Flip chip bonding structure and substrate thereof
The flip chip bonding structure uses a translucent carrier and support layer to expose shadow projections for inspecting bonding states, addressing the issue of hidden alignment and distortion detection in conventional structures.
Patent Information
- Application Number
- JP2023106199
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-07-08
- Filing Date
- 2023-06-28
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2043-06-28
AI Technical Summary
Conventional flip chip bonding structures shield bumps and circuits between the substrate and the chip, making it impossible to visually inspect the bonding state due to diagonal alignment, hindering the detection of potential misalignment or distortion.
A flip chip bonding structure with a translucent carrier and a support layer that exposes identification bumps and circuits through openings, allowing inspection of bonding states by analyzing shadow projections.
Enables visual inspection of bump and circuit bonding states by exposing shadow projections, ensuring alignment and distortion detection, thereby improving the reliability of the bonding process.
Smart Images

Figure 0007569414000001 
Figure 0007569414000002 
Figure 0007569414000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a flip chip bonding structure, and more particularly to a flip chip bonding structure and a substrate thereof that enable inspection of the bonding state of bumps and circuits. [Background technology]
[0002] In a conventional flip chip bonding structure, a patterned metal layer is applied to the surface of a substrate, and multiple bumps of the chip are bonded to multiple circuits on the patterned metal layer. Summary of the Invention [Problem to be solved by the invention]
[0003] However, in the conventional flip chip bonding technology described above, the bumps and circuits are located between the substrate and the chip and are shielded by the chip and the substrate, so it is not possible to see from the outside of the flip chip bonding structure whether the bumps are bonded to the circuits at an angle.
[0004] Therefore, the present inventors believed that the above-mentioned drawbacks could be improved, and as a result of extensive research, they came to propose the present invention, which effectively improves the above-mentioned problems through rational design.
[0005] The present invention has been made in view of the above, and its object is to provide a flip chip bonding structure and a substrate thereof, which is to say, a support layer is placed on the surface of a transparent carrier, and the shadows of the dummy leads, the identification circuit, and the identification bumps projected on the surface of the transparent carrier are exposed through the openings of the support layer, thereby judging whether the bonding state of the bumps and the patterned metal layer shielded by the support layer and the chip meets the specification. [Means for solving the problem]
[0006] In order to solve the problem, a flip chip bonding structure according to an embodiment of the present invention includes a chip and a substrate, the chip having a plurality of first bumps, a plurality of second bumps, and at least one identification bump, and the substrate includes a light-transmitting carrier, a patterned metal layer, and a support layer. The light-transmitting carrier has a first surface and a second surface, the first surface defines a chip mounting area and a circuit area, and the second surface defines a support area, the support area being located opposite the chip mounting area. The patterned metal layer is disposed in the chip mounting area and the circuit area, the patterned metal layer has a plurality of first circuits, a plurality of second circuits, at least one identification circuit, and a first dummy lead, and the first lead of each of the first circuits, the second lead of each of the second circuits, the identification lead of the identification circuit, and the first dummy lead are located in the chip mounting area. The second lead is adjacent to the first lead, the identification lead is located on a side of the first dummy lead, and the identification lead is projected onto the second surface and forms a lead shadow. The first dummy lead is projected onto the second surface and forms a first measurement shadow. Each of the first bumps is bonded to the first lead of each of the first circuits, each of the second bumps is bonded to the second lead of each of the second circuits, and the identification bump is bonded to the identification lead. The chip shields the first lead, the second lead, the identification lead, the first bump, the second bump, and the identification bump. The identification bump is projected onto the second surface and forms a second measurement shadow, and along the first axis direction, the width of the lead shadow is narrower than the width of the second measurement shadow. The support layer is disposed on the support area, and the support layer shields the shadows of the first lead, the second lead, the first bump, and the second bump projected onto the second surface. The first measurement shadow and the second measurement shadow are exposed from an opening in the support layer, and there is a first distance between the first measurement shadow and the second measurement shadow along the first axis.
[0007] According to one embodiment of the present invention, a substrate with a flip chip bonding structure is provided. That is, one embodiment of the present invention includes the following configuration. The substrate includes a light-transmitting carrier, a patterned metal layer, and a support layer, the light-transmitting carrier having a first surface and a second surface, a chip mounting area and a circuit area defined on the first surface, and a support area defined on the second surface, the support area being located opposite the chip mounting area. The patterned metal layer is disposed on the chip mounting area and the circuit area, the patterned metal layer having a plurality of first circuits, a plurality of second circuits, at least one identification circuit, and a first dummy lead, the first lead of each of the first circuits, the second lead of each of the second circuits, the identification lead of the identification circuit, and the first dummy lead being located on the chip mounting area. The second lead is adjacent to the first lead, the identification lead is located on a side of the first dummy lead, and the identification lead is projected on the second surface and forms a lead shadow. The first dummy lead is projected on the second surface and forms a first measurement shadow. The support layer is placed on the support area, and the support layer blocks shadows projected by the first lead and the second lead onto the second surface, and the lead shadows and the first measurement shadow are exposed from an opening in the support layer. Effect of the Invention
[0008] The present invention determines whether the first and second bumps are displaced or distorted by inspecting the bonding state between the identification bump and the identification circuit through the identification circuit, the dummy lead, and the shadow of the identification bump exposed from the opening. Based on the first distance between the first measurement shadow and the second measurement shadow, it is determined whether the bonding state between the first bump and the first lead, which are shielded by the support layer and the chip, and the bonding state between the second bump and the second lead, which are shielded by the support layer and the chip, meet the specifications.
[0009] Other objects, configurations and effects of the present invention will become apparent from the following detailed description of the preferred embodiments of the present invention. [Brief description of the drawings]
[0010] [Figure 1] 1 is a cross-sectional view showing a flip chip bonding structure according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a bottom view showing a chip of a flip chip bonding structure according to an embodiment of the present invention. [Diagram 3] 1 is a perspective view showing a flip chip bonding structure according to an embodiment of the present invention; [Figure 4] FIG. 2 is a bottom view showing a flip chip bonding structure according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The present invention will be described below through embodiments of the invention, but the embodiments do not limit the scope of the invention according to the claims. Furthermore, not all of the combinations of features described in the embodiments are necessarily essential to the solution of the invention.
[0012] 1 to 4, a flip chip bonding structure and its substrate according to an embodiment of the present invention will be described based on the drawings.
[0013] The flip chip bonding structure 100 according to an embodiment of the present invention includes a chip 110 and a substrate 120. The chip 110 is flip chip bonded to the substrate 120 to form the flip chip bonding structure 100.
[0014] 1 and 2, a chip 110 has a plurality of first bumps 111, a plurality of second bumps 112, and at least one identification bump 113. In this embodiment, the identification bumps 113 are located at the corners of the active surface of the chip 110, but are not limited thereto, and the identification bumps 113 may be function bumps or dummy bumps.
[0015] 1, 3 and 4, the substrate 120 includes a transparent carrier 121, a patterned metal layer 122 and a support layer 123, and the transparent carrier 121 has a first surface 121a and a second surface 121b. A chip mounting area 121c and a circuit area 121d are defined on the first surface 121a, and a support area 121e is defined on the second surface 121b, and the support area 121e is located opposite to the chip mounting area 121c.
[0016] 1 and 3, the patterned metal layer 122 is disposed on the chip mounting area 121c and the circuit area 121d of the first surface 121a, and the patterned metal layer 122 has a plurality of first circuits A, a plurality of second circuits B, at least one identification circuit C, and a first dummy lead D. The first lead A1 of each first circuit A, the second lead B1 of each second circuit B, the identification lead C1 of the identification circuit C, and the first dummy lead D are located in the chip mounting area 121c, and the second lead B1 of each second circuit B is adjacent to the first lead A1 of each first circuit A. In this embodiment, each second lead B1 is located between two first leads A1, and in another embodiment, each first lead A1 is located between two second leads B1. The identification lead C1 is located on the side of the first dummy lead D, and in this embodiment, the patterned metal layer 122 further has a second dummy lead E. The second dummy lead E is located in the chip mounting area 121c, and the identification lead C1 is located between the first dummy lead D and the second dummy lead E.
[0017] 3, in this embodiment, there is a third spacing S3 between adjacent first lead A1 and second lead B1, and a fourth spacing S4 between the identification lead C1 and the adjacent first lead A1 or second lead B1, the fourth spacing S4 being larger than the third spacing S3. In this embodiment, there is a fifth spacing S5 between the identification lead C1 and the first dummy lead D, and there is a sixth spacing S6 between the identification lead C1 and the second dummy lead E, the fifth spacing S5 and the sixth spacing S6 being equal to the third spacing S3. In other embodiments, the fifth spacing S5 and the sixth spacing S6 are larger or smaller than the third spacing S3.
[0018] Referring to Figures 3 and 4, the identification lead C1 is projected onto the second surface 121b and forms a lead shadow F, the first dummy lead D is projected onto the second surface 121b and forms a first measurement shadow G, and the second dummy lead E is projected onto the second surface 121b and forms a third measurement shadow I.
[0019] 1, 3 and 4, the first bump 111 is bonded to the first lead A1, the second bump 112 is bonded to the second lead B1, and the identification bump 113 is bonded to the identification lead C1. In this embodiment, each first bump 111 is bonded to the first joint A2 of each first lead A1, each second bump 112 is bonded to the second joint B2 of each second lead B1, and the identification bump 113 is bonded to the third joint C2 of the identification lead C1. The first axis X1 passes through the first joint A2 of each first lead A1 and the third joint C2 of the identification lead C1, the second axis X2 passes through the second joint B2 of each second lead B1, and the second axis X2 is parallel to the first axis X1.
[0020] Returning to Figures 3 and 4, the identification bump 113 joined to the identification lead C1 is projected onto the second surface 121b and forms a second measurement shadow H, and along the first axis X1 direction, the width of the lead shadow F is narrower than the width of the second measurement shadow H.
[0021] 1 and 4, the support layer 123 is disposed at least on the support area 121e of the second surface 121b, and the support layer 123 is a patterned metal layer having functionality. A connection via hole (not shown) provided in the transparent carrier 121 is electrically connected to the patterned metal layer 122 located on the first surface 121a, so that the support layer 123 has functionality and the support layer 123 increases the pressure resistance and warpage resistance of the transparent carrier 121.
[0022] 1, 3 and 4, when the chip 110 is bonded to the metal layer 122 patterned with the first bump 111, the second bump 112, and the identification bump 113, the chip 110 shields the first lead A1, the second lead B1, the identification lead C1, the first bump 111, the second bump 112, and the identification bump 113. The support layer 123 shields the shadows projected by the first lead A1, the second lead B1, the first bump 111, and the second bump 112 onto the second surface 121b.
[0023] 1 and 4, the support layer 123 has an opening 123a, through which a lead shadow F, a first measurement shadow G, and a second measurement shadow H are exposed. In this embodiment, a third measurement shadow I is also exposed through the opening 123a. By inspecting whether or not there is any misalignment between the lead shadow F of the identification lead C1 and the second measurement shadow H of the identification bump 113 through the opening 123a, it is determined whether or not the first bump 111 bonded to the first lead A1 and the second bump 112 bonded to the second lead B1 are shifted or distorted.
[0024] 3 and 4, preferably, a first distance S1 between the first measurement shadow G and the second measurement shadow H is measured along the first axis X1 direction, and a second distance S2 between the third measurement shadow I and the second measurement shadow H is measured. Based on the first distance S1 and the second distance S2, it is determined whether the deviation or distortion amount of the first bump 111 bonded to the first lead A1 and the second bump 112 bonded to the second lead B1 conforms to the specification.
[0025] As described above, the present invention is not limited to the above-described embodiment, and can be embodied in various forms without departing from the spirit and scope of the present invention. [Explanation of symbols]
[0026] 100 Flip chip bonding structure 110 Chips 111 First Bump 112 2nd Bump 113 Identification Bump 120 Substrate 121 Translucent carrier 121a 1st page 121b 2nd side 121c Chip mounting area 121d Circuit Area 121e Support Area 122 Patterned Metal Layer 123 Supporter layer 123a opening A 1st circuit A1 1st lead A2 1st joint B 2nd circuit B1 2nd lead B2 2nd joint C identification circuit C1 Identification Lead C2 3rd joint D First dummy lead E Second dummy lead F Lead Shadow G First measurement shadow H 2nd measurement shadow I 3rd measurement shadow S1 First interval S2 2nd interval S3 Third interval S4 Fourth interval S5 5th interval S6 6th interval X1 1st axis X2 2nd axis
Claims
1. 1. A flip chip bonding structure comprising: a chip having a plurality of first bumps, a plurality of second bumps, and at least one identification bump; and a substrate, The substrate is an optically transparent carrier having a first surface and a second surface, the first surface defining a chip mounting area and a circuit area, and the second surface defining a support area, the support area being positioned opposite the chip mounting area; a patterned metal layer disposed on the chip mounting area and the circuit area, the patterned metal layer having a plurality of first circuits, a plurality of second circuits, at least one identification circuit, and a first dummy lead, a first lead of each of the first circuits, a second lead of each of the second circuits, an identification lead of the identification circuit, and the first dummy lead are located on the chip mounting area, the second leads are adjacent to the first leads, the identification leads are located on the sides of the first dummy leads, the identification leads are projected onto the second surface and form lead shadows, and the first dummy leads are projected onto the second surface. the patterned metal layer being shadowed on the second surface and forming a first measurement shadow, each of the first bumps being bonded to the first lead of each of the first circuits, each of the second bumps being bonded to the second lead of each of the second circuits, the identification bumps being bonded to the identification leads, the chip shielding the first leads, the second leads, the identification leads, the first bumps, the second bumps, and the identification bumps, the identification bumps being projected on the second surface and forming a second measurement shadow, and a width of the lead shadows is narrower than a width of the second measurement shadow along a first axis direction; a support layer disposed in the support area, the support layer shielding shadows projected by the first lead, the second lead, the first bump, and the second bump on the second surface, the first measurement shadow and the second measurement shadow being exposed from an opening, and the support layer having a first interval between the first measurement shadow and the second measurement shadow along the first axial direction.
2. 2. The flip chip bonding structure of claim 1, wherein the patterned metal layer further comprises a second dummy lead, the second dummy lead is located in the chip mounting area, the identification lead is located between the first dummy lead and the second dummy lead, the second dummy lead is projected onto the second surface and forms a third measurement shadow, the third measurement shadow is exposed from the opening, and there is a second distance between the third measurement shadow and the second measurement shadow along the first axial direction.
3. 3. The flip chip bonding structure of claim 2, wherein each of the first bumps is bonded to a first joint of the first lead in each of the first circuits, each of the second bumps is bonded to a second joint of the second lead in each of the second circuits, and the identification bump is bonded to a third joint of the identification lead, the first axis passing through the first joint and the third joint, the second axis passing through the second joint, and the second axis being parallel to the first axis.
4. 4. The flip chip bonding structure of claim 1, wherein there is a third spacing between adjacent first leads and adjacent second leads, and a fourth spacing between the identification lead and an adjacent first lead or adjacent second lead, the fourth spacing being greater than the third spacing.
5. 5. The flip chip bonding structure of claim 4, wherein there is a fifth spacing between the identification lead and the first dummy lead, the fifth spacing being equal to the third spacing.
6. 3. The flip chip bonding structure of claim 2, wherein a third spacing is provided between adjacent first and second leads, a fourth spacing is provided between the identification lead and the adjacent first or second lead, the fourth spacing being greater than the third spacing, a fifth spacing is provided between the identification lead and the first dummy lead, and a sixth spacing is provided between the identification lead and the second dummy lead, the fifth spacing and the sixth spacing being equal to the third spacing.
7. an optically transparent carrier having a first surface and a second surface, the first surface defining a chip mounting area and a circuit area, and the second surface defining a support area, the support area being positioned opposite the chip mounting area; a patterned metal layer disposed on the chip mounting area and the circuit area, the patterned metal layer having a plurality of first circuits, a plurality of second circuits, at least one identification circuit, and a first dummy lead, wherein a first lead of each of the first circuits, a second lead of each of the second circuits, an identification lead of the identification circuit, and the first dummy lead are located on the chip mounting area, the second leads are adjacent to the first leads, the identification leads are located on a side of the first dummy leads, the identification leads are projected onto the second surface and form a lead shadow, and the first dummy lead is projected onto the second surface and form a first measurement shadow; A substrate having a flip chip bonding structure, comprising: a support layer disposed in the support area, the support layer shielding shadows projected by the first lead and the second lead onto the second surface, and an opening from which the lead shadows and the first measurement shadow are exposed.
8. 8. The substrate of claim 7, wherein the patterned metal layer further comprises a second dummy lead, the second dummy lead being located in the chip mounting area, the identification lead being located between the first dummy lead and the second dummy lead, the second dummy lead being projected onto the second surface and forming a third measurement shadow, and the third measurement shadow being exposed from the opening.
9. 9. A substrate with a flip chip bonding structure as described in claim 7 or 8, characterized in that there is a third spacing between adjacent first leads and second leads, and a fourth spacing between the identification lead and the adjacent first lead or second lead, the fourth spacing being greater than the third spacing.
10. 10. The substrate of claim 9, further comprising a fifth spacing between the identification lead and the first dummy lead, the fifth spacing being equal to the third spacing.
11. 9. The substrate of claim 8, wherein the substrate has a third spacing between adjacent first leads and adjacent second leads, a fourth spacing between the identification lead and the adjacent first lead or the adjacent second lead, the fourth spacing being greater than the third spacing, a fifth spacing between the identification lead and the first dummy lead, and a sixth spacing between the identification lead and the second dummy lead, the fifth spacing and the sixth spacing being equal to the third spacing.
Citation Information
Patent Citations
Liquid crystal display device
JP2000235191A
Connection structure of electronic component and connection inspecting method thereof
JP2008141022A
Display device
JP2017181984A
COG panel, organic el panel, and manufacturing method of COG panel
JP2018032584A
Display device
US20170287939A1