Holding device

The holding device with an annular convex portion and multiple pressure sensors addresses the issue of inaccurate gas pressure detection in electrostatic chucks, enabling precise maintenance timing prediction and stable heat transfer.

JP7576425B2Active Publication Date: 2024-10-31NITERRA CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020175224
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-19
Publication Date
2024-10-31
Estimated Expiration
2040-10-19

AI Technical Summary

Technical Problem

Existing electrostatic chucks face issues with inaccurate detection of gas pressure between the wafer and the chuck surface, leading to deteriorated sealing performance and reduced heat transfer due to surface wear, making it difficult to predict maintenance timing and lifespan.

Method used

A holding device with an annular convex portion and gas holes, equipped with multiple pressure sensors to accurately detect gas pressure at various locations, allowing for precise monitoring of sealing performance and predicting maintenance needs.

Benefits of technology

Enables accurate prediction of maintenance timing and lifespan by monitoring gas pressure, ensuring stable heat transfer and effective removal of heat from the wafer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007576425000001
    Figure 0007576425000001
  • Figure 0007576425000002
    Figure 0007576425000002
  • Figure 0007576425000003
    Figure 0007576425000003
Patent Text Reader

Abstract

To provide a holding device which can estimate the timing when a plate-like member holding an object needs maintenance or the life of the plate-shaped member.SOLUTION: A holding device comprises an electrostatic chuck 1 having a ceramic member 10. The ceramic member 10 includes an upper surface 11 to hold a semiconductor wafer W, a circular-shaped convex part 14 which is formed along an outer periphery 13a of a facing region 13 facing the semiconductor wafer W on the upper surface 11, and a gas opening 18 on the upper surface 11 to supply gas to the upper surface 11. The ceramic member 10 also includes a plurality of pressure sensors 51 to detect a pressure of gas supplied to the upper surface 11.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a holding device for holding an object. [Background technology]

[0002] As a conventional technique related to a holding device, Patent Document 1 discloses an electrostatic chuck in which a gas is supplied between the surface of the electrostatic chuck and a wafer attracted and held by the electrostatic chuck, and in this electrostatic chuck, the gas pressure is detected by a pressure detector in a gas supply pipe that supplies the gas. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5003102 Summary of the Invention [Problem to be solved by the invention]

[0004] When the surface of the electrostatic chuck deteriorates over time, the gas sealing performance between the wafer and the surface of the electrostatic chuck may decrease, and the pressure of the gas filled between the wafer and the surface of the electrostatic chuck may decrease. This may decrease the heat transfer performance between the wafer and the electrostatic chuck, making it difficult to properly remove heat from the wafer. Therefore, it is necessary to perform maintenance on the surface of the electrostatic chuck, or to replace the electrostatic chuck if the electrostatic chuck has reached the end of its life.

[0005] In the electrostatic chuck disclosed in Patent Document 1, a pressure detector is provided in a gas supply pipe, so the gas pressure in the gas supply pipe can be detected, but the pressure of the gas filling the gap between the wafer and the surface of the electrostatic chuck cannot be accurately detected. Therefore, even if the gas sealing performance between the wafer and the surface of the electrostatic chuck is reduced due to deterioration of the surface of the electrostatic chuck over time, causing a reduction in the pressure of the gas filling the gap between the wafer and the surface of the electrostatic chuck, this cannot be accurately detected, and therefore the maintenance timing and lifespan of the electrostatic chuck cannot be predicted.

[0006] Therefore, the present disclosure has been made to solve the above-mentioned problems, and aims to provide a holding device that can predict the maintenance timing and lifespan of a plate-like member, such as an electrostatic chuck, that holds an object such as a semiconductor wafer. [Means for solving the problem]

[0007] One aspect of the present disclosure made to solve the above problems is a holding device having a plate-shaped member including a surface for holding an object, an annular convex portion formed in a ring shape along an outer periphery near an outer periphery of a facing region of the surface facing the object, and a gas hole opening in the surface and supplying a gas to the surface, the plate-shaped member including: A gas intake passage that opens to the surface and can take in the gas supplied to the surface is provided separately from the gas hole, and the gas taken in through the gas intake passage The pressure sensor for detecting the pressure of the gas may be provided in plurality.

[0008] According to this aspect, by detecting and monitoring the pressure of the gas supplied to the surface using a pressure sensor, the gas sealing ability between the object and the annular convex portion can be determined, and the maintenance timing and lifespan of the ceramic component can be predicted.

[0009] Furthermore, since the pressure sensor is provided on the ceramic member and is provided at a position close to the object and the surface, the pressure of the gas supplied to the surface can be accurately detected by the pressure sensor.

[0010] In addition, since multiple pressure sensors are provided, the gas pressure can be detected at multiple locations in the ceramic member, and therefore, by detecting and monitoring the gas pressure at multiple locations along the circumferential direction of the annular convex portion with the multiple pressure sensors, it is possible to determine the gas sealing performance between the object and the annular convex portion over the entire circumferential direction of the annular convex portion.

[0011] In the above aspect, it is preferable that the plate-shaped member has a base member that is thermally connected to a back surface thereof opposite the front surface, the base member having a through hole for passing an extension wire of the pressure sensor, and the multiple extension wires of the pressure sensor are passed through the through hole and concentrated.

[0012] According to this aspect, the number of through holes that become temperature singular points in the base member can be reduced, and therefore heat transfer between the plate-like member and the base member can be ensured, thereby allowing stable heat removal from the object.

[0013] In the above aspect, it is preferable that the surface has a plurality of convex portions formed inwardly of the annular convex portion, and the detection position of the pressure sensor is a first position between the annular convex portion and the convex portion closest to the annular convex portion.

[0014] According to this aspect, the gas pressure at a position close to the annular convex portion can be detected and monitored by the pressure sensor, so that the gas sealing property between the object and the annular convex portion can be determined more accurately.

[0015] In the above aspect, it is preferable that the detection position of the pressure sensor is further set to a second position which is more inward on the surface than the first position.

[0016] According to this aspect, the pressure sensor can detect the gas pressure at a position close to the annular convex portion as well as the gas pressure at a position distant from the annular convex portion, and therefore the difference in gas pressure between the position close to the annular convex portion and the position distant from the annular convex portion can be monitored to determine the gas sealing ability between the object and the annular convex portion. Effect of the Invention

[0017] According to the holding device of the present disclosure, it is possible to predict the maintenance timing and lifespan of the plate-like member that holds an object. [Brief description of the drawings]

[0018] [Figure 1] FIG. 1 is a perspective view of an electrostatic chuck according to an embodiment of the present invention. [Diagram 2] 2 is a cross-sectional view (XZ cross-sectional view in FIG. 1) of the electrostatic chuck of the present embodiment. [Diagram 3] FIG. 3 is an enlarged view of a region α in FIG. [Figure 4] 1 is a plan view of an electrostatic chuck according to an embodiment of the present invention (as viewed in the Z-axis direction (planar view)). [Diagram 5] 10 is a cross-sectional view (XZ cross-sectional view in FIG. 1) of the electrostatic chuck of the present embodiment, showing an example in which a pressure sensor and a gas inlet are also disposed at inner positions on the upper surface. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] A holding device according to an embodiment of the present disclosure will be described below. In this embodiment, an electrostatic chuck 1 for holding a semiconductor wafer W as an object will be described as an example of the holding device.

[0020] <Overall explanation of electrostatic chuck> The electrostatic chuck 1 of this embodiment is a device that attracts and holds a semiconductor wafer W (object) by electrostatic attraction, and is used, for example, to fix the semiconductor wafer W in a vacuum chamber of a semiconductor manufacturing device. As shown in Fig. 1, the electrostatic chuck 1 has a ceramic member 10, a base member 20, and a bonding layer 30 that bonds the ceramic member 10 and the base member 20. The ceramic member 10 is an example of a "plate-like member" in the present disclosure.

[0021] In the following description, for convenience of explanation, the X, Y and Z axes are defined as shown in Fig. 1. Here, the Z axis is an axis in the axial direction of the electrostatic chuck 1 (a direction along the central axis AX, the vertical direction in Fig. 1), and the X and Y axes are axes in the radial directions of the electrostatic chuck 1.

[0022] As shown in FIG. 1, the ceramic member 10 is a disk-shaped member and is made of ceramics. Specifically, the ceramic member 10 has a stepped disk shape in which two disks of different diameters are overlapped with a common central axis (specifically, a disk-shaped upper part having a smaller diameter is overlapped on a disk-shaped lower part having a larger diameter). As the ceramic, various ceramics are used, but from the viewpoint of strength, abrasion resistance, plasma resistance, etc., it is preferable to use ceramics whose main component is, for example, aluminum oxide (alumina, Al2O3) or aluminum nitride (AlN). Note that the main component here means a component with the highest content (for example, a component with a volume content of 90 vol% or more).

[0023] 1 and 2, the ceramic member 10 has an upper surface 11 provided on the side that holds a semiconductor wafer W, and a lower surface 12 (rear surface) provided on the opposite side to the upper surface 11 in the thickness direction (a direction that coincides with the Z-axis direction, the up-down direction) of the ceramic member 10. Note that the upper surface 11 is an example of the "front surface" in the present disclosure, and the lower surface 12 is an example of the "rear surface" in the present disclosure.

[0024] The ceramic member 10 has a diameter of, for example, about 150 to 300 mm at the upper portion and about 180 to 350 mm at the lower portion. The ceramic member 10 has a thickness of, for example, about 2 to 6 mm. The ceramic member 10 desirably has a thermal conductivity in the range of 10 to 50 W / mK (more preferably, 18 to 30 W / mK).

[0025] The upper surface 11 of the ceramic member 10 has an uneven shape. Specifically, as shown in Fig. 2 and Fig. 4, an annular convex portion 14 is formed on the upper surface 11 in the vicinity of the outer periphery 13a of the facing region 13 facing the semiconductor wafer W, and the annular convex portion 14 is formed in a ring shape along the outer periphery 13a. In addition, a plurality of independent columnar convex portions 15 are formed on the upper surface 11 on the inside of the annular convex portion 14.

[0026] The annular protrusion 14 is formed in an annular shape at a position on the outer periphery side of the plurality of protrusions 15 on the upper surface 11 of the ceramic member 10 so as to surround all of the protrusions 15. This annular protrusion 14 is also called a seal band. The cross section (XZ cross section) of the annular protrusion 14 has a substantially rectangular shape as shown in FIG. 2. The height (dimension in the Z-axis direction) of the annular protrusion 14 is, for example, about 10 μm to 20 μm. The width (dimension in the X-axis direction) of the annular protrusion 14 is, for example, about 0.5 mm to 5.0 mm.

[0027] As shown in FIG. 4, each of the protrusions 15 has a substantially circular shape when viewed in the Z-axis direction (plan view), and is disposed at substantially equal intervals. The shape of the cross section (XZ cross section) of each of the protrusions 15 is substantially rectangular, as shown in FIG. 2. The height of the protrusions 15 is substantially the same as the height of the annular protrusion 14, and is, for example, about 10 to 20 μm. The width of the protrusions 15 (maximum diameter of the protrusions 15 when viewed in the Z-axis direction) is, for example, about 0.5 to 1.5 mm. The portion of the upper surface 11 of the ceramic member 10 inside the annular protrusion 14 where the protrusions 15 are not formed is a recess 16. The protrusions 15 are also called mesas.

[0028] 2, the semiconductor wafer W is supported by the annular convex portion 14 and the multiple convex portions 15 on the upper surface 11 of the ceramic member 10, specifically, by the holding portion 14a at the upper end of the annular convex portion 14 and the holding portion 15a at the upper ends of the multiple convex portions 15, and is held by the electrostatic chuck 1. When the semiconductor wafer W is held by the electrostatic chuck 1, a space S exists between the surface (lower surface) of the semiconductor wafer W and the upper surface 11 of the ceramic member 10 (specifically, the recess 16 of the upper surface 11) (see FIG. 2). A gas (for example, an inert gas such as helium gas) is supplied to this space S.

[0029] The ceramic member 10 also includes a chuck electrode 17 (adsorption electrode) therein. The chuck electrode 17 is substantially circular when viewed in the Z-axis direction, and is made of a conductive material (e.g., tungsten, molybdenum, etc.). When a voltage is applied to the chuck electrode 17 from a power source (not shown), an electrostatic attraction is generated in the chuck electrode 17, and the semiconductor wafer W is attracted to and held on the upper surface 11 by the electrostatic attraction.

[0030] The ceramic member 10 also has a gas hole 18 that opens to the upper surface 11 and supplies gas to the upper surface 11 to fill the space S with gas. The gas hole 18 is connected to a gas supply source (not shown) via a gas supply path 41 that is formed by penetrating the bonding layer 30 and the base member 20.

[0031] The base member 20 is cylindrical, for example, as shown in Fig. 1, and more specifically, as shown in Fig. 2, is a stepped cylindrical shape formed by stacking two cylinders of different diameters, with the lower surface of the smaller diameter cylinder placed on the upper surface of the larger diameter cylinder, with a common central axis AX. The base member 20 is preferably made of a metal (e.g., aluminum or an aluminum alloy), but may be made of a material other than metal. An O-ring 42 is disposed between the outer periphery of the ceramic member 10 and the outer periphery of the base member 20.

[0032] 1 and 2, the base member 20 has an upper surface 21 and a lower surface 22 provided on the opposite side to the upper surface 21 in the thickness direction (the direction corresponding to the Z-axis direction, the up-down direction) of the base member 20. The upper surface 21 of the base member 20 is thermally connected to the lower surface 12 of the ceramic member 10 via a bonding layer 30.

[0033] The diameter of the base member 20 is, for example, about 75 to 345 mm at the upper portion and about 180 to 350 mm at the lower portion. The thickness (dimension in the Z-axis direction) of the base member 20 is, for example, about 20 mm to 50 mm. The thermal conductivity of the base member 20 (assumed to be aluminum) is desirably within the range of 180 to 250 W / mK (preferably about 230 W / mK).

[0034] 2, the base member 20 is formed with a coolant flow passage 23 for flowing a coolant (e.g., a fluorine-based inert liquid, water, etc.). The coolant flow passage 23 is connected to a supply port and a discharge port (not shown) provided on the lower surface 22 of the base member 20, and the coolant supplied to the base member 20 from the supply port flows through the coolant flow passage 23 and is discharged from the discharge port to the outside of the base member 20. In this way, the base member 20 is cooled by flowing the coolant through the coolant flow passage 23 of the base member 20, and the ceramic member 10 is cooled through the bonding layer 30. As a result, the semiconductor wafer W is cooled by the ceramic member 10, that is, heat is transferred between the ceramic member 10 and the semiconductor wafer W, and heat is removed from the semiconductor wafer W.

[0035] In this embodiment, the base member 20 has a through hole 24 for passing an extraction wire 52 of a pressure sensor 51 described later.

[0036] The bonding layer 30 is disposed between the lower surface 12 of the ceramic member 10 and the upper surface 21 of the base member 20, and bonds the ceramic member 10 to the base member 20. The bonding layer 30 has a through hole 31 for passing a lead wire 52 of a pressure sensor 51 described later.

[0037] The bonding layer 30 is made of an adhesive material such as silicone resin, acrylic resin, or epoxy resin. The thickness (dimension in the Z-axis direction) of the bonding layer 30 is, for example, about 0.1 to 1.0 mm. The thermal conductivity of the bonding layer 30 is, for example, 1.0 W / mK. The thermal conductivity of the bonding layer 30 (assuming a silicone resin) is preferably within a range of 0.1 to 2.0 W / mK (preferably 0.5 to 1.5 W / mK).

[0038] <Regarding detection of pressure of gas filled in space> Next, detection of the pressure of the gas filled in the space S will be described.

[0039] The upper surface 11 of the ceramic member 10 deteriorates over time due to contact with the semiconductor wafer W, contact with cleaning plasma, and the like, and its condition changes. In particular, the annular protrusion 14 on the upper surface 11 has the role of sealing the gas filling the space S existing between the semiconductor wafer W and the upper surface 11 from the atmosphere outside the ceramic member 10 when the semiconductor wafer W is held in contact with the upper surface 11.

[0040] Therefore, if the state of the annular protrusion 14, i.e., the surface state or shape of the annular protrusion 14, changes, the contact state between the semiconductor wafer W and the annular protrusion 14 changes, and there is a risk that the gas sealing performance between the semiconductor wafer W and the annular protrusion 14 will decrease. If this happens, the gas filled in the space S will leak to the outside of the ceramic member 10, the pressure of the gas filled in the space S will decrease, and the heat transferability between the semiconductor wafer W and the ceramic member 10 (i.e., the heat transferability between the semiconductor wafer W and the ceramic member 10 via the gas filled in the space S) will decrease, making it difficult to properly remove heat from the semiconductor wafer W.

[0041] Therefore, if the upper surface 11 of the ceramic member 10 deteriorates over time, and in particular the condition of the annular protrusion 14 changes, causing a decrease in the gas sealing ability between the semiconductor wafer W and the annular protrusion 14, it will be necessary to perform maintenance on the upper surface 11 of the ceramic member 10, or to replace the ceramic member 10 if it has reached the end of its life.

[0042] Therefore, in this embodiment, in order to enable maintenance and replacement of the ceramic member 10 at the appropriate time, the pressure of the gas filled in the space S is detected and monitored, and the degree of deterioration of the gas sealing property between the semiconductor wafer W and the annular convex portion 14 is determined, making it possible to predict the maintenance timing and lifespan of the ceramic member 10.

[0043] 2 to 4, the ceramic member 10 is provided with a pressure sensor 51 that detects the pressure of the gas supplied to the upper surface 11 through the gas hole 18 and filling the space S. The pressure sensor 51 is, for example, a sensor that uses a piezoelectric element.

[0044] More specifically, as shown in Figures 2 and 3, the ceramic member 10 has a recessed portion 61 formed on the lower surface 12 of the ceramic member 10 so as to be recessed toward the upper surface 11, and the pressure sensor 51 is disposed in this recessed portion 61.

[0045] The countersunk portion 61 communicates with the space S via a gas intake passage 62 that connects the countersunk portion 61 and the recess 16. As a result, the gas filled in the space S is taken into the countersunk portion 61 through the gas intake passage 62, so that the pressure of the gas filled in the space S can be detected by the pressure sensor 51 disposed in the countersunk portion 61.

[0046] In this embodiment, the gas intake port 62a, which is an inlet on the recess 16 side of the gas intake passage 62, is provided at a position of the recess 16 (hereinafter referred to as the "outer peripheral recess 16a") between the annular convex portion 14 and the protrusion 15 closest to the annular convex portion 14 in the radial direction (X-axis direction in FIG. 2) of the ceramic member 10. Thus, the pressure of the gas in the space S at the position of the outer peripheral recess 16a close to the annular convex portion 14 is detected by the pressure sensor 51. That is, the detection position of the pressure sensor 51 is the position of the outer peripheral recess 16a close to the annular convex portion 14 (an example of the "first position" in this disclosure).

[0047] 2, the gas intake passage 62 may be bent midway toward the outer periphery in the radial direction of the ceramic member 10, and the gas intake port 62a may be provided at a position closer to the annular protrusion 14 in the outer periphery-side recess 16a. This allows the pressure sensor 51 to detect the gas pressure at a position closer to the annular protrusion 14.

[0048] Further, the position where the pressure sensor 51 is disposed is not particularly limited, but is desirably a position on the outer periphery close to the gas inlet 62a in the radial direction of the ceramic member 10, as shown in Fig. 2. This allows the length of the gas inlet passage 62 to be as short as possible, making it easier to take in the gas in the space S into the countersunk portion 61, improving the detection accuracy of the pressure sensor 51. Furthermore, the number of steps required to form the gas inlet passage 62 can be reduced, thereby reducing the manufacturing cost of the ceramic member 10.

[0049] In this embodiment, a plurality of pressure sensors 51 are provided, and therefore a plurality of gas intake ports 62a (gas intake passages 62) are also provided. Specifically, for example, as shown in Fig. 4, as viewed in the Z-axis direction (plan view), four pressure sensors 51 and four gas intake ports 62a are provided at equal intervals in the circumferential direction of the ceramic member 10, i.e., along the circumferential direction of the annular convex portion 14, at positions close to the annular convex portion 14. The number of pressure sensors 51 and gas intake ports 62a is not particularly limited as long as there are a plurality of them, and may be, for example, six, eight, or twelve.

[0050] In addition, in this embodiment, as shown in FIG. 3, two lead wires 52, which are output lines that transmit the output of the pressure sensor 51, are passed through one through hole 24 of the base member 20 and are collected at one output terminal 53 provided at a position on the lower surface 22 side of the through hole 24.

[0051] Here, the lead wire 52 is composed of a via 54a, a conductor 54, and a via 54b wired inside the ceramic member 10, a pin terminal 55 connected to the via 54b and a terminal pad (not shown), and a conductor 56a of a connection terminal 56 electrically connected to the pin terminal 55. The pressure sensor 51 is connected to the output terminal 53 through the lead wire 52. More specifically, in the lead wire 52, the via 54a electrically connected to the electrode 51a of the pressure sensor 51 is connected to one end of the conductor 54. The via 54b connected to the other end of the conductor 54 is connected to a terminal pad (not shown), and the pin terminal 55 is connected to the terminal pad by, for example, brazing. The pin terminal 55 and the output terminal 53 are connected by the conductor 56a.

[0052] In this manner, the output of the pressure sensor 51 (i.e., the detected gas pressure value) can be obtained from the output terminal 53. The detected gas pressure value thus obtained is then monitored. For example, the difference between the detected gas pressure values ​​of the multiple pressure sensors 51, or the difference between the detected gas pressure value by the gas supply path 41 obtained by a pressure detection unit (not shown) and the detected gas pressure value by the pressure sensor 51 is monitored. This makes it possible to determine the gas sealing performance between the semiconductor wafer W and the annular convex portion 14 and to predict the maintenance timing and lifespan of the ceramic member 10.

[0053] 5, the gas intake port 62a of the gas intake passage 62 may be provided at the position of the inner circumferential recess 16b on the upper surface 11, which is more inward than the position of the outer circumferential recess 16a, in addition to the position of the outer circumferential recess 16a in the radial direction of the ceramic member 10. That is, the detection position of the pressure sensor 51 may be the position of the inner circumferential recess 16b (an example of the "second position" in the present disclosure) in addition to the position of the outer circumferential recess 16a.

[0054] Furthermore, the lead wires 52 of the multiple pressure sensors 51 may be passed through one through hole 24 of the base member 20 and collected at one output terminal 53. For example, as shown in FIG. 5, a total of six lead wires 52 drawn from three pressure sensors 51 may be passed through one through hole 24 of the base member 20 and collected at one output terminal 53.

[0055] <Effects of this embodiment> According to this embodiment, the ceramic member 10 is provided with multiple pressure sensors 51 that detect the pressure of gas supplied to the upper surface 11 through the gas holes 18 and filling the space S between the semiconductor wafer W and the upper surface 11.

[0056] In this way, by detecting and monitoring the pressure of the gas filled in the space S between the semiconductor wafer W and the upper surface 11 using the pressure sensor 51, the gas sealing ability between the semiconductor wafer W and the annular convex portion 14 can be determined, and the maintenance timing and lifespan of the ceramic member 10 can be predicted.

[0057] In addition, since the pressure sensor 51 is provided in the ceramic member 10 rather than in the gas supply path 41 provided in the base member 20 and the bonding layer 30, and is provided at a position close to the semiconductor wafer W and the upper surface 11, the pressure of the gas filled in the space S can be detected more accurately.

[0058] Furthermore, since a plurality of pressure sensors 51 are provided, the gas pressure can be detected at a plurality of locations in the ceramic member 10. Therefore, by arranging a plurality of gas inlets 62a along the circumferential direction of the annular convex portion 14 near the annular convex portion 14 and detecting and monitoring the gas pressure at a plurality of locations along the circumferential direction of the annular convex portion 14 with the plurality of pressure sensors 51, the gas sealing property between the semiconductor wafer W and the annular convex portion 14 can be determined over the entire circumferential direction of the annular convex portion 14.

[0059] In addition, by controlling the amount of gas supplied to the space S based on the gas pressure detected by the pressure sensor 51 and controlling the pressure of the gas filled in the space S, it is possible to maintain the thermal conductivity between the semiconductor wafer W and the ceramic member 10.

[0060] Furthermore, two lead wires 52 of the pressure sensor 51 are passed through one through hole 24 of the base member 20 and are integrated into one output terminal 53 provided at a position on the lower surface 22 side of the through hole 24.

[0061] This eliminates the need to provide a through hole 24 in the base member 20 for each lead wire 52, and therefore reduces the number of through holes 24 that become temperature singular points in the base member 20. This ensures heat transfer between the ceramic member 10 and the base member 20. This allows stable heat extraction from the semiconductor wafer W.

[0062] The detection position of the pressure sensor 51 is set to the position of the outer peripheral recess 16 a between the annular protrusion 14 and the protrusion 15 closest to the annular protrusion 14 .

[0063] This allows the pressure sensor 51 to detect and monitor the gas pressure at a position close to the annular convex portion 14. Therefore, the gas sealing performance between the semiconductor wafer W and the annular convex portion 14 can be determined more accurately.

[0064] Furthermore, the detection position of the pressure sensor 51 may be the position of the outer circumferential recess 16a and also the position of the inner circumferential recess 16b which is further inward than the position of the outer circumferential recess 16a.

[0065] This allows the pressure sensor 51 to detect not only the gas pressure at a position close to the annular convex portion 14, but also the gas pressure at a position distant from the annular convex portion 14. Therefore, by monitoring the difference in the detected gas pressure at a position close to the annular convex portion 14 and a position distant from the annular convex portion 14, the gas sealing performance between the semiconductor wafer W and the annular convex portion 14 can be determined.

[0066] It should be noted that the above-described embodiments are merely examples and do not limit the present disclosure in any way. Needless to say, various improvements and modifications are possible without departing from the spirit and scope of the present disclosure. [Explanation of symbols]

[0067] 1. Electrostatic chuck 10 Ceramic materials 11 Top side 12 Bottom side 13 Face-to-face area 13a Outer circumference 14 Annular protrusion 15 Convex 16 Recess 16a Outer circumferential recess 16b Inner circumference recess 18 Gas Vent 20 Base material 21 Top side 22 Bottom side 24 Through hole 30 Bonding layer 31 Through hole 41 Gas supply line 51 Pressure Sensor 51a electrode 52 Lead Line 53 Output terminal 54 Conductor 54a Via 54b Via 55-pin terminal 56 Connection terminal 56a conductor 61 Counterbore 62 Gas intake passage 62a Gas intake W Semiconductor wafer AX center axis S space

Claims

1. A holding device having a plate-like member including a surface for holding an object, an annular convex portion formed in a ring shape along an outer periphery near an outer periphery of a facing region of the surface facing the object, and a gas hole opening in the surface and supplying a gas to the surface, The plate-like member includes: a gas intake passage that opens to the surface and is capable of taking in the gas supplied to the surface is provided separately from the gas hole; a plurality of pressure sensors are provided to detect the pressure of the gas taken in through the gas intake passage; A holding device comprising:

2. 2. The holding device of claim 1, a base member that is thermally connected to a back surface of the plate-like member that is provided on the opposite side to the front surface, the base member has a through hole for passing a lead wire of the pressure sensor, the plurality of lead wires of the pressure sensor are passed through the through hole and collected together; A holding device comprising:

3. The holding device according to claim 1 or 2, a plurality of convex portions formed on the surface on the inner side of the annular convex portion; a detection position of the pressure sensor being a first position between the annular convex portion and the convex portion closest to the annular convex portion; A holding device comprising:

4. The holding device according to claim 3, a detection position of the pressure sensor is further set to a second position on the surface that is more inward than the first position; A holding device comprising:

Citation Information

Patent Citations

  • JP1975003102A

  • Plasma processing device

    JP1995106095A

  • Semiconductor manufacturing equipment

    JP2002141332A

  • Plasma processing apparatus, substrate holding mechanism, and substrate position shift detecting method

    JP2011243834A

  • Electrostatic chuck

    JP2016076646A