Tea processed products and their manufacturing method

A particulate tea product with controlled sphericity and particle size, produced via a rotor-type granulator, addresses dispersibility issues in powdered green tea, ensuring rapid wetting and dispersibility, improved flowability, and convenient packaging.

JP7575214B2Active Publication Date: 2024-10-29AMOREPACIFIC CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2020135009
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-08-21
Filing Date
2020-08-07
Publication Date
2024-10-29
Estimated Expiration
2040-08-07

AI Technical Summary

Technical Problem

Powdered green tea products face issues with dispersibility in water, leading to inconvenience and potential defects during packaging and consumption due to cohesive forces and low fluidity, especially in stick-form packaging.

Method used

A particulate tea product with tea particles having a sphericity of 0.68 or more, an average particle size of 100 to 300 μm, and minimal fine powder content, produced using a rotor-type fluidized bed granulator with controlled water application, ensuring rapid wetting and dispersibility.

Benefits of technology

The processed tea product achieves quick wetting and dispersibility in water, maintaining a dispersed state without aggregation, enhancing flowability and ease of packaging, and eliminating the need for stirring, with improved palatability and reduced packaging defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007575214000005
    Figure 0007575214000005
  • Figure 0007575214000006
    Figure 0007575214000006
  • Figure 0007575214000007
    Figure 0007575214000007
Patent Text Reader

Abstract

To provide a particulate processed product of tea which is readily wetted and dispersed in water, and a method for preparing the same.SOLUTION: There are disclosed a particulate processed product of tea and a method for preparing the same. In the particulate processed product of tea, when the cumulative distribution of the spherical degree of the tea particles is measured, the sphericity S10 value of the particles corresponding to 10% from the bottom of the cumulative distribution is 0.68 or more. The processed product of tea is convenient to drink because it is readily wetted and dispersed in water. In addition, it can be easily packaged and used due to a low angle of repose and thus excellent flowability.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] [CROSS REFERENCE TO RELATED APPLICATIONS] This application claims priority to Korean Patent Application No. 10-2019-0102336, filed on August 21, 2019, the entire contents of which are incorporated herein by reference.

[0002] Disclosed herein is a particulate tea product that quickly wets and disperses in water and a method for making the same. [Background technology]

[0003] In order to drink powdered green tea, tea utensils and tea ceremony tools are required, and the dispersibility is reduced due to the cohesive force between the particles, which makes it inconvenient to consume a lot of time. In recent years, many products have been sold in disposable stick packaging so that powdered green tea can be put into a water bottle or tumbler for drinking, but the problem remains that the powder hardens when put into water and is difficult to disperse, and it is inconvenient to have to shake it for a considerable amount of time before drinking it. In addition, in the case of stick-type products in which powdered green tea is packaged in small amounts (e.g., Rishi Matcha travel packs, Rishi-Tea, USA), it is difficult to dispense the powdered green tea in a fixed amount due to the low fluidity of the powder, and there is a high possibility of defects occurring due to fine powder during sealing. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Korean Patent Publication No. 10-2006-0090894 Summary of the Invention [Problem to be solved by the invention]

[0005] In one aspect, the present disclosure aims to provide a particulate tea product that quickly wets and disperses in water.

[0006] In another aspect, the present specification aims to provide a method for producing a particulate tea product that quickly wets and disperses in water. [Means for solving the problem]

[0007] In one aspect, the technology disclosed herein is a particulate tea product, the tea product comprising tea particles, the tea particles having a sphericity S of 0.68 or more. 10 The sphericity S 10 The value is the sphericity of the particles that falls in the bottom 10% of the cumulative distribution when the cumulative distribution of the sphericity of tea particles is measured, and provides a granular tea process.

[0008] In an exemplary embodiment, when the cumulative distribution of the sphericity of the tea particles is measured, the sphericity S of the particles corresponding to a distribution rate of 50% is 50 The value may be 0.80 or greater.

[0009] In an exemplary embodiment, the sphericity S 10 The value may be 0.70 or greater.

[0010] In an exemplary embodiment, the sphericity S 10 The value may be between 0.72 and 0.84.

[0011] In an exemplary embodiment, when a cumulative distribution of the sphericity of the tea particles is measured, the sphericity S of the particles corresponding to the bottom 90% of the cumulative distribution is 90 value and the sphericity S of the particles that fall into the bottom 10% of the cumulative distribution 10 Difference from the value (S 90 -S 10 ) may be less than 0.20.

[0012] In an exemplary embodiment, the S 90 -S 10 may be less than 0.15.

[0013] In an exemplary embodiment, the processed tea product may have an average particle size of whole tea particles of 100 to 300 μm.

[0014] In an exemplary embodiment, the fine powder may be contained in an amount of 20% by weight or less based on the total weight of the tea particles, and the fine powder may have a particle size of 75 μm or less.

[0015] In an exemplary embodiment, the tea particles may have one or more particle size distribution values ​​among the following i) to iii): i) Particle size distribution D 10 values ​​≥ 50 μm; ii) Particle size distribution D 50 value is 100 μm or more; and iii) Particle size distribution D 90 Value is 200μm or more.

[0016] In the above i) to iii), D 10 , D 50 , D 90 respectively mean the particle size of the bottom 10% of particles in the cumulative distribution, the median particle size, and the particle size of the bottom 90% of particles in the cumulative distribution when the cumulative distribution of particle sizes of tea particles is measured.

[0017] In an exemplary embodiment, the particle size distribution D 10 Value is 50μm≦D 10 ≦200 μm, and the particle size distribution D 50 Value is 100μm≦D 50 ≦250 μm, and the particle size distribution D 90 Value is 200μm≦D 90 It may be ≦600 μm.

[0018] In an exemplary embodiment, the tea product may have an angle of repose of 35° or less.

[0019] In an exemplary embodiment, the tea processed product may have a wetting time of 100 seconds or less when contacted with water, and the wetting time may be the time it takes for the entire tea processed product to sink below the surface of the water when 1.5 g of the tea processed product is placed on the surface of the water.

[0020] In an exemplary embodiment, the tea may be tea leaves.

[0021] In an exemplary embodiment, the tea may be one or more selected from the group consisting of unfermented tea, semi-fermented tea, fermented tea, and post-fermented tea.

[0022] In an exemplary embodiment, the tea may be green tea.

[0023] In an exemplary embodiment, the tea product may be in the form of granules or powder.

[0024] In another aspect, the technology disclosed herein provides a method for producing a particulate tea product, the method comprising the step of producing the particulate tea product.

[0025] In an example embodiment, the method may be to manufacture a granulated tea product using a rotor-type fluidized bed granulator including a rotating plate.

[0026] In an illustrative embodiment, the rotor-type fluidized bed granulator may include a container; and a rotating plate installed inside the container, a gap forming unit installed between the rotating plate and a wall of the container to supply air, and a nozzle forming unit installed adjacent to the gap forming unit to inject water into the inside of the container.

[0027] In an exemplary embodiment, the manufacturing method may include the steps of placing tea powder on a rotating plate and rotating the rotating plate; supplying air to levitate the tea powder; and spraying water onto the levitated tea powder.

[0028] In an exemplary embodiment, the tea powder may have a particle size of 75 μm or less, which corresponds to 99% or more by weight based on the total weight of the tea powder. Effect of the Invention

[0029] In one aspect, the technology disclosed herein has the advantage of providing a particulate tea product that quickly wets and disperses in water.

[0030] In another aspect, the technology disclosed herein has the advantage of providing a method for producing particulate tea products that are quickly wetted and dispersed in water.

[0031] The processed tea product according to the present specification is convenient to drink as it quickly wets and disperses in water, and has a low angle of repose, which makes it easy to flow and package as a product. [Brief description of the drawings]

[0032] [Figure 1] FIG. 1 shows a photograph of a tea product dispersed in water, visually observed immediately (13 seconds) after the sample of Example 2 was placed in water and the wetting time was measured according to an experimental example of the present specification. [Diagram 2] FIG. 2 shows a photograph of a tea product dispersed in water, visually observed immediately (11 seconds) after the sample of Example 3 was placed in water and the wetting time was measured according to an experimental example of the present specification. [Diagram 3] FIG. 3 shows a photograph of a tea product dispersed in water, visually observed immediately (23 seconds) after the sample of Example 4 was placed in water and the wetting time was measured according to an experimental example of the present specification. [Figure 4] FIG. 4 shows a photograph of the sample of Comparative Example 1 dispersed in water after 3 minutes had elapsed since being placed in water according to an experimental example of the present specification, as observed with the naked eye. [Diagram 5] FIG. 5 shows a photograph of the sample of Comparative Example 4 dispersed in water after 3 minutes had elapsed since being placed in water according to an experimental example of the present specification, the photograph being observed with the naked eye. [Figure 6]FIG. 6 shows a photograph of the sample of Comparative Example 5 dispersed in water after 3 minutes had elapsed since being placed in water according to an experimental example of the present specification, the photograph being observed with the naked eye. [Figure 7] FIG. 7 shows a photograph of the sample of Comparative Example 6 dispersed in water after 3 minutes had elapsed since being placed in water according to an experimental example of the present specification, the photograph being observed with the naked eye. [Figure 8] 8 shows a photograph of the sample of Comparative Example 7 dispersed in water after 3 minutes had elapsed since being placed in water according to an experimental example of the present specification. Even after 3 minutes, the samples of Comparative Examples 1 and 4 to 7 were not wetted and a considerable amount of the samples remained on the water surface. [Figure 9] FIG. 9 shows a photograph of the tea product of Example 3 visually observed after it was placed in a water bottle containing 500 mL of water and turned upside down once. [Figure 10] FIG. 10 shows a photograph of the tea product of Example 3, which was visually observed after being placed in a beaker containing 500 mL of water and stirred once. [Figure 11] FIG. 11 shows a photograph of the visually observed dispersion state after 1.5 g of the sample of Example 1 was placed in a beaker containing 500 mL of water and allowed to stand for 20 seconds according to an experimental example of the present specification. [Figure 12] FIG. 12 shows a photograph of the visually observed dispersion state after 1.5 g of the sample of Comparative Example 8 was placed in a beaker containing 500 mL of water and allowed to stand for 20 seconds according to an experimental example of the present specification. [Figure 13] FIG. 13 is a schematic diagram of a rotor-type fluidized bed granulator according to one embodiment of the present specification. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0033] The present invention will be described in detail below.

[0034] In one aspect, the technology disclosed herein is a particulate tea product, the tea product comprising tea particles, the tea particles having a sphericity S of 0.68 or more. 10The sphericity S 10 The value is the sphericity of the particles that is in the bottom 10% of the cumulative distribution when the cumulative distribution of the sphericity of tea particles is measured, and provides a granular tea product.

[0035] In an exemplary embodiment, the processed tea product may be made of tea particles.

[0036] In an example embodiment, the tea particles may be made of tea powder.

[0037] In this specification, "particulate tea processed product" means a processed tea product having a particulate form. The tea processed product may have a particulate form formed by agglomeration of multiple tea powder particles. For example, the tea processed product may include tea particles formed by adding water to tea powder and agglomerating multiple tea powder particles. When water is added to a finely powdered dried product, the powder components become sticky, and the sticky properties cause them to agglomerate together to form particles that are about 30 to 150 times larger than the powder. Such particles that are dried are sometimes called fine particles or granules, and powders are generally used in a fine or granular form to improve flowability and shelf life.

[0038] In an example embodiment, the particles may have a spherical or elliptical shape. In this specification, "tea powder" refers to a powder obtained from tea plants (Camellia sinensis) as a raw material, and may be, for example, a powder obtained by crushing, crushing or grinding tea plant leaves, or a powder obtained by powdering an extract or extract of tea plant leaves through a process such as spray drying. The tea leaves can be used without any particular restrictions on the harvesting time, the presence or absence of processing, or the processing method.

[0039] In an exemplary embodiment, the tea powder can be obtained using a grinding device. Grinding devices can be broadly classified into crushers, grinders, and the like. Crushers are devices that crush large solid lumps, and examples of such devices include jaw crushers and gyratory crushers. Grinders are devices that further grind powder that has been primarily ground in a crusher into finer products, or grind powder without the need for primary grinding, and include hammer mills, roller mills, ball mills, attrition mills, and air-flow type mills. When powdered green tea is produced by grinding tea leaves, grinding devices, particularly electric mills, ball mills, hammer mills, and the like, are used.

[0040] In an exemplary embodiment, the tea powder may have a particle size of 50 μm or less, or 1 to 50 μm, or 10 to 50 μm.

[0041] In an exemplary embodiment, the tea powder may have a particle size of 75 μm or less, which corresponds to 99% or more by weight based on the total weight of the tea powder.

[0042] In an exemplary embodiment, the tea may be tea leaves.

[0043] In an exemplary embodiment, the tea may be one or more selected from the group including unfermented tea, such as green tea, fermented tea, such as black tea, semi-fermented tea, such as oolong tea, white tea, flower tea, and post-fermented tea, such as pu-erh tea, yellow tea, and the like.

[0044] In an exemplary embodiment, the tea may be green tea.

[0045] In an exemplary embodiment, the tea may be green tea leaves.

[0046] In one exemplary embodiment, the processed tea product may be 100% tea powder without using other additives, and in another exemplary embodiment, the processed tea product may be 90% or more by weight, or 95% or more by weight, of the tea powder based on the total weight of the processed tea product.

[0047] In this specification the sphericity of tea particles may refer to the sphericity of the particulate tea product.

[0048] The tea processed product according to the present specification has excellent wettability and dispersibility (diffusibility of particles). The tea processed product has such a fast dispersion speed that it is unnecessary to perform a process of stirring or shaking to disperse conventional powdered green tea or powdered green tea granules in water. In addition, the tea processed product has excellent redispersibility, so that the particles do not stick to each other or aggregate after being dispersed in water, and the dispersed state is maintained over time. The tea processed product exhibits excellent dispersibility and redispersibility in both cold water and hot water, regardless of the temperature of the water.

[0049] In addition, the processed tea product according to the present specification has an advantage of excellent flowability or fluidity, which makes it easy to package, providing advantageous advantages in manufacturing processes such as filling and sealing when packaging sticks (e.g., it is easy to package a fixed amount and prevents defects that may occur during sealing), and is convenient for consumers to use because particles can be easily removed.

[0050] In an exemplary embodiment, the sphericity S 10 The value may be 0.68 or more, 0.69 or more, 0.70 or more, 0.71 or more, 0.72 or more, or 0.73 or more.

[0051] In an exemplary embodiment, the sphericity S 10 The value may be between 0.68 and 0.88.

[0052] In another exemplary embodiment, the sphericity S 10The value may be 0.68 or more, 0.69 or more, 0.70 or more, 0.71 or more, 0.72 or more, or 0.73 or more, and 0.88 or less, 0.87 or less, 0.86 or less, 0.85 or less, 0.84 or less, 0.83 or less, or 0.82 or less.

[0053] In an exemplary embodiment, the sphericity S 10 The value may be between 0.72 and 0.84.

[0054] In an exemplary embodiment, when a cumulative distribution of the sphericity of the tea particles is measured, the sphericity S of the particles corresponding to the bottom 90% of the cumulative distribution is 90 value and the sphericity S of the particles that fall into the bottom 10% of the cumulative distribution 10 Difference from the value (S 90 -S 10 ) may be less than 0.20.

[0055] In an exemplary embodiment, the S 90 -S 10 may be less than 0.15.

[0056] In an exemplary embodiment, the processed tea product may have an average particle size of whole tea particles of 100 to 300 μm.

[0057] In another exemplary embodiment, the processed tea product may have an average particle size of whole tea particles of 100 μm or more, 110 μm or more, 120 μm or more, 130 μm or more, 140 μm or more, 150 μm or more, 160 μm or more, 170 μm or more, 180 μm or more, 190 μm or more, or 200 μm or more, and 300 μm or less, 290 μm or less, 280 μm or less, 270 μm or less, 260 μm or less, 250 μm or less, 240 μm or less, 230 μm or less, 220 μm or less, 210 μm or less, or 200 μm or less.

[0058] In an exemplary embodiment, the processed tea product may contain 20% by weight or less of fine powder based on the total weight of the tea particles.

[0059] In this specification, the term "fine powder" refers to tea particles having a size, i.e., a particle diameter (also referred to as particle size or grain size) of 75 μm (200 mesh) or less. In this specification, the particle diameter may refer to the longest diameter of the particle.

[0060] In an exemplary embodiment, the processed tea product may contain 20% by weight or less, 19% by weight or less, 18% by weight or less, 17% by weight or less, 16% by weight or less, 15% by weight or less, 14% by weight or less, 13% by weight or less, 12% by weight or less, 11% by weight or less, 10% by weight or less, 9% by weight or less, 8% by weight or less, 7% by weight or less, 6% by weight or less, 5% by weight or less, 4% by weight or less, 3% by weight or less, 2% by weight or less, or 1% by weight or less of fine powder based on the total weight of tea particles. In another exemplary embodiment, the processed tea product may contain no fine powder or 0.0001 to 20% by weight, 0.001 to 20% by weight, 0.01 to 20% by weight, 0.05 to 20% by weight, or 0.1 to 20% by weight of fine powder based on the total weight of tea particles. Here, the total weight of tea particles may refer to the total weight of the processed tea product.

[0061] In an example embodiment, the tea particles may have one or more particle size distribution values ​​among the following i) to iii), where the tea particles may refer to processed tea products. i) Particle size distribution D 10 values ​​≥ 50 μm; ii) Particle size distribution D 50 value is 100 μm or more; and iii) Particle size distribution D 90 Value is 200μm or more.

[0062] In the above i) to iii), D 10 , D 50 , D 90 respectively mean the particle size of the bottom 10% of particles in the cumulative distribution, the median particle size, and the particle size of the bottom 90% of particles in the cumulative distribution when the cumulative distribution of particle sizes of tea particles is measured.

[0063] In an exemplary embodiment, the particle size distribution D 10The value may be 50 μm or more, 60 μm or more, 70 μm or more, 80 μm or more, 90 μm or more, or 100 μm or more, and 200 μm or less, 190 μm or less, 180 μm or less, 170 μm or less, 160 μm or less, 150 μm or less, 140 μm or less, 130 μm or less, 120 μm or less, 110 μm or less, or 100 μm or less.

[0064] In an exemplary embodiment, the particle size distribution D 50 The value may be 100 μm or more, 110 μm or more, 120 μm or more, 130 μm or more, 140 μm or more, or 150 μm or more, and 250 μm or less, 240 μm or less, 230 μm or less, 220 μm or less, 210 μm or less, or 200 μm or less.

[0065] In an exemplary embodiment, the particle size distribution D 90 The value may be 200 μm or more, 220 μm or more, 240 μm or more, 260 μm or more, 280 μm or more, or 300 μm or more, and 600 μm or less, 550 μm or less, 500 μm or less, 450 μm or less, 400 μm or less, 350 μm or less, 340 μm or less, 330 μm or less, 320 μm or less, 310 μm or less, or 300 μm or less.

[0066] In an exemplary embodiment, the particle size distribution D 10 Value is 50μm≦D 10 ≦200 μm, and the particle size distribution D 50 Value is 100μm≦D 50 ≦250 μm, and the particle size distribution D 90 Value is 200μm≦D 90 It may be ≦600 μm.

[0067] In an exemplary embodiment, the tea processed product has an angle of repose of 35° or less, preferably 30° or less, which has excellent flowability and fluidity, and is advantageous in terms of ease of product packaging and use. The angle of repose refers to the angle at which tea particles can be stably held when piled up, and the higher the angle of repose, the lower the flowability.

[0068] In an exemplary embodiment, the tea product may have a wetting time when contacted with water of 100 seconds or less, 90 seconds or less, 80 seconds or less, 70 seconds or less, 60 seconds or less, 50 seconds or less, 40 seconds or less, 30 seconds or less, 20 seconds or less, or 10 seconds or less.

[0069] In an exemplary embodiment, the wetting time may be the time it takes for the entire tea product to sink below the surface of water when 1.5 g of the tea product is placed on the surface of water, i.e., the wetting time may mean the time it takes for the entire tea product to be immersed in water when 1.5 g of the tea product is placed quietly on the surface of water without any physical or chemical treatment.

[0070] In one exemplary embodiment, the amount of water may be 500 mL.

[0071] In an exemplary embodiment, the wetting time may be the time it takes for the entire tea product to sink below the surface of the water when 1.5 g of the tea product is placed on the surface of water at room temperature of 15 to 25°C.

[0072] In an exemplary embodiment, the tea product may be in the form of granules or powder.

[0073] In an exemplary embodiment, the processed tea product may be produced by filling processed tea particles into capsules or stick-shaped packets, or by further processing the processed tea particles into effervescent tablets or suspension tablets.

[0074] The processed tea product according to the present specification may be made of 100% tea powder without any binders, etc. In the conventional production of fine granules or granules, a liquid in which a binder is dissolved in water is sprayed onto tea powder, which leaves a cloudy color and a dull aftertaste when dispersed or dissolved in water. However, the processed tea product according to the present specification not only eliminates such factors that hinder palatability, but also has the effect of significantly improving dispersibility in a solvent, for example, water. In addition, since it does not contain binders, it can provide the effects of simplifying the process and improving palatability.

[0075] In another aspect, the technology disclosed herein provides a method for producing a particulate tea product, the method comprising the step of producing the particulate tea product.

[0076] In an example embodiment, the method may produce a tea product using only tea powder and water.

[0077] In an exemplary embodiment, the method may be to manufacture a granular tea product using a rotor-type fluidized bed granulator including a rotor disc. By using the rotor-type fluidized bed granulator including a rotor disc, it is possible to manufacture a granular tea product with excellent dispersibility and flowability using only tea powder and water without using other additives.

[0078] Fluidized bed granulators are generally used for powdering and granulating liquids, granulating powders, coating pharmaceutical ingredients, etc., and are mainly used in the production of food and pharmaceutical products. When considering the general operation method of a fluidized bed granulator, granules having a composition ratio of a designed specification are produced in a fluidized bed where liquid, powder, and granules are fluidized by air pressure. In this specification, a rotor-type fluidized bed granulator is a fluidized bed granulator including a rotating plate, and centrifugal force can be applied to tea powder by the rotation of the rotating plate.

[0079] In an example embodiment, the rotating plate may have an adjustable speed.

[0080] In an example embodiment, the rotor-type fluidized bed granulator may include a container; and a rotating plate installed inside the container.

[0081] In an example embodiment, the rotor-type fluidized bed granulator may include a container; and a horizontal rotating plate installed inside the container, and may supply air to a gap between the rotating plate and a wall of the container.

[0082] In an example embodiment, the rotor-type fluidized bed granulator may spray water into the inside of a vessel through a spray nozzle installed adjacent to a gap through which air is supplied.

[0083] In an example embodiment, the rotor-type fluidized bed granulator may include a gap forming unit provided between a rotating plate and a wall of a vessel through which air is supplied.

[0084] In an example embodiment, the rotor-type fluidized bed granulator may include a nozzle forming unit disposed adjacent to the gap forming unit and configured to inject water into the inside of the vessel and onto the upper portion of the rotating plate.

[0085] In an example embodiment, the nozzle forming part may be configured to spray water upward.

[0086] In an exemplary embodiment, the rotor-type fluidized bed granulator may produce granular tea products at a rotating plate speed of 90 to 1,200 rpm. The rotating plate speed may vary greatly depending on the size of the equipment, for example, in the case of laboratory equipment, the rotating plate is generally small (e.g., the rotating plate diameter of Glatt's GPCG-1 is 30 cm), so it may be operated at a range of about 360 to 1,200 rpm when producing tea particles, and in the case of production equipment with a rotating plate size of 1,200 cm, it may be operated at a range of about 90 to 300 rpm.

[0087] In an exemplary embodiment, the rotating plate may produce a particulate tea product at a tip speed of 2-20 m / sec, 3-20 m / sec, 4-20 m / sec, or 5-20 m / sec to improve the dispersibility and flowability of the tea particles.

[0088] In an exemplary embodiment, the rotor-type fluidized bed granulator may produce a granulated tea product under conditions of an inlet air temperature of 15°C to 40°C, an exhaust air temperature of 10°C to 35°C, a spray nozzle diameter of 1.0 to 2.0 mm, a spray pressure of 1.0 to 5.0 bar and / or a drying temperature of 40°C to 80°C.

[0089] In an exemplary embodiment, the rotor-type fluidized bed granulator may produce a granulated tea product under conditions of an inlet air temperature of 25°C to 35°C, an exhaust air temperature of 15°C to 30°C, a spray nozzle diameter of 1.0 to 2.0 mm, a spray pressure of 1.0 to 3.0 bar and / or a drying temperature of 60°C to 80°C.

[0090] In an exemplary embodiment, the rotor type fluidized bed granulator has an air supply of 150 to 2,000 m 3 / hr or 600~1,000m 3 / hr, and can be appropriately adjusted depending on the scale of the rotor-type fluidized bed granulator.

[0091] In an example embodiment, the method may be a method for producing a granular tea product by injecting water onto tea powder.

[0092] In one illustrative embodiment, the manufacturing method may include the steps of placing tea powder on a rotating plate and rotating the rotating plate to apply centrifugal force to the tea powder; supplying air to levitate the tea powder with the air; injecting water onto the levitated tea powder; and allowing the tea powder that has come into contact with the water to fall by gravity.

[0093] As described above, in the method for producing granular tea products according to the present specification, granular tea products may be produced using three forces: centrifugal force due to the rotation of the rotating plate, buoyancy force due to inlet air passing through the gap between the rotating plate and the wall of the container, and gravity which drops materials onto the rotating plate.

[0094] Conventionally, powders with a particle size of 50 μm or less are too fine, and even when processed in a fluidized bed granulator, the size of the produced particles is limited to a desired size, but the method for producing tea processed products according to the present specification makes it possible to produce tea particles of a desired size in a short time of about 2 hours or less, even when the particle size of tea powder that corresponds to 99% or more by weight based on the total weight of the tea powder is 75 μm or less. The tea processed products produced by this method have excellent dispersibility in solvents and improve the flowability of tea particles, making the product easier to package and use.

[0095] In an exemplary embodiment, in the preparation method, water in an amount corresponding to 0.3 to 1.5 times the mass of the tea powder may be injected onto the tea powder.

[0096] According to an example embodiment, the method may further include removing fine powder having a particle size of 75 μm or less.

[0097] The present invention will be described in more detail below with reference to examples. However, it will be obvious to those skilled in the art that these examples are merely for the purpose of illustrating the present invention and that the scope of the present invention is not limited by these examples.

[0098] Example 1. 600g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a rotor type fluidized bed granulator (GPCG-1, rotor type, Glatt, Germany), and 750g of water was sprayed under the following conditions while measuring the sphericity S 10 The powdered tea product was produced with a value of 0.68 or more. The powder was passed through a 30 mesh (600 μm) sieve. Intake air temperature: 30°C, exhaust air temperature: 23±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, rotor rpm: 540rpm, drying temperature: 70°C.

[0099] Example 2. 600g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a rotor type fluidized bed granulator (GPCG-1, rotor type, Glatt, Germany), and 660g of water was sprayed under the following conditions while measuring the sphericity S 10 The powdered tea product was produced with a value of 0.68 or more. The powder was passed through a 30 mesh (600 μm) sieve. Intake air temperature: 30°C, exhaust air temperature: 23±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, rotor rpm: 540rpm, drying temperature: 70°C.

[0100] Example 3. 600g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a rotor type fluidized bed granulator (GPCG-1, rotor type, Glatt, Germany), and 600g of water was sprayed under the following conditions while measuring the sphericity S 10 The powdered tea product was produced with a value of 0.68 or more. The powder was passed through a 30 mesh (600 μm) sieve. Intake air temperature: 30°C, exhaust air temperature: 23±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, rotor rpm: 720rpm, drying temperature: 70°C.

[0101] Example 4. 600g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a rotor type fluidized bed granulator (GPCG-1, rotor type, Glatt, Germany), and 500g of water was sprayed under the following conditions while measuring the sphericity S 10 The powdered tea product was produced with a value of 0.68 or more. The powder was passed through a 30 mesh (600 μm) sieve. Intake air temperature: 30°C, exhaust air temperature: 23±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, rotor rpm: 360rpm, drying temperature: 50°C.

[0102] Example 5. 600g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a rotor type fluidized bed granulator (GPCG-1, rotor type, Glatt, Germany), and 600g of water was sprayed under the following conditions while measuring the sphericity S 10 The powdered tea product was produced with a value of 0.68 or more. The powder was passed through a 30 mesh (600 μm) sieve. Intake air temperature: 30°C, exhaust air temperature: 23±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, rotor rpm: 720rpm, drying temperature: 65°C.

[0103] Example 6. 600g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a rotor type fluidized bed granulator (GPCG-1, rotor type, Glatt, Germany), and 700g of water was sprayed under the following conditions while measuring the sphericity S 10 The powdered tea product was produced with a value of 0.68 or more. The powder was passed through a 30 mesh (600 μm) sieve. Intake air temperature: 30°C, exhaust air temperature: 23±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 23~28%, rotor rpm: 360rpm, drying temperature: 80°C.

[0104] Example 7. 40 kg of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a rotor type fluidized bed granulator (WBF200 / 120 / 100, Rotor type, Enger, China), and 34 kg of water was sprayed under the following conditions to measure the sphericity S 10 The powdered tea product was produced with a value of 0.68 or more. The powder was passed through a 30 mesh (600 μm) sieve. Intake air temperature: 23℃, exhaust air temperature: 23±5℃, nozzle inner diameter: 1.5mm, spray pressure: 3.0bar, intake air volume: 800m 3 / hr, rotor rpm: 240 rpm, drying temperature: 70°C.

[0105] Comparative Example 1 500g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a top spray fluidized bed granulator (GPCG-1, Top spray type, Glatt, Germany) and 300g of water was sprayed under the following conditions to produce a granular tea product. The tea was also passed through a 30 mesh (600μm) sieve. Intake air temperature: 30°C, exhaust air temperature: 23±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, drying temperature: 70°C.

[0106] Comparative Example 2 475g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a top spray fluidized bed granulator (GPCG-1, Top spray type, Glatt, Germany) and a solution of 25g of maltitol in 485g of water was sprayed under the following conditions to produce a granular tea product. The tea was also passed through a 30mesh (600μm) sieve. Intake air temperature: 50°C, exhaust air temperature: 27±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, drying temperature: 70°C.

[0107] Comparative Example 3. 350g of powdered green tea (Osulloc Farm, Republic of Korea) and 125g of mannitol were mixed and placed in a top spray fluidized bed granulator (GPCG-1, Top spray type, Glatt, Germany), and a solution of 25g of maltitol in 525g of water was sprayed under the following conditions to produce a granular tea product. The tea was also passed through a 30mesh (600μm) sieve. Intake air temperature: 50℃, exhaust air temperature: 25±5℃, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, drying temperature: 70℃.

[0108] Comparative Example 4. 495g of powdered green tea (Osulloc Farm, Republic of Korea) was placed in a top spray fluidized bed granulator (GPCG-1, Top spray type, Glatt, Germany) and a solution of 5g of maltodextrin dissolved in 295g of water was sprayed under the following conditions to produce a granular tea product. The tea was also passed through a 30mesh (600μm) sieve. Intake air temperature: 60°C, exhaust air temperature: 30±5°C, nozzle inner diameter: 1.0mm, spray pressure: 1.0bar, air flap: 25~30%, drying temperature: 70°C.

[0109] Comparative Example 5. Powdered green tea (Osulloc Farm, Republic of Korea) was designated as Comparative Example 5 and was used in the following experimental examples.

[0110] Comparative Example 6. A commercially available product, Rishi Matcha travel packs (Rishi-Tea), was designated as Comparative Example 6 and used in the following experimental examples.

[0111] Comparative Example 7. A commercially available product, Encha organic matcha green tea powder packets (Encha), was designated as Comparative Example 7 and used in the following experimental examples.

[0112] Comparative Example 8. Microcrystalline cellulose (CELLETS® 100, IPC (International Process Center), Germany), which is a commercially available crystalline particle, was used in the following experimental example as Comparative Example 8. The sphericity of the microcrystalline cellulose used in Comparative Example 8 was measured with a particle shape analyzer and shown in Table 1 below, and the microcrystalline cellulose was shown to have a ratio of fine powder with a particle size of 75 μm or less of 0.1% when measured with a particle size analyzer.

[0113] Experimental Example 1. Sphericity Measurement The sphericity of Examples 1 to 7 and Comparative Examples 1 to 8 was measured using a particle shape analyzer (QICPIC450, Sympatec, Germany), and the results are shown in Table 1. The sphericity was measured by dispersing particles in an airflow at a pressure of 2 bar, photographing the projection of each particle using a photographing device, and then measuring the shape of the particle. The sphericity was calculated by dividing the circumference of a circle having the same area as the area of ​​the particle measured from the projection of each particle by the circumference of the actual particle (see the formula below). The sphericity has a value between 0 and 1, and the closer to 1, the more spherical the particle shape is.

[0114]

number

[0115] Experimental Example 2: Particle size analysis Using a particle size analyzer (Mastersizer, Malvern, UK), the particle size distribution, average particle size, and ratio of fine powder having a specific particle size range (75 μm or less) of Examples 1 to 7 and Comparative Examples 1 to 8 were measured, and the results are shown in Table 2.

[0116] Experimental Example 3. Measurement of Wetting Time 1.5 g of each of the samples of Examples 1 to 7 and Comparative Examples 1 to 8 was carefully placed in a beaker containing 500 mL of water at the same temperature as room temperature, and the wetting time until the sample sank to the bottom without solidifying on the water surface was measured, and the results are shown in Table 2 and Figures 1 to 8, 11 and 12. The wetting time was measured by the time until the sample sank to the bottom of the water surface after being left without applying physical force such as stirring or shaking.

[0117] Experimental Example 4: Measurement of angle of repose The samples of Examples 1 to 7 and Comparative Examples 1 to 7 were placed in a funnel, which was fixed to the bottom, and the funnel was gradually raised to form a piled cone-shaped mass. The average diameters of the four piled cones and the heights of the cones were measured, and the angle of repose was calculated using the following formula. The results are shown in Table 2.

[0118]

number

[0119] The angle of repose is an index showing the fluidity (flowability) of particles, and generally, 25° to 30° means very good, 31° to 35° means good, and 36° to 40° means slightly good. The better the fluidity, the easier it is to fill the desired amount of particles when filling capsules or stick packets or compressing them into tablets, which has the advantage of making the process smoother.

[0120] Experimental results.

[0121] [Table 1]

[0122] [Table 2]

[0123] From the above Experimental Example 1, the sphericity S 10 In the cases of Examples 1 to 7 where the value is 0.68 or more, the sphericity S 10 It was confirmed that the wetting time was significantly shorter than that of Comparative Examples 1 to 7, which had a wetting time of less than 0.68. The dispersion speed of the tea processed product according to the present specification in a solvent (e.g., water) was significantly superior to that of powdered green tea or existing powdered green tea granules. In fact, when the tea processed product according to the present specification was placed in a cup, tumbler, water bottle, etc., it was easily dispersed in water and could be conveniently consumed (see Figures 9 and 10).

[0124] In Comparative Examples 2 to 4, where tea products were prepared by adding maltitol or maltodextrin according to a conventional method to improve dispersibility, the wetting time was long and the desired effect could not be achieved. Specifically, in Comparative Examples 2 to 4, no wetting occurred during the measurement of the wetting time (3 minutes), and a considerable amount of the tea products remained on the water surface, and when the tea products were placed in a water bottle and shook, the tea products adhered to the opening of the water bottle, confirming that the wettability was significantly low.

[0125] Even after wetting, the sunken green tea powder or granules of the green tea powder are difficult to disperse and clump together, but the tea processed product according to the present specification has excellent dispersibility and hardly clumps even without shaking or stirring (see Figures 1 to 3). In particular, the wetting time of Example 4 is relatively long compared to Examples 2 and 3, but looking at the photograph taken immediately after measuring the wetting time, it was visually confirmed that the tea processed product was well dispersed in water during wetting, and that the tea processed product containing insoluble substances did not stick to each other or clump together even after being dispersed in water, showing excellent redispersibility.

[0126] As mentioned above, the sphericity S 10 It was confirmed that tea processed products with a value of 0.68 or more can be made of tea powder alone without using additives such as binders and have rapid dispersion characteristics. Such dispersion characteristics were significantly superior to those of Comparative Examples 1 to 7. Therefore, it was confirmed that the sphericity, size and size distribution of particles affect the dispersibility of granular tea processed products, and that the smaller the particle size of the tea processed product, the greater the dispersibility.

[0127] From the above Experimental Example 4, it was confirmed that in the cases of Examples 1 to 7, the flowability was very good, unlike Comparative Examples 1 to 7, which had angles of repose exceeding 35°. Therefore, it was found that the processed tea products according to the present specification have extremely good flowability, and therefore provide the advantage of being easy to package and use.

[0128] In addition, when the samples of Example 1 and Comparative Example 8 were added to water under the same conditions, the tea product of Example 1 was well dispersed in water even after 20 seconds, whereas the crystalline cellulose of Comparative Example 8 sank to the bottom after 20 seconds (see Figures 11 and 12). Thus, although crystalline cellulose had the highest sphericity among the Examples and Comparative Examples, it showed low dispersibility and redispersibility. Therefore, it was confirmed that sphericity and dispersion characteristics are not collectively proportional or inversely proportional, but that the type of particle acts as a factor that affects dispersion characteristics, and that even if the sphericity is high, different dispersion characteristics can be shown depending on the type of particle.

[0129] Although the specific parts of the present invention have been described in detail above, it is clear to those skilled in the art that such specific descriptions are merely preferred embodiments and do not limit the scope of the present disclosure. Therefore, the substantial scope of the present invention is defined by the claims and their equivalents.

Claims

1. A granular tea product using only tea powder and water as raw materials, Particulate tea products consist of tea particles formed by agglomeration of tea powder, The tea particles have a sphericity S of 0.68 to 0.

84. 10 indicates the value, The sphericity S 10 The value is the sphericity of the particles that is in the bottom 10% of the cumulative distribution when the cumulative distribution of the sphericity of tea particles is measured.

2. The sphericity S 10 The particulate tea product according to claim 1, wherein the value is 0.70 or more and 0.83 or less.

3. The sphericity S 10 The particulate tea processed product according to claim 1 or 2, wherein the value is 0.73 to 0.

82.

4. When the cumulative distribution of the sphericity of the tea particles is measured, the sphericity S of the particles corresponding to the bottom 90% of the cumulative distribution is 90 The value and the sphericity S of the particles that fall into the bottom 10% of the cumulative distribution 10 The difference between the values ​​(S 90 -S 10 4. The particulate tea processed product according to any one of claims 1 to 3, wherein the ratio of the saturation temperature to the saturation temperature is less than 0.

20.

5. The S 90 -S 10 The particulate tea product according to claim 4, wherein the β-dispersion coefficient is less than 0.

15.

6. The particulate tea processed product according to any one of claims 1 to 5, wherein the average particle size of the whole tea particles is 100 to 300 μm.

7. The particulate tea processed product according to any one of claims 1 to 6, comprising 20% ​​by mass or less of fine powder based on the total mass of the tea particles, and the fine powder has a particle diameter of 75 μm or less.

8. The particulate tea processed product according to any one of claims 1 to 7, wherein the tea particles have one or more particle size distribution values ​​of the following i) to iii): i) Particle size distribution D 10 value is 50 μm or more; ii) Particle size distribution D 50 a value of 100 μm or more; and iii) Particle size distribution D 90 Value is 200 μm or more. In the above i) to iii), D 10 , D 50 , D 90 respectively mean the particle size of the particles corresponding to the bottom 10% of the cumulative distribution, the median particle size, and the particle size of the particles corresponding to the bottom 90% of the cumulative distribution when the cumulative distribution of particle sizes of tea particles is measured.

9. The particle size distribution D 10 The value is 50 μm≦D 10 ≦200 μm, and the particle size distribution D 50 The value is 100 μm≦D 50 ≦250 μm, and the particle size distribution D 90 The value is 200 μm≦D 90 9. The particulate tea product according to claim 8, having a size of ≦600 μm.

10. The particulate tea processed product according to any one of claims 1 to 9, wherein the tea processed product has an angle of repose of 35° or less.

11. The particulate tea processed product according to any one of claims 1 to 10, wherein the wetting time of the tea processed product when contacted with water is 100 seconds or less, and the wetting time is the time required for the entire tea processed product to sink below the surface of the water when 1.5 g of the tea processed product is placed on the surface of the water.

12. The particulate tea processed product according to any one of claims 1 to 11, wherein the tea is tea leaves.

13. The particulate tea processed product according to any one of claims 1 to 12, wherein the tea is one or more selected from the group consisting of unfermented tea, semi-fermented tea, fermented tea, and post-fermented tea.

14. The particulate tea product according to claim 13, wherein the tea is green tea.

15. The particulate tea processed product according to any one of claims 1 to 14, wherein the tea processed product is a granular product or a powder.

16. A method for producing a particulate tea product comprising the step of producing a particulate tea product according to any one of claims 1 to 15.

17. The method for producing a granulated tea product according to claim 16, wherein the granulated tea product is produced in a rotor-type fluidized bed granulator including a rotating plate.

18. The method for producing a granulated tea product according to claim 17, wherein the rotor-type fluidized bed granulator comprises a container; and a rotating plate installed inside the container, a gap forming section installed between the rotating plate and a wall of the container through which air is supplied, and a nozzle forming section installed adjacent to the gap forming section and which sprays water into the inside of the container.

19. The method for producing the granular tea product according to any one of claims 16 to 18, comprising the steps of: placing tea powder on a rotating plate and rotating the rotating plate; supplying air to levitate the tea powder; and spraying water onto the levitated tea powder.

20. The method for producing a granulated tea product according to claim 19, wherein the tea powder has a particle size of 75 μm or less, which corresponds to 99% by mass or more of the total mass of the tea powder.

Citation Information

Patent Citations

  • Flavoring granules

    JP2000513204A

  • Method for inhibiting aggregation of tea leaf powder

    JP2011125297A

  • Granulated tea leaf and method for producing the same

    JP2019041660A

  • Method of preparing the granular green tea powder

    KR1020060090894A