Manufacturing method of blow molded products
The described blow molding process enhances liquid repellency on inner surfaces by using specific resins and ethanol mist to achieve a desired roughness, effectively reducing residual liquid in blow-molded products.
Patent Information
- Application Number
- JP2021076640
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-04-28
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-04-28
AI Technical Summary
Existing blow-molded products lack sufficient liquid repellency on their inner surfaces, leading to residual liquid accumulation.
A blow molding process involving the use of a resin with a surface tension of 25 mN/m or less, combined with ethanol mist, to create an inner surface with a centerline average roughness of 60 nm to 150 nm, achieved through extrusion blow molding with specific resin compositions and alcohol adhesion.
The process results in a blow-molded product with enhanced liquid repellency, reducing residual liquid adherence and improving sustainability by minimizing liquid retention.
Smart Images

Figure 0007566430000001 
Figure 0007566430000002 
Figure 0007566430000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a blow molded article and a method for producing the same. [Background technology]
[0002] Molded products whose surfaces have liquid repellency (water repellency) are useful in various applications. For example, if the inner surface of a container that holds liquid is made liquid repellent, the amount of liquid that remains on the inner surface of the container and cannot be used can be reduced. For example, Patent Document 1 describes an injection molded product whose surface has liquid repellency. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 6732372 Summary of the Invention [Problem to be solved by the invention]
[0004] Blow molded articles having good liquid repellency on the inner surface are desired.
[0005] SUMMARY OF THE PRESENT EMBODIMENT An object of the present invention is to provide a blow molded article having an inner surface with good liquid repellency, and a method for producing the same. [Means for solving the problem]
[0006] Blow molded article of the present invention Manufacturing method teeth, The present invention includes an extrusion blow molding process in which a gas and a mist of alcohol are supplied into a precursor having an inner surface formed of a resin having a surface tension of 25 mN / m or less, and the precursor is molded into a blow molded product having an inner surface with a center line average roughness Ra of 60 nm to 150 nm, and the center line average roughness Ra is within the range of JIS B the resin is a silicone-containing olefin resin containing 15% by weight or more and 30% by weight or less of silicone, the alcohol is ethanol, the extrusion blow molding process has a preparation step, a pressurization step, and a drying step, the preparation step is a step of placing the precursor in a bottomed cylindrical state in a closed blow molding die, the pressurization step is a step of supplying the pressurized gas and the atomized alcohol into the precursor in the cavity of the blow molding die, the atomized alcohol collides with and adheres to the inner surface, and the precursor is molded into the blow molded product having a shape that conforms to the shape of the cavity, and the drying step is a step of evaporating the alcohol adhered to the inner surface of the blow molded product. A blow molded article characterized by Manufacturing method It is.
[0008] The blow molded article of the present invention Manufacturing method In the above configuration, The blow molded product is Forming at least a portion of the container 、 Blow Molding Manufacturing method It is preferable that: Effect of the Invention
[0010] According to the present invention, it is possible to provide a blow molded article having an inner surface with good liquid repellency and a method for producing the same. [Brief description of the drawings]
[0011] [Figure 1] FIG. 2 is a conceptual diagram showing a state when a precursor is sandwiched between molds (mold clamping step) to produce a blow molded article according to one embodiment of the present invention. [Diagram 2] FIG. 2 is a conceptual diagram showing a state when the supply of gas and atomized alcohol into the precursor (pressurization step) is started from the state shown in FIG. 1. [Diagram 3] FIG. 3 is a conceptual diagram showing a state when the supply of gas and atomized alcohol (pressurization step) has progressed further from the state shown in FIG. 2. [Figure 4] FIG. 4 is a conceptual diagram showing the state when the supply of gas and atomized alcohol (pressurizing step) from the state shown in FIG. 3 is completed and the alcohol has evaporated (drying step). [Diagram 5] FIG. 13 is a diagram showing the evaluation results of liquid repellency in the examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
[0013] A blow molded product 1 according to one embodiment of the present invention (see FIG. 4) is characterized in that the center line average roughness Ra of an inner surface 1d formed from a resin having a surface tension of 25 mN / m or less is 60 nm or more and 150 nm or less.
[0014] The blow molded product 1 may form at least a part of a container. The blow molded product 1 may be a container manufactured by going through the blow molding process shown in Figs. 1 to 4. When such a container is used as a container for storing liquid, it is possible to reduce the amount of liquid that remains on the inner surface 1d of the container and cannot be used up. When food such as water, sauce, soy sauce, etc. is used as the liquid, it is possible to reduce food waste and improve environmental compatibility (sustainability).
[0015] The resin forming the inner surface 1d is not particularly limited as long as it has a surface tension of 25 mN / m or less, but is preferably, for example, a silicone-containing olefin-based resin. The silicone-containing olefin-based resin is not particularly limited, but may be, for example, a silicone-containing polypropylene, a silicone-containing polyethylene, or a combination thereof. The silicone content is not particularly limited, but may be, for example, 15% by weight or more and 30% by weight or less.
[0016] The blow molded article 1 may have a second layer adjacent to the outer side of the innermost layer as the first layer in addition to the innermost layer having the inner surface 1d. One or more layers adjacent to the outer side of the second layer may be provided. The thickness of the first layer is not particularly limited, but is, for example, 30 μm or more and 70 μm or less. The thickness of the second layer is not particularly limited, but is, for example, 650 μm or more and 700 μm or less.
[0017] The material forming the second layer is not particularly limited, but may be, for example, an olefin resin. The olefin resin forming the second layer is not particularly limited, but may be, for example, polyethylene such as low density polyethylene (LDPE), linear low density polyethylene (LLDPE), high density polyethylene (HDPE), polypropylene, or a combination thereof.
[0018] The center line average roughness Ra described above is a three-dimensional extension of the center line average roughness Ra specified in JIS B 0601 so that it can be applied to a measurement surface, and can be measured, for example, by an atomic force microscope (AFM). The inner surface 1d of the blow molded product 1, i.e., the inner surface 1d of the innermost layer, can exhibit good liquid repellency, especially against food such as sauces, by forming the inner surface 1d so that the center line average roughness Ra is 60 nm or more and 150 nm or less.
[0019] The blow molding process shown in Figs. 1 to 4 is a process for molding the precursor 2 into a blow molded product 1 having a center line average roughness Ra of 60 nm to 150 nm on the inner surface 1d by supplying gas and mist-like alcohol 3 into the precursor 2, whose inner surface is formed of a resin having a surface tension of 25 mN / m or less (hereinafter, also referred to as mist blowing process). More specifically, the mist blowing process includes a preparation process, a pressurizing process, and a drying process. This mist blowing process is performed by extrusion blow molding (EBM: Extrusion Blow Molding). Note that this mist blowing process is not limited to extrusion blow molding, and may be performed by biaxial stretch blow molding using a preform formed into a bottomed cylindrical shape as the precursor 2.
[0020] As shown in FIG. 1, the preparation step is a step of placing a bottomed tubular precursor 2 in a closed blow mold 4. The blow mold 4 has a cavity 5 (molding surface) of a shape corresponding to the outer shape of the blow molded product 1, and is provided as a split mold that can be closed and opened. In the mist blowing step, the blow molded product 1 is a bottle-shaped container having a cylindrical mouth 1a, a body 1b connected to the mouth 1a, and a bottom 1c connected to the body 1b. In the preparation step, a cylindrical precursor 2, also called a parison, having a layered structure corresponding to the layered structure of the blow molded product 1 is extruded downward from an extruder, and the bottom of the precursor 2 is cut off by closing the mold, so that a bottomed tubular precursor 2 is placed in the cavity 5 as shown in FIG. 1.
[0021] 2 and 3, the pressurizing step is a step in which pressurized gas and atomized alcohol 3 (shown by white circles in FIGS. 2 and 3) are supplied into precursor 2 in cavity 5, thereby molding precursor 2 into blow-molded article 1 having a shape that conforms to the shape of cavity 5. In the pressurizing step, an appropriate amount of alcohol 3 is atomized and supplied into precursor 2 together with gas, so that the atomized alcohol 3 collides with and adheres to inner surface 1d to obtain blow-molded article 1.
[0022] The alcohol 3 is not particularly limited, but is, for example, ethanol.
[0023] As shown in Fig. 4, the drying process is a process for evaporating the alcohol 3 adhering to the inner surface 1d of the blow molded article 1. The alcohol 3 evaporates naturally due to the heat held by the blow molded article 1 immediately after molding, but it can also be evaporated by heating. The alcohol 3 can also be evaporated before or after the mold is opened. By going through the drying process, a blow molded article 1 with a center line average roughness Ra of the inner surface 1d of 60 nm to 150 nm can be obtained.
[0024] The present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the spirit and scope of the present invention.
[0025] Therefore, the blow molded article 1 of the above-described embodiment and the manufacturing method thereof can be modified in various ways, for example as described below.
[0026] The blow molded product 1 of the above-mentioned embodiment can be modified in various ways as long as it is a blow molded product 1 characterized in that the center line average roughness Ra of the inner surface 1d formed from a resin having a surface tension of 25 mN / m or less is 60 nm or more and 150 nm or less.
[0027] For example, the blow molded article 1 is not limited to a blow molded article 1 produced by a blow molding process (mist blow process) in which gas and mist-like alcohol 3 are supplied into a precursor 2 whose inner surface is formed of a resin having a surface tension of 25 mN / m or less, and the precursor 2 is molded into a blow molded article 1 whose inner surface 1d has a center line average roughness Ra of 60 nm or more and 150 nm or less.
[0028] That is, instead of the blow molding process in which a blow molded article 1 having a roughened inner surface 1d is formed by using atomized alcohol 3 as described above, for example, a blow molding process in which fine particles are mixed into the material of precursor 2 to form a blow molded article 1 having a roughened inner surface 1d with fine particles, or a blow molding process in which precursor 2 is formed by mixing different incompatible materials to form a blow molded article 1 having a roughened inner surface 1d with a sea-island structure, may be used.
[0029] In addition, the blow molded article 1 of the above-mentioned embodiment is preferably a blow molded article 1 having the above-mentioned configuration, in which the resin is a silicone-containing olefin-based resin.
[0030] Moreover, the blow molded article 1 of the above-described embodiment is preferably a blow molded article 1 that forms at least a part of a container in the above-described configuration. EXAMPLES
[0031] Blow molded products of sample numbers 1 to 10 were manufactured and liquid repellency was evaluated. All samples were 200 ml containers with a cylindrical body, and had a two-layer structure with an innermost layer of silicone-containing polypropylene and an outer layer of polyethylene, and were manufactured by extrusion blow molding. Sample numbers 1 to 7 used Polyfine (registered trademark) (MF18R) manufactured by Prime Polymer Co., Ltd. as the silicone-containing polypropylene. Sample numbers 8 to 10 used a material with an adjusted silicone content based on polypropylene. The silicone content in the Polyfine (registered trademark) was 15% by weight, 20% by weight in sample number 8, 25% by weight in sample number 9, and 30% by weight in sample number 10. The surface tension of the Polyfine (registered trademark) was 25 mN / m.
[0032] In addition, sample number 1 was manufactured by supplying only air into the precursor in the blow molding process, sample number 2 was manufactured by supplying 1 ml of mist-like ethanol into the precursor in the blow molding process, sample number 3 was manufactured by supplying 3 ml of mist-like ethanol into the precursor in the blow molding process, sample number 4 was manufactured by supplying 5 ml of mist-like ethanol into the precursor in the blow molding process, sample number 5 was manufactured by supplying 1 ml of mist-like water into the precursor in the blow molding process, sample number 6 was manufactured by supplying 3 ml of mist-like water into the precursor in the blow molding process, sample number 7 was manufactured by supplying 5 ml of mist-like water into the precursor in the blow molding process, and sample numbers 8 to 10 were manufactured by supplying 3 ml of mist-like ethanol into the precursor in the blow molding process.
[0033] FIG. 5 shows the surface shape and center line average roughness Ra of each sample measured using an atomic force microscope (AFM: Nanoscope 3a, manufactured by Nippon Veeco Co., Ltd.).
[0034] In addition, each sample was filled with Otafuku Okonomiyaki Sauce, which was applied to the entire inside surface of the body, and the container was then left upright for 10 minutes, after which the liquid repellency against sauce was evaluated based on the state of the sauce sliding off immediately after the container was left upright. The results are shown in Figure 5. A circle indicates that the liquid level had returned to its initial position, and the liquid repellency was good, while a cross indicates that the liquid level had not returned to its initial position, and the liquid repellency was poor. Additionally, "At the start" shows the appearance of the container just before it was left for 10 minutes, and "After 10 minutes" shows the appearance of the container just after it was left for 10 minutes.
[0035] As can be seen from the results shown in FIG. 5, sample numbers 1, 2, and 4 to 7, which do not correspond to the embodiments of the present invention, had poor liquid repellency, whereas sample numbers 3 and 8 to 10, which correspond to the embodiments of the present invention, were confirmed to have good liquid repellency. [Explanation of symbols]
[0036] 1 Blow Molding 1a Mouth 1b Torso 1c bottom 1d Inner surface 2. Precursor 3. Alcohol 4 Blow mold 5 Cavity
Claims
1. The method includes an extrusion blow molding step of supplying a gas and a mist of alcohol into a precursor having an inner surface formed of a resin having a surface tension of 25 mN / m or less, and molding the precursor into a blow molded article having an inner surface with a center line average roughness Ra of 60 nm to 150 nm, The center line average roughness Ra is a three-dimensional extension of the center line average roughness Ra defined in JIS B 0601 so that it can be applied to the measurement surface, the resin is a silicone-containing olefin resin containing 15% by weight or more and 30% by weight or less of silicone, the alcohol is ethanol; The extrusion blow molding process includes a preparation process, a pressurization process, and a drying process, The preparation step is a step of placing the precursor having a bottomed tubular shape in a clamped blow molding die, the pressurizing step is a step of supplying the pressurized gas and the atomized alcohol into the precursor in the cavity of the blow molding die, so that the atomized alcohol collides with and adheres to the inner surface of the precursor, thereby forming the blow molded product having a shape that conforms to the shape of the cavity; The method for producing a blow molded product, wherein the drying step is a step of evaporating the alcohol adhering to the inner surface of the blow molded product.
2. A method for producing a blow molded article as described in claim 1, wherein the blow molded article forms at least a part of a container.
Citation Information
Patent Citations
Structuralized surface and method for using the same
JP2002321224A
Manufacturing method of container
JP2017019249A
Container having inner surface formed of olefin resin layer
JP2017019516A
Resin injection molded product and its manufacturing method
JP6732372B2
Structure having lubricating layer formed on surface
WO2015194625A1