How to manage mixed resins

By pre-mixing boron-adsorbing resin with anion and cation exchange resins in a sealed, inert gas-filled container with a gas barrier, the startup time for mixed-bed resin columns is drastically reduced, ensuring efficient and rapid production of pure water.

JP7573770B1Active Publication Date: 2024-10-25NOMURA MICRO SCI CO LTD
View PDF 15 Cites 0 Cited by

Patent Information

Application Number
JP2024015737
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2024-02-05
Publication Date
2024-10-25
Estimated Expiration
2044-02-05

AI Technical Summary

Technical Problem

Existing mixed-bed resin columns, particularly those containing boron-adsorbing resin, require an excessively long startup time due to the presence of impurities and thermal decomposition during storage, which affects the efficiency and speed of pure water production.

Method used

A method involving the mixing of boron-adsorbing resin with basic anion and acidic cation exchange resins in a sealed container under inert gas conditions, ensuring a wet state with a gas barrier layer, and transporting this mixture directly to the installation site for immediate use in pure water production systems.

Benefits of technology

This approach significantly reduces startup time by minimizing thermal decomposition and impurity introduction, allowing for rapid and efficient production of high-quality pure water.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573770000001_ABST
    Figure 0007573770000001_ABST
Patent Text Reader

Abstract

To speed up the start-up of equipment filled with mixed resin. [Solution] A method of managing a mixed resin involves mixing a boron adsorbent resin with at least one of a basic anion exchange resin and an acidic cation exchange resin, sealing the mixed resin in a wet state in an airtight container, transporting the airtight container containing the mixed resin to a site where a pure water production system is installed to produce pure water, and filling the boron adsorbent resin mixed ion exchange system installed in the pure water production system with the mixed resin inside the airtight container when using the boron adsorbent resin mixed ion exchange system.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for managing mixed resins. To Regarding. [Background technology]

[0002] 2. Description of the Related Art Conventionally, pure water producing apparatuses for producing pure water are known.

[0003] The following Patent Document 1 discloses a pure water production apparatus using a mixed-bed resin tower in which a boron adsorbent resin is mixed with another resin, an ion exchange resin. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 6310819 Summary of the Invention [Problem to be solved by the invention]

[0005] Generally, ion exchange resins are sold sealed to prevent contamination during the period from delivery to the start of use. In the case of boron adsorbent resin, which is a type of ion exchange resin, it is sold in a sealed state as a single unit. Therefore, when using a mixed-bed resin tower filled with a mixture of boron adsorbent resin and other resins, the boron adsorbent resin and other resins are obtained separately and then mixed together for use.

[0006] Generally, an ion exchange resin tower requires a start-up operation before it can be put into operation. Here, start-up refers to a state in which the ion exchange resin tower can be powered and operated, that is, the treated water from the ion exchange resin tower has sufficient water quality to be able to produce pure water or ultrapure water in the pure water production system or ultrapure water production system in which it is installed. For example, in the start-up of an ion exchange resin tower, pure water is passed through the ion exchange resin tower for a long period of time to wash the ion exchange resin filled therein. The outlet water from the ion exchange resin tower initially has a high total organic carbon (TOC), but the TOC decreases over time and eventually becomes constant. In this state, the start-up of the ion exchange resin tower is completed and the ion exchange resin tower can be operated. It may take several tens of days to start up the ion exchange resin tower. Here, total organic carbon (TOC) is the total amount of carbon that constitutes the organic matter present in water, and is one of the water quality indicators that indicate the "pollution of water."

[0007] Patent Document 1 discloses a mixed-bed resin tower of boron adsorbent resin and other resins. However, this mixed-bed resin tower of boron adsorbent resin and other resins has a problem that it takes a long time to start up the mixed-bed resin tower after the boron adsorbent resin and other resins are filled in the mixed-bed resin tower. This was thought to be due to the fact that the boron adsorbent resin contains a large amount of impurities.

[0008] The present disclosure has been made in consideration of the above problems, and provides a method for managing a mixed resin that can quickly start up an apparatus filled with the mixed resin. of The purpose is to provide. [Means for solving the problem]

[0009] In order to solve the above problems, the mixed resin management method described in the first aspect includes mixing a boron adsorbent resin with at least one of a basic anion exchange resin and an acidic cation exchange resin, sealing the mixed resin in a wet state in a sealed container, transporting the sealed container containing the mixed resin to a site where a pure water production apparatus for producing pure water is installed, and filling the boron adsorbent resin mixed ion exchange apparatus installed in the pure water production apparatus with the mixed resin inside the sealed container when the boron adsorbent resin mixed ion exchange apparatus is used.

[0010] In the above-mentioned method for managing a mixed resin, the sealed container preferably has a gas barrier layer containing a gas barrier resin or a metal.

[0011] In the above-mentioned method for managing a mixed resin, it is preferable that the mixed resin is sealed in the sealed container in a state in which the inside of the sealed container is replaced with an inert gas.

[0012] In the above-mentioned mixed resin management method, it is preferable to mix the boron adsorbent resin with at least one of the basic anion exchange resin and the acidic cation exchange resin in pure water, seal the mixed resin in the sealed container, and store the mixed resin in a wet state until the boron adsorbent resin mixed ion exchange device is used. In the present disclosure, the wet state refers to a state in which the ion exchange resin is mixed with pure water. The amount of pure water, i.e., the water content, of the ion exchange resin, i.e., the mixed resin composed of the boron adsorbent resin and at least one of the basic anion exchange resin and the acidic cation exchange resin, is more preferably 10% by weight to 200% by weight, and even more preferably 30% by weight to 100% by weight.

[0013] In the packaging structure of the mixed resin according to the second embodiment, a mixed resin obtained by mixing a boron adsorbent resin with at least one of a basic anion exchange resin and an acidic cation exchange resin is sealed in a sealed container.

[0014] In the above-mentioned mixed resin packaging structure, the sealed container preferably has a gas barrier layer containing a gas barrier resin or a metal.

[0015] In the above-mentioned mixed resin packaging structure, it is preferable that the mixed resin is sealed in the sealed container with the inside of the sealed container replaced with an inert gas. Effect of the Invention

[0016] According to the present disclosure, the start-up of an apparatus filled with a mixed resin can be accelerated. [Brief description of the drawings]

[0017] [Figure 1] 1 is a configuration diagram showing an example of a pure water producing system according to a first embodiment. [Diagram 2] FIG. 1 is a flow diagram showing an example of a method for managing a mixed resin used in a pure water production system. [Figure 3A] FIG. 2 is a diagram showing an example of a process for mixing a boron adsorbent resin with another ion exchange resin. [Figure 3B] FIG. 2 is a diagram showing an example of a process for mixing a boron adsorbent resin with another ion exchange resin. [Figure 4] FIG. 1 is a diagram showing a state in which a mixed resin obtained by mixing a boron adsorbent resin with another ion exchange resin is sealed in a container. [Diagram 5] FIG. 11 is a configuration diagram showing an example of a pure water producing system according to a second embodiment. [Figure 6] FIG. 11 is a configuration diagram showing an example of a pure water producing system according to a third embodiment. [Figure 7] FIG. 13 is a configuration diagram showing an example of a pure water producing system according to a fourth embodiment. [Figure 8] 1 is a graph showing the relationship between the TOC of outlet water and water flow time of each boron adsorbent resin mixed ion exchange device in the examples. [Figure 9] 1 is a graph showing the relationship between the resistivity and water flow time of each boron adsorbent resin mixed ion exchange device in the examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0018] Hereinafter, an embodiment of the present disclosure will be described with reference to the drawings. In each drawing, components having common functions are given the same reference numerals, and duplicated descriptions are omitted. In addition, in each drawing, components that are less relevant to the present disclosure are omitted. Note that the present disclosure is not limited to the following embodiments.

[0019] [First embodiment] FIG. 1 is a configuration diagram showing an example of a pure water manufacturing system 10 of the first embodiment. As shown in FIG. 1, the pure water manufacturing system 10 includes a pretreatment device 11 and a boron adsorbent resin mixed ion exchange device 12. As an example, the boron adsorbent resin mixed ion exchange device 12 includes a boron adsorbent resin / cation exchange / anion exchange mixed resin that is a mixture of a boron adsorbent resin, a strongly acidic cation exchange resin, and a strongly basic anion exchange resin. The strongly acidic cation exchange resin is an example of an acidic cation exchange resin, and the strongly basic anion exchange resin is an example of a basic anion exchange resin. The boron adsorbent resin / cation exchange / anion exchange mixed resin is an example of a mixed resin.

[0020] The mixed resin filled in the boron adsorbent resin mixed ion exchange device 12 is applied with an example of a mixed resin management method and an example of a mixed resin packaging structure, which will be described later.

[0021] In addition, in this disclosure, pure water refers to pure water that has been treated, for example, with an ion exchange resin, a reverse osmosis membrane, or a combination of these, and ultrapure water refers to ultrapure water that has been further purified in a secondary pure water system (subsystem).

[0022] (Configuration of pure water production equipment) In the pure water production system 10 of the first embodiment, the pretreatment device 11 removes suspended solids from the raw water and treats the raw water to a water quality suitable for supplying to the boron adsorbent resin mixed ion exchange device 12 .

[0023] The raw water may be city water, well water, industrial water, etc. The raw water contains about 5 to 100 μg B / L of boron. Of this, boron that is not removed by the pretreatment device 11 remains in the water to be treated.

[0024] The pretreatment device 11 is configured by appropriately selecting, for example, a sand filter, a precision filter, etc., and is further configured with a heat exchanger, etc., for adjusting the temperature of the water to be treated as necessary. Note that, depending on the quality of the raw water, etc., the pretreatment device 11 may not be provided.

[0025] In the pure water production system 10 of the first embodiment, pretreated water treated in the pretreatment device 11 is subjected to a desalination treatment and an oxidative decomposition treatment, which will be described later, as necessary, and then supplied to the boron adsorbent resin mixed ion exchange device 12. The water to be treated in the boron adsorbent resin mixed ion exchange device 12 contains total organic carbon (TOC) components as well as boron. Among the TOC components, carbon dioxide and / or carboxylic acid compounds may be adsorbed by the boron adsorbent resin, thereby reducing the boron adsorption capacity of the boron adsorbent resin. However, by using the boron adsorbent resin mixed ion exchange device 12, it is possible to suppress the reduction in the boron adsorption capacity of the boron adsorbent resin.

[0026] The carboxylic acid compound is, for example, an aliphatic carboxylic acid having 0 or 1 or more carbon atoms and having 1 or more carboxyl groups in the molecule, and is preferably an aliphatic carboxylic acid having 0 to 5 carbon atoms. When the carboxylic acid compound has 2 or more carboxyl groups and the carbon number is 1 or more, it is preferable that the carboxyl groups of the carboxylic acid compound are bonded to the same carbon atom. When the carboxylic acid compound has 2 or more carboxyl groups and the carbon number is 2 or more, it is preferable that the carboxyl groups are bonded to a carbon atom closer to the carbon atom, and more preferably to the same carbon atom or adjacent carbon atoms.

[0027] Specific examples of such carboxylic acid compounds include formic acid, acetic acid, oxalic acid, etc. Among them, oxalic acid reduces the boron removal ability of the boron adsorbent resin mixed ion exchange device 12, so when the water to be treated contains oxalic acid, the effect of the boron adsorbent resin mixed ion exchange device 12 described below is significantly obtained.

[0028] The concentration of carbon dioxide and / or carboxylic acid compounds in the water to be treated is preferably 1 μg / L (as C) or more and 50 μg / L (as C) or less in terms of TOC. If the concentration of carboxylic acid compounds exceeds 50 μg / L (as C), the load on the boron adsorbent resin mixed ion exchange device 12 increases, and the quality of the treated water may deteriorate. If the concentration is less than 1 μg / L (as C), it may be difficult to obtain the effect of improving the boron adsorption capacity in the boron adsorbent resin mixed ion exchange device 12.

[0029] In the pure water producing apparatus 10 of the first embodiment, the boron adsorbent resin mixed ion exchange device 12 is configured with a boron adsorbent / cation exchange / anion exchange mixed resin as an example of a mixed resin formed by mixing a boron adsorbent resin, a strongly acidic cation exchange resin, and a strongly basic anion exchange resin, as described above.

[0030] In addition, the boron adsorbent resin mixed ion exchange device 12 may be configured to include, as another example of the mixed resin, a boron adsorbent / anion exchange mixed resin obtained by mixing a boron adsorbent resin and a strongly basic anion exchange resin, or a boron adsorbent / cation exchange mixed resin obtained by mixing a boron adsorbent resin and a strongly acidic cation exchange resin.

[0031] Boron is usually present in the treated water as borate ions, hydrogen borate ions, etc., but since these are weak ions, they are hardly removed even by using, for example, a strongly basic anion exchange resin, a strongly acidic cation exchange resin, or a mixed bed ion exchange resin in which a strongly acidic cation exchange resin and a strongly basic anion exchange resin are mixed. Therefore, when boron removal is required, a boron adsorbent resin is used. However, although this boron adsorbent resin has high boron selectivity, when total organic carbon components are contained in the treated water, the adsorption of boron may be inhibited by adsorbing carbon dioxide and carboxylic acid compounds from the total organic carbon components.

[0032] In the boron adsorbent resin mixed ion exchange device 12, a boron adsorbent resin, a strong acid cation exchange resin, and a strong basic anion exchange resin are mixed to treat the water to be treated, which contains carbon dioxide and / or carboxylic acid compounds and boron. The boron adsorbent resin, a strong acid cation exchange resin, and a strong basic anion exchange resin, can simultaneously adsorb boron with the boron adsorbent resin and adsorb carbon dioxide, carboxylic acid compounds, and eluted substances (organic substances) from the boron adsorbent resin with the strong acid cation exchange resin or the strong basic anion exchange resin. Therefore, the boron adsorbent resin mixed ion exchange device 12 of the first embodiment can exhibit excellent boron removal ability for a long period of time.

[0033] In the first embodiment, a boron adsorbent resin, a strong acid cation exchange resin, and a strong basic anion exchange resin are mixed in advance according to an example of a mixed resin management method described later (see FIG. 2). The mixed resin is filled in the boron adsorbent resin mixed ion exchange device 12 (see FIG. 2).

[0034] The mixing ratio of the boron adsorption resin, the strong acid cation exchange resin and the strong basic anion exchange resin in the boron adsorption / cation exchange / anion exchange mixed resin is preferably 0.3 to 1.3, more preferably 0.4 to 1.0, in terms of exchange capacity ratio, where the exchange capacity of the boron adsorption resin is represented by CB, the exchange capacity of the strong acid cation exchange resin by CC, and the exchange capacity of the strong basic anion exchange resin by CA. If CC / (CA+CB) exceeds 1.3, the boron adsorption / cation exchange / anion exchange mixed resin may become an acidic atmosphere, and the boron adsorption capacity may decrease. If it is less than 0.3, the effect of the mixed resin of the strong acid cation exchange resin and the strong basic anion exchange resin decreases, and the resistivity of the treated water may decrease.

[0035] The boron adsorbent resin used in the boron adsorbent resin mixed ion exchange device 12 is not limited as long as it can selectively adsorb boron, and may be a polystyrene resin having excellent heat resistance, water resistance, and chemical resistance, or an ion exchange resin obtained by adding a polyhydric alcohol group as a functional group to a phenolic resin. As the boron adsorbent resin, an ion exchange resin containing an N-methylglucamine group having a high ion exchange capacity is particularly preferable. In terms of boron removal capacity, the exchange capacity of the boron adsorbent resin is preferably 0.155 meq / mL or more and 1.5 meq / mL or less. The specific gravity of the boron adsorbent resin is 1.05 to 1.15 g / cm 3 It is preferable that:

[0036] Examples of commercially available boron-adsorbing resins include Amberlite (registered trademark: manufactured by Rohm and Haas Company) IRA-743T and Diaion CRB02 (manufactured by Mitsubishi Chemical Corporation).

[0037] As the strongly acidic cation exchange resin, a styrene-based resin having a sulfonic acid group as a functional group is preferable because the hydrolysis of the ion exchange resin is small and the elution of organic cation components into ultrapure water is small. The strongly acidic cation exchange resin is preferably one having an exchange capacity of 1.5 meq / mL or more and 2.5 meq / mL or less, more preferably 2 meq / mL or more and 2.5 meq / mL or less.

[0038] As the strongly acidic cation exchange resin, H type is preferable because it can remove cationic components with low ion selectivity. One having an H type conversion rate of 99.95% or more is preferably used. The specific gravity of the strong acid cation exchange resin is 1.2 g / cm 3 More than 1.3g / cm 3 It is preferable that: Commercially available strong acid cation exchange resins include Duolite CGP (manufactured by Rohm and Haas Company) and Diaion SKT20L (manufactured by Mitsubishi Chemical Corporation).

[0039] As the strongly basic anion exchange resin, a styrene-based resin having a quaternary ammonium group as a functional group is preferably used because the hydrolysis of the ion exchange resin is small and the elution of organic anion components into ultrapure water is small. As the strongly basic anion exchange resin, one having an exchange capacity of preferably 0.7 meq / mL to 1.5 meq / mL, more preferably 1 meq / mL to 1.5 meq / mL, is suitable.

[0040] In addition, the strongly basic anion exchange resin is preferably an OH type, since it can remove anion components with low ion selectivity. The OH type conversion rate is preferably 99.95% or more. The specific gravity of the strong basic anion exchange resin is 1.0 to 1.1 g / cm 3 It is preferable that: Commercially available strong basic anion exchange resins include Duolite AGP (manufactured by Rohm and Haas Company) and Diaion SAT20L (manufactured by Mitsubishi Chemical Corporation).

[0041] The pure water production system 10 of the first embodiment preferably includes an oxidative decomposition device between the pretreatment device 11 and the boron adsorbent resin mixed ion exchange device 12, and more preferably includes a demineralization device between the pretreatment device 11 and the oxidative decomposition device. In this case, treated water from the oxidative decomposition device is supplied to the boron adsorbent resin mixed ion exchange device.

[0042] As the desalting device, a reverse osmosis membrane device and an electric deionization device are preferably used because they have excellent ability to remove ionic components, and these can be used alone or in combination.

[0043] The reverse osmosis membrane device removes salts and ionic and colloidal organic matter from the pretreated water to produce concentrated water and permeate. As the reverse osmosis membrane device, a membrane module using a cellulose triacetate asymmetric membrane or a polyamide composite membrane, such as a flat sheet membrane, a spiral membrane, a tubular membrane, or a hollow fiber membrane, can be used. Among them, a polyamide composite membrane is preferable from the viewpoint of increasing the impurity removal rate, and the membrane shape is preferably a spiral membrane.

[0044] The reverse osmosis membrane device may be configured as a multi-stage device by connecting two or more reverse osmosis membrane devices in series. In this case, the salt rejection rate in the reverse osmosis membrane device is increased, and as a result, the load on the boron adsorption / cation exchange / anion exchange mixed resin in the boron adsorbent resin mixed ion exchange device 12 can be reduced, thereby improving the boron removal ability. When the reverse osmosis membrane device is configured as a multi-stage device, a two-stage reverse osmosis membrane device is preferable.

[0045] The electrodeionization apparatus is configured such that a gap formed by an anion exchange membrane and a cation exchange membrane is filled with an ion exchanger to form a desalting compartment and a concentration compartment, and a direct current is applied to remove ions from the water to be treated. As the electrodeionization apparatus, a commercially available product such as the MK-3 series (manufactured by E-Cell) or the VNX series (manufactured by IONPURE) can be used. The water recovery rate of the electrodeionization apparatus is preferably 80 to 98%. One electrodeionization apparatus may be used in a single stage, or two or more electrodeionization apparatuses may be connected in series to be used in multiple stages.

[0046] The demineralization apparatus may also be constructed by connecting a two-bed, three-tower (2B3T) apparatus to a reverse osmosis membrane apparatus. The two-bed, three-tower apparatus is configured to include a cation exchange tower, a decarbonation tower, and an anion exchange tower in this order, and removes ionic components as impurities, particularly ionic components that generate scale in the reverse osmosis membrane apparatus. The water from which these impurities have been removed is supplied to the reverse osmosis membrane apparatus, where ionic components, non-ionic organic matter, fine particles, etc. are removed. Next, the permeated water from the reverse osmosis membrane apparatus is supplied to an oxidative decomposition apparatus.

[0047] The oxidative decomposition device oxidatively decomposes organic matter in the water to be treated. The oxidative decomposition device oxidatively decomposes the organic matter in the water to be treated, for example, into carbon dioxide and low-molecular-weight organic acids. As a result, carbon dioxide and carboxylic acid compounds can be produced.

[0048] Examples of the oxidative decomposition device that can be used include an ultraviolet oxidation device, a hypobromous acid oxidation device, and an ozone oxidation device. The hypobromous acid oxidation device oxidizes and decomposes urea and other difficult-to-decompose substances in the water to be treated, for example, by adding and mixing hypobromous acid to the water to be treated. The ozone oxidation device generates ozone using an ozone generator and supplies the generated ozone to the water to be treated, thereby decomposing organic matter and the like in the water to be treated.

[0049] The ultraviolet oxidation device has, for example, an ultraviolet lamp capable of irradiating ultraviolet rays having a wavelength of about 185 nm, and oxidatively decomposes TOC in the water to be treated by irradiating the water with ultraviolet rays from this ultraviolet lamp. The ultraviolet lamp used in the ultraviolet oxidation device does not have to be a lamp that emits only 185 nm ultraviolet rays, and for example, a low-pressure mercury lamp that emits 185 nm ultraviolet rays as well as ultraviolet rays around 254 nm can be used.

[0050] The UV oxidation device uses UV rays with a wavelength of about 185 nm to decompose water and generate OH radicals, which oxidize and decompose the organic matter contained in the water to be treated. The amount of UV irradiation is appropriately changed depending on the quality of the water to be treated.

[0051] Although the configuration of each part of the boron adsorbent resin mixed ion exchange apparatus 12 is not shown in the drawings, the boron adsorbent resin mixed ion exchange apparatus 12 is configured to be capable of being regenerated.

[0052] Next, a method for producing pure water using the pure water production apparatus shown in FIG. 1 will be described. First, raw water is passed through the pretreatment device 11 to obtain pretreated water. This pretreated water is subjected to desalination and oxidative decomposition as necessary, and then passed through the boron adsorbent resin mixed ion exchange device 12. At this time, the water passing speed through the boron adsorbent resin mixed ion exchange device 12 is not particularly limited, and can be appropriately determined according to the boron concentration in the water to be treated, the exchange capacity of each ion exchange resin to be mixed, and the like. From the viewpoint of removing boron highly for a long period of time, the water passing speed through the boron adsorbent resin mixed ion exchange device 12 is preferably 10 [1 / h] or more and 100 [1 / h] or less in terms of space velocity SV, and particularly preferably 20 [1 / h] or more and 50 [1 / h] or less. If the water passing speed is too fast compared to the upper limit value, boron may not be sufficiently removed. On the other hand, if it is slower than the lower limit value, organic matter may be eluted from the mixed resin, and the quality of the treated water may be reduced.

[0053] The temperature of the water to be treated in the boron adsorbent resin mixed ion exchange device 12 is not particularly limited, but is preferably 5° C. or higher and 40° C. or lower. In order to stabilize the quality of the treated water, it is preferable to keep the temperature of the water to be treated constant. For this reason, it is preferable to provide a plate-type heat exchanger or the like in the upstream of the reverse osmosis membrane device.

[0054] In this way, pure water having a boron concentration of 1.0 ng / L (as B) or less and a TOC concentration of 5.0 μg / L (as C) or less can be obtained as treated water from the boron adsorbent resin mixed ion exchange device 12.

[0055] (An example of a mixed resin management method and an example of a mixed resin packaging structure) Next, an example of a method for managing the mixed resin filled in the boron adsorbent resin mixed ion exchange device 12 of the pure water production system 10 and an example of a packaging structure for the mixed resin will be described.

[0056] FIG. 2 is a flow diagram showing an example of a method for managing mixed resins. As shown in FIG. 2, first, the boron adsorbent resin is mixed with other ion exchange resins (mixing step S101). In the first embodiment, the other ion exchange resins are a strongly acidic cation exchange resin and a strongly basic anion exchange resin. That is, in the first embodiment, the boron adsorbent resin, the strongly acidic cation exchange resin, and the strongly basic anion exchange resin are mixed. Here, mixing refers to a state in which the boron adsorbent resin, the strongly acidic cation exchange resin, and the strongly basic anion exchange resin are mixed evenly so as to be almost uniform. That is, mixing is different from a state in which the boron adsorbent resin, the strongly acidic cation exchange resin, and the strongly basic anion exchange resin are layered.

[0057] As long as the boron adsorbent resin, the strongly acidic cation exchange resin, and the strongly basic anion exchange resin can be mixed in advance, the mixing method is not particularly limited. For example, the three types of resins (i.e., the boron adsorbent resin, the strongly acidic cation exchange resin, and the strongly basic anion exchange resin) may be obtained individually in bags, and the bags may be opened at the factory to mix the three types of resins.

[0058] In addition, when a mixed bed (MB) in which a strongly acidic cation exchange resin and a strongly basic anion exchange resin are mixed in a specified ratio is available, the mixed bed (MB) may be mixed with a boron adsorbent resin obtained separately.

[0059] As an example, a boron adsorbent resin, a strong acid cation exchange resin, and a strong basic anion exchange resin may be mixed using a mixer 200 shown in Figures 3A and 3B. Figure 3A is a configuration diagram showing the state of each resin before mixing in the mixer 200, and Figure 3B is a configuration diagram showing the state of each resin during mixing in the mixer 200. Note that Figures 3A and 3B are shown schematically to make the configuration of the mixer 200 easier to understand, and are different from the actual dimensions of the mixer 200 and the diameters of the particles of each resin. The mixer 200 is installed, for example, in a factory.

[0060] 3A, the mixing device 200 includes a cylindrical housing 202 with an open top. Although not shown, a first inlet pipe for introducing pure water into the housing 202 and a second inlet pipe for introducing an inert gas into the housing 202 are connected to the lower part of the housing 202. An inert gas is a gas that does not easily cause a chemical reaction, and examples of the inert gas include rare gas elements such as helium, neon, and argon, and nitrogen gas. In the first embodiment, nitrogen gas is used as the inert gas.

[0061] As shown in FIG. 3A, the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 are placed in a predetermined ratio inside the housing 202. The boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 are particles having a diameter of, for example, 1 mm or more and 5 mm or less. The diameters of the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 may be different. Furthermore, pure water PW is introduced into the housing 202 from a first introduction pipe (not shown). In FIG. 3A, the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 are arranged in layers in the order in which they are placed in the housing 202.

[0062] As shown in FIG. 3B, pure water PW is introduced from a first introduction pipe (not shown) at the bottom of the housing 202, and an inert gas G is introduced from a second introduction pipe (not shown) at the bottom of the housing 202. For example, the pure water PW and the inert gas G are introduced so that the internal volume of the housing 202 increases by about 30%. By introducing the pure water PW and the inert gas G, the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 are raised in the pure water PW inside the housing 202 and are stirred. As a result, the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 are mixed. In the first embodiment, the pure water and the inert gas are used in combination and mixed, but the pure water or the inert gas may be used alone and mixed.

[0063] 2, the mixed resin 220 obtained by mixing the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong base anion exchange resin 214 is sealed in a container 300 (see FIG. 4) (sealing step S102). The container 300 is an example of a sealed container.

[0064] As shown in Fig. 4, as an example, the container 300 is bag-shaped and made of a film member. Furthermore, the bag-shaped container 300 is housed in, for example, an outer container (not shown) that is larger than the container 300. The outer container is a hard container made of, for example, polypropylene (PP) or polyethylene (PE). The outer container is, for example, barrel-shaped, and includes a container body with an opening at the top and a lid for opening and closing the opening. The capacity of the outer container is, for example, about 25 L.

[0065] The bag-shaped container 300 preferably includes a gas barrier layer containing a gas barrier resin. For example, the container 300 has a multi-layer structure, and the gas barrier layer is provided in an intermediate layer that is resistant to scratches due to rubbing from the outside. Here, the gas barrier layer refers to a layer that has high barrier properties and is less permeable to gases such as water vapor and oxygen (low gas permeability) compared to layers made of general resins (e.g., simple ethylene).

[0066] The gas barrier layer contains at least one gas barrier resin. Examples of the gas barrier resin include polyamide, ethylene-vinyl acetate copolymer (EVOH), ethylene-vinyl alcohol copolymer, polyglycol (PGA), polyvinylidene chloride copolymer (PVDC), polyacrylonitrile, polyvinyl alcohol (PVA), polytetrafluoroethylene (PTFE), and styrene-isobutylene-styrene copolymer. Examples of the polyamide include aromatic polyamide such as metaxylene adipamide (MXD-6), and aliphatic polyamide such as nylon 6, nylon 6,6, and nylon 6 / nylon 6,6 copolymer. Among these, polyamide is preferred, aromatic polyamide is more preferred, and metaxylene adipamide is even more preferred. The gas barrier layer may be made of metal such as aluminum foil.

[0067] The oxygen permeability of the film member of the container 300 is preferably 0.1 cc / day to 2000 cc / day, more preferably 0.2 cc / day to 100 cc / day. The oxygen permeability is a value measured in accordance with JIS K 7126-2:2006 using an oxygen permeability measuring device (for example, MOCON, product name: OX-TRAN 2 / 20) under conditions of 23°C and humidity 40% RH.

[0068] As an example, the container 300 has a heat seal layer having heat sealability on the innermost side. Heat sealability refers to the property of being able to fuse films together with heat. A heat seal layer is formed on the film surface with a temperature-melting resin material, and then the heat seal layer can be melted by adjusting the heating temperature, pressure, and time to bond the films together. This allows the peripheral portion 302 of the container 300 to be hermetically sealed by the heat seal layer with the mixed resin 220 placed inside the container 300.

[0069] The heat seal layer is made of, for example, polyethylene. As the polyethylene, high density polyethylene, medium density polyethylene, low density polyethylene, linear low density polyethylene and very low density polyethylene can be used. Among these, low density polyethylene and / or linear low density polyethylene are preferred from the viewpoint of heat sealability.

[0070] As shown in FIG. 4, the mixed resin 220 is enclosed in the container 300 (i.e., the container 300 is hermetically sealed) in a state where the inside of the container 300 is replaced with an inert gas G. For example, in a state where the mixed resin 220 is accommodated in the container 300, the inside of the container 300 is purged with the inert gas G, and the container 300 is sealed by heat fusion of the heat seal layer. The inert gas G is, for example, nitrogen gas. Purging the inside of the container 300 with the inert gas G prevents the mixed resin 220 from coming into contact with oxygen. The mixed resin 220 is enclosed in the container 300 in a state where the pure water PW is attached thereto. This completes the packaging structure 310 in which the mixed resin 220 is enclosed (i.e., hermetically sealed) in the container 300. The packaging structure 310 is an example of a packaging structure for the mixed resin of the first embodiment.

[0071] Since the container 300 has a gas barrier layer containing a gas barrier resin, oxygen permeation into the inside of the container 300 is suppressed. This makes it possible to suppress oxidation of the mixed resin 220 inside the container 300. In addition, since the pure water PW adheres to the mixed resin 220, deterioration of the mixed resin 220 can be suppressed compared to the case where the mixed resin 220 is stored in a dry state.

[0072] Next, as shown in FIG. 2, the container 300 containing the mixed resin 220 is stored (storage step S103). For example, the container 300 containing the mixed resin 220 may be stored in a warehouse until there is a demand for using the mixed resin 220 in the boron adsorbent resin mixed ion exchange device 12 of the pure water production system 10. The method for storing the container 300 containing the mixed resin 220 is not particularly limited. It is sufficient that the container 300 containing the mixed resin 220 can be stored so that the container 300 containing the mixed resin 220 is not damaged. In addition, during storage, it is preferable that the mixed resin 220 is managed at a temperature at which the mixed resin 220 is unlikely to deteriorate, for example, at room temperature or in cool, dark conditions, avoiding direct sunlight.

[0073] 2 includes a storage step S103, but if there is a demand for immediate use of the mixed resin 220 in the boron adsorbent resin mixed ion exchange device 12 of the pure water production system 10, the storage step S103 is not necessary. That is, in one example of the method for managing the mixed resin, the storage step S103 can be omitted.

[0074] 2, the container 300 containing the mixed resin 220 is transported to the site where the pure water production system 10 is installed (transportation step S104). For example, when there is a demand for using the mixed resin 220 in the boron adsorbent resin mixed ion exchange device 12 of the pure water production system 10, the container 300 containing the mixed resin 220 is transported to the site where the pure water production system 10 is installed.

[0075] 2, the container 300 is opened, and the mixed resin 220 is filled into the boron adsorbent resin mixed ion exchange device 12 of the pure water production system 10 on-site (filling step S105). For example, when using the boron adsorbent resin mixed ion exchange device 12 of the pure water production system 10, the container 300 is opened, and the mixed resin 220 is filled into the boron adsorbent resin mixed ion exchange device 12. As a result, the boron adsorbent resin 210, the strongly acidic cation exchange resin 212, and the strongly basic anion exchange resin 214 are filled in a premixed state into the boron adsorbent resin mixed ion exchange device 12.

[0076] Thereafter, pure water or the like is introduced into the boron adsorbent resin mixed ion exchange apparatus 12 to wash the mixed resin 220, thereby starting up the boron adsorbent resin mixed ion exchange apparatus 12.

[0077] (Action and Effects) Next, the operation and effects of the first embodiment will be described.

[0078] In the mixed resin management method of the first embodiment, the boron adsorbent resin 210, the strongly acidic cation exchange resin 212, and the strongly basic anion exchange resin 214 are mixed (mixing step S101). Furthermore, the mixed resin 220 obtained by mixing the boron adsorbent resin 210, the strongly acidic cation exchange resin 212, and the strongly basic anion exchange resin 214 is sealed in a container 300 (sealing step S102). Furthermore, the container 300 is transported to the site where the pure water manufacturing system 10 is installed (transporting step S104). Then, when the boron adsorbent resin mixed ion exchange device 12 of the pure water manufacturing system 10 is used, the mixed resin 220 in the container 300 is filled into the boron adsorbent resin mixed ion exchange device 12 (filling step S105).

[0079] As a result, the boron adsorbent resin mixed ion exchange device 12 is filled with a mixed resin 220 in which the boron adsorbent resin 210, the strongly acidic cation exchange resin 212, and the strongly basic anion exchange resin 214 are mixed in advance.

[0080] Therefore, in the mixed resin management method of the first embodiment, the boron adsorbent resin mixed ion exchange apparatus 12 can be started up more quickly than in the case where the boron adsorbent resin, the strong acid cation exchange resin, and the strong basic anion exchange resin are each obtained separately and these three types of resins are placed in a mixed bed resin tower and then mixed.

[0081] This effect is believed to be due to the following phenomenon. Compared to other ion exchange resins, the boron adsorbent resin 210 is significantly more susceptible to thermal decomposition, etc. Therefore, depending on the storage conditions, thermal decomposition, etc. may progress significantly, which may have a significant impact on the start-up of the pure water system. When the boron adsorbent resin 210 and the strong acid cation exchange resin 212 are mixed, the boron adsorbent resin 210 is gradually thermally decomposed during storage, etc., and there is a risk that functional groups will be desorbed from the resin. However, the strong acid cation exchange resin 212 adsorbs these desorbed functional groups, thereby suppressing an increase in impurities in the mixed resin 220. Furthermore, when the strongly acidic cation exchange resin 212 and / or the strongly basic anion exchange resin 214 are mixed, the overall water content of the mixed resin 220 increases. Since the boron adsorbent resin 210 contains, for example, metals and impurities derived from the catalyst used during synthesis, these may be desorbed from the boron adsorbent resin 210 and promote the decomposition of functional groups of the boron adsorbent resin 210. However, if the water content increases, the metals and impurities derived from the catalyst used during synthesis are diffused into the water, suppressing this effect. Furthermore, cations of metals and impurities derived from the catalyst are adsorbed onto the strongly acidic cation exchange resin 212 .

[0082] Since these phenomena occur in a complex manner, the effect of accelerating the start-up varies depending on the ion exchange resin to be mixed. From the viewpoint of accelerating the start-up, any of weakly basic anion exchange resins, weakly acidic cation exchange resins, strongly basic anion exchange resins, and strongly acidic cation exchange resins are preferable, and strongly acidic cation exchange resins and weakly acidic cation exchange resins are more preferable. Although inactive resins also have the effect of accelerating the start-up, they are not preferable because they are not useful for improving the quality of pure water when the water is passing through.

[0083] From the viewpoint of enabling early start-up, the mixing ratio of the boron adsorbent resin to the ion exchange resin is preferably 0.05 or more and 4 or less. Moreover, from the viewpoint of improving the water quality in the production of pure water, the mixing ratio of the ion exchange resin to be mixed with the boron adsorbent resin is preferably 0.2 or more and 3.5 or less.

[0084] Moreover, in the mixed resin management method of the first embodiment, the container 300 is provided with a gas barrier layer containing a gas barrier resin. This prevents gas such as oxygen from passing from the outside of the container 300 into the container 300. Therefore, in the mixed resin management method of the first embodiment, deterioration of the mixed resin 220 in the container 300 due to oxidation or the like can be prevented.

[0085] Moreover, the mixed resin 220 is sealed in the container 300 in a state in which the inside of the container 300 is replaced with an inert gas G. Therefore, in the mixed resin management method of the first embodiment, deterioration due to oxidation of the mixed resin 220 in the container 300 can be suppressed compared to a case in which a gas such as oxygen remains in the container.

[0086] In addition, the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 are mixed in the pure water PW, and the mixed mixed resin 220 is sealed in the container 300, and the mixed resin 220 is stored in a wet state until the boron adsorbent resin mixed ion exchange device 12 is used. Therefore, in the mixed resin management method of the first embodiment, the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 can be mixed smoothly compared to the case where only gas is introduced into the boron adsorbent resin, the strong basic anion exchange resin, and the strong acid cation exchange resin and mixed. And, even if the boron adsorbent resin 210, the strong acid cation exchange resin 212, and the strong basic anion exchange resin 214 are mixed in advance, the mixed resin 220 can be stored in a sealed state in the container 300.

[0087] In the packaging structure 310 for the mixed resin 220 of the first embodiment, the mixed resin 220 obtained by mixing the boron adsorbent resin 210, the strongly acidic cation exchange resin 212, and the strongly basic anion exchange resin 214 is sealed in the container 300. This allows the mixed resin 220 to be filled into the boron adsorbent resin mixed ion exchange device 12. Therefore, in the packaging structure 310 for the mixed resin 220 of the first embodiment, the boron adsorbent resin, the strongly acidic cation exchange resin, and the strongly basic anion exchange resin are obtained individually, and these three types of resins are each placed in a mixed bed resin tower and then mixed, so that the start-up of the boron adsorbent resin mixed ion exchange device 12 can be made faster.

[0088] In addition, the container 300 includes a gas barrier layer containing a gas barrier resin. Therefore, in the packaging structure 310 for the mixed resin 220 of the first embodiment, deterioration of the mixed resin 220 in the container 300 due to oxidation or the like can be suppressed.

[0089] In the packaging structure 310 for the mixed resin 220 of the first embodiment, the mixed resin 220 is sealed in the container 300 in a state in which the inside of the container 300 is replaced with an inert gas G. Therefore, in the packaging structure 310 for the mixed resin 220 of the first embodiment, deterioration due to oxidation of the mixed resin 220 in the container 300 can be suppressed compared to a case in which a gas such as oxygen remains in the container.

[0090] [Second embodiment] Next, a description will be given of an ultrapure water producing system according to the second embodiment. Fig. 5 is a configuration diagram showing an ultrapure water producing system 20 according to the second embodiment.

[0091] As shown in FIG. 5, the ultrapure water production system 20 is an ultrapure water production system that uses the pure water production apparatus 10, and includes a secondary pure water system 26 downstream of the pure water production apparatus 10.

[0092] The ultrapure water production system 20 is equipped with a pretreatment device 11, a two-bed three-tower device 22, a reverse osmosis membrane device 23, and an ultraviolet oxidation device 24 in that order, and treated water from the ultraviolet oxidation device 24 is supplied to a boron adsorbent resin mixed ion exchange device 12. The boron adsorbent resin mixed ion exchange device 12 is filled with a mixed resin 220 similar to that of the first embodiment. The mixed resin 220 is applied with a mixed resin management method and mixed resin packaging structure 310 similar to those of the first embodiment. The pretreatment device 11 may be equipped with a sand filtration device, an activated carbon treatment device, or the like.

[0093] In the ultrapure water production system 20, a secondary pure water system 26 is connected to the downstream side of the boron adsorbent resin mixed ion exchange device 12 via a tank 25 that stores treated water from the boron adsorbent resin mixed ion exchange device 12. The secondary pure water system 26 includes, for example, an ultraviolet oxidation device, a non-regenerative polisher, a membrane degassing device, and an ultrafiltration device, and produces ultrapure water by reducing the total organic carbon (TOC) concentration in the primary pure water to about 1 μgC / L. A mixed bed ion exchange device (MB), an electrodeionization device (EDI), etc. may be installed downstream of the boron adsorbent resin mixed ion exchange device 12. By using this system, it is possible to produce ultrapure water with extremely low boron concentration, for example, 1 ng / L or less.

[0094] [Third embodiment] Next, an ultrapure water producing system according to the third embodiment will be described below. Fig. 6 is a configuration diagram showing an ultrapure water producing system 30 according to the third embodiment.

[0095] As shown in FIG. 6, the ultrapure water producing system 30 has the same configuration as the ultrapure water producing system 20 of the second embodiment, except that it is equipped with two-stage reverse osmosis membrane devices 31, 32 instead of the two-bed, three-tower device 22 and the reverse osmosis membrane device 23.

[0096] The ultrapure water production system 30 comprises a pretreatment device 11, a reverse osmosis membrane device 31, a reverse osmosis membrane device 32, an ultraviolet oxidation device 24, a boron adsorbent resin mixed ion exchange device 12, a tank 25, and a secondary pure water system 26 in that order.

[0097] In the ultrapure water production system 30, the first-stage reverse osmosis membrane device 31 removes ionic components, nonionic organic matter, and fine particles from the pretreated water. In the first-stage reverse osmosis membrane device 31, an alkali such as sodium hydroxide may be added at the inlet to remove dissolved carbon dioxide, thereby adjusting the pH of the water to an alkaline level of, for example, 7.5 to 11.0.

[0098] The second-stage reverse osmosis membrane device 32 removes ionic components remaining in the permeated water from the first-stage reverse osmosis membrane device 31. A portion of the concentrated water from the first-stage and second-stage reverse osmosis membrane devices 31, 32 may be supplied to the water inlet of the first-stage reverse osmosis membrane device 31. In this way, by using two-stage reverse osmosis membrane devices, it is possible to obtain ultrapure water with a significantly reduced boron concentration while increasing the water recovery rate. It is possible to produce ultrapure water with a boron concentration of, for example, 1 ng / L or less.

[0099] [Fourth embodiment] Next, a description will be given of an ultrapure water producing system according to the fourth embodiment. Fig. 7 is a configuration diagram showing an ultrapure water producing system 40 according to the third embodiment.

[0100] As shown in FIG. 7, the ultrapure water producing system 40 differs from the ultrapure water producing system 20 of the second embodiment in that it is equipped with a reverse osmosis membrane device 41 and an electric deionization device 42 instead of the two-bed, three-tower device 22 and the reverse osmosis membrane device 23. However, the ultrapure water producing system 40 has the same configuration as the ultrapure water producing system 20 of the second embodiment.

[0101] The ultrapure water production system 40 comprises a pretreatment device 11, a reverse osmosis membrane device 41, an electric deionization device 42, an ultraviolet oxidation device 24, a boron adsorbent resin mixed ion exchange device 12, a tank 25, and a secondary pure water system 26 in that order.

[0102] In the ultrapure water production system 40, the reverse osmosis membrane device 41 can remove ionic components that cause scale formation in the electrodeionization device 42. Furthermore, since boron is also slightly removed in the electrodeionization device 42, ultrapure water with a significantly reduced boron concentration can be obtained, and the life of the boron adsorbent resin mixed ion exchange device 12 can be extended. Furthermore, since the removal of ionic components is performed by the reverse osmosis membrane device 41 and the electrodeionization device 42, if the boron adsorbent resin mixed ion exchange device 12 is configured as a non-regenerative type, an ultrapure water production system 40 that does not require chemical regeneration can be constructed.

[0103] In the ultrapure water manufacturing systems of the second to fourth embodiments, the mixed resin 220 filled in the boron adsorbent resin mixed ion exchange device 12 is subjected to the same mixed resin management method and mixed resin packaging structure 310 as in the first embodiment. Therefore, the same actions and effects can be obtained by the same configuration and management method as in the first embodiment.

[0104] In the first to fourth embodiments, a mixed resin obtained by mixing a boron adsorbent resin, a strong acid cation exchange resin, and a strong basic anion exchange resin is used, but the present disclosure is not limited thereto. For example, a mixed resin obtained by mixing a boron adsorbent resin and a strong basic anion exchange resin may be used, or a mixed resin obtained by mixing a boron adsorbent resin and a strong acid cation exchange resin may be used.

[0105] Furthermore, although the present disclosure has been described in detail with respect to a particular embodiment, the present disclosure is not limited to such embodiment, and it will be apparent to those skilled in the art that various other embodiments are possible within the scope of the present disclosure. EXAMPLES

[0106] Next, examples will be described. In Examples 1 and 2, a boron adsorbent resin mixed ion exchange device 12 shown in FIG.

[0107] Example 1 Three types of resins, namely, boron adsorbent resin (Diaion CRB03, manufactured by Mitsubishi Chemical Corporation, exchange capacity: 0.8 meq / mL), strongly acidic cation exchange resin (Duolite CGP, manufactured by Rohm and Haas Co., exchange capacity: 2.0 meq / mL), and strongly basic anion exchange resin (Duolite AGP, manufactured by Rohm and Haas Co., exchange capacity: 1.1 meq / mL), were obtained in a bag. Then, immediately after opening each bag of the three types of resin, 750 mL of boron adsorbent resin, 530 mL of strongly acidic cation exchange resin, and 1920 mL of strongly basic anion exchange resin were mixed. The three types of resins were mixed by the same mixing method as in the first embodiment. As a result, a mixed resin was produced in which the boron adsorbent resin, the strongly basic anion exchange resin, and the strongly acidic cation exchange resin were mixed.

[0108] The mixed resin immediately after the production was filled into the boron adsorbent resin mixed ion exchange device 12. Then, isopropyl alcohol (IPA) in an amount of 15 μg / L and boric acid (H3BO3) in an amount of 0.41 μg / L were added as TOC components to ultrapure water with a resistivity of 18.0 MΩ·cm or more and a boron (B) concentration of 10 ng / L (as B) or less, and the water was passed through the boron adsorbent resin mixed ion exchange device 12 at a flow rate of 1700 mL / min (space velocity SV = 32 / h, linear velocity LV = 52 m / L). The outlet water of the boron adsorbent resin mixed ion exchange device 12 was periodically collected and the TOC was measured. In addition, the outlet water of the boron adsorbent resin mixed ion exchange device 12 was collected at predetermined time intervals and the resistivity was measured. The TOC measurement results are shown in the graph of Fig. 8, with the horizontal axis representing the time that water was passed through the boron adsorbent resin mixed ion exchange device 12 and the vertical axis representing the TOC of the treated water from the boron adsorbent resin mixed ion exchange device 12. The resistivity measurement results are shown in the graph of Fig. 9, with the horizontal axis representing the time that water was passed through the boron adsorbent resin mixed ion exchange device 12 and the vertical axis representing the resistivity. The measurement results using the mixed resin immediately after production were used as initial data.

[0109] In Example 1, the mixed resin obtained by mixing the boron adsorbent resin, the strongly basic anion exchange resin, and the strongly acidic cation exchange resin was filled in a container 300 (bag) (Speren 35E type, manufactured by UBE Corporation) having a gas barrier layer made of ethylene-vinyl acetate copolymer (EVOH) in a wet state after replacing with nitrogen gas, and the container 300 was sealed. The water content of the ion exchange resin in the sealed state was 70% by weight. In this state, the container 300 containing the mixed resin was stored. This storage method is called the first storage method. The container 300 containing the mixed resin was stored for 30 days. After the storage days had elapsed, the container 300 was opened and the mixed resin was filled into the boron adsorbent resin mixed ion exchange device 12.

[0110] In Example 1, water was passed through the boron adsorbent resin mixed ion exchange device 12 under the same conditions as those for the mixed resin immediately after production described above, and the TOC and resistivity were measured. The TOC measurement results are shown in the graph of Fig. 8, with the horizontal axis representing the time of passing water through the boron adsorbent resin mixed ion exchange device 12 and the vertical axis representing the TOC of the treated water from the boron adsorbent resin mixed ion exchange device 12. The resistivity measurement results are shown in the graph of Fig. 9, with the horizontal axis representing the time of passing water through the boron adsorbent resin mixed ion exchange device 12 and the vertical axis representing the resistivity.

[0111] Example 2 A mixed resin was produced by mixing a boron adsorbent resin, a strongly basic anion exchange resin, and a strongly acidic cation exchange resin under the same conditions as in Example 1. The produced mixed resin was then sealed in a normal container (bag) (made of low density polyethylene (LDPD), 0.03 mm thick) without a gas barrier layer, and the container was sealed. At this time, the air in the container was not replaced with nitrogen gas. In this state, the container in which the mixed resin was sealed in a wet state was stored. This storage method is the second storage method. The container in which the mixed resin was sealed was stored for the same number of days as in Example 1. After the number of storage days had elapsed, the container was opened and the mixed resin was filled into the boron adsorbent resin mixed ion exchange device 12.

[0112] In Example 2, water was passed through the boron adsorbent resin mixed ion exchange device 12 under the same conditions as in Example 1, and the TOC and resistivity were measured. The TOC measurement results are shown in the graph of FIG. 8. The resistivity measurement results are shown in the graph of FIG. 9.

[0113] Comparative Example 1 As in Example 1, three types of resins, boron adsorbent resin, strong acid cation exchange resin, and strong basic anion exchange resin, were obtained in a bag. Then, the boron adsorbent resin, strong acid cation exchange resin, and strong basic anion exchange resin were each transferred separately to a normal container without a gas barrier layer similar to Example 2, and each container was sealed. At this time, the air in the container was not replaced with nitrogen gas. In this state, the container in which the mixed resin was sealed in a wet state was stored (second storage method). The container in which the mixed resin was sealed was stored for the same number of days as in Example 1.

[0114] After the storage period, the containers of the three resins were opened, and the three resins were filled in the same amounts as in Example 1 into a mixed bed tower, which was an actual equipment. The three resins were then mixed in the mixed bed tower. In the mixed bed tower, pure water was introduced from the bottom of the mixed bed tower to mix the three resins.

[0115] After mixing the three types of resins, water was passed through the mixed bed tower and the TOC and resistivity were measured under the same conditions as in Example 1. The TOC measurement results are shown in the graph of Figure 8. The resistivity measurement results are shown in the graph of Figure 9.

[0116] Comparative Example 2 Two types of resins, a boron adsorbent resin and a strong basic anion exchange resin, were obtained in a bag. Then, the boron adsorbent resin and the strong basic anion exchange resin were separately transferred to normal containers without a gas barrier layer similar to Comparative Example 2, and each container was sealed. At this time, the air in the container was not replaced with nitrogen gas. In this state, the container in which the mixed resin was sealed in a wet state was stored (second storage method). The container in which the mixed resin was sealed was stored for the same number of days as in Example 1.

[0117] After the storage period had elapsed, the containers containing the two types of resins were opened, and the two types of resins in the same amounts as in Example 1 were loaded into a mixed bed tower, which was an actual machine, in the same manner as in Comparative Example 1. Then, the two types of resins were mixed in the mixed bed tower.

[0118] After mixing the two types of resins, water was passed through the mixed bed tower and the TOC was measured under the same conditions as in Example 1. The results of the TOC measurement are shown in the graph of FIG.

[0119] In the initial data, Example 1, Example 2, Comparative Example 1, and Comparative Example 2, the TOC concentration was measured with a TOC concentration meter (Anatel A1000 XP, manufactured by Anatel), and the resistivity was measured with a resistivity meter (HORIBA HE-960RW).

[0120] From FIG. 8, in Example 1, it can be seen that the TOC is reduced in a short time by sealing and storing the mixed resin obtained by mixing the boron adsorbent resin, the strongly basic anion exchange resin, and the strongly acidic cation exchange resin in the container 300 in a state where the atmosphere is replaced with nitrogen gas. Also, in Example 2, it can be seen that the TOC is reduced in a short time by sealing and storing the mixed resin obtained by mixing the boron adsorbent resin, the strongly basic anion exchange resin, and the strongly acidic cation exchange resin in a normal container. The measured values ​​of TOC in Examples 1 and 2 are close to the initial data. For example, the start-up of the boron adsorbent resin mixed ion exchange device 12 is completed when the TOC reaches about 1.0 ppb.

[0121] 9, in Examples 1 and 2, resistivity is almost constant from the beginning of water flow through the boron adsorbent resin mixed ion exchange device 12, similar to the initial data. Resistivity is a value that indicates how difficult it is for electricity to pass, and a higher resistivity value indicates less contamination. This shows that in Examples 1 and 2, the outlet water from the boron adsorbent resin mixed ion exchange device 12 is almost pure water (fewer ions, etc.).

[0122] For this reason, in Examples 1 and 2, it is understood that the start-up of the boron adsorbent resin mixed ion exchange device 12 filled with the mixed resin is quick.

[0123] [Preferred embodiment of the present disclosure] Preferred aspects of the present disclosure will be described below.

[0124] [Additional note 1] Mixing a boron adsorbent resin with at least one of a basic anion exchange resin and an acidic cation exchange resin; The mixed resin is placed in a sealed container in a wet state, A method for managing a mixed resin, comprising transporting the sealed container containing the mixed resin to a site where a pure water production apparatus for producing pure water is installed, and filling the boron adsorbent resin mixed ion exchange apparatus installed in the pure water production apparatus with the mixed resin inside the sealed container when the boron adsorbent resin mixed ion exchange apparatus is used.

[0125] [Additional note 2] 2. The method for managing a mixed resin according to claim 1, wherein the sealed container has a gas barrier layer containing a gas barrier resin or a metal.

[0126] [Additional note 3] The method for managing a mixed resin according to claim 1 or 2, wherein the mixed resin is sealed in the sealed container in a state in which the inside of the sealed container is replaced with an inert gas.

[0127] [Additional note 4] The boron adsorbent resin is mixed with at least one of the basic anion exchange resin and the acidic cation exchange resin in pure water; The mixed resin is sealed in the sealed container, and the mixed resin is stored in a wet state until the boron adsorbent resin mixed ion exchange device is used.

[0128] [Additional note 5] A packaging structure for a mixed resin, in which a mixed resin obtained by mixing a boron adsorbent resin with at least one of a basic anion exchange resin and an acidic cation exchange resin is sealed in a sealed container.

[0129] [Additional note 6] 6. The mixed resin packaging structure according to claim 5, wherein the sealed container has a gas barrier layer containing a gas barrier resin or a metal.

[0130] [Additional note 7] 7. The packaging structure for a mixed resin according to claim 5 or 6, wherein the mixed resin is sealed in the sealed container with the inside of the sealed container replaced with an inert gas. [Explanation of symbols]

[0131] 10 Pure water production equipment 12 Boron adsorbent resin mixed ion exchange device 20 Ultrapure water production system 30 Ultrapure water production system 40 Ultrapure water production system 210 Boron Adsorbent Resin 212 Strongly acidic cation exchange resin 214 Strongly basic anion exchange resin 220 Mixed resin 300 containers 310 Packaging structure G Inert gas PW pure water

Claims

1. Mixing a boron adsorbent resin with at least one of a basic anion exchange resin and an acidic cation exchange resin; The mixed resin is placed in a sealed container in a wet state, A method for managing a mixed resin, comprising transporting the sealed container containing the mixed resin to a site where a pure water production apparatus for producing pure water is installed, and filling the boron adsorbent resin mixed ion exchange apparatus installed in the pure water production apparatus with the mixed resin inside the sealed container when the boron adsorbent resin mixed ion exchange apparatus is used.

2. The method for managing a mixed resin according to claim 1 , wherein the sealed container has a gas barrier layer containing a gas barrier resin or a metal.

3. The method for managing a mixed resin according to claim 1 , wherein the mixed resin is sealed in the sealed container with the inside of the sealed container replaced with an inert gas.

4. The boron adsorbent resin is mixed with at least one of the basic anion exchange resin and the acidic cation exchange resin in pure water; 2. The method for managing a mixed resin according to claim 1, further comprising the steps of: sealing the mixed resin in the sealed container; and storing the mixed resin in a wet state until the boron adsorbent resin-mixed ion exchange device is used.

Citation Information

Patent Citations

  • Time setting device for timer

    JP1988010819A

  • Method for reducing eluted substance from mixed resin bed

    JP1990099146A

  • Packing material for ion-exchange resin

    JP1996053162A

  • Method and device for production of pure water or ultrapure water

    JP1996084986A

  • Method for conditioning ion exchange resin and ion exchange device

    JP1997070546A