparted to the grain-oriented electromagnetic steel sheet 40 by the bending process is extremely small. The assembly section 56 assembles the bent grain-oriented electromagnetic steel sheets 40 into a wound shape to form the wound core 10 (assembly step).
[0040] 6 is a schematic diagram showing a beam irradiation mode in the beam irradiation unit 52. The type of beam irradiated from the beam irradiation unit 52 is not particularly limited, and may be, for example, a laser or an electron beam. The beam light is guided from a beam light source (not shown) to a beam emitting unit by an optical fiber or a mirror reflection transmission system (not shown), scanned in the width direction W of the grain-oriented electromagnetic steel sheet 40 by a rotating polygon mirror of a polyhedron or a vibration mirror caused by a galvanometer motor in the beam irradiation device 52A, and collected by an fθ lens or a parabolic mirror to be irradiated onto the grain-oriented electromagnetic steel sheet 40.
[0041] As an example of the beam irradiation conditions for imparting the magnetic domain control distortion 20 and for forming the grooves 25, when using a laser, the following conditions can be set: when imparting the magnetic domain control distortion 20, the laser power P can be set to 300 W, the focused shape can be an ellipse with a diameter dx in the beam scanning direction of 0.1 mm and a diameter dy in the perpendicular direction of 4.0 mm, and the beam scanning speed Vx can be set to 20 m / s. On the other hand, when forming the grooves 25, the laser power P can be set to 2000 W, the focused shape can be an ellipse with a diameter dx in the beam scanning direction of 0.05 mm and a diameter dy in the perpendicular direction of 0.3 mm, and the beam scanning speed Vx can be set to 30 m / s. The change in beam power is performed by the power adjustment function of the beam irradiation device 52A, the change in the focusing diameter is performed by the beam expansion / focusing function within the beam irradiation device 52A, and the scanning speed may be changed by changing the speed of a vibrating mirror or a rotating polygon mirror, which is the beam scanning function within the beam irradiation device 52A.
[0042] The present invention is not limited to the above-mentioned embodiment, and can be modified in various ways without departing from the gist of the present invention. For example, in the above-mentioned embodiment, the same beam irradiation device 52A is used to apply the distortion 20 for magnetic domain control and to form the grooves 25. However, the distortion 20 for magnetic domain control and the grooves 25 may be applied using independent beam irradiation units. Furthermore, in the above-described embodiment, the surface of the grain-oriented electromagnetic steel sheet 40 is irradiated with a beam to impart the magnetic domain control strain 20 extending in the width direction W intersecting the rolling direction D of the grain-oriented electromagnetic steel sheet 40, but the grain-oriented electromagnetic steel sheet 40 to which the magnetic domain control strain 20 has been imparted may be obtained from outside, and the grooves 25 may be formed in the grain-oriented electromagnetic steel sheet 40 thus obtained. In that case, the strain imparting step (beam irradiation unit) may be unnecessary. In the embodiment described above, the grooves 25 are formed immediately above the bent portion R1 at the corner R of the grain-oriented electrical steel sheet 40, but the grooves 25 do not have to be formed immediately above the bent portion R1. In the above, the magnetic domain control strain 20 is applied by using a beam such as a laser or an electron beam, but the method of applying the magnetic domain control strain 20 is not limited to this, and other known methods can be used. For example, the magnetic domain control strain 20 can be applied by irradiating the magnetic domain with plasma, or by scratching the surface of the grain-oriented magnetic steel sheet 40 with hard protrusions or by using shot peening or the like to apply a compressive stress to the grain-oriented magnetic steel sheet 40. In the above, an example has been described in which the grooves 25 are formed using a laser or an electron beam, but the method for forming the grooves 25 is not limited to these, and other known methods can also be used. For example, the grooves 25 can be formed by irradiating a beam other than a laser or an electron beam, by etching, or by mechanical pressing. Furthermore, within the scope of the present invention, some or all of the above-described embodiments may be combined, or part of the configuration may be omitted from one of the above-described embodiments. [Explanation of symbols]
[0043] 10-wound iron core 20 Distortion for magnetic domain control 25 groove 40 Grain-oriented electrical steel sheet 50 Steel plate supply section 52 Beam irradiation unit 52A Beam irradiation device 54 Bending section 56 Assembly section R corner R1 bent part
Claims
1. A wound core in which grain-oriented electrical steel sheets having a bent portion and a strain for controlling magnetic domains on the surface extending in a width direction intersecting with the rolling direction are stacked in layers, a groove extending in the width direction is formed on a surface of the grain-oriented electrical steel sheet in the bent portion and in a region in the vicinity of the bent portion.
2. The grooves are formed at intervals of 2 mm to 10 mm in the rolling direction, 2. The wound iron core according to claim 1, wherein the vicinity of the bent portion is in a range of 1 mm to 50 mm from the bent portion in the rolling direction.
3. a distortion imparting step of imparting a distortion for controlling magnetic domains extending in a width direction intersecting a rolling direction of the grain-oriented electrical steel sheet by irradiating a beam onto a surface of the grain-oriented electrical steel sheet; a groove forming step of forming grooves extending in the width direction of the grain-oriented electromagnetic steel sheet by irradiating a beam onto a surface of the grain-oriented electromagnetic steel sheet; a bending step of individually bending the grain-oriented electrical steel sheet to which the distortion for magnetic domain control has been imparted and the grooves have been formed; an assembling step of assembling the bent grain-oriented electrical steel sheets into a wound shape to form a wound iron core; having the distortion imparting step comprises imparting the magnetic domain control distortion to a region of the surface of the grain-oriented electrical steel sheet other than a portion that will become a bent portion in the bending process and its vicinity, The groove forming step forms the grooves in a portion of the surface of the grain-oriented electrical steel sheet that will become a bent portion in the bending process and in a region adjacent to the portion.
4. 4. The method for manufacturing a wound iron core according to claim 3, wherein the distortion imparting step and the groove forming step are performed using a same beam irradiation device, and the processing between the distortion imparting step for magnetic domain control and the groove forming step is switched by changing at least one of the power, the focusing shape, and the irradiation speed of the beam.
5. A grain-oriented electrical steel sheet is used, in which a beam is irradiated onto the surface to impart distortion for magnetic domain control extending in the width direction, which intersects with the rolling direction. a groove forming step of forming grooves extending in the width direction of the grain-oriented electromagnetic steel sheet by irradiating a beam onto a surface of the grain-oriented electromagnetic steel sheet; a bending step of individually bending the grain-oriented electrical steel sheet to which the distortion for magnetic domain control has been imparted and the grooves have been formed; an assembling step of assembling the bent grain-oriented electrical steel sheets into a wound shape to form a wound iron core; having The groove forming step forms the grooves only in areas of the surface of the grain-oriented electrical steel sheet that will become bent portions in the bending process and in areas adjacent to the areas.
6. a beam irradiation unit that irradiates a surface of the grain-oriented electromagnetic steel sheet with a beam to impart a distortion for magnetic domain control extending in a width direction intersecting a rolling direction of the grain-oriented electromagnetic steel sheet, and that irradiates the surface of the grain-oriented electromagnetic steel sheet with a beam to form a groove extending in the width direction of the grain-oriented electromagnetic steel sheet; a bending processing unit that individually bends the grain-oriented electrical steel sheet to which a distortion for magnetic domain control has been imparted and a groove has been formed; an assembly unit that assembles the folded electromagnetic steel sheets into a wound shape to form a wound iron core; having The beam irradiation unit includes: imparting the magnetic domain control distortion to a region of the surface of the grain-oriented electrical steel sheet other than a portion that will become a bent portion in the bending process and its vicinity; a groove is formed in a portion of a surface of the grain-oriented electrical steel sheet that will become a bent portion in the bending process and in a region adjacent thereto.
7. a beam irradiation unit that uses a grain-oriented electromagnetic steel sheet having a surface to which a strain for controlling magnetic domains extending in a width direction intersecting a rolling direction is imparted by irradiating a beam onto the surface of the grain-oriented electromagnetic steel sheet, and forms grooves extending in the width direction of the grain-oriented electromagnetic steel sheet by irradiating a beam onto the surface of the grain-oriented electromagnetic steel sheet; a bending processing unit that individually bends the grain-oriented electrical steel sheet to which a distortion for magnetic domain control has been imparted and a groove has been formed; an assembly unit that assembles the bent grain-oriented electrical steel sheet into a wound shape to form a wound iron core; having The beam irradiation unit includes: a groove is formed only in a portion of the surface of the grain-oriented electrical steel sheet that will become a bent portion in the bending process and in an area adjacent to the portion.
Citation Information
Patent Citations
Wound core and its manufacturing method
JP2003347128A
Wound core, and manufacturing method of wound core
JP2018037572A
Unidirectional magnetic steel sheet excellent in iron loss characteristic
WO2008050700A1
Directional electromagnetic steel plate and method for manufacturing same
WO2011125672A1
Wound core and method for manufacturing same
WO2018131613A1