Method for manufacturing multiple device chips

The use of a thermocompression bonding sheet on wafers to stabilize groove alignment during chip division enhances productivity by minimizing meandering and allowing for efficient chip production with conventional cutting tools.

JP7566418B2Active Publication Date: 2024-10-15DISCO CORP
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
JP2020147957
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-09-03
Publication Date
2024-10-15
Estimated Expiration
2040-09-03

AI Technical Summary

Technical Problem

The meandering of grooves between device chips during the manufacturing process reduces productivity due to the need for slower machining speeds to maintain alignment with the laser beam focal point.

Method used

A method involving the use of a thermocompression bonding sheet without an adhesive layer, which is bonded to the wafer surface, followed by grinding and cutting processes to minimize groove meandering, allowing for efficient division into device chips using less expensive cutting devices.

Benefits of technology

This approach reduces groove meandering, enabling higher productivity and cost-effectiveness by using conventional cutting devices instead of expensive laser processing, while maintaining precise alignment and reducing thermal stress impacts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566418000001
    Figure 0007566418000001
  • Figure 0007566418000002
    Figure 0007566418000002
  • Figure 0007566418000003
    Figure 0007566418000003
Patent Text Reader

Abstract

To manufacture a device chip having a DAF attached to the back surface side by performing processing in a state in which the meandering of a groove between a plurality of device chips is reduced.SOLUTION: A manufacturing method for a plurality of device chips includes a groove forming step of forming a groove having a depth corresponding to the rising thickness on the surface side of a wafer, a thermocompression bonding step of crimping and attaching a thermocompression bonding sheet to the surface side of the wafer, a grinding step of dividing the wafer into a plurality of device chips by grinding the back side of the wafer, a pasting step of pasting a die attach film on the back surface of the wafer after the grinding step, and a cutting step of attaching the die attach film to the back surface of each of the plurality of device chips corresponding to the back surface of the wafer, and cutting the thermocompression bonding sheet and the die attach film between the plurality of device chips along the groove in which the thermocompression bonding sheet is attached to the front surface of each of the plurality of device chips corresponding to the front surface of the wafer.SELECTED DRAWING: Figure 8
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing multiple device chips, in which a wafer having a plurality of planned division lines set in a grid pattern on its surface and devices formed on each of the surface sides of areas partitioned by the plurality of planned division lines is divided along each of the planned division lines to manufacture multiple device chips. [Background technology]

[0002] Device chips are mounted on electronic devices such as mobile phones and personal computers. In the process of manufacturing device chips, for example, a wafer is divided along each of the division lines, on which a plurality of division lines are set in a lattice pattern on the surface and on which devices such as ICs (Integrated Circuits) and LSIs (Large Scale Integrations) are formed on the surface side of the regions partitioned by the division lines.

[0003] There are various methods for dividing a wafer, and for example, a dicing before grinding (DBG) process has been proposed (see, for example, Patent Document 1). In the dicing before grinding process, first, a cutting groove having a depth corresponding to the thickness of the device chip is formed on the front side of the wafer along each planned division line, and then the back side of the wafer is ground to thin the wafer, thereby dividing the wafer into a plurality of device chips.

[0004] Incidentally, in order to die-bond the individual device chips onto a lead frame, an adhesive film called DAF (Die Attach Film) (hereinafter sometimes abbreviated as DAF) which is made of a thermosetting resin such as epoxy resin and has a thickness of about 10 μm may be attached to the back side of the device chip.

[0005] When applying DAF attachment to the DBG process, the following procedure has been proposed: First, a groove of a specified depth is formed on the front side of the wafer along each planned division line, and then a protective tape is attached to the front side of the wafer. Then, while the front side of the wafer is held by suction, the back side of the wafer is ground to divide the wafer into multiple device chips.

[0006] Then, the DAF side of the DAF attached tape, which is made up of the DAF and dicing tape, is heated to about 70°C and attached to the back side of the divided wafer, and the protective tape is peeled off from the front side of the wafer. This protective tape peeling process is performed with the dicing tape side of the DAF attached tape being suction-held by the chuck table of the peeling device.

[0007] After the protective tape is peeled off, the stack of the wafer and the tape with the DAF is transported to the chuck table of a laser processing device, and the dicing tape side is suction-held by this chuck table. Then, with the focal point of the laser beam positioned on the DAF exposed between the device chips, the chuck table is moved in the processing feed direction to melt and cut the DAF (see, for example, Patent Document 2).

[0008] However, between the time when the protective tape is peeled off and the time when the dicing tape side is suction-held by the chuck table of the laser processing equipment, the position of the device chips may change slightly due to shrinkage distortion of the tape with DAF, and a phenomenon called kerf shift may occur in which the grooves (kerfs) between the device chips, which were previously straight, become meandering. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2000-21820 A [Patent Document 2] JP 2002-118081 A Summary of the Invention [Problem to be solved by the invention]

[0010] When the grooves between the device chips meander, the processing feed speed of the chuck table relative to the focal point of the laser beam must be made relatively slow, which reduces productivity. The present invention has been made in consideration of such problems, and has an object to manufacture device chips with a DAF attached to the back surface side by performing processing in a state in which the meandering of the grooves between the device chips is reduced. [Means for solving the problem]

[0011] According to one aspect of the present invention, there is provided a method for manufacturing a plurality of device chips, in which a wafer having a plurality of planned dividing lines set on a surface thereof and a device formed on the surface side of each of areas partitioned by the plurality of planned dividing lines is divided along each of the planned dividing lines to manufacture a plurality of device chips, the method including a groove forming step of forming grooves on the surface side of the wafer along each of the planned dividing lines, the grooves having a depth corresponding to a finished thickness of each of the device chips; a thermocompression bonding step of pressing a thermocompression bonding sheet having a base layer not provided with an adhesive layer onto the surface side of the wafer having the grooves formed thereon; a grinding step of grinding the back side of the wafer while holding the thermocompression bonding sheet side of the wafer on a chuck table of a grinding device to expose the grooves on the back side of the wafer, thereby dividing the wafer into the plurality of device chips; and The laminate having the dicing tape and the die attach film Die Attach Film side a cutting step of cutting the thermocompression sheet and the die attach film along the grooves between the device chips in a state in which the die attach film is attached to the back surface of each of the device chips corresponding to the back surface of the wafer and the thermocompression sheet is attached to the front surface of each of the device chips corresponding to the front surface of the wafer; an integration step of heating and melting the thermocompression sheet cut into the plurality of device chips after the cutting step, thereby connecting and integrating the plurality of device chips; A method for manufacturing a plurality of device chips comprising:

[0012] Preferably, the method for manufacturing a plurality of device chips comprises: ,one a first peeling step for peeling the integrated thermocompression sheet from the plurality of device chips; The process Prepare further.

[0015] Also, preferably, in the cutting step, the thermocompression sheet and the die attach film are cut along the grooves between the plurality of device chips using a cutting unit including an annular cutting blade having a cutting edge.

[0016] Preferably, the thermocompression sheet is a polyolefin-based sheet or a polyester-based sheet.

[0017] Preferably, the thermocompression sheet is a polyolefin-based sheet, and the polyolefin-based sheet is a polyethylene sheet, a polypropylene sheet or a polystyrene sheet.

[0018] In addition, preferably, the temperature of the thermo-compression-bonded sheet in the thermo-compression bonding step is 120°C or higher and 140°C or lower when the thermo-compression-bonded sheet is the polyethylene sheet, 160°C or higher and 180°C or lower when the thermo-compression-bonded sheet is the polypropylene sheet, and 220°C or higher and 240°C or lower when the thermo-compression-bonded sheet is the polystyrene sheet.

[0019] Preferably, the thermocompression sheet is a polyester-based sheet, and the polyester-based sheet is a polyethylene terephthalate sheet or a polyethylene naphthalate sheet.

[0020] In addition, preferably, the temperature of the thermo-compression sheet in the thermo-compression bonding step is 250°C or higher and 270°C or lower when the thermo-compression sheet is a polyethylene terephthalate sheet, and 160°C or higher and 180°C or lower when the thermo-compression sheet is a polyethylene naphthalate sheet. Effect of the Invention

[0021] A method for manufacturing a plurality of device chips according to one embodiment of the present invention includes a cutting step in which, with a die attach film (DAF) attached to the back surface of each device chip and a thermocompression sheet attached to the front surface of each device chip, the thermocompression sheet and the DAF are cut along grooves between the plurality of device chips.

[0022] In this way, because both sides of each device chip are sandwiched between the thermocompression sheet and the DAF, even if internal stress such as shrinkage distortion of the tape with DAF occurs, the positional relationship between the device chips is less likely to change compared to when no protective tape or thermocompression sheet is provided on the front side of the device chip. Therefore, processing can be performed with the degree of meandering of the grooves between the device chips reduced.

[0023] In addition, since the degree of meandering can be reduced, the thermocompression sheet and the DAF can be cut using a relatively inexpensive cutting device without using a relatively expensive laser processing device. Furthermore, compared to cutting the DAF with a laser processing device when the grooves between the device chips are meandering, the thermocompression sheet and the DAF can be cut by performing linear processing, which can improve productivity. [Brief description of the drawings]

[0024] [Figure 1] FIG. 2 is a flow diagram of a manufacturing method according to the first embodiment. [Diagram 2] FIG. 2 is a perspective view showing an example of a configuration of a wafer. [Diagram 3] FIG. 3(A) is a diagram showing a groove forming step, and FIG. 3(B) is a perspective view of the wafer after the groove forming step. [Figure 4] 13 is a diagram showing how a thermocompression sheet is placed on the front surface side of a wafer. FIG. [Diagram 5] FIG. [Figure 6] FIG. 6(A) is a diagram showing a grinding step, and FIG. 6(B) is a diagram showing a plurality of device chips etc. separated in the grinding step. [Figure 7] FIG. 13 is a diagram showing the frame unit after a bonding step. [Figure 8] FIG. [Figure 9] FIG. 9(A) is a diagram showing the integration step, and FIG. 9(B) is a diagram showing the first peeling step. [Figure 10] FIG. 6 is a flow diagram of a manufacturing method according to a second embodiment. [Figure 11] FIG. 11 illustrates a second peeling step. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0025] An embodiment according to one aspect of the present invention will be described with reference to the accompanying drawings. Fig. 1 is a flow diagram of a manufacturing method according to a first embodiment. Below, a method of manufacturing a plurality of device chips 21 (see Fig. 6(B) and the like) will be described basically according to this flow diagram.

[0026] First, a description will be given of the wafer 11 which is the workpiece. Fig. 2 is a perspective view showing a configuration example of the wafer 11. The wafer 11 has a substantially disk-shaped silicon substrate, and has a substantially circular front surface 11a and a back surface 11b.

[0027] A plurality of planned division lines (streets) 13 are set in a lattice pattern on the surface 11a. Devices 15 such as ICs (Integrated Circuits) and LSIs (Large Scale Integrations) are formed on the surface 11a side of each of the areas partitioned by the plurality of planned division lines 13.

[0028] The material of the substrate constituting the wafer 11 is not limited to silicon. There are also no limitations on the material, shape, structure, size, etc. of the substrate. Similarly, there are no limitations on the type, number, structure, size, etc. of the devices 15.

[0029] In this embodiment, a plurality of device chips 21 are manufactured from the wafer 11 through a so-called pre-dicing process. To this end, first, cut grooves (grooves) 11c (see FIG. 3(A)) having a depth 11d equivalent to the finished thickness 21c (see FIG. 6(B)) of each device chip 21 are formed on the front surface 11a side along each of the planned division lines 13 (groove forming step S10).

[0030] 3(A) is a diagram showing the groove forming step S10. In the groove forming step S10, a cutting device 2 is used. The cutting device 2 has a chuck table 4. The chuck table 4 has a disk-shaped frame body made of metal.

[0031] A disk-shaped recess (not shown) is formed in the upper part of the frame, and a porous plate (not shown) made of porous ceramics is fixed in the recess. The porous plate is connected to a suction source (not shown) such as an ejector through a predetermined flow path.

[0032] When the suction source is operated, negative pressure is transmitted to the upper surface of the porous plate through the flow path. The upper surface of the porous plate and the upper surface of the frame are substantially flush with each other, forming a substantially flat holding surface 4a. A θ table (not shown) for rotating the chuck table 4 is connected to the lower part of the chuck table 4.

[0033] A ball screw type processing feed mechanism (not shown) is provided below the θ table. The processing feed mechanism moves the chuck table 4 and the θ table in the processing feed direction (X-axis direction). A cutting unit 6 for cutting the wafer 11 is disposed above the chuck table 4.

[0034] The cutting unit 6 has a spindle 8 whose axis is disposed approximately parallel to the indexing feed direction (Y-axis direction). An annular cutting blade 10 is attached to one end of the spindle 8 by a receiving flange and a retaining nut.

[0035] The cutting blade 10 of this embodiment is a hubless type (washer type) and includes a cutting edge 10a having a blade thickness of about 50 μm. The cutting edge 10a has abrasive grains made of diamond or the like, and the abrasive grains are fixed with a bond material (for example, an electroformed bond formed by nickel plating).

[0036] A first rotation drive source (not shown) such as a motor is connected to the other end of the spindle 8. A part of the spindle 8 is rotatably accommodated in a spindle housing (not shown), and an elevation mechanism (not shown) that moves the cutting unit 6 in the cutting feed direction (Z-axis direction, height direction, up-down direction) is connected to the spindle housing.

[0037] A ball screw type indexing mechanism (not shown) that moves the cutting unit 6 and the lifting mechanism in the Y-axis direction is connected to the lifting mechanism. The cutting unit 6 is provided with a microscope unit (not shown) including a lens, an image sensor, etc.

[0038] The microscope unit captures images of alignment marks, key patterns, and the like (not shown) provided on the front surface 11a of the wafer 11. The images obtained by capturing images are used to align the wafer 11, for example.

[0039] In the groove forming step S10, first, the back surface 11b of the wafer 11 is suction-held by the holding surface 4a. Next, the θ table is operated based on an image obtained by the microscope unit, and the planned dividing line 13 is adjusted (aligned) to be approximately parallel to the X-axis direction.

[0040] Then, the lower end of the cutting blade 10, which is rotated at high speed, is positioned at a height corresponding to the finished thickness 21c in the Z-axis direction (i.e., at a depth 11d from the surface 11a), and is positioned on an extension of the planned division line 13 in the X-axis direction.

[0041] In this state, by moving the chuck table 4 in the X-axis direction, a cut groove 11c is formed on the front surface 11a side of one of the planned division lines 13. After the cut groove 11c is formed, the cutting unit 6 is indexed and fed by a predetermined index amount, and the cut groove 11c is formed in the same manner.

[0042] After the cutting grooves 11c are formed on all the division lines 13 along one direction, the chuck table 4 is rotated 90 degrees, and similarly, the cutting grooves 11c are formed on all the division lines 13 along the other direction. Fig. 3(B) is a perspective view of the wafer 11 after the groove forming step S10.

[0043] After the groove forming step S10, a thermocompression sheet 17 that functions as a surface protection member is attached to the front surface 11a of the wafer 11 (thermocompression bonding step S20). Fig. 4 is a diagram showing how the substantially circular thermocompression sheet 17 is disposed on the front surface 11a of the wafer 11.

[0044] Thermocompression sheet 17 is different from a protective tape (not shown) that is normally used as a surface protection member. A normal protective tape has a base layer made of resin and an adhesive layer (glue layer) that is provided on one side of the base layer and is made of a resin adhesive.

[0045] The adhesive layer can be bonded to the adherend by simply applying pressure at room temperature for a short time while the adherend and the adhesive layer are in contact with each other, without using water, solvent, heat, etc. However, the thermocompression sheet 17 of this embodiment has only a base layer without an adhesive layer.

[0046] That is, no adhesive layer is provided on one surface 17a of the thermocompression sheet 17 that is in close contact with the front surface 11a of the wafer 11. In this embodiment, the base layer constituting the thermocompression sheet 17 has approximately the same diameter as the wafer 11 and a thickness of about 50 μm to 250 μm. In addition, the base layer is transparent to visible light or is thin enough to transmit visible light.

[0047] The base layer is formed of a polyolefin-based sheet or a polyester-based sheet. Examples of the polyolefin-based sheet that can be used include a polyethylene sheet made of polyethylene (PE), a polypropylene sheet made of polypropylene (PP), and a polystyrene sheet made of polystyrene (PS).

[0048] As the polyester-based sheet, a polyethylene terephthalate sheet made of polyethylene terephthalate (PET), a polyethylene naphthalate sheet made of polyethylene naphthalate (PEN), or the like can be used.

[0049] In the thermocompression bonding step S20, a thermocompression bonding device 14 is used. The thermocompression bonding device 14 has a chuck table (not shown) that holds the back surface 11b by suction, for example. A heating element (not shown) that generates heat by any method such as resistance heating, induction heating, or dielectric heating is provided inside the chuck table.

[0050] The heating element is used to heat the thermocompression sheet 17 to a predetermined temperature and soften the thermocompression sheet 17. The predetermined temperature at which the thermocompression sheet 17 softens varies depending on the material, as described below.

[0051] Polyethylene sheet: 120℃ to 140℃ Polypropylene sheet: 160℃ to 180℃ Polystyrene sheet: 220℃ to 240℃ Polyethylene terephthalate sheet: 250℃ to 270℃ Polyethylene naphthalate sheet: 160℃ to 180℃

[0052] A cylindrical roller 16 (see FIG. 5) having a length (height) longer than the diameter of the wafer 11 is disposed above the chuck table. FIG. 5 is a diagram showing a thermocompression bonding step S20. In the thermocompression bonding step S20, the wafer 11 is heated to bring the thermocompression bonding sheet 17 to the above-mentioned predetermined temperature.

[0053] In this state, roller 16 is pressed against thermocompression sheet 17 and moved while rotating in a predetermined direction from one end of other surface 17b, through the center of other surface 17b, to the other end of other surface 17b.

[0054] In this manner, by bonding the thermocompression sheet 17 to the wafer 11, a first laminate 19 is formed in which one surface 17a of the softened thermocompression sheet 17 is in intimate contact with the front surface 11a of the wafer 11.

[0055] After the thermocompression bonding step S20, as shown in FIG. 6A, the back surface 11b side of the wafer 11 is ground using a grinding device 18 to divide the wafer 11 into a plurality of device chips 21 (grinding step S30).

[0056] 6(A) is a diagram showing the grinding step S30. The grinding device 18 has a chuck table 20 that suctions and holds the thermocompression sheet 17 side of the first laminate 19. The chuck table 20 has a disk-shaped frame made of ceramics.

[0057] A disk-shaped recess (not shown) is formed in the upper part of the frame, and a porous plate (not shown) made of porous ceramics is fixed in the recess. The porous plate is connected to a suction source (not shown) such as an ejector through a predetermined flow path.

[0058] When the suction source is operated, negative pressure is transmitted to the upper surface of the porous plate through the flow path. The upper surface of the porous plate is conical with a slight protrusion in the center. The upper surface of the porous plate and the upper surface of the frame are approximately flush with each other and form the holding surface of the chuck table 20.

[0059] When the first laminate 19 is sucked and held by this holding surface, the first laminate 19 deforms to follow the shape of the holding surface. The chuck table 20 is supported by an inclination adjustment mechanism (not shown) in a manner that allows it to rotate by a second rotation drive source (not shown) such as a motor.

[0060] The tilt adjustment mechanism tilts the rotation axis of the second rotation drive source by a predetermined angle from the Z-axis direction (height direction, up-down direction) so that a part of the holding surface is approximately parallel to the lower surface (grinding surface) of the grinding wheel 32. Above the chuck table 20, a grinding unit 22 is disposed.

[0061] A ball screw type grinding feed unit (not shown) for moving the grinding unit 22 along the Z-axis direction is connected to the grinding unit 22. The grinding unit 22 has a cylindrical spindle housing (not shown).

[0062] A part of a cylindrical spindle 24 arranged along the Z-axis direction is rotatably accommodated inside the spindle housing. A third rotation drive source (not shown) such as a motor is connected to the upper end of the spindle 24.

[0063] The lower end of the spindle 24 is exposed from the spindle housing, and the center of the upper surface of a disk-shaped mount 26 is fixed to the lower end. An annular grinding wheel 28 is attached to the lower surface side of the mount 26. The grinding wheel 28 has an annular base 30 having approximately the same diameter as the mount 26.

[0064] A plurality of grinding wheels 32 are discretely arranged on the lower surface side of the annular base 30 along the circumferential direction of the annular base 30. The grinding wheels 32 have a substantially rectangular parallelepiped shape, and are formed by fixing abrasive grains made of diamond, cBN (cubic boron nitride), or the like, with a binder such as metal, resin, or vitrified.

[0065] In the grinding step S30, first, the thermocompression sheet 17 side (i.e., the other surface 17b) of the first laminate 19 is suction-held by the holding surface of the chuck table 20. At this time, the back surface 11b side of the wafer 11 is exposed upward. Also, the rotation axis of the chuck table 20 is inclined at a predetermined angle so that a part of the back surface 11b and the grinding surface are approximately parallel to each other.

[0066] In this state, the chuck table 20 and the spindle 24 are rotated, for example, in substantially the same direction to feed the grinding unit 22 downward for grinding. The grinding wheel 32 comes into contact with the back surface 11b side of the wafer 11, whereby the wafer 11 is ground and thinned.

[0067] When the back surface 11b side is ground by a predetermined amount, the cut grooves 11c are exposed on the back surface 11b side. As a result, the wafer 11 is divided into a plurality of device chips 21 along each of the intended division lines 13. Fig. 6(B) is a diagram showing a plurality of device chips 21 etc. divided in the grinding step S30.

[0068] After the grinding step S30, the first laminate 19 is removed from the grinding device 18, and a die attach film (hereinafter, DAF 23) is attached to the back surface 21b (see Figures 7 and 8) of each device chip 21 (i.e., the back surface 11b side of the wafer 11 after the grinding step S30) (attaching step S40).

[0069] In the bonding step S40, a general bonding device (not shown) may be used. For example, first, the thermocompression sheet 17 side is suction-held by a chuck table of the bonding device (not shown), and the back surface 11b of the wafer 11 after the grinding step S30 is exposed upward.

[0070] In this state, a metal annular frame 29 is placed around the wafer 11 after the grinding step S30. Then, the DAF 23 side of a DAF-attached tape 27 having a DAF 23 and a dicing tape 25 is attached to the back surface 11b and one surface of the frame 29 (see FIG. 7).

[0071] The DAF 23 is, for example, an adhesive layer (glue layer) made of a thermosetting resin and having a thickness of about 10 μm to 20 μm. The DAF 23 in this embodiment has a diameter slightly larger than that of the wafer 11 as shown in FIG. 7, but may have approximately the same diameter as the wafer 11.

[0072] The DAF 23 is provided on the adhesive layer side of the dicing tape 25. The dicing tape 25 is composed of a base layer made of resin and an adhesive layer provided on one side of the base layer and formed of, for example, an ultraviolet-curable resin.

[0073] In one example, the thickness of the base layer is about 90 μm to 95 μm, the thickness of the adhesive layer is about 5 μm to 10 μm, and the thickness of the dicing tape 25 is about 100 μm. Fig. 7 is a diagram showing the frame unit 31 after the attachment step S40.

[0074] By the attachment process S40, a DAF 23 is attached to the back surface 21b of each device chip 21, an adhesive layer of a dicing tape 25 is attached to one surface of the frame 29, and a thermo-compression sheet 17 is attached to the front surface 21a (corresponding to the front surface 11a of the wafer 11) of each device chip 21 to form a frame unit 31.

[0075] After the bonding step S40, the thermocompression bonding sheet 17 and the DAF 23 in the state of the frame unit 31 are cut along the cut grooves 11c (cutting step S50). Fig. 8 is a diagram showing the cutting step S50.

[0076] In the cutting step S50, for example, a cutting device 42 different from the cutting device 2 used in the groove forming step S10 is used. The cutting device 42 has a chuck table 44. The configuration of the chuck table 44 is similar to that of the chuck table 4 described above.

[0077] A holding surface 44a of the chuck table 44 suction-holds the dicing tape 25 side of the frame unit 31. This causes the other surface 17b side of the thermocompression sheet 17 to be exposed upward. A cutting unit 46 is disposed above the chuck table 44.

[0078] The cutting unit 46 has a cylindrical spindle 48. The configuration of the cutting unit 46 is similar to that of the above-mentioned cutting unit 6. An annular cutting blade 50 is attached to one end of the spindle 48 by a receiving flange and a retaining nut.

[0079] The cutting blade 50 of this embodiment is of a hubless type (washer type) and has a cutting blade 50a that is thinner than the cutting blade 10a used in the groove forming step S10. The cutting blade 50a has a thickness of, for example, 30 μm.

[0080] By making the cutting blade 50a thinner than the cutting blade 10a, the wear resistance is reduced compared to the cutting blade 10a, but it becomes easier to cut the thermocompression sheet 17 and the DAF 23 without coming into contact with the device chip 21 in the cutting step S50.

[0081] However, the abrasive grains and bond material of the cutting blade 50a may be the same as or different from those of the cutting blade 10a. The abrasive grains constituting the cutting blade 50a in this embodiment are made of diamond, and the abrasive grains are fixed with an electroformed bond formed by nickel plating.

[0082] Although a description of other components of the cutting device 42 will be omitted, the cutting device 42 has the same components as those of the cutting device 2. In the cutting step S50, first, the dicing tape 25 side of the frame unit 31 is suction-held by the holding surface 44a.

[0083] Next, the cut groove 11c is adjusted to be approximately parallel to the X-axis direction based on an image of the surface 11a (surface 21a) side captured through the thermocompression sheet 17. Thereafter, the lower end of the cutting blade 50 rotated at high speed is positioned between the holding surface 44a and the upper surface of the dicing tape 25, and is arranged on the extension line of the cut groove 11c.

[0084] In this state, the chuck table 44 is moved in the processing feed direction, whereby the thermocompression sheet 17 and the DAF 23 are cut along the cutting grooves 11c. After the thermocompression sheet 17 and the DAF 23 are cut along one cutting groove 11c, the cutting unit 46 is indexed and fed by a predetermined index amount.

[0085] Then, similarly, the thermocompression bonding sheet 17 and the DAF 23 are cut along the cut grooves 11c. After the thermocompression bonding sheet 17 and the DAF 23 have been cut along all the cut grooves 11c along one direction, the chuck table 44 is rotated by 90 degrees.

[0086] As a result, the cut grooves 11c along the other directions are adjusted to be approximately parallel to the X-axis direction. Similarly, the thermocompression sheet 17 and the DAF 23 are cut along the cut grooves 11c to have shapes corresponding to the device chips 21.

[0087] In the cutting step S50 of this embodiment, both surfaces (front surface 21a and back surface 21b) of each device chip 21 are sandwiched between the thermocompression sheet 17 and the DAF 23, so that the positional relationship between the device chips 21 is unlikely to change.

[0088] Therefore, even if internal stress such as shrinkage distortion occurs in the DAF tape 27, the cut grooves 11c between the device chips 21 are less likely to meander, so processing can be performed with the degree of meandering of the cut grooves 11c reduced.

[0089] In addition, since the degree of meandering can be reduced, the thermocompression bonding sheet 17 and the DAF 23 can be cut using a relatively inexpensive cutting device 42, without using a relatively expensive laser processing device.

[0090] Furthermore, compared to cutting the DAF 23 with a laser processing device when the cutting grooves 11c between the device chips 21 are meandering, the thermocompression sheet 17 and the DAF 23 can be cut by performing linear processing, thereby improving productivity.

[0091] After the cutting step S50, the thermocompression sheet 17 divided into pieces corresponding to the device chips 21 is melted and integrated (integrating step S60) In the integrating step S60, a heating device 52 (see FIG. 9(A)) is used.

[0092] The heating device 52 has a mounting table (not shown) on which the frame unit 31 is placed. A hot air spraying unit 54 is disposed above the mounting table. The hot air spraying unit 54 has a heating element (not shown) that generates heat by any method such as resistance heating, induction heating, or dielectric heating.

[0093] The heat generated by the heating element is blown as hot air 56 from an opening (not shown) of hot air blowing unit 54 toward the mounting table by an air blowing mechanism (not shown) such as a fan. Fig. 9(A) is a diagram showing the integration step S60.

[0094] In the integration process S60, if the thermocompression sheet 17 is a polyethylene sheet, the polyethylene sheet is heated for a predetermined time of at least one minute with hot air 56 having a temperature of about 200°C near the opening so that the temperature is above the melting point of the polyethylene sheet (e.g., 160°C).

[0095] For example, in the case of a polyethylene sheet having a thickness of about 130 μm, the polyethylene sheet is heated for 1 minute or more and 2 minutes or less with hot air 56 having a temperature of about 200° C. near the opening. However, the heating temperature and heating time may be appropriately changed depending on the material of the thermocompression sheet 17.

[0096] When the thermocompression sheet 17 is a polypropylene sheet, the polypropylene sheet is heated for a predetermined time of at least one minute using hot air 56 having a temperature of 200°C or higher near the opening of the hot air spraying unit 54 so that the temperature is above the melting point of the polypropylene sheet.

[0097] When the thermocompression sheet 17 is a polystyrene sheet, the polystyrene sheet is heated for a predetermined time of at least one minute using hot air 56 having a temperature of 260°C or higher near the opening of the hot air spraying unit 54 so that the temperature is above the melting point of the polystyrene sheet.

[0098] When the thermocompression sheet 17 is a polyethylene terephthalate sheet, the polyethylene terephthalate sheet is heated for a predetermined time of at least one minute using hot air 56 having a temperature of 290°C or higher near the opening of the hot air spraying unit 54 so that the temperature is above the melting point of the polyethylene terephthalate sheet.

[0099] When the thermocompression sheet 17 is a polyethylene naphthalate sheet, the polyethylene naphthalate sheet is heated for a predetermined time of at least one minute using hot air 56 having a temperature of 200°C or higher near the opening of the hot air spraying unit 54 so that the temperature is above the melting point of the polyethylene naphthalate sheet.

[0100] By applying hot air 56 at a predetermined temperature to the thermocompression sheet 17 for a predetermined period of time, at least the other surface 17b side of the divided thermocompression sheet 17 melts, and the cut thermocompression sheets 17 are joined together and integrated (see Figure 9(B)).

[0101] The integration step S60 may be performed using a heating roller (not shown) or a flat heating plate having a built-in heating element instead of the hot air blowing unit 54. By using a heating roller or a heating plate, the area to be heated in the planar direction and thickness direction of the thermocompression sheet 17 can be easily controlled, so that the influence of heat on the DAF 23 and the dicing tape 25 can be reduced.

[0102] Since the DAF 23 is formed of, for example, a thermosetting resin, reducing the thermal effect on the DAF 23 can contribute to stabilizing the treatment process after the integration step S60. Similarly, reducing the thermal deformation of the dicing tape 25 can contribute to stabilizing the treatment process after the integration step S60.

[0103] After the integration step S60, the integrated thermocompression sheet 17 is peeled off from each device chip 21 (first peeling step S70). In the first peeling step S70, for example, a peeling unit (not shown) is used.

[0104] The peeling unit has a chuck table (not shown) that suction-holds the dicing tape 25 side of the frame unit 31. An arm portion (not shown) is disposed above the chuck table, and a gripper portion (not shown) is disposed at the tip of the arm portion.

[0105] The gripping portion grips a strip of peeling tape (not shown). After the peeling tape is attached to a part of the other surface 17b of the thermocompression sheet 17 near the end, the gripping portion is raised to roll up the thermocompression sheet 17 (see the arrow in FIG. 9(B)).

[0106] 9(B) is a diagram showing a first peeling step S70. After the thermocompression sheet 17 is peeled up, the arm part is operated to peel the thermocompression sheet 17 from each device chip 21. Note that in the first peeling step S70, it is not necessary to use a strip-shaped peeling tape.

[0107] For example, the thermocompression sheet 17 can be peeled off by, for example, pinching the outer periphery of the integrated thermocompression sheet 17 and rolling up the thermocompression sheet 17. In addition, in the first peeling step S70, the thermocompression sheet 17 may be peeled off manually by an operator.

[0108] After the first peeling step S70, the adhesive layer of the dicing tape 25 is irradiated with ultraviolet light to reduce the adhesive force. Thereafter, the front surface 21a side of the device chip 21 is sucked using a collet (not shown) or the like, and the device chip 21 with the DAF 23 attached thereto is transported.

[0109] In the above-mentioned groove forming process S10, the cutting groove 11c is formed using the cutting device 2, but a groove corresponding to the cutting groove 11c may also be formed by ablation processing the wafer 11 using a laser processing device (not shown) that irradiates a pulsed laser beam having a wavelength that is absorbed by the wafer 11.

[0110] In addition, a groove corresponding to the cut groove 11c may be formed by etching the wafer 11 with an etching gas using an etching device (not shown) such as a plasma etcher, while the surface 11a side is partially covered with a photoresist layer or a water-soluble resin layer (neither of which is shown) that is patterned so as to expose the intended division lines 13.

[0111] Next, the second embodiment will be described. Fig. 10 is a flow diagram of a method for manufacturing a plurality of device chips 21 according to the second embodiment. In the second embodiment, after the cutting step S50, the integration step S60 and the first peeling step S70 are not performed, and each cut thermocompression sheet 17 is peeled off using a peeling tape 33 (see Fig. 11) (second peeling step S80).

[0112] 11 is a diagram showing the second peeling step S80. In the second peeling step S80, a bonding / peeling unit (not shown) is used. The bonding / peeling unit includes, for example, a general tape mounter and a general tape peeling device, respectively.

[0113] In the second peeling step S80, first, a peeling tape 33 having approximately the same diameter as the wafer 11 is attached to the entire other surface 17b of the thermocompression sheet 17 cut in the cutting step S50. The peeling tape 33 is a tape having a base layer and an adhesive layer.

[0114] The type of adhesive constituting the adhesive layer of the peeling tape 33 is not particularly limited as long as the adhesive strength between the peeling tape 33 and the thermocompression sheet 17 is higher than the adhesive strength between the device chip 21 and the thermocompression sheet 17 .

[0115] After the peeling tape 33 is attached, the peeling tape 33 is peeled off using an attachment / peeling device, and the cut thermocompression sheet 17 is peeled off from each device chip 21. Note that the second peeling step S80 may be performed manually by an operator instead of using an attachment / peeling device.

[0116] The second peeling step S80 has the advantage that thermal damage to the device chip 21, the DAF 23, and the dicing tape 25 can be significantly reduced compared to the case where the integration step S60 and the first peeling step S70 are performed.

[0117] Of course, in the second embodiment, both sides of each device chip 21 are sandwiched between the thermocompression sheet 17 and the DAF 23 in the cutting step S50, so that the positional relationship between the device chips 21 is unlikely to change even if internal stress such as shrinkage distortion occurs in the DAF-attached tape 27. Therefore, processing can be performed in a state where the degree of meandering of the cut grooves 11c between the device chips 21 is reduced.

[0118] In addition, since the degree of meandering can be reduced, the thermocompression sheet 17 and the DAF 23 can be cut without using a relatively expensive laser processing device, even with a relatively inexpensive cutting device 42. Furthermore, compared to the case where the DAF 23 is cut by a laser processing device when the cutting grooves 11c between the device chips 21 are meandering, the thermocompression sheet 17 and the DAF 23 can be cut by performing linear processing, so that productivity can be improved.

[0119] In addition, the structures, methods, etc. according to the above-mentioned embodiments can be appropriately modified and implemented without departing from the scope of the present invention. In the above-mentioned thermocompression bonding step S20, the wafer 11 is heated and the thermocompression bonding sheet 17 is compressed, but the thermocompression bonding step S20 is not limited to this method.

[0120] For example, with the wafer 11 placed on the thermocompression sheet 17 with the back surface 11b facing upward, the wafer 11 can be heated and pressed onto the thermocompression sheet 17 by a roller 16 equipped with a heating element.

[0121] In this manner, by indirectly heating the thermocompression sheet 17 via the wafer 11, it is easier to soften one surface 17a of the thermocompression sheet 17 (near the interface between the thermocompression sheet 17 and the wafer 11) than the other surface 17b, and there is an advantage in that the thermocompression sheet 17 is less likely to stick to the roller 16, etc.

[0122] In addition, with the wafer 11 placed on the thermocompression sheet 17 with the back surface 11b facing upward, the thermocompression sheet 17 may be heated by heating the chuck table on the thermocompression sheet 17 side, and the wafer 11 may be pressed onto the thermocompression sheet 17 by the rollers 16.

[0123] However, in a state where the thermocompression sheet 17 is placed on the wafer 11, the thermocompression sheet 17 may be heated by a roller 16 equipped with a heating element and the thermocompression sheet 17 may be pressed against the wafer 11. In this way, the thermocompression sheet 17 may be attached to the wafer 11. [Explanation of symbols]

[0124] 2: cutting device, 4: chuck table, 4a: holding surface 6: cutting unit, 8: spindle, 10: cutting blade, 10a: cutting edge 11: wafer, 11a: front surface, 11b: back surface, 11c: cutting groove (groove), 11d: depth 13: Planned division line, 15: Device 14: Thermocompression device, 16: Roller 17: thermocompression sheet, 17a: one side, 17b: other side 18: Grinding device, 20: Chuck table 19: First laminate 21: device chip, 21a: front surface, 21b: back surface, 21c: finished thickness 22: grinding unit, 24: spindle, 26: mount 23: DAF (die attach film), 25: dicing tape 27: Tape with DAF 28: grinding wheel, 30: annular base, 32: grinding stone 29: Frame, 31: Frame unit 33: Peeling tape 42: cutting device, 44: chuck table, 44a: holding surface 46: cutting unit, 48: spindle, 50: cutting blade, 50a: cutting edge 52: heating device, 54: hot air blowing unit, 56: hot air

Claims

1. A method for manufacturing a plurality of device chips, comprising the steps of: dividing a wafer having a plurality of planned dividing lines set on a surface thereof, the wafer having devices formed on the surface side of each of areas partitioned by the plurality of planned dividing lines, along the respective planned dividing lines, thereby manufacturing a plurality of device chips, a groove forming step of forming grooves having a depth corresponding to a finished thickness of each device chip on the front surface side of the wafer along each of the planned dividing lines; a thermocompression bonding step of bonding a thermocompression sheet having a base layer without an adhesive layer to the front surface side of the wafer on which the grooves are formed; a grinding step of grinding the back side of the wafer while holding the thermocompression sheet side of the wafer on a chuck table of a grinding machine to expose the grooves on the back side of the wafer and divide the wafer into the plurality of device chips; a bonding step of bonding a die attach film side of a laminate having a dicing tape and a die attach film to the back surface of the wafer after the grinding step; a cutting step of cutting the thermocompression sheet and the die attach film along the grooves between the device chips in a state in which the die attach film is attached to the back surface of each of the device chips corresponding to the back surface of the wafer and the thermocompression sheet is attached to the front surface of each of the device chips corresponding to the front surface of the wafer; an integration step of heating and melting the thermocompression sheet cut into the plurality of device chips after the cutting step, thereby connecting and integrating the plurality of device chips; A method for manufacturing a plurality of device chips, comprising:

2. A method for manufacturing a plurality of device chips as described in claim 1, further comprising a first peeling step of peeling the integrated thermo-compression sheet from the plurality of device chips.

3. 3. The method for manufacturing a plurality of device chips as described in claim 1 or 2, characterized in that in the cutting step, a cutting unit including an annular cutting blade having a cutting edge is used to cut the thermocompression sheet and the die attach film along the grooves between the plurality of device chips.

4. 4. The method for manufacturing a plurality of device chips according to claim 1, wherein the thermocompression sheet is a polyolefin-based sheet or a polyester-based sheet.

5. The thermocompression sheet is a polyolefin-based sheet, 5. The method for manufacturing a plurality of device chips according to claim 4, wherein the polyolefin sheet is a polyethylene sheet, a polypropylene sheet or a polystyrene sheet.

6. 6. The method for manufacturing a plurality of device chips according to claim 5, characterized in that the temperature of the thermocompression sheet in the thermocompression bonding step is 120°C or higher and 140°C or lower when the thermocompression sheet is the polyethylene sheet, 160°C or higher and 180°C or lower when the thermocompression sheet is the polypropylene sheet, and 220°C or higher and 240°C or lower when the thermocompression sheet is the polystyrene sheet.

7. the thermocompression sheet is a polyester-based sheet, 5. The method for manufacturing a plurality of device chips according to claim 4, wherein the polyester sheet is a polyethylene terephthalate sheet or a polyethylene naphthalate sheet.

8. 8. The method for manufacturing a plurality of device chips according to claim 7, characterized in that the temperature of the thermocompression sheet in the thermocompression step is 250°C or higher and 270°C or lower when the thermocompression sheet is a polyethylene terephthalate sheet, and 160°C or higher and 180°C or lower when the thermocompression sheet is a polyethylene naphthalate sheet.

Citation Information

Patent Citations

  • Division work method for semiconductor wafer

    JP2000021820A

  • Method of manufacturing semiconductor device

    JP2002118081A

  • Process for manufacturing semiconductor chip, and process for manufacturing semiconductor device

    JP2005285824A

  • Method for manufacturing semiconductor apparatus

    JP2006140303A

  • Manufacturing method of semiconductor device

    JP2007036292A