Systems and methods for forming wire and cable - Patents.com

By temporarily increasing the hardness of polymeric insulation through cryogenic exposure, the method addresses deformation issues in cable manufacturing, improving electrical performance and enabling faster production.

JP7565386B2Active Publication Date: 2024-10-10DAIKIN INDUSTRIES LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2022575872
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-06-20
Filing Date
2021-06-09
Publication Date
2024-10-10
Estimated Expiration
2041-06-09

AI Technical Summary

Technical Problem

Existing methods for manufacturing electrical wires and cables face challenges in maintaining the integrity of polymeric insulation layers due to compressive and torsional forces during the manufacturing process, leading to deformation and compromised signal transmission capabilities.

Method used

The method involves temporarily altering the hardness and Young's modulus of polymeric insulation by exposing it to cryogenic fluids or chilled media during the manufacturing process to increase its resistance to deformation, thereby maintaining conductor spacing and improving electrical performance.

Benefits of technology

This approach reduces deformation of polymeric insulation layers, maintains conductor-to-conductor spacing, and enhances the electrical properties of the cables, allowing for faster production speeds and reduced material usage while maintaining signal integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007565386000009
    Figure 0007565386000009
  • Figure 0007565386000010
    Figure 0007565386000010
  • Figure 0007565386000011
    Figure 0007565386000011
Patent Text Reader

Abstract

Systems and methods are provided for manufacturing wire and cable products using polymer cable components. The systems and methods include increasing the hardness of the polymer cable components to reduce compression and deformation of the cable components during manufacturing. In some cases, the hardness is temporarily increased before or during the twisted pair manufacturing process or during the cable manufacturing process.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of U.S. Provisional Patent Application No. 63 / 041,878, filed June 20, 2020, which is incorporated by reference in its entirety.

[0002] FIELD OF THE DISCLOSURE This disclosure relates to making communication cables, and more particularly to tailoring the hardness of polymer cable components to make high performance communication cables with reduced crush rates. [Background technology]

[0003] A variety of means may be utilized to transmit power or signals, and the invention disclosed herein is generally focused on wire and cable products that utilize insulated conductors to transmit electrical current.

[0004] Many factors must be considered when designing wire and cable products. Applications such as Ethernet, CATV, and factory floor-based systems may dictate certain design features such as size, electrical properties, and physical attributes. For size, it may be important that the cable fits into standard connectivity, piping, raceways, and conduits. For electrical properties, capacitance, inductance, DC resistance, current, and current-carrying capacity may be design considerations. For certain dedicated high-bandwidth cables, additional electrical parameters such as attenuation, velocity of propagation, delay time skew, impedance, insertion loss, and noise mitigation may be important. For physical attributes, flame resistance, smoke resistance, chemical resistance, ozone resistance, moisture resistance, and / or tensile strength are common attributes considered. Fortunately, there are many tools and equations available to assist design engineers in considering the best options for building wire and cable products.

[0005] The process for manufacturing wire and cable is typically continuous in nature. A continuous manufacturing line typically includes a payout device where material is paid out or dispensed to start the line process. There may also be an accumulator that stores a portion of the payout material to help facilitate a consistent line speed. At the end of the line there is typically a take-up device, which may also include an accumulator, to produce a product at a consistent line speed and allow the finished product to be wound into a roll or other form of packaging. Such operations may include, among other things, insulation, entangling, cable making, braiding, jacketing and putting up the wire and cable product. In most wire and cable products, the first step is the insulation process, in which the conductor is coated or covered with a polymeric material to electrically insulate the conductor.

[0006] During and after the insulation process, forces are likely to be created that can affect the ability of the final product to meet its intended specifications. For example, in the case of coaxial type cables, it is desirable to add foil and / or metal braid to protect the inner insulation layer and the electrical signals contained therein. It is well known that metal braid installations can create indentations along the surface of the insulation it encases. In other words, because the surface of the insulation is often softer than the metal wires applied to it, the bare strands of the braided shield wire will deform the surface of the insulation underneath. Such deformation of the insulation can affect the signal transmission capabilities of the final cable as an increase in capacitance and insertion loss. To account for these indentations, design engineers may add extra insulation material to accommodate the depth of the indentations.

[0007] In multi-conductor cables, the various insulated conductors are bundled together through a stranding mechanism, often called a entangler, buncher, or cabler. The forces generated by each of these mechanisms can compress and distort the polymeric components of the cable. Again, cable designers often add insulation to compensate for the compression, thus increasing the size and cost of the final product. Similar compressive forces can also be generated during jacketing and tensioning operations. To compensate for any deformation due to compression, thicker and / or stiffer jacket layers are sometimes used, which increases both the size and cost of the final product.

[0008] Adverse or compressive forces acting on cable components can be periodic in nature. For example, if a wheel is not properly aligned, it can wobble back and forth as it traverses in a circular rotation. This creates a sinusoidal deformation in the material. If this sinusoidal pattern coincides with the intended frequency of the application (or any harmonics thereof), signal integrity can be compromised. Existing methods that help reduce the effects of such forces include slowing down the speed of the production line, whether constant or sinusoidal in nature. Slowing down the speed can mitigate and reduce the compressive forces caused by the manufacturing equipment as the product is produced. For this reason, it is common to run the equipment at a fraction of its original speed. However, this is undesirable as it does not fully utilize the capacity of the equipment.

[0009] Another way in which compressive forces can potentially cause problems is with regard to capacitance targets. Capacitance is a function of the distance between metal surfaces and the properties of the material between those metal surfaces. In the case of wire and cable, the conductive surfaces may include, among other things, two conductors in close proximity or a shield and a conductor in close proximity. The distance between these conductive surfaces is an important design consideration in manufacturing wire and cable products. Therefore, care is taken to ensure that the conductors are spaced apart appropriately.

[0010] In some embodiments, two insulated conductors are formed together to make a twisted pair. Similarly, many insulated conductors can be formed together to make a multi-conductor cable unit. When two insulated conductors are twisted together, a helical pattern is obtained along the length of the twisted pair unit. A twisted pair unit typically consists of a metal conductor, an insulating material, and air contained in the gaps between two approximately circular insulated conductors. It is well known that air is a highly desirable dielectric material. For example, air has a dielectric constant of 1.0, whereas materials such as polyolefins have a typical dielectric constant between 2.3 and 2.6. Thus, the more air is preserved in the gaps of a twisted pair unit, the more favorable the electrical outcome. However, when the insulated conductors are brought closer together by the compressive forces generated during cable construction, insulating material may migrate into these gaps, thus reducing the total air content. This results in a higher, generally less favorable, capacitance, which may in some cases reduce the signal speed and reduce the signal propagation capability.

[0011] Insulated conductors, such as twisted pair communication cables, are typically used for high frequency signal transmission in the plenum areas of buildings. In twisted pair data cable embodiments, individual conductive wires are insulated using a polymer, and then two such insulated conductors are twisted around each other to form a single twisted pair. Twisted pair cables are typically constructed from multiple twisted pairs contained within a single outer jacket to form a cable. Each twisted pair in a cable may be twisted with a different twist (conventionally measured in mm / turn) to reduce electrical coupling (i.e., crosstalk) between adjacent twisted pairs.

[0012] The process of twisting the individual insulated conductors together often compresses the polymer insulation layer. The amount of force compressing the insulation layer varies depending on the twisting equipment and the twist tightness (i.e., turns per inch). The compressive force caused by twisting the insulated conductors deforms the insulation layer, reducing the thickness of the insulation layer separating the two conductors. This results in an increase in the capacitance measured between the two conductors and therefore a decrease in the overall impedance of the twisted pair unit.

[0013] It should also be mentioned that in the case of torsional forces (the type or forces that occur when insulated conductors are twisted together), the deformation may not be uniform. This is because the insulation may move unbalanced depending on the direction of the torsional force. This condition is especially undesirable in balanced pair applications. For example, in some applications involving twisted pair units using two insulated conductors, it is desirable for the signals in each of the two insulated conductors to be mirror images of each other. In this way, electrical noise that couples with each insulated conductor of the twisted unit will couple in the same way, thereby allowing electronic filtering mechanisms to cancel out the noise components. If one insulated conductor in the pair is shaped unbalanced, it becomes difficult to subtract any noise components from the desired signal. Wire and cable specifications often have specifications for both near-end and far-end crosstalk to ensure that the amount of noise between the transmitting pairs is small enough that it does not interfere with signal transmission. Having poorly balanced insulated conductors makes these specifications difficult to meet.

[0014] When cable designers consider how much additional insulation material is needed to offset any insulation material displacement or deformation resulting from forces encountered during the manufacturing process, they need to understand the softness of the insulation material. Since these are generally permanent in nature, it is most appropriate to understand the hardness of the compound. Hardness is often expressed in Pascals and measures a material's resistance to surface deformation. In other words, hardness is the resistance of a surface to localized deformation. Indentation hardness can be measured in a variety of ways, including Brittnell, Mayer, Vickers, Rockwell, and / or Shore durometer. For example, for polymeric materials such as fluorinated ethylene propylene (FEP), polyethylene (PE), polypropylene (PP), polyether ether ketone (PEEK), polyether ketone ketone (PEKK), and polyvinyl chloride (PVC), the Shore D hardness scale is commonly used. For other materials, such as rubber, other Shore scales, such as Shore A, can be used. For Shore D, the testing protocols are defined in ASTM D2240 and / or ISO 868, which are used herein as the baseline hardness standard.

[0015] It is understood that changes in ambient temperature conditions can affect the softness of a material. For example, in warm climates, temperature control of the manufacturing floor may be required during months of seasonally higher ambient temperatures, which may reduce the hardness of any polymeric materials on the manufacturing floor. Additionally, when a cable component is subjected to compression, twisting, or other deformation forces, heat is generated within the cable component. In some applications, the forces involved may cause the temperature of the component to be higher than the ambient temperature as the component is deformed, thereby reducing the hardness of the component and making it more susceptible to deformation during that deformation event, as well as any subsequent deformation events.

[0016] Conversely, the hardness of the compound may increase when the compound is cooled below ambient temperature. This hardening can make the material more resistant to compressive forces that would cause the material to deform or dent.

[0017] The temperature adjustment does not need to persist beyond the compression event. Since the deformations discussed herein are permanent in nature (i.e., not elastic), the disclosed methods need only be applied before or during the compression event. Once the compression event is over, the material may return to ambient temperature. Other methods described above are more permanent in nature (e.g., slowing down the machine, adding skin layers, or adding harder materials to the insulation). Temporarily adjusting the hardness of the material can avoid many of the negative effects of these solutions.

[0018] It is desirable for industry to have a way to harden the compound or reduce the compressive forces applied that is less costly than adding insulation to counter the effects of deforming polymer cable components. Any method incorporated to reduce the impact of compressive forces on the insulation would also be desirable to fit within the footprint of current machinery with little change in the positioning of the equipment itself. One such method is to control the temperature of the compound to vary the hardness of the compound. It can be seen that a harder compound will be less affected by compressive forces than a softer compound. When using the Shore D scale, the higher the number means the harder the compound. This assumes that the type of material is the same and only the temperature of the material itself changes.

[0019] As explained above, reducing deformation due to forces generated during the manufacturing process can improve performance and reduce costs, and changing the hardness of a material with a temporary temperature change can accomplish both.

[0020] Increasing the hardness of a polymeric cable component can reduce deformation of the polymeric insulation layer, cross-web filler, polymeric tube, or other polymeric cable component that is typically caused by compressive or torsional forces during manufacturing operations such as stranding, braiding, and mechanical devices such as pulleys (wheels) and winders. Summary of the Invention [Problem to be solved by the invention]

[0021] What is needed is a cost-effective method of increasing the harness of the material. What is needed is a method of cooling the insulating material at or near the location where the compressive force is applied. This method can increase the hardness of the material relative to what it would be at ambient temperature and reduce any deformation caused by the compressive force. [Means for solving the problem]

[0022] SUMMARY This disclosure relates generally to the creation of wire and cable products that incorporate methods for temporarily altering the hardness and / or Young's modulus of the material.

[0023] Some disclosed embodiments relate to methods and devices for increasing the hardness and / or Young's modulus of a polymeric insulation that may be used in-line as part of a continuous or semi-continuous manufacturing process. Some disclosed embodiments relate to a method of reducing the effect of compressive forces on a polymeric cable component, the method including providing a polymeric cable component having a first hardness, the first hardness being a hardness of the polymeric cable component under ambient conditions, temporarily changing the hardness of the polymeric cable component to a second hardness, the second hardness being different from the first hardness, applying a compressive force to the polymeric cable component, and allowing the polymeric cable component to return to the first hardness.

[0024] Some disclosed embodiments relate to a method for forming a twisted pair, the method including providing a first polymer insulated conductor including a first conductor electrically insulated by a first polymer insulating layer and a second polymer insulated conductor including a second conductor electrically insulated by a second polymer insulating layer, exposing the first insulated conductor to a cryogenic fluid, and twisting the first and second polymer insulated conductors around each other to form the twisted pair.

[0025] In some embodiments, polymer cable components, such as polymer insulated conductors, are exposed to chilled fluid for different periods of time to tailor the hardness of the polymer cable components. In some embodiments, polymer cable components, such as polymer insulated conductors, are exposed to chilled fluid for different periods of time to create cables with reduced delay skew.

[0026] Some disclosed embodiments relate to methods of manufacturing communication cables to reduce deformation of polymeric cable components and maintain the roundness of insulated conductors and other cable components.

[0027] Some disclosed embodiments relate to system installations for manufacturing wire and cable products having improved electrical properties. Some of these embodiments relate to cooling vessels and / or secondary structures for holding a cooling medium, such as, for example, a chilled fluid or a cooled solid surface.

[0028] Some disclosed embodiments relate to methods of making communication cables with reduced fuel loading, including forming wire and cable products having less total polymer insulation relative to conventional cables, such that the cables having less total polymer insulation have lower total fuel loading and improved flammability and / or smoke generation characteristics. Some disclosed embodiments relate to methods of producing communication cables at faster speeds. Some of these embodiments relate to operating the entangling device at faster speeds, which typically increases the compressive force on the polymer insulation layer. Some of these embodiments relate to curing the polymer insulation prior to entangling so that the entangling device can be operated at faster speeds to produce cables with an acceptable amount of deformation and desired electrical properties.

[0029] The disclosed invention may be applied to any form of polymeric cable component or cable structure including, for example, solid, foam, shaped extrusion, insulation layer, hollow tube, cross-web, rod-filler, film, tape, coaxial structures including braided processes, and / or multi-layer insulation.

[0030] In addition to reducing deformation of insulation layers when insulated wires are twisted into twisted pairs, the disclosed invention may be used to reduce deformation of any polymeric material exposed to compressive forces, such as braid indentation, or mechanical systems such as winders, pulleys, or wheels.

[0031] The above presents a simplified summary of the invention in order to provide a basic understanding of some aspects of the claimed subject matter. This summary is not an extensive overview. It is not intended to identify key or critical elements of the invention, nor is it intended to delineate the scope of the claimed subject matter. Its sole purpose is to present some concepts in a simplified form as a prelude to the more detailed description that is presented later.

[0032] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate several aspects of the disclosure and, together with the description, serve to explain the principles of the disclosure. [Brief description of the drawings]

[0033] [Figure 1] 1 is a schematic cross-sectional view of an embodiment of an insulated conductor according to the present disclosure. [Figure 2A] FIG. 2 is a schematic cross-sectional view of an embodiment of a twisted pair. [Figure 2B] FIG. 2 is a schematic cross-sectional view of an embodiment of a twisted pair. [Diagram 3] 1 is a schematic cross-sectional view of an embodiment of an insulated conductor according to the present disclosure. [Figure 4A] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 4B] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 4C] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 5A] 1 is a schematic diagram of an embodiment of a cooling vessel having a secondary structure according to the present disclosure. [Figure 5B] 1 is a schematic diagram of an embodiment of a cooling vessel having a secondary structure according to the present disclosure. [Figure 6] 1 is a graph of crush rate data. [Figure 7] 1 is a graph of surface temperature data and crush rate data versus exposure time. [Figure 8] 1 is a cross-sectional image of a foam-insulated conductor. [Figure 9] 1 is a graph of surface temperature data for foamed and solid polymer insulation versus exposure time. [Figure 10] 1 is a graph showing temperature over time for foamed and solid polymer insulated copper conductors. [Figure 11] 1 is a graph showing temperature over time for foamed and solid polymer insulated copper conductors. [Figure 12] FIG. 2 is a schematic diagram of an embodiment of a twisted pair according to this disclosure. [Figure 13] 1 is a diagram of an embodiment of a cable according to the present disclosure. [Figure 14] 1 is a schematic cross-sectional view of an embodiment of a cable according to the present disclosure. [Figure 15] 1 is a schematic cross-sectional view of an embodiment of a cable according to the present disclosure. [Figure 16] 1 is a schematic cross-sectional view of an embodiment of an insulated conductor according to the present disclosure. [Figure 17] 1 is a schematic cross-sectional view of an embodiment of a cable according to the present disclosure. [Figure 18] 1 is a schematic diagram of an embodiment of a cable according to this disclosure. [Figure 19A] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 19B] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 19C] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 20A] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 20B] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 20C] 1 is a schematic diagram of an embodiment of a cooling vessel according to the present disclosure. [Figure 21] 1 is a graph of Shore D hardness of solid FEP versus time of exposure to liquid nitrogen. [Figure 22] 1 is a graph of Shore D hardness of solid FEP versus exposure time to ambient atmosphere after exposure to liquid nitrogen. [Figure 23A] 1 is a graph of Shore D hardness of solid FEP versus exposure time to ambient atmosphere after exposure to liquid nitrogen. [Figure 23B] 1 is a graph of Shore D hardness of solid FEP versus exposure time to ambient atmosphere after exposure to liquid nitrogen. [Figure 23C] 1 is a graph of Shore D hardness of solid FEP versus exposure time to ambient atmosphere after exposure to liquid nitrogen. [Figure 24] 1 is a graph of Shore D hardness of foamed FEP versus time of exposure to liquid nitrogen. [Diagram 25] 1 is a graph of Shore D hardness of foamed FEP versus exposure time to ambient atmosphere after exposure to liquid nitrogen. [Figure 26] 1 is a graph of Shore D hardness of foamed FEP versus exposure time to ambient atmosphere after exposure to liquid nitrogen. [Figure 27] 1 is a graph showing a comparison of Shore D hardness of solid and foam FEP versus time of exposure to liquid nitrogen. [Figure 28] 1 is a graph showing a comparison of Shore D hardness of solid and foam FEP versus exposure time to ambient atmosphere after exposure to liquid nitrogen. [Figure 29] 1 is a graph showing a comparison of temperature of solid and foam FEP versus time of exposure to ambient atmosphere after exposure to liquid nitrogen. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0034] The embodiments described below represent the necessary information to enable those skilled in the art to practice the present disclosure and show the best mode of carrying out the present disclosure. Upon reading the following description in light of the accompanying drawings, those skilled in the art will understand the concepts of the present disclosure and recognize applications of these concepts not specifically addressed herein. It should be understood that these concepts and applications are included within the scope of the present disclosure and the appended claims.

[0035] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as those commonly understood by those skilled in the art of the present disclosure. Furthermore, terms such as those defined in commonly used dictionaries should be interpreted as having a meaning consistent with the meaning in the context of the specification, and should not be interpreted as such unless they are clearly defined in this specification in an ideal or overly formal sense. Well-known functions or structures may not be described in detail for brevity or clarity.

[0036] The terms "about" and "approximately" are generally intended to mean an acceptable degree of error or variation for the quantity being measured, given the nature or precision of the measurement. Typically, the exemplary degree of error or variation is within 20 percent (%), preferably within 10%, and more preferably within 5% of a given value or range of values. Quantities given in this description are approximate quantities unless otherwise stated, meaning that the term "about" or "approximately" can be inferred if not expressly stated. Quantities in the claims are exact quantities unless otherwise stated.

[0037] When a feature or element is referred to as being "on" another feature or element, it will be understood that it may be directly on the other feature or element and that intervening features and / or elements may also be present. In contrast, when a feature or element is referred to as being "directly on" another feature or element, there are no intervening features or elements. When a feature or element is referred to as being "connected," "attached," or "coupled" to another feature or element, it will be understood that it may be directly connected, attached, or coupled to the other feature or element and that intervening features or elements may also be present. In contrast, when a feature or element is referred to as being "directly connected," "directly attached," or "directly coupled" to another feature or element, there are no intervening features or elements. Although described or illustrated with respect to one embodiment, the features and elements so described or illustrated may be applicable to other embodiments.

[0038] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting. As used herein, the singular forms "a," "an," and "the" are intended to include the plural forms as well, unless the context clearly dictates otherwise.

[0039] Terms such as "first", "second", etc. are used herein to describe various features or elements, but these features or elements should not be limited by these terms. These terms are only used to distinguish one feature or element from another. Thus, a first feature or element discussed below can also be referred to as a second feature or element, and similarly, a second feature or element discussed below can also be referred to as a first feature or element, without departing from the teachings of the present disclosure.

[0040] Terms such as "at least one of A and B" should be understood to mean "A only, B only, or both A and B." The same structure should be applied to longer lists (e.g., "at least one of A, B, and C").

[0041] The term "consisting essentially of" means that in addition to the recited elements, what is stated may also contain other elements (steps, configurations, ingredients, components, etc.) that do not adversely affect the operability of what is stated for the intended purposes set forth in this disclosure. This term excludes other elements that adversely affect the operability of what is stated for the intended purposes set forth in this disclosure, even if such elements may enhance the operability of what is stated for some other purpose.

[0042] In some places, reference is made to standard methods, such as, but not limited to, methods of measurement. It should be understood that such standards are revised from time to time and, unless expressly stated otherwise, references to such standards in this disclosure should be construed as referring to the most recently published standards at the time of filing.

[0043] This disclosure describes embodiments of methods and systems for making wire and cable products having improved electrical performance and / or improved manufacturing features. Although the disclosed invention is generally discussed in the context of intertwining polymer insulated wires to form twisted pairs, it will be understood that the disclosed invention can be adapted for many applications beyond intertwining insulated conductors, including, for example, polymer insulation layers, foamed insulation layers, foam skins, cloth webs, polymer tapes, hollow tubes, rod fillers, armor, and other polymer cable components.

[0044] When a polymeric cable component, such as an insulated conductor, is subjected to a compressive force, for example when the wires are intertwined to form a twisted pair, the polymeric component may be compressed or otherwise deformed. In a polymeric insulation layer, this deformation may disrupt the conductor-to-conductor spacing of the conductive wire, affecting the electrical performance of the wire or resulting cable.

[0045] 1 illustrates a schematic cross-section of an insulated wire having a polymeric insulation layer 110 around a conductor 120. When a force is applied to the insulated wire, the insulation layer 110 may deform. The degree of deformation of the insulation layer 110 may be described by the crush ratio, which is defined as the deformed length / initial OD×100 and expressed as a percentage.

[0046] Figure 2A illustrates a schematic cross-section of two insulated wires, each having a polymer insulation layer 210 around a conductor 220. Figure 2A shows two insulated wires with circular polymer insulation layers in contact with each other and undeformed. The shaded areas of the polymer insulation layer 210 in Figure 2A indicate areas that would be deformed by a compressive force if the two wires were intertwined together.

[0047] Figure 2B illustrates a schematic cross-section of two insulated wires, each having a polymer insulation layer 210 around a conductor 220. Figure 2B shows the two wires in contact with each other after a compressive force has caused deformation of the polymer insulation layer.

[0048] A comparison of the conductor-to-conductor distance between the crushed wire in FIG. 2B and the uncrushed wire in FIG. 2A shows that the deformation of the two insulation layers reduces the distance between the two conductors. This type of compression can occur when twisting the wires together or during other compression events. This reduction in conductor-to-conductor distance has a detrimental effect on the electrical performance of the twisted wires and any resulting cable.

[0049] The forces applied to the polymeric cable components depend on the type and manufacturer of equipment utilized by any particular wire and cable company. For example, there are many different types of cable making machines. Each of these machines will present unique forces to the various elements being cabled. When a wire and cable manufacturer determines how much additional insulation to incorporate into their design to offset deformation, experience, in large part, along with knowledge of the harness of materials, will ultimately determine how much extra insulation is required.

[0050] Within the industry, the term "wall thickness" is used to capture how much insulation and / or sheathing material is needed to produce a desired product. Most application designs will have an absolute minimum wall thickness, an average minimum wall thickness, a nominal wall thickness, and an absolute maximum wall thickness. When compensating for deformation and recession of the insulation layer, the nominal wall thickness is typically considered.

[0051] The softer the insulation material, the greater the amount of additional wall thickness typically required to compensate for lost wall thickness for compression under a given set of conditions. FEP, for example, is a softer insulation than HDPE or PP and will require a greater amount of additional insulation. Understanding the hardness of the insulation material is useful in determining the amount of compensation required. With better control over the amount of deformation, the amount of additional insulation required can be reduced. This benefits both the size and cost of the final product. In some embodiments, the amount of additional insulation added to create a desired cable is reduced by at least about 0.0005 inches, or at least about 0.001 inches, at least about 0.003 inches, at least about 0.005 inches, or at least about 0.01 inches, relative to a cable created under the same conditions but without the cooling techniques described herein.

[0052] Softer insulating polymers, such as fluorinated ethylene propylene (FEP), tend to deform more when a force is applied to the insulation layer than insulation layers made of harder polymers. Foam insulation layers may also be more susceptible to deformation than solid polymers.

[0053] The resistance of an insulating layer to deformation can generally be measured or described in terms of the hardness of the insulating material. As discussed, hardness is a measure of the resistance to localized plastic deformation caused by mechanical indentation or abrasion. Different materials generally have different hardnesses. In some embodiments, Young's modulus can affect the degree of deformation that occurs as a result of a compressive force. Young's modulus is a mechanical property that measures the hardness of a solid material in the elastic region, rather than the plastic region. Young's modulus defines the relationship between stress (force per unit area) and strain (deformation) in a material. The higher the Young's modulus, the less elastic deformation of the material will occur under the same force.

[0054] One method for increasing the hardness and Young's modulus of the polymeric insulation layer is to cool the polymeric material. This cooling can be accomplished by any reasonable method, such as by directly or indirectly exposing the material to a chilled fluid, such as a chilled liquid or gas. In some embodiments, the polymeric cable components can be exposed to chilled water or aqueous solutions. In some embodiments, the polymeric cable components can be exposed to a cryogenic fluid, such as liquid nitrogen. In some embodiments, the polymeric cable components can be exposed to chilled gas or steam. In some embodiments, the polymeric cable components can be exposed to one or more of chilled wheels, rollers, tubes, or other solid surfaces. In some embodiments, the polymeric cable components can be cooled indirectly. For example, the polymeric cable components can be passed through the interior of a tube while the exterior of the tube is cooled. The atmosphere within the tube is chilled, thereby cooling the polymeric cable components. Although the invention described herein is generally described in the context of cryogenic fluids, it will be understood that any of these methods can be used similarly or interchangeably.

[0055] In some circumstances, the time required to cool the entire thickness of the polymeric insulation layer may be impractical. In one embodiment, the disclosed invention cools the exterior surface of the insulation layer and does not cool the interior bulk of the insulation layer to the same extent. In some embodiments, cooling only the outer portion of the insulation layer helps reduce overall deformation of the insulation layer, since the exterior surface is typically the portion of the insulation layer that experiences the most compressive forces during manufacturing.

[0056] FIG. 3 illustrates a schematic cross-section of an insulated wire having a polymeric insulation layer around a conductor 340. The insulation layer in the embodiment depicted in FIG. 3 is a single homogenous polymer layer, but for clarity, FIG. 3 illustrates the homogenous insulation layer as divided into separate concentric sections. The outer surface 310 of the polymeric insulation layer is generally exposed to the external environment and is the first to experience any external compressive forces. The outer portion 320 of the insulation layer is immediately below the outer surface. The inner bulk of the insulation layer 330 surrounds the conductor 340 and is exposed to the least amount of external compressive forces because both the outer surface 310 and the outer portion 320 of the insulation layer must deform before the inner bulk 330 is affected.

[0057] When the polymer insulated wire is exposed to a chilled liquid or cryogenic fluid, such as liquid nitrogen, the outer surface 310 cools rapidly due to direct contact with the cryogenic fluid. The outer portion 320 of the insulation layer will cool next as heat is drawn from the insulation layer into the cryogenic fluid. The rate at which the outer portion of the insulation layer cools will vary based on the thermal conductivity of the polymer material forming the insulation layer. The inner bulk 330 of the insulation layer will cool after the outer surface and outer portion. It will be appreciated that a temperature gradient, rather than a sharp line, forms separating the outer portion 320 from the inner bulk 330.

[0058] As the outer surface and outer portions of the insulation layer cool, the hardness of these portions of the insulation layer will increase, in some embodiments, creating a hardened "skin" on the outer portions of the insulation layer that surrounds the relatively hot inner bulk of the insulation layer.

[0059] If the insulation layer remains in contact with the cryogenic fluid long enough, eventually the entire bulk of the insulation layer will cool, and the hardness of the entire insulation layer will increase. However, wire and cable manufacturing facilities typically make cables at relatively high speeds. To cool the entire thickness of the insulation layer while the cable is moving at relatively high speeds, the length of the cooling equipment may be required to be longer than desired for a particular application. By using embodiments of the disclosed invention, the length of the cooling equipment required may be reduced and deformation of the insulation layer may be minimized. By creating a hardened skin within the homogenous polymer insulation layer, the crush rate can be reduced when the insulated wires are intertwined together or when the polymer insulated wire is exposed to other external compressive forces.

[0060] It will be appreciated that when the polymer insulated conductor is removed from the cryogenic fluid or other cooling medium and exposed to the ambient atmosphere, the polymer insulation begins to return to ambient temperature. As the temperature increases, the hardness of the polymer insulation decreases, making the polymer insulation more susceptible to deformation by compressive forces. In some embodiments of the disclosed invention, the polymer insulation layer is cooled immediately prior to being subjected to a compressive event, such as, for example, intertwining to form a twisted pair. In some applications, the speed at which the insulated conductor moves and the distance between the cooling vessel and the intertwining take-up device will determine the time the polymer insulated conductor is exposed to the ambient atmosphere after cooling but before the application of the compressive force. In some embodiments, the end of the cooling vessel is less than 10 feet from the point at which the polymer insulated conductor is subsequently subjected to the compressive force. In some embodiments, the end of the cooling vessel is less than 8 feet, 6 feet, 4 feet, or 2 feet away from the point at which the polymer insulated conductor is subsequently subjected to the compressive force.

[0061] It will be understood that the harness of a given material is determined by the temperature of that material. Thus, as the temperature of a given material increases and decreases, the hardness decreases and increases, respectively. In some embodiments, the material is cooled just prior to the compressive force, which increases the hardness, and then allowed to return to ambient temperature. The increased hardness at the time of the compressive force can help the material resist deformation due to the compressive force, even though the hardness is only increased temporarily.

[0062] It will be appreciated that the disclosed invention does not require a change in the composition of the polymeric insulation material. The composition of the polymeric insulation layer remains unchanged while the polymeric insulation is cooled, thereby increasing its hardness. The composition of the polymeric insulation layer remains unchanged when any compressive or deforming force is applied to the insulation, and when the polymeric insulation is allowed to return to ambient temperature, thereby reducing its hardness.

[0063] In some embodiments, the conductor may be insulated by more than one layer of insulation. In some embodiments, the conductor may be insulated, for example, by a polymer foam layer and also a solid polymer layer. In some embodiments, the multiple layers of polymer insulation may be made from different polymers. In some embodiments, the multiple layers of polymer insulation may be made from the same polymer. Each layer of insulation may be of a different thickness than any other insulation layer, or may be of approximately the same thickness.

[0064] It will be appreciated that thicker polymer insulation layers may require more time to reach a higher hardness relative to thinner polymer insulation layers because a temperature gradient must propagate through the bulk of the thicker polymer insulation layer, hi some embodiments, the exposure time for which the insulated conductor is exposed to the cryogenic fluid may be adjusted based on the thickness of the polymer insulation layer.

[0065] In some embodiments, some of the conductors of each of multiple twisted pairs contained in a single cable may be exposed to the cryogenic fluid for different amounts of time. By controlling the amount of time the conductors are exposed to the cryogenic fluid, the degree of collapse and the resulting electrical properties of the twisted pairs can be adjusted.

[0066] In some embodiments, increasing the hardness of the polymer insulated conductors causes the conductors to maintain a generally circular cross-section rather than deforming under compressive forces, which can reduce the amount of surface-to-surface contact between two polymer insulated conductors and can reduce frictional or twisting forces between the insulated conductors.

[0067] In some embodiments, the polymer insulated conductor or other polymer cable component is cooled prior to exposure to the compressive force to increase its hardness. In some embodiments, the temperature of the polymer cable component is reduced to offset any heat generated within the polymer cable component by the compressive force. In some embodiments, the temperature of the polymer cable component during or immediately after the compressive event is at or below ambient temperature.

[0068] In some embodiments, the disclosed invention may be utilized to intertwine polymer insulated wires to form a twisted pair. Twisted pair wires are typically formed by twisting two polymer insulated wires around each other using a machine called an intertwining machine. The process of intertwining wires to form a twisted pair creates a compressive force between the two wires at the point where they contact each other. This compressive force increases as the pitch or twisting speed of the twisted pair increases.

[0069] The purpose of intertwining wires to form twisted pairs is to improve the electromagnetic compatibility of the wires. Twisting the pairs reduces electromagnetic radiation from the pairs and reduces crosstalk and electromagnetic interference between adjacent twisted pairs compared to untwisted wires. A single twisted pair can be used to form a single-pair Ethernet cable, or multiple twisted pairs can be combined to form various other forms of cabling, including Ethernet cabling. It is desirable for each insulated conductor of a twisted pair to be a mirror image of the other insulated conductor in the twisted pair. When the two insulated conductors in a twisted pair are mirror images of each other, this achieves improved noise cancellation between the insulated conductors, creating a system of balanced pairs. Often, the layers of insulation around the conductors contained in the twisted pair are affected differently by compressive forces. This can create a difference between the two insulated conductors, resulting in an imbalance, which can reduce noise cancellation and result in undesirable results in the end product.

[0070] In one embodiment, the polymer insulated wire is passed through a cooling vessel before being fed to the entangler. In some embodiments, the cooling vessel exposes the insulated wire to a cryogenic fluid, which increases the hardness of at least the outer surface of the polymer insulation layer. In some embodiments, the cooling vessel contains a pool of cryogenic fluid, such as liquid nitrogen. In some embodiments, the cooling vessel contains a spray of cryogenic fluid. It will be understood that the cooling vessel can be used to expose any polymer cable component to any form of cooling medium. For clarity, the disclosed invention is described in the context of a cryogenic fluid, but chilled air, or any other gas or vapor, and chilled water or any other chilled liquid, or chilled solid surface can be used.

[0071] Figure 4A shows a schematic diagram of a cooling vessel 410 according to one embodiment. As shown in Figure 4A, the insulated wire 420 may enter the cooling vessel 410 through a hole 440 in the cooling vessel below the surface of the cryogenic fluid 430, causing the insulated wire to sink into a pool of cryogenic fluid 430. The cooled insulated wire 420 may exit the cooling vessel 410 through a similar hole 440 in the side of the cooling vessel. In some embodiments, a flexible gasket, membrane or valve may be used to restrict the flow of cryogenic fluid out of the cooling vessel.

[0072] 4B shows another schematic diagram of a cooling vessel 411 according to one embodiment. In some embodiments, an insulated wire 421 is fed downward into a pool of cryogenic fluid 431 using wheels, rollers, or wire guides 441. This allows the cooling vessel to maintain a pool of liquid without leaking. In some embodiments, the cooling vessel includes a perforated top or lid (not shown) that allows the wire to enter the cooling vessel and reduces the overall loss of cryogenic fluid due to evaporation or dissipation.

[0073] 4C shows another schematic diagram of the cooling vessel 412 according to one embodiment. In some embodiments, the cooling vessel 412 includes one or more nozzles 432 that spray the cryogenic fluid or another chilled liquid or gas onto the insulated wire 422. In some embodiments, the insulated wire 422 does not physically contact the cooling vessel or associated equipment, thereby avoiding any compressive forces prior to cooling. In some embodiments, the insulated wire enters and exits the cooling chamber through small holes 442 and is sprayed with the cryogenic fluid. In some nozzle embodiments, there is no permanent pool of cryogenic fluid, so loss of cryogenic fluid is less of a concern.

[0074] It will be appreciated that some embodiments include combinations of the cooling vessels described above. In some embodiments, multiple cooling vessels may be used in series to achieve a particular desired effect. In some embodiments, a single cooling chamber may pass one, or two, or multiple insulated conductors through the cooling chamber simultaneously. In some embodiments, a single cooling chamber may be used to cool two wires for forming into a single twisted pair. In some embodiments, a single cooling chamber may be used to cool multiple insulated wires that may be used to form multiple twisted pairs.

[0075] In some embodiments, the cooling vessel may be at least about 2 feet long, or about 4 feet long, or about 6 feet long, or about 10 feet long, or about 15 feet long. In some embodiments, the cooling vessel may be up to about 20 feet long, or about 15 feet long, or about 10 feet long, or about 8 feet long, or about 6 feet long. In some embodiments, one or more pulleys, wheels, capstans, and / or rollers may be used within the cooling vessel to redirect the path of the polymer cable component within the cooling vessel. This arrangement allows the polymer cable component to remain within the cooling vessel for a longer period of time without increasing the length of the cooling vessel or slowing down the linear velocity of the component. In some embodiments, the polymer cable component enters the cooling vessel in a vapor region at the top of the vessel, where the evaporated cryogenic fluid rises above the liquid cryogenic fluid, and is subsequently redirected through a liquid region of the vessel, where the liquid cryogenic fluid remains. This arrangement allows heat to be transferred from the polymer cable components to the cryogenic vapor first before contacting the cryogenic liquid, thereby reducing the overall heat load transfer to the cryogenic liquid and increasing the total residence time of the polymer cable components within the cooling vessel.

[0076] The length of time the insulated wire is exposed to the cryogenic fluid will depend on the length of the cooling vessel and the speed at which the insulated wire is moving. In some embodiments, the wire is exposed to the cryogenic fluid for a time period of at least about 1 second, or at least about 2 seconds, or at least about 4 seconds, or at least about 6 seconds, or at least about 8 seconds, or at least about 10 seconds. In some embodiments, the wire is exposed to the cryogenic fluid for a time period of up to about 30 seconds, or up to about 20 seconds, or up to about 10 seconds, or up to about 8 seconds, or up to about 6 seconds, or up to about 4 seconds.

[0077] In some embodiments, after exiting the cooling vessel, the insulated wire enters an intertwining device where it is twisted around a second cooled insulated wire to form a twisted pair with less deformation of the two insulation layers. In some embodiments, the insulated wire enters the intertwining device within about 1 second of exiting the cooling vessel, or within about 2 seconds, or within about 4 seconds of exiting the cooling vessel. In some embodiments, the cooling vessel is positioned relative to the intertwining device or other device that applies a compressive force to the insulated wire such that the polymer insulated wire is subjected to a compressive force before the increased hardness of the polymer insulated wire is reduced by more than about 10%, or before the increased hardness of the polymer insulated wire is reduced by more than about 20%, or before the increased hardness of the polymer insulated wire is reduced by more than about 30%. In other words, in some embodiments, the cooling vessel is positioned such that the polymer insulated wire exiting the cooling vessel is subjected to any subsequent compressive force before the polymer insulated wire warms significantly, thereby reducing its hardness.

[0078] In some embodiments, one or more secondary structures may be positioned around the polymer insulated conductors after they exit the cooling chamber to maintain an atmosphere cooler than the ambient temperature. FIG. 5A illustrates an example of a cooling vessel 510 with a secondary structure 550 positioned around the polymer insulated conductors 520 as they leave the cooling vessel. In some embodiments, the secondary structure 550 is a hollow tube positioned to maintain a chilled atmosphere around the polymer insulated wires prior to application of compressive forces to the wires as part of the entanglement process. The secondary structure 550 may be made of any thermally conductive material, including, for example, metal and / or polymer. In some embodiments, the secondary structure 550 may be a larger tube positioned to surround the wires as they exit the cooling chamber to maintain an increased hardness before the wires are exposed to any compressive or deforming forces. In some embodiments, the secondary structure 550 may be a tube with an adjustable length that can expand and / or contract to adjust the residence time of the polymer cable components within the tube. In some embodiments, the secondary structure includes a portion that can be removed or opened, such as a top or lid. In such an embodiment, the secondary structure can be opened to allow for the initial treading or lacing of the wire or cable line, and then closed to seal off the ambient atmosphere and retain a cooler atmosphere within the secondary structure.

[0079] In some embodiments, the secondary structure is arranged to receive the cryogenic fluid from a cooling vessel. In one example, the secondary structure may be arranged to receive cold nitrogen vapor from a pool of evaporated liquid nitrogen contained within the cooling vessel. By maintaining an atmosphere at a cooler temperature than ambient around the wires leaving the cooling vessel, the secondary structure can help maintain the increased stiffness as the wires move from the cooling vessel to the entanglement device or during other subsequent steps involving compressive forces. In some embodiments, any cryogenic fluid that leaks out of the cooling vessel is received by the secondary structure. In the case of a cryogenic liquid, the cryogenic liquid received by the secondary structure may evaporate within the secondary structure, thereby creating a chilled atmosphere within the secondary structure and preventing any leakage of the cryogenic liquid onto the manufacturing floor.

[0080] In some embodiments, the secondary vessel may be connected to the cooling vessel, the entanglement device, or both. In some embodiments, the secondary structure may direct cryogenic vapor expanding or evaporating from the cooling vessel through the secondary structure and into the entanglement device. In such embodiments, the atmosphere within the entanglement device may be maintained at a lower temperature than the ambient atmosphere surrounding the entanglement device.

[0081] Although the present invention is generally described in the context of exposing polymer cable components to cryogenic fluids, it will be understood that other methods of cooling the polymer cable components and thereby increasing their hardness may be used.

[0082] In some embodiments, the polymer cable components may be passed inside a chilled tube. The exterior of the tube may be exposed to a cooling medium, such as chilled or cryogenic fluid, which reduces the temperature of the tube itself. In such an embodiment, the atmosphere inside the chilled tube will be indirectly cooled by the chilled or cryogenic fluid, as heat is drawn from the tube into the chilled or cryogenic fluid. The polymer cable components may be cooled by exposure to the chilled atmosphere inside the tube, which increases the hardness of the polymer cable components. In some embodiments, the tube is only slightly larger than the polymer cable components passing through it. The degree of cooling of the polymer cable components can be controlled by reducing the distance between the inner surface of the tube and the polymer cable components. In some embodiments, the tube may have a removable or hinged lid that can open the tube to facilitate initial lacing of the polymer cable components through the tube. Once the tube is closed, the exterior of the tube can be exposed to chilled or cryogenic fluid to establish a chilled interior atmosphere within the tube. In some embodiments, the tube may be telescopic and modular components may be used to increase or decrease the length of the tube during continuous operation, which in some embodiments allows operators to adjust the total residence time of the polymer cable components in the cooling atmosphere of the tube without stopping production to change the tube, tube length, and / or tube components.

[0083] FIG. 5B illustrates a schematic of the chilled tube embodiment described above. In the illustrated embodiment, the tube 610 passes through a chilled material 620, which creates a chilled atmosphere within the tube 610. The polymer cable component 605 passes through the chilled tube 610 and is exposed to the chilled atmosphere within the tube 610. In the illustrated embodiment, a heat exchanger 630 may be used to control the temperature of the chilled material 620. In some embodiments, the temperature of the chilled material 620 may be adjusted depending on the temperature of the atmosphere within the tube 610. In some embodiments, the chilled material 620 may be a chilled liquid that is circulated around the tube 610. If the atmosphere within the tube 610 increases beyond a desired range, the chilled liquid may be circulated faster and the temperature of the chilled liquid may be reduced until the temperature of the atmosphere within the tube 610 is in the desired range.

[0084] In some embodiments, the chilled tube contains intake holes or slits configured to allow a certain amount of chilled material to move into the tube. The size, shape and number of these holes or slits may be arranged differently depending on the expected conditions. In some embodiments, the chilled material is a cryogenic liquid that can enter the tube through the holes or slits. This will reduce the temperature inside the tube and also allow some direct contact between the polymer cable components and the cryogenic fluid. In some embodiments, the amount of cryogenic fluid that enters the tube can be adjusted such that under operating conditions, all of the cryogenic fluid that enters the tube evaporates within the tube. This prevents the cryogenic liquid from leaking out of the cooling device and allows for faster and / or greater cooling of the polymer cable components.

[0085] In some embodiments, chilled wheels, rollers or pulleys may be used to increase the hardness of the polymer cable components. Wire and cable manufacturing is generally a continuous process involving a number or wheels, rollers and / or pulleys for a variety of different purposes, such as to guide the process, control tension, and / or gather the components for cable making. When the polymer cable components contact these wheels, at least some compressive force is applied to the cable components. In some embodiments, chilled or cryogenic fluid may be passed through the inside of the wheels, which cools the wheels. Because the solid surface of the wheels rotates, the polymer cable components in contact with the rotating surface can be cooled without incurring significant additional deformation forces. When the polymer cable components contact the wheels, they are at least slightly cooled, resulting in them becoming harder. In some embodiments, a series of chilled wheels, rollers or pulleys may be used to increase the exposure time between the cable components and the chilled surfaces, allowing the cable components to reach a desired degree of hardness before being subjected to a subsequent compressive force.

[0086] In some embodiments, rather than using a liquid or solid cooling medium, chilled air or another chilled gas or vapor can be used to reduce the temperature and increase the hardness of the polymer cable components. Seasonal variations in wire and cable manufacturing are a known phenomenon. During warmer months, manufacturing facilities may have higher ambient temperatures. This can increase the temperature and correspondingly decrease the hardness of the polymer cable components used in a particular facility. To address this seasonal variation, some manufacturing facilities utilize standard air conditioning to maintain a relatively constant temperature within the facility. However, maintaining moderate temperatures throughout the manufacturing facility is not required to increase the electrical performance of the cables produced.

[0087] In some embodiments, air conditioning equipment can be used to direct cool air directly to the entanglement device or cooling chamber surrounding the polymer cable components. The temperature of the atmosphere surrounding the polymer cable components can be reduced to increase the hardness of the polymer just before or during the compression event. In some embodiments, air conditioning equipment can be used to generate air at a temperature lower than would be fully acceptable throughout the manufacturing facility. In some embodiments, the air conditioning system can be configured to direct air at less than about 60°F to the polymer cable components. In some embodiments, the air conditioning or refrigeration system can be configured to direct air at less than about 50°F, or less than about 40°F, or less than about 30°F, or less than about 20°F, or less than about 10°F, or less than about 0°F to the polymer cable components. In some embodiments, the air conditioning or refrigeration system may be configured to direct air below about 10°C, or below about 5°C, or below about 0°C, or below about -5°C, or below about -10°C, or below about -15°C to the polymer cable components.

[0088] In some embodiments, a structure may be used to contain a cooler atmosphere around the polymeric cable components before or during a compression event. In some embodiments, a chamber may be used around the entanglement winding device to contain a cooler atmosphere. It will be appreciated that for some applications, dedicated refrigeration equipment may be required to generate large volumes of very cold air. It will also be appreciated that cold air may be applied to the polymeric cable components at any step in the manufacturing process where increased hardness would help reduce deformation due to compression forces.

[0089] In one illustrative example, multiple twisted pairs of fluorinated ethylene propylene (FEP) insulated wire were produced at a line speed of 19 m / min, or about 63 ft / min. The entanglement machine parameters were set at 3,000 twists / min and a twist length of 6.2 mm. Prior to entering the entanglement machine, the wires were passed through a cooling vessel and submerged in liquid nitrogen for various lengths of time. The crush rate of the resulting twisted pairs was examined using computed tomography (CT) scans.

[0090] Table 1 below shows a table of data collected over three trials. Each trial included four samples that were passed through cooling vessels of varying lengths. The lengths of the cooling vessels varied from zero feet (control) to two feet, four feet, and six feet. The entanglement parameters listed above, including linear speed, were kept constant throughout all trials.

[0091] [Table 1]

[0092] As can be seen from Table 1, the average crush rate decreased as the length of the cooling vessel increased. Since a linear velocity of 19 meters / min is approximately 1 foot / second, the length of the cooling vessel in feet is approximately equal to the time the wire was exposed to liquid nitrogen, measured in seconds.

[0093] Figure 6 shows a graph of the data presented in Table 1. As can be seen by the graph in Figure 6 and Table 1, the average crush rate was reduced from 6.74% when the FEP insulated wire was not exposed to liquid nitrogen to 1.09% when the FEP insulated wire was exposed to liquid nitrogen for a period of about 6 seconds, which corresponds to a reduction in the crush rate of about 83% in about 6 seconds.

[0094] Table 2 (below) shows the surface temperature of samples of FEP insulated wire exposed to various lengths of liquid nitrogen. A temperature probe was used to measure the surface temperature while the FEP insulated wire was entangled after passing through the cooling chamber. The entanglement parameters match those listed above, including line speed.

[0095] [Table 2]

[0096] Figure 7 shows the data presented in both Tables 1 and 2 presented on a single graph. As can be seen from Figure 7, the surface temperature of the FEP coated wire decreases significantly after exposure to liquid nitrogen for about 2 seconds and then continues to decrease at a slower rate. The crush rate of the FEP insulated wire decreases after exposure to liquid nitrogen for about 2 seconds and continues to decrease as the length of the cooling vessel and the time the wire is exposed to liquid nitrogen increases.

[0097] The reduction in surface temperature of the insulated wire and the corresponding reduction in crush rate indicate that it is not always necessary to expose the insulated wire to cryogenic fluid for extended periods of time to reduce the crush rate. In some embodiments, it is not necessary to reduce the temperature throughout the thickness of the insulation layer to dramatically reduce the crush rate. The outer skin of the insulation layer can be cooled, which increases the hardness of the outer portion of the insulation layer and reduces the amount of crush caused by intertwining the insulated wire.

[0098] Without being bound by theory, it is believed that the decrease in crush rate is due to an increase in hardness of the outer portion of the FEP insulated wire. As the insulated wire is exposed to liquid nitrogen for an extended period of time, the thickness of the outer portion of the insulation layer with increased hardness increases. The extent of the increase in hardness at the outer surface of the polymer insulation layer may also increase as the wire is exposed to liquid nitrogen for an extended period of time.

[0099] By briefly exposing the polymer insulated wire to liquid nitrogen or another cryogenic fluid, a skin of hardened polymer can be formed in a homogenous polymer layer. This hardened layer of polymer reduces deformation of the polymer insulation layer when the wire is exposed to external forces. By reducing deformation of the polymer insulation, the conductor-to-conductor distance can be maintained more consistently. In some embodiments, the disclosed method can be used to reduce the total amount of polymer insulation used while maintaining the same conductor-to-conductor distance. In some examples, reducing deformation of the polymer insulation layer increases the electrical performance of the wire and the resulting cable. The reduced amount of deformation also helps maintain the shape of each insulated conductor, improving the electrical integrity between the two insulated conductors of the twisted pair and maintaining the balance of the twisted pair.

[0100] In some embodiments, the exterior surface of the polymeric insulation layer drops below 0° C. while the interior portion of the polymeric insulation layer remains above about 5° C. In some embodiments, less than half the thickness of the polymeric insulation layer will have a temperature below about 5° C.

[0101] In some embodiments, the polymer insulation layer, or a portion of the polymer insulation layer, may be a foamed polymer. In such embodiments, the foamed polymer insulation contains many small pockets of air that arise during the manufacturing process. Air is known to be an excellent electrical insulator, and therefore, incorporating air pockets throughout the polymer insulation layer reduces the dielectric constant of the insulation layer. This is because air has a dielectric constant of 1.0, which is favorable relative to the dielectric constants of other materials, such as FEP (2.0), polyethylene (2.3), and polyvinyl chloride (3.5).

[0102] Air has good dielectric values ​​but does not provide mechanical hardness. Therefore, foamed materials or other polymer components incorporating air will have a lower hardness than similar components that do not incorporate air. Air can be incorporated into polymer cable components in multiple ways (small bubbles, large bubbles, cavities, etc.), ultimately resulting in reduced strength depending on the percentage of air substituted for solid polymer and the size of the air cavity utilized. In some embodiments, the methods for increasing hardness described herein are useful for increasing the hardness of the remaining polymer material that is not substituted by air. Foamed polymers are more susceptible to deformation than solid polymers, and the amount of additional material added to inhibit deformation may increase. In some embodiments, the Shore D hardness of the foamed polymer material increases by at least about 10% before or during a compression event relative to a similar material at 20°C.

[0103] Figure 8 shows a cross-sectional image of a foam insulated conductor having multiple air pockets distributed throughout the insulation layer, it will be understood that these air pockets are closed and do not allow air or any other fluid to migrate through the insulation layer.

[0104] In some instances, a single wire insulated with foamed FEP (rather than solid FEP) was entangled in a Setic entangler and analyzed for crush rate and electrical impedance. Samples of the foamed FEP insulated wire were exposed to cryogenic fluid for various lengths of time. The samples exposed to cryogenic fluid were compared to samples of the same foam insulated wire that were not exposed to cryogenic fluid.

[0105] In one example, a pair of intertwined wires was used as a control and was not exposed to any cryogenic fluid, while a similar pair of foamed polymer insulated wires was exposed to a liquid nitrogen bath for a period of 5.6 seconds prior to intertwining. The twist length of the intertwined pair made using both sets of wires was 8.5 mm. For this analysis, a 6 inch sample of each of the two intertwined pairs was imaged using X-ray / CT at three separate locations along its length.

[0106] As can be seen in Table 3 below, the average crush rate for the foam insulated twisted wires decreased from an average of 17.75% when the wires were not exposed to liquid nitrogen to an average of 12.92% when the twisted wires were exposed to liquid nitrogen for a period of 5.6 seconds. This represents an improvement of 27.21%. Crush rate analysis was performed using X-ray / CT. Table 3 shows the crush rate data for each of the three locations analyzed for both the control and treated wires. The electrical impedance of the cryogenically cooled twisted pairs also increased from 136 ohms to 146 ohms, which was an increase of 10 ohms or 7.4% over the control twisted pairs.

[0107] [Table 3]

[0108] In another example, a second pair of FEP foam insulated intertwined wires was used as a control and was not exposed to any cryogenic fluid, while a similar pair of wires was exposed to a liquid nitrogen bath for a period of 9.1 seconds prior to intertwining. The twist length of the intertwined pairs made using these wires was 8.5 mm. Again for this analysis, a 6 inch sample of each of the intertwined pairs was imaged using X-ray / CT at three separate locations along its length.

[0109] As can be seen in Table 4 below, the average crush rate of the intertwined wires decreased from an average of 18.84% when the wires were not exposed to liquid nitrogen to an average of 9.74% when the wires were exposed to liquid nitrogen for a time of 9.1 seconds. This represents an improvement of 48.3%. Crush rate analysis was performed using X-ray / CT. Table 4 shows the crush rate data for each of the three locations analyzed for both the control and treated wires. The electrical impedance of the cryogenically cooled twisted pairs also increased from 142 ohms to 154 ohms, which was an increase of 12 ohms or 8.5% over the control twisted pairs.

[0110] [Table 4]

[0111] One benefit of the disclosed invention is the ability to create twisted pairs and / or other cable designs with improved electrical properties due to increased hardness and reduced amount of deformation during the intertwining, cable making and / or manufacturing process. One source of deformation of the insulation layer in a twisted pair is the intertwining process, where two insulated conductors are twisted around each other. The degree of deformation that occurs during the intertwining process is affected by several factors, including, for example, the twist length, the tension of the wires, the insulation material, the hardness of the insulation and / or the amount of heat generated within the polymer insulation during the intertwining process. To minimize deformation, it may be desirable to increase the hardness of the insulation material during the intertwining process, when the insulated conductors are exposed to the greatest deformation forces. As discussed, one way to temporarily increase the hardness of the insulation layer is to reduce the temperature. In some embodiments, it is desirable to reduce the temperature of the insulation layer while the wires are being intertwined.

[0112] In some examples, the relationship between cryogenic fluid exposure time, surface temperature and crush rate was further investigated for both solid and foamed polymer insulated conductors. In the example below, a pair of FEP insulated conductors were entangled together at a speed of 19 m / min after exposure to a cryogenic fluid. The surface temperature of the insulation layer was measured by direct contact with a temperature probe placed at the first contact point of the two insulated conductors.

[0113] Both the foam FEP insulated wire and the solid FEP insulated wire were exposed to cryogenic fluid (liquid nitrogen) for various lengths of time and the surface temperatures were measured. Table 5 shows the results of this example. Figure 9 shows a graph of these results.

[0114] [Table 5]

[0115] Table 5 and Figure 9 show that there is a significant difference in the surface temperatures of the foamed and solid polymer insulated conductors, even when exposed to cryogenic fluid for the same amount of time. After exposure to liquid nitrogen for a period of 6 seconds, the foamed insulated wire maintained a significantly lower surface temperature than the solid polymer insulated conductor.

[0116] The surface temperature of the insulated conductor was measured approximately 1 second after the conductor was removed from the liquid nitrogen. Without being bound by theory, it is believed that the surface of the solid polymer insulation warms up faster than the surface of the foam insulation layer. The foam insulation layer contains multiple closed air pockets. The air trapped in these air pockets cools while the foam insulated wire is immersed in liquid nitrogen, and the cooled air can then slow down the warming of the surrounding insulation layer. In other words, the cooled air pockets in the foam insulation layer can help maintain a lower surface temperature of the foam insulation layer compared to the solid polymer insulation layer. Over time, both the solid polymer insulation layer and the foam insulation layer will warm up to the ambient temperature, but the foam insulation layer may maintain a significantly cooler temperature for a longer period of time.

[0117] In some embodiments, the cable is made without significantly deforming the polymer cable components that are incorporated into the cable. Many polymer cable components have generally circular cross sections, and many have approximately equal diameters. Similarly, the generally circular cross sections of many polymer cable components will have many radii that are all approximately equal to each other before the cable is compressed or deformed. To be clear, the radius with the maximum length is approximately equal to the radius with the minimum length before the polymer cable component is compressed or deformed. Although there are some natural deviations in the wall thickness of the polymer cable components, the maximum and minimum radii are generally within 3% of each other. In some polymer cable components, the initial maximum and minimum radii may be within 5% of each other before being compressed or deformed.

[0118] In some embodiments, the generally circular cross-section of the polymer cable component is preserved after the polymer cable component is subjected to a compressive or deforming force. As described herein, increasing the hardness of the polymer cable component may cause the polymer component to deform less, thereby maintaining the generally circular cross-section. In some embodiments, after the polymer cable component is subjected to a compressive force, the maximum and minimum major radii are within about 10% of each other. In some embodiments, the maximum and minimum major radii are within about 8% or about 5% of each other. In some embodiments, the maximum and minimum major radii are within about 15% or about 12% of each other. It will be appreciated that the closer the maximum and minimum major radii are to each other, the closer the cross-section is to a circle and generally the less the polymer cable component is deformed.

[0119] In some embodiments, cooling the cable component for a time period of less than about 10 seconds can increase the hardness of the polymeric cable component such that the polymeric component is less deformed after being subjected to a compressive or deforming force. In some embodiments, after the polymeric cable component is subjected to a compressive force, the maximum and minimum major diameters are within about 10% of each other. In some embodiments, the maximum and minimum major diameters are within about 8% or about 5% of each other. In some embodiments, the maximum and minimum major diameters are within about 15% or about 12% of each other. It will be appreciated that the closer the maximum and minimum major diameters are to each other, the more circular the cross section will be and generally the less deformation the polymeric cable component will have.

[0120] Intertwining the insulated conductors while they are still in a cooled state and therefore have a high hardness is one way to reduce the amount of deformation during the intertwining process. In some embodiments, this results in a lower crush rate and improves the electrical properties of the resulting twisted pair. In some embodiments, the amount of time the insulated conductors are exposed to the cryogenic fluid and / or the amount of time the cooled insulated conductors are exposed to ambient temperature before intertwining may be adjusted to adjust the electrical properties of the resulting twisted pair.

[0121] In some embodiments, the crush ratio and / or associated electrical properties of the individual conductors or twisted pairs may be tailored to create multiple twisted pairs with approximately the same propagation delay. In some embodiments, twisted pairs with shorter twist lengths may be intertwined while the individual insulated conductors are cooler and therefore have a higher hardness to create twisted pairs with reduced propagation delays than twisted pairs with longer twist lengths. In some embodiments, twisted pairs with longer twist lengths may be intertwined while the individual insulated conductors are hotter than twisted pairs with shorter twist lengths to create twisted pairs with greater propagation delays than twisted pairs with shorter twist lengths. In some embodiments, the surface temperature of the insulated conductors of the first twisted pair may be adjusted relative to the surface temperature of the insulated conductors of the second twisted pair to create first and second twisted pairs with approximately equal propagation delays over 100 meters, or within 10 nanoseconds of each other over 100 meters, or within 15 nanoseconds of each other over 100 meters, or within 25 nanoseconds of each other over 100 meters, or within 50 nanoseconds of each other over 100 meters. It will be appreciated that the surface temperature of the insulated conductors may be adjusted by adjusting the time interval during which the insulated conductors are exposed to the cryogenic fluid, or by adjusting the time interval after the insulated conductors are removed from the cryogenic fluid but before entangling the conductors or applying other compressive forces. It will also be appreciated that other methods of cooling may be used besides exposure to a cryogenic fluid as described herein. In all forms of cooling, the overall degree of cooling may be adjusted by controlling the temperature of the cooling material and / or the time the polymer cable components are exposed to the cooling material. Similarly, regardless of the cooling method used, the temperature of the polymer cable component when exposed to a compressive or deforming force can be controlled by adjusting the amount of time the polymer cable component is exposed to the ambient atmosphere after cooling and before being exposed to the force.

[0122] In some embodiments, the first, second, third and / or fourth pairs of polymer insulated conductors, each pair including two polymer insulated conductors, are temporarily cooled to increase the hardness of each pair to a degree. In some embodiments, the degree of hardness increase may be different for each pair. Once the pairs of polymer insulated conductors are at the desired hardness, the pairs are twisted together to form the first, second, third and / or fourth twisted pairs. Each twisted pair has a propagation delay over 100 meters. In some embodiments, for the first, second, third and fourth propagation delays over 100 meters, the difference in propagation delay over 100 meters is within 50 nanoseconds of each other. In some embodiments, the propagation delays are all within 25 nanoseconds of each other. In some embodiments, the first, second, third and fourth propagation delays over 100 meters have a delay time difference of less than about 25 nanoseconds.

[0123] In some embodiments, the first, second, third and / or fourth pairs of polymer insulated conductors are cooled for different times in order for each pair to individually reach a desired hardness. In some embodiments, the cooling periods are all less than about 20 seconds, or all less than about 15 seconds, or all less than about 10 seconds. In some embodiments, the first time is between about 8-10 seconds, the second time is between about 6-8 seconds, and the third time is between about 4-6 seconds. In some embodiments, the fourth time is less than about 4 seconds, or may be zero seconds, indicating that one of the four pairs may not be significantly cooled at all.

[0124] In some embodiments, the cooling time and / or degree of hardness increase of a polymer insulated conductor is related to the expected twist length of a twisted pair made from that polymer insulated conductor. In general, shorter twist lengths require a longer cooling period and / or a greater hardness increase before entanglement than other pairs of conductors.

[0125] In some embodiments, the first, second, third and / or fourth twisted pairs have first, second, third and / or fourth twist lengths, respectively. The first twist length is shorter than the second twist length, and the second twist length is shorter than the third twist length. In some embodiments, the first cooling time is longer than the second cooling time, and the second cooling time is longer than the third cooling time.

[0126] In some embodiments, the first, second, third and / or fourth twisted pairs have a first, second, third and / or fourth collapse ratio, respectively, In some embodiments, the first collapse ratio is less than the second collapse ratio, and the second collapse ratio is less than the third collapse ratio.

[0127] In some embodiments, the first, second, third and fourth twisted pairs have first, second, third and fourth signaling rates, respectively. In some embodiments, the first signaling rate is greater than the second signaling rate, and the second signaling rate is greater than the third signaling rate.

[0128] In some embodiments, the first, second, third and / or fourth pair of polymer insulated conductors each have a different increased hardness, in some embodiments, the increased hardness of the first pair of polymer insulated conductors is greater than the increased hardness of the second pair of polymer insulated conductors, which is greater than the increased hardness of the third pair of polymer insulated conductors.

[0129] It will be appreciated that when two insulated conductors are intertwined together, the generally circular cross-section of each insulated conductor is at least slightly distorted. The more circular the cross-section of each insulated conductor, the greater the amount of air that is retained in the gap between the two insulated conductors. If more air is retained in the gap, the overall dielectric constant of the twisted pair of conductors is reduced and the speed of propagation is increased. By cooling the polymer insulated conductor to increase its hardness while the conductors are intertwined to form the twisted pair, the polymer insulation is less distorted and maintains a more circular cross-section. It will be appreciated that the dielectric constant of the insulating material itself is not increased or decreased. However, if the insulation layer retains a generally circular cross-section and more air is incorporated in the gaps of the twisted pair, the dielectric constant of the resulting twisted pair may be reduced. In some embodiments, the purpose of cooling the polymer insulated conductor is to retain more air in the gaps of the resulting twisted pair.

[0130] In some examples, the temperature of the conductors in the twisted pairs was analyzed both during and after exposure to a cryogenic fluid (liquid nitrogen). The analysis was based on the electrical resistance of the conductors using the equation shown below. Equation 1:

number

[0131] In one example, the a of copper at 20°C is 0.00393K. -1 It is known that R refwas determined to be 1.25 ohms based on the calculations described below. To analyze the conductor temperature, the twisted pair was connected to a handheld cable analyzer which recorded the conductor's resistance in real time. The insulated conductor was immersed in a liquid nitrogen bath and the resistance was recorded over time. Equation 1 (above) was then solved for T.

[0132] In this example, a 24' 9" length of FEP insulated copper wire was used. The resistance of the 24' 9" wire is known to be 1.51 ohms. The resistance of the 6" wire is known to be 0.26 ohms. R ref To calculate the value of R, subtract the resistance of the 6 inch copper conductor from the resistance of the 24 ft 9 in copper conductor to subtract the approximate resistance of any other components in the circuit that are not insulated conductors. R ref Once R is determined to be 1.25 ohms, the measured value of R can be used to solve Equation 1 for T.

[0133] The calculated temperature of the copper conductor over time is shown in Figures 10 and 11. Figure 10 shows the first 20 seconds after the conductor was immersed in liquid nitrogen in more detail. Figure 11 shows the temperature of the conductor as it was immersed in liquid nitrogen and also after removal from liquid nitrogen. The conductor was placed in the liquid nitrogen bath at time = 0. During the first 5-10 seconds, the conductor temperature dropped rapidly until it leveled off at about -176°C. The cable remained in the liquid nitrogen bath for 120 seconds. As shown in Figure 11, when the conductor was removed from the liquid nitrogen bath at 120 seconds, the conductor temperature started to warm up in reverse. Both the solid insulated conductor and the foam insulated conductor reached about 0°C about 40 seconds after removal from liquid nitrogen. As can be seen from Figures 10 and 11, the solid insulated conductor and the foam insulated conductor maintained generally similar temperatures relative to each other when cooling in liquid nitrogen and when warming after removal from liquid nitrogen.

[0134] The disclosed invention is generally described in terms of intertwining twisted pairs, but may be applied to a wide variety of other applications.

[0135] In some embodiments, when two insulated conductors are brought together to form a twisted pair, additional tape, filler, or hollow tube may be added or incorporated into the twisted pair. In the case of tape, the tape may be added between the insulated conductors, on the exterior surface of the twisted pair unit, and / or surrounding the twisted pair unit.

[0136] FIG. 12 shows a schematic diagram of a twisted pair incorporating tape, according to an embodiment. As shown in FIG. 12, a tape 930 may be placed between two insulated conductors 920 of a twisted pair 910. The tape 930 is subjected to forces during twisting of the twisted pair. As a result of these forces, the tape 930 may be compressed or otherwise deformed during the entanglement process. Deformation of the tape 930 may result in increased capacitance, increased insertion loss, decreased electrical impedance, and / or other undesirable effects in the electrical properties of the resulting twisted pair. Increasing the hardness of the tape 930 just prior to subjecting it to the forces of the entanglement process may reduce deformation of the tape and may preserve or enhance the electrical properties of the resulting twisted pair. As described elsewhere herein, the hardness of the tape may be increased by exposing the tape to a cryogenic fluid.

[0137] FIG. 13 illustrates a schematic of an embodiment of wrapping tape around twisted pairs. In some embodiments, one or more twisted pairs 1010 can be surrounded by tape 1020. Each twisted pair 1010 may contain two conductors 1030 surrounded by an insulating layer 1040. In some cables, multiple twisted pairs 1010 are surrounded by an armor 1050. The tape 1020 can be tightly formed around the twisted pairs 1010, which can cause deformation, increase capacitance, decrease impedance, and / or increase insertion loss. In some embodiments, the tape 1020 can include a combination of metal and polymer insulating materials. As described, polymer materials can be susceptible to compression or other forms of deformation. In some embodiments, before wrapping the tape around the twisted pairs, the tape is passed through a cooling chamber where it is immersed, sprayed with, or otherwise exposed to a cryogenic fluid or other cooling medium. By exposing the tape to a cryogenic fluid, the hardness of the polymer increases, making the tape more rigid and resistant to deformation. The amount of air between the twisted pairs and the layer of tape surrounding the twisted pairs can be increased through a higher stiffness (i.e., increased stiffness) of the tape. This is because a stiffer tape, by itself, will not conform more tightly around the insulated conductor and will maintain a larger amount of air space inside the wrapped tape than a polymer tape having a lower hardness. Increasing the amount of air trapped between the tape and the twisted pairs will improve the electrical performance of the wire or resulting cable. Air is a ferroelectric material. Increasing the volume of air within a cable or insulation layer generally has a positive effect on the electrical performance of the resulting wire and / or cable.

[0138] FIG. 14 illustrates, in schematic form, a cross-section of an embodiment in which a hollow tube is incorporated into a twisted pair cable. FIG. 14 shows a cable including two conductors 1110, each surrounded by an insulation layer 1120. The insulated conductors are positioned within an outer sheath 1130. In some embodiments, the twisted pair may be combined with a hollow tube 1140 and / or a filler positioned in the gap between the two insulated conductors to create additional air space 1150 within the outer sheath 1130. These hollow tubes 1140 are typically made from polymeric materials and may be compressed or otherwise deformed when compressed against the insulated wires of the twisted pair during the entanglement process. If the hollow tube or filler deforms, the amount of air contained within the hollow tube and / or contained within the outer sheath may be reduced. Additionally, if the hollow tubes or fillers deform, the pair-to-pair spacing may decrease or become inconsistent, thereby increasing the amount of crosstalk between different twisted pairs. In some cases, reduced pair-to-pair spacing may also increase the capacitance, increase insertion loss, decrease impedance, and / or otherwise degrade the electrical performance of the resulting cable.

[0139] Exposing the hollow tubes 1140 or filler to cryogenic fluid increases their hardness, allowing them to withstand deformation and collapse into the gaps in the twisted pairs, thereby maintaining the air spaces 1150 and improving electrical performance. The air pockets formed between the hollow tubes 1140 and gaps in the pairs are useful for electrical performance because air has a dielectric constant of 1.0, which is favorable relative to the dielectric constants of other materials, such as FEP (2.0), polyethylene (2.3), and polyvinyl chloride (3.5). In some embodiments, maximizing the air content is useful for the electrical performance of the wire and cable.

[0140] FIG. 15 illustrates a cross-section of an embodiment in which protrusions are used to increase air space, reduce material costs, and / or reduce weight. In some embodiments, the outer sheath 1210, twisted pairs 1220, and / or hollow tube 1230 include protrusions 1240 or striations on the inner and / or outer surfaces to create additional air space 1250. In some embodiments, the protrusions 1240 and / or striations are susceptible to deformation. In such embodiments, increasing the hardness of the striations and / or hollow tube 1230 including the protrusions 1240 to prevent deformation or collapse of the protrusions 1240 may help maintain and / or maximize the air space 1250 in the cable.

[0141] In some embodiments, the protrusions from the hollow tube, insulation layer, or armor layer are formed during the profile extrusion of the cable component. In some embodiments, the protrusions can be easily compressed or deformed. Hardening the surface by exposing the material to a cryogenic fluid can help reduce the effect of forces on the protrusions, thereby maintaining the volume of air that would be present if the protrusions were not compressed or deformed.

[0142] It will be appreciated that not only may the polymer insulated wire be exposed to a cryogenic fluid to increase hardness, but the hollow tube, filler tube, tape, sheath and / or other polymer cable making components may be exposed to a cryogenic fluid or another cooling medium. By reducing deformation of the cable components, the volume of air within the cable may be maintained or increased, improving the electrical performance of the cable over similar cables that are compressible or deformable.

[0143] FIG. 16 illustrates a schematic cross-section of an embodiment in which a conductor is insulated by multiple layers of insulation. In some embodiments, multiple layers of different insulation materials may be used to surround the conductor. In some embodiments, a layer of an outer material with a high inherent hardness may be used, which may help reduce compression of the softer inner material layer. In some embodiments, a layer of foam insulation 1320 may be used to insulate the conductor 1310. Because foam insulation contains many separate air pockets, the hardness of the foam insulation layer may be significantly lower than a solid insulation layer of the same polymeric material. As such, the foam insulation layer may be more susceptible to compression during manufacturing. A skin layer 1330, which is a material with a higher hardness than the underlying foam insulation 1320, may be used to reduce compression of the foam insulation 1320. To reduce compression or deformation of the insulation layer during the manufacturing or cable making process, the hardness of the outer portion of the insulation material may be temporarily increased by exposing the insulated conductor (including the foam insulation and skin) to a cryogenic fluid. It will be appreciated that the entire thickness of the inner foam insulation layer may not need to be cooled in order for the outer portion of the foam insulation layer to have a temporary increased hardness and withstand compression during the cable fabrication process. It will be appreciated that the skin 1330 may or may not be a foam itself. In some embodiments, the skin will be a solid polymer designed to protect the underlying foam insulation. In some embodiments, the skin layer will comprise a different polymer than the foam insulation layer.

[0144] In some cable embodiments, separator tapes, cross webs and / or star fillers are utilized between the twisted pair units to separate them from one another. Due to the forces experienced during the cable construction process, deformation of these separators can occur, which reduces the air volume within the cable and adversely affects the electrical performance of the cable.

[0145] Figure 17 illustrates a schematic cross-section of an embodiment in which multiple twisted pairs are separated by cross webs. In the embodiment shown in Figure 17, the twisted pairs 1410 are separated from each other by a polymer cross web 1420. This reduces the amount of electromagnetic interference between the twisted pairs 1420. The cross web 1420 and the twisted pairs are encased in an outer sheath 1430.

[0146] In some embodiments, the separator tape, cross-web and / or star-filler are extruded polymer shapes without the benefit of a metal backing or rigid internal elements. The polymer separator may be made of a high dielectric material (3.0 or higher). In some embodiments, the separator may be made of a foamed material, which improves dielectric properties and increases susceptibility to deformation. During the cable fabrication process, the cable components are typically subjected to multiple compressive or deforming forces. Exposing the separator tape, cross-web or star-filler to a cryogenic fluid before or during the cable fabrication process to temporarily increase the hardness may reduce compression or deformation of the separator or other components, thereby increasing the volume of air within the cable and improving the electrical performance of the resulting cable.

[0147] In some embodiments, the polymer cable components may be cured before being compressed to reduce the degree of deformation to the polymer cable components. In some embodiments, the polymer cable components may be cured before being compressed so that the polymer cable components can withstand greater compressive forces while remaining nearly as compressible as if the cable had not been cured before being compressed.

[0148] In some embodiments, a first twisted pair is made by running a twinning apparatus or twinner at a first line speed. The resulting first twisted pair has a certain first crush rate. Another twisted pair can be made by cooling the polymer insulated conductor to increase the hardness of the polymer insulation layer, and then running the cable twinning apparatus at a second, faster speed to twine the polymer insulated conductor and make a second twisted pair having a second crush rate. In some embodiments, the second twisted pair is made at a second, faster speed and has about the same crush rate as the first twisted pair. In some embodiments, the second crush rate is within about 10% of the first crush rate. In some embodiments, the second crush rate is less than the first crush rate. In some embodiments, the second speed is at least about 15% faster than the first speed. In some embodiments, the second rate is at least about 25% faster than the first rate.

[0149] In some embodiments, the twinner or twinning apparatus used will have a rated speed for a particular type of wire and cable product. In some embodiments, the first speed described above is the rated speed for a given twinner and cable product, and the second speed is at least about 10% faster than the rated speed for the same product. In some embodiments, the first line speed is about 60 feet / min and the second speed is about 70 feet / min. In some embodiments, the first line speed is about 160 feet / min and the second speed is about 180 feet / min. In some embodiments, the first line speed is about 220 feet / min and the second speed is about 275 feet / min.

[0150] FIG. 18 illustrates a schematic cross-section of an embodiment in which an electric wire includes a metal braid. In some embodiments, a conductor 1510 is insulated by a polymeric insulation layer 1520, and a wire braid 1530 is constructed on top of the insulation layer 1520. The wire braid 1530 may be made of a metal, such as copper, and may be plated with silver or tin. The wire braid 1530 may contain multiple metal strands woven together. When the braid is applied to the polymeric insulation layer 1520, the individual metal strands that make up the braid may create indentations on the surface and / or compress the polymeric insulation layer 1520, which may adversely affect the electrical properties of the cable. In some embodiments, multiple polymer cable components, such as insulated conductors and hollow tubes, are cabled together using a metal braid. In such embodiments, each of the polymer cable components in contact with the metal strands may be deformed by the compressive force of the metal strands, which may adversely affect the electrical properties of the resulting cable.

[0151] In some instances, the impressions of the braid on the polymer insulation layer are repeated at regular intervals. This can adversely affect periodic electrical signals, or any harmonics thereof, that repeat at approximately the same regular intervals or frequency. Increasing the hardness of the polymer insulation layer prior to application of the braid or metal strands can reduce impressions, compression, and other deformations of the polymer insulation layer.

[0152] In some embodiments, the cooling chamber or other structure containing the cooling medium located immediately prior to the braiding machine is less than about 5 ft. in length, or less than about 3 ft. in length, or less than about 1 ft. Due to the relatively slow line speeds of most braiding machines, the cooling chamber signature can be reduced without reducing the residence time of the polymeric cable components within the cooling chamber.

[0153] In one non-limiting embodiment, non-insulated copper conductor wire was used to simulate the indentations that occur in polymeric cable components during the metal braiding process. Metal braids are typically applied over polymeric cable components by weaving or braiding multiple individual metal strands together over the polymeric component. As these individual strands are braided together, they compress and deform the underlying polymeric component. To simulate this deformation process, a entanglement machine was used to entangle one foam FEP insulated conductor with one non-insulated copper conductor wire. When the non-insulated copper conductor wire is twisted around the foam FEP insulation, the indentations left in the foam FEP insulation layer can be inspected. The bare copper wire was a 24 AWG wire and the FEP foam insulated conductor had an outside diameter of about 82.68 mils, or about 2.1 mm.

[0154] Samples were prepared using a 6.2mm twist length and a twisting machine operating at 30 ft / min with 1400 twists / min. Samples were collected after exposing the FEP foam insulation to liquid nitrogen for a period of 10 seconds, and as a control, a sample without the cooling chamber. The depth of the impression left by the copper conductor in the foam insulation was analyzed using a laser microscope.

[0155] Upon initial visual inspection, the polymer insulation layer that was not exposed to liquid nitrogen was deformed into a generally helical shape when intertwined with the exposed copper wire. The polymer insulation exposed to liquid nitrogen for a period of 10 seconds was found to have increased hardness and appeared to be generally straight, with the copper wire wrapping in a helical shape around the straight foam insulation layer. The foam FEP insulation layer appeared to be unchanged by the intertwining process with the exposed copper wire.

[0156] The depth of the impression caused by the exposed copper wire entering the FEP foam insulation layer was measured three times at each of three locations: before winding on the intertwining machine, inside the bend, and on the intertwining take-up reel. The data is presented in Table 6 below.

[0157] [Table 6]

[0158] As the intertwined pair moves from pre-wind, to the inside of the bend, to the take-up reel, the amount of force and the number of total compression events increases and the twist length decreases. The distance and time since the polymer insulation left the cooling chamber also increases, which causes the hardness of the polymer insulation to decrease as the polymer returns to ambient temperature.

[0159] As can be seen in Table 6, at all locations, samples exposed to liquid nitrogen for 10 seconds showed a significant reduction in the indentation made by the copper wire. Therefore, it can be expected that a metal braid shield layer applied over a polymeric insulation layer will cause less deformation of the polymeric insulation layer if the polymer is cured by cooling the polymer before applying the braid. Wire and cable products with less deformation of the polymeric insulation layer generally have improved electrical properties over wire and cable products having a compressed or otherwise deformed polymeric insulation layer.

[0160] In some embodiments, during the cable making process, when individual insulated conductors and / or other cable components are bundled together, compression and / or deformation may occur. This deformation may push the insulated conductors into the cross-web or other separator, resulting in compression of the insulation layers and / or collapse of the armor layers. During the cable making process, the twisting of the current twisted pairs may increase the twisting speed of the twisted pairs, which creates additional compression forces within the current twisted pairs. Hardening the cable components by temporarily increasing their hardness during the cable making process may help reduce or avoid deformation of the various cable components, both individually and relative to each other. The desired arrangement of the cable can be maintained by exposing the cable making components to a cryogenic fluid before and / or during the cable making process. Avoiding deformation maximizes the air space within the cable, improving electrical performance. Allowing deformation of the cable's physical arrangement has a negative effect on the cable's electrical performance.

[0161] As described herein, air is a preferred dielectric material, but it does not provide physical support and does not prevent conductors from touching each other. Therefore, insulation is utilized to prevent contact between conductors and reduce interference. To improve the electrical performance of the insulation layer, air may be introduced into the insulation via air channels (profile extrusion) or foaming (creating air bubbles within the insulation material). Since air does not have physical strength by itself, introducing air into the insulation layer reduces the overall hardness of the insulation. A lower hardness results in more compression or deformation as a result of the same external force. The insulation element may be exposed to a cryogenic fluid to temporarily increase the hardness of the insulation layer, thereby mitigating deformations that occur during the manufacturing process. In some embodiments, introducing air into the insulation layer allows the cryogenic fluid to cool any enclosed air pockets. This may help the insulation layer to remain at a lower temperature for a longer period of time than a solid insulation layer without any air pockets.

[0162] In some embodiments, by increasing the hardness of polymer cable components before or during manufacturing, lighter, smaller, and / or more useful cables can be made. If the cable components are not compressed or otherwise deformed, less total insulation material may be required to achieve the same electrical performance. If the insulation layers are less compressed due to increased hardness during manufacturing, the total thickness of the insulation layers may be reduced.

[0163] In some embodiments, untwisted wires may benefit from a temporary increase in the hardness of the polymer insulation layer. For example, the polymer insulation layer of a single polymer insulated conductor may deform when the wire contacts rollers, guide bars, or other equipment during the manufacturing process. The polymer insulation layer may also deform when two wires are joined to form a non-twisted pair.

[0164] Many cables contain two or more twisted pairs. To reduce electrical interference between the twisted pairs, each twisted pair in a cable can have a different twist length or a different number of twists per meter. The difference in twist length and other differences in the twisted pairs can lead to a particular twisted pair having a faster or slower signal speed. One factor in one twisted pair having a faster or slower signal speed is the amount of air in the gap between the two insulated conductors of the twisted pair. The more the conductors in the twisted pair are deformed by the compressive force of the entanglement, the less air remains in the gap. The less the conductors in the twisted pair are deformed by the compressive force of the entanglement, the more air remains in the gap, the lower the dielectric constant of the twisted pair and the higher the signal speed of the twisted pair. In addition to the air contained in the gaps of the twisted pairs, air may also be contained between various components in the cable. In some cable embodiments, air pockets may form between the twisted pairs, between the twisted pairs and the cross members, between the twisted pairs and the filler tube, and / or within the hollow tube. In general, the more air contained within a cable, the better the electrical properties of the cable.

[0165] In certain applications, data may be transferred using multiple twisted pairs within a single cable. For that data to be properly processed, the data must be sent over and received from each of the twisted pairs at a specific time. In some embodiments, different twist lengths are used to reduce electrical noise between different twisted pairs. It is common that four pairs may be used to transmit a signal. By using different twist lengths for each of these four pairs, the conductor path of one twisted pair may be shorter or longer than another twisted pair. For example, a twisted pair with a longer twist length and fewer twists per inch will have a shorter conductor path than a twisted pair with a shorter twist length and more twists per inch.

[0166] In many applications, it is important that the signals on each twisted pair arrive at approximately the same time. Different conductor lengths can cause the signals to arrive at different times. This can cause an effect called differential delay. In some embodiments, it is beneficial to slow down or not modulate the first arriving signal (shortest conductor pair path) and naturally speed up the last arriving signal (longest conductor pair path).

[0167] The difference between the signal received from the twisted pair with the fastest signal rate and the signal received from the slowest signal rate is called the delay skew. It is desirable for the delay skew to be less than 25 ns. In some applications, a delay skew of less than 50 ns is acceptable.

[0168] As discussed, deformation of the polymer insulation layer in a twisted pair can affect the electrical performance of the twisted pair, including signal speed. The tighter the twist or the shorter the twist length of the twisted pair, the greater the compression force applied during intertwining, typically resulting in a greater degree of deformation of the polymer insulation layer and subsequent reduction in the air dielectric between the insulated conductors.

[0169] In some embodiments, the multiple twisted pairs are exposed to the cryogenic fluid for different lengths of time to tailor the signal speed and reduce the delay difference of the resulting cable. By exposing the polymer insulated conductor to the cryogenic fluid for different lengths of time, a desired amount of deformation of the polymer layer can be introduced. By controlling the degree of deformation of the polymer, a desired amount of air can be controlled within the gaps of the twisted pairs. Generally, the deformation adversely affects the electrical properties of the resulting twisted pairs, but being able to control the degree of the adverse effect allows the signal speed between the multiple twisted pairs to be standardized, resulting in a cable with reduced delay difference across the multiple twisted pairs.

[0170] In one non-limiting example, four twisted pairs are manufactured to be incorporated into a single Ethernet cable. The polymer insulated conductors forming each of the four twisted pairs are exposed to a cryogenic fluid before being intertwined. The polymer insulated conductors forming the twisted pair with the longest twist length may be exposed to the cryogenic fluid for, for example, about 2 seconds to reduce the degree of deformation of the polymer insulation layer. The polymer insulated conductors forming the twisted pair with the shortest twist length may be exposed to the cryogenic fluid for, for example, about 10 seconds to reduce the degree of deformation of the polymer insulation layer and preserve most of the air dielectric between the insulated conductors. The polymer insulated conductors forming the twisted pair with a medium twist length may be exposed to the cryogenic fluid for a period of time between 2 and 10 seconds. By exposing the wires constituting different twisted pairs to the cryogenic fluid for different periods of time, the signal speed of the resulting twisted pairs can be adjusted and the delay time difference of the resulting cable can be reduced.

[0171] While the dielectric constant of a given polymer may be known, the total amount of insulating material and air gap surrounding the conductors in a twisted pair is a function of the original polymer-insulated conductors, the cable design, and the degree of deformation of the various cable components introduced during the manufacturing process. In the case of foamed polymer insulation, the amount of air gap around the conductor is closely related to the degree of deformation of the polymer insulation.

[0172] For a given conductor, the dielectric constant is inversely related to the velocity of propagation. Thus, the time it takes a signal to travel a given length of twisted pair is also related to the dielectric constant. The higher the total dielectric constant (the sum of the insulation layer and the air gap) around the conductor, the longer the signal will travel in the twisted pair. For example, by controlling the degree of deformation of various cable components such as the insulation layer, twisted pair, hollow tube, feed tube, and / or jacketing, the electrical performance of the twisted pair and / or cable can be tuned. By combining twisted pairs with known or controlled signal speeds, cables with reduced delay time differences can be produced.

[0173] The velocity of propagation in a twisted pair can be measured directly using commercially available instruments. The velocity of propagation measurements can be used to determine the coupling dielectric constant (ε) using the following equation:

[0174] [Table 7]

[0175] By directly measuring the velocity of propagation, it is possible to calculate the combined dielectric constant (ε), which takes into account the dielectric effects of both the polymer insulation and the air gap surrounding the conductor.

[0176] In one non-limiting example, the propagation velocity of the twisted pair is measured to be 68%. Based on the equation above, the coupling permittivity is calculated to be 2.16. Using the time delay calculation also shown above, the time delay of signals traveling down this twisted pair corresponds to approximately 1.5 nanoseconds per foot. If a second twisted pair is produced and exposed to a cryogenic fluid before twisting the polymer insulated wires together, the amount of air gap surrounding the conductors may be increased to improve the propagation velocity. If the improved propagation velocity is 70%, increased by 2%, the resulting coupling permittivity is calculated to be 2.04, and the calculated time delay is 1.45 nanoseconds per foot. For twisted pairs over 330 feet long, a difference of 0.05 nanoseconds per foot between the two twisted pairs results in a total difference of 16.5 nanoseconds of signal delay. By exposing the polymer insulated conductor to a cryogenic fluid for a specific time, the coupling permittivity and propagation velocity can be controlled. This will enable the development of faster twisted pairs and the creation of cables with reduced delay time skew.

[0177] By exposing the polymer insulated conductor to a cryogenic fluid for various periods of time, a desired amount of deformation in the polymer layer can be induced. Although the deformation generally adversely affects the electrical properties of the resulting twisted pair, the degree of the adverse effect can be controlled to allow standardization of signal speeds among multiple twisted pairs, resulting in cables with reduced delay skew.

[0178] In some embodiments, the entanglement device can be adjusted to operate at a faster or slower linear speed to control the time the insulated conductor is exposed to the cryogenic fluid. In some embodiments, multiple cooling vessels of different lengths may be used to expose the polymer insulated conductor to the cryogenic fluid for different times. In some embodiments, a displacement block or adjustable partition can be used to control which portion of the cooling vessel actually contains the cryogenic fluid, thereby exposing the polymer to the cryogenic fluid for different times using a single cooling vessel. By using a displacement block or adjustable partition, a portion of the cooling vessel can be left free of cryogenic fluid, functionally creating a variable length cooling vessel.

[0179] In some embodiments, one or more pulleys, wheels, capstans, and / or rollers can be used in the cooling vessel to redirect the path of the polymer cable components in the cooling vessel. This arrangement can allow the polymer cable components to remain in the cooling vessel for a longer period of time without increasing the length of the cooling vessel or slowing the linear velocity of the components. In some embodiments, the polymer cable components enter the cooling vessel at an upper vapor region of the vessel where the evaporated cryogenic vapor rises above the cryogenic liquid, and are then redirected through a liquid region of the vessel where the liquid cryogenic fluid remains. This arrangement can allow the polymer cable components to transfer heat to the cryogenic vapor first before contacting the cryogenic liquid, thereby reducing the total heat load transferred to the cryogenic liquid and increasing the total residence time of the polymer cable components in the cooling vessel. In some embodiments, the redirecting wheels can be adjustable to control the total residence time of the polymer cable components in the cooling vessel.

[0180] It will be appreciated that the cable can be made with one or more twisted pairs, for example, 2, 3, 4, 6, or 8 twisted pairs. Each twisted pair in the cable can be exposed to the cryogenic fluid for a unique, predetermined time to adjust the signal speed. By adjusting the signal speed, the delay time difference of the resulting cable can be reduced.

[0181] In some embodiments, the cable jacket is formed around the twisted pairs or other cable components using an extruder with a profile die. The cable components are passed through the extruder die and a polymer is extruded around the cable components to form the jacket. In some embodiments, to avoid deformation of the cable jacket, the cable jacket is exposed to a cryogenic fluid after being extruded around the cable components.

[0182] In some embodiments, the polymer may be exposed to a cryogenic fluid after being extruded to form a polymer shape, including but not limited to a hollow tube, a solid tube, a rectangular shape, an irregular shape, a shape with protrusions, depressions or cavities, or any other profile design. By exposing the extruded polymer shape to a cryogenic fluid after the polymer shape is extruded, the hardness of the extruded shape can be increased over a relatively short distance. In some embodiments, exposure to a cryogenic fluid may be used to tailor the crystal structure of the extruded shape and / or to control the physical properties of the resulting polymer shape. In some embodiments, the extruded polymer may be exposed to a water bath before being exposed to a cryogenic fluid. By exposing the extruded polymer shape to a cryogenic fluid, the resulting polymer may be easier to handle, grind, machine, or cut. The resulting polymer may be able to withstand deformation and / or produce less shavings, dust, chips, or unusable material during processing. In some embodiments, improved tensile and elongation properties may be achieved by tailoring the crystal structure of the polymer cable components.

[0183] In some embodiments, a cryogenic cooling vessel may be incorporated into an in-line continuous or semi-continuous process. In some embodiments, an intertwining machine may be configured to incorporate a cryogenic cooling chamber before, during, and / or after the intertwining machine pairs the polymer insulated conductors to form twisted pairs. In some embodiments, a cable making machine may be configured to incorporate a cryogenic cooling chamber before, during, and / or after the cable making machine gathers and / or twists the cable components to form a cable core.

[0184] In some embodiments, the cryogenic cooling vessel includes a vessel arranged to contain a cryogenic liquid, a liquid level sensor, e.g., a float switch, and an inlet arrangement for supplying the cryogenic liquid and / or an exhaust arrangement for removing vaporized cryogenic liquid. In some cryogenic cooling vessels, the inlet is arranged to allow a polymer component, e.g., a polymer insulated conductor, to enter the cooling vessel, and the outlet is arranged to allow the polymer component to exit the cooling vessel. In some embodiments, the inlet and outlet each have a diameter less than 0.3 mm greater than the diameter of the polymer sample. In some embodiments, the inlet and / or outlet are arranged in a shape corresponding to the profile to accommodate various shaped polymer samples, e.g., cross webs. In some embodiments, the cooling vessel incorporates sensors and / or labeling devices to maintain consistent wire or cable quality during operation and / or line shutdown.

[0185] In some embodiments, the cooling vessel is positioned to expose the polymer insulated conductors to the cryogenic fluid prior to the initial contact between the polymer insulated conductors. The initial contact point may be several feet before the polymer insulated conductors actually enter the winding device of the entanglement machine. At the initial contact point, a compressive force between the polymer insulated conductors exists, but may be vulnerable to the peak compressive force that occurs when the polymer insulated conductors are entangled together. In some embodiments, the cooling vessel is positioned to expose the polymer insulated conductors to the cryogenic fluid after the initial contact point and before the polymer insulated conductors enter the entanglement machine.

[0186] In some embodiments, the automated cryogenic exposure system may be utilized as part of an in-line continuous or semi-continuous process. The automated cryogenic exposure system may be used with entangling lines, cable making lines, jacketing lines, and / or any other process where polymeric members may be compressed or deformed.

[0187] In some embodiments, the cryogenic exposure system includes a cooling vessel having one or more sensors positioned to determine variable length, variable component paths, multiple component paths, wire, twisted pair, cable core, or cable diameter, and / or a machine automation controller.

[0188] In one non-limiting example, an optical sensor can be used to measure the diameter of one or two polymer insulated conductors being unwound at the beginning of the twisted pair entanglement process. As described herein, the polymer insulated conductors may be passed through a cooling vessel containing a cryogenic fluid, such as liquid nitrogen, to increase the hardness of at least a portion of the polymer insulation layer. After passing through the cooling vessel, the two polymer insulated conductors are twisted together to form a twisted pair. A second optical sensor can also be used to measure the width of the final twisted pair.

[0189] By measuring the diameter of both of the polymer insulated conductors before they come into contact with each other, the two diameters can be combined to determine the potential width of the resulting twisted pair when no crushing or deformation of the polymer insulation layers has occurred. In some embodiments, the potential zero deformation width may also be determined by measuring the diameter of one of the polymer insulated conductors at the start of the intertwining process and doubling it.

[0190] When measuring the resulting width of the twisted pair, the optical sensor may measure the width of the twisted pair as it passes through a beam, such as a photon beam emitted by the optical sensor. It will be appreciated that the peak width measurement is used to represent the width of the twisted pair when the individual conductors are oriented in a plane perpendicular to the beam of the optical sensor. If the two conductors of the twisted pair are stacked in line with the beam of the optical sensor, the measured width may be approximately equivalent to the width of one insulated conductor and is not representative of the width of the twisted pair. By comparing the measured width of the twisted pair to a theoretical zero-collapse width, the collapse rate of the twisted pair can be determined in real time.

[0191] As part of the twisted pair cable design, a desired crush ratio can be established to achieve the desired electrical properties. If the measured crush ratio is determined to be higher than the desired crush ratio set value, the cooling vessel can be adjusted to extend the length that the polymer-insulated conductor is exposed to the cryogenic fluid. By extending the length of the cooling vessel containing the cryogenic fluid, the exposure time of the polymer-insulated conductor can be increased and the hardness of the polymer-insulated conductor can be increased before the polymer-insulated conductor is exposed to the compressive force of the entanglement process. By increasing the hardness of the polymer-insulated conductor prior to entanglement, the crush ratio of the resulting twisted pair can be reduced. In some embodiments, the speed of the entanglement device can be adjusted to help increase or decrease both the residence time of the insulated conductor in the cryogenic fluid and / or the compressive force caused by the entanglement process.

[0192] In some embodiments, the optical sensor and the variable length cooling vessel may be connected to one or more processors or machine automation controllers to create an automated quality control process. If the measured crush rate deviates from the desired crush rate set point, the controller may respond to the variable length cooling vessel by adjusting the position of the diverter wheels to extend or contract the length of the portion of the cooling vessel containing the cryogenic fluid and / or to extend or contract the length of the component path within the cooling vessel. By automatically adjusting the length of the portion of the cooling vessel containing the cryogenic fluid, the exposure time of the polymer insulated conductor to the cryogenic fluid and therefore the hardness of the polymer insulation layer can be adjusted. By adjusting the hardness of the polymer insulation layer, the crush rate of the twisted pair can be controlled.

[0193] In some embodiments, minor modifications to the variable length cooling vessel may be made continuously. Having granular and / or automatic control over the length of the cooling vessel and therefore the exposure time of the polymer insulated conductor to the cryogenic fluid allows the collapse rate to be controlled and maintained regardless of many potentially complex factors, including but not limited to ambient temperature, ambient sunlight, relative humidity, line speed, twist length, entangler parameters, entangler design, the type of polymer insulation used, whether the polymer insulation is foamed or solid and / or the degree to which the polymer insulation is foamed, variances in polymer insulated conductor from reel to reel, and many others.

[0194] In some embodiments, multiple cooling vessels can be used to control the total exposure time of the polymer-insulated conductor to the cryogenic fluid. By using multiple separate cooling vessels, different methods of applying the cryogenic fluid to the polymer insulation can be used on the same polymer insulation. For example, a first cooling vessel can immerse the polymer conductor in a cryogenic fluid bath, while a second cooling vessel can use a spray of the cryogenic fluid. It will be appreciated that any number of cooling vessels can be used in any of a number of configurations. By varying the configuration of some or all of the multiple cooling vessels, the exposure time of the polymer-insulated conductor and the temperature of the polymer-insulated conductor upon application of entanglement or other compressive force can be controlled in an adjustable manner.

[0195] Previously, obtaining the desired degree of crush required a trial and error process of making a reel of twisted pairs and testing the electrical properties of the resulting reel. If the electrical properties are not within the predetermined specifications, the reel is labeled non-conforming and one of many variables is changed. Another reel of twisted pairs is then made and the electrical properties of that reel are tested. This trial and error process took a great deal of time and also resulted in loss of material. Since it is known that the physical properties of the polymer insulated conductors, and the resulting twisted pairs, affect the electrical properties, by controlling the degree of crushing of the twisted pairs, the electrical properties of the twisted pairs can also be controlled. The disclosed continuous and / or automated processes can be used to obtain the desired physical properties, and therefore the desired electrical properties, with less time and less wasted material.

[0196] 19A-C show schematic diagrams of a variable length cooling vessel according to one embodiment. As shown in FIG. 19A, the variable length cooling vessel may include a partition 1630 arranged to move back and forth to change the length of the cooling vessel containing the cryogenic fluid 1620. The partition 1630 may be controlled by a motor 1650 connected to a threaded rod or screw drive 1660. As shown in FIG. 19A, the polymer insulated conductor 1610 may enter the cooling vessel through a hole 1640. After passing through a portion of the cooling vessel that does not contain the cryogenic fluid 1620, the polymer insulated conductor may pass through the partition 1630 through a similar hole 1640. After passing through the partition 1630, the polymer insulated conductor 1610 is exposed to the cryogenic fluid 1620. As shown in FIGS. 19B and 19C, the position of the partition 1630 may be controlled using a motor 1650 and / or a screw drive 1660 to extend or reduce the portion of the cooling vessel containing the cryogenic fluid 1620. By adjusting the length of the portion of the cooling vessel containing the cryogenic fluid, the time the polymer insulated conductor is exposed to the cryogenic fluid can be controlled. By controlling the time the polymer insulated conductor is exposed to the cryogenic fluid, the crush rate and therefore the electrical performance of the twisted pair or cable can be controlled.

[0197] In some embodiments, the motor, screw drive, or other mechanism for controlling the position of the partition within the variable length cooling vessel may be operably connected to a machine controller. In some embodiments, the machine controller may be used to control the position of a diverting wheel within the cooling vessel to adjust the length of the component path within the cooling vessel. This dynamic component path may be controlled to adjust the residence time of the polymer cable component within the cooling vessel. The machine controller may be in data communication with one or more processors in data communication with a first sensor for determining the diameter of the polymer insulated conductor and a second sensor for determining the width of the twisted pair. The processor and machine controller may compare the diameter of the polymer insulated conductor and the resulting width of the twisted pair to determine a crush rate and compare the determined crush rate to a predetermined desired crush rate set point. The machine controller may then command the motor and / or screw drive to adjust the exposure time of the polymer insulated conductor to the cryogenic fluid until the determined crush rate is approximately equal to the desired crush rate set point. Although the cryogenic exposure system described above is described in the context of an entanglement system, it will be understood that the system may also be applied to any other process in which a polymer component may be compressed or deformed.

[0198] In some embodiments, the cooling vessel includes nozzles configured to spray the cryogenic fluid onto the polymeric component. In some embodiments, rather than changing the physical size of the cooling chamber containing the cryogenic fluid, some of the nozzles may be closed, bypassed, or prevented from spraying the cryogenic fluid. This allows for control of the exposure time of the polymeric component and the resulting collapse rate of the polymeric component, as described above.

[0199] 20A-C show schematic diagrams of a variable spray cooling vessel according to one embodiment. As shown in FIG. 20A, the polymer insulated conductor 1710 can enter the cooling vessel through a hole 1730. The cryogenic spray nozzles 1720 can be activated to expose the polymer insulated conductor 1710 to the cryogenic fluid. As shown in FIG. 20A, all of the multiple spray nozzles 1720 can be activated to expose the polymer insulated conductor to a maximum amount of cryogenic fluid. As shown in FIG. 20B, some of the multiple cryogenic spray nozzles 1720 can be deactivated to reduce the exposure time of the polymer insulated conductor to the cryogenic fluid. As shown in FIG. 20C, even more of the spray nozzles 1720 can be deactivated to reduce the exposure time of the polymer insulated conductor to the cryogenic fluid. In some embodiments, the flow rate of the cryogenic fluid through one or more nozzles may also be adjusted to adjust the hardness of the polymer component passing through the cooling vessel. In some embodiments, all of the spray nozzles may be deactivated so that the polymer component is not exposed to the cryogenic fluid at all. By adjusting the flow of at least one of the multiple cryogenic nozzles, the exposure time of the polymer insulated conductor to the cryogenic fluid can be adjusted. In some embodiments, the flow of the cryogenic fluid through the nozzles of the cooling vessel may be adjusted in response to the measured collapse rate to precisely control the collapse rate of the twisted pairs or the deformation of any other polymer components passing through the cooling vessel.

[0200] In some embodiments, by reducing the crush or deformation of polymer insulated conductors, cables, cable jackets, and other cable components, less polymer material can be used to manufacture those components while maintaining or improving electrical performance. By using less polymer material, the resulting cable has less flammable material and a lower fuel load. Cables with lower fuel loads are more likely to pass the UL 910 Steiner Tunnel test.

[0201] In some embodiments, the process of adding additional insulation and / or jacketing material to compensate for expected deformations introduces a new set of problems. For example, many cables must pass certain flame and smoke standards that ensure the cable is safe for use inside a building or dwelling. One factor in a cable's propensity to propagate flame and generate smoke is the amount of material contained within the cable, commonly referred to as the "fuel load." In general, the more fuel (here polymer insulation or jacketing material) the more smoke will be generated and the more flame will propagate from the cable under test.

[0202] An example of a fuel load test is the UL 910 Steiner Tunnel test, which is related to ASTM E84, NFPA255, UL 723, and ULC S102. In this test, a flame is applied to a bundle of cables inside a 24 ft x 1.8 ft x 1 ft noncombustible horizontal box or tunnel. The flame intensity is set at 89 kilowatts, and air is forced through the tunnel to replicate plenum ceiling conditions. Materials tested to these standards are required to exhibit a maximum flame spread distance of 5 feet, a maximum peak optical density of 0.5, and a maximum average optical density of 0.15.

[0203] Design engineers generally select materials optimized to meet cost and required fuel load standards. Potential problems arise when extra material is added to compensate for deformation of the cable due to forces generated during cable manufacturing. This extra material increases the fuel load, driving up costs and limiting the types of materials that can be employed. For example, some Cat6A cables have shorter lay lengths that generate higher compression forces during manufacturing. These cables typically use FEP and PVC resins for insulation due to the greater than normal deformations faced during the manufacturing of these products. Cat6 cables on the other end utilize longer lay lengths and have comparatively reduced compression forces during manufacturing. As such, these cables require less additional insulation to compensate for deformation. This lower fuel load allows for the utilization of other materials and / or materials that are less costly.

[0204] In some embodiments, the cable is manufactured by temporarily increasing the hardness of the polymer cable components before or during a compression event. The increased hardness reduces the degree of deformation that occurs during the compression event, and therefore less additional insulating material is required to achieve the desired electrical performance. In some embodiments, increasing the hardness of the polymer cable components can reduce the total fuel load of the resulting cable, thereby allowing the cable to pass the UL 910 Steiner Tunnel Test, whereas a similar cable without the increased hardness and including additional polymer material to offset the increased sag would not pass the UL 910 Steiner Tunnel Test.

[0205] In some embodiments, cables can be developed that have lower fuel loadings of more cost-effective materials, but would not have passed UL 910 Steiner Tunnel testing without the reduced fuel loading. In some embodiments, cables manufactured using the disclosed technology contain reduced fuel loadings and are less likely to propagate flame or smoke.

[0206] In some embodiments, cables made using the disclosed technology may have a smaller outer diameter, which may allow existing buildings to be retrofitted with modern, high performance cables that have a similar or smaller diameter than the lower performance cables previously used.

[0207] In some embodiments, the wire and cable product has a certain amount of polymeric insulation and / or other polymeric cable components that contribute to its fuel load. In some embodiments, the fuel load is designed to produce a flame travel distance of about 5 feet or less, a peak smoke optical density of about 0.5 or less, and / or an average smoke optical density of about 0.15 or less, when measured according to the Steiner Tunnel Test Method of ASTM E84, UL 910, NFPA 255, UL 723, or ULC S102.

[0208] In some embodiments, the polymer cable components are cooled and / or hardened prior to undergoing the compression event, which can provide desired electrical properties because the polymer cable components do not deform as much as if the polymer cable components had not been cooled and / or hardened prior to compression.

[0209] In some embodiments, the polymer cable components deform less after being cured, so less overall polymer is incorporated into the wire and cable product, which may reduce the total fuel loading of the wire and cable product. In some embodiments, the reduced fuel loading wire and cable product has a capacitance value of less than about 20 pf / ft. In some embodiments, the reduced fuel loading wire and cable product has an impedance value of between about 50 ohms and 150 ohms, or between about 75 ohms and 125 ohms, or equal to about 100 ohms. In some embodiments, the reduced fuel loading wire and cable product has a propagation velocity of between about 62% and 80%, or between about 66% and 70%.

[0210] In some manufacturing facilities, there is ample space to slowly cool the very hot insulated conductors or other polymer cable components after they are extruded. In some facilities, this initial cooling step involves prolonged exposure of the recently extruded polymer components to ambient air or water contained in a trough. Because wire and cable manufacturing is generally a continuous process in which the cable components move at high speeds, each of these cooling methods may require a significant amount of space, e.g., greater than about 40 feet. The long distances required to allow the extruded polymer components to cool require large amounts of manufacturing floor space. Furthermore, these cooling methods generally do not bring the temperature of the polymer cable components below ambient temperature.

[0211] In some embodiments, a faster temperature drop is advantageous for both saving time and reducing the footprint of the extruder manufacturing run. In some embodiments, a cooling chamber with chilled or cryogenic fluid can be used to rapidly cool the polymer cable component immediately after it is extruded. In some embodiments, the cooling chamber after the extruder is less than about 10 feet long, or less than about 8 feet long, or less than about 5 feet long, or less than about 3 feet long.

[0212] In one non-limiting example, the Shore D hardness of solid FEP plaques was measured as described below. Injection molded plaques of solid FEP polymer were used throughout this example. The plaques were 61 mm long, 61 mm wide, and 2 mm high. The Shore D hardness of the solid FEP plaques was measured at an ambient temperature of about 20° C. The plaques were then exposed to liquid nitrogen for different lengths of time by submerging them in a pool of liquid nitrogen. The Shore D hardness of the plaques was measured after the different exposure times. The data is shown in FIG.

[0213] As can be seen in Figure 21, the Shore D hardness of the FEP plaque increases from about 60 to about 83 after about 10 seconds of exposure to liquid nitrogen. After about 10 seconds of exposure to liquid nitrogen, the FEP plaque reached a maximum hardness of about 83. Continuing exposure to liquid nitrogen beyond 10 seconds did not cause the hardness of the FEP plaque to continue to increase.

[0214] In the examples that follow, the Shore D hardness of solid FEP plaques was measured when the plaques returned to ambient temperature after exposure to liquid nitrogen for a set period of time. The plaques were immersed in liquid nitrogen for either 6, 10, or 30 seconds and then removed from the liquid nitrogen. For each of the three tests, the Shore D hardness of the plaques was measured at set time intervals until the plaques returned to ambient temperature.

[0215] Figure 22 shows the Shore D hardness of the plaque as it returns to ambient temperature after immersion in liquid nitrogen for 6, 10, or 30 seconds. As shown in Figure 22, there is relatively no difference in the change in hardness over time between the samples exposed to liquid nitrogen for 10 seconds and the samples exposed to liquid nitrogen for 30 seconds. This correlates with the data shown in Figure 21, which suggests that the FEP plaque reached a maximum hardness after approximately 10 seconds of exposure to liquid nitrogen. The plaque exposed to liquid nitrogen for 6 seconds likely reached a lower initial Shore D hardness of approximately 76, which decreased as the plaque was exposed to ambient conditions.

[0216] In the subsequent example, a solid FEP plaque was immersed in liquid nitrogen for 10 seconds and then removed. The Shore D hardness and temperature (°C) of the plaque were measured when the plaque returned to ambient temperature. Figures 23A-23C show this data over different time periods.

[0217] Figure 23A shows the Shore D hardness decrease and temperature increase of a solid FEP plaque over about 390 seconds. Figure 23B shows the Shore D hardness decrease and temperature increase of a solid FEP plaque over about 180 seconds. Figure 23C shows the Shore D hardness decrease and temperature increase of a solid FEP plaque over about 30 seconds. Note that in Figures 23A-C, the temperature data below -60°C is a prediction, not a direct measurement.

[0218] In another non-limiting example, the Shore D hardness of foamed FEP was measured. To make a foamed FEP sample, a FEP foam insulated wire was tightly wrapped around a plaque of solid FEP. The Shore D hardness of the foamed FEP insulated wire was measured at an ambient temperature of about 20° C. The FEP foam insulated wire was then exposed to liquid nitrogen for different lengths of time by submerging it in a pool of liquid nitrogen. The Shore D hardness of the foamed FEP was measured after different exposure times. The data is shown in FIG. 24.

[0219] As shown in Figure 24, the Shore D hardness of FEP foam is about 29 at ambient temperature and increases to about 63 after about 15 seconds of exposure to liquid nitrogen. Once the foam FEP reaches a Shore D hardness of about 63, the Shore D hardness plateaus and does not increase significantly after additional exposure times to liquid nitrogen.

[0220] Figure 25 shows the Shore D hardness of an FEP foam insulated wire after immersion in liquid nitrogen for 10 seconds and returning to ambient temperature. As the foam FEP is exposed to ambient temperature for longer periods of time, the Shore D hardness decreases until it reaches a Shore D hardness of about 29 at ambient temperature.

[0221] In the subsequent example, the foam FEP insulated wire was immersed in liquid nitrogen for 10 seconds and then removed. The Shore D hardness and temperature of the foam FEP insulated wire were measured as the foam FEP returned to ambient temperature. Figure 26 shows this data over a period of time.

[0222] 26 shows the Shore D hardness decrease and temperature increase of a solid FEP plaque over about 390 seconds. Note that no initial temperature data was collected below about -55°C.

[0223] Figure 27 shows the Shore D hardness for both solid and foam FEP as they are exposed to liquid nitrogen over time. As can be seen from Figure 27, the Shore D hardness of the solid FEP generally stops increasing after about 10 seconds. The Shore D hardness of the foam FEP generally stops increasing after about 15 seconds.

[0224] Figure 28 shows the Shore D hardness of both solid and foamed FEP when exposed to liquid nitrogen for 10 seconds and then exposed to ambient conditions. Of note is that the Shore D hardness of the foamed FEP decreased more slowly, taking over 3 minutes longer than the solid FEP to return to its Shore D hardness at ambient temperature.

[0225] Figure 29 shows the temperature of solid and foam FEP when exposed to liquid nitrogen for 10 seconds and then exposed to ambient conditions. The temperature of the foam FEP increased more slowly and took over 10 minutes longer than the solid FEP to return to ambient temperature.

[0226] Without wishing to be bound by theory, it is believed that the air pockets in foam FEP change temperature more slowly than solid FEP. Thus, foam FEP insulation takes longer to reach its minimum temperature and associated increased hardness when exposed to liquid nitrogen. After being removed from the liquid nitrogen, foam FEP also takes longer to return to ambient temperature and associated hardness.

[0227] While the above examples are described in terms of solid and foam FEP, it will be understood that similar data can be readily collected for any form and type of polymer. Understanding the rate at which the hardness of the polymer returns to ambient hardness allows the hardness of the polymer cable component when subjected to a compression event to be controlled by adjusting the amount of time the polymer component is exposed to ambient temperature after exiting the cooling vessel. In some embodiments, the distance between the cooling vessels and / or the linear speed of the manufacturing line can be adjusted to reach the desired hardness of the polymer cable component at the time of compression device or deformation.

[0228] It will also be appreciated that the amount of cooling time (e.g., exposure time to cryogenic fluid or other cooling medium) can alternatively or additionally be adjusted to reach a desired hardness of the polymer cable component upon being subjected to a compressive or other deforming force.

[0229] In some embodiments, the methods described herein for increasing hardness result in an increase in Shore D hardness of the polymeric cable component of at least about 10% compared to a similar component at ambient temperature before the polymeric cable component is subjected to a compressive force or at the time the polymeric cable component is subjected to a compressive force.

[0230] In some embodiments, the hardness increasing methods described herein result in at least about a 10% increase in Shore D hardness of the polymer cable component relative to a similar component made of the same polymer at 20° C. In some embodiments, the hardness increasing methods described herein result in at least about a 10% increase in Shore D hardness of the polymer cable component relative to a similar component at 20° C. and reduce the deformation caused by a compression event by at least about 0.0005 inches.

[0231] In some embodiments, a cooling chamber less than about 10 feet in length is used to produce at least about a 10% increase in Shore D hardness relative to a similar component at ambient temperature.

[0232] In all cases, it will be understood that the 10% increase in Shore D hardness can be converted to other hardness tests such as Britnell, Meyer, Vickers, Rockwell, and other Shore Durometer scales, e.g., Shore A.

[0233] For reference, the Shore D durometer test is described in ASTM D2240 and ISO 868. Hardness values ​​are determined by penetrating the tip of a durometer indenter into a specimen. Shore hardness measurements are dimensionless and range between 0 and 100. The higher the Shore hardness number, the harder the material is and the more resistant it is to deformation. In some embodiments, the disclosed methods for increasing hardness are most advantageous for substrates that exhibit a Shore hardness between 40 and 80.

[0234] The methods, systems, and embodiments described herein generally relate to tailoring the hardness of polymeric components. Polymers contemplated herein include, but are not limited to, thermoplastics, thermosets, rubbers, and / or elastomers, each of which may be foams or solids and may include various additives and / or flame retardants. Specific polymers contemplated include, but are not limited to, linear low density polyethylene-LLDPE, high density polyethylene-HDPE, polyethylene-PE, perfluoroalkoxyalkane-PFA, polytetrafluoroethylene-PTFE, polypyridene fluoride-PVDF, ethylene chlorotrifluoroethylene-ECTFE, tetrafluoroethylene perfluoromethylvinylether-MFA, polyphenylene sulfide-PPS, polyetheretherketone-PEEK, polyetherketone-PEK, polyethyleneimine-PEI, fluorinated ethylene propylene-FEP, ethylene tetrafluoroethylene-ETFE, ethylene fluoroethylene propylene-EFEP, polypropylene-PP, nylon-PA, polyvinyl chloride-PVC, polycarbonate-PC, acrylonitrile butadiene styrene-ABS, polystyrene-PS, polyesters such as polyethylene terephthalate (PET), polyamide-PI, polyamideimide-PAI, natural rubber, synthetic rubber, fluoroelastomer-FKM, and blends or alloys thereof.

[0235] Disclosed embodiments include a method of reducing the effect of a compressive force on a polymer cable component, the method comprising: providing a polymer cable component having a first hardness, the first hardness being the hardness of the polymer cable component under ambient conditions; temporarily changing the hardness of the polymer cable component to a second hardness, the second hardness being different from the first hardness; applying a compressive force to the polymer cable component; and allowing the polymer cable component to return to the first hardness. In some embodiments, the polymer cable component is exposed to the compressive force while the polymer cable component has the second hardness. In some embodiments, the compressive force causes less deformation in the polymer cable component at the second hardness than in the polymer cable component at the first hardness. In some embodiments, the second hardness is greater than the first hardness. In some embodiments, temporarily changing the hardness of the polymer cable component comprises cooling the polymer cable component. In some embodiments, cooling the polymer cable component comprises exposing the polymer cable component to a chilled fluid. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a chilled solid surface. In some embodiments, the chilled solid surface rotates. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a cryogenic fluid. In some embodiments, the polymer cable component is exposed to the cryogenic liquid for about 10 seconds or less. In some embodiments, the polymer cable component is exposed to the cryogenic liquid for between 6 seconds and 10 seconds. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a chilled gas. In some embodiments, the chilled gas is between 15° C. and −10° C. In some embodiments, the polymer cable component includes an exterior surface, an interior bulk, and an interior surface, and cooling the polymer cable component includes cooling the exterior surface of the polymer cable component.In some embodiments, the polymer cable component is a polymer insulation surrounding the conductor. In some embodiments, the polymer cable component is a fluoropolymer insulation surrounding the conductor. In some embodiments, the polymer cable component is not cooled for 10 seconds or less before being exposed to the compressive force. Some embodiments further include ceasing cooling of the polymer cable component for 5 seconds or less before being exposed to the compressive force.

[0236] Additional disclosed embodiments include a method of manufacturing a communication cable, comprising: providing a polymer cable component having a first cross-sectional radius and a second cross-sectional radius, the first cross-sectional radius being a maximum distance from a center of the polymer cable component to an end of the polymer cable component along the cross-section, and the second cross-sectional radius being a minimum distance from a center of the polymer cable component to an end of the polymer cable component along the cross-section, the first cross-sectional radius being approximately equal to the second cross-sectional radius + / - 3%, the polymer cable component having a first hardness, the first hardness being a hardness of the polymer cable component under ambient conditions; temporarily changing a hardness of the polymer cable component to a second hardness, the second hardness being greater than the first hardness; and applying a compressive force to the polymer cable component, wherein after the compressive force, the first cross-sectional radius is approximately equal to the second cross-sectional radius + / - 10%. In some embodiments, the compressive force causes less deformation in the polymer cable component at the second hardness than in the polymer cable component at the first hardness. In some embodiments, temporarily altering the hardness of the polymer cable component includes cooling the polymer cable component. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a chilled fluid. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a cryogenic fluid. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a chilled gas. In some embodiments, the polymer cable component is not cooled for a period of 10 seconds or less before the compressive force is applied. Some embodiments further include ceasing cooling of the polymer cable component for a period of 5 seconds or less before the polymer cable component is exposed to the compressive force. In some embodiments, the polymer cable component is a polymer insulation surrounding a conductor. In some embodiments, the polymer cable component is a fluoropolymer insulation surrounding a conductor.Additional disclosed embodiments include a method of manufacturing a communication cable, the method including providing a polymer cable component having a first diameter and a second diameter, the first diameter and the second diameter being at right angles to one another, the first diameter approximately equal to the second diameter + / - 3%, the polymer cable component having a first hardness, the first hardness being a hardness of the polymer cable component under ambient conditions, temporarily changing a hardness of the polymer cable component to a second hardness, the second hardness being greater than the first hardness, applying a compressive force to the polymer cable component, the first diameter approximately equal to the second diameter + / - 10% after the compressive force, and allowing the polymer cable component to return to the first hardness. In some embodiments, the polymer cable component is exposed to the compressive force while the polymer cable component is at the second hardness. In some embodiments, the deformation caused by the compressive force is less in the polymer cable component at the second hardness than in the polymer cable component at the first hardness. In some embodiments, the second hardness is greater than the first hardness. In some embodiments, temporarily altering the hardness of the polymer cable component includes cooling the polymer cable component. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a chilled solid surface. In some embodiments, the chilled solid surface rotates. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a cryogenic fluid. In some embodiments, cooling the polymer cable component includes exposing the polymer cable component to a chilled gas. In some embodiments, the chilled gas is between 15°C and -10°C.

[0237] An additional disclosed embodiment is a method of manufacturing a communications cable comprising the steps of providing first, second, third, and fourth pairs of polymer insulated conductors, each pair of polymer insulated conductors including two polymer insulated conductors, each polymer insulated conductor having a first hardness, the first hardness being a hardness of the polymer insulated conductors under ambient conditions; temporarily changing the hardness of the polymer insulated conductors in the first, second, and third pairs of polymer insulated conductors to a second hardness, the second hardness being different from the first hardness; twisting the polymer insulated conductors of the first pair together to form a first twisted pair, the first twisted pair having a first propagation delay over 100 meters; and twisting the polymer insulated conductors of the second pair together. The method includes twisting together a first pair of polymer-insulated conductors to form a second twisted pair, the second twisted pair having a second propagation delay over 100 meters, twisting together a third pair of polymer-insulated conductors to form a third twisted pair, the third twisted pair having a third propagation delay over 100 meters, and twisting together a fourth pair of polymer-insulated conductors to form a fourth twisted pair, the fourth twisted pair having a fourth propagation delay over 100 meters, wherein for the first, second, third, and fourth propagation delays over 100 meters, the difference in propagation delays over 100 meters is within 50 nanoseconds of each other. In some embodiments, the first, second, third, and fourth propagation delays over 100 meters have a delay time difference of less than about 25 nanoseconds. In some embodiments, temporarily altering the hardness of the polymer-insulated conductor includes cooling the polymer-insulated conductor. In some embodiments, temporarily modifying the hardness of the polymer insulated conductors in the first, second, third and fourth pairs of polymer insulated conductors includes cooling the polymer insulated conductors in the first, second, third and fourth pairs for a first, second, third and fourth time period, respectively. In some embodiments, the first time period is greater than the second time period and the second time period is greater than the third time period. In some embodiments, the first time period is between about 8-10 seconds, the second time period is between about 6-8 seconds and the third time period is between about 4-6 seconds.In some embodiments, the first, second, third and fourth twisted pairs have first, second, third and fourth twist lengths, respectively, where the first twist length is shorter than the second twist length and the second twist length is shorter than the third twist length. In some embodiments, the first, second, third and fourth twisted pairs have first, second, third and fourth twist lengths, respectively, where the first twist length is shorter than the second twist length and the second twist length is shorter than the third twist length, the first time is longer than the second time and the second time is longer than the third time. In some embodiments, the polymer insulated conductors of the first, second, third and fourth twisted pairs have first, second, third and fourth crush ratios, respectively. In some embodiments, the first crush ratio is less than the second crush ratio and the second crush ratio is less than the third crush ratio. In some embodiments, the first, second, third and fourth twisted pairs have first, second, third and fourth signaling rates, respectively. In some embodiments, the first signaling rate is greater than the second signaling rate, and the second signaling rate is greater than the third signaling rate. In some embodiments, the first, second, third and fourth pairs of polymer insulated conductors each have a different second hardness. In some embodiments, the second hardness of the first pair of polymer insulated conductors is greater than the second hardness of the second pair of polymer insulated conductors, and the second hardness of the second pair of polymer insulated conductors is greater than the second hardness of the third pair of polymer insulated conductors.An additional embodiment is a method of manufacturing a communications cable comprising the steps of providing a first pair of polymer insulated conductors and a second pair of polymer insulated conductors, each pair of polymer insulated conductors including two polymer insulated conductors, each polymer insulated conductor having a first hardness, the first hardness being a hardness of the polymer insulated conductors under ambient conditions; temporarily changing a hardness of the polymer insulated conductors in the first pair of polymer insulated conductors to a second hardness, the second hardness being different from the first hardness; and The method includes twisting together polymer insulated conductors to form a first twisted pair, the first twisted pair having a first propagation delay over 100 meters, and twisting together a second pair of polymer insulated conductors to form a second twisted pair, the second twisted pair having a second propagation delay over 100 meters, wherein the first propagation delay over 100 meters and the second propagation delay over 100 meters are within 25 nanoseconds of each other. In some embodiments, temporarily altering the hardness of the polymer insulated conductors in the first and second pairs of polymer insulated conductors includes cooling the polymer insulated conductors in the first and second pairs.

[0238] Some disclosed embodiments relate to a system for manufacturing wire and cable products, the system including a payout device configured to pay out a polymer cable component, a cooling vessel configured to receive the polymer cable component, the cooling vessel containing a chilled fluid, and a winding device configured to wind the polymer cable component. In some embodiments, the cooling vessel contains liquid nitrogen. Some embodiments further include a secondary structure configured to receive the polymer cable component, the interior of the secondary structure being in fluid communication with the interior of the cooling chamber. In some embodiments, the cooling vessel contains liquid nitrogen, and nitrogen vapor travels from the interior of the cooling vessel to the interior of the secondary structure. In some embodiments, the secondary structure is a hollow tube. In some embodiments, the atmosphere within the cooling vessel is below ambient temperature. In some embodiments, the cooling vessel is thermally insulated. Some embodiments further include a refrigeration facility, the refrigeration facility configured to provide cold air to the cooling vessel. In some embodiments, the polymer cable component is a polymer insulated conductor, the system further includes a entanglement device configured to receive the first polymer insulated conductor and the second polymer insulated conductor to form a twisted pair. In some embodiments, the atmosphere within the entanglement device is below ambient temperature. Some embodiments further include a secondary structure configured to receive the polymer cable component, an interior of the secondary structure in fluid communication with an interior of the cooling chamber, and the secondary structure in fluid communication with an interior of the entangling device. Additional embodiments relate to a system for manufacturing wire and cable products, the system including an unwinding device configured to unwind the polymer cable component, a cooling surface configured to contact the polymer cable component, and a winding device configured to wind the polymer cable component. In some embodiments, the cooling surface is a chilled roller. Some embodiments further include a plurality of chilled rollers.

[0239] Yet more disclosed embodiments include a method for manufacturing a low fuel load wire and cable product, the method comprising establishing desired electrical properties of the wire and cable product, the wire and cable product including a polymeric cable component, the polymeric cable component having a first fuel load and a first hardness, and a polymeric cable component having a hardness greater than or equal to ASTM D 122 . the polymeric cable component has a flame travel distance of about 5 feet or less, a peak smoke optical density of about 0.5 or less, and an average optical density of about 0.15 or less, when measured according to the Steiner Tunnel Test Method of E84, the first hardness being the hardness of the polymeric cable component under ambient conditions; temporarily changing the hardness of the polymeric cable component to a second hardness, the second hardness being greater than the first hardness; applying a compressive force to the polymeric cable component while the polymeric cable component is at the second hardness, thereby causing a first amount of deformation in the polymeric cable component; and forming a wire and cable product using the polymeric cable component, wherein the wire and cable product meets established desired electrical properties when the polymeric cable component is deformed by the first amount of deformation, but may not meet the desired electrical properties when the polymeric cable component is deformed by the second amount of deformation, the second amount of deformation being an amount that the polymeric cable component deforms when exposed to the compressive force when the polymeric cable component is at the first hardness. In some embodiments, the polymeric cable component is a polymeric insulation layer around the conductive wires. In some embodiments, the wire and cable product is a twisted pair. In some embodiments, the wire and cable product produces a flame travel distance of less than 4 feet when measured by the Steiner Tunnel Test Method of ASTM E84. In some embodiments, the wire and cable product produces a peak smoke optical density of less than 0.4 when measured by the Steiner Tunnel Test Method of ASTM E84. In some embodiments, the wire and cable product produces an average optical density of less than 0.15 when measured by the Steiner Tunnel Test Method of ASTM E84. In some embodiments, the desired electrical property of the wire and cable product is a capacitance value of less than about 20 pf / ft.In some embodiments, the desired electrical characteristic of the wire and cable product is an impedance value between about 75 ohms and 125 ohms. In some embodiments, the desired electrical characteristic of the wire and cable product is a velocity of propagation between about 62% and 80%.

[0240] Additional disclosed embodiments include a method for forming a twisted pair, the method comprising: operating a cable entanglement device at a first speed to produce a first twisted pair of a first collapse ratio; providing a first polymer insulated conductor including a first conductor electrically insulated by a first polymer insulating layer; providing a second polymer insulated conductor including a second conductor electrically insulated by a second polymer insulating layer; exposing at least the first polymer insulated conductor to a cryogenic fluid; and operating the cable entanglement device at a second speed to produce a second twisted pair of a second collapse ratio, the second twisted pair including the first and second polymer insulated conductors, the second speed being faster than the first speed. In some embodiments, the second collapse ratio is within 10% of the first collapse ratio. In some embodiments, the second collapse ratio is less than the first collapse ratio. In some embodiments, the second speed is at least 15% faster than the first speed. In some embodiments, the second speed is at least 25% faster than the first speed. In some embodiments, the first speed is the rated speed of a cable entanglement machine for wire and cable products and the second speed is at least 10% faster than the first speed. In some embodiments, the second speed is at least 10% faster than the first speed and the second crush rate is less than the first crush rate. In some embodiments, the first speed is at least 60 feet / min and the second speed is at least 70 feet / min. In some embodiments, the first speed is at least 160 feet / min and the second speed is at least 180 feet / min. In some embodiments, the first speed is at least 220 feet / min and the second speed is at least 275 feet / min. In some embodiments, the cryogenic fluid is liquid nitrogen.

[0241] Those skilled in the art will recognize improvements and modifications to the preferred embodiments of the present disclosure. All such improvements and modifications are considered to be within the scope of the concepts disclosed herein and the claims that follow. It will be understood that any given element of the disclosed embodiments of the present invention may be embodied in a single structure, a single step, a single material, etc. Likewise, any given element of the disclosed embodiments may be embodied in multiple structures, steps, materials, etc.

[0242] The foregoing description illustrates and describes the process, machine, manufacture, composition of matter, and other teachings of the present disclosure. Moreover, the present disclosure illustrates and describes only certain embodiments of the disclosed process, machine, manufacture, composition of matter, and other teachings, but as stated above, it will be understood that the teachings of the present disclosure can be used in various other combinations, modifications, and environments, and can be changed or modified within the scope of the teachings expressed herein, consistent with the skill and / or knowledge of those of ordinary skill in the relevant art. The embodiments described herein above illustrate certain best modes known for implementing the process, machine, manufacture, composition of matter, and other teachings of the present disclosure, and it is further intended that those skilled in the art can utilize the teachings of the present disclosure in such or other embodiments, and with various modifications as required by a particular application or use. Thus, the process, machine, manufacture, composition of matter, and other teachings of the present disclosure are not intended to be limited to the exact embodiments and examples disclosed herein. Any section headings herein are provided solely for consistency with proposed 37 CFR §1.77 and otherwise to provide organizational cues, and in no way limit or characterize the invention described herein.

Claims

1. 1. A method for reducing the effects of compressive forces on a polymer cable component, comprising: providing a polymeric cable component having a first hardness, the first hardness being a hardness of the polymeric cable component under ambient conditions; temporarily changing a hardness of the polymer cable component to a second hardness, the second hardness being different from the first hardness; applying a compressive force to the polymer cable component; and returning the polymer cable component to the first hardness. The method, wherein the step of temporarily altering a hardness of the polymer cable component comprises cooling the polymer cable component, and the step of cooling the polymer cable component comprises exposing the polymer cable component to a cryogenic liquid, and the polymer cable component is exposed to the cryogenic liquid for between 6 seconds and 10 seconds.

2. The method of claim 1 , further comprising applying a compressive force to the polymeric cable component while the polymeric cable component has the second hardness.

3. 10. The method of claim 1, wherein the compressive force causes less deformation in the polymeric cable component at the second hardness than in the polymeric cable component at the first hardness.

4. The method of claim 1 , wherein the second hardness is greater than the first hardness.

5. The method of claim 1 , wherein the polymer cable component comprises an exterior surface, an interior bulk, and an interior surface, and cooling the polymer cable component comprises cooling the exterior surface of the polymer cable component.

6. The method of claim 1 , wherein the polymer cable component is a polymer insulation surrounding the conductor.

7. The method of claim 1 , wherein the polymeric cable component is a fluoropolymer insulation surrounding the conductor.

8. The method of claim 1 , wherein the polymer cable component is not allowed to cool for a period of 10 seconds or less before the compressive force is applied.

9. The method of claim 1 , further comprising the step of stopping cooling of the polymer cable component for a period of 5 seconds or less before the polymer cable component is subjected to a compressive force.

Citation Information

Patent Citations

  • Stranded wire and method of manufacture therefor

    WO2019208401A1