Plastic container
The resin container with a silica vapor-deposited film and hydrophobic surface enhances both barrier properties and foaming by utilizing aggregates with specific roughness and contact angle, addressing the limitations of existing resin containers.
Patent Information
- Application Number
- JP2021109711
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-06-30
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-06-30
AI Technical Summary
Resin containers for sparkling beverages exhibit inferior barrier properties and lack effective promotion of foaming compared to metal cans.
A resin container with a silica vapor-deposited film on the inner surface featuring aggregates with an arithmetic mean roughness of 2 μm or more, and a hydrophobic surface with a water contact angle of 90° or more, which includes a barrier layer and an adhesive layer to enhance barrier properties and promote foaming.
The resin container achieves improved barrier properties and promotes effective foaming upon opening, with enhanced foaming properties and reduced gas permeation.
Smart Images

Figure 0007566434000003 
Figure 0007566434000004 
Figure 0007566434000005
Abstract
Description
[Technical field]
[0001] The present invention relates to a resin container. [Background technology]
[0002] Containers having irregularities on the inner surface to promote foaming are known as containers for beer, carbonated drinks, and other sparkling beverages. For example, Patent Document 1 describes a can having irregularities on the surface of an organic resin coating layer. Patent Document 2 describes a resin container having irregularities on the inner surface. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 4758693 [Patent Document 2] Patent No. 6804189 Summary of the Invention [Problem to be solved by the invention]
[0004] Since resin containers have inferior barrier properties compared to cans, it would be desirable to provide a resin container that can simultaneously achieve improved barrier properties and accelerated foaming.
[0005] SUMMARY OF THE PRESENT DISCLOSURE An object of the present invention is to provide a resin container that can simultaneously achieve improved barrier properties and accelerated foaming, and a method for producing the same. [Means for solving the problem]
[0006] The resin container of the present invention is A resin container for a sparkling beverage having a mouth portion, a body portion connected to the mouth portion, and a bottom portion connected to the body portion, The deposition film containing aggregates with an arithmetic mean roughness Ra of 2 μm or more The resin container On the inner surface of the resin substrate the aggregates have a width of 1 μm or more and 50 μm or less, the aggregates are scattered on the smooth surface of the vapor-deposited film having an arithmetic mean roughness Ra of several nm or less, and the vapor-deposited film forms irregularities on the inner surface of the resin container, which serve as starting points for foaming, in order to promote foaming when the closure is removed from the mouth. The container is made of resin.
[0007] In addition, in the resin container of the present invention having the above-mentioned configuration, the vapor-deposited film is preferably a silica vapor-deposited film.
[0008] In addition, in the resin container of the present invention having the above-mentioned configuration, it is preferable that the arithmetic mean roughness Ra of the vapor-deposited film containing the aggregate is 9 μm or less.
[0009] In addition, in the resin container of the present invention having the above-mentioned configuration, it is preferable that the water contact angle of the inner surface of the vapor-deposited film is 90° or more.
[0010] In addition, the manufacturing method for a resin container of the present invention preferably includes a substrate forming step of forming the resin substrate, and a vapor deposition step of forming a silica vapor deposition film as the vapor deposition film on the inner surface of the resin substrate, and the vapor deposition step preferably includes a surface layer forming step of forming a surface layer having a water contact angle of 90° or more using a rare gas as a carrier gas. Effect of the Invention
[0011] According to the present invention, it is possible to provide a resin container that can simultaneously achieve improved barrier properties and promoted foaming, and a method for producing the same. [Brief description of the drawings]
[0012] [Figure 1] 1 is a partially cross-sectional side view showing a resin container according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a partially enlarged view of FIG. [Diagram 3] FIG. 4 is a cross-sectional view showing a part of a resin container according to a second embodiment of the present invention. [Figure 4] 4 is a microscope image showing the surface state of the evaporated film in the first embodiment. [Diagram 5] 11 is a microscope image showing the surface state of the evaporated film in the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
[0014] As shown in FIG. 1, in the first embodiment of the present invention, a resin container 1 (hereinafter simply referred to as container 1) is a container 1 for carbonated beverages, which are liquid beverages containing carbon dioxide gas, such as beer, sparkling beer, shochu highball, sparkling wine, carbonated drinks, and carbonated water.
[0015] The container 1 is in the shape of a bottle having a cylindrical mouth 1a, a body 1b connected to the mouth 1a, and a bottom 1c connected to the body 1b. A closure (not shown) that seals the mouth 1a so that it can be opened is attached to the mouth 1a. More specifically, the closure is a cap that is detachably attached to the mouth 1a via a male screw 1d provided on the outer circumferential surface of the mouth 1a. The locking structure for detachably attaching the cap to the mouth 1a is not limited to a structure including the male screw 1d. The mouth 1a is cylindrical, but may be elliptical, square, or other cylindrical shapes. The closure is not limited to a cap.
[0016] A sparkling beverage is contained in the internal space S of the container 1. When the closure is removed from the mouth 1a, the internal space S is opened to the atmosphere and the pressure in the internal space S decreases, causing the beverage to foam. In this embodiment, in order to promote foaming when the closure is removed from the mouth 1a, the vapor deposition film 3 forms irregularities on the inner surface of the container 1 that serve as foaming starting points.
[0017] 2, the container 1 has a resin substrate 2 and a vapor-deposited film 3 formed on the inner surface of the resin substrate 2. The vapor-deposited film 3 is not particularly limited, but in this embodiment, it is a silica vapor-deposited film. In this embodiment, the vapor-deposited film 3 has an adhesive layer 3a formed on the inner surface of the resin substrate 2 and a barrier layer 3b formed on the inner surface of the adhesive layer 3a, and the inner surface of the barrier layer 3b is the inner surface of the container 1.
[0018] The resin forming the resin substrate 2 is not particularly limited, and may be, for example, polyester such as polyethylene terephthalate (PET), polyolefin such as polypropylene or polyethylene. In this embodiment, the resin substrate 2 is formed of polyethylene terephthalate. The method for forming the resin substrate 2 is not particularly limited, and may be, for example, blow molding or injection molding. The resin substrate 2 may have a single layer structure or a laminated structure.
[0019] The method for forming the vapor-deposited film 3 is not particularly limited, and may be, for example, chemical vapor deposition (CVD), physical vapor deposition (PVD), etc. Examples of chemical vapor deposition include plasma CVD and thermal CVD. Examples of the power source used in plasma CVD include direct current, high frequency, and microwave.
[0020] The adhesive layer 3a is a layer for adhering the barrier layer 3b to the inner surface of the resin substrate 2. If the adhesiveness between the barrier layer 3b and the resin substrate 2 is good, the adhesive layer 3a does not need to be provided. The barrier layer 3b can be formed, for example, by plasma CVD using hexamethyldisiloxane (HMDSO, (CH3)3Si-O-Si(CH3)3) as a raw material gas and oxygen (O2) as a carrier gas. In this case, it is preferable to use microwaves as a power source.
[0021] The barrier layer 3b is a layer having a barrier property that suppresses the permeation of gases such as oxygen and water vapor. The barrier layer 3b can be formed, for example, by plasma CVD using hexamethyldisilazane (HMDSN, (CH3)3Si-NH-Si(CH3)3) as a raw material gas and oxygen (O2) as a carrier gas. In this case, it is preferable to use microwaves as a power source.
[0022] By forming the deposited film 3 to contain aggregates so that the arithmetic mean roughness Ra is 2 μm or more, the uneven surface of the aggregates contained in the inner surface of the deposited film 3 (the inner surface of the container 1) can be utilized as the starting point of foaming. To enhance the promotion of foaming, the arithmetic mean roughness Ra of the deposited film containing aggregates is preferably 3 μm or more and preferably 9 μm or less. The aggregates are aggregates of the deposition material, and in this embodiment, are aggregates of an organosilicon compound.
[0023] The size (width) of the aggregates is, for example, about 1 to 50 μm. The greater the number (density) of aggregates, the greater the number of starting points for foaming, which is preferable. As shown in the example of FIG. 4, the aggregates are scattered on a smooth surface having an arithmetic mean roughness Ra of, for example, several nm or less.
[0024] The container 1 can be manufactured, for example, through a base material forming step and a vapor deposition step. The base material forming step is a step of forming a resin base material 2. The vapor deposition step is a step of forming a vapor-deposited film 3 on the inner surface of the resin base material 2.
[0025] The vapor deposition process includes, for example, an adhesive layer forming process and a barrier layer forming process. The adhesive layer forming process is a process of forming an adhesive layer 3a on the inner surface of the resin substrate 2. The barrier layer forming process is a process of forming a barrier layer 3b on the inner surface of the adhesive layer 3a.
[0026] Although the foaming-promoting effect can be obtained even if the inner surface of the vapor-deposited film 3 is hydrophilic, i.e., the water contact angle is less than 90°, a higher effect can be obtained if the inner surface is hydrophobic, i.e., the water contact angle is 90° or more. Therefore, although the inner surface of the vapor-deposited film 3 may be hydrophilic, it is preferable that the inner surface is hydrophobic. For this reason, when the inner surface of the barrier layer 3b is hydrophilic, the vapor deposition process preferably includes a surface layer formation process of forming a hydrophobic surface layer 3c (see FIG. 3) on the inner surface of the barrier layer 3b. The hydrophobic surface layer 3c can be formed, for example, by using a rare gas as a carrier gas.
[0027] When the barrier layer 3b is formed by plasma CVD using hexamethyldisiloxane and oxygen as described above, the inner surface of the barrier layer 3b becomes hydrophilic. In this case, for example, as in the second embodiment shown in FIG. 3, it is preferable to form a hydrophobic surface layer 3c on the inner surface of the barrier layer 3b by deposition. The surface layer 3c can be formed by plasma CVD using, for example, hexamethyldisiloxane as a raw material gas and a rare gas as a carrier gas. In this case, it is preferable to use argon (Ar) or helium (He) as the rare gas, and it is preferable to use microwaves as the power source.
[0028] Even when the surface layer 3c is provided, it is possible to form a deposited film containing aggregates having an arithmetic mean roughness Ra of 2 μm or more, as in the example shown in Fig. 5. Therefore, the uneven surfaces of the aggregates contained in the hydrophobic inner surface of the deposited film 3 serve as the starting points for foaming, and foaming can be strongly promoted.
[0029] According to the embodiment described above, the vapor deposition film 3 can simultaneously improve the barrier properties and promote foaming.
[0030] The present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the spirit and scope of the present invention.
[0031] Therefore, the resin container 1 of the above-described embodiment can be modified in various ways, for example as described below.
[0032] The resin container 1 of the above-described embodiment can be modified in various ways as long as it is a resin container 1 having a vapor-deposited film 3 containing aggregates with an arithmetic mean roughness Ra of 2 μm or more on the inner surface of the resin substrate 2.
[0033] For example, in the above-described embodiment, the shape of the container 1 is a wide-mouthed bottle in which the size of the mouth 1a is equal to that of the body 1b, but the shape is not limited to this and may be a narrow-mouthed bottle. The shapes of the body 1b and the bottom 1c can be appropriately set. The body 1b may have, for example, an annular groove or an annular protrusion extending in the circumferential direction. The layer structure of the vapor-deposited film 3 is not limited to two or three layers as in the above-described embodiment, but may be four or more layers.
[0034] In addition, the resin container 1 of the above-described embodiment is preferably a resin container 1 in which the vapor-deposited film 3 is a silica vapor-deposited film in the above configuration.
[0035] In addition, the resin container 1 of the above-described embodiment is preferably a resin container 1 in which the arithmetic mean roughness Ra of the vapor-deposited film 3 containing the aggregates is 9 μm or less in the above configuration.
[0036] In addition, the resin container 1 of the above-described embodiment is preferably a resin container 1 in which the water contact angle of the inner surface of the vapor-deposited film 3 is 90° or more in the above configuration.
[0037] In addition, the manufacturing method for the resin container 1 of the above-mentioned embodiment preferably includes a substrate forming process for forming a resin substrate 2, and a vapor deposition process for forming a silica vapor deposition film as a vapor deposition film 3 on the inner surface of the resin substrate 2, and the vapor deposition process preferably includes a surface layer forming process for forming a surface layer 3c having a water contact angle of 90° or more using a rare gas as a carrier gas. EXAMPLES
[0038] A bottle-shaped container having the layer structure of the first embodiment was produced as Example 1, a bottle-shaped container having the layer structure of the second embodiment was produced as Example 2, and a bottle-shaped container without a vapor deposition film was produced as Comparative Example 1, and foamability was evaluated. In Comparative Example 2, an attempt was made to produce a bottle-shaped container having the same layer structure as Example 1 at lower power.
[0039] In each of Example 1, Example 2, and Comparative Example 2, a vapor-deposited film was formed on a resin substrate made of polyethylene terephthalate under the conditions shown in Table 1. In Comparative Example 1, the container was made of only a resin substrate made of polyethylene terephthalate. [Table 1]
[0040] For each of Comparative Example 1, Example 1, Example 2, and Comparative Example 2, the water contact angle and the arithmetic mean roughness Ra were measured, and the foaming property and the oxygen barrier property (oxygen permeability) were evaluated. The results are shown in Table 2. FIG. 4 shows an image obtained by photographing the inner surface of the vapor-deposited film of Example 1 (the inner surface of the barrier layer) with a microscope, and FIG. 5 shows an image obtained by photographing the inner surface of the vapor-deposited film of Example 2 (the inner surface of the surface layer) with a microscope. Note that the sizes of the scattered aggregates are indicated in FIG. 4 and FIG. 5. [Table 2]
[0041] The water contact angle is the minimum and maximum values obtained when the contact angle with water on the inner surface of the container is measured at several points using a contact angle meter "CA-D" (manufactured by Kyowa Interface Science Co., Ltd.) as a measuring device. The arithmetic mean roughness Ra is the arithmetic mean roughness Ra measured at 10 random points using a measuring device VR3000 (manufactured by Keyence Corporation).
[0042] The foaming property was evaluated visually, with × being poor, ◯ being good, and ⊚ being extremely good. Beer was used as the foaming beverage. Particularly in Example 2, extremely good foaming like draft beer could be observed upon opening. In addition, in Comparative Example 2, which had a small microwave output (power), there were few aggregates and good foaming property was not obtained.
[0043] The oxygen permeability was measured by the MOCON method under the conditions of 23°C-55% RH outside and 23°C-90% RH inside. In particular, in Example 2, the BIF (Barrier Improvement Factor) based on Comparative Example 1 was 21.8, confirming high barrier properties. [Explanation of symbols]
[0044] 1. Plastic container 1a Mouth 1b Torso 1c bottom 1d Male thread 2. Resin substrate 3. Evaporation film 3a Adhesive layer 3b Barrier layer 3c surface layer S interior space
Claims
1. A resin container for a sparkling beverage, the resin container having a mouth, a body connected to the mouth, and a bottom connected to the body, The resin container has a vapor-deposited film containing aggregates having an arithmetic mean roughness Ra of 2 μm or more on an inner surface of a resin substrate, The width of the aggregate is 1 μm or more and 50 μm or less, the aggregates are scattered on a smooth surface of the deposited film having an arithmetic mean roughness Ra of several nm or less, A resin container, in which the vapor deposition film forms irregularities on the inner surface of the resin container, which serve as starting points for foaming, in order to promote foaming when the closure is removed from the mouth.
2. The resin container according to claim 1 , wherein the vapor deposition film is a silica vapor deposition film.
3. 3. The resin container according to claim 1, wherein the vapor-deposited film containing the aggregates has an arithmetic mean roughness Ra of 9 μm or less.
4. The resin container according to any one of claims 1 to 3, wherein the water contact angle of the inner surface of the vapor-deposited film is 90° or more.
5. A base material forming step of forming the resin base material; a vapor deposition step of forming a silica vapor deposition film as the vapor deposition film on the inner surface of the resin substrate, The method for manufacturing a resin container according to any one of claims 1 to 4, wherein the vapor deposition step includes a surface layer formation step of forming a surface layer having a water contact angle of 90° or more using a rare gas as a carrier gas.
Citation Information
Patent Citations
Bottle and manufacturing process of bottle
JP2009046162A
Non-adhesive container and manufacturing method thereof
JP2010254377A
Container
JP2014148332A
Water-repellent film for lid material, lid material, and packaging container
JP2015025052A
Can for effervescent beverages and method for manufacturing the same
JP4758693B2