Radiation Therapy Bolus Material
A self-healing polymer bolus material with a crosslinkable structure and laminated thermoplastic elastomer allows for reusable radiation therapy applications by rejoining cut pieces and preventing drying, addressing the reusability and waste issues of conventional materials.
Patent Information
- Application Number
- JP2020206421
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-12-14
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-12-14
AI Technical Summary
Existing bolus materials for radiation therapy are difficult to reuse due to their flexibility and low strength, leading to waste generation from cut sheets.
A self-healing polymer bolus material with a crosslinkable structure impregnated by a highly hydrophilic solvent, allowing cut pieces to rejoin and integrate, and a laminated structure with a styrene-based thermoplastic elastomer to prevent drying, enabling reuse.
The self-healing polymer bolus material can be repeatedly used by rejoining cut pieces and maintaining functionality through laminating with a non-water permeable elastomer, reducing waste and extending its usable life.
Smart Images

Figure 0007570629000001 
Figure 0007570629000002 
Figure 0007570629000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a bolus material for use in radiation therapy. [Background technology]
[0002] When performing radiation therapy on cancer tissue or the like inside the human body by irradiating the human body with radiation, it is desirable to concentrate the radiation on the affected area and to avoid exposing healthy tissue other than the affected area to radiation as much as possible.
[0003] Therefore, as shown in Patent Documents 1 to 3, a resin material called a bolus material is attached to the surface of the human body to adjust the position of the peak point of the radiation energy to match the depth of the affected area. Patent Document 1 discloses a bolus material made of an aqueous gel, Patent Document 2 discloses a polyurethane-based bolus material, and Patent Document 3 discloses a silicone rubber-based bolus material.
[0004] In addition to the characteristics of having a specific gravity close to that of the human body, not impeding the permeability of radiation, and being transparent, radiotherapy bolus materials are required to be flexible and adhere easily to the human body. However, flexible soft materials have low strength, making them difficult to reuse. In addition, radiotherapy bolus materials are often used in sheet form, cut according to the shape of the radiation site, but the remaining parts of the cut sheets are usually discarded. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Publication No. 62-204770 [Patent Document 2] JP 2018-76478 A [Patent Document 3] Japanese Patent Application Publication No. 11-221294 Summary of the Invention [Problem to be solved by the invention]
[0006] SUMMARY OF THE PRESENT EMBODIMENT An object of the present invention is to solve the above-mentioned problems of the conventional technology and to provide a reusable bolus material for radiotherapy. [Means for solving the problem]
[0007] The bolus material for radiotherapy of the present invention, which has been made to solve the above problems, is made of a self-repairing polymer in which a highly hydrophilic solvent is contained in a crosslinked structure in which a host group and a guest group are crosslinked by interaction. The cut pieces are rejoined to each other and are tightly integrated to form a bolus material for radiotherapy having a larger volume than the cut pieces. The present invention is characterized in that: The present invention also provides a method for using the bolus material for radiotherapy, which comprises contacting at least two or more sheets of the bolus material for radiotherapy with each other to form a bolus material for radiotherapy having a larger volume than the original bolus material for radiotherapy.
[0008] Also, The self-repairing polymer is characterized by a crosslinked structure in which a host group and a guest group are crosslinked by interaction, and is made by incorporating a highly hydrophilic solvent. The bolus material for radiation therapy can be constructed by laminating a styrene-based thermoplastic elastomer with polystyrene as the hard segment and polyethylene / polybutylene as the soft segment. Effect of the Invention
[0009] The bolus material for radiotherapy is often used in the form of a sheet that is cut to fit the shape of the surface of the human body at the radiation site, but the bolus material for radiotherapy of the present invention is made of a self-repairing polymer and has self-repairing properties, so if the cut pieces are overlapped, they will rejoin and become one piece. This allows it to be used repeatedly. In addition, this type of self-repairing polymer loses its self-repairing properties when it dries, but by laminating it with a sheet of a soft and water-impermeable thermoplastic elastomer, it is possible to prevent drying without impairing its function as a bolus material. This allows it to be reused for a longer period of time. [Brief description of the drawings]
[0010] [Figure 1] FIG. 2 is a diagram illustrating the principle of the bolus material. [Diagram 2] FIG. 1 is a diagram illustrating the principle of a self-repairing polymer. [Diagram 3] FIG. 11 is a cross-sectional view showing an embodiment having a laminated structure. [Figure 4] FIG. 11 is a cross-sectional view showing another embodiment of a laminate structure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Figure 1 shows the principle of bolus material for radiation therapy. For example, when the depth from the surface 10 of the human body to the affected tissue 11 is d, if radiation is applied as shown in Fig. 1(A), the position of the peak point P of the radiation dose will be Δd lower than d as shown in the graph on the right, and the radiation dose may not be maximum in the affected tissue 11. In such a case, as shown in Fig. 1(B), if a bolus material 12 for radiotherapy with a thickness Δd and radiation permeability equivalent to that of the human body is brought into close contact with the surface 10 of the human body, the position of the peak point P with the maximum dose will shift upward by Δd, and the radiation dose can be maximized in the affected tissue 11.
[0012] The bolus material for radiotherapy of the present invention will be described below.
[0013] The bolus material for radiotherapy of the present invention is made of a self-repairing polymer in which a highly hydrophilic solvent is impregnated in a crosslinked structure in which a host group and a guest group are crosslinked by interaction. As conceptually shown in Figure 2, this self-repairing polymer is a crosslinked structure in which a host group having a host molecule 20 in its side chain is crosslinked with a guest molecule group having a guest molecule 21 in its side chain. This self-repairing polymer itself is sold as a self-repairing gel by Yushiro Chemical Industry Co., Ltd., and an overview of this is provided below.
[0014] The host molecule 20 is, for example, cyclodextrin. Cyclodextrin is a cyclic oligosaccharide with a donut-shaped molecular structure, and has the property of encapsulating a guest molecule 21 of a suitable size inside this ring. Known cyclodextrins include α-cyclodextrin with six glucose residues, β-cyclodextrin with seven glucose residues, and γ-cyclodextrin with eight glucose residues, and any of them can be used.
[0015] The guest molecule 21 is a chain or cyclic alkyl compound or a derivative thereof having 4 to 18 carbon atoms. Examples of the alkyl compound having 4 to 18 carbon atoms include butane, pentane, hexane, heptane, octane, nonane, decane, undecane, dodecane, tetradecane, pentadecane, hexadecane, octadecane, and adamantane.
[0016] A bond is formed between the host molecule 20 and the guest molecule 21 by interaction, and a crosslinked structure is formed with the bond as a crosslinking point. Examples of the interaction include hydrophobic interaction, hydrogen bond, intermolecular force, electrostatic interaction, coordinate bond, etc. between the host molecule 20 and the guest molecule 21, but are not limited to these.
[0017] The most preferable combinations of the host molecule 20 and the guest molecule 21 are α-cyclodextrin and an n-dodecyl group, and β-cyclodextrin and an adamantyl group. This is because the closer the size of the guest molecule 21 and the size of the internal cavity of the host molecule 20 are, the stronger the inclusion force becomes.
[0018] Examples of monomers having a host molecule in their molecular structure include 6-(meth)acrylamide-α-cyclodextrin, 6-(meth)acrylamide-β-cyclodextrin, α-cyclodextrin methacrylate, β-cyclodextrin methacrylate, α-cyclodextrin acrylate, and β-cyclodextrin acrylate.
[0019] Examples of monomers having a guest molecule in their molecular structure include n-butyl (meth)acrylate, t-butyl (meth)acrylate, 1-acrylamidodamantane, N-(1-adamantyl)(meth)acrylamide, N-benzyl(meth)acrylamide, and N-1-naphthylmethyl(meth)acrylamide.
[0020] The crosslinked structure described above contains a highly hydrophilic solvent. This is because the self-repairing polymer dries up when water evaporates, and the self-repairing function that occurs in the hydrogel state decreases. Examples of this highly hydrophilic solvent include ethylene glycol, diethylene glycol, propylene glycol, dipropylene glycol, polyethylene glycol, polypropylene glycol, glycerin, and diethylene glycol monoethyl ether. This makes it difficult for the polymer to dry out even over time or when the temperature environment changes, so that the self-repairing function can be maintained stably for a long period of time.
[0021] Such a self-repairing polymer can be produced by mixing a monomer having a host molecule in its molecular structure, a monomer having a guest molecule in its molecular structure, a monomer not including a host molecule or a guest molecule, a highly hydrophilic solvent as an anti-drying liquid, and a polymerization initiator, and polymerizing them at room temperature. The monomers can be mixed together to prepare an aqueous monomer solution. The amount of the aqueous monomer solution added is preferably 30% by weight to 70% by weight. The amount of the anti-drying agent added is preferably 20% to 40%. Furthermore, the amount of the polymerization initiator is preferably 1% to 10%.
[0022] Examples of the polymerization initiator include ammonium persulfate, azobisisobutylnitrile, 2,2'-azobis[2-(2-imidazolin-2-yl)propane]dihydrochloride, etc., but are not limited thereto. Various polymerization initiators such as benzoyl peroxide and photopolymerization initiators can be used.
[0023] This self-repairing polymer contains host molecules 20 and guest molecules 21 inside, and even if it is cut, the host molecules 20 exposed at the interface encapsulate the guest molecules 21 to form crosslinks again, repairing the cut surface. This self-repairing function occurs in a swollen state, and its function decreases in a dry state, but by including a highly hydrophilic solvent, a stable self-repairing function can be obtained. It has been confirmed that the gel strength of the self-repaired part after cutting reaches 85% of that before cutting.
[0024] The bolus material for radiotherapy of the present invention is made of the above-mentioned self-repairing polymer, and is often formed into a sheet for use. For example, by varying the thickness of the sheets in 1 mm increments and stacking the required number of sheets according to the depth of the affected area, the sheets will adhere to each other and can be used as a bolus material for radiotherapy of the required thickness. Even if the sheet is cut according to the condition of the affected area, if the cut pieces are collected, they can be adhered to each other and integrated, and can be used again. Therefore, there is no waste as with conventional bolus materials for radiotherapy.
[0025] As described above, the self-repairing polymer can be used alone as a bolus material for radiotherapy, but it can also be used by laminating a sheet 22 of the self-repairing polymer and a sheet 23 of a styrene-based thermoplastic elastomer as shown in Fig. 3. Fig. 3 shows a bolus material for radiotherapy in which these two types of sheets 22 and 23 are alternately laminated.
[0026] As a styrene-based thermoplastic elastomer with polystyrene as the hard segment, one that is soft, impermeable, and has a specific gravity of less than 1 is preferable, and in this embodiment, a thermoplastic elastomer with polystyrene as the hard segment and polyethylene-polybutylene as the soft segment was used. This is a material called SEBS (styrene-ethylene-butylene-styrene), obtained by hydrogenating a polystyrene-polybutadiene-polystyrene block copolymer.
[0027] Other examples of styrene-based block-type thermoplastic elastomers with polystyrene as hard segments include styrene-ethylene block copolymers, styrene-ethylene-butadiene block copolymers, styrene-butadiene block copolymers, styrene-butadiene block copolymers, and styrene-isoprene block copolymers. and othersHowever, from the viewpoints of being easily deformed to conform to the contours of the human body, being easily fitted to the human body with an appropriate degree of adhesion, and being strong and resistant to damage, SEBS (styrene-ethylene-butylene-styrene) obtained by hydrogenating a polystyrene-polybutadiene-polystyrene block copolymer is preferred.
[0028] This styrene-based thermoplastic elastomer has excellent rubber elasticity close to that of cross-linked rubber at room temperature, so it can easily be made to adhere to the irregularities of the human body. Moreover, when heated to 140-230°C, it exhibits fluidity and can be molded in the same way as general resins. It also has excellent transparency, and has a tensile strength of 1.3 MPa according to the JIS K 6251 test method, which is sufficient strength. This styrene-based thermoplastic elastomer material itself is an existing product, and is commercially available, for example, from Aronkasei Co., Ltd.
[0029] From the viewpoint of radiation permeability, it is preferable that the specific gravity of the radiotherapy bolus material is as close as possible to the specific gravity of the human body (1.0). The specific gravity of the above-mentioned self-repairing polymer is 1.25, which is slightly above the preferred range. In contrast, the specific gravity of the above-mentioned styrene-based thermoplastic elastomer is 0.86. Therefore, by laminating them alternately, the overall specific gravity can be brought closer to 1.0, making it possible to prevent deterioration of radiation permeability due to the difference in specific gravity with the human body. In addition, since the styrene-based thermoplastic elastomer is not permeable to water, laminating it with the self-repairing polymer has the effect of reliably preventing the self-repairing polymer from drying out.
[0030] Furthermore, as shown in FIG. 4, if a laminate structure is formed in which thermoplastic elastomer sheets 23 are disposed on both the top and bottom of a sheet 22 of a self-repairing polymer, the self-repairing polymer can be more reliably prevented from drying out. EXAMPLES
[0031] A 60% by weight aqueous monomer solution, available from Yushiro Chemical Industry Co., Ltd. under the trade name "Wizard Monomer," was mixed with 35% by weight of an anti-drying liquid, and then 5% by weight of an aqueous polymerization initiator solution was added and stirred, and the mixture was poured into a mold to form a sheet. The aqueous monomer solution was a mixture of a host group-containing polymerizable polymer, a guest group-containing polymerizable monomer, and a polymerizable monomer. The host group-containing polymerizable polymer was acrylamide-cyclodextrin, the guest group-containing polymerizable monomer was N-(1-adamantyl)acrylamide, and the polymerizable monomer was 4-hydroxybutyl acrylate. The anti-drying liquid was a water-soluble alcohol, and the polymerization initiator was ammonium persulfate. The mixture hardened in about 20 minutes at room temperature and was peeled off from the mold to form a sheet-shaped bolus material for radiation therapy. Its specific gravity was 1.25, and it had excellent adhesion and transparency. The cut pieces of the sheet were collected and left in the air at room temperature, and they were fused together and integrated within 24 hours.
[0032] Next, a sheet was made from styrene-based thermoplastic elastomer pellets (SEBS) sold by Aronkasei Co., Ltd. The sheet was made by molding the pellet-shaped resin with a roll heated to 150℃ to 190℃. The sheet made was layered alternately with a sheet of self-repairing resin to make a bolus material for radiation therapy consisting of a total of six sheets. The overall specific gravity was 1.0, and it also had excellent adhesion and transparency. There are many possible forms for the layering, such as varying the thickness of each layer.
[0033] As explained above, the bolus material for radiotherapy of the present invention has self-repairing properties and can be used repeatedly. In addition, by laminating it with a sheet of soft and water-impermeable thermoplastic elastomer, it is possible to prevent drying and reuse it for a longer period of time. [Explanation of symbols]
[0034] 10 Human body surface 11 Affected tissue 12 Bolus material for radiotherapy 20 Host Molecules 21 Guest molecules 22 Self-healing polymer sheet 23 Thermoplastic elastomer sheet P Peak radiation dose
Claims
1. A bolus material for radiation therapy comprising a self-repairing polymer containing a highly hydrophilic solvent in a crosslinked structure in which a host group and a guest group are crosslinked by interaction, characterized in that the cut pieces can be rejoined to form a bolus material for radiation therapy having a larger volume than the cut pieces by tightly bonding the cut pieces together.
2. A method for using a radiotherapy bolus material, comprising contacting at least two or more sheets of the radiotherapy bolus material described in claim 1 with each other to form a radiotherapy bolus material having a larger volume than the original radiotherapy bolus material.
3. A bolus material for radiation therapy, characterized in that it is made of a self-healing polymer containing a highly hydrophilic solvent and a cross-linked structure in which host groups and guest groups are cross-linked by interaction, and is laminated with a styrene-based thermoplastic elastomer having polystyrene as a hard segment.
Citation Information
Patent Citations
Bolus for radiation therapy
JP1987204770A
Manufacture of silicone bolus for radiotherapy
JP1999221294A
Flexible composite sheet
JP2014041040A
Self-repairing material and production method of the same
JP2017071710A
Method for producing bolus and bolus
JP2018076478A