Refiner packing with variable coated bars
Variable coating on refiner bars optimizes wear resistance and hydraulic capacity by distributing coating thickness based on wear patterns, extending service life and reducing costs in pulp refiners.
Patent Information
- Application Number
- JP2023548975
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-10-22
- Filing Date
- 2021-08-16
- Publication Date
- 2024-10-07
- Estimated Expiration
- 2041-08-16
AI Technical Summary
Existing refiner bars in pulp refiners wear out quickly due to abrasives in the pulp suspension, requiring frequent replacement and leading to reduced hydraulic capacity and high costs, while uniform wear-resistant coatings reduce hydraulic power and are brittle.
Refiner bars coated with a variable coating that varies in thickness to maximize abrasion resistance where needed and minimize it where unnecessary, maintaining hydraulic capacity and reducing stress concentrations.
The variable coating extends the service life of refiner bars, reduces costs, and maintains hydraulic capacity by optimizing coating distribution based on wear patterns, enhancing durability and efficiency.
Smart Images

Figure 0007562875000001 
Figure 0007562875000002 
Figure 0007562875000003
Abstract
Description
[Technical field]
[0001] The present invention relates generally to refiner filling for refiners for the making and refining of lignocellulosic materials in the production of paper, paperboard, tissue, towel, or fiberboard products, and more particularly to refiner filling bars. [Background technology]
[0002] Rotary-type pulp refiners, which may be disk-type refiners or cone-type refiners, use replaceable refiner packing consisting of refiner filling pieces attached to a rotor and stator to mechanically shear and compress the cellulosic fibers in the pulp suspension. The refiner filling pieces may be unitary parts or may be segments assembled together. The refiner filling pieces have a number of refiner bars that perform the shearing and compressing action on the cellulosic fibers in the pulp suspension.
[0003] In disk and cone refiners, the presence of abrasives in the pulp suspension accelerates wear of the refiner bars of the refiner packing, thereby reducing the depth of the grooves between adjacent bars. As a result, the refiner packing typically needs to be replaced quite frequently. Typically, a refiner packing may have a useful life of around one month to two years, because as the packing wears and the grooves become shallower, it no longer provides sufficient hydraulic capacity.
[0004] It is known to apply a uniform wear-resistant coating to the front face of the bars to extend their service life, but this coating can occupy a significant portion of the groove volume between the refiner bars, thus reducing the hydraulic capacity of the refiner charge. To obtain the desired hardness, these coatings are usually made of "exotic" alloys and are therefore expensive. The hard coatings are inherently hard and brittle, which can lead to bar breakage under severe service conditions.
[0005] It would therefore be highly desirable to provide new refiner bar technology that overcomes at least some of the shortcomings of the prior art. Summary of the Invention [Problem to be solved by the invention]
[0006] Generally, embodiments of the invention provide refiner packing pieces and refiners in which the bars are coated with a variable coating. [Means for solving the problem]
[0007] An inventive aspect of the present disclosure is a refiner packing piece for a refiner having a rotor that rotates about an axis of rotation and cooperates with the stator to mechanically treat pulp including cellulosic fibers. The refiner packing piece can be attached to the rotor or the stator. The refiner packing piece has a plurality of spaced apart refiner bars, each bar defined by a bar length and a bar height. At least some of the refiner bars have surfaces coated with a variable coating. The variably coated surface can be a leading surface and / or a trailing surface. The variable coating can be variable radially along the bar length or axially across the bar height.
[0008] The foregoing presents a simplified summary of the invention in order to provide a basic understanding of some aspects of the invention. This summary is not an exhaustive overview of the invention. It is not intended to identify essential, critical or critical elements of the invention or to delineate the scope of the invention. Its sole purpose is to present some concepts in a simplified form as a prelude to the more detailed description that is presented later. Other aspects of the invention are described below in conjunction with the accompanying drawings. [Brief description of the drawings]
[0009] Further features and advantages of the present technology will become apparent from the following detailed description taken in conjunction with the accompanying drawings. [Figure 1] FIG. 1 is a perspective view of a refiner having a rotor and a stator according to an embodiment of the invention, illustrating the replacement of refiner packing pieces in the stator. [Diagram 2] FIG. 2 is another perspective view of the refiner of FIG. 1 showing replacement of the refiner packing pieces in the rotor. [Figure 2A] FIG. 2A is a plan view of four refiner packing pieces shaped as four arcuate segments as an example of segmented packing pieces for a disk-type refiner. [Diagram 3] FIG. 3 is a cross-sectional view of a refiner packing piece having a variable coating on the front surface of the bar. [Figure 4] FIG. 4 is a cross-sectional view showing a refiner packing piece having a variable coating on the front face of the bar. [Diagram 5] FIG. 5 is a cross-sectional view showing a refiner packing piece having a variable coating on the front face of the bar. [Figure 6] FIG. 6 is a cross-sectional view of a refiner packing piece having a variable coating on the front surface and a thinner variable coating on the rear surface. [Figure 7] FIG. 7 is a cross-sectional view of a refiner packing piece having a variable coating on the front surface and a thinner variable coating on the back surface. [Figure 8] FIG. 8 is a cross-sectional view of a refiner packing piece having a variable coating on the front surface and a thinner variable coating on the back surface. [Figure 9] FIG. 9 is a plan view of a refiner packing piece according to one embodiment of the present invention, in which the variable coating varies linearly along the bar length at the front face. [Figure 10] FIG. 10 is a plan view of a refiner packing piece according to another embodiment of the invention, in which a variable coating varies linearly along the bar length at the front face and a thinner variable coating varies along the bar length at the rear face. [Figure 11] 11 depicts a conical refiner packing piece to which a variable coating may be applied according to another embodiment of the present invention. It should be noted that throughout the accompanying drawings, like features are identified with like reference numerals. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Disclosed herein are various embodiments of a refiner packing piece having refiner bars coated with a variable coating. Disclosed herein are also refiners having one or more refiner packing pieces that include refiner bars coated with a variable coating.
[0011] FIG. 1 is a perspective view of a refiner, generally designated by reference numeral 10, according to one embodiment of the present invention. In the embodiment depicted in FIG. 1, refiner 10 has a housing 12, a stator 14, and a rotor 16. The rotor rotates about an axis of rotation and cooperates with the stator to mechanically process pulp (or a pulp suspension) that includes cellulosic fibers. The axis of rotation defines an axial direction and a radial direction. In the illustrated embodiment of FIG. 1, the refiner is a disk-type refiner with replaceable refiner packing. The refiner is a disk-type refiner having a replaceable refiner packing. The refiner packing is composed of a plurality of refiner packing pieces. In the example of FIG. 1, the refiner packing pieces are segments of a generally flat annular disk- or plate-like structure (also referred to herein as a "plate"). However, it will be understood that the refiner packing pieces may also be cone-shaped packing pieces in a conical refiner. In this specification, the expression "refiner packing pieces" shall be interpreted as embracing a flat disk-shaped plate or an arcuate segment thereof, or a cone structure or an angular segment thereof. In the case of a disk-type refiner, the refiner packing pieces may be integral circular plates, annular plates, or arcuate segments assembled with other arcuate segments to form a complete circular or annular plate. Similarly, in the case of a conical refiner, the refiner packing pieces may be integral conical (or frusto-conical) structures, or angular segments of a cone (or frusto-conical) assembled with other such angular segments to form a complete conical (or frusto-conical) structure. From the above, it will be appreciated that refiner packing pieces may be circular, annular or conical (i.e., defining a complete 360 degree component), or segmented (i.e., defining an arcuate or angular component of less than 360 degrees that is designed to be assembled with other segments to form a complete circular or annular plate or to form a cone, as the case may be).
[0012] FIG. 1 depicts replacement of refiner packing pieces 20 in stator 14. Refiner packing pieces 20 may be attached to stator 14 using fasteners, such as threaded fasteners, as shown. In this example, multiple refiner packing pieces 20 are attached to stator 14 in an annular arrangement to form a stator-side refiner plate. In the embodiment depicted in FIG. 1, stator 14 is attached to a door-like cover 15 that pivots about a hinge mechanism to allow replacement of refiner packing pieces 20.
[0013] Figure 2 is another perspective view of refiner 10 of Figure 1, illustrating the replacement of refiner packing pieces 20 in rotor 16. The refiner packing pieces 20 may be attached to rotor 16 using fasteners, such as threaded fasteners, as shown. A plurality of refiner packing pieces 20 are attached to rotor 16 in an annular arrangement to form a rotor-side refiner plate. In the embodiment depicted in Figure 2, rotor 16 is mounted inside housing 12 of refiner 10.
[0014] In the embodiment of Figs. 1 and 2, the refiner packing pieces 20 are replaceable refiner packing pieces having a segmented plate-like shape. During refiner maintenance, the refiner packing may be replaced if worn by replacing the assembly of refiner packing pieces that make up the packing. For example, as shown in Fig. 2A, four refiner packing pieces shaped as four arcuate segments may be assembled to provide a complete annular plate structure for a disk-type refiner. The angular arc of each arcuate or segmented packing piece may be varied from that shown in these examples. The angular arc of the packing pieces may be, for example, 360 degrees, 180 degrees, 90 degrees, 45 degrees, 30 degrees, 22.5 degrees, 20 degrees, 15 degrees, 10 degrees, etc., and when assembled, they form an annular arrangement having a complete 360 degrees. Fig. 2A also shows that the annular refiner packing pieces may be characterized by an inner diameter (ID) and an outer diameter (OD). Thus, the refiner packing pieces extend radially from the inner diameter to the outer diameter. It will also be appreciated that a complete plate or annulus of arcuate or segmented packing pieces may be made up of packing pieces of different shapes, for example, one 180 degree packing and two 90 degree packing pieces, two 90 degree packing pieces and four 45 degree packing pieces, three 60 degree packing pieces and six 30 degree packing pieces, etc.
[0015] As shown in FIGS. 3-10, the refiner packing piece 20 has a base 22. The base may alternatively have a non-uniform thickness, but in some embodiments may have a uniform thickness in the axial direction. The base extends radially from an inner diameter ID to an outer diameter OD, as depicted in FIG. 2A. The refiner charge piece 20 has a plurality of spaced apart refiner bars 30 (also known as "blades"). The bars may be spaced apart by a uniform or non-uniform groove width, i.e., the spacing between adjacent bars may vary or may be constant. Optionally, the refiner bars are spaced apart by spacers 24, but in other embodiments, spacers may be absent. Each bar is defined by a bar length BL that extends toward the outer diameter, i.e., generally radially, and further by a bar height BH that projects generally axially from the base. The bar height may be constant or may vary. In some embodiments, the bar height may be a value that is in the range of 3-14 mm, for example. At least some of the refiner bars 30, in this embodiment of the invention, have a front surface 32 that is coated with a variable coating 34.
[0016] The variable coating, unlike the prior art, is applied non-uniformly to the front surface of the bar and, optionally or alternatively, to the rear surface of the bar. The coating varies in thickness, i.e., the coating varies dimensionally or geometrically. The coating thickness varies such that the coating is thickest in areas that provide the greatest wear resistance and is minimal or absent in areas where it has limited usefulness or where excess coating may be detrimental.
[0017] As depicted in Figures 3-10, a variable coating has a coating thickness that is variable either along the refiner bar height (e.g., increasing from the base to the top of the bar) or radially (e.g., increasing from the inner diameter ID to the outer diameter OD of the packing).
[0018] The coating thickness may be a function of the bar height. For example, the coating thickness may increase with the bar height (e.g., the coating gets thicker as the height increases and is at its maximum thickness at the top of the bar). This maximizes the space at the bottom of the groove to maintain or improve hydraulic capacity while minimizing stress concentrations at the root of the bar where bending stresses are highest. Additionally, variable coatings can reduce costs by not applying coatings where they are not needed or would be less effective.
[0019] The coating may also, or alternatively, vary in thickness along the radial length, for example, from the ID (where the coating is least) to the OD (where the coating is most), or toward the OD. This maximizes the open area or volume at the ID, which is critical for hydraulic capacity. Because the OD of the packing typically experiences a higher peripheral speed (in disc refiners) than the ID, the OD consumes more energy, exerts more shear and compression, and performs the majority of the refining work. Thus, concentrating the coating on the OD of the packing piece can improve service life compared to the same amount of coating applied uniformly.
[0020] Figure 3 is a cross-sectional view showing a refiner packing piece 20 having a variable coating 34 on the front face 32 of the bar 30. In the embodiment depicted in Figure 3, the variable coating 34 has a coating thickness that varies axially with bar height.
[0021] As shown in FIG. 3, the coating thickness in this exemplary embodiment increases linearly with bar height.
[0022] FIG. 3 also shows the gap between the rear face of one bar and the covered front face of the bar immediately behind it. FIG. 2 shows the groove space occupying a volume of 100 mm. The coating on the front face of the bars reduces wear on the bars, thus preserving the hydraulic capacity of the refiner by maintaining the desired groove space between adjacent bars.
[0023] 4, the variable coating 34 on the front surface 32 of the bar 30 has a coating thickness that increases non-linearly with bar height, for example. For example, in one specific embodiment, the non-linear coating may be applied parabolically or exponentially with bar height. For example, the coating thickness may increase as the square of the axial height.
[0024] Alternatively, in the embodiment depicted in FIG. 5, the variable coating 34 on the front surface 32 of the bar 30 has a coating thickness that, for example, increases over a first portion of the bar height, then decreases over a second portion of the bar height, and then increases over a third portion of the bar height.
[0025] Figure 6 is a cross-sectional view showing a refiner packing piece 20 having a variable coating 34 on the front surface 32 and a thinner variable coating 36 on the back surface 38. In the embodiment of Figure 6, the coatings on the front and back surfaces increase linearly with bar height, although at different rates.
[0026] In the exemplary embodiment depicted in FIG. 7, the front and rear faces 32, 38 have variable coatings 34, 36, respectively, that increase non-linearly with bar height, although at different rates.
[0027] In the exemplary embodiment depicted in Figure 8, the rear face has a thinner variable coating than the variable coating on the front face, similar to Figures 6 and 7. In Figure 8, the thinner variable coating increases over a first portion of the bar height, then decreases over a second portion of the bar height, then increases over a third portion of the bar height.
[0028] 9 is a plan view of a refiner packing piece 20 according to one embodiment of the present invention in which the variable coating 34 varies radially along the bar length BL at the front face 32. Specifically, in this example, the variable coating has a coating thickness that varies linearly along the bar length.
[0029] Figure 10 is a plan view of a refiner packing piece 20 according to another embodiment of the invention, in which a variable coating 34 varies radially along the bar length BL at the front face 32 and a thinner variable coating 36 varies radially along the bar length BL at the rear face 38. In this embodiment, the variable coating has a coating thickness that varies linearly along the bar length. As shown in Figure 10, the rear face has a thinner variable coating than the variable coating on the front face.
[0030] FIG. 11 depicts a conical refiner fill piece 20 to which a variable coating may be applied according to another embodiment of the present invention. The conical refiner fill piece 20 is characterized by an inner diameter ID and an outer diameter OD, as shown in FIG. 11. The refiner bars 30 of the conical refiner fill piece 20 have a variable coating, which may be varied in any of the various ways described above. In this example, the conical refiner fill piece 20 is a single piece that defines a complete conical structure, although it will be understood that the conical refiner fill piece may also be a segmented conical fill piece that is assembled with other segmented conical fill pieces to form a complete conical (or frustoconical) structure.
[0031] In some embodiments, the front faces of all refiner bars have a variable coating, i.e., all refiner bars are coated with a variable coating. In other embodiments, only some of the rear faces of the refiner bars have a variable coating. For example, an alternating pattern of coated and uncoated bars may be implemented. As another example, every third or fourth bar may be coated. Conversely, every third or fourth bar may be uncoated.
[0032] In some embodiments, the variable coating extends along the entirety of the bar length. In other embodiments, the variable coating extends only partially along the bar length. For example, the variable coating may extend over 90%, 80%, 70%, 60%, 50%, 40%, 30%, 20%, 10%, etc. of the length. As another example, one bar may be coated with a first percentage and the next bar may be coated with a different percentage. In some embodiments, the variable coating extends from the base to the top of the bar, i.e., the coating covers the entirety of the bar height. In other embodiments, the variable coating extends only over a portion of the bar height. For example, the variable coating may begin at a point higher than the base, e.g., the midpoint, one-quarter of the height, one-third of the height, three-quarters of the height, etc.
[0033] For purposes of interpreting this specification, when referring to elements of various embodiments of the invention, the articles "a," "an," "the," and "said" are intended to mean that there are one or more of the element. The terms "comprising," "including," "having," "entailing," and "involving," and their verb tense variations, are intended to be inclusive and open-ended, meaning that there may be additional elements other than the listed elements.
[0034] The present invention has been described in terms of specific embodiments, implementations, and configurations that are intended to be illustrative only. Those skilled in the art will recognize that many obvious variations, modifications, and variations may be made without departing from the inventive concepts presented herein. Accordingly, it is intended that the scope of the exclusive rights sought by applicants be limited only by the scope of the appended claims.
Claims
1. A refiner packing piece for a refiner having a rotor that rotates about an axis of rotation and cooperates with a stator to mechanically treat pulp containing cellulosic fibers, the refiner packing piece being attachable to the rotor or the stator, the refiner packing piece comprising: A base and a plurality of spaced apart refiner bars; Including, Each refiner bar is defined by a bar length and a bar height and has a front face and a rear face; A refiner packing piece, wherein at least some of the refiner bars have a surface coated with a variable thickness coating.
2. A refiner filler piece as described in claim 1, wherein the surface coated with the variable thickness coating is the front surface.
3. The refiner charge piece of claim 1 or claim 2, wherein the variable coating has a coating thickness that varies along the bar length.
4. The refiner charge piece of claim 3 , wherein the variable coating has a coating thickness that varies linearly along the bar length.
5. A refiner filler piece as described in claim 4, wherein the rear surface has a variable coating that is thinner at a particular cross section of the refiner bar than the variable coating on the front surface.
6. The refiner packing piece of claim 1 or claim 2, wherein the front surface of all refiner bars has the variable coating.
7. The refiner charge piece of claim 1 or claim 2, wherein only some of the front faces of the refiner bars have the variable coating.
8. The refiner charge piece of claim 1 or claim 2, wherein the variable coating extends along the entirety of the bar length.
9. The refiner charge piece of claim 1 or claim 2, wherein the variable coating extends only partially along the bar length.
10. The refiner charge piece of claim 1 or claim 2, wherein the variable coating has a coating thickness that varies with the bar height.
11. The refiner charge piece of claim 10 , wherein the coating thickness increases linearly with the bar height.
12. The refiner charge piece of claim 10 , wherein the coating thickness increases non-linearly with the bar height.
13. 11. The refiner charge piece of claim 10, wherein the coating thickness increases over a first portion of the bar height, then decreases over a second portion of the bar height, and then increases over a third portion of the bar height.
14. A refiner filler piece as described in claim 10, wherein the rear surface has a variable coating that is thinner at a particular cross section of the refiner bar than the variable coating on the front surface.
15. A refiner filler piece as described in claim 11, wherein the rear surface has a thinner variable coating than the variable coating on the front surface, the thinner variable coating increasing linearly with the bar height.
16. A refiner filler piece as described in claim 12, wherein the rear surface has a thinner variable coating than the variable coating on the front surface, and the thinner variable coating increases nonlinearly with the bar height.
17. A refiner filler piece as described in claim 13, wherein the rear surface has a thinner variable coating than the variable coating on the front surface, the thinner variable coating increasing across the first portion of the bar height, then decreasing across the second portion of the bar height, and then increasing across the third portion of the bar height.
18. A refiner comprising: A housing and a stator supported within the housing; a rotor that rotates about a rotation axis and cooperates with the stator to mechanically process pulp containing cellulosic fibers; a first refiner packing piece according to any one of claims 1 to 17 secured to the rotor; A second refiner packing piece according to any one of claims 1 to 17 secured to the stator; Including, refiner.
Citation Information
Patent Citations
JP1990010496U
Refiner-element pattern for effecting continuous compression before impact application
JP1991113086A
Edged tool for preparing paper stock
JP1994065880A
Plate for refiner
JP1997111683A
refiner lining
JP1998506686A