Dual Slot Die Coater
The dual slot die coater addresses non-uniformity and complexity in conventional coaters by facilitating easy die lip alignment and consistent coating gaps, enhancing electrode quality and productivity.
Patent Information
- Application Number
- JP2023530717
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-06-13
- Filing Date
- 2022-09-07
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2042-09-07
AI Technical Summary
Conventional slot die coaters face challenges in uniformly coating thick active material layers for secondary batteries, leading to non-uniform electrodes due to binder and conductive material migration during drying, and require complex alignment of die lips that is skill-dependent and time-consuming.
A dual slot die coater with integrated die blocks and shims that allow for easy alignment of die lips, maintaining a consistent coating gap through surface contact with the base and use of fixed bolts, reducing reliance on operator skill and adjustment time.
Ensures uniform coating of active material layers with improved productivity and reproducibility, preventing die block deformation and maintaining coating quality under high-speed conditions.
Smart Images

Figure 0007566152000001 
Figure 0007566152000002 
Figure 0007566152000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a dual slot die coater capable of simultaneously forming two or more layers by a wet process, and more particularly to a vertical die type dual slot die coater in which the coating liquid is discharged in the direction opposite to gravity.
[0002] This application claims priority to Korean Patent Application No. 10-2021-0167687 filed on November 29, 2021, and Korean Patent Application No. 10-2022-0071278 filed on June 13, 2022, and the contents disclosed in the specification and drawings of said applications are incorporated herein in their entirety. [Background technology]
[0003] As technology for mobile devices develops and demand increases, the need for secondary batteries as an energy source is growing rapidly. Such secondary batteries essentially include an electrode assembly, which is a power generating element. The electrode assembly has a form in which a positive electrode, a separator, and a negative electrode are laminated at least once, and the positive electrode and the negative electrode are manufactured by coating and drying a positive electrode active material slurry and a negative electrode active material slurry on a current collector made of aluminum foil and copper foil, respectively. In order to make the charge and discharge characteristics of the secondary battery uniform, the positive electrode active material slurry and the negative electrode active material slurry must be uniformly coated on the current collector, and a slot die coater has been used in the past.
[0004] FIG. 1 is a cross-sectional view showing a conventional slot die coater.
[0005] Referring to FIG. 1, in a conventional method for manufacturing an electrode using a slot die coater 30, an active material slurry discharged from the slot die coater 30 is applied onto a current collector 20 conveyed by a coating roll 10. The active material slurry discharged from the slot die coater 30 is widely applied to one side of the current collector 20 to form an active material layer. The slot die coater 30 includes two die blocks 31 and 32, and a slot 35 is formed between the two die blocks 31 and 32. One type of active material slurry is discharged from a discharge port 37 communicating with one slot 35 to form one active material layer. The slot die coater has an advantage of being able to apply at high speed compared to bar coating and comma coating, and is therefore widely used from the viewpoint of high productivity. The slot die coater illustrated in FIG. 1 is a vertical die type that discharges an active material slurry in the direction opposite to gravity.
[0006] In order to manufacture secondary batteries with high energy density, the thickness of the active material layer, which was about 130 μm, has gradually increased to 300 μm. If this thick active material layer is formed using a conventional slot die coater 30, the migration of the binder and conductive material in the active material slurry becomes severe during drying, resulting in a non-uniform final electrode. To solve this problem, a two-step coating process is performed in which the active material layer is thinly coated, dried, and then coated again on top of that and dried, but this process takes a long time. In order to simultaneously improve electrode performance and productivity, a dual slot die coater that can coat two types of active material slurries at the same time is required.
[0007] In a slot die coater, a slot is formed on the bonding surface of the die block, so that a dual slot die coater having two slots basically requires three die blocks. In a process using such a dual slot die coater, it is necessary to use active material slurry that is simultaneously discharged from different discharge ports that communicate with the two slots, respectively, so that it is very difficult to form each active material layer to the desired thickness.
[0008] In particular, the alignment (positioning) of the die lip, which is the tip of each die block, is important. The alignment of the die lip can be performed by inserting a block or a spacer to assemble and align the die block, or by adjusting the position using a bolt or the like. However, the insertion of the block or spacer has multiple conditions, such as the need to properly align multiple contact surfaces in order to align the die lip, and is therefore difficult simply in terms of probability. In addition, the adjustment function of bolts or the like takes time, and is highly dependent on the skill of the fastening (tightening) operator, which can lead to problems such as poor reproducibility.
[0009] Thus, there is a need in the art for a dual slot die coater that allows easier and more accurate alignment of the die lips. Summary of the Invention [Problem to be solved by the invention]
[0010] The present invention has been made in consideration of the above-mentioned problems, and the problem that the present invention aims to solve is to provide a dual slot die coater that can easily align the die lips.
[0011] However, the problems to be solved by the present invention are not limited to the problems described above, and other problems not mentioned will be clearly understood by those skilled in the art from the description of the invention described below. [Means for solving the problem]
[0012] The dual slot die coater of the present invention for solving the above-mentioned problems is a dual slot die coater having a first slot and a second slot for ejecting a coating liquid in a direction opposite to gravity, and includes: a first die block that is hung integrally with the base at the rear of the upper surface of the base; a second die block that is arranged in front of the first die block in contact with the base and forms the first slot between it and the first die block; and a third die block that is arranged in front of the second die block in contact with the base and forms the second slot between it and the second die block.
[0013] In one embodiment, a lower surface of the second die block and a lower surface of the third die block may be in overall surface contact with the base.
[0014] In another embodiment, a lower surface of the second die block and a lower surface of the third die block may be in intermittent surface contact with the base.
[0015] In this case, a pressing portion may be connected to the lower end of the base portion.
[0016] The pressing portion may be a servo motor.
[0017] The dual slot die coater of the present invention may further include a first shim disposed between the first die block and the second die block to form the first slot, and a second shim disposed between the second die block and the third die block to form the second slot, and the first shim and the second shim may have at least one area cut out to have an opening.
[0018] In this case, the one region may be intermittently cut to provide a plurality of openings.
[0019] In a preferred example, a lower surface of the second die block may be formed with reinforcing portions so as to be in discontinuous surface contact with the base, and a bending space may be formed between the reinforcing portions. A lower surface of the third die block may be formed with reinforcing portions so as to be in discontinuous surface contact with the base, and a bending space may be formed between the reinforcing portions.
[0020] In this preferred example, a servo motor for deforming the bending space may be connected to a lower end of the base. More preferably, the servo motor may be connected to a center of the lower end of the base.
[0021] A plurality of the reinforcing parts may be provided in the longitudinal direction of the dual slot die coater. Preferably, the reinforcing parts may be arranged symmetrically in the longitudinal direction with respect to the center of the dual slot die coater in the longitudinal direction. Preferably, the spacing between the reinforcing parts in the central part among the plurality of reinforcing parts may be configured to be larger than the spacing between the other reinforcing parts.
[0022] In the present invention, the first die block may include a first manifold that contains a first coating liquid and communicates with the first slot, and the third die block may include a second manifold that contains a second coating liquid and communicates with the second slot.
[0023] In the dual slot die coater according to the present invention, a bolt may be fastened perpendicular to a contact surface between the base and the second die block, and a bolt may be fastened perpendicular to a contact surface between the base and the third die block.
[0024] The first slot may be disposed perpendicular to the base.
[0025] The cross section of the second die block may be a right triangle.
[0026] Each of the first die block, the second die block and the third die block may have a first die lip, a second die lip and a third die lip forming a tip end thereof, and the first die lip, the second die lip and the third die lip may be positioned on a straight line.
[0027] The thickness of the third die lip is preferably greater than the thickness of the first die lip and the thickness of the second die lip.
[0028] A second outlet communicating with the second slot is formed between the third die lip and the second die lip, and a first outlet communicating with the first slot is formed between the second die lip and the first die lip, the second outlet outlet outlets a second coating liquid onto a substrate, and the first outlet outlet is spaced apart from the second outlet downstream in a coating direction and outlets a first coating liquid onto the substrate. Effect of the Invention
[0029] According to the present invention, the die block is disposed in contact with the base, so that the die lip can be easily aligned. The positional deviation between the die blocks can be prevented, and the distance between the die lip and the substrate, i.e., the coating gap, can be always maintained at a desired level. Since the alignment of the die lip is uniform for each assembly and hardly changes during the process, the occurrence of deviation in the coating gap in the width direction perpendicular to the traveling direction of the substrate can be suppressed.
[0030] Therefore, according to the present invention, it is not necessary to adjust the coating gap by disassembling and reassembling the die block, which is structurally fragile due to its thinness, or to use auxiliary devices such as blocks or spacers. Instead, a constant coating gap can be maintained at all times through the simple assembly process of assembling the die blocks.
[0031] According to the present invention, even when considering that the die block is deformed by the pressure of the discharged active material slurry, a uniform (±2%) coating gap is maintained, so that the coating amount and the resulting coating quality can be uniformly controlled. Therefore, by using a dual slot die coater having a uniform coating gap, a coated product, particularly an electrode for a secondary battery, having uniform quality can be obtained.
[0032] According to one aspect of the present invention, there is provided a dual slot die coater having a one-contact fastening system, which is the minimum condition for assembly and alignment, and a structure that does not require a position adjustment system using bolts or the like. With an adjustment function using bolts or the like, the adjustment itself takes time, is highly dependent on the skill of the fastening operator, and there is a possibility that reproducibility is poor. According to the present invention, the die lip can be aligned without the need for a position adjustment system using bolts or the like, so the adjustment does not take time, is not dependent on the skill of the operator, and is highly reproducible.
[0033] According to another aspect of the present invention, even with a single contact surface clamping method, it is possible to ensure space for bending. Bending is a process of deforming a portion that needs to be aligned, and according to the present invention, even when a pressing portion is used to control the coating uniformity in the width direction, the deformation is achieved with high uniformity. Thus, according to the present invention, the deformation of the die block can be controlled extremely uniformly, resulting in excellent coating uniformity, which is a major advantage in that it can be easily achieved.
[0034] Thus, the present invention has an excellent effect of maintaining the coating gap once adjusted even if the discharge pressure of the active material slurry becomes high or a thin die block is used. In particular, in the case of a vertical die type, there is a problem that the die block spreads due to discharge, but the present invention has an effect of preventing the die block from spreading, thereby ensuring the coating processability and reproducibility.
[0035] Use of such a dual slot die coater allows a coating layer, particularly an active material layer, to be formed uniformly to a desired thickness, and preferably allows two types of active material slurries to be coated simultaneously, resulting in the advantages of excellent performance and productivity.
[0036] In this way, when the dual slot die coater of the present invention is used, there is an advantage in that, when producing electrodes for secondary batteries, etc., it is possible to uniformly coat the active material slurry onto the current collector while the current collector is traveling, even under high-speed traveling conditions or long-width coating conditions.
[0037] The following drawings attached to this specification illustrate preferred embodiments of the present invention and, together with the detailed description of the invention described below, serve to further understand the technical ideas of the present invention. Therefore, the present invention should not be interpreted as being limited only to the matters depicted in such drawings. [Brief description of the drawings]
[0038] [Figure 1] FIG. 1 is a schematic cross-sectional view of a dual slot die coater according to the prior art. [Diagram 2] FIG. 2 is a perspective view of a dual slot die coater according to one embodiment of the present invention. [Diagram 3] FIG. 2 is a cross-sectional view of a dual slot die coater according to one embodiment of the present invention. [Figure 4] FIG. 4 is an enlarged view of part A in FIG. [Diagram 5] FIG. 2 is a perspective view of a dual slot die coater according to another embodiment of the present invention. [Figure 6] 6 is a cross-sectional view taken along line VI-VI' of FIG. 5. [Figure 7] 7 is a cross-sectional view taken along the line VII-VII' of FIG. 5. [Figure 8] 13 is a flowchart of the steps for assembling a dual slot die coater according to yet another embodiment of the present invention. [Figure 9]11A-11D are diagrams illustrating the assembly steps of a dual slot die coater according to yet another embodiment of the present invention. [Figure 10] 11A-11D are diagrams illustrating the assembly steps of a dual slot die coater according to yet another embodiment of the present invention. [Figure 11] 11A-11D are diagrams illustrating the assembly steps of a dual slot die coater according to yet another embodiment of the present invention. [Figure 12] 11A-11D are diagrams illustrating the assembly steps of a dual slot die coater according to yet another embodiment of the present invention. [Figure 13] FIG. 1 is a diagram to aid in understanding the structure of a die block. [Figure 14] FIG. 1 is a diagram to aid in understanding the structure of a die block. [Figure 15] FIG. 1 is a diagram to aid in understanding the structure of a die block. [Figure 16] FIG. 2 is a cross-sectional view of a dual slot die coater according to a comparative example. [Figure 17] FIG. 2 is a diagram showing the assembly steps of a dual slot die coater according to a comparative example. [Figure 18] FIG. 2 is a diagram showing the assembly steps of a dual slot die coater according to a comparative example. [Figure 19] FIG. 2 is a diagram showing the assembly steps of a dual slot die coater according to a comparative example. [Figure 20] FIG. 2 is a diagram showing the assembly steps of a dual slot die coater according to a comparative example. [Figure 21] FIG. 13 is a diagram showing the effect of reducing the mold replacement (mold exchange) time due to the die block structure / simplified assembly design in yet another embodiment of the present invention, compared to the comparative example. [Figure 22] This shows the effect of improving electrode quality due to improved assembly quality in yet another embodiment of the present invention compared to the comparative example. [Diagram 23] FIG. 13 is a schematic diagram for analyzing the operation effect of a servo motor after bolt tightening in a comparative example and still another embodiment of the present invention. [Figure 24]13 is a graph comparing deformation (μm) in the coating gap direction due to operation of a servo motor in a comparative example and yet another embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0039] Hereinafter, a preferred embodiment of the present invention will be described in detail with reference to the accompanying drawings. Prior to this, the terms and words used in the present specification and claims should not be interpreted as being limited to their ordinary or dictionary meanings, but should be interpreted as being in accordance with the meaning and concept of the technical idea of the present invention, in accordance with the principle that the inventor himself can appropriately define the concept of the term in order to best describe the invention. Therefore, it should be understood that the embodiment described in this specification and the configuration shown in the drawings are merely one most preferred embodiment of the present invention, and do not represent the entire technical idea of the present invention, and therefore there may be various equivalents and modifications that can be substituted therefor at the time of this application. The same drawing symbols indicate the same components. Also, in the drawings, the thickness, ratio, and size of the components are exaggerated for the effective description of the technical contents.
[0040] The dual slot die coater of the present invention is an apparatus that includes a first slot and a second slot for discharging the coating liquid in a direction opposite to gravity, and coats the substrate with the coating liquid in a double layer. The "substrate" described below is a current collector, and the "coating liquid" is an active material slurry. The first coating liquid and the second coating liquid are both active material slurries, and may refer to active material slurries having the same or different compositions (types of active material, conductive material, and binder), contents (amounts of active material, conductive material, and binder), and physical properties. The dual slot die coater of the present invention is optimized for manufacturing an electrode in which two types of active material slurries are applied simultaneously or two types of active material slurries are applied alternately to perform pattern coating. However, the scope of the present invention is not necessarily limited thereto. For example, the substrate is a porous support constituting a separator, and the first coating liquid and the second coating liquid may be organic materials having different compositions and physical properties. In other words, if a thin film coating is required, the substrate, the first coating liquid, and the second coating liquid may be any type.
[0041] Fig. 2 is a perspective view of a dual slot die coater according to an embodiment of the present invention, Fig. 3 is a cross-sectional view of the dual slot die coater according to an embodiment of the present invention, and Fig. 4 is an enlarged view of part A in Fig. 3.
[0042] 2 and 3, a dual slot die coater 100 according to an embodiment of the present invention is for discharging a coating liquid in a direction opposite to gravity, and includes a first slot 101 and a second slot 102. Two types of coating liquids, which may be the same or different from each other, may be discharged through the first slot 101 and the second slot 102 and coated onto a substrate 170 simultaneously or alternately.
[0043] For example, a rotatable coating roll 160 is disposed in front of the dual slot die coater 100, and the substrate 170 to be coated is moved by rotating the coating roll 160, and the first coating liquid 50, which is a first electrode active material slurry, and the second coating liquid 60, which is a second electrode active material slurry, are successively brought into contact with the surface of the substrate 170, thereby simultaneously coating the substrate 170 in a two-layer structure. The first coating liquid 50 is first coated onto the substrate 170 to form a lower slurry layer, and almost simultaneously, the second coating liquid 60 is coated onto the lower slurry layer to form an upper slurry layer.
[0044] The dual slot die coater 100 is disposed in a direction (X direction) in which the active material slurry as a coating liquid is discharged almost vertically (approximately ±5 degrees). In the embodiment of the present invention, the X-axis direction shown in the drawings means the direction in which the coating liquid is discharged, the Z-axis direction means the longitudinal direction of the dual slot die coater 100, and the Y-axis direction means a horizontal direction perpendicular to both the X-axis direction and the Z-axis direction, and particularly means the direction from the first die block of the dual slot die coater 100 to the third die block 130 side, and for convenience, it can be said to be the front side of the dual slot die coater 100.
[0045] The dual slot die coater 100 includes a base 90. The first die block 110 is vertically attached integrally to the base 90 at the rear of the upper surface of the base 90. The first die block 110 has a plate-like structure extending in the longitudinal direction. The first die block 110 is placed on the base 90 for assembly. When the base 90 and the first die block 110 are integrated in this manner, they do not need to be aligned with the base 90 and can be handled as a single unit, making handling easy. The first die block 110 integrated with the base 90 may be referred to as a body block or an upper plate. The XY cross section of the first die block 110 may be substantially L-shaped.
[0046] The second die block 120 is disposed in front of the first die block 110 in contact with the base 90, and forms a first slot 101 between the second die block 120 and the first die block 110. To define the first slot 101, a first shim 113 is provided between the second die block 120 and the first die block.
[0047] A first slot 101 corresponding to a passage through which the coating liquid can flow may be formed by providing a gap between the second die block 120 and the first die block using the first shim 113. In this case, the vertical width (slot gap) of the first slot 101 is determined by the thickness of the first shim 113. The first shim 113 may be referred to as an upper layer shim.
[0048] The first shim 113 may have at least one region cut out to provide an opening, and may be disposed in the remaining portion except for one side of the edge region of each of the opposing surfaces of the first die block 110 and the second die block 120. As a result, a first discharge port 110a through which the coating liquid can be discharged to the outside is formed only between the front end of the first die block 110 and the front end of the second die block 120.
[0049] 4, the leading end of the first die block 110 and the leading end of the second die block 120 are defined as the first die lip and the second die lip 121, respectively, and in other words, the first discharge port 101a is formed by separating the first die lip 111 and the second die lip 121 from each other. The first die lip 111 and the second die lip 121 may extend in the longitudinal direction and may have a rectangular parallelepiped shape with a flat upper surface.
[0050] For reference, the first shim 113 is preferably made of a material having sealing properties, since it also functions as a gasket to prevent the coating liquid from leaking from the gap between the first die block 110 and the second die block 120, except for the area where the first discharge port 101a is formed.
[0051] The second die block 120 is a block located in the middle of the die blocks constituting the dual slot die coater 100, and is disposed between the first die block 110 and the third die block 130 to form a double slot. The second die block 120 in this embodiment has a right-angled triangular cross section, but is not necessarily limited to such a shape, and may have an isosceles triangular cross section, for example. When the cross section is a right-angled triangle, the first slot 101 is aligned approximately perpendicular to the substrate 170, and therefore, the discharge of the coating liquid by the first slot 101 can be easily controlled.
[0052] The second die block 120 also has a plate-like structure extending in the longitudinal direction. In the second die block 120, the first surface 120a facing the first die block 110 is positioned approximately perpendicular to the base 90. That is, the first surface 120a of the second die block 120 is a vertical surface. In the first die block 110, the second surface 110b, which is the surface facing the first surface 120a of the second die block 120, and the first surface 110a, which is the opposite surface (i.e., the surface forming the rear surface of the outer circumferential surface of the dual slot die coater 100), are also positioned approximately perpendicular to the base 90. That is, the first surface 110a and the second surface 110b of the first die block 110 are also vertical surfaces. As a result, the first slot 101 is perpendicular to the base 90. In this way, the first surface 120a of the second die block 120 and the first surface 110a and second surface 110b of the first die block 110 are approximately parallel to each other, resulting in a stable and well-balanced structure overall. In the first die block 110, an inclined surface 110a' inclined toward the discharge direction is formed on the upper side of the first surface 110a, so that the upper cross section of the first die block 110 has an approximately triangular shape and has a structure concentrated toward the first die lip. The second die block 120 is sometimes called an inner die or a middle plate.
[0053] The first die block 110 has a first manifold 112 having a predetermined depth in the second surface 110b and communicating with the first slot 101. The first manifold 112 is a space provided in the first die block 110 from the second surface 110b facing the second die block 120 toward the first surface 110a, which is the opposite surface of the second surface 110b. The first manifold 112 is a recessed (concave) chamber provided in the first die block 110 and contains a first coating liquid. The first manifold 112 is connected to a first coating liquid supply chamber (not shown) disposed outside by a supply pipe and receives the supply of the first coating liquid. When the first manifold 112 is filled with the first coating liquid, the flow of the first coating liquid is guided along the first slot 101 and discharged to the outside through the first discharge port 101a.
[0054] The first die block 110 may further include an air vent (not shown) that penetrates the first die block 110 and is connected to the first manifold 112. The air vent removes air bubbles contained in the first coating liquid in the first manifold 112. This air vent may be provided by simply drilling a hole in the first die block 110, or by inserting a hollow pipe into the hole.
[0055] The third die block 130 is disposed on the front surface of the second die block 120 in contact with the base 90, and forms a second slot 102 between the third die block 130 and the second die block 120. A second shim 133 is provided between the third die block 130 and the second die block 120 to define the second slot 102. In this manner, the second slot 102 is formed between the second die block 120 and the third die block 130 facing each other. That is, the second slot 102 is formed by the joining of the third die block 130 and the second die block 120.
[0056] Similar to the above-described first slot 101, a second slot 102 corresponding to a passage through which the coating liquid can flow is formed between the second die block 120 and the third die block 130 by providing a gap by the second shim 133. In this case, the vertical width (slot gap) of the second slot 102 is determined by the thickness of the second shim 133. The second shim 133 may be referred to as a lower shim.
[0057] The second shim 133 also has a structure similar to the first shim 113 described above, with at least one region cut out to provide an opening, and is interposed only in the remaining portions except for one side of the edge regions of the opposing surfaces of the second die block 120 and the third die block 130. Similarly, the second slot 102 is closed in the circumferential direction except for the front, and a second discharge port 102a is formed only between the tip end of the second die block 120 and the tip end of the third die block 130.
[0058] 4, the tip of the third die block 130 is defined as the third die lip 131. In other words, the second discharge port 102a is formed by separating the second die lip 121 and the third die lip 131 from each other. The third die lip 131 may also extend in the longitudinal direction and may have a rectangular parallelepiped shape with a flat upper surface.
[0059] In this manner, the second discharge port 102a communicating with the second slot 102 is formed between the third die lip 131 and the second die lip 121, and the first discharge port 101a communicating with the first slot 101 is formed between the second die lip 121 and the first die lip 111. The second discharge port 102a discharges the second coating liquid 60 forming the lower slurry layer onto the substrate 170, and the first discharge port 101a is spaced downstream in the coating direction from the second discharge port 102a and discharges the first coating liquid 50 forming the upper slurry layer onto the lower slurry layer on the substrate 170. When the first coating liquid 50 and the second coating liquid 60 such as an electrode active material slurry are supplied while the substrate 170 is traveling in a direction from the third die lip 131 toward the first die lip, an electrode can be formed while an upper slurry layer is formed on the lower slurry layer.
[0060] The third die block 130 also has a plate-like structure extending in the longitudinal direction. In addition, the second surface 120b of the second die block 120 facing the third die block 130, the first surface 130a of the third die block 130 facing the second surface 120b of the second die block 120, and the second surface 130b (i.e., the surface forming the front surface of the outer circumferential surface of the dual slot die coater 100) are almost parallel to each other, and the third die block 130 has a stable and well-balanced structure in appearance. On the upper side of the second surface 130b of the third die block 130, an inclined surface 130b' inclined toward the discharge direction is formed. The upper cross section of the third die block 130 also has a nearly triangular shape and has a structure concentrated toward the third die lip 131. A lower surface 130b'' of the second surface 130b of the third die block 130 is positioned approximately perpendicular to the base 90. The third die block 130 may be referred to as an outer die or a lower plate.
[0061] The third die block 130 also includes a second manifold 132 that has a predetermined depth on a first surface 130a that faces the second die block 120 and communicates with the second slot 102. The second manifold 132 is a space that is provided in the third die block 130 from the first surface 130a that faces the second die block 120 toward a second surface 130b that faces the first surface 130a. The second manifold 132 is a recessed (concave) chamber that is provided in the third die block 130 and contains the second coating liquid. Although not shown in the figure, the second manifold 132 is connected to a second coating liquid supply chamber provided outside by a supply pipe to receive the supply of the second coating liquid. When the second coating liquid is supplied from the outside along a pipe-shaped supply tube and fills the second manifold 132, the flow of the second coating liquid is guided along the second slot 102 communicating with the second manifold 132 and is discharged to the outside through the second discharge port 102a.
[0062] The third die block 130 may further include an air vent (not shown) that penetrates the third die block 130 and is connected to the second manifold 132. The air vent removes air bubbles contained in the second coating liquid in the second manifold 132. This air vent may be provided by simply drilling a hole in the third die block 130, or by inserting a hollow pipe into the hole.
[0063] The second slot 102 and the first slot 101 may form a certain angle, which may be about 20 degrees to 70 degrees. The second slot 102 and the first slot 101 may intersect with each other at one point, and the second outlet 102a and the first outlet 101a may be provided near the intersection. This allows the first coating liquid 50 and the second coating liquid 60 to be discharged at approximately one point.
[0064] The angle θ between the second surface 120b of the second die block 120 facing the third die block 130 and the first surface 120a of the second die block 120 facing the first die block 110 is preferably within a range in which the second coating liquid 60 discharged from the second outlet 102a and the first coating liquid 50 discharged from the first outlet 101a do not form a vortex immediately after simultaneous discharge. If the angle θ is too small, the second die block 120 becomes too thin and is very weak against deformation and twisting. Such an angle θ may determine the angle between the second slot 102 and the first slot, so it may be an angle of about 20 degrees to 70 degrees. It may be preferably 25 degrees. The angle between the second surface 110b and the inclined surface 110a' of the first die block 110 may be 70 degrees. The angle between the first surface 130a and the inclined surface 130b' of the third die block 130 may be 60 degrees. When configured in this manner, the die blocks 110, 120, 130 have an overall appearance of a roughly rectangular parallelepiped when assembled, and only the front part from which the coating liquid is ejected has an oblique shape toward the substrate 170, so that in the unlikely event that the coating liquid does flow down, it is easy to deal with. Furthermore, the shape after assembly is almost similar to that of a slot die coater equipped with a single slot, which has the advantage that the support body of the slot die coater can be shared.
[0065] The first manifold 112 and the second manifold 132 are formed in the first die block 110 and the third die block 130, respectively. In this manner, it is possible to reduce the influence on the deformation of the second die block 120, which is structurally the weakest. In addition, by dividing the second die block 120 into a left die and a right die, and configuring the left die to move integrally with the first die block 110 and the right die to move integrally with the third die block 130, the left die block and the right die block can be slid at the interface between the left die and the right die, thereby realizing a structure in which the positions of the first slot 101 and the second slot 102 can be changed more easily.
[0066] The surfaces opposite to the direction in which the coating liquid is discharged from the first die block, the second die block 120, and the third die block 130, i.e., the bottom surfaces, are approximately horizontal (YZ plane). In such die blocks 110, 120, and 130, the corners between the surfaces form right angles, so that right angles exist in a cross-sectional view and a vertical or horizontal plane can be used as the reference surface. This makes them easy to manufacture and handle, and also ensures precision.
[0067] The die blocks 110, 120, 130 are made of, for example, SUS material. Materials that are easy to process, such as SUS420J2, SUS630, SUS440C, SUS304, SUS316L, etc., can be used. SUS has the advantages of being easy to process, inexpensive, highly corrosion resistant, and capable of being manufactured into a desired shape at low cost.
[0068] A bolt 141 may be fastened perpendicular to the contact surface between the base 90 and the second die block 120, and a bolt 142 may be fastened perpendicular to the contact surface between the base 90 and the third die block 130. The first die block 110 and the second die block 120 may be fastened to each other by a bolt (not shown). The second die block 120 and the third die block 130 may also be fastened to each other by a bolt (not shown). When the first die block, the second die block 120, and the third die block 130 are fastened to each other by the bolts 141 and 142 in an assembled state, the facing portions can be supported to each other with a high degree of surface contact, which provides excellent fastening and maintenance.
[0069] As described above, the dual slot die coater 100 may be manufactured from SUS (stainless steel). In general, liquid leakage is likely to occur at the joint surfaces of SUS assemblies, so liquid leakage is suppressed by interposing a rubber ring or other soft material between the components to seal them. However, such a sealing method is not suitable for controlling a uniform assembly form (e.g., assembly deviation of less than 10 μm), and therefore it has been difficult to apply it to a dual slot die coater.
[0070] For this reason, the dual slot die coater 100 is assembled by fastening the die blocks 110, 120, 130, which have been machined to extremely high precision (straightness and flatness ±5 μm), with bolts. Since it is necessary to prevent liquid leakage, the bolts are preferably fastened with a high pressure of about 200 to 350 N.
[0071] According to the present invention, the assembly method is improved. Since all the bolts used for fastening are fixed type and not adjustable type, there is no time loss caused by the adjustment itself, it does not depend on the skill level of the tightening (fastening) operator, and the method is highly reproducible.
[0072] According to the present invention, the structure of the die blocks 110, 120, and 130 is changed compared to the conventional structure. The lower surface of the second die block 120 and the lower surface of the third die block 130 are in surface contact with the base 90 as a whole. There is no free space between the second die block 120 and the base 90. As a result, even if torque is generated due to the internal pressure of the dual slot die coater 100, the first die block 110 and the second die block 120 can support their abutting surfaces with the first shim 113 sandwiched therebetween. In other words, the first slot 101 can be prevented from widening. Similarly, there is no free space between the third die block 130 and the base 90. Therefore, even if torque is generated due to the internal pressure of the dual slot die coater 100, the second die block 120 and the third die block 130 can support their abutting surfaces with the second shim 133 sandwiched therebetween. In other words, the second slot 102 can be prevented from widening.
[0073] In the conventional vertical die type slot die coater, there is a problem that the gap between the die blocks widens due to the pressure when the coating liquid is discharged. In the dual slot die coater 100 of the present invention, the lower surface of the second die block 120 and the lower surface of the third die block 130 are in surface contact with the base 90 as a whole, and the second die block 120 and the third die block 130 are fixed by the base 90, so that the gap between the first slot 101 and the second slot 102 is prevented from widening. When the gap between the die blocks widens and the active material slurry flows in, the active material slurry intermittently adheres to the non-coated portion, causing a problem of surface defects. However, when the dual slot die coater 100 of the present invention is used, an electrode can be formed without surface defects.
[0074] Moreover, since the second die block 120 and the third die block 130 are disposed adjacent to the base 90, according to the present invention, alignment (alignment) of the die blocks 110, 120, 130 is not required separately and is very easy. Since the second die block 120 and the third die block 130 are always disposed adjacent to the base 90 so that there is no empty space between them, the positions of the die lips 111, 121, 131 are fixed for each assembly. Therefore, alignment of the die lips is easy, accurate, and not dependent on the operator.
[0075] The vertical lengths of the die blocks 110, 120, and 130 may be the same. The vertical length refers to the vertical distance from the lower surface of each die block to the die lip. If the vertical lengths of the die blocks 110, 120, and 130 are equal, the first die lip 121, the second die lip 131, and the third die lip 131 can be positioned on the same straight line simply by assembling them, as shown in FIG.
[0076] As described above, according to the present invention, a separate operation for aligning the die lip is not required. The present invention has a one-surface fastening method (the upper surface of the base 90 and the lower surface of the second die block 120, and the upper surface of the base 90 and the lower surface of the third die block 130), which is the minimum condition for assembly and alignment, and has a structure that does not require an adjustment function. In addition, the alignment state during assembly is very excellent.
[0077] In the coating process using the dual slot die coater 100, the first and second coating liquids 50, 60 are simultaneously discharged from different discharge ports 101a, 102a, so it is desirable that problems such as leaking and side rings do not occur. Among these, leaking means instability in which a part of the coating liquid flows out from the outside of the die lip to the upstream side. This means a loss of the coating liquid that has been measured in advance, and as a result, the final coating thickness cannot be predicted. Such leakage may cause the coating liquid to remain for a long time and solidify, or cause deviations in the coating thickness in the width direction. In particular, when the coating liquid is discharged at high pressure with the coating gap lowered to several hundred μm in order to achieve the purpose of thin film coating or to reduce the thickness deviation in the width direction of the coating layer, such leakage may become serious.
[0078] There is an appropriate coating area (window margin) between the leak occurrence area and the side ring occurrence area. The wider this appropriate process area, the higher the productivity. The coating gap greatly affects the size and shape of the coating bead formed between the substrate 170 and the die lips 111, 121, 131 during coating, as well as the position of the dynamic contact line. According to the present invention, there is an advantage that the coating gap can be temporarily kept uniform by aligning the die lips 111, 121, 131, and by adjusting the size of the die lips 111, 121, 131 to widen the coating gap to the appropriate process area, it is possible to adjust the initial conditions such as the physical properties of the coating liquid, the flow rate and flow speed of the coating liquid, and the like, and thus have more leeway in setting the initial conditions to minimize the occurrence of leakage.
[0079] Preferably, the third die lip thickness D3 is greater than the second die lip thickness D2 and the first die lip thickness D1. Thus, the third die lip thickness D3 is greater than the average thickness of the first die lip thickness D1 and the second die lip thickness D2. In this way, the third die lip thickness D3 is the largest (D3>D2, D3>D1, D3>(D1+D2) / 2), and the second die lip thickness D2 and the first die lip thickness D1 may be equal to each other.
[0080] The third die lip thickness D3:first die lip thickness D1 may be 1.2:1 or more. That is, the third die lip thickness D3 may be 1.2 times or more than the first die lip thickness D1. If the third die lip thickness D3 is larger than the first die lip thickness D1, the suitable process area may increase, but if the third die lip thickness D3 is 1.2 times or more than the first die lip thickness D1, the occurrence of leakage can be reliably suppressed. If the third die lip thickness D3 and the first die lip thickness D1 are the same or the first die lip thickness D1 is larger than the third die lip thickness D3, leakage will occur.
[0081] The third die lip thickness D3:second die lip thickness D2 may be 1.2:1 or more. That is, the third die lip thickness D3 may be 1.2 times or more the second die lip thickness D2. When the third die lip thickness D3 is larger than the second die lip thickness D2, the suitable process area may increase, but when the third die lip thickness D3 is 1.2 times or more the second die lip thickness D2, the occurrence of leakage can be reliably suppressed. When the third die lip thickness D3 and the second die lip thickness D2 are the same, leakage occurs. When the second die lip thickness D2 is larger than the third die lip thickness D3, other pattern defects may occur even if leakage does not occur.
[0082] According to the above example, the third die lip thickness D3 is the largest because it is larger than the second die lip thickness D2 and the first die lip thickness D1. The inventors of the present invention have confirmed that the larger the third die lip thickness D3, the wider the suitable process area. Therefore, there is more room for controlling the coating gap and setting the initial conditions. Therefore, such a configuration has excellent productivity and allows the dynamic contact line during coating to be used at various positions depending on the target coating product and quality. According to the present invention, as a result of the widening of the suitable process area, the leak limit can be improved, that is, expanded. In addition, the side ring occurrence area can be reduced. When the dynamic contact line moves in the opposite direction to the coating due to the reduction of the coating gap, leakage occurs at a certain level or more, so according to this configuration, the third die lip thickness D3 can be increased to improve leakage. This is because the electrode active material slurry can remain in large amounts on the third die lip 131 without leaking out later. According to the present invention, leakage is reduced even when the coating gap is insufficient or when the amount of slurry supplied is large compared to the running speed of the substrate 170.
[0083] The average thickness of the lower slurry layer formed by the second coating liquid 60 discharged through the second discharge port 102a and the average thickness of the upper slurry layer formed by the first coating liquid 50 discharged through the first discharge port 101a may each be 60 μm or more. Also, each may be 200 μm or less. Usually, the average particle size of the secondary battery active material is about 10 μm, but since the particle size follows a normal normal distribution, d(90) or d(max) is generally larger than 10 μm. Since such active material is included, it is difficult to form a slurry layer having a thickness of less than 40 μm. Also, if it is 60 μm or more, the active material does not overlap the coating gap that is usually maintained, and the coating can be performed smoothly. Also, if the thickness of the slurry layer is 200 μm or more, it may be advantageous in some cases, but there is a problem that it is practically difficult to make the coating amount used in an actual secondary battery exceed 200 μm.
[0084] For example, the method for coating an electrode active material slurry using the dual slot die coater 100 of the present invention is applied to the manufacture of a positive electrode of a secondary battery. The positive electrode has a structure in which a lower active material layer made of a lower slurry layer and an upper active material layer made of an upper slurry layer are sequentially laminated on a current collector. The lower active material layer contains a high content of conductive material, and the upper active material layer contains a relatively low content of conductive material. In this case, the content of the conductive material in the lower active material layer can be adjusted to a range of 0.5 to 5% by weight. In the upper active material layer, the content of the conductive material can be reduced to increase the active material content on the electrode surface and reduce the conductivity (electrical conductivity) to a certain level. In particular, if the content of the conductive material in the upper active material layer is controlled to a very low level of 0.02% by weight or less, the exothermic reaction during a short circuit inside the cell can be reduced.
[0085] In another example, the average particle size P1 of the active material forming the lower active material layer is in the range of 50 to 95% of the average particle size P2 of the active material forming the upper active material layer. In this case, an active material with a relatively small particle size is applied to the lower active material layer. By applying an active material with a relatively large particle size to the upper active material layer, it is possible to facilitate impregnation with the electrolyte and induce smooth movement of ions and holes.
[0086] Here, the flow rate ratio of the first coating liquid 50 and the second coating liquid 60 may be 1:1. The viscosity of the first coating liquid 50 and the second coating liquid 60 may be 1000 cps or more. Since the dual slot die coater 100 of the present invention must be capable of coating a coating liquid having a viscosity of 1000 cps or more, the structure of the dual slot die coater 100 of the present invention is different from that of a device for applying a coating liquid having a lower viscosity than the above, for example, a photosensitive emulsion liquid, a magnetic liquid, a liquid that provides anti-reflection or anti-glare properties, a liquid that provides a widening effect of the viewing angle, a pigment liquid for a color filter, and other general resin liquids, and is not an apparatus that can be conceived by modifying the structure. The first coating liquid 50 and the second coating liquid 60 may contain graphite, a conductive material, CMC, and a binder.
[0087] Under the above coating conditions, most preferably, the ratio of the third die lip thickness D3: the second die lip thickness D2: the first die lip thickness D1 is 3:1:1. When an active material layer having a two-layer structure is formed on a current collector, such a dual slot die coater 100 can improve process efficiency and reduce the defective rate.
[0088] Fig. 5 is a perspective view of a dual slot die coater according to another embodiment of the present invention, Fig. 6 is a cross-sectional view taken along line VI-VI' in Fig. 5, and Fig. 7 is a cross-sectional view taken along line VII-VII' in Fig. 5.
[0089] 5 to 7 differs from the dual slot die coater 100 described with reference to Figures 2 to 4 only in that the lower surface of the second die block 120' and the lower surface of the third die block 130' are in intermittent surface contact with the base 90. In the dual slot die coater 200, the same parts as those in the dual slot die coater 100 are denoted by the same reference symbols, and duplicated explanations will be omitted.
[0090] The second die block 120 and the third die block 130 in the above-mentioned dual slot die coater 100 are extended in the vertical direction so as to be in surface contact with the base 90. The surface contact area is increased by making surface contact with the base 90, and thus the support force is increased. Compared to such a dual slot die coater 100, the dual slot die coater 200 of the present embodiment is configured so that the lower surfaces of the second die block 120' and the third die block 130' are partially reinforced. That is, reinforcing parts RR are intermittently added to the lower part of each die block so that the second die block 120' and the third die block 130' are in intermittent surface contact with the base 90. The lower surfaces of the second die block 120' and the third die block 130' may be provided with a plurality of reinforcing parts RR in the longitudinal direction. In the second die block 120', an empty space may be formed between the reinforcing parts RR. In the third die block 130', an empty space may also be formed between the reinforcing parts RR. With this configuration, the surface contact area with the base 90 is reduced compared to the dual slot die coater 100, but the free space can provide a stress relief effect.
[0091] The reinforcing portion RR of the second die block 120' is not separated from the second die block 120', and the reinforcing portion RR of the third die block 130' is not separated from the third die block 130'. The second die block 120' including the reinforcing portion RR and the third die block 130' including the reinforcing portion RR are each a monolithic part. That is, they are integral parts without joints. In this way, the structure is strong and very safe against external shocks during handling and use. If the reinforcing portion RR is not included in each die block and is formed of two or more separate parts, the alignment of each part must be considered when mounting, and the total tolerance between each part after assembly becomes large.
[0092] On the other hand, the empty space between the reinforcing portions RR and RR in the second die block 120' and the empty space between the reinforcing portions RR and RR in the third die block 130' may be used as the bending space. For this purpose, a pressing unit 190 may be connected to the lower end of the base 90. The pressing unit 190 may preferably be a servo motor. The pressing unit 190 may preferably be disposed in the center of the base 90. If necessary, the pressing unit 190 may be disposed closer to the second die block 120' or closer to the third die block 130'. The closer to the pressing unit 190, the greater the force applied, and the greater the bending effect. The pressing unit 190 may push the second die block 120' and the third die block 130' in the discharge direction, or pull the second die block 120' and the third die block 130' in the direction opposite to the discharge direction.
[0093] A plurality of reinforcing parts RR may be provided in the longitudinal direction of the dual slot die coater 200. According to such a configuration, it is possible to provide bending spaces separated at a plurality of positions in the longitudinal direction of the dual slot die coater 200, so that uniform bending can be realized.
[0094] Preferably, the multiple reinforcing parts RR may be provided symmetrically in the longitudinal direction with respect to the center in the longitudinal direction of the dual slot die coater 200. According to such a configuration, since both sides are uniformly bent with respect to the center in the longitudinal direction of the dual slot die coater 200, no deviation in left and right alignment occurs, and a uniform fastening force can be applied to the left and right by fastening at the contact surfaces.
[0095] Preferably, the interval between the reinforcing parts RR in the central part among the multiple reinforcing parts RR may be made larger than the interval between the other reinforcing parts RR. With this configuration, bending in the central part can be further increased, and coating gap control in the central part can be performed more reliably.
[0096] In the dual slot die coater 200, the coating liquid is injected toward the center of the die blocks 110, 120', and 130', so that the amount of liquid applied at the center is greater than that at the side portions, which may result in an uneven coating profile in the width direction (perpendicular to the MD direction) of the substrate 170. In other words, the loading of the coating liquid may be concentrated at the center of the width direction of the first slot 101 and the second slot 102. In this case, the second die block 120' and the third die block 130' are pushed and pulled by the pressing unit 190 to deform the second die lip 121 and the third die lip 131, thereby adjusting the coating gap and thereby adjusting the variation in loading. When each of the die blocks 120' and 130' is pushed toward the discharge direction by the pressing unit 190, the coating gap at the center can be reduced. Conversely, if each of the die blocks 120' and 130' is pulled in the direction opposite to the discharge direction by the pressing portion 190, the coating gap in the center can be increased.
[0097] According to the present invention, while allowing deformation of each die block 120', 130' through the bending space defined as the space between the reinforcing portions RR, the second die block 120' and the third die block 130' maintain a contact state with the base portion 90, so that deformation can be achieved with high uniformity even when using the pressing portion 190 to control the uniformity of the coating in the width direction.
[0098] In this way, the dual slot die coater 200 has a single-contact fastening system, which is the minimum condition for assembly and alignment, and has a structure that does not require an adjustment function. Furthermore, the die structure has a space secured for bending. In this way, according to the present invention, even though it has a single-contact fastening system, a space for bending is secured. Bending deforms the parts that need to be aligned, but according to the present invention, the deformation of each plate of the second die block 120' and the third die block 130' can be controlled very uniformly.
[0099] Therefore, according to the present invention, excellent coating uniformity can be easily achieved, and as a result, according to the present invention, the quality / yield / operating rate of the electrode can be improved.
[0100] Fig. 8 is a flow chart of the assembly steps of a dual slot die coater according to yet another embodiment of the present invention. Figs. 9 to 12 are diagrams showing the assembly steps of a dual slot die coater according to yet another embodiment of the present invention. The assembly steps in Figs. 9 to 12 are based on the flow chart shown in Fig. 8. Figs. 13 to 15 are diagrams for aiding in understanding the structure of the die block.
[0101] In the dual slot die coater 300 of Figures 9 to 12, the same parts as those of the dual slot die coaters 100 and 200 described above are given the same reference numerals, and duplicated explanations will be omitted.
[0102] First, the first die block 110 integrated with the base 90 is prepared, and a first shim 113' is attached onto the first die block as shown in step S1 of Fig. 8 and Fig. 9. Fig. 13 is a front view of the first die block 110 as viewed from the Y-axis direction. The first shim 113' is disposed on the first manifold 112.
[0103] 9, the first shim 113' may have a generally U-shape to define the first discharge port 101a, and in particular, one area is intermittently cut to have a plurality of openings (arrow positions). The first shim 113' included in the dual slot die coater 300 of this embodiment has two openings, and therefore, a coating layer may be formed on the substrate 170 in the shape of two parallel stripe patterns.
[0104] Bolts (not shown) may be used to assemble the first shim 113' and the first die block 110. As shown in Figs. 9 and 13, the first shim 113' and the first die block may be formed with bolt holes H1 for fastening such bolts. A bolt is fastened to each bolt hole H1, and the total number of bolts may be, for example, 13. These bolts are fixed and do not require adjustment, and are not dependent on the skill of the operator. The bolts can be selected according to mechanical properties stipulated according to the required strength (tensile strength). The strength varies depending on the material; for example, for SUS304 material, it is 700N / mm 2 The material may be selected based on the characteristics, taking into consideration corrosion resistance and the like.
[0105] The bolt may be of an appropriate standard depending on the bolt tension required for the fastening position. The bolt tension is a value obtained by multiplying the tensile strength of the bolt by the effective cross-sectional area of the bolt, and the effective cross-sectional area of the bolt varies depending on the shape of the thread (the inner diameter of the thread, which is the diameter at the root portion formed between the threads, the outer diameter of the thread, which is the diameter at the thread portion, and the effective diameter corresponding to the value between the inner diameter of the thread and the outer diameter of the thread are all taken into consideration, and can be calculated by a person having ordinary skill in the technical field to which the present invention pertains). In the embodiment of the present invention, the bolt for assembling the first shim 113' and the first die block 110 may be of a standard of, for example, M5 to M16.
[0106] Meanwhile, FIG. 9 is a diagram showing an example including an offset block installation section 114 for installing a first shim offset block (not shown). The offset block installation section 114 may be installed at a plurality of locations. The first shim offset block is configured to adjust the offset, which is the distance between the die lip and the end of the first shim 113', by pulling the first shim 113' to the opposite side of the die lip. By adjusting the offset, the coating width can be changed. Reducing the offset shortens the length of the land portion through which the coating liquid moves, and thus reduces the coating width.
[0107] Next, as shown in step S2 of Fig. 8 and Fig. 10, the second die block 120' is assembled onto the first shim 113'. Fig. 14 is a front view of the second die block 120' as viewed from the Y-axis direction.
[0108] The second die block 120' can be assembled to the first die block 110. Bolts (not shown) may be used to assemble the second die block 120' to the first die block 110. As shown in FIGS. 10 and 14, the second die block 120' may have bolt holes H2 for such bolt fastening. A bolt is fastened to each bolt hole H2, and the total number of bolts may be, for example, 22. The bolts here are also fixed type that do not require adjustment.
[0109] 10 and 14, as described above, the second die block 120' is formed with the reinforcing parts RR such that the lower surface thereof is in intermittent surface contact with the base 90, and a bending space is formed between the reinforcing parts RR. A plurality of reinforcing parts RR are provided in the longitudinal direction of the dual slot die coater 300. The reinforcing parts RR may be arranged symmetrically in the longitudinal direction with respect to the center in the longitudinal direction. The interval L1 between the reinforcing parts RR in the central part among the plurality of reinforcing parts RR may be configured to be larger than the interval L2 between the other reinforcing parts RR. With this configuration, the bending in the central part can be further increased, and the coating gap control in the central part can be more reliably performed.
[0110] The second die block 120' may be fastened with a bolt (not shown) perpendicular to the contact surface with the base 90. Since the contact surface is formed at the reinforcing portion RR, the bolt may be fastened to the reinforcing portion RR. As shown in Fig. 9, the base corresponding to the reinforcing portion RR may have a bolt hole HR for such bolt fastening.
[0111] Next, as shown in step S3 of FIG. 8 and in FIG. 11, a second shim 133' is assembled onto the second die block 120'.
[0112] The second shim 133' may have a generally U-shape to define the second discharge port 102a, and in particular, one region is intermittently cut to have a plurality of openings (arrow positions). The second shim 133' included in the dual slot die coater 300 of this embodiment has two openings, and therefore, a coating layer may be formed in the shape of two parallel patterns. The openings of the first shim 113' and the openings of the second shim 133' are aligned with each other. This allows the upper slurry layer to be aligned and formed on the lower slurry layer.
[0113] Bolts (not shown) may also be used to assemble the second shim 133' and the second die block 120'. As shown in FIG. 11, the second shim 133' may have bolt holes H3 for fastening such bolts. A bolt is fastened in each bolt hole H3, and the total number of bolts may be, for example, 13. These bolts are also fixed bolts that do not require adjustment.
[0114] A second shim offset block (not shown) may also be provided. Such a second shim offset block may be provided between the reinforcement portions RR of the second die block 120'. The second offset block is configured to adjust the offset, which is the distance between the die lip and the end of the second shim 133', by pulling the second shim 133' against the die lip.
[0115] 8 and 12, the third die block 130' is attached onto the second shim 133' to complete the assembly of the dual slot die coater 300. Fig. 15 is a front view of the third die block 130' as viewed from the Y-axis direction.
[0116] The third die block 130' can be assembled to the second die block 120'. Bolts (not shown) may be used to assemble the third die block 130' to the second die block 120'. As shown in FIG. 12 and FIG. 15, the third die block 130' may have bolt holes H4 for such bolt fastening. A bolt is fastened to each bolt hole H4, and the total number of bolts may be, for example, 22. Such bolts are also of a fixed type that do not require adjustment. All of the bolts used in the dual slot die coater 300 of the present invention are of a fixed type that do not require adjustment.
[0117] As described above, the third die block 130' also has reinforcing parts RR formed such that the lower surface thereof intermittently comes into surface contact with the base 90. Here, a plurality of reinforcing parts RR are also provided in the longitudinal direction of the dual slot die coater 300. The reinforcing parts RR may be arranged symmetrically in the longitudinal direction with respect to the center in the longitudinal direction. The interval L1 between the reinforcing parts RR in the central part among the plurality of reinforcing parts RR may be configured to be larger than the interval L2 between the other reinforcing parts RR. With this configuration, bending in the central part can be further increased, and coating gap control in the central part can be performed more reliably.
[0118] The third die block 130' may be fastened with a bolt (not shown) perpendicular to the contact surface with the base 90. Since the contact surface is formed at the reinforcing portion RR, the bolt may be fastened to the reinforcing portion RR. As shown in Figs. 9 to 11, the base corresponding to the reinforcing portion RR may have a bolt hole HR' for such bolt fastening.
[0119] Next, the assembly state is confirmed in step S5 of FIG. 8. If an assembly defect is confirmed (NO in FIG. 8), the process returns to the initial state in order to correct the assembly defect item (S6 in FIG. 8). However, in the dual slot die coater 300 of the present invention, all bolts are fixed, and the die lips 111, 121, and 131 are automatically aligned by simply assembling the first die block 110, the second die block 120', and the third die block 130'. This means that no assembly defect occurs during assembly (YES in FIG. 8), and the final assembly can be completed in a single assembly run (step S7 in FIG. 8).
[0120] The dual slot die coater 300 of the present invention has an advantage that it can be assembled by a simple manual because it uses a single contact surface fixing method, and does not require any adjustment by the operator. At the same time, a space for bending is secured between the reinforcing parts RR.
[0121] According to the dual slot die coater 100, 200, 300 of the present invention having such a configuration, the rotatable coating roll 160 is disposed above the dual slot die coater 100, 200, 300, and the coating roll 160 is rotated, for example, in a clockwise direction to run the substrate 170 to be coated, while the first coating liquid 50 and the second coating liquid 60 are continuously brought into contact with the surface of the substrate 170, so that the substrate 170 can be coated with a double layer. Alternatively, the first coating liquid 50 may be supplied and stopped, and the second coating liquid 60 may be supplied and stopped alternately, to intermittently coat the substrate 170 in a pattern.
[0122] As a specific example, the slot die coater 100, 200, 300 of the present invention By using the above, the positive electrode active material slurry can be coated, and the positive electrode can be applied to the manufacture of a positive electrode of a secondary battery. The positive electrode includes a current collector and a positive electrode active material layer formed on the surface of the current collector. The current collector is made of Al, Cu, or the like, and can be appropriately selected according to the polarity of the current collector electrode known in the field of secondary batteries. The positive electrode active material layer may further include one or more of a plurality of positive electrode active material particles, a conductive material, and a binder. The positive electrode may further include various additives for the purpose of complementing or improving electrochemical characteristics.
[0123] The active material is not limited to any particular component as long as it can be used as a positive electrode active material for a lithium ion secondary battery. Non-limiting examples include layered compounds such as lithium manganese composite oxides (LiMn2O4, LiMnO2, etc.), lithium cobalt oxide (LiCoO2), and lithium nickel oxide (LiNiO2), as well as compounds substituted with one or more transition metals, and compounds represented by the chemical formula Li 1+x Mn 2-xLithium manganese oxides such as LiMnO3, LiMn2O3, and LiMnO2, lithium copper oxide (Li2CuO2), vanadium oxides such as LiV3O8, LiV3O4, V2O5, and Cu2V2O7, and vanadium oxides with the chemical formula LiNi 1-x M x O2 (where M=Co, Mn, Al, Cu, Fe, Mg, B or Ga, and x=0.01 to 0.3), and LiMn 2-x M x The positive electrode may include one or a mixture of two or more of a lithium manganese composite oxide represented by Li2Mn3MO8 (wherein M=Co, Ni, Fe, Cr, Zn, or Ta, and x=0.01 to 0.1) or Li2Mn3MO8 (wherein M=Fe, Co, Ni, Cu, or Zn), LiMn2O4 in which part of the Li in the chemical formula is replaced with an alkaline earth metal ion, a disulfide compound, and Fe2(MoO4)3. In the present invention, the positive electrode may include, as a solid electrolyte material, one or more of a polymer-based solid electrolyte, an oxide-based solid electrolyte, and a sulfide-based solid electrolyte.
[0124] The conductive material may be added in an amount of 1 wt% to 20 wt% based on the total weight of the mixture containing the active material. Such a conductive material is not particularly limited as long as it does not induce chemical changes in the battery and has conductivity, and examples thereof include graphite such as natural graphite and artificial graphite, carbon black such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, and thermal black, conductive fibers such as carbon fibers and metal fibers, metal powders such as carbon fluoride, aluminum, and nickel powder, conductive whiskers such as zinc oxide and potassium titanate, conductive metal oxides such as titanium oxide, and conductive materials such as polyphenylene derivatives, or a mixture of two or more kinds.
[0125] The binder is not particularly limited as long as it is a component that aids in binding between the active material and the conductive material and the current collector, and examples thereof include polyvinylidene fluoride, polyvinyl alcohol, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene monomer (EPDM), sulfonated EPDM, styrene butadiene rubber, fluororubber, various copolymers, etc. The binder may usually be included in a range of 1 wt% to 30 wt%, or 1 wt% to 10 wt%, based on 100 wt% of the electrode layer.
[0126] The slot die coater 100, 200, 300 of the present invention can be used to coat the negative electrode active material slurry and to manufacture the negative electrode of a secondary battery. The negative electrode includes a current collector and a negative electrode active material layer formed on the surface of the current collector. The negative electrode active material layer may further include one or more of a plurality of negative electrode active material particles, a conductive material, and a binder. The negative electrode may further include various additives for the purpose of complementing or improving electrochemical properties.
[0127] The negative electrode active material may be a carbon material such as graphite, amorphous carbon, diamond-like carbon, fullerene, carbon nanotube, or carbon nanohorn, a lithium metal material, an alloy material such as silicon or tin, Nb2O5, Li5Ti4O 12 For the negative electrode, oxide-based materials such as TiO2, or a composite of these can be used. For the conductive material, binder, and current collector, refer to the contents described for the positive electrode.
[0128] Such an active material slurry containing a positive electrode active material or a negative electrode active material has a very high viscosity. For example, the viscosity may be 1000 cps or more. The viscosity of the active material slurry for use in forming an electrode of a secondary battery may be 2000 cps to 30000 cps. For example, the viscosity of the negative electrode active material slurry may be 2000 cps to 4000 cps. The viscosity of the positive electrode active material slurry may be 8000 cps to 30000 cps. Since the coating liquid with a viscosity of 1200 cps or more must be coated, the slot die coater 100, 200, 300 of the present invention has a structure different from that of a device for applying a coating liquid with a lower viscosity than this, such as a photosensitive emulsion liquid, a magnetic liquid, a liquid that provides anti-reflection or anti-string properties, a liquid that provides a viewing angle widening effect, a pigment liquid for a color filter, and other ordinary resin liquids, and is not a device that can be conceived by changing it. The slot die coaters 100, 200, and 300 of the present invention are for applying an active material slurry that may contain an active material having an average particle size of about 10 μm, and therefore have a different structure from that of an apparatus for applying other coating liquids that do not contain particles of such a particle size, and are not an apparatus that can be achieved by modifying the apparatus. The slot die coaters 100, 200, and 300 of the present invention are optimized as coaters for producing electrodes.
[0129] FIG. 16 is a cross-sectional view of a dual slot die coater according to a comparative example, and FIGS. 17 to 20 are views showing each assembly step of the dual slot die coater according to the comparative example.
[0130] 16, in the dual slot die coater 400 according to the comparative example, the vertical length of the second die block 120″ and the third die block 130″ is shorter than the vertical length of the first die block 110. In this state, when the tip of the second die block 120″ and the tip of the first die block 110 are aligned with each other, the lower surface of the second die block 120″ and the upper surface of the base are separated from each other, so that an empty space is formed between the lower surface of the second die block 120″ and the upper surface of the base. This space is a space whose upper surface is formed on the lower surface of the second die block 120″, whose upper portion is formed on the upper surface of the base 90, whose front surface is open, whose rear surface is formed on the front surface of the first die block 110, and whose left and right sides are open. That is, in the comparative example, the second die block 120″ and the third die block 130″ are not disposed in contact with the base 90.
[0131] In the comparative example, due to the characteristics of the bending die, space is required for bending, and in order to secure that space, two of the three die blocks 110, 120'', and 130'' must secure space in the alignment direction, resulting in a floating structure that adversely affects alignment.
[0132] For this reason, the comparative example further includes a die lip adjustment bolt 410 for aligning (aligning) the die block. Note that the die lip adjustment bolt 410 is a push-pull bolt, so there is concern that it may be dependent on the skill of the operator and may be deformed.
[0133] For comparison with the present invention, the assembly of a dual slot die coater 400 according to a comparative example will be described below with reference to FIGS. 17 to 20 in accordance with the flow chart of FIG.
[0134] A first die block 110 integrated with a base portion 90 is prepared, and a first shim 113'' is attached onto the first die block 110 as shown in step S1 of FIG. 8 and in FIG.
[0135] Bolts (not shown) may be used to assemble the first shim 113" and the first die block 110. As an example, the first shim 113" may be formed with bolt holes H1" for such bolt fastening. A bolt is fastened to each bolt hole H1", and the total number of bolts may be, for example, 22. However, unlike the present invention, these bolts are of an adjustable type that require adjustment.
[0136] Next, as shown in step S2 of FIG. 8 and in FIG. 18, the second die block 120'' is assembled onto the first shim 113''.
[0137] The second die block 120" can be assembled to the first die block 110. Bolts (not shown) may be used to assemble the second die block 120" to the first die block 110. The total number of bolts may be, for example, 22. However, unlike the present invention, such bolts are of an adjustable type that require adjustment. The second die block 120" does not come into surface contact with the base 90 and has a floating structure.
[0138] Next, as shown in step S3 of FIG. 8 and FIG. 19, the second shim 133″ is assembled onto the second die block 120″. Bolts (not shown) may be used to assemble the second shim 133″ and the second die block 120″. As an example, the second shim 125″ may have a bolt hole H3″ formed therein for fastening such a bolt. A bolt is fastened into each bolt hole H3″, and the total number of bolts may be, for example, 19. Such bolts are also of an adjustable type that require adjustment, unlike the present invention. Also, unlike the present invention, a die lip adjustment bolt 410 is required.
[0139] Next, as shown in step S4 of FIG. 8 and in FIG. 20, the third die block 130'' is assembled onto the second shim 133''.
[0140] The third die block 130" can be assembled to the second die block 120". Bolts (not shown) may be used to assemble the third die block 130" to the second die block 120". As an example, the third die block 130" may be formed with bolt holes H4" for such bolt fastening. The total number of bolts may be, for example, 20. Such bolts are also of an adjustable type that requires adjustment, unlike the present invention. The third die block 130" also has a floating structure without surface contact with the base 90.
[0141] Next, the assembly state is confirmed in step S5 of Fig. 8. If an assembly defect is confirmed, the process returns to the initial state in order to correct the assembly defect item, as shown in step S6 of Fig. 8.
[0142] In the case of the dual slot die coater 400 of the comparative example, when assembling according to the flow chart shown in Fig. 8, an average of 1 to 2 assembly defects occurred. Correcting each assembly defect takes 120 minutes. This shows that the assembly time is longer than that of the dual slot die coater 300 of the present invention, which can be completed with only one assembly.
[0143] FIG. 21 shows the effect of shortening the mold replacement time due to the die block structure / simplified assembly design in yet another embodiment of the present invention, compared to the comparative example.
[0144] In the die block assembly process according to the flowchart of FIG. 8, as described above with reference to FIGS. 17 to 20, the number of fastening bolts when assembling the first shim 113″ in the comparative example was 22, the number of fastening bolts when assembling the second die block 120″ was 22, the number of fastening bolts when assembling the second shim 133″ was 19, and the number of fastening bolts when assembling the third die block 130″ was 20. As a result, the total number of bolts was 83, and six wrench changes were required. All of the bolts were adjustable, as described above. When one assembly failure occurred and the conditions were readjusted, the die assembly time took 120 minutes. The die replacement time was 12 hours.
[0145] Meanwhile, in the die assembly process according to FIG. 8, as described with reference to FIG. 9 to FIG. 12, the first shim 113' of the dual slot die coater 300 according to another embodiment of the present invention has 13 fastening bolts when assembling, 22 fastening bolts when assembling the second die block 120', 13 fastening bolts when assembling the second shim 133', and 22 fastening bolts when assembling the third die block 130'. As a result, the total number of bolts is 70, and four wrench changes are required. Compared to the comparative example, the number of bolts and the number of wrench changes can be reduced. In the embodiment of the present invention, all the bolts are fixed. Therefore, compared to the comparative example, there is an advantage that there is no time loss in the adjustment itself, it does not depend on the skill of the fastening worker, and reproducibility is not reduced.
[0146] In the embodiment of the present invention, since no assembly failure occurs, it took 30 minutes to assemble the die. The time required to replace the mold is 8 hours. Thus, compared to the comparative example, the embodiment of the present invention has the effect of reducing the die block assembly time by 75% and reducing the time required to replace the mold by 25%.
[0147] FIG. 22 shows the effect of improving electrode quality due to improved assembly quality in yet another embodiment of the present invention compared to the comparative example.
[0148] It was found that the dual slot die coater 300 according to yet another embodiment of the present invention had excellent die lip alignment, but the comparative example had a poor level of alignment. As a result, the comparative example had problems such as poor loading variation and uneven coating width. However, when the die assembly quality was improved according to the embodiment of the present invention, the loading variation was good and the electrode quality was improved by approaching the design value.
[0149] FIG. 23 is a schematic diagram for analyzing the influence of the operation of the servo motor after the bolt is tightened in the comparative example and still another embodiment of the present invention.
[0150] In the dual slot die coater 400 according to the comparative example and the dual slot die coater 300 according to the present invention, a servo motor serving as the pressing unit 190 was connected to the lower end of the base 90 for evaluation.
[0151] In the dual slot die coater 400 of the comparative example, the second die block 120" and the third die block 130" have a floating structure, so die bending may occur due to the servo motor. In the dual slot die coater 300 of the embodiment of the present invention, the space between the reinforcing portions RR of the second die block 120' and the third die block 130' becomes a bending space, so die bending may occur due to the servo motor. The operating load of the servo motor is 4.5 kN in the comparative example and 6 kN (when moving 40 μm) in the embodiment.
[0152] FIG. 24 is a graph comparing deformation (μm) in the coating gap direction due to operation of a servo motor in a comparative example and yet another embodiment of the present invention.
[0153] In both the embodiment and the comparative example, the servo motor movement amount is reflected as it is. After the bolt tightening is completed, the deformation from the longitudinal center portion toward the coating gap direction is a negative value, and as the operating length of the servo motor becomes longer, the deformation toward the coating gap direction increases to a positive value. When the deformation deviation of each die block after the bolt tightening is completed is small, it is determined that the gap deviation correction by the servo motor is easy.
[0154] In the comparative example, the deformation caused by the servo motor is greater in the third die block 130" than in the first die block and the second die block 120". This is because the third die block 130" is not in surface contact with the base 90 and is floating.
[0155] However, in the embodiment of the present invention, the deformation caused by the servo motor is almost the same for all die blocks 110, 120', 130'. That is, it can be seen that the deformation of each of the first to third die blocks during die bending is more uniform and superior in the embodiment of the present invention compared to the comparative example due to the widthwise loading control. This is because the bending space allows deformation of each die block 110, 120', 130', while the second die block 120' and the third die block 130' are maintained in face contact with the base 90, so that deformation can be performed with high uniformity.
[0156] Meanwhile, in the present embodiment, examples have been described in which the coating liquid is applied in two layers, and in which the coating liquid is alternately supplied to perform pattern coating. However, it should be understood without further explanation that the present invention is also applicable to a case in which three or more slots are provided and three or more layers are applied simultaneously.
[0157] Although the present invention has been described above using limited embodiments and drawings, the present invention is not limited thereto, and it goes without saying that various modifications and variations can be made by a person having ordinary knowledge in the technical field to which the present invention pertains within the equivalent scope of the technical concept of the present invention and the scope of the claims.
[0158] Meanwhile, although terms indicating directions such as front, back, up, down, left, and right are used in this specification, it will be clear to those skilled in the art that these terms are used merely for convenience of explanation and may vary depending on the position of the target object, the position of the observer, etc. [Explanation of symbols]
[0159] 50 First coating liquid 60 Second coating liquid 90 base 100, 200, 300 Dual Slot Die Coater 101 1st Slot 101a 1st discharge port 102 2nd Slot 102a 2nd outlet 110 First Die Block 111 First die lip 112 First manifold 113, 113' 1st shim 120, 120' 2nd die block 121 Second die lip 130, 130' 3rd die block 131 3rd die lip 132 Second manifold 133, 133' 2nd shim 141, 142 volts 160 Coating roll 170 Base material 190 Pressing part RR reinforcement
Claims
1. A dual slot die coater having a first slot and a second slot for discharging a coating liquid in a direction opposite to gravity, a first die block vertically disposed integrally with the base at a rear portion of an upper surface of the base; a second die block disposed on a front surface of the first die block in contact with the base and defining the first slot between the first die block and the second die block; a third die block disposed on a front surface of the second die block in contact with the base and defining the second slot between the third die block and the second die block; a lower surface of the second die block and a lower surface of the third die block are in overall surface contact with the base.
2. A dual slot die coater having a first slot and a second slot for discharging a coating liquid in a direction opposite to gravity, a first die block vertically disposed integrally with the base at a rear portion of an upper surface of the base; a second die block disposed on a front surface of the first die block in contact with the base and defining the first slot between the first die block and the second die block; a third die block disposed on a front surface of the second die block in contact with the base and defining the second slot between the third die block and the second die block; A dual slot die coater, wherein a lower surface of the second die block and a lower surface of the third die block are in intermittent surface contact with the base.
3. The dual slot die coater of claim 2 , wherein a pressing portion is connected to a lower end of the base.
4. The dual slot die coater according to claim 3 , wherein the pressing unit is a servo motor.
5. A dual slot die coater having a first slot and a second slot for discharging a coating liquid in a direction opposite to gravity, a first die block vertically disposed integrally with the base at a rear portion of an upper surface of the base; a second die block disposed on a front surface of the first die block in contact with the base and defining the first slot between the first die block and the second die block; a third die block disposed on a front surface of the second die block in contact with the base and defining the second slot between the third die block and the second die block; a first shim disposed between the first die block and the second die block to form the first slot, and a second shim disposed between the second die block and the third die block to form the second slot, wherein the first shim and the second shim have an opening in at least one region.
6. The dual slot die coater according to claim 5 , wherein a lower surface of the second die block is formed with reinforcing portions so as to be in intermittent surface contact with the base portion, and a bending space is formed between the reinforcing portions.
7. The dual slot die coater according to claim 5 or 6, wherein a lower surface of the third die block is formed with reinforcing portions so as to be in intermittent surface contact with the base portion, and a bending space is formed between the reinforcing portions.
8. The dual slot die coater according to claim 7 , wherein a servo motor for deforming the bending space is connected to a center of a lower end of the base.
9. The dual slot die coater according to claim 7 , wherein a plurality of the reinforcing parts are provided in the longitudinal direction of the dual slot die coater.
10. The dual slot die coater according to claim 9 , wherein the plurality of reinforcing parts are arranged symmetrically in the longitudinal direction with respect to a center of the dual slot die coater in the longitudinal direction.
11. The dual slot die coater according to claim 10 , wherein the spacing between the reinforcing parts located in the center of the plurality of reinforcing parts is configured to be larger than the spacing between the other reinforcing parts.
12. 2. The dual slot die coater of claim 1, wherein the first die block includes a first manifold containing a first coating fluid and in communication with the first slot, and the third die block includes a second manifold containing a second coating fluid and in communication with the second slot.
13. A dual slot die coater having a first slot and a second slot for discharging a coating liquid in a direction opposite to gravity, a first die block vertically disposed integrally with the base at a rear portion of an upper surface of the base; a second die block disposed on a front surface of the first die block in contact with the base and defining the first slot between the first die block and the second die block; a third die block disposed on a front surface of the second die block in contact with the base and defining the second slot between the third die block and the second die block; a bolt is fastened perpendicular to a contact surface between the base and the second die block, and a bolt is fastened perpendicular to a contact surface between the base and the third die block.
14. The dual slot die coater of claim 1 , wherein the first slot is disposed perpendicular to the base.
15. A dual slot die coater having a first slot and a second slot for discharging a coating liquid in a direction opposite to gravity, a first die block vertically disposed integrally with the base at a rear portion of an upper surface of the base; a second die block disposed on a front surface of the first die block in contact with the base and defining the first slot between the first die block and the second die block; a third die block disposed on a front surface of the second die block in contact with the base and defining the second slot between the third die block and the second die block; A dual slot die coater, wherein a cross section of the second die block is a right-angled triangle.
16. A dual slot die coater having a first slot and a second slot for discharging a coating liquid in a direction opposite to gravity, a first die block vertically disposed integrally with the base at a rear portion of an upper surface of the base; a second die block disposed on a front surface of the first die block in contact with the base and defining the first slot between the first die block and the second die block; a third die block disposed on a front surface of the second die block in contact with the base and defining the second slot between the third die block and the second die block; a first die block having a first die lip, a second die lip, and a third die lip, each of the first die block, the second die block, and the third die block having a first die lip, a second die lip, and a third die lip, each of the first die lip, the second die lip, and the third die lip, each of the first die lip, the second die lip, and the third die lip are positioned on a same straight line.
17. 17. The dual slot die coater of claim 16, wherein a thickness of the third die lip is greater than a thickness of the first die lip and a thickness of the second die lip.
18. 18. The dual slot die coater according to claim 17, wherein a second outlet communicating with the second slot is formed between the third die lip and the second die lip, and a first outlet communicating with the first slot is formed between the second die lip and the first die lip, the second outlet outlet outlet discharging a second coating liquid onto a substrate, and the first outlet outlet is spaced apart from the second outlet downstream in a coating direction and outlets a first coating liquid onto the substrate.
Citation Information
Patent Citations
Painting method
JP1981095363A
Coating method and apparatus
JP2003260400A
Coating metal fitting and coating method
JP2003320292A
Coating device
JP2019107606A
Coating device for magnetic recording media
WO1997024714A1