Corrugations for expanding against high rigidity shape
The expanded corrugated design of the polymeric liner in Type IV pressure vessels addresses leakage and distortion issues by ensuring full support from the outer shell, enhancing structural integrity and reducing strain.
Patent Information
- Application Number
- JP2021577443
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-06-28
- Filing Date
- 2020-06-29
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2040-06-29
AI Technical Summary
Type IV pressure vessels experience leakage and distortion due to air pockets in the annular cavity of the corrugated liner, leading to non-uniform pressure support and potential rupture during inflation.
The corrugated polymeric liner is designed with expanded corrugations that have varying wall thickness and curvature, ensuring full support by the outer synthetic shell, minimizing air pockets and reducing strain on the liner.
The solution effectively prevents leakage and distortion by uniformly supporting the corrugated sections, reducing the likelihood of bulging and rupture, thus enhancing the structural integrity of the pressure vessel.
Smart Images

Figure 0007569339000001 
Figure 0007569339000002 
Figure 0007569339000003
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0001] This application claims priority to U.S. Provisional Patent Application No. 62 / 867,914, filed June 28, 2019.
[0002]
[0002] The present invention relates to corrugations for use in Type IV pressure vessels for the storage of compressed gases. More particularly, the present invention relates to a corrugation profile for a corrugated polymeric liner that is covered with a rigid outer composite shell of fabric and resin to form a tank for a Type IV pressure vessel. [Background technology]
[0003]
[0003] Type IV pressure vessels for storage of compressed gases comprise a non-metallic liner completely encased in a matrix of fibers and resin. The resin matrix usually comprises polyester or epoxy resin. Type IV pressure vessels generally have a metal pressure vessel closure with a valve.
[0004]
[0004] Type IV pressure vessels are desirable for use in vehicles because they have a low unit weight compared to other types of pressure vessels. Type IV pressure vessels are formed from a non-metallic liner and are lined with fabric and resin. Other types of pressure vessels generally have a higher unit weight than Type IV pressure vessels because they contain more metal than Type IV pressure vessels. For example, a Type I pressure vessel comprises a metal cylinder. A Type II pressure vessel comprises a metal cylinder partially encased in a fabric material. A Type III pressure vessel comprises a metal liner completely encased in fabric. Thus, Type IV pressure vessels are desirable for use in vehicles because of the low weight associated with using a polymeric liner instead of a metal liner.
[0005]
[0005] If the vehicle has a hydrogen fuel cell and / or if the vehicle uses compressed natural gas as fuel, the vehicle is optionally equipped with a Type IV pressure vessel. Although other types of pressure vessels, such as Types I-III, can be used for the vehicle, Type IV is preferred due to its low weight of the pressure vessel.
[0006] A known method of manufacturing a pressure vessel with a polymer liner is disclosed in US Publication No. 2016 / 363265, in which fibers are braided around a corrugated polymer liner and coated with resin. The polymer liner has a general tubular shape with a corrugated portion. The corrugated portion has a plurality of spaced ridges extending circumferentially around the liner with valleys between adjacent ridges. The spaced ridges are separated by valleys to form a conventional corrugated shape. Sidewalls extend between the ridges and adjacent valleys. A gap between adjacent sidewalls defines an annular cavity. The polymer liner is coated with braided fibers and liquid resin before the resin cures to form a hard outer synthetic shell. The cured coated polymer liner is assembled with a metal pressure vessel to form a Type IV pressure vessel.
[0007]
[0007] However, in some cases, the liquid resin does not completely fill the annular cavity of the corrugation, forming an air pocket within the annular cavity. When pressure is applied to a pressure vessel, the pressure is applied uniformly along the inner surface of the liner. If an air pocket is present within the annular cavity of the corrugated liner, the pressure applied to the liner is not supported uniformly by the resin and the rigid outer composite shell during the expansion process. Strain on the corrugated liner adjacent to the annular cavity can cause the liner to bulge outwardly toward the annular cavity. This distortion of the corrugated liner can cause leakage. In certain instances, the corrugated liner can cause ruptures in the area of the air pocket, accelerating the leakage of compressed gas through the liner. Summary of the Invention [Problem to be solved by the invention]
[0008]
[0008] It is therefore desirable to provide a Type IV pressure vessel having a liner with corrugated sections that is resistant to leakage through the corrugated sections. Additionally, it is desirable to reduce the strain on the corrugated sections due to expanding the pressure vessel. Additionally, it is desirable to locate high stress zones formed during expansion in locations that are fully supported by the outer composite shell. Finally, it is desirable to fully support the side walls of the corrugations after the pressure vessel is expanded. [Means for solving the problem]
[0009]
[0009] A corrugation is provided in a polymeric liner that is configured to expand against a rigid shape. The polymeric liner has a cylindrical wall with opposed inner and outer surfaces. The liner has a first liner section having a plurality of annular corrugations. Each of the corrugations has curved peak regions with ridges, curved valleys between adjacent spaced peak regions, and a sidewall joining each successive peak region and valley. The distance between successive ridges defines a period of the corrugation. The wall thickness of the liner at the ridges is greater than the wall thickness at the valleys. The radial distance between the ridges and valleys defines an amplitude of the corrugation. The amplitude is between about 0.65 and about 0.75 times the period of the corrugation.
[0010] The advantages of the present invention will be readily appreciated as the same becomes better understood by reference to the following detailed description when considered in connection with the accompanying drawings, in which: [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a cross-sectional view of a polymeric liner for a Type IV pressure vessel, in accordance with one embodiment of the present invention. [Diagram 2]
[0012] FIG. 2 is an enlarged cross-sectional view of portion 2 of the polymer liner of FIG. 1. [Diagram 3]
[0013] FIG. 1 is a perspective view of a compatible pressure vessel according to one embodiment of the present invention. [Figure 4]
[0014] FIG. 4 is a partial cross-sectional view showing portion 4 of the pressure vessel of FIG. [Diagram 5]
[0015] 3 is an enlarged cross-sectional view of portion 5 of the polymer liner of FIG. 2 showing a first embodiment of a novel corrugation. [Figure 6]
[0016] FIG. 6 is a side view of the liner of FIG. 5 before the liner is covered with resin and fiber. [Figure 7]
[0017] FIG. 4 is a side view of the pressure vessel of FIG. 3 showing the pressure vessel folded into a stacked configuration. [Figure 8]
[0018] 3 is an enlarged cross-sectional view of portion 8 of the liner of FIG. 2 showing a first embodiment of the novel corrugation. [Figure 9]
[0019] 3 is an enlarged cross-sectional view of portion 8 of the liner of FIG. 2 showing a second embodiment of the novel corrugation. [Figure 10]
[0020] FIG. 3 is a cross-sectional view showing the liner of FIG. 2 covered with an outer synthetic shell to form a pressure vessel. [Figure 11]
[0021] FIG. 11 is an enlarged cross-sectional view of a portion 11 of the pressure vessel of FIG. [Figure 12]
[0022] 6 is a perspective cross-sectional view of the novel corrugation of FIG. 5 showing compression force, edge crush force, and bendability. [Figure 13]
[0023] FIG. 12 is a perspective cross-sectional view of the pressure vessel of FIG. 11 showing the compressive forces on the outer synthetic shell and the pressure applied to the liner during the expansion process. [Figure 14]
[0024] 1 is a cross-sectional view of a known corrugated liner having conventional corrugations. [Figure 15]
[0025] 15 is a cross-sectional view of portion 15 of the known corrugated liner of FIG. 14. [Figure 16]
[0026] FIG. 15 is an enlarged cross-sectional view showing a portion 16 of the known corrugated liner of FIG. 14 being covered with an outer synthetic shell to form a known pressure vessel. [Figure 17]
[0027] 15 is an enlarged perspective cross-sectional view of the known corrugated liner of FIG. 14 illustrating compression force, edge crush force, and bowing. [Figure 18]
[0028] 17 is an enlarged perspective cross-sectional view of the known pressure vessel of FIG. 16 illustrating the compressive forces on the outer synthetic shell and the pressure applied to the corrugated liner during the expansion process. [Figure 19]
[0029] FIG. 11 is an enlarged cross-sectional view of portion 11 of the pressure vessel of FIG. 10 after the expansion process, showing the maximum stress concentration immediately after self-contact is made. [Figure 20]
[0030] FIG. 11 is an enlarged cross-sectional view of portion 11 of the pressure vessel of FIG. 10 after the expansion process, showing the maximum stress concentration immediately after self-contact is made. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012]
[0031] Referring to the figures, in which like numerals indicate like or corresponding parts throughout the several views, Figures 1 and 2 show a polymeric liner 20 suitable for use in a Type IV elongated pressure vessel 24 as shown in Figure 3. The polymeric liner 20 of Figure 1 has a connector section 28 with novel corrugations 32 according to one embodiment of the present invention.
[0013]
[0032] Referring to FIG. 4, a Type IV pressure vessel 24 generally has a polymeric liner 20 that is covered with an outer synthetic shell 36 of resin and fiber. The pressure vessel 24 shown in FIGS. 3 and 4 is described as an elongated pressure vessel 24 and alternatively a compatible pressure vessel 24. The elongated pressure vessel 24 generally has a polymeric liner 20 having a plurality of tubular sections 40, with each successive tubular section 40 being joined to a connector section 28 as shown in FIG. 1. However, alternative embodiments of the elongated pressure vessel 24 may have other liner 20 configurations. For example, one embodiment of the liner 20 has an elongated tube 40 with novel corrugations 32 extending along at least a portion of the elongated tube 40, where, by way of non-limiting example, the liner 20 is covered with an outer synthetic shell 36 and then folded into a large spiral shape.
[0014]
[0033] 1 illustrates one embodiment of a bare liner 20 comprising a hollow body 44 having a connector section 28, a tapered section 48, and a tubular section 40. The hollow body 44 is defined by an elongated cylindrical wall 52 extending between a first end 56 and a second end 60 of the liner 20. The polymeric liner 20 has an inlet opening 64 at the first end 56 of the liner 20 and an outlet opening 68 at the second end 60 of the liner 20. Each of the inlet opening 64 and the outlet opening 68 into the liner 20 may be used to pass fluid into and / or out of the interior 44 of the liner 20 as desired. The liner 20 may have any size, shape, length, material, and configuration desired for a particular application without changing the scope of the invention.
[0015]
[0034] As further shown in FIG. 1 , the liner 20 has a plurality of elongated rigid tubular sections 40 having a first diameter 72, a plurality of connector sections 28 having a second diameter 76 smaller than the first diameter 72, and a tapered section 48 disposed between and joining successive elongated rigid tubular sections 40 and connector sections 28. The first diameter 72 and the second diameter 76 are measured as the outside diameters of the respective sections 40, 28. Each of the plurality of elongated rigid tubular sections 40 defines a respective chamber 80 for storing fluids and / or gases. A repeated liner section 92 is defined as comprising a single rigid tubular section 40 in combination with the tapered section 48 and connector section 28 attached to the rigid tubular section 40. Various embodiments of the liner 20 can have any desired number of repeated liner sections 92 forming any desired number of chambers 80 for storing fluids and / or gases.
[0016]
[0035] However, each repeated liner section 92 may have any combination, order, geometry, length, diameter, wall thickness, and / or number of corrugated sections 28, non-corrugated sections 40, 48, and rib sections, and may even have selected omitted sections 28, 40, 48, without altering the scope of the invention. For example, in one embodiment, the liner 20 may include a non-corrugated section 96 adjacent each end 56, 60 of the liner 20. In another embodiment, the liner 20 may have a uniform outer diameter from one end 56 to the opposite end 60 of the liner 20.
[0017]
[0036] The non-corrugated connector sections 96, 108 may be rigid in various embodiments. In various embodiments, the connector section 28 may have a diameter 76 that is smaller than the diameter 72 of the tubular section 40, where the tapered section 48 provides a transition between the diameters 72, 76 of the connector section 28 and the tubular section 40. However, other embodiments may include a liner 20 that includes sections 28, 40 having one or more suitable diameters 72, 76, and in other embodiments, the liner 20 may have non-cylindrical sections 28, 40, 48 that may have a variety of shapes. Similarly, in some embodiments, the tubular section 40 may include corrugations 32.
[0018]
[0037] The connector sections 28A at the first and second ends 56, 60 of the liner 20 can have cuff sections 96 configured to matingly and / or frictionally engage boss-form fittings 112 (as shown in FIG. 3).
[0019]
[0038] An enlarged view of the connector section 28 of FIG. 1 is shown in FIG. 2. FIG. 5 shows a cross-sectional view of the corrugations 32 of the connector section 28. The corrugations 32 are annular corrugations that extend around the outer periphery 28' of the liner 20. With reference to FIGS. 2 and 5, the connector section 28 has a plurality of adjacent corrugations 32 having a novel shape that will be further described below. Each corrugation 32 extends circumferentially around the outer periphery 28' of the connector section 28. The corrugations 32 increase the flexibility of the connector section 28, thereby allowing the liner 20 to fold at the connector section 28 as shown in FIG. 6. The novel corrugations 32 allow the connector portion 28 to be repositioned from a generally cylindrical shape shown in FIG. 1 to an arcuate shape 114B shown in FIG. 6. The arcuate shape of the connector section 28 is defined by an inner bend radius R1 and an outer bend radius R2 as shown in FIG. 6. Any desired number of corrugations 32 may be included, where this number is selected based on the dimensions of the liner 20 and the anticipated inner and outer bend diameters R1, R2 of the folded liner 20. Typically, the required maximum number of novel corrugations 32 in the connector portion 28 will depend, in part, on the anticipated inner and outer bend diameters R1, R2 of the connector portion 28. 3 / 4 , and diameter 76. For example, as the inner bend radius Ri and the outer bend radius R2 decrease, the minimum number of new corrugations 32 required increases.
[0020]
[0039] 1, the liner 20 is preferably manufactured as a seamless liner 20 using a single piece of material without welds. However, in some embodiments, individual liner segments 92 with a single chamber 80 may be connected together to form an elongated liner 20 with multiple chambers 80. In some embodiments, the liner 20 may be made by forming the various pieces 28, 40, 48, 96 of the liner 20 and bonding the pieces 28, 40, 48, 96 together. For example, the connector section 28 may be manufactured separately from the tapered section 48, the tubular section 40, and / or the cuff section 96. Such separate sections 28, 40, 48, 96 may then be bonded together to form the liner 20.
[0021]
[0040] The polymeric liner 20 shown in FIG. 1 is generally formed from one or more polymeric materials, such as nylon (PA), nylon 6 (PA6), ethylene-vinyl acetate (EVA), linear low-density polyethylene (LLDPE), low-density polyethylene (LDPE), high-density polyethylene (HDPE), polypropylene (PP), ethylene vinyl alcohol (EVOH), polytetrafluoroethylene (PTFE), polyurethane (PU), and / or polyvinyl chloride (PVC). The polymeric liner 20 may be formed from a single layer of polymeric material or may comprise a multi-layer structure of two or more polymeric layers, and may even have one or more metal layers, as required for a particular application. For example, such a liner 20 may be produced via deposition, multi-layer extrusion, and / or molding, and the like. Thus, the liner 20 may include a single material, such as nylon, as an example, or may include a multi-layer material. Exemplary embodiments of the multi-layer liner 20 include, by way of non-limiting example, an EVOH layer between a first and a second nylon layer, an EYOH layer between a first and a second polyethylene (DPE) layer, an EVAL™ ethylene vinyl alcohol copolymer (EVOH) LA170B layer between a first and a second Rilsan® TIEFLEX S442 NAT TL layer sandwiched between a first and a second Rilsan® polyamide 11 (PA11) BESN Black P126 TL layer. In various embodiments, the liner 20 can include or be constructed of any suitable number of layers of material, including one layer, two layers, three layers, four layers, five layers, or six layers, etc. The liner 20 is generally a non-metallic polymeric liner 20, although the polymeric polymer 20 can have a metal layer within the liner 20, forming the inner surface 146 and / or the outer surface 148 of the liner 20.
[0022]
[0041] 4, the liner 20 may be wrapped and / or over-braided with fiber impregnated fiber strands 150 or other suitable material to increase the strength of the liner 20 and thereby the duty pressure under which the liner 20 can be safely operated. Additionally, in various embodiments, the over-braided and / or wrapped fiber strands 150 may be arranged in multiple layers. One or more layers of resin impregnated fiber strands 150 form the hard outer synthetic shell 36 after the resin cures. Suitable fibers 150 for the outer synthetic shell 36 include one or more of carbon fiber, glass fiber, basalt fiber, boron fiber, aramid fiber, high density polyethylene fiber (HDPE), Zylon™ poly(p-phenylene-2,6-benzobisoxazole fiber) (PBO), aramid fiber, Kevlar® polyparaphenylene terephthalamide fiber, polyethylene terephthalate fiber (PET), nylon fiber (PA), polyethylene naphthalate (PEN), polyester fiber (PL), polypropylene fiber (PP), polyethylene fiber (PE), metal, ethylene vinyl alcohol fiber (EVOH), and polyurethane fiber (PU), and the like. Suitable resins include one or more of epoxy resins, vinyl ester resins, polyester resins, urethanes, thermoplastic resins, and the like. The selection of the material and dimensions of the liner 20 as well as the type and amount of resin and fiber 150 forming the outer synthetic shell 36 is based, in part, on the desired operating conditions of the pressure vessel 24.
[0023]
[0042] One or both ends 56, 60 of the liner 20 are fluidly connected to a boss-type fitting 112 as shown in FIGURE 3, thereby forming a sealed pressure vessel 24. Alternatively, one end 56, 60 of the liner 20 may be closed by other commonly known methods. If desired and appropriate for the selected boss-type fitting 112, the boss-type fitting 112 may be assembled with the liner 20 before or after the liner 20 is covered with the outer synthetic shell 36.
[0024]
[0043] After the liner 20 is covered with the outer synthetic shell 36, the covered liner 20 is folded into a stacked configuration 120 as shown in FIG. 7. The corrugations 32 in the connector section 28 increase the flexibility of the connector section 28, thereby allowing the liner 20 to be folded to fill a predetermined space 124 and / or to be folded into a housing 124. Once the liner 20 is covered with the outer synthetic shell 36 and folded into the desired folded shape 120, and the resin cures to strengthen the outer synthetic shell 36, the elongated pressure vessel 24 is formed. For example, FIG. 3 illustrates one embodiment in which the elongated pressure vessel 24 is folded and held in the stacked configuration 120 within the housing 124.
[0025]
[0044] When fully assembled, the pressure vessel 24 is suitable for storing liquids, compressed gases, and / or compressed liquids, such as hydrogen, nitrogen, natural gas, helium, dimethyl ether, liquefied petroleum gas, and xenon. Pressure vessels 24 for storing hydrogen for automotive applications are designed for internal pressures of about 5,000 PSI to about 10,000 PSI during normal use. In comparison, pressure vessels 24 for storing compressed natural gas are typically designed for internal pressures of about 3,000 PSI during normal use. Thus, the selection of the material and dimensions of the liner 20 as well as the type and amount of resin and fibers 150 forming the outer synthetic shell 36 are selected based on the desired operating conditions of the pressure vessel 24.
[0026]
[0045] In one exemplary embodiment of the liner 20 shown in FIG. 1, the repeated liner sections 92 have a suitable overall length of about 1 meter. The larger diameter tubular section 40 has an outer diameter 72 of about 46 mm and extends longitudinally for about 650 mm. Circumferential ribs and / or grooves are optionally disposed along the length of the larger diameter tubular section 40. The smaller diameter non-corrugated sections 96, 108 and the smaller diameter corrugated section 28 have an outer diameter 76 of about 21 mm. Suitable overall lengths of the smaller diameter non-corrugated sections 96, 108 and the smaller diameter corrugated section 28 are about 60 mm and 140 mm, respectively. Each tapered section 48 has an outer diameter 72 of about 46 mm on a first end 48A, an outer diameter 76 of about 21 mm on an opposite end 48B, and an overall length of about 75 mm. The wall thickness 110 of the liner wall 52 is generally between about 0.3 mm and about 1.2 mm, with the non-corrugated sections 40, 48, 96 having a wall thickness 52A in the range of about 0.5 to about 1.2 mm, and a minimum wall thickness 52B in the corrugated sections 28 of about 0.3 mm. However, it will be recognized that the wall thicknesses 52A, 52B, outer diameters 72, 76, inner diameters 76', lengths, and number of the corrugated and non-corrugated sections 28 and 96, 108 of the liner 20 may be greater (more) or less (fewer) than this range, if desired for the intended application without varying the scope of the invention.
[0027]
[0046] As shown in Figures 2 and 5, the corrugated section 28 has a novel corrugation 32 having a plurality of spaced ridges 140, 140' extending circumferentially around the liner 20 with valleys 144 present between adjacent ridges 140, 140'. A first embodiment of the novel corrugation 32 is shown in Figures 5 and 8. The novel corrugation 32 includes an inner surface 146 and an outer surface 128. While the inner surface 146 and the outer surface 148 have similar profiles, the distance 52A between the inner surface 146 and the outer surface 148 may vary as will be further described below. As shown in Figure 1, the novel corrugation 32 has a minimum outer diameter 76 defined on the outer surface 148 of the liner 20 at the location of the ridges 140. Additionally, the novel corrugation 32 has a minimum inner diameter 76' defined on the inner surface 146 of the liner 20 at the location of the valleys 144.
[0028]
[0047] A first embodiment of a novel corrugation 32 shown in FIG. 5 is defined by a period T, an amplitude A, a valley width Wv, and a peak width Wm. The period T of the corrugation 32 is defined as the distance between adjacent ridges 140, 140'. The amplitude A is defined as the vertical distance between a ridge 140, 140' and a valley 144 on the outer surface 148 as shown in FIGS. 5 and 8. With reference to FIG. 5, each ridge 140, 140' defines a peak 140, 140' of the peak 168. Imaginary vertical reference lines 140A, 144A are shown passing through the centers of the peaks 140, 140' and the valleys 144, respectively. The horizontal distance between the imaginary vertical reference lines 140 and 144A is one-half of the period T, shown in FIG. 5 as ½T.
[0029]
[0048] 5, each peak 168 has a curved profile 170 on the outer surface 148 indicated by a radius Rm, and a width indicated as Wm. The horizontal distance from the ridge 140, 140' of the peak 168 to each end 168A, 168B is defined as 1 / 2Wm, measured from the imaginary vertical reference line 140A. Imaginary vertical reference lines 184 and 184' spaced from the imaginary vertical reference line 140A define the width Wm of the peak 168. The approximate horizontal location of the ends 168A, 168B of the peak 168 is indicated by the imaginary vertical reference lines 184 and 184'. The curved profile 170 of the peak 168 is defined by a radius Rm that is tangent at the center of the peak 140, 140' to an imaginary horizontal reference line A' that passes through the plurality of peaks 140, 140'. The locations of the intersection of the curved profile 170 and each of the imaginary vertical reference lines 184 , 184 ′ along the outer surface 148 of the liner 20 define the ends 168 A, 168 B of the peaks 168 .
[0030]
[0049] 5, the valley 144 has a curved profile 172 on the outer surface 148 of the liner 20. The curved profile of the valley 144 is defined by a radius Rv tangent to an imaginary horizontal reference line A' that is spaced from the imaginary horizontal reference line A' a vertical distance equal to the amplitude A. Additionally, radius Rv meets imaginary horizontal reference line A″ at point 144 that is spaced an amount ½T from imaginary vertical reference line 140A passing through ridge peaks 140, 140′. The width of valley 144 is defined by a horizontal distance Wv centered about imaginary vertical reference line 144A passing through the center of valley 144. For reference, imaginary vertical reference lines 196, 196′ are shown in FIG. 5 spaced an amount ½Wv from imaginary vertical reference line 144A passing through the center of valley 144. The intersections of curved profile 172 and imaginary vertical reference lines 196, 196′ define ends 152, 152′ of valley 144 along the outer surface 148 of liner 20.
[0031]
[0050] A transition profile 200, 200' between the points 168A, 168B and 152, 152' is created by selecting a spline profile between the end points 168A, 168B and 152, 152' that smoothly blends into the curved profiles 170, 172 of the peaks 168 and valleys 144. The transition profile 200, 200' may extend past the end points 168A, 168B, 152, 152' to create a smooth spline profile between the ridges 140 and valleys 144. The transition profile 200, 200' is created by gradually changing the radius of curvature along the transition profile 200, 200'.
[0032]
[0051] Exemplary dimensions for the first embodiment of the novel corrugation 32 are based in part on the outer diameter 76 of the liner connector section 28. For a liner connector section 32 having a tubular outer diameter 76 of about 21 mm and an intended bend radius R1 of about 27 mm when the liner 20 is folded into the desired stack configuration 120, the preferred period T is about 3.1 mm to 3.3 mm, the preferred amplitude A is about 2.15 mm to about 2.35 mm, the preferred radius Rm of the peaks 168 is about 1.3 mm, and the preferred radius Rv of the valleys 144 is about 0.16 mm. Additionally, the minimum inner diameter 76' of the inner surface 146 at the valleys 144 is preferably between about 15.6 mm to about 16.2 mm. The minimum wall thickness 52A between the inner surface 146 and the outer surface 148 at the valleys 144 is about 0.3 mm. The remaining wall thickness 52A between the inner surface 146 and the outer surface 148 is typically between about 0.5 mm and about 1.2 mm.
[0033]
[0052] A second embodiment of the novel corrugation 32 is shown in Figure 9. As with the first embodiment, the second embodiment of the novel corrugation 32 has adjacent peaks 168 ridges 140, 140' spaced apart by valleys 144, and an inner surface 146 and an outer surface 148 on opposite sides of the liner wall 52. Additionally, each peak 168 has an undulating profile 170 that defines the upper surface 148 of the peak 168. As with the first embodiment, the corrugation 32 has a maximum outer diameter 76 measured at the ridges 140, 140 relative to the outer surface 148, and a minimum inner diameter 76' measured at the valleys 144 relative to the inner surface 146.
[0034]
[0053] The novel corrugation 32 of FIG. 9 is defined by the period T, the amplitude A, the wall thickness Tm at the ridges 140 of the peaks 168, the wall thickness Tv at the valleys 144, and the radius of curvature Rm of the undulation profile 170. The novel corrugation 32 of FIG. 9 further has a flat segment 212 having a width 212' at the base 144C of the valleys 144. The corrugation 32 has a sidewall section 216 that is offset from the vertical at an angle Θ shown in FIG. 9. The inner and outer surfaces 146 and 148 of the liner wall 52 are integrated between the flat section 212, the sidewall segment 216, and the undulation profile 170 to create smooth splines for each of the inner and outer surfaces 146 and 148 as desired while maintaining the respective liner thicknesses Tm and Tv at the ridges 140 and valleys 144.
[0035]
[0054] The exemplary nominal dimensions of the second embodiment shown in FIG. 9 of the novel corrugation 32 are based in part on the outer diameter 76 of the liner connector section 28 and the intended bend radius Ri of the collapsed liner 20 (shown in FIG. 6). The exemplary second embodiment has a nominal outer diameter 76 of the liner connector section 28 of about 21 mm and an intended bend radius Ri of about 27 mm. As the outer diameter 76 increases, the intended bend radius Ri increases; that is, as the tubing size increases, the bend radius Ri increases.
[0036]
[0055] 9, the preferred period T of the second embodiment of the novel corrugation 32 is about 0.15 times the outer diameter (OD) of the novel corrugation 32, e.g., T=0.15OD. Preferably, the period T scales with the change in the outer diameter 76. Additionally, the remaining parameters scale with the period T. The amplitude A is preferably defined as about 0.7 times the period T, e.g., A=0.7T. The radius of curvature Rm of the undulating section 170 is preferably defined as 0.41 times the period T, e.g., Rm=0.41T. The angle Θ of the sidewall section 216 is preferably about 5.3 degrees.
[0037]
[0056] For the second embodiment shown in Fig. 9, the width 212' of the flat section 212 is preferably selected as about 0.038 times the period T, e.g., flat = 0.038T. Preferably, the width 212' of the flat segment 212 is at least 0.12 mm, and the period T is at least about 3.2 mm to facilitate processing during manufacturing. Furthermore, the thickness Tm of the liner wall 52 at the ridge 140 is preferably about 0.31 times the amplitude A, e.g., Tm = 0.31A. Similarly, the thickness Tv of the liner wall 52 at the valley 144 is preferably about 0.13 times the amplitude A, e.g., Tv = 0.13A.
[0038]
[0057] Exemplary preferred ranges for the parameters T, A, Rm, Θ, Tm, and Tv are defined as follows for the second embodiment of the novel corrugation 32 shown in Figure 9: The exemplary liner section 28 has an outside diameter (OD) 76 of about 21 mm, and an intended bend radius R1 of about 27 mm.
[0039]
[0058] The period T is T=T k OD is calculated as, where T k is a factor preferably having a preferred range of about 0.135 to about 0.165, and OD is the outside diameter 76 of the liner section 28.
[0040]
[0059] Amplitude A is A=A kCalculated as T, where A k is a factor having a preferred range of about 0.65 to about 0.75.
[0060] Radius Rm is Rm=R k Calculated as T, where R k is a coefficient having a preferred range of about 0.40 to about 0.45.
[0041]
[0061] The angle Θ has a preferred range of between about 5.0 degrees and about 7.0 degrees.
[0062] The width 212' of the flat segment 212 is flat=F k Calculated as T, where F k is a coefficient having a preferred range of between about 0 and about 0.040.
[0042]
[0063] A preferred range for the thickness Tm has a preferred minimum value calculated as Tm≦0.01OD, where Tm is at least 0.5 mm. A preferred maximum value for the thickness Tm is calculated as Tm≦0.32. Similarly, a preferred range for the thickness Tv has a preferred minimum value calculated as Tv≦0.01, where Tv is at least 0.3 mm. A preferred maximum value for the thickness Tv is calculated as Tv=0.27A. Furthermore, preferably, the selected thickness Tm is greater than the selected thickness Tv, e.g., Tm>Tv.
[0043]
[0064] In embodiments where the 3 / 4 bend radius is not applicable and / or is a large value, the period T may be selected as desired. For example, if the corrugations 32 are located within the tubular section 40 of the liner 20 or near the ends 56, 60 of the liner 20, the period T may be selected as desired since the liner 20 has the least curvature in these areas.
[0044]
[0065] Figures 10 and 11 show the corrugated section 28 of the liner 20 of Figure 2 covered by the outer synthetic shell 36. Referring to Figure 11, between adjacent new corrugations 32, a cavity 220 may be formed between the lower surface 36' of the outer synthetic shell 36 and the liner 20. The cavity 220 is bounded by the lower surface 36' of the outer synthetic shell 36, the upper surface 148 of the adjacent valley 68, the valley 144, and sidewall portions 228, 228' extending between the peak 168 and the valley 144.
[0045]
[0066] 12 shows a compressive force C applied to the valleys 144 and ridges 140, as well as an edge crushing force E applied to the end faces 232, 232' of the novel corrugation 32. Typically, the strength of the corrugation 32 is evaluated based on the compressive force C, the edge crushing force E, and the amount that the corrugation 32 will bend as shown by arrow B.
[0046]
[0067] FIG. 13 shows the corrugation section 28 covered by the outer synthetic shell 36. After the resin cures, the outer synthetic shell 36 becomes rigid. The outer synthetic shell 36 absorbs the compressive force C applied to the pressure vessel 24. Thus, the corrugations 32 are not affected by the compressive force C applied to the pressure vessel 24. The edge crush force E is not applicable because the liner 28 is cylindrical and the outer synthetic shell 36 surrounds the outer periphery 28' of the liner 28. After the outer synthetic shell 36 is applied and the covered liner 20 is folded into the stacked structure 120 and the resin cures to stiffen the outer synthetic shell 36, the amount that the corrugations 32 would bend (arrow B in FIG. 12) is not applicable because the outer synthetic shell 36 holds the liner 20 in a fixed position.
[0047]
[0068] However, when pressure is applied to the pressure vessel 24, the pressure P is applied non-uniformly along the inner surface 146 of the liner 20 as shown in FIG. 13. When pressure is applied, the liner 20 expands against the outer synthetic shell 36. The cavities 220 formed between adjacent new corrugations 32 are not fully supported by the outer synthetic shell 36. While resin may seep into the cavities 220 during processing, the outer wall 148 is often not uniformly supported by the outer synthetic shell 36 because air bubbles are trapped within the cavities 220. The gaps 240 in the cavities 220 near the transition between the peaks 168 and the sidewalls 228, 228' and the gaps 244 between the opposing sidewalls 228, 228' are of great importance. The novel corrugations 32 are specifically configured within these gaps 240, 244 to minimize the possibility of blisters, cracking, and pinhole leaks within the outer surface 148.
[0048]
[0069] The advantages of the novel corrugations 32 are best illustrated by analyzing a conventional corrugation configuration 260 when used as part of a liner 20A for a pressure vessel 24A, as shown in Figures 14-18. With reference to Figure 14, an exemplary tubular liner 20A has a known conventional corrugation 260 with spaced apart ridges 268, 268'. Valleys 276 are defined between adjacent ridges 268, 268'. The conventional corrugations 260 are intended to provide improved stiffness while still allowing for bending.
[0049]
[0070] An enlarged view of the conventional corrugation 260 is shown in FIG. 15. FIG. 16 shows an enlarged cross-sectional view of a portion of the liner 20A covered by the outer synthetic shell 36. Referring to FIG. 15, the conventional corrugation 260 is formed by the outer wall 52' of the liner 20A having an inner surface 146' and an outer surface 148'. The geometry of the conventional corrugation 260 is defined by an amplitude A2, a period T', a width Wv' of the valleys 276, and a peak width Wm' as shown in FIG. Both the ridges 268, 268' and the valleys 276 have generally horizontal upper and lower surfaces 146' and 148' as further indicated by imaginary horizontal reference lines H, FI' that extend across the ridges 268, 268' and the valleys 276, respectively. Similar to novel corrugation 32, the vertical spacing between ridges 268, 268' and valleys 276 of conventional corrugation 260 is defined by an amplitude A2, as shown in Figure 15. An imaginary horizontal reference line FI is spaced from an imaginary horizontal reference line H by an amount of amplitude A2.
[0050]
[0071] In contrast, the novel corrugation 32 has a curved upper profile of radius Rm at the peaks 168 and a curved lower profile 170 of radius Rv at the valleys 144, as shown in Figure 5. A second embodiment of the novel corrugation 32, shown in Figure 9, has flat segments 212 in the valleys 144, where the flat segments 212 are defined as having a width between 0.0 mm and a maximum width of about 0.040 times the period T of the corrugation 32.
[0051]
[0072] Referring again to Figure 15, a conventional corrugation 260 is generally defined by a period T' between center points cp of adjacent ridges 268, 268'. The width of the ridges 268, 268' is defined as Wm' as shown in Figure 16. Each ridge 268, 268' has flat portions on either side of the center point cp with a width of ½Wm' as shown in Figure 15. An approximate end point M1 of each ridge 268, 268' is generally defined by a boundary point M1 between an imaginary horizontal reference line H and an imaginary vertical reference line V" that is spaced from the center point cp by an amount 1 / 2Wm'. The outer profile 148' of the conventional corrugation 260 has a radius Rm' that merges into a corner M1 between the ridge 268, 268' and the adjacent sidewall 280, 280'. In contrast, the novel corrugation 32 shown in FIG. 8 has a curved profile 170 that extends on either side of the ridge peak 140, 140' having a width of 1 / 2Wm. The curved profile 170 of the novel corrugation 32 reduces the occurrence of leakage as compared to the flat ridges 268, 268' of the conventional corrugation 260 of FIG. 15.
[0052]
[0073] Each valley 276 of the conventional corrugation 260 has a generally flat valley 276 having a width defined by Wv' as shown in FIG. 15. A center point 276' of the valley 276 is defined by an intersection point 276' of an imaginary horizontal reference line H' and an imaginary vertical reference line Y that is spaced from the center point cp of the adjacent ridge 268, 268' by one-half the period T' as shown as ½T'. An approximate end M2 of the valley 276 is defined by an intersection point M2 of the imaginary horizontal reference line H' and an imaginary vertical reference line V' that is spaced from the imaginary vertical reference line V by an amount ½Wv' as shown in FIG. The outer profile 148' of the conventional corrugation 160 has a radius Rv' that merges into a corner M2 between the valley 276' and the adjacent sidewall 280, 280'.
[0053]
[0074] 9, the width of the flat segments 212 is limited to a maximum width of about 0.040 times the period T of the novel corrugation 32. In contrast, as shown in FIG. 15, the overall width Wv' of the valley 276 of the conventional corrugation 260 is flat except for a radius Rv' that merges the valley 276 into the adjacent sidewalls 280, 280' of the conventional corrugation 260.
[0054]
[0075] As further shown in FIG. 15, sidewalls 280, 280' connect the ridges 268, 268' and valleys 276 of the conventional corrugation 260. The sidewalls 280, 280' are generally straight walls 280, 280' with end points M1 and M2. A radius Rm' is defined between the ridges 268, 268' and the adjacent sidewalls 280, 280' to form a transition between the ridges 268, 268' and the sidewalls 280, 280'. Similarly, a radius Rv' is defined between the sidewalls 280, 280' and the valleys 276 to form a transition between the valleys 276 and the adjacent sidewalls 280, 280'. Additionally, a cavity 220' is defined in the space between the adjacent sidewalls 280, 280' and the valleys 276. The cavities 220' of the conventional corrugations 260 are similar to the cavities 220 formed in the novel corrugations 32. That is, the cavities 220, 220' are bounded by the upper surfaces 148, 148' of the liners 20, 20A and the lower surface 36' of the outer synthetic shell 36, which form the sidewalls 228, 228', 280, 280' of each valley 144, 276. Similar to the cavities 220 of the novel corrugations 32 of FIG. 11, the cavities 220' of the conventional corrugations 260 of FIG. 16 may be filled with resin during the manufacturing process of the pressure vessel 24A. Similar to the novel corrugations 32, irregular air pockets may be formed in the cavities 220' of the conventional corrugations 260 if the resin does not completely fill the cavities 220'.
[0055]
[0076] 15, the profile of the outer surface 148' of the conventional corrugation 260 is generally uniformly offset from the profile of the inner surface 146' by a wall thickness Wt. For example, the wall thickness Wtr of the ridges 268, 268' is generally equal to the wall thickness Wtv of the valleys 276. Further, the wall thickness Wt of the sidewalls 280, 280' is generally equal to the wall thicknesses Wtr, Wtv of the ridges 268, 268' and valleys 276.
[0056]
[0077] In contrast, the novel corrugations 32 shown in FIG. 9 have a wall thickness Tm at the ridges 140 that is thinner than the wall thickness Tv at the valleys 144. Specifically, the wall thickness Tm is preferably selected as at least a maximum value (which is 0.01 OD or 0.5 mm) and even less than 0.32 A. Similarly, the wall thickness Tv at the valleys 144 is preferably selected as at least a maximum value (which is 0.0 LOD or 0.3 mm) and even less than 0.27 A. Furthermore, the novel corrugations 32 specifically require a wall thickness Tm that is greater than or equal to the wall thickness Tv. Preferably, the novel corrugations 32 have a wall thickness Tm that is greater than the wall thickness Tv. However, for smaller outer diameter tubes used in some embodiments, the wall thickness Tm may be selected to be approximately equal to the wall thickness Tv for the pressure vessel 20, as a non-limiting example.
[0057]
[0078] 9, in a particular embodiment of the novel corrugation 32 having an outer diameter of about 21 mm, Tm may be preferably selected between about 0.5 mm and about 1.2 mm, Tv may be selected as at least 0.3 mm, with Tm being selected as a value greater than the selected value of Tv. The wall thickness Tm is preferably selected as a value greater than the wall thickness Tv, as will be further explained in connection with FIG. 20, which will be explained later.
[0058]
[0079] 17 illustrates a compressive force C applied to the valleys 276 and ridges 268, and an edge crushing force E applied to the end faces 284, 284′ of the conventional corrugation 260. Generally, the strength of the conventional corrugation 260 is evaluated based on the compressive force C, the edge crushing force E, and the amount that the conventional corrugation 260 will bend as shown by arrow B. The conventional corrugation 260 is generally designed to withstand a given compressive force C and edge crushing force E while allowing the conventional corrugation 260 to be flexible. The relative magnitude of the compressive force C that can be supported by the conventional corrugation 260 is greater than the relative magnitude of the compressive force C that can be supported by the novel corrugation 32. Similarly, the relative magnitude of the edge crushing force E that can be supported by the conventional corrugation 260 is greater than the relative magnitude of the edge crushing force E that can be supported by the novel corrugation 32. The uniform wall thickness Wt, straight sidewalls 280, 280', flat ridges 268, and flat valleys 276 of the conventional corrugation 260 increase the magnitude of the compression force C and edge crush force E that can be supported by the conventional corrugation 260 compared to the new corrugation 32.
[0059]
[0080] FIG. 18 shows the corrugation section 20A of FIG. 14 covered by the outer synthetic shell 36. After the resin cures, the outer synthetic shell 36 becomes rigid. Thus, the outer synthetic shell 36 absorbs the compressive force C applied to the pressure vessel 24A. Thus, the conventional corrugations 260 are not affected by the compressive force C applied to the pressure vessel 24A. The edge crush force E is not applicable because the liner 20A is cylindrical and the outer synthetic shell 36 surrounds the outer periphery 28' of the liner 20A. After the outer synthetic shell 36 is applied and the covered liner 20A is folded into the stacked structure 120 and the resin cures to stiffen the outer synthetic shell 36, the amount that the conventional corrugations 260 would bend (arrow B in FIG. 17) is not applicable because the outer synthetic shell 36 keeps the liner 20A in a fixed position. Thus, the inherent ability of the conventional corrugations 260 to support high levels of compressive forces C and edge crush forces E on the novel corrugations 36 does not provide an advantage when integrated into the pressure vessel 20, 20A, as further explained in Figures 19 and 20.
[0060]
[0081] When the conventional corrugations 260 are included as part of the pressure vessel 24A' and pressure is applied to the pressure vessel 24A, as shown in FIG. 18, pressure P' is applied non-uniformly along the inner surface 146' of the liner 20A. When pressure is applied, the liner 20A expands against the outer synthetic shell 36. The cavities 220' formed between adjacent conventional corrugations 260 are not fully supported by the outer synthetic shell 36. While resin may seep into the cavities 220' during processing, the outer sidewall 148' is often not uniformly supported by the outer synthetic shell 36 because air bubbles are trapped within the cavities 220'. The gaps 240' in the cavities 220 near the transitions between the peaks 268, 268' and the sidewalls 228, 228' and the gaps 244' between the opposing sidewalls 228, 228' are of great importance.
[0061]
[0082] FIG. 19 is a cross-sectional view of the conventional corrugations 260 of the pressure vessel 24A after the liner 20A is covered with the outer synthetic shell 36 and the resin has cured to strengthen the outer synthetic shell 36, and after expansion. Specifically, FIG. 19 shows the conventional corrugations 260 after expansion at the point of maximum stress concentration, which occurs just after the adjacent sidewalls 280, 280' self-contact. Self-contact is defined as the expansion of the conventional corrugations 260 during the expansion process until the liner 20A is in firm contact with the outer synthetic shell 36, and the adjacent sidewalls 280, 280' are forced toward each other until they abut the opposing sidewalls 280', 280. This process of self-contact is further described as a reaction under pressure.
[0062]
[0083] 19, during expansion, pressure P' is applied uniformly along the inner surface 146' of the conventional corrugation 260. Because the sidewalls 280, 280' of the valleys 276 are not fully supported by the outer synthetic shell 36, as the pressure P' increases beyond the resistive strength of the corrugation 268, the sidewalls 280, 280' will be forced toward each other until they contact the opposing sidewalls 280', 280'. During the expansion process, the sidewalls 280, 280' are forced into the gap 224' of the cavity 220'. The sidewalls 280, 280' have a contact point 292 in the center of the sidewalls 280, 280' as shown in FIG. 19, where the gap 224' in the cavity 220' is fully forced. When the sidewalls 280, 280' abut against the adjacent sidewalls 280', 280 at the contact points 292, both sidewalls 280, 280' are uniformly supported by the opposing sidewalls 280', 280. It is therefore desirable to compress the sidewalls 280, 280' until they contact the opposing sidewalls 280', 280, because once compressed, the sidewalls 280, 280' are uniformly supported. It is further desirable to have the sidewalls 280, 280' begin to compress toward the adjacent sidewalls 280' at low values of pressure P', because the magnitude of strain on the liner wall 52' is related to the applied pressure level P'.
[0063]
[0084] As shown in FIG. 19, when pressure is applied near the transitions between the ridges 268, 268' and the sidewalls 280, 280' of the conventional corrugations 260 at the inner surface 146', high pressure zones 296 are formed. These high pressure zones 296 are formed near the gaps 240' in the cavities 220'. In the high pressure zones 296, the liner walls 52' forming the sidewalls 280, 280' and the ridges 268, 268' are not fully supported by the outer synthetic shell 36 because the cavities 220' are formed between the outer synthetic shell 36 and the valleys 276 of the conventional corrugations 260. These high pressure zones 296 have a high potential for causing blistering, cracking, and pinhole leaks in the liner walls 52'. Additionally, these high pressure zones 296 are formed at the inner surface 146' of the liner 20A. An inner surface 146' of the liner 20A contacts the fluid exerting pressure on the pressure vessel 24A. Constant exposure to the pressurized fluid within the pressure vessel 24A can increase the likelihood of failure of the high stress zones 296.
[0064]
[0085] 19 is prevented from forming in locations that are not fully supported by the outer composite shell 36 or adjacent sidewalls 280, 280', since an unsupported high stress zone 26 may cause leakage. In particular, it is desirable to space the high pressure zone 296 away from gaps 240' in the cavity 220', since such gaps 240 have a high potential for leakage.
[0065]
[0086] FIG. 20 shows a cross-sectional view of the pressure vessel 20 after the liner 20 is covered by the outer synthetic shell 36, the resin has cured to consolidate the outer synthetic shell 36, and after expansion causing the liner 20 to make self-contact. Specifically, FIG. 20 shows the corrugations 32 after expansion at the point of maximum stress concentration, which occurs just after the self-contact of the adjacent side walls 228, 228'. During expansion, when the pressure vessel 24 is pressurized, pressure P is applied uniformly along the inner surface 146 of the corrugations 32. During expansion, the liner 20 expands to make firm contact with the outer synthetic shell 36. Specifically, after expansion, the new corrugations 32 are supported on the outer diameter 76 by the rigid outer synthetic shell 36.
[0066]
[0087] Because the sidewalls 228, 228' of the valleys 144 are not fully supported by the outer synthetic shell 36, when the pressure P increases beyond the resistive strength of the corrugations 32 during expansion, the sidewalls 280, 280' will be forced towards each other until they contact the opposing sidewalls 280', 280' and close the gap 244 in the cavity 220. In essence, during the expansion process, the new corrugations 32 expand to contact themselves 32 for support. The sidewalls 228, 228' have a contact point 292' in the center of the sidewalls 228, 228' as shown in FIG. 20. When the sidewalls 228, 228' abut the adjacent sidewalls 228', 228 at the contact point 292', both sidewalls 228, 228' are uniformly supported by the opposing sidewalls 228', 228. It is preferred to compress the side walls 228, 228' until they contact the opposing side walls 228', 228', because once compressed, the side walls 228, 228' are uniformly supported.
[0067]
[0088] Moreover, it is desirable for the sidewalls 228', 228 to begin to compress toward the adjacent sidewalls 228', 228 at low values of pressure P because the amount of strain on the liner wall 52 is related to the applied pressure level P. The novel corrugations 32 are configured to minimize the amount of pressure P required to compress the sidewalls 228, 228'. Specifically, the width Wv of the valleys 144 of the novel corrugations 32 of FIG. 8 is reduced as compared to the width Wv' of the valleys 276 of the conventional corrugations 260 shown in FIG. 15.
[0068]
[0089] Additionally, the valleys 276 have a profile 172 with a radius Rv extending between adjacent sidewalls 228, 228' as shown in Figure 8. The valleys 276 can have flat segments 212 as shown in Figure 9, but the width 212' of the flat segments 212 is limited to be no greater than 0.040 times the period T of the novel corrugation 32. If flat segments 212 are included in the novel corrugation 32, the width 212' of the flat segments 212 is preferably at least 0.12 mm for ease of processing. In contrast, the width Wv' of the flat valleys 276 of the conventional corrugation 260 shown in Figure 15 generally extends across the entire width Wv' of the valleys 276. Comparing the novel corrugation 32 of Figure 8 and the conventional corrugation 260 of Figure 15, the radius Rv' between the valley 276 and the sidewall 280, 280' of the conventional corrugation 260 is a smaller radius than the radius Rv of the valley 144 of the novel corrugation 32. This results in a sharper corner M2 between the sidewall 280, 280' and the valley 276 of the conventional corrugation 260 compared to the radius Rv between the sidewall 228, 228' and the valley 144 of the novel corrugation 32 shown in Figure 8. By reducing and / or eliminating the flat segments 212 within the valleys 144, reducing the width Wv of the valleys 144, and increasing the radius Rv between the valleys 144 and the adjacent sidewalls 228, 228', the amount of pressure P required to initiate compression of the sidewalls 228, 228' of the new corrugation 32 under pressure is effectively reduced.
[0069]
[0090] 9, other modifications in the novel corrugation 32 that reduce the pressure P required to initiate compression of the sidewalls 228, 228' include reducing the amplitude P as well as reducing the wall thickness Tv of the sidewalls 228, 228' and the valleys 144. As shown in FIG. 9, the wall thickness Tm of the ridges 140, 140' is greater than the wall thickness Tv of the valleys 144. The wall thickness of the sidewalls 228, 228' increases progressively from the wall thickness Tv where the sidewalls 228, 228' join the valleys 144 to the wall thickness Tm at the ridges 140, 140'. The reduced wall thickness Tv of the valleys 144 in combination with the tapered sidewalls 228, 228' reduces the pressure P required to initiate compression of the sidewalls 228, 228'. Considering the response under pressure for the corrugations 32, the geometric dimensions T, A, Wm, Wv, Tm, and Tv that describe the shape of the corrugations 32 scale with the tubular outer diameter 76. In general, as the tube outer diameter 76 increases, the possible bend radii R1, R2 increase. By reducing the wall thicknesses Tm, Tv for larger tubular outer diameters 76 (to a minimum thickness of about 0.01 times the outer diameter 76), the pressure P required to initiate self-contact during expansion is further reduced. Changing the wall thicknesses Tm, Tv has minimal effect on the overall stress on the liner 20 during expansion. If bendability is not an issue, i.e., if the bend radii R1, R2 are very large, the period T does not need to be selected based on the outer diameter 76 of the tubing 20, 28.
[0070]
[0091] 20, the amplitude A of the novel corrugation 32 and the amplitude A2 of the conventional corrugation 260 are shown for comparison. The amplitude A2 is also shown for comparison in FIG. 19. The amplitude A of the novel corrugation 32 is reduced compared to the amplitude A2 of the conventional corrugation 260. Reducing the amplitude A of the novel corrugation 32 compared to the conventional corrugation 260 further reduces the amount of pressure P required to initiate the indentation of the sidewalls 228, 228'. Although the sidewalls 228, 228', 280, 280' of both the novel corrugation 32 and the conventional corrugation 260 are indented under the pressures P, P', the amount of pressure P required to initiate the indentation of the sidewalls 228, 228' of the novel corrugation 32 is less than the pressure P' required to initiate the indentation of the sidewalls 280, 280' of the conventional corrugation 260. The pressure P required to initiate compression of the side walls 228, 228' of the novel corrugations 32 is approximately half the pressure P required to initiate compression of the side walls 280, 280' of the conventional corrugations 260. Furthermore, the reduced pressure P required to initiate compression of the side walls 228, 228' of the novel corrugations 32 also reduces strain on the liner walls 52. Furthermore, the reduced strain on the liner walls 52 of the novel corrugations 32 reduces the likelihood of leakage through the liner 20.
[0071]
[0092] In summary, by increasing the radii Rv, Rm, selecting a suitable amplitude A, selecting a suitable period T, and further reducing the valley width Wv relative to the total period T, the amount of pressure P required to initiate the compression of the sidewalls 228, 228' during the expansion process is reduced. Reducing the amount of pressure P required to initiate the compression of the sidewalls 228, 228' during the expansion process reduces the strain on the liner 20 and reduces the possibility of leakage. To allow the corrugations 32 to interact / compress with a lower pressure P, the width Wv of the valleys 144 is reduced. The width Wv of the valleys 144 has an approximate overall minimum value determined to facilitate manufacturing. Selecting a suitable circumference T of the corrugations 32 is favorable in maximizing the width Wv of the peaks 168. Reducing the width Wm of the peaks 68 increases the stress during expansion. This is because the contact area of the peaks 168 with the outer synthetic shell 36 is reduced. A moderate amplitude A of the corrugations 32 is preferred in providing the liner wall 52 with sufficient flexibility to allow self-contact to occur during expansion.
[0072]
[0093] These changes in the shape of the novel corrugations 32 reduce the stiffness of the novel corrugations 32 compared to the conventional corrugations 260. This reduction in stiffness is offset by the rigid outer synthetic shell 36 supporting the perimeter of the liner 20. These changes are offset by a reduction in the required pressure P needed to initiate collapse of the liner 20 during expansion.
[0073]
[0094] Further examination of the novel corrugations 32 after exposure to pressure P, as shown in FIG. 20, indicates that high stress zones 300 form near the centers of the ridges 140 of the novel corrugations 32 on the inner surface 140 of the liner 20. These high stress zones 300 are fully supported by the outer synthetic shell 36 because they are located in the middle of the peaks 168. Furthermore, the degree of stress concentration in the high stress zones 300 of the novel corrugations 32 is less than the degree of stress concentration in the high stress zones 296 of the conventional corrugations 260. Additionally, the wall thickness 304, Tm, between the inner surface 146 and the outer surface 148 is greatest in this high stress zone 300. The increased wall thickness 304 (compared to sidewalls 228, 228' and valleys 144), combined with the full support of high stress zones 300 by the outer synthetic shell 36, significantly reduces the likelihood of the liner 20 developing blistering, cracks, pinhole leaks, and the like.
[0074]
[0095] Similar to the conventional corrugation 260 shown in FIG. 19, a high stress zone 296' is formed near the transition between the peak 168 of the valley 144 and the sidewalls 228, 228' of the novel corrugation 32, as shown in FIG. 20. However, in contrast to the high stress zone 296 formed on the inner surface 146' of the conventional corrugation 260, the high stress zone 296' is located on the outer surface 148 of the novel corrugation 32. The magnitude of the stresses in the high stress zone 296' of the novel corrugation 32 is significantly less than the magnitude of the stresses in the high stress zone 296 of the conventional corrugation 260. The reduced magnitude of the high stress zone 296, in combination with the location of the stress zone 296' on the outer surface 148 of the liner 20, significantly reduces the likelihood of leakage occurring at this location 296'.
[0075]
[0096] 19 and 20, the substantially rounded shape of the novel corrugations 32 of FIG. 20 reduces the number and severity of stress concentrations during expansion as compared to the conventional corrugations 260 shown in FIG. 19. Additionally, stress concentrations 300 are shifted toward the center of the ridges 140, 140' of the novel corrugations 32, where the novel corrugations 32 are fully supported by the rigid outer synthetic shell 36.
[0076]
[0097] Therefore, the novel corrugation 32 shown in Figures 8 and 9 is more preferable than the conventional corrugation 260 shown in Figure 15 when the corrugation 32 is part of the liner 20 for the pressure vessel 20. One advantage of the novel corrugation 32 is that the amount of pressure P required to initiate the collapse of the sidewalls 228, 228' is reduced. A second advantage is that the high stress zones 296' formed on the outer surface 148 of the liner 20 upon application of pressure are formed along the sidewalls 228, 228', thereby reducing the possibility of leakage within the high stress zones 26'. A third advantage is that the high stress zones 300 formed on the inner surface 146 of the liner 20 upon application of pressure are formed near the ridges 140, 140' of the peaks 168, where the wall thickness Tm is enlarged and the outer surface 148 is fully supported by the outer synthetic shell 36. A fourth advantage is that the bending flexibility (indicated by arrow B in FIG. 12) is sufficient to allow the liner 20 to be folded into the predetermined stack configuration 120.
[0077]
[0098] The present invention has been described in an illustrative manner. It is to be understood that the terminology used is intended to be descriptive and not limiting in nature. Many modifications and variations of the present invention are possible in light of the above teachings. It is therefore to be understood that, within the scope of the appended claims, the invention may be practiced otherwise than as specifically described.
Claims
1. 1. A pressure vessel for containing liquids and / or gases under pressure, said pressure vessel comprising: A polymeric liner comprising: a hollow body having a cylindrical wall extending from a first end to an opposite end of the liner, the cylindrical wall having an inner surface and an outer surface, the hollow body having a corrugated section having circumferential corrugations providing alternating ridges and valleys disposed from one end of the corrugated section to an opposite end thereof, each of the corrugations comprising curved peak regions having ridges, curved valleys between adjacent spaced peak regions, and sidewalls joining each successive peak region and valley, the outer periphery of the ridges being curved inwardly and outwardly. a polymeric liner having side surfaces defining an outer diameter (OD) of the corrugated section, a gap between the outer surfaces of adjacent sidewalls defining an annular cavity, a distance between successive ridges defining a period (T) of the corrugation, a distance between the inner and outer surfaces of the liner at the ridges defining a peak wall thickness (Tm), a distance between the inner and outer surfaces of the liner at the midpoints of the valleys defining a valley wall thickness (Tv), and a radial distance between the outer surface at the ridges and the outer surface at the valleys defining an amplitude (A) of the corrugation; an outer synthetic shell comprising a resin and a fiber surrounding an outer periphery of the liner; Equipped with the annular cavity being bounded by an upper surface of the liner forming a sidewall of each of the valleys and a lower surface of the outer synthetic shell; a wall thickness Tm of the peak portion is greater than a wall thickness Tv of the valley portion, and the amplitude A is between about 0.65 times the period T of the corrugation and about 0.75 times the period T; the sidewall begins to be forced into the annular cavity toward the adjacent sidewall until the sidewall contacts the opposing sidewall in response to pressurizing the pressure vessel at a low pressure value. Pressure vessel.
2. The wall thickness Tv of the valley is less than or equal to about 0.27 times the amplitude A of the corrugation.
2. The pressure vessel of claim 1.
3. The wall thickness Tm of the peak portion is about 0.32 times or less than the amplitude A of the corrugation.
3. The pressure vessel of claim 2.
4. the upper surface of the peak region is defined by a radius Rm such that the peak region has a curved upper surface; The curved upper surface of the peak region has a radius Rm between about 0.40 times the period T of the corrugation and about 0.45 times the period T.
4. The pressure vessel of claim 3.
5. the upper surface of the valley is defined by a radius Rv such that the valley has a curved upper surface; 5. The pressure vessel of claim 4.
6. the valley has a flat segment centered at the midpoint of the valley, the flat segment having a width less than or equal to about 0.040 times the period T of the corrugation.
6. The pressure vessel of claim 5.
7. The period T of the corrugation is between about 0.135 times the outer diameter OD of the ridge and about 0.165 times the outer diameter OD of the ridge.
6. The pressure vessel of claim 5.
8. The amplitude A of the corrugations is between about 2.15 mm and about 2.35 mm, an inner diameter defined on the inner surface of the liner at the midpoint of the valley is between about 15.6 mm and about 16.2 mm, and the period T of the corrugations is between about 3.1 mm and about 3.2 mm. and wherein the wall thickness Tv of the valley is at least 0.3 mm, the peak region has an upper surface profile defined by a radius Rm of about 1.3 mm, the valley has an upper surface profile defined by the radius Rv of about 0.16 mm, and the wall thickness Tm of the peak is at least 0.5 mm.
8. The pressure vessel of claim 7.
9. The polymeric liner may include one or more of nylon, ethylene vinyl acetate (EVA), linear low density polyethylene (LLDPE), low density polyethylene (LDPE), high density polyethylene (HDPE), polypropylene (PP), ethylene vinyl alcohol (EVOH), polytetrafluoroethylene (PTFE), polyurethane (PU), and / or polyvinyl chloride (PVC).
9. The pressure vessel of claim 8.
10. 10. The pressure vessel of claim 9, wherein the resin of the outer synthetic shell includes one or more of an epoxy resin, a vinyl ester resin, a thermoplastic resin, a polyester resin, and / or a urethane.
11. The fibers of the outer synthetic shell are one or more of carbon fibers, aramid fibers, polyester fibers, polyethylene fibers, nylon fibers, metal, and / or glass fibers.
11. The pressure vessel of claim 10.
Citation Information
Patent Citations
A sheet of a synthetic resin corrugated pipe -
JP1985143982U
Method and device for manufacturing meandering corrugated material
JP1995001045A
Systems and methods for shape-fitting pressure vessels
JP2018519480A
Systems and methods for braiding liners and applying resins - Patents.com
JP2019507850A
Tank enclosure and tank mount system and method
US20180283610A1