Film for film capacitors

A three-layer film capacitor structure with an oxidation-inhibiting layer formed during aluminum deposition simplifies the manufacturing process and enhances product quality by preventing aluminum oxidation.

JP7566275B2Active Publication Date: 2024-10-15MASCH TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2020132746
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-08-05
Publication Date
2024-10-15
Estimated Expiration
2040-08-05

AI Technical Summary

Technical Problem

Existing film capacitor manufacturing processes require multiple steps and additional coatings to prevent aluminum oxidation, which complicates the process and can affect product quality, especially when using general-purpose vacuum evaporation apparatus.

Method used

A film capacitor with a three-layer structure comprising a polymer film, an aluminum thin film, and an oxidation-inhibiting layer formed using patterning oil during aluminum deposition, allowing for a simpler manufacturing process.

Benefits of technology

This approach enables the production of high-quality film capacitors with fewer steps and effective oxidation prevention using a general-purpose vacuum vapor deposition apparatus.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566275000001
    Figure 0007566275000001
  • Figure 0007566275000002
    Figure 0007566275000002
  • Figure 0007566275000003
    Figure 0007566275000003
Patent Text Reader

Abstract

To provide a method for manufacturing a high-quality aluminum deposited film for a film capacitor which can be achieved in a small number of steps.SOLUTION: A film for a film capacitor having three layers of a film 11, an aluminum thin film layer 12 and an oxidation-inhibiting layer 14 derived from pattering oil can be achieved by: forming a pattern 16 made of fine lines with predetermined widths in which an area, surrounded by the fine lines, which should become a divided electrode 13 is connected to adjacent areas which should become divided electrodes, at places which should become fuse parts 17 which are gaps of end parts of the fine lines, by adhesion of the patterning oil, in a same vacuum chamber of a vacuum deposition device; then forming aluminum thin film layers 12 by deposition, in the areas which should become the divided electrodes, by applying aluminum steam to the areas and making the film 11 rise by evaporating the oil adhesion portion by an atmospheric temperature or radiation heat; and further forming aluminum oxidation inhibiting layers 14 so that a portion of the evaporated oil re-adheres to the aluminum thin film surface layers.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a film for a film capacitor in which an oxidation prevention layer is formed on the aluminum surface layer without the need for a separate application of after-oil. [Background technology]

[0002] Conventionally, metallized films made by vapor-depositing aluminum onto OPP (biaxially oriented polypropylene) films, that is, films for film capacitors, are known. Two of these films are stacked and rolled up to produce large-capacity film capacitors. One known example is an OPP film in which aluminum is vapor-deposited over the entire surface to a thickness of about 80 Å, leaving or exposing non-vapor-deposited areas in a predetermined line-like pattern, and zinc is formed as a heavy edge only on one end of the film. The reason for providing the pattern is that even if a certain point shorts out, the island part surrounded by the pattern, including that point, is separated from the neighboring islands in terms of the circuit. The narrow aluminum layer between the patterns breaks, making it possible to gradually reduce the decrease in capacitance, resulting in a capacitor with excellent voltage resistance and a long product life.

[0003] Here, a thin aluminum layer is suitable for ease of handling during both the deposition process and the film capacitor manufacturing process, but it is also prone to oxidation, which can cause changes in capacitance and dielectric breakdown. Therefore, after the aluminum is deposited, an anti-oxidation coating is sometimes formed by further depositing another metal or applying an after-oil such as silicone oil separately.

[0004] However, film for film capacitors is made by unwinding a roll of strip-shaped film inside a vacuum chamber, winding it around a cooling roller, and then winding it up, during which time the patterning oil is transferred and metal vapor deposition is performed. If another metal deposition process or post-oil spraying were to be performed, there would be cases where it would be impossible to incorporate these processes due to the design constraints of the chamber. Also, as the number of processes increases, the control becomes more complicated, which can easily affect the product quality. In other words, there has been a latent demand for producing a high-quality film for a film capacitor with a small number of steps using a general-purpose vacuum deposition apparatus. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent Publication No. 2007-250829 [Patent Document 2] Patent Publication 2019-186391 Summary of the Invention [Problem to be solved by the invention]

[0006] The present invention has been made in view of the above, and has an object to produce a high-quality aluminum vapor-deposited film for a film capacitor with a small number of steps using a general-purpose vacuum deposition apparatus. [Means for solving the problem]

[0007] The film for film capacitors described in claim 1 is a film capacitor having three layers composed of a long, strip-shaped polymer film in one direction, an aluminum thin film layer vapor-deposited on the polymer film, and an oxidation inhibitor layer formed on the surface of the aluminum thin film, wherein the film is exposed to form a pattern of fine lines of a predetermined width, and an area surrounded by the fine lines to become a split electrode is connected to an area to become an adjacent split electrode at a location to become a fuse portion, which is the gap between the ends of the fine lines, and the oxidation inhibitor layer is a layer derived from oil that evaporates during the aluminum vapor deposition of patterning oil that has been attached to the pattern.

[0008] That is, the invention according to claim 1 forms an oxidation prevention layer simply and easily by utilizing patterning oil.

[0009] The vacuum chamber, the cylindrical cooling roller with its axis arranged horizontally, and although not specified in the claims, the long vapor deposition crucible or container having a length of about the axial length of the cooling roller, its heating means, the oil spraying or transfer roller, the deaeration section, etc. can be configured in the same manner as in general equipment (metallized film manufacturing equipment) used to manufacture films for film capacitors. Examples of polymer films include those having a width of 200 to 700 mm, a length of 150 m to 750 m, a thickness of 1.0 μm to 6.5 μm, and made of PPS, PVDF, PP, or PEN. As the patterning oil, an ester-based oil, a glycol-based oil, or a fluorine-based oil can be used. The fuse section, which is the gap between the area to become the split electrode and the end of the thin wire, is, simply put, a relationship in which a (usually) periodic shaped area is divided by the thin wire, and some of the thin wire is interrupted to connect to the adjacent area. This area becomes the split electrode, and the interrupted part is the fuse section to avoid insulation breakdown. The area is usually a continuous rectangle or diamond of the same shape. The thickness of the aluminum (Al) varies depending on the required physical properties of the film capacitor, but may be, for example, 50 Å to 100 Å. The ambient temperature or amount of radiant heat also depends on the amount of aluminum evaporated, the surface temperature of the cooling roller, the temperature of the crucible, the heating temperature of the aluminum, the distance between the aluminum evaporation position and the cooling roller surface, the diffusion angle (diffusion width), etc., but the ambient atmosphere should at least be such that the patterning oil in the pattern portion evaporates. The patterning oil may be transferred by pressing a cylindrical roller engraved with a pattern against a cooling roller with the film sandwiched therebetween, or by heating a long oil tank and spraying the oil through a slit. The amount of oil adhering to the film also depends on the manufacturing conditions, but it should be at least the amount that will be redeposited on the aluminum surface layer. As a guideline, the amount of oil is 0.05% to 10% of the volume of the aluminum thin film layer, but since both are thin and roughly the same thickness, it can also be calculated in terms of area, and the pattern fine line area may be about 0.1% to 5% of the aluminum area. As long as the film has three layers, an additional metal layer or the like may be formed on the film.

[0010] The film for film capacitors according to claim 2 has the film structure according to claim 1, wherein the width of the thin lines is 0.1 mm to 0.2 mm, and the width of the thin lines is 1.0 mm in the middle or at the intersections. 2 ~2.0mm 2 The pattern is characterized in that squares, circles, and other shapes are scattered at a predetermined density.

[0011] That is, in the invention according to claim 2, the oxidation-inhibiting layer is stably formed without causing oil shortage due to evaporation from the so-called oil pool (oil-rich portion).

[0012] The area surrounded by the pattern, i.e. the island part (split electrode part), is approximately 4 mm 2 ~200mm 2 On the other hand, from the viewpoint of capacity, the width of the thin wire is at most 0.2 mm. Therefore, in consideration of the case where there is not enough oil to be reattached, an oil reservoir is provided appropriately, but the area is 1.0 mm 2 If the area is less than 2.0 mm, the effect is small, and if the number of locations is increased, the capacity of each island tends to vary. 2 If the temperature exceeds this limit, the amount of aluminum vapor and radiant heat may be insufficient, and the oil will not evaporate completely from the oil pool. It should be noted that quadrilaterals include squares, rectangles, and rhombuses, and circles include ellipses.

[0013] The manufacturing method of a film for film capacitors described in claim 3 is characterized in that a long, unidirectional, strip-shaped polymer film is brought into contact with a cooling roller over a predetermined central angle in a vacuum chamber and fed at a predetermined speed, and within the contact area, a pattern consisting of fine lines of a predetermined width is first applied to the film to form a pattern in which an area to become a split electrode surrounded by the fine lines is connected to an area to become an adjacent split electrode at a location to become a fuse portion, which is the gap between the ends of the fine lines, and then aluminum vapor is applied to form an aluminum thin film layer by vapor deposition in the area to become the split electrode, and the oil portion is evaporated by ambient temperature or radiant heat to expose the film, and further, a part of the evaporated oil is redeposited on the aluminum thin film surface layer to form an aluminum oxidation inhibition layer, and the film has three layers: film - aluminum thin film layer - oxidation inhibition layer derived from patterning oil.

[0014] That is, the invention according to claim 3 forms an oxidation prevention layer simply and easily by utilizing patterning oil.

[0015] In the film for film capacitors according to claim 3, the width of the thin lines is 0.1 mm to 0.2 mm, and the width of the thin lines is 1.0 mm in the middle or at the intersections. 2 ~2.0mm 2 It goes without saying that the pattern may be one in which squares, circles, or other shapes are scattered at a predetermined density. Effect of the Invention

[0016] According to the present invention, a high-quality aluminum vapor-deposited film for a film capacitor can be produced with a small number of steps using a general-purpose vacuum deposition apparatus. [Brief description of the drawings]

[0017] [Figure 1] 1A is a schematic cross-sectional view and FIG. 1B is a schematic plan view of a metallized film. [Diagram 2] FIG. 2 is a schematic diagram showing an example of the configuration of a manufacturing apparatus for a metallized film. [Diagram 3] 2 is a flowchart showing a method for manufacturing a metal film of the present invention. [Figure 4] This is another example of a pattern. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. The film for a film capacitor will be referred to as a metallized film. FIG. 1 is a schematic cross-sectional view (a) and a schematic plan view (b) of the metallized film of the present invention (FIG. 1a is the AA cross section of FIG. 1b). In the figures, the ratio and scale are appropriately changed for the convenience of explanation. FIG. 2 is a schematic diagram showing an example of the configuration of a manufacturing apparatus for a metallized film. FIG. 3 is a flow chart of the manufacturing method for a metallized film of the present invention.

[0019] <Construction of metallized film> First, the structure of the metallized film manufactured by the manufacturing method of the metallized film of the present invention will be described. This metallized film is finally used as a film capacitor by stacking two sheets alternately, forming metallikon electrodes on the ends, and winding them (not shown).

[0020] Metallized film 10 is formed by vapor-depositing aluminum to a thickness of 70 Å over substantially the entire surface of a strip-shaped OPP film 11, 50 mm wide and 2.5 μm thick (hereinafter, this aluminum thin film layer will be referred to as aluminum layer 12).

[0021] However, at one end of the longitudinal direction of the strip, a heavy edge H of Zn with a width of 3 mm and a thickness of 350 Å is formed on the aluminum layer 12, and at the other end, a margin portion 15 with a width of 2.0 mm is formed as an area in which the OPP film 11 remains and no aluminum layer 12 is formed.

[0022] As shown in the figure, similar to the margin portion 15, a periodic pattern 16 in the shape of a series of crosses made of thin lines with a width of 0.15 mm is formed on the surface of the OPP film 11 as is (without a deposition layer). The aluminum layer 12 is divided by this pattern 16 to form islands 13 . Furthermore, the connecting portions (the portions with the smallest spacing between the patterns 16) connecting the islands 13 constitute the fuse portions 17, so that even if one of the islands 13 shorts out, the fuse portions 17 melt and connect the patterns, electrically isolating (insulating) the island 13. This improves the reliability and lifespan of the capacitor. In this embodiment, the spacing between the fuse portions 17 is 0.2 mm.

[0023] Furthermore, an extremely thin oxidation prevention layer 14 is formed on aluminum layer 12 of metallized film 10. This is an oil film derived from patterning oil, formed by a manufacturing method described below. The thickness of the film is difficult to measure, but since it is so thin that lines drawn with an oil pen or the like are repelled, it is thought to be on the order of angstroms (0.1 nm) or more, and at most a dozen nm.

[0024] <Metallized film manufacturing equipment and manufacturing process> Next, a description will be given of a manufacturing apparatus and manufacturing process (manufacturing method) for metallized film 10. Note that the formation of the heavy edge (Zn vapor deposition) will be omitted here, and only the manufacture of the Al vapor-deposited film on which pattern 16 is formed will be described.

[0025] In metallized film manufacturing equipment 100, OPP film 11 is set in a wound state on delivery roller 113 in vacuum chamber 101, and is taken up by take-up roller 114. Between the two rollers are cooling roller 110 (can roller), a rotating cylinder of a predetermined diameter against which the film comes into contact, and arranged around it are oil transfer unit 120 and aluminum deposition unit 130. Although not shown in the figure, a degassing device is attached to vacuum chamber 101, and the chamber is degassed to a predetermined vacuum level during deposition.

[0026] The cooling roller 110 is cylindrical with a diameter of 80 cm and a width of 53 cm, and rotates in one direction with its axis 111 horizontal. The surface of the cooling roller 110 is kept at about 5° C. to promote the condensation and solidification of the aluminum vapor.

[0027] The oil transfer unit 120 is elongated in the direction of the axis 111 and is composed of a cylindrical transfer roller 121 and an oil storage chamber 122 . The transfer roller 121 has a thin line pattern formed in a convex shape on its surface, and comes into contact with the cooling roller 110 via the film 11, and rotates in response to the rotation of the cooling roller 110. At this time, the transfer roller 121 transfers patterning oil from the oil reservoir 122 onto the surface of the film 11. The amount of oil attached depends on the manufacturing conditions, but is set so that a predetermined amount is redeposited on the aluminum layer 12 by the aluminum deposition unit 130.

[0028] The aluminum deposition unit 130 faces the cooling roller 110 immediately downstream of the oil transfer unit 120 and dissipates aluminum vapor. It is configured with a heating tank 131 long in the direction of axis 111, in which an aluminum ingot is heated and vapor is dissipated toward the cooling roller 110. Here, the amount of evaporation is set to be such that an aluminum thin film 47 cm wide and 70 Å thick is formed.

[0029] By appropriately heating the portion of film 11 exposed to the aluminum vapor, such as by the heat of the aluminum vapor or radiant heat from heating tank 131, the patterning oil in pattern 16 evaporates and film 11 is exposed again. At this time, a portion of the evaporated oil is reattached to the surface layer of aluminum layer 12. The uppermost layer thus formed is oxidation prevention layer 14. Note that, even if film 11 is exposed, it is acceptable for oil to remain to the extent of oxidation prevention layer 14.

[0030] Depending on the specification, a plasma irradiation section 140 may be provided immediately downstream of the aluminum deposition section 130 to ensure complete removal of oil from the pattern 16 and formation of the oxidation prevention layer 14.

[0031] The above is just an example, and the film structure of the present invention may adopt other forms. For example, the film may be made of heat-resistant resin, PP (polypropylene), or may be made of PPS (polyphenylene sulfide), PEN (polyethylene naphthalate), or PVDF (polyvinylidene fluoride). Furthermore, the film thickness, film width, fuse circuit pattern (patterning pattern), and pattern spacing may also be changed appropriately in accordance with required physical properties, etc.

[0032] In particular, a pattern 16 may be formed in which square or circular oil-rich portions 18 are provided in the middle of the thin lines or at the intersections of the thin lines. This allows the oxidation inhibition layer 14 to be formed uniformly during aluminum deposition (preventing oil shortages during re-deposition). Figure 4 shows another example of a pattern. Here, a pattern is shown in which oil-rich portions 18 are provided in the middle of the thin lines or at the intersections. It is not necessary to provide oil-rich portions 18 in the middle of all the thin lines or at all the intersections, and they may be scattered so as to prevent a supply shortage or oversupply. [Industrial Applicability]

[0033] A film capacitor using the metallized film of the present invention can be used for in-vehicle applications such as HEVs. [Explanation of symbols]

[0034] 10 Metallized Film 11 OPP film 12 Aluminum layer 13 islands (split electrode) 14 Oxidation suppression layer 15 Margin 16 Patterns 17 Fuse section 18 Oil Enrichment Section 100 Metallized film manufacturing equipment 101 Vacuum chamber 110 Cooling Roller 111 Axis 113 Delivery roller 114 Winding roller 120 Oil transfer section 121 Transfer roller 122 Oil Storage Chamber 130 Aluminum vapor deposition section 131 Heating tank 140 Plasma irradiation unit

Claims

1. A strip-shaped polymer film that is long in one direction; an aluminum thin film layer deposited on the polymer film; an oxidation prevention layer formed on the surface layer of the aluminum thin film; A film capacitor having three layers, a pattern consisting of thin lines of a predetermined width exposed from the film, in which an area surrounded by the thin lines and which is to become a split electrode is connected to an adjacent area which is to become a split electrode at a location which is to become a fuse portion, which is a gap between the ends of the thin lines; The film capacitor is characterized in that the oxidation prevention layer is a layer derived from oil that evaporates during aluminum deposition of patterning oil that has been attached to the pattern.

2. The width of the thin line is 0.1 mm to 0.2 mm, and the middle or intersection of the thin line is 1.0 mm. 2 ~2.0mm 2 2. The film for a film capacitor according to claim 1, characterized in that the film has a pattern in which squares, circles, or other shapes are scattered at a predetermined density.

3. A strip-shaped polymer film that is long in one direction is brought into contact with a cooling roller at a predetermined central angle in a vacuum chamber and fed at a predetermined speed. Within the contact area, First, a patterning oil is applied to form a pattern consisting of thin lines of a predetermined width, in which an area surrounded by the thin lines and to become a split electrode is connected to an adjacent area to become a split electrode at a location to become a fuse portion, which is a gap between the ends of the thin lines; Next, aluminum vapor is applied to the area that will become the split electrodes to form an aluminum thin film layer by vapor deposition, and the oil is evaporated by atmospheric temperature or radiant heat to expose the film. Furthermore, some of the evaporated oil is redeposited on the aluminum thin film surface to form an aluminum oxidation inhibition layer. A method for producing a film for a film capacitor, comprising three layers: a film, an aluminum thin film layer, and an oxidation prevention layer derived from patterning oil.

Citation Information

Patent Citations

  • Metallized film capacitor

    JP2007250829A

  • Method and device for manufacturing metallized film

    JP2008124245A

  • Metalization film and film capacitor using the same

    JP2019186391A

  • Metallized film, metallized film roll, plate roll

    WO2019035457A1