Complex for reducing noise

Thermoplastic polymer-wollastonite and elastomer-wollastonite composites address noise reduction challenges by utilizing wollastonite's properties to enhance noise damping and mechanical stability, offering effective noise-reducing articles for devices.

JP7573442B2Active Publication Date: 2024-10-25IMERYS USA INC
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020555824
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-04-13
Filing Date
2019-04-11
Publication Date
2024-10-25
Estimated Expiration
2039-04-11

AI Technical Summary

Technical Problem

Existing materials fail to effectively reduce noise emitted by electrical devices across various frequencies and temperatures while maintaining precise physical properties, making it challenging to address noise pollution in open living spaces.

Method used

Thermoplastic polymer-wollastonite and thermoplastic elastomer-wollastonite composites are used to dampen noise through absorption and barrier treatments, utilizing wollastonite's specific particle size, aspect ratio, and BET surface area to enhance noise reduction and mechanical properties.

Benefits of technology

The composites provide significant noise reduction, improved mechanical properties, and thermal stability, suitable for manufacturing noise-reducing articles like panels for devices, demonstrating superior performance in sound transmission loss, damping, and vibration isolation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573442000004
    Figure 0007573442000004
  • Figure 0007573442000005
    Figure 0007573442000005
  • Figure 0007573442000006
    Figure 0007573442000006
Patent Text Reader

Abstract

The present invention relates to the use of thermoplastic polymer-wollastonite composites and / or thermoplastic elastomer-wollastonite composites for reducing noise. The present invention also relates to articles comprising the thermoplastic polymer-wollastonite composites and / or thermoplastic elastomer-wollastonite composites, methods for making articles according to the invention, and devices comprising articles according to the invention.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Priority claim This PCT international application claims the benefit of priority to U.S. Provisional Patent Application No. 62 / 657,226, filed April 13, 2018, the contents of which are incorporated herein by reference in their entirety. The present invention generally relates to the use of thermoplastic polymer-wollastonite and / or thermoplastic elastomer-wollastonite composites for reducing noise. The present invention further relates to articles comprising thermoplastic polymer-wollastonite and / or thermoplastic elastomer-wollastonite composites, methods of making articles according to the invention, and devices comprising articles according to the invention. [Background technology]

[0002] Many electrical devices, including household devices such as washing machines, tumble dryers, vacuum cleaners, and air conditioning units, emit noise. Loud and / or prolonged exposure to noise can be harmful to hearing and can also disrupt sleep and / or cause stress. There remains a need to find materials that silence the noise emitted by such devices or shield this noise from the human ear. Reducing device noise is particularly relevant with the trend toward more open living spaces. There are many challenges in developing materials that can be used for noise reduction. Such materials are required to meet a wide range of requirements. In particular, suitable materials may be required to reduce noise across different frequencies and temperatures while having precise physical properties to match the device that produces the noise. It would be desirable to provide alternative or improved materials for noise reduction that meet one or more of these requirements. Summary of the Invention

[0003] The invention is defined in the appended claims. According to a first aspect, there is provided the use of a thermoplastic polymer-wollastonite composite and / or a thermoplastic elastomer-wollastonite composite for reducing noise. According to a second aspect there is provided a thermoplastic polymer-wollastonite composite and / or a thermoplastic elastomer-wollastonite for use as a noise reducing material. According to a third aspect, there is provided an article comprising a thermoplastic polymer-wollastonite composite and / or a thermoplastic elastomer-wollastonite according to the second aspect. According to a fourth aspect there is provided a method of producing an article according to the third aspect by extrusion, injection moulding and / or thermoforming. According to a fifth aspect there is provided a method of reducing noise comprising use according to the first aspect. According to a sixth aspect there is provided an apparatus comprising an article according to the third aspect.

[0004] Certain embodiments of the invention may provide one or more of the following advantages: Desired noise reduction; Desired noise isolation; desired mechanical properties; desired thermal properties; desired rheological properties; desired density; Desired mold shrinkage; The desired cost. The details, examples and preferences provided with respect to one or more particular aspects of the invention described above apply equally to all aspects of the invention. Any combination of the embodiments, examples and preferences described herein in all possible variations thereof is encompassed by the invention, unless otherwise indicated herein or clearly contradicted by context. The invention is further illustrated with reference to the following figures. [Brief description of the drawings]

[0005] [Figure 1]FIG. 2 depicts sound transmission loss results for Composition A and Composition B. [Diagram 2] FIG. 2 is a graph depicting the tan δ results for Composition A and Composition B. [Diagram 3] FIG. 1 depicts composite loss factor results for Composition A and Composition B. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0006] It will be understood that the following description and references to the figures are directed to exemplary embodiments of the invention and should not be construed as limiting the scope of the claims. The present invention is based on the surprising discovery that thermoplastic polymer-wollastonite composites and / or thermoplastic elastomer-wollastonite composites are effective as noise reducing agents. Wollastonite is an industrial mineral that chemically contains calcium, silicon and oxygen. Its molecular formula is CaSiO3 and its theoretical composition consists of 48.28% CaO and 51.72% SiO2. Natural wollastonite may also contain trace or small amounts of various metal ions such as aluminum, iron, magnesium, potassium and sodium.

[0007] Wollastonite disclosed herein has a particle size. Particle size may be measured by any suitable measurement technique now known or hereafter discovered to one of skill in the art. Unless otherwise specified, particle size and particle size characteristics such as particle size distribution ("psd") are measured using a Leeds and Northrup Microtrac X100 laser particle size analyzer (Leeds and Northrup, North Wales, PA, USA) capable of determining particle size distribution over a particle size range of 0.12 μm to 704 μm. The size of a given particle is expressed in terms of the diameter of a sphere of equivalent diameter settling through a suspension, also known as the equivalent spherical diameter or "esd". The median particle size, i.e., d 50The value is the value when 50% of the particles are 50 The value has an ESD less than the value d. 10 The value is the d 10 The value has an ESD less than the value d. 90 The value is the value when 90% of the particles are 90 The value has an ESD less than the value. In one embodiment, the wollastonite has an average particle size d of about 1 μm to about 90 μm, or about 3 μm to about 85 μm, or about 5 μm to about 80 μm, or about 8 μm to about 75 μm, or about 10 μm to about 70 μm, or about 12 μm to about 65 μm, or about 15 μm to about 60 μm, or about 17 μm to about 55 μm, or about 20 μm to about 50 μm, or about 23 μm to about 45 μm, or about 25 μm to about 40 μm, or about 30 μm to about 35 μm. 50 has.

[0008] The morphology of wollastonite according to some embodiments can be characterized by its aspect ratio. The aspect ratio of a particle generally refers to the ratio of the length to the width of the particle. For a given sample of particles, the aspect ratio can be determined as an average. For example, the aspect ratio of wollastonite particles according to some embodiments can be determined by first depositing a slurry containing a sample of wollastonite particles on the stage of a standard SEM and coating the dried slurry with platinum. Images of the particles are then obtained and the dimensions of the particles can be determined, for example, using computer-based analysis, where the thickness and width of the particles are assumed to be equal. The aspect ratio can then be determined by averaging many calculations (e.g., 50 calculations) of the aspect ratio of the length to the width of individual particles. Other methods of determining the aspect ratio are also contemplated. In some embodiments, the wollastonite particles can have an aspect ratio of at least 2: 1. For example, the wollastonite particles may have an aspect ratio of at least 3: 1, an aspect ratio of at least 4: 1, an aspect ratio of at least 7: 1, an aspect ratio of at least 12: 1, an aspect ratio of at least 15: 1, or an aspect ratio of at least 20: 1.

[0009] In some embodiments of the method, the wollastonite particles can have a median plate thickness value of less than or equal to about 2 μm, for example, less than or equal to about 1 μm. According to some embodiments, the wollastonite can have a median plate thickness value in the range of about 3 to about 70 μm, or about 4 to about 60 μm, or about 5 to about 50 μm, or about 6 to about 40 μm, or about 7 to about 30 μm, or about 8 to about 20 μm, or about 9 to about 15 μm. The median plate thickness value can be measured using a Leeds and Northrup Microtrac X100 laser particle size analyzer (Leeds and Northrup, North Wales, PA, USA). The surface area of ​​the minerals is measured using the BET method by the amount of nitrogen adsorbed on the surface of the particle so as to form a monolayer completely covering the surface (BET method, measured according to AFNOR standards X11-621 and 622 or ISO 9277).

[0010] In one embodiment, the BET surface area is from about 0.2 to about 5.0 m 2 / g, or about 0.4 to about 4.8 m 2 / g, or about 0.6 to about 4.6 m 2 / g, or about 0.8 to about 4.4 m 2 / g, or about 0.6 to about 4.2 m 2 / g, or about 1.0 to about 4.0 m 2 / g, or about 1.2 to about 3.8 m 2 / g, or about 1.4 to about 3.6 m 2 / g, or about 1.6 to about 3.0 m 2 / g, or about 1.7 to about 2.7 m 2 / g, or about 1.8 to about 2.5 m 2 / g, or about 1.9 to about 2.2 m 2 / g. Thermoplastic polymers according to the present invention are a type of plastic that changes its properties when heated and cooled. Thermoplastic polymers are composed of long unlinked polymer molecules and can generally have high molecular weights. They soften and melt when heated, while they harden when cooled. This property allows thermoplastics to be remolded and recycled without adversely affecting the physical properties of the material.

[0011] As used in this specification and the appended claims, the singular forms "a," "and," and "the" include plural referents unless the context clearly dictates otherwise. For example, "a thermoplastic polymer," "the thermoplastic polymer," and "thermoplastic polymer" can refer to a polymer that includes two or more thermoplastic polymers. Similarly, "a thermoplastic elastomer," "the thermoplastic elastomer," and "thermoplastic elastomer" can refer to a polymer that includes two or more thermoplastic elastomers.

[0012] Examples of thermoplastic polymers include, but are not limited to, polypropylene, polyethylene, polystyrene, polyvinyl chloride, acrylics, polyamides, polycarbonates, poly(methyl methacrylate), acrylonitrile-butadiene-styrene, thermoplastic starch, and combinations thereof. In an embodiment, the thermoplastic polymer may be selected from polypropylene, polyamides, polycarbonates, or combinations thereof. In an embodiment, the thermoplastic polymer according to the present invention is a recycled thermoplastic polymer, such as a recycled polymer of polyethylene or polypropylene. In an embodiment, the thermoplastic polymer according to the present invention is a partially recycled thermoplastic polymer.

[0013] Thermoplastic elastomers exhibit both thermoplastic and elastomeric properties. Thermoplastic elastomers may be selected from thermoplastic polyurethanes, thermoplastic vulcanizates, thermoplastic olefins, thermoplastic polyamides, thermoplastic styrenics, thermoplastic copolyesters, and combinations thereof. In an embodiment, the thermoplastic elastomer according to the present invention is a recycled thermoplastic elastomer. In an embodiment, the thermoplastic elastomer according to the present invention is a partially recycled thermoplastic elastomer. Thermosetting polymers, including thermosetting elastomers, retain their shape and strength when heated. Thermosetting polymers may be selected from epoxy resins, polyesters, phenol formaldehyde, urea formaldehyde, melamine formaldehyde, polyimides, polyisocyanurates, vinyl esters. Thermosetting elastomers may be selected from styrene-butadiene rubber, nitrile rubber, butyl rubber, polybutadiene, polyisoprene, ethylene propylene or ethylene propylene diene (EPDM), silicones, or combinations thereof.

[0014] In some embodiments, the thermoplastic polymer and / or elastomer comprises 50 weight percent or less of thermosetting polymer and / or elastomer, or 40 weight percent or less of thermosetting polymer and / or elastomer, or 30 weight percent or less of thermosetting polymer and / or elastomer, or 20 weight percent or less of thermosetting polymer and / or elastomer, or 10 weight percent or less of thermosetting polymer and / or elastomer, based on the total weight of the thermoplastic polymer and / or elastomer. In some embodiments, the thermoplastic polymer and / or elastomer does not include a thermosetting polymer and / or elastomer. The thermoplastic polymer-wollastonite composite according to the present invention is a composite material comprising a thermoplastic polymer and wollastonite.The thermoplastic elastomer-wollastonite composite according to the present invention is a composite material comprising a thermoplastic elastomer and wollastonite.

[0015] Thermoplastic foams are produced by inflating a thermoplastic polymer with one or more gases. In this way, the polymer can be expanded by a factor of 1.5 to 50, e.g. to 15 kg / m 3 ~750kg / m 3 The thermoplastic foam may be made from polyethylene, polypropylene, polystyrene, polyvinyl chloride, polycarbonate, poly(methyl methacrylate), poly(ethylene terephthalate) or ethylene vinyl acetate. In some embodiments, the thermoplastic polymers and thermoplastic elastomers according to the present invention are not treated with one or more gases to form a foam. In some embodiments of the present invention, the composite is essentially free of thermoplastic foam, which means that in some instances, thermoplastic foam is present in the thermoplastic polymer-wollastonite composite and / or the thermoplastic elastomer-wollastonite composite in an amount of less than 0.1 weight percent, or less than 0.5 weight percent, or less than 1.0 weight percent, or less than 1.5 weight percent, or less than 2.0 weight percent, or less than 2.5 weight percent, based on the total weight of the composite.

[0016] In some embodiments, the thermoplastic polymer-wollastonite composite or thermoplastic elastomer-wollastonite composite comprises wollastonite in an amount of from about 5 to about 50 weight percent, or from about 10 to about 45 weight percent, or from about 15 to about 40 weight percent, or from about 20 to about 35 weight percent, or from about 25 to about 30 weight percent, based on the total weight of the composite. In some embodiments, the thermoplastic polymer-wollastonite composite comprises the thermoplastic polymer in an amount of about 40 to about 95 weight percent, or about 45 to about 90 weight percent, or about 50 to about 85 weight percent, or about 55 to about 80 weight percent, or about 60 to about 75 weight percent, or about 65 to about 70 weight percent, based on the total weight of the composite.

[0017] In some embodiments, the thermoplastic elastomer-wollastonite composite comprises the thermoplastic elastomer in an amount of about 40 to about 95 weight percent, or about 45 to about 90 weight percent, or about 50 to about 85 weight percent, or about 55 to about 80 weight percent, or about 60 to about 75 weight percent, or about 65 to about 70 weight percent, based on the total weight of the composite. In one embodiment, the combination of thermoplastic polymer-wollastonite composite and thermoplastic elastomer-wollastonite composite includes thermoplastic polymer and thermoplastic elastomer in an amount of about 40 to about 95 weight percent, or about 45 to about 90 weight percent, or about 50 to about 85 weight percent, or about 55 to about 80 weight percent, or about 60 to about 75 weight percent, or about 65 to about 70 weight percent, based on the total weight of the composite.

[0018] In certain embodiments, the thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite further comprises one or more components, such as plastic additives selected from plasticizers, stabilizers, impact modifiers, fillers / extenders, flame retardants, tackifiers, thickeners / rheology modifiers, antioxidants, compatibilizers, accelerators, and the like, and combinations thereof. Plastic additives include antifoam agents, anti-chafing agents, biocides, foaming agents, and the like, as described, for example, in Plastic Additives Handbook 6 thOther plastic additives may also be selected from the list, including but not limited to, those listed in The Journal of Polymer Science, Vol. 13, No. 1, pp. 111-115, 2002, and the like, or found at www.polymer-additives.specialchem.com / selectors.

[0019] Plastic additives include compatibilizers, such as maleic anhydride grafted polypropylene: POLYBOND®, Lotryl®, Epolene®, Fusabond®, etc.; rheology improvers, such as blends of fatty acid derivatives: Strucktol® (e.g. Strucktol® RP-11), Quent® (e.g. Quent® TPP), Peroxan TPO, TEGOMER® (e.g. TEGOMER® P122). , Luperox® (e.g., Luperox® 101PP7.5); antioxidants, such as ANOX® (e.g., ANOX® BB011), NAUGARD® (e.g., NAUGARD® P), ULTRANOX® (e.g., ULTRANOX® 626), Irgafos® (e.g., Irgafos® 168), Irganox® (e.g., Irganox® 1010), and the like.

[0020] Noise reduction is perceived by the human ear when the intensity of sound waves, such as frequencies within the range of 20Hz to 20,000Hz, is reduced. A reduction in the level of sound or vibration within this frequency range is desirable. For example, for a dishwasher, the sound frequency is within 200 to 800Hz. Noise reduction may be defined, for example, as a reduction in sound intensity / pressure. In some instances, reduction in sound intensity / pressure may be achieved by absorption and / or barrier treatments. In absorption treatments, such as the use of foams, internal reflection of sound waves allows for the conversion of sound energy into heat. In barrier treatments, waves are reflected from a surface based on the high surface density of the material.

[0021] Noise reduction may also be defined as vibration reduction. In some instances, vibration reduction may be achieved by damping and / or isolation. In damping mode, vibration energy is absorbed by a material and converted to heat or other forms of energy. Isolation treatment simply isolates the device / part that produces the vibration from the rest of the device to prevent the vibration from being transmitted to other parts. In some embodiments, the article according to the present invention comprises a thermoplastic polymer-wollastonite composite and / or a thermoplastic elastomer-wollastonite composite. Such articles can be manufactured using extrusion, injection molding and / or thermoforming. In some embodiments, the article can be a panel that can be used as an enclosure, an acoustic partition and / or a suspended baffle.

[0022] The article, such as a panel, can be used to encase an apparatus according to the invention. The apparatus can generate noise. The apparatus can be selected from an air conditioning unit, a washing machine, a tumble dryer, a washer / tumble dryer, a refrigerator, a freezer, a dishwasher, a grinder, a vacuum cleaner, a hair dryer, a pump, a compressor, a generator, a lawn mower, a car, construction equipment, garden equipment or agricultural equipment.

[0023] In some embodiments, the thermoplastic polymer-wollastonite composite and / or articles comprising the thermoplastic polymer-wollastonite composite have one or more of the following advantages: Reduced noise; A reduction in noise at one or more frequencies; A decrease in sound at one or more frequencies; A decrease in vibration at one or more frequencies; Adequate tensile strength; Suitable heat resistance; Fit Izod shock; Adequate stiffness; Proper part density and mold shrinkage; Suitable melt flow rate of the compound.

[0024] For the avoidance of doubt, this application relates to the subject matter described in the following numbered paragraphs: 1. Use of thermoplastic polymer-wollastonite composites and / or thermoplastic elastomer-wollastonite composites to reduce noise. 2. Wollastonite has a median particle size d 50 The use according to paragraph 1, wherein the diameter of the nanoparticles is in the range of about 1 μm to about 90 μm. 3. The use according to paragraph no. 1 or paragraph no. 2, wherein the wollastonite particles have an aspect ratio of at least 2:1. 4. Wollastonite has a BET surface area of ​​about 0.2 to about 5.0 m 2 / g. 5. The use of any one of the preceding paragraph numbers, wherein the wollastonite is present in an amount of about 5 to about 50 weight percent based on the total weight of the composite. 6. The use according to any one of the preceding paragraph numbers, wherein the thermoplastic polymer is selected from polypropylene, polyethylene, polystyrene, polyvinyl chloride, acrylic, polyamide, polycarbonate, poly(methyl methacrylate), acrylonitrile-butadiene-styrene, thermoplastic starch or combinations thereof. 7. The use of any one of the preceding paragraph numbers, wherein the thermoplastic elastomer is selected from a thermoplastic polyurethane, a thermoplastic vulcanizate, a thermoplastic olefin, a thermoplastic polyamide, a thermoplastic styrenic resin, a thermoplastic copolyester, or a combination thereof. 8. The use of any one of the preceding paragraph numbers, wherein the thermoplastic polymer and / or thermoplastic elastomer is present in an amount of about 40 to about 95 weight percent based on the total weight of the composite. 9. The use of any one of the preceding paragraph numbers, wherein the composite further comprises one or more components selected from plasticizers, stabilizers, impact modifiers, fillers / extenders, flame retardants, tackifiers, thickeners / rheology modifiers, antioxidants, compatibilizers, accelerators or combinations thereof. 10. The use of any one of the preceding paragraph numbers, wherein the composite is essentially free of thermoplastic foam. 11. The use according to paragraph 10, wherein the composite comprises a thermoplastic foam in an amount of less than 0.1 weight percent based on the total weight of the composite.

[0025] 12. Thermoplastic polymer-wollastonite composites and / or thermoplastic elastomer-wollastonite composites for use as noise reducing materials. 13. Wollastonite has a median particle size d 50 13. The thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite according to paragraph 12, having a particle size distribution in the range of about 1 μm to about 90 μm. 14. A thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite according to paragraph 12 or paragraph 13, wherein the wollastonite particles have an aspect ratio of at least 2:1. 15. Wollastonite has a BET surface area of ​​about 0.2 to about 5.0 m 2 15. A thermoplastic polymer-wollastonite composite and / or a thermoplastic elastomer-wollastonite composite according to any one of paragraphs 12 to 14, having a molecular weight of 1 / g or more. 16. A thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite described in any one of paragraphs 12 to 15, wherein the wollastonite is present in an amount of about 5 to about 50 weight percent based on the total weight of the composite. 17. A thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite according to any one of paragraphs 12 to 16, wherein the thermoplastic polymer is selected from polypropylene, polyethylene, polystyrene, polyvinyl chloride, acrylic resins, polyamides, polycarbonates, poly(methyl methacrylate), acrylonitrile-butadiene-styrene, thermoplastic starch or combinations thereof. 18. A thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite described in any one of paragraphs 12 to 17, wherein the thermoplastic elastomer is selected from thermoplastic polyurethanes, thermoplastic vulcanizates, thermoplastic olefins, thermoplastic polyamides, thermoplastic styrenics, thermoplastic copolyesters, or combinations thereof. 19. A thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite described in any one of paragraphs 12 to 18, wherein the thermoplastic polymer and / or thermoplastic elastomer is present in an amount of about 40 to about 95 weight percent based on the total weight of the composite. 20. A thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite described in any one of paragraphs 12 to 19, wherein the composite further comprises one or more components selected from plasticizers, stabilizers, impact modifiers, fillers / extenders, flame retardants, tackifiers, thickeners / rheology modifiers, antioxidants, compatibilizers, accelerators or combinations thereof. 21. A thermoplastic polymer-wollastonite composite and / or thermoplastic elastomer-wollastonite composite described in any one of paragraphs 12 to 20, which is essentially free of thermoplastic foam. 22. The use according to paragraph 21, wherein the composite comprises a thermoplastic foam in an amount of less than 0.1 percent by weight based on the total weight of the composite. 23. An article comprising a thermoplastic polymer-wollastonite composite and / or a thermoplastic elastomer-wollastonite composite described in any one of paragraphs 12 to 22. 24. Panel, item no. 23. 25. A method for producing an article according to paragraph 23 or 24 by extrusion, injection molding and / or thermoforming. 26. A method for reducing noise comprising the use described in paragraphs 1 to 11. 27. Apparatus containing an article according to paragraph 23 or paragraph 24. 28. An apparatus as described in paragraph no. 27 which is an air conditioning unit, a washing machine, a tumble dryer, a washer / tumble dryer, a refrigerator, a freezer, a dishwasher, a grinder, a vacuum cleaner, a hair dryer, a pump, a compressor, a generator or a lawnmower. EXAMPLES

[0026] Pellets of composites A-D were obtained by combining the ingredients shown in Table 1 using a twin screw extrusion process using the conditions in Table 2. [Table 1] [Table 2]

[0027] The pellets were used in an injection molding process using a 66 ton Arburg Allrounder 370E600-170 injection molding machine to obtain standard specimens for each of the ASTM tests described below. All compounds were dried at 80°C in a convection oven prior to injection molding. Table 3 shows the injection molding parameters used in this study. The injection pressures for the electrically driven injection molding machine are also shown in parentheses along with the approximately equivalent hydraulic pressures.

[0028] [Table 3] Compression molded test specimens with dimensions 10 inches by 10 inches were used to test sound transmission loss according to SAE J1400 (August 2010). Injection molded specimens were used for measurements of tan δ and composite loss factor.

[0029] Tan δ was measured using Dynamic mechanical analysis using a TA Instruments RSA G2 equipped with a 40 mm three-point bend fixture over a temperature range of 0 to 80°C with a tensile strain of 0.05% at an angular frequency of 10 rad / sec. The dimensions of the test specimens were approximately 12.6 × 3.1 × 54 mm. Composite loss factor was measured using ISO 16940 (2008) at 23°C and 60°C using specimens with dimensions 125mm x 12.5mm (also referred to as vibration damping / center point test). The results of the sound transmission loss, tan δ and composite loss factor tests for compositions A and B can be seen in Figures 1, 2 and 3, respectively. All three tests demonstrate the superior performance of composition B (an example of the invention) over composition A (a comparative example).

[0030] As can be seen in Figure 1, composition B outperformed composition A in sound transmission testing, particularly in the 1 / 3 octave band of frequencies between 250 Hz and 4,000 Hz. Figure 2 shows the damping performance of compositions A and B as measured by tan δ. Composition B according to the invention again outperformed comparative composition A, having a higher tan δ over the range of temperatures. Figure 3 shows the composite loss factor at a number of frequencies (200, 400 and 800 Hz) for both compositions A and B. In each of these examples, composition B according to the invention outperforms comparative composition A. In addition to the noise reducing properties of composition B according to the invention, composition B has also been found to have suitable mechanical properties for a range of applications, in particular as panels for noise producing equipment.

[0031] Specimens prepared and molded to perform the tests discussed above were conditioned for 7 days at 23° C. and 50% relative humidity and also tested for the following properties: Ash content (internal method - using microwave ashing oven) Density Measurement Using a Mettler Toledo MS Semi-Microbalance and Density Kit Flexural properties using ASTM D790 (at 0.05 in / min) Tensile properties using ASTM D638 (at 2 in / min) Notched Izod impact using ASTM D256 at 23°C Heat Deflection Temperature Measured Per ASTM D648 Gloss Measurement Using the Gardner Micro Tri-Glossmeter Mold shrinkage (flow and cross flow) using in-house developed equipment

[0032] In each of the tests listed, the compositions according to the invention were found to perform successfully. In some tests, as shown below, a significant improvement was found over compositions containing neat resin. In addition, the mechanical properties of the compositions according to the invention meet the requirements of most household electrical appliances. Ash content (internal method-using microwave ashing oven)-filler addition was verified and found to be within acceptable limits; Density measurement using a Mettler Toledo MS semi-microbalance and density kit - measured density values ​​were similar to theoretical density values ​​for the desired filler loading; Flexural properties using ASTM D790 (at a speed of 0.05 in / min) - composition B according to the invention provided approximately 200% improvement in flexural modulus over the composition containing the neat resin; Notched Izod impact using ASTM D256 at 23° C.--Composition B provided approximately a 200% improvement in flexural modulus over the composition containing the neat resin. Heat Deflection Temperature (HDT) as measured by ASTM D648 - Composition B provided a 30° C. HDT improvement over the composition containing the neat resin.

Claims

1. 1. Use of a thermoplastic elastomer-wollastonite composite for reducing noise, wherein the thermoplastic elastomer is selected from a thermoplastic polyurethane, a thermoplastic vulcanizate, a thermoplastic olefin, a thermoplastic polyamide, a thermoplastic styrenic, a thermoplastic copolyester, or a combination thereof, and the thermoplastic elastomer is present in an amount of 40 to 95 weight percent based on the total weight of the composite.

2. The median particle size value d of the wollastonite 50 The use according to claim 1, wherein the thickness of the nanoparticles is between 1 μm and 90 μm.

3. The BET surface area of ​​the wollastonite is 0.2 to 5.0 m 2 The use according to claim 1 or claim 2, wherein the molecular weight of the polymer is 1000 or more.

4. The use according to any one of claims 1 to 3, wherein the wollastonite is present in an amount of 5 to 50 weight percent based on the total weight of the composite.

5. 5. The use according to any one of claims 1 to 4, wherein the composite further comprises one or more components selected from plasticizers, stabilizers, impact modifiers, fillers / extenders, flame retardants, tackifiers, thickeners / rheology modifiers, antioxidants, compatibilizers, accelerators or combinations thereof.

6. 1. A thermoplastic elastomer-wollastonite composite for use as a noise reducing material, wherein the thermoplastic elastomer is selected from a thermoplastic polyurethane, a thermoplastic vulcanizate, a thermoplastic olefin, a thermoplastic polyamide, a thermoplastic styrenic, a thermoplastic copolyester, or combinations thereof, and the thermoplastic elastomer is present in an amount of 40 to 95 weight percent based on the total weight of the composite.

7. An article comprising the thermoplastic elastomer-wollastonite composite of claim 6.

8. The article of claim 7 which is a panel.

9. A method for producing an article according to claim 7 or 8 by extrusion, injection moulding and / or thermoforming.

10. A method for reducing noise comprising the use of any one of claims 1 to 5.

11. 9. An apparatus comprising an article according to claim 7 or 8.

12. 12. The apparatus of claim 11 which is an air conditioning unit, a washing machine, a tumble dryer, a washer / tumble dryer, a refrigerator, a freezer, a dishwasher, a grinder, a vacuum cleaner, a hair dryer, a pump, a compressor, a generator or a lawnmower.

Citation Information

Patent Citations

  • Low cost and high efficient soundproof material and manufacturing method thereof

    CN103897262A

  • Three-layer composite silencing plastic drain pipe core material and preparation method and application thereof

    CN105237850A

  • Vibration-damping thermoplastic resin composition

    JP1997194743A

  • Composition for sound-isolating sheet and sound-isolating sheet made therefrom

    JP2000129036A

  • Interlayer for laminated glass, and laminated glass

    JP2016108229A